Inkjet recording method, ink, and recording media set
By using yellow ink with controlled aluminum content and dispersants, the issue of sedimentation in inkjet inks is mitigated, ensuring stable ejection and improved storage stability, thus preventing nozzle clogging.
Patent Information
- Application Number
- JP2024055955
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-11
AI Technical Summary
Yellow inkjet inks face issues with sedimentation of water-insoluble colorants, leading to clogging of inkjet head nozzles and impaired storage stability, which are not adequately addressed by existing technologies.
The use of yellow ink containing a water-insoluble colorant with less than 400 ppm of aluminum compounds, preferably aluminum hydroxide, along with a dispersant and other components, to minimize sedimentation and ensure stable ejection.
The solution significantly reduces sedimentation, preventing nozzle clogging and ensuring stable ink delivery, thereby enhancing the storage stability and performance of inkjet recording devices.
Smart Images

Figure 2024144393000001
Abstract
Description
[Technical field]
[0001] The present invention relates to an inkjet recording method, an ink, and a recording medium set. [Background technology]
[0002] Among various color printing methods, the printing method using an inkjet printer, which is one of the most representative methods, generates small droplets of ink and deposits them on a printing medium such as paper to perform printing. In recent years, demand for inkjet printers for industrial use has increased, and there is a demand for inks that can be used for printing on a variety of printing media.
[0003] In recent years, the development of technology to meet the demands of higher image resolution and faster printing speeds has led to higher nozzle density and finer internal structures in inkjet heads. For this reason, inkjet recording devices that employ ink circulation mechanisms to prevent ink discharge defects caused by ink settling and drying of the nozzles have also been developed (for example, Patent Document 1, etc.).
[0004] There is an increasing demand for inkjet inks that can deal with such changes. In particular, since water-insoluble colorants are present in an uneven state in the ink, the water-insoluble colorants may settle out during long-term storage. If the water-insoluble colorants settle out, the storage stability is impaired, and the risk of clogging the inkjet head increases. In order to reduce such risks, inks containing water-insoluble colorants with excellent ejection stability have also been developed (for example, Patent Document 2, etc.). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2018-075751 A [Patent Document 2] Re-tabled publication 2015 / 152291 Summary of the Invention [Problem to be solved by the invention]
[0006] However, it has been found that even with such a composition, sedimentation occurs in the yellow ink, causing problems such as clogging of the inkjet head nozzles, and the above-mentioned requirements may not be met.
[0007] The present invention has been made in consideration of the above circumstances, and has an object to provide an inkjet recording method that uses a yellow ink having excellent storage stability in which sedimentation of a water-insoluble colorant is significantly reduced, and a yellow ink and a recording media set for use therein. [Means for solving the problem]
[0008] The present inventors conducted extensive research to solve the above-mentioned problems and discovered that the above-mentioned problems can be solved by using a yellow ink in which the amount of an aluminum compound contained in a water-insoluble colorant is controlled, thereby completing the present invention.
[0009] That is, the present invention relates to the following [1] to [5]. [1] An inkjet recording method for recording with an inkjet recording apparatus using a yellow ink containing a water-insoluble colorant, comprising: an inkjet recording method comprising a discharge step of discharging the yellow ink onto a recording medium by a discharge head to perform recording, wherein the insoluble colorant contains an aluminum compound in an amount of less than 400 ppm. [2] The ink-jet recording method according to [1], wherein the water-insoluble colorant is C.I. Pigment Yellow 74. [3] The ink-jet recording method according to [1], wherein all or a part of the aluminum compound is aluminum hydroxide. [4] The inkjet recording method according to [1], wherein the inkjet recording apparatus is provided with a circulation mechanism for circulating the yellow ink between a container for storing yellow ink and the ejection head, or within the ejection head, and further includes a circulation step of circulating the yellow ink by the circulation mechanism before being subjected to the ejection step. [5] The inkjet recording method according to [1], wherein the recording medium is a recording medium that is poorly ink-absorbent or non-ink-absorbent. [6] A yellow ink for ink-jet recording, comprising a water-insoluble colorant, the water-insoluble colorant containing less than 400 ppm of an aluminum compound. [7] A recording media set comprising the yellow ink according to [6] and a recording medium. Effect of the Invention
[0010] The present invention can provide an inkjet recording method using a yellow ink having excellent storage stability in which sedimentation of a water-insoluble colorant is significantly reduced, and a yellow ink and a recording medium set used therein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention will be described in detail below. The inkjet recording method according to the present invention is an inkjet recording method for recording by an inkjet recording apparatus using yellow ink, and includes a discharge step of discharging the yellow ink from a discharge head onto a recording medium for recording.
[0012] <Yellow ink> The yellow ink (hereinafter also simply referred to as "ink") used in the inkjet recording method of the present invention contains a water-insoluble colorant, and optionally further contains other components such as a dispersant, a surfactant, and ink preparation agents.
[0013] [Water-insoluble colorants] The water-insoluble colorant is characterized by including a yellow colorant and containing less than 400 ppm of an aluminum compound. The content of the aluminum compound is preferably 100 ppm or less, more preferably 50 ppm or less. The higher the temperature, the more likely the aluminum compound is to precipitate. During operation of the inkjet recording device, the temperature inside the device may exceed 30°C, creating an environment in which precipitation is more likely than when stored at room temperature. By having the aluminum compound content of less than 400 ppm, the occurrence of precipitation is reduced, the stability of the ink is improved, and the occurrence of problems such as blocking of fine flow paths inside the components of the inkjet recording device and inhibition of stable liquid delivery due to precipitates is significantly reduced. The lower limit of the content of the aluminum compound in the water-insoluble colorant is, for example, 2 ppm. To reduce the content to less than 2 ppm requires considerable washing, which is not usually possible. The aluminum compound contained in the yellow colorant may be aluminum hydroxide.
[0014] In the specification and claims of this application, "water-insoluble" means that the solubility in 1 liter of water at 25°C is usually 5 g or less, preferably 3 g or less, more preferably 1 g or less, and even more preferably 0.5 g or less. The lower limit of the solubility includes 0 g. Hereinafter, unless otherwise specified, "water-insoluble colorant" is also simply referred to as "colorant".
[0015] As the colorant, for example, known organic pigments, inorganic pigments, disperse dyes, etc. can be used. The colorant is preferably a pigment.
[0016] Examples of organic pigments include various pigments such as azo, diazo, isoindolinone, perylene, thioindigo, anthraquinone, and quinophthalone. Specific examples of organic pigments include pigments such as CI Pigment Yellow 1, 2, 3, 12, 13, 14, 16, 17, 24, 55, 73, 74, 75, 83, 93, 94, 95, 97, 98, 108, 114, 128, 129, 138, 139, 150, 151, 154, 180, 185, 193, 199, 202, and 213. The organic pigment is preferably CI Pigment Yellow 74.
[0017] The inorganic pigment is preferably a body pigment. Examples of the body pigment include silica, calcium carbonate, talc, clay, barium sulfate, and white carbon. The body pigment is often used in combination with other colorants.
[0018] The disperse dye may be any known disperse dye. Among them, dyes selected from CI Dispers are preferred. Specific examples thereof include yellow disperse dyes such as CI Dispers Yellow 9, 23, 33, 42, 49, 54, 58, 60, 64, 66, 71, 76, 79, 83, 86, 90, 93, 99, 114, 116, 119, 122, 126, 149, 160, 163, 165, 180, 183, 186, 198, 200, 211, 224, 226, 227, 231, and 237.
[0019] The content of the colorant relative to the total mass of the yellow ink is usually 1 to 30%, preferably 1 to 10%, and more preferably 2 to 8%. Herein, in the specification and claims of the present application, "%" and "parts" are stated on a mass basis unless otherwise specified.
[0020] The average particle size of the colorant is usually 50 nm to 250 nm, preferably 60 nm to 200 nm. By setting the average particle size of the colorant within this range, it is possible to suppress the settling of the colorant over time. In the specification and claims of this application, the average particle size refers to the particle size at 50% of the integrated value in the particle size distribution determined by a laser diffraction / scattering method.
[0021] [Dispersant] In order to disperse the water-insoluble colorant in the ink, it is preferable to further include a dispersant in the yellow ink. The dispersant is not particularly limited, and a known dispersant can be used. As the dispersant, a polymer dispersant such as a resin is generally used. Examples of such resins include polymers derived from polyvinyl alcohol, cellulose derivatives, polyethylene oxide, polypropylene oxide, acrylic acid, methacrylic acid, crotonic acid, itaconic acid, itaconic acid monoester, maleic acid, maleic acid monoester, fumaric acid, fumaric acid monoester, vinyl sulfonic acid, sulfoethyl methacrylate, sulfopropyl methacrylate, α,β-unsaturated monomers of sulfonated vinyl naphthalene, styrene, styrene derivatives, vinyl naphthalene, vinyl naphthalene derivatives, aliphatic alcohol esters of α,β-ethylenically unsaturated carboxylic acids, acrylonitrile, vinylidene chloride, vinyl acetate, vinyl chloride, acrylamide, methacrylamide, hydroxyethyl methacrylate, hydroxypropyl methacrylate, glycidyl methacrylate, N-butoxymethyl acrylamide, and the like.
[0022] Examples of the resin as a dispersant include copolymers composed of at least two monomers (preferably at least one of which is a hydrophilic monomer) selected from the group consisting of monomers such as styrene and its derivatives, vinylnaphthalene and its derivatives, aliphatic alcohol esters of α,β-ethylenically unsaturated carboxylic acids, acrylic acid and its derivatives, maleic acid and its derivatives, itaconic acid and its derivatives, faric acid and its derivatives, vinyl acetate, vinyl alcohol, vinylpyrrolidone, acrylamide, and their derivatives. Examples of such copolymers include styrene-(meth)acrylic acid copolymers, styrene-(meth)acrylic acid-(meth)acrylic acid ester copolymers, (meth)acrylic acid ester-(meth)acrylic acid copolymers, polyethylene glycol (meth)acrylate-(meth)acrylic acid copolymers, and styrene-maleic acid copolymers. Among these, styrene-(meth)acrylic acid copolymer, styrene-(meth)acrylic acid-(meth)acrylic acid ester copolymer, (meth)acrylic acid ester-(meth)acrylic acid copolymer, polyethylene glycol (meth)acrylate-(meth)acrylic acid copolymer are preferred; styrene-(meth)acrylic acid copolymer, styrene-(meth)acrylic acid-(meth)acrylic acid ester copolymer, (meth)acrylic acid ester-(meth)acrylic acid copolymer are more preferred; (meth)acrylic acid ester-(meth)acrylic acid copolymer is even more preferred; and methacrylic acid ester-methacrylic acid copolymer is particularly preferred. In the present specification and claims, the term "(meth)acrylic acid" is used to mean both "acrylic acid" and "methacrylic acid." Similarly, "(meth)acrylate" means both methacrylate and acrylate. Examples of types of copolymers include block copolymers, random copolymers, and graft copolymers, and / or salts thereof.
[0023] The resin as the dispersant can be synthesized or obtained as a commercially available product. Specific examples of commercially available products include styrene-acrylic copolymers such as Joncryl 62, 67, 68, 678, and 687 (manufactured by BASF), Movinyl S-100A (modified vinyl acetate copolymer manufactured by Japan Coating Resins), and Julimer AT-210 (polyacrylic acid ester copolymer manufactured by Toa Gosei Co., Ltd.). Preferred examples of copolymers obtained by synthesis include the AB block polymers disclosed in International Publication No. WO 2013 / 115071.
[0024] The acid value of the dispersant is usually from 90 to 200 mgKOH / g, preferably from 100 to 150 mgKOH / g, and more preferably from 100 to 120 mgKOH / g. The mass average molecular weight of the dispersant is usually 10,000 to 60,000, preferably 10,000 to 40,000, more preferably 15,000 to 30,000, and further preferably 20,000 to 25,000. The PDI (mass average molecular weight / number average molecular weight) of the dispersant is about 1.29 to 1.49. By setting it in the above range, the dispersibility and storage stability of the ink can be improved.
[0025] The resin as a dispersant can be used in a state where it is mixed with the colorant, or in a state where a part or all of the surface of the colorant is coated with the resin as a dispersant, or both of these states can be used in combination.
[0026] [Surfactants] The yellow ink may further contain a surfactant for the purpose of adjusting the surface tension, etc. Examples of the surfactant include known surfactants such as anionic surfactants, cationic surfactants, nonionic surfactants, amphoteric surfactants, silicone-based surfactants, and fluorine-based surfactants.
[0027] Examples of anionic surfactants include alkyl sulfocarboxylates, α-olefin sulfonates, polyoxyethylene alkyl ether acetates, polyoxyethylene alkyl ether sulfates, N-acylamino acids or salts thereof, N-acylmethyltaurines, alkyl sulfates, polyoxyalkyl ether sulfates, alkyl sulfates, polyoxyethylene alkyl ether phosphates, rosin acid soaps, castor oil sulfates, lauryl alcohol sulfates, alkylphenol phosphates, alkyl phosphates, alkylaryl sulfonates, diethyl sulfosuccinates, diethylhexyl sulfosuccinates, and dioctyl sulfosuccinates. Specific examples of commercially available products include, for example, Hitenol TMLA-10, LA-12, LA-16, Neo Hitenol TMECL-30S, and ECL-45, all manufactured by Daiichi Kogyo Seiyaku Co., Ltd.
[0028] Examples of the cationic surfactant include 2-vinylpyridine derivatives and poly(4-vinylpyridine) derivatives.
[0029] Examples of nonionic surfactants include ether surfactants such as polyoxyethylene nonylphenyl ether, polyoxyethylene octylphenyl ether, polyoxyethylene dodecylphenyl ether, polyoxyethylene oleyl ether, polyoxyethylene lauryl ether, and polyoxyethylene alkyl ether; polyoxyethylene oleate, polyoxyethylene distearate, sorbitan laurate, sorbitan monostearate, sorbitan monooleate, sorbitan sesquioleate, and polyoxyethylene monooleate; Examples of such surfactants include esters such as polyoxyethylene stearate; acetylene glycol (alcohol)-based surfactants such as 2,4,7,9-tetramethyl-5-decyne-4,7-diol, 3,6-dimethyl-4-octyne-3,6-diol, and 3,5-dimethyl-1-hexyne-3-ol; Surfynol™ 104, 104PG50, 105PG50, 82, 420, 440, 465, and 485, all manufactured by Nissin Chemical Industry Co., Ltd.; Olfine™ TG; and polyglycol ether-based surfactants (e.g., TergItol™ 15-S-7 manufactured by SIGMA-ALDRICH).
[0030] Examples of amphoteric surfactants include lauryl dimethylaminoacetate betaine, 2-alkyl-N-carboxymethyl-N-hydroxyethyl imidazolinium betaine, coconut oil fatty acid amidopropyl dimethylaminoacetate betaine, polyoctyl polyaminoethyl glycine, and imidazoline derivatives.
[0031] Examples of silicone surfactants include polyether-modified siloxanes and polyether-modified polydimethylsiloxanes. Specific examples include BYK-306, BYK-307, BYK-333, BYK-341, BYK-345, BYK-346, BYK-347, BYK-348, BYK-349, and BYK-3455 (manufactured by BYK-Chemie), KF-351A, KF-352A, KF-353, KF-354L, KF-355A, KF-615A, KF-945, KF-640, KF-642, KF-643, KF-6020, X-22-4515, KF-6011, KF-6012, KF-6015, and KF-6017 (manufactured by Shin-Etsu Chemical Co., Ltd.).
[0032] Examples of fluorine-based surfactants include perfluoroalkylsulfonic acid compounds, perfluoroalkyl carboxylic acid compounds, perfluoroalkyl phosphate compounds, perfluoroalkyl ethylene oxide compounds, and polyoxyethylene ether polymer compounds having perfluoroalkyl ether groups on the side chains. Specific examples include Zonyl TBS, FSP, FSA, FSN-100, FSN, FSO-100, FSO, FS-300 (manufactured by DuPont); Capstone FS-30, FS-31, FS-3100 (Chemours); PF-151N, PF-154N (Omnova); F-114, F-410, F-444, EXP.TF-2066, EXP.TF-2148, EXP.TF-2149, F-430, F-477, F-552, F-553, F-554, F-555, F-556, F-5 57, F-558, F-559, F-561, F-562, R-40, R-41, RS-72-K, RS-75, RS-76-E, RS-76-NS, RS-77, EXP.TF-1540, EXP.TF-1760 (manufactured by DIC Corporation); BYK-340, BYK-3440, BYK-3441, etc. (manufactured by BYK-Chemie Japan).
[0033] Among the above, anionic, nonionic, silicone-based and fluorine-based surfactants are preferred. These surfactants may be used alone or in combination of two or more. When the ink contains surfactants, the total content of the surfactants is usually 0.1% by mass to 5% by mass, and preferably 0.1% by mass to 2% by mass, relative to the total mass of the ink.
[0034] [Ink preparations] The yellow ink may further contain ink preparation agents, such as binders, penetrants, viscosity adjusters, preservatives, antifungal agents, pH adjusters, chelating agents, rust inhibitors, water-soluble ultraviolet absorbers, and antioxidants. The total content of ink preparation agents excluding binders, penetrants, and viscosity modifiers is usually about 0 to 30%, preferably about 0.1 to 20%, and more preferably about 0.5 to 10%, based on the total mass of the ink.
[0035] (a) Binder The binder is preferably at least one selected from wax and (meth)acrylic acid-based polymers. By including a binder in the ink, the scratch resistance of the printed image can be improved. The binder is preferably included in the form of an emulsion, and among these, a water-based emulsion is more preferable. The average particle size of the binder is preferably 50 nm to 5 μm, and more preferably 100 nm to 1 μm, in order to prevent clogging of the inkjet head. When the ink contains a binder, the content of the binder relative to the total mass of the ink is usually 0.1 to 14%, preferably 0.5 to 12%, more preferably 2 to 10%, and even more preferably 3 to 8%, calculated as a solid content. At such a content, the scratch resistance of the printed image can be improved.
[0036] As the wax, natural wax and synthetic wax can be used. Examples of natural waxes include petroleum-based waxes such as paraffin wax and microcrystalline wax; lignite-based waxes such as montan wax; vegetable waxes such as carnauba wax and candelilla wax; and animal and vegetable waxes such as beeswax and lanolin, etc., dispersed in an aqueous medium. Examples of synthetic waxes include polyalkylene waxes (preferably poly C2-C4 alkylene waxes), oxidized polyalkylene waxes (preferably poly C2-C4 alkylene waxes), and paraffin waxes. Among the above, one or more waxes selected from polyethylene wax, polypropylene wax, oxidized polyethylene wax, oxidized polypropylene wax, and paraffin wax are preferred, and oxidized polyethylene wax is more preferred. Examples of commercially available wax emulsions include CERAFLOUR 925, 929, 950, and 991 manufactured by BYK-Chemie; AQUACER 498, 515, 526, 531, 537, 539, 552, and 1547; AQUAMAT 208, 263, and 272; and MINERPOL 221, manufactured by Mitsui Chemicals, Inc.; Mitsui Hiwax NL100, NL200, NL500, 4202E, 1105A, 2203A, NP550, NP055, and NP505, manufactured by Mitsui Chemicals, Inc.; and KUE-100 and 11, manufactured by Sanyo Chemical Co., Ltd. Among these, AQUACER 515, 531, 537, 539, and 1547 are preferred, and AQUACER 515, 531, 537, and 1547 are more preferred.
[0037] The (meth)acrylic acid-based polymer used as the binder is a polymer different from the dispersant. The (meth)acrylic acid-based polymer is preferably a (meth)acrylic acid-based polymer composed of four types of monomers, namely, C1-C4 alkyl methacrylate, C6-C10 alkyl acrylate, methacrylic acid, and allyl methacrylate. As the C1-C4 alkyl methacrylate, the alkyl moiety is preferably a straight chain or branched chain, more preferably a straight chain. The C1-C4 alkyl methacrylate is preferably a C1-C3 alkyl methacrylate, more preferably a C1-C2 alkyl methacrylate, and even more preferably methyl methacrylate. The C6-C10 alkyl acrylate preferably has an alkyl moiety that is linear or branched, more preferably branched. The C6-C10 alkyl acrylate is preferably a C7-C9 alkyl acrylate, more preferably a C8 alkyl acrylate, and even more preferably 2-ethylhexyl acrylate. The contents of the four monomers, C1-C4 alkyl methacrylate, C6-C10 alkyl acrylate, methacrylic acid, and allyl methacrylate, in the (meth)acrylic acid-based polymer are usually 40-60%, 38-58%, 1-10%, and 1-5%, respectively, on a mass basis, and preferably 45-55%, 52-42%, 2-4%, and 1-3%. It is preferable that the total of these monomer contents is 100%. The acid value (unit: mgKOH / g) of the (meth)acrylic acid-based polymer is usually from -10 to 35, preferably from -5 to 30, and more preferably from 0 to 25. The glass transition temperature (Tg) of the (meth)acrylic acid-based polymer is usually from -20 to 30°C, preferably from -15 to 25°C, and more preferably from -10 to 20°C.
[0038] (b) Penetrating agent The ink may further contain at least one organic solvent selected from glycol ether and C4-C9 alkanediol, each having a water-octanol partition coefficient of 0.00 or more and less than 2.00, as a penetrant, which tends to improve the wetting and spreading of the ink on non- or poorly ink-absorbing media, and the drying of the ink. Examples of penetrants having a Clog P within the above numerical range include 1,2-pentanediol (-0.00), ethylene glycol monoallyl ether (0.03), isopropyl alcohol (0.07), isopropyl glycol (0.09), diethylene glycol ethyl methyl ether (0.13), dipropylene glycol dimethyl ether (0.36), 3-methoxy-3-methyl-1-butanol (0.42), butyl triglycol (0.49), diethylene glycol diethyl ether (0.52), 1,2-hexanediol (0.53), diethylene glycol monoisobutyl ether (0.54), propyl propylene glycol (0.62), butyl diglycol (0.67), dipropylene glycol n-propyl ether (0.75), 2,2-diethyl-1,3-propanediol (0.82), 2,2,4-trimethyl-1,3-pentanediol (1.00), 2-ethyl-1,3-hexanediol (1.26), 1,2-octanediol (1.58), and hexyl diglycol (1.72). When the ink contains a penetrant, the total content of the penetrant in the total mass of the ink is usually 0.1 to 30%, preferably 0.2 to 20%, and more preferably 0.5 to 10%.
[0039] (c) Viscosity modifier The ink may further contain a viscosity modifier. Industrial inkjet printers usually have a set viscosity range for ink that can be ejected based on the specifications of the printer head (the head that ejects the ink) that is installed in the printer. For this reason, a viscosity modifier can be added to the ink to adjust the viscosity to an appropriate range. The viscosity adjuster is not particularly limited as long as it is a substance that can adjust the viscosity of the ink, and known substances can be used. Specific examples thereof include water-soluble organic solvents (which do not include the "organic solvents" listed as the penetrants above), sugars, and the like. Among these, water-soluble organic solvents having a ClogP value usually less than 0.00, preferably -0.05 or less, and more preferably -0.08 or less can be used. The lower limit of the ClogP value of the water-soluble organic solvent is not particularly limited, but is usually -4.00 or more, preferably -3.00 or more, more preferably -2.00 or more, and even more preferably -1.50 or more. Examples of such water-soluble organic solvents include 2-methyl-2,4-pentanediol (-0.02), tripropylene glycol monomethyl ether (-0.03), isopropyl diglycol (-0.08), dipropylene glycol monomethyl ether (-0.16), ethanol (-0.24), 3-methyl-1,5-pentanediol (-0.24), diethylene glycol dimethyl ether (-0.26), propylene glycol monomethyl ether (-0.30), 3-methyl-1,3-butanediol (-0.33), trimethylolpropane (-0.39), N-methyl-2-pyrrolidone (-0.40), 1,2-butanediol (-0.53), 3-ethyl-3-hydroxymethyl ether (-0.53), 1,2-butanediol (-0.53), 1,2-butanediol (-0.53), 1,2-butanediol (-0.53), 1,3 ... Examples of these include ethyl oxetane (-0.58), 1,5-pentanediol (-0.64), 2-methyl-1,3-propanediol (-0.64), dipropylene glycol (-0.69), 1,3-butanediol (-0.73), methyl diglycol (-0.78), methyl triglycol (-0.96), 2-pyrrolidone (-0.97), propylene glycol (-1.06), 1,4-butanediol (-1.16), diethylene glycol (-1.30), ethylene glycol (-1.37), triethylene glycol (-1.48), glycerin (-1.54), diglycerin (-2.96), Aoki Oil Industry's glycereth-3 (-3.49), and glycereth-20 (-5.42). When the ink contains a water-soluble organic solvent, the total content of the water-soluble organic solvent is usually about 0% to 55%, preferably about 1% to 40%, and more preferably about 2% to 30%.
[0040] (d) Preservatives Examples of preservatives include organic sulfur compounds, organic nitrogen sulfur compounds, organic halogen compounds, haloarylsulfone compounds, iodopropargyl compounds, haloalkylthio compounds, nitrile compounds, pyridine compounds, 8-oxyquinoline compounds, benzothiazole compounds, isothiazolin compounds, dithiols, pyridine oxide compounds, nitropropane compounds, organic tin compounds, phenol compounds, quaternary ammonium salt compounds, triazine compounds, thiazine compounds, anilides, adamantane compounds, dithiocarbamate compounds, brominated indanone compounds, benzyl bromoacetate compounds, and inorganic salt compounds. Specific examples of commercially available preservatives include Proxel GXL(S) and XL-2(S) manufactured by Arch Chemicals.
[0041] (e) Antifungal agents Antifungal agents include sodium dehydroacetate, sodium benzoate, sodium pyridinethione-1-oxide, p-hydroxybenzoic acid ethyl ester, and 1,2-benzisothiazolin-3-one and salts thereof.
[0042] (f) pH adjuster Any substance can be used as the pH adjuster as long as it does not adversely affect the prepared ink and can adjust the pH to 5 to 11. Specific examples of the pH adjuster include alkanolamines such as diethanolamine, triethanolamine, and N-methyldiethanolamine; alkali metal hydroxides such as lithium hydroxide, sodium hydroxide, and potassium hydroxide; ammonium hydroxide (aqueous ammonia); alkali metal carbonates such as lithium carbonate, sodium carbonate, sodium hydrogen carbonate, and potassium carbonate; alkali metal salts of organic acids such as sodium silicate and potassium acetate; and inorganic bases such as disodium phosphate.
[0043] (g) Chelating agents Examples of chelating agents include disodium ethylenediaminetetraacetate, sodium nitrilotriacetate, sodium hydroxyethylethylenediaminetriacetate, sodium diethylenetriaminepentaacetate, and sodium uracildiacetate.
[0044] (h) Rust inhibitors Examples of the rust inhibitor include acid sulfite, sodium thiosulfate, ammonium thioglycolate, diisopropylammonium nitrite, pentaerythritol tetranitrate, and dicyclohexylammonium nitrite.
[0045] (i) Water-soluble ultraviolet absorbers Examples of the water-soluble ultraviolet absorber include sulfonated benzophenone compounds, benzotriazole compounds, salicylic acid compounds, cinnamic acid compounds, and triazine compounds.
[0046] (j) Antioxidants Examples of the antioxidant include various organic and metal complex-based anti-fading agents. Examples of the organic anti-fading agents include hydroquinones, alkoxyphenols, dialkoxyphenols, phenols, anilines, amines, indanes, chromans, alkoxyanilines, and heterocycles.
[0047] The yellow ink preferably does not contain any component containing an aluminum compound other than the water-insoluble colorant.
[0048] [water] The ink contains the above-mentioned components, with the remainder being water. The water used in the ink is preferably ion-exchanged water, distilled water, or the like, which has a low content of impurities such as metal ions. The content of water in the total mass of the ink is preferably 40% or more, more preferably 50 to 95%, and particularly preferably 60 to 90%.
[0049] The ink can be prepared by preparing a dispersion containing a water-insoluble colorant and a dispersant, and then mixing it with other components. A known method can be used to prepare the dispersion. One example is the phase inversion emulsification method. That is, a resin as a dispersant is dissolved in an organic solvent such as 2-butanone, and an aqueous solution of a neutralizing agent is added to prepare an emulsion. A water-insoluble colorant is added to the obtained emulsion, and a dispersion treatment is performed. The organic solvent and a part of the water are distilled off under reduced pressure from the liquid obtained in this manner, to obtain the desired dispersion. Dispersion treatment can be carried out using, for example, a sand mill (bead mill), a roll mill, a ball mill, a paint shaker, an ultrasonic disperser, a microfluidizer, etc. As an example, when using a sand mill, beads with a particle diameter of about 0.01 mm to 1 mm are used, and the bead packing rate can be appropriately set to carry out dispersion treatment. If foaming occurs during preparation of the dispersion liquid, a very small amount of a known silicone-based, acetylene glycol-based, or other defoaming agent can be added.
[0050] Methods for preparing a dispersion liquid other than the phase inversion emulsification method include an acid precipitation method, an interfacial polymerization method, an in-situ polymerization method, a liquid hardening coating method, a coacervation (phase separation) method, a liquid drying method, a melt dispersion cooling method, an air suspension coating method, and a spray drying method, etc. Among these, the acid precipitation method and the interfacial polymerization method are preferred.
[0051] The obtained dispersion liquid may be subjected to a procedure such as filtration and / or centrifugation, etc. By this procedure, the particle diameter of the particles contained in the dispersion liquid can be made uniform.
[0052] The average particle size (D50) of the colorant dispersion in the dispersion is usually 300 nm or less, preferably 30 to 280 nm, more preferably 40 to 270 nm, and even more preferably 50 to 250 nm. D90 is usually 400 nm or less, preferably 350 nm or less, and more preferably 300 nm or less. The lower limit is preferably 100 nm. D10 is usually 10 nm or more, preferably 20 nm or more, more preferably 30 nm or more, and the upper limit is 100 nm. By ensuring the ink storage stability by having the particle size of the colorant in the dispersion within the above range, the ink can be stably discharged without clogging the inkjet head nozzle. Here, the average particle size (D50) is the particle size at which the cumulative particle size distribution from the small particle size side in the particle size distribution obtained by the laser diffraction / scattering method is 50%, D10 is the particle size at which the cumulative particle size distribution from the small particle size side is 10%, and D90 is the particle size at which the cumulative particle size distribution from the small particle size side is 90%.
[0053] The dispersion liquid, water, and other components are mixed by adding each component to a container and then stirring.
[0054] When the dispersion liquid and water are mixed, it is preferable to add a neutralizing agent. Examples of the neutralizing agent used to dissolve the dispersion liquid of the colorant prepared using the block copolymer as a dispersant in water include ammonia, hydroxides of alkali metals, hydroxides of alkaline earth metals, aliphatic amine compounds, and alkanolamine compounds. Ammonia and hydroxides of alkali metals are preferable, and ammonia is particularly preferable. The amount of the neutralizing agent used is not particularly limited. As a guideline, the neutralization degree is usually 30 to 300%, more preferably 50 to 200%, with the neutralization degree being 100% when neutralized with the theoretical equivalent of the acid value of the dispersant.
[0055] The pH of the ink is usually 7 to 11, and preferably 8 to 10. The surface tension of the ink is usually 10 to 50 mN / m, and preferably 20 to 40 mN / m. The viscosity of the ink composition is usually 2 to 30 mPa·s, and preferably 3 to 20 mPa·s. The pH and surface tension of the ink can be adjusted by using a pH adjuster, a surfactant, a water-soluble organic solvent, and the like.
[0056] The ink can be used in various printing applications, for example, writing instruments, various printing applications, information printing, textile printing, etc., and is particularly preferably used in inkjet printing.
[0057] The ink has the effect of significantly reducing sedimentation of the water-insoluble colorant and exhibiting excellent storage stability. By performing an ink-jet recording method using the ink in an ink-jet recording apparatus, it is possible to significantly reduce the problems of clogging of the ink-jet head nozzles and of the accumulation of the colorant in the internal structure of the head, including the circulation mechanism, causing ejection defects.
[0058] <Inkjet recording method> An inkjet recording method according to the present invention is an inkjet recording method for recording by an inkjet recording apparatus using the above yellow ink, and includes a discharge step of discharging the yellow ink from a discharge head onto a recording medium for recording.
[0059] The ejection process is a process of ejecting the yellow ink onto the recording medium by the ejection head and recording on the recording medium. An ejection head of the inkjet system is used to eject the yellow ink. As the inkjet system, a known system can be used, for example, a charge control system, a drop-on-demand (pressure pulse) system, an acoustic inkjet system, a thermal inkjet system, etc. are included. In addition, the inkjet system also includes a system of ejecting a large number of inks with a small content of colorant in the ink in a small volume to improve image quality, a system of using multiple inks with substantially the same hue but different concentrations of colorant in the ink to improve image quality, and a system of using colorless and transparent ink to improve fixability of the colorant.
[0060] As the inkjet recording device used in the inkjet recording method, a general inkjet recording device can be used as long as it has an inkjet type ejection head. The inkjet recording device has a configuration including at least a container for storing ink, and an ejection head that receives ink from the container through a supply path and ejects the ink toward a recording medium.
[0061] The inkjet recording apparatus preferably further comprises a circulation mechanism for circulating the ink between a container for storing the ink and the ejection head or within the ejection head, and the inkjet recording method preferably further comprises a circulation step for circulating the ink by the circulation mechanism before the ink is subjected to the ejection step. The circulation step by the circulation mechanism can prevent clogging of the ink in the ejection head and drying of the ink in the nozzles. The circulation mechanism preferably comprises a circulation flow path connecting the container for storing the ink and the ejection head, and a circulation pump provided in the circulation flow path.
[0062] By using the above yellow ink in an inkjet recording method, the occurrence of precipitation is suppressed or significantly reduced, and problems such as clogging of the ink flow path inside the inkjet recording device and the ejection head are unlikely to occur. When the inkjet recording device is equipped with a circulation mechanism, there is a risk of problems such as clogging or inhibition of stable liquid transfer due to gradual accumulation of sediment generated from the yellow ink, but in the present disclosure, since the water-insoluble colorant contained in the yellow ink contains less than 400 ppm of an aluminum compound, the occurrence of precipitation is suppressed or significantly reduced even when the yellow ink is circulated, and problems such as clogging of the circulation path or inhibition of stable liquid transfer are unlikely to occur.
[0063] <Recording media set> The recording media set is a set including the yellow ink and the recording media. The recording media refers to a material to which the ink can be attached. Examples of print media include paper, film, fibers and cloth (cellulose, nylon, wool, etc.), leather, and color filter substrates.
[0064] Recording media can be broadly divided into those with and without an ink-receiving layer. The ink described above can be applied to any printing media, but is preferably used for printing media without an ink-receiving layer.
[0065] Recording media having an ink-receiving layer are usually called inkjet paper, inkjet film, glossy paper, etc. Representative examples of commercially available products include Professional Photo Paper, Super Photo Paper, Gloss Gold, and Matte Photo Paper manufactured by Canon Inc.; Photo Paper Crispia (high gloss), Photo Paper (gloss), and Photo Matte Paper manufactured by Seiko Epson Corporation; Advanced Photo Paper (gloss) manufactured by Hewlett-Packard Japan, Ltd.; and Gasai Photo Finishing Pro manufactured by Fujifilm Corporation.
[0066] Examples of printing media that do not have an ink-receiving layer include various papers such as coated paper and art paper used in applications such as gravure printing and offset printing; and cast-coated paper used in label printing. When using a recording medium that does not have an ink-receiving layer, it is also preferable to subject the recording medium to a surface modification treatment in order to improve the fixation of the colorant. Examples of surface modification treatments include known methods such as corona discharge treatment, plasma treatment, and frame treatment.
[0067] For all of the above items, combinations of preferred items are more preferred, and combinations of more preferred items are even more preferred. The same applies to combinations of preferred items and more preferred items, combinations of more preferred items and even more preferred items, etc. Moreover, unless otherwise specified, all of the above-mentioned components can be used alone or in combination of two or more kinds. EXAMPLES
[0068] The present invention will be described in detail below with reference to examples. The present invention is not limited to the following examples. In the examples, when it was necessary to measure the content (solid content) of colorant contained in various liquids, it was calculated as a converted value of only the colorant by the dry weight method using a heat-dry type moisture meter (MS-70, manufactured by A&D Co., Ltd.).
[0069] [Preparation Example 1: Preparation of Yellow Dispersion 1] The block copolymer described in Synthesis Example 3 of WO 2013 / 115071 was prepared, and the obtained block copolymer (6 parts) was dissolved in 20 parts of methyl ethyl ketone to obtain a homogeneous solution. A mixed solution of sodium hydroxide (0.45 parts) dissolved in water (53.55 parts) was added to this liquid, and then 20 parts of Pigment Yellow 74 (containing 13 ppm of aluminum compound) with an aluminum compound content of less than 400 ppm was added, and dispersion treatment was performed in a sand grinder under conditions of 1500 rpm for 15 hours to obtain a liquid. Water (100 parts) was added to the obtained liquid, and the liquid was filtered using glass filter paper GA-100 to remove aggregates and the like, and a filtrate was obtained. The obtained filtrate was subjected to reduced pressure distillation of the methyl ethyl ketone and a part of the water in the filtrate using an evaporator, and the pigment content in the filtrate was adjusted to 12.0%, thereby obtaining a yellow dispersion liquid 1. The water content of the yellow dispersion liquid 1 was 84.1%.
[0070] [Preparation Example 2: Preparation of Yellow Dispersion 2] Yellow Dispersion 2 having a pigment content of 12.0% was obtained by the same procedure as in Preparation Example 1, except that Pigment Yellow 74 having an aluminum compound content of 400 ppm or more (containing 400 ppm of aluminum compound) was used instead of Pigment Yellow 74 having an aluminum compound content of less than 400 ppm used in Preparation Example 1. The water content of Yellow Dispersion 2 was 84.1%.
[0071] [Preparation Example 3: Preparation of Resin 1] A resin emulsion having an acid value of 6 KOHmg / g and a solid content of 25% was prepared by following Preparation Example 4 of WO 2015 / 147192. This is designated Resin 1.
[0072] [Example 1 and Comparative Example 1: Preparation of ink composition] The components shown in Table 1 below were mixed and then filtered through a 3 μm membrane filter to obtain inks for evaluation tests.
[0073] [Evaluation of subsidence]
[0074] Each ink of Example 1 and Comparative Example 1 was placed in a sealed container to prepare a test sample, which was then left to stand for 3 days in a thermo-hygrostat at 70°C and then evaluated according to the following two-stage criteria. This corresponds to an accelerated test that assumes that the ink is placed at the temperature (approximately 30 to 35°C) of an ink storage container, ink flow paths such as circulation paths, and ejection head inside an inkjet printing device. [Evaluation Criteria Table] No settling occurs × Settlement occurs
[0075] As shown in Table 1, the ink of Example 1 did not undergo sedimentation and was excellent in storage stability. On the other hand, the ink of Comparative Example 1 underwent sedimentation and was poor in storage stability. This shows that when inkjet printing is performed using an inkjet printing device using the ink of Example 1, the occurrence of sedimentation is suppressed or significantly reduced, clogging of the circulation path is unlikely to occur, and there is a low risk of problems such as ejection defects occurring.
[0076] [Table 1]
[0077] The abbreviations in Table 1 represent the following: PG: Propylene glycol. 1,2HD: 1,2-hexanediol. TEA: Triethanolamine. Resin 1: Resin emulsion obtained in Preparation Example 3. DW: Ion-exchanged water. [Industrial Applicability]
[0078] According to the present invention, it is possible to provide an ink that can significantly reduce sedimentation of a water-insoluble colorant due to storage, and an ink-jet recording method and a print media set using the ink. The ink, ink-jet recording method and print media set are extremely useful for various printing applications, particularly ink-jet printing applications.
Claims
1. An inkjet recording method for recording with a yellow ink by an inkjet recording apparatus, comprising the steps of: An inkjet recording method comprising a discharge step of discharging the yellow ink onto a recording medium by a discharge head for recording, the yellow ink containing a water-insoluble colorant, the insoluble colorant containing less than 400 ppm of an aluminum compound.
2. 2. The ink-jet recording method according to claim 1, wherein the water-insoluble colorant is CI Pigment Yellow 74.
3. 2. The ink-jet recording method according to claim 1, wherein the aluminum compound is entirely or partly aluminum hydroxide.
4. 2. The inkjet recording method according to claim 1, wherein the inkjet recording apparatus comprises a circulation mechanism that circulates the yellow ink between a container that stores yellow ink and the ejection head, or within the ejection head, and the inkjet recording method further comprises a circulation step of circulating the yellow ink by the circulation mechanism before being subjected to the ejection step.
5. 2. The ink jet recording method according to claim 1, wherein the recording medium is a recording medium that is poorly ink-absorbent or non-ink-absorbent.
6. A yellow ink for ink-jet recording, comprising a water-insoluble colorant, the water-insoluble colorant containing less than 400 ppm of an aluminum compound.
7. A recording media set comprising the yellow ink according to claim 6 and a recording medium.
Citation Information
Patent Citations
Ink discharge device and ink discharge method
JP2018075751A