Solid electrolyte composite

The solid electrolyte composite with a stepped shape and varying filler content addresses the challenge of achieving both energy density and structural strength in solid-state batteries by ensuring a reaction area and maintaining ionic conductivity.

JP2024145939APending Publication Date: 2024-10-15HONDA MOTOR CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023058556
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing solid-state batteries face challenges in achieving both high energy density and structural strength, particularly due to the need for thin solid electrolytes that can withstand confining pressure and prevent internal short circuits.

Method used

A solid electrolyte composite with a stepped shape is introduced, featuring a higher content of filler and/or porous base material in the negative electrode side layer, which includes a filler and/or porous base material, and a lower content near the interface with other layers, ensuring a reaction area and improved bondability while maintaining ionic conductivity.

Benefits of technology

The solution enhances both the energy density and structural strength of the solid battery by ensuring a reaction area and reducing ionic conductivity loss, while also improving the bondability between electrode layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024145939000001_ABST
    Figure 2024145939000001_ABST
Patent Text Reader

Abstract

To provide a solid electrolyte composite that can achieve both the energy density and strength of a solid-state battery.SOLUTION: In a solid-state battery, a solid electrolyte composite is disposed between a positive electrode layer and a negative electrode layer, and includes a positive electrode-side solid electrolyte layer disposed on the positive electrode layer side and a negative electrode-side solid electrolyte layer disposed on the negative electrode layer side, and the positive electrode-side solid electrolyte layer and the negative electrode-side solid electrolyte layer have a stepped shape with a step between them, and at least the negative electrode-side solid electrolyte layer contains a filler and / or a porous substrate, and the content of the filler and / or the porous substrate in the negative electrode-side solid electrolyte layer is higher than the content of the filler and / or the porous substrate in the positive electrode-side solid electrolyte layer.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a solid electrolyte composite. [Background technology]

[0002] In recent years, research and development into secondary batteries that contribute to energy efficiency has been conducted in order to ensure that more people have access to affordable, reliable, sustainable and advanced energy.

[0003] As a secondary battery, a solid-state battery having a solid electrolyte is known. As a technology related to a solid-state battery, a technology related to a solid electrolyte laminate has been disclosed, which has a multilayer structure in which a first low-insulator-containing solid electrolyte layer, a high-insulator-containing solid electrolyte layer, and a second low-insulator-containing solid electrolyte layer are laminated in this order, and the insulator content of each of the first and second low-insulator-containing solid electrolyte layers is smaller than the insulator content of the high-insulator-containing solid electrolyte layer (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2019-185877 A Summary of the Invention [Problem to be solved by the invention]

[0005] The technology disclosed in Patent Document 1 aims to suppress internal short circuits and suppress the decrease in discharge capacity by incorporating an insulator such as alumina into the solid electrolyte. On the other hand, the solid electrolyte needs to be thin in consideration of the energy density, and needs to be strong enough to withstand high confining pressure. However, detailed consideration has not been given to the configuration of a solid-state battery that can achieve both energy density and strength.

[0006] The present invention has been made in view of the above, and has an object to provide a solid electrolyte composite that can achieve both energy density and strength for a solid-state battery. [Means for solving the problem]

[0007] (1) The present invention relates to a solid electrolyte composite disposed between a positive electrode layer and a negative electrode layer in a solid-state battery, the solid electrolyte composite having a positive electrode-side solid electrolyte layer disposed on the positive electrode layer side and an anode-side solid electrolyte layer disposed on the anode layer side, the solid electrolyte composite having a stepped shape with a step between the positive electrode-side solid electrolyte layer and the anode-side solid electrolyte layer, at least the anode-side solid electrolyte layer containing a filler and / or a porous substrate, and a content of the filler and / or the porous substrate in the anode-side solid electrolyte layer being higher than a content of the filler and / or the porous substrate in the cathode-side solid electrolyte layer.

[0008] According to the invention of (1), it is possible to provide a solid electrolyte composite that can achieve both the energy density and strength of a solid-state battery.

[0009] (2) The solid electrolyte composite according to (1), wherein the anode-side solid electrolyte layer has a lower content of the filler and / or the porous substrate near the interface on the anode layer side and near the interface on the cathode-side solid electrolyte layer side than other locations, and the cathode-side solid electrolyte layer has a lower content of the filler and / or the porous substrate near the interface on the cathode layer side and near the interface on the anode-side solid electrolyte layer side than other locations.

[0010] According to the invention of (2), a reaction area is ensured at the interface between the positive electrode side solid electrolyte layer and the negative electrode side solid electrolyte layer and other layers, and a decrease in ion conductivity is suppressed. Also, the bonding between the positive electrode side solid electrolyte layer and the negative electrode side solid electrolyte layer and other layers can be improved. Furthermore, the total amount of the filler and / or the porous substrate is reduced to suppress a decrease in ion conductivity, thereby improving the output of the solid-state battery and maintaining the necessary strength.

[0011] (3) The solid state battery further includes an insulating member, and the positive electrode-side solid electrolyte layer and the negative electrode-side solid electrolyte layer each have a lower content of the filler and / or the porous substrate near an interface with the insulating member than at other portions.

[0012] According to the invention of (3), it is possible to more preferably achieve both energy density and strength of the solid-state battery.

[0013] (4) The solid electrolyte composite according to any one of (1) to (3), wherein a filler-rich region is provided inside the solid electrolyte composite, in which a content of the filler and / or porous substrate is higher than other portions, and the filler-rich region has a stepped shape having a step between the positive electrode-side solid electrolyte layer side and the negative electrode-side solid electrolyte layer side.

[0014] According to the invention of (4), when the θ deviation during stacking is suppressed by the stepped shape of the solid electrolyte composite, the solid electrolyte composite can have a strength sufficient to withstand an impact during stacking, and the shape of the solid electrolyte composite can be maintained. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a top view showing a solid-state battery according to a first embodiment. [Diagram 2] 2 is a cross-sectional view taken along line AA in FIG. 1. [Diagram 3] FIG. 2 is a cross-sectional view taken along line BB in FIG. [Figure 4] FIG. 4 is a cross-sectional view that typically illustrates the solid electrolyte composite in FIG. [Diagram 5] 5 is a cross-sectional view of a solid electrolyte composite according to a second embodiment, corresponding to FIG. 3. FIG. [Figure 6] 7 is a cross-sectional view of a solid electrolyte composite according to a third embodiment, corresponding to FIG. 3. FIG. [Figure 7] 10 is a cross-sectional view corresponding to FIG. 3 of a solid electrolyte composite according to a fourth embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] <Solid battery> 1 to 3, in solid-state battery 1, solid electrolyte composite 40 according to this embodiment is disposed by being laminated between a negative electrode layer made of a negative electrode mixture layer 21 and a negative electrode current collector 22, and a positive electrode layer made of a positive electrode mixture layer 31 and a positive electrode current collector 32. In this embodiment, solid-state battery 1 further includes intermediate layer 50, and insulating frame 61 and insulating layer 62 as insulating members.

[0017] The solid-state battery 1 is not particularly limited as long as it is a solid-state battery having a solid electrolyte, but is preferably, for example, an all-solid-state lithium metal battery using lithium metal or a lithium alloy for the negative electrode, or an all-solid-state lithium ion battery using silicon or tin for the negative electrode. This is because the above-mentioned solid-state batteries undergo relatively large expansion and contraction due to charging and discharging, and are constrained under high constraining pressure, so that the solid electrolyte layer (laminate) is required to have high strength.

[0018] <Solid electrolyte complex> First Embodiment As shown in FIGS. 2 and 3, the solid electrolyte composite 40 according to this embodiment is formed by laminating a cathode-side solid electrolyte layer 41 arranged on the cathode layer side and an anode-side solid electrolyte layer 42 arranged on the anode layer side.

[0019] The positive electrode solid electrolyte layer 41 and the negative electrode solid electrolyte layer 42 each essentially contain a solid electrolyte. The solid electrolyte is not particularly limited as long as it is a material capable of conducting lithium ions, and examples of the solid electrolyte include oxide-based electrolytes and sulfide-based electrolytes.

[0020] As shown in Figs. 2 to 4, the positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42 have a stepped shape with a step between them. The above configuration can suppress θ misalignment during stacking. In this embodiment, in a direction (direction Y in each figure) perpendicular to the current collector extension direction (direction X in each figure) and stacking direction (direction Z in each figure), the length L1 of the positive electrode side solid electrolyte layer 41 in the direction Y is shorter than the length L2 of the negative electrode side solid electrolyte layer 42 in the direction Y. The ratio of the lengths L1 and L2 is not particularly limited, but can be, for example, L1:L2 = 1:1.001 to 1:2.

[0021] The anode-side solid electrolyte layer 42 includes a filler and / or a porous substrate. As shown in FIG. 2, the anode-side solid electrolyte layer 42 is disposed so as to abut against the insulating frame 61 in the stacking direction Z and to partially cover the intermediate layer 50. An end of the anode-side solid electrolyte layer 42 in the current collector extending direction (direction X in FIG. 2) extends outward from the center of the solid battery 1 beyond the insulating frame 61. In order to tolerate a certain degree of reaction non-uniformity when the anode layer expands and contracts and to maintain the electrode structure, the anode-side solid electrolyte layer 42 having the above configuration is required to have high strength. In addition, in the manufacturing process of the solid battery 1, the anode-side solid electrolyte layer 42 and the anode layer, and the cathode-side solid electrolyte layer 41 and the cathode layer may be formed and joined, respectively, and at this time, the anode-side solid electrolyte layer 42 and the anode layer have a smaller thickness in the stacking direction (direction Z in FIG. 2) than the cathode-side solid electrolyte layer 41 and the cathode layer. Therefore, in order to improve the handleability of the negative electrode solid electrolyte layer 42 and the negative electrode layer, the negative electrode solid electrolyte layer 42 is required to have high strength.

[0022] The inclusion of the filler and / or the porous substrate in the negative electrode solid electrolyte layer 42 provides toughness and improves strength against external pressure. In addition, the energy density of the solid battery 1 can be improved, for example, compared to a case where a SUS plate or a nonwoven fabric having a predetermined size or more is used for the negative electrode solid electrolyte layer 42. The filler is not particularly limited, but examples thereof include organic fillers and inorganic fillers such as polyethylene terephthalate (PET), polyamide, polyimide, and polycarbonate. The filler may be fibrous, particulate, or bulk. The porous substrate is a substrate having voids formed therein, and the voids are impregnated with a solid electrolyte. Examples of the porous substrate include nonwoven fabric, woven fabric, organic porous body, and inorganic porous body. Examples of the shape of the organic porous body and the inorganic porous body include a mesh body, an embossed body, a punched body, an expanded body, and a foam body. The porous substrate may have a predetermined shape or may be chopped. Both the filler and the porous substrate have electronic insulation properties.

[0023] The content of the filler and / or porous substrate in the negative electrode solid electrolyte layer 42 is not particularly limited, but can be, for example, more than 0 mass % and 50 mass % or less.

[0024] The positive electrode-side solid electrolyte layer 41 may also contain the filler and / or porous substrate. In consideration of the energy density of the solid battery 1, the thickness of the solid electrolyte composite 40 in the stacking direction Z needs to be thin, and the positive electrode-side solid electrolyte layer 41 is also required to have a certain degree of strength according to the thickness. However, the content of the filler and / or porous substrate is higher in the negative electrode-side solid electrolyte layer 42, which is required to have a higher strength, than in the positive electrode-side solid electrolyte layer 41. Hereinafter, a configuration in which the positive electrode-side solid electrolyte layer 41 contains a predetermined amount of the filler and / or porous substrate will be described, but the positive electrode-side solid electrolyte layer 41 may not contain the filler and / or porous substrate.

[0025] The positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42 preferably have a lower content of filler and / or porous substrate near the interface with other layers than other portions. This ensures a reaction area at the interface between the positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42 and other layers, and suppresses a decrease in ion conductivity. In addition, the bonding between the positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42 and other layers can be improved. In addition, the total amount of filler and / or porous substrate can be reduced, improving the energy density of the solid battery 1 and maintaining the necessary strength.

[0026] The interface of the positive electrode side solid electrolyte layer 41 with the other layers means the interface between the positive electrode side solid electrolyte layer 41 and the positive electrode mixture layer 31, and the interface between the positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42.

[0027] The interface of the anode-side solid electrolyte layer 42 with the other layers means the interface between the anode-side solid electrolyte layer 42 and the intermediate layer 50, and the interface between the anode-side solid electrolyte layer 42 and the cathode-side solid electrolyte layer 41.

[0028] In addition to the above, the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 preferably have a lower content of filler and / or porous substrate at the interface with the insulating frame 61 and the insulating layer 62 as insulating members than at other locations.

[0029] A solid electrolyte for bonding may be applied to the interface between the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42. This can improve the bonding between the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42.

[0030] Specific examples of the positive electrode side solid electrolyte layer 41 and the negative electrode side solid electrolyte layer 42 having the above-mentioned filler and / or porous substrate content include the embodiment shown in FIG. 4. In FIG. 4, the positive electrode side solid electrolyte layer 41 is composed of solid electrolyte layers 411, 412, and 413. The solid electrolyte layers 411 and 413 are layers having a lower filler and / or porous substrate content than the solid electrolyte layer 412. Similarly, the negative electrode side solid electrolyte layer 42 is composed of solid electrolyte layers 421, 422, and 423. The solid electrolyte layers 421 and 423 are layers having a lower filler and / or porous substrate content than the solid electrolyte layer 422. Each of the above layers can be formed by stacking layers having different filler and / or porous substrate contents.

[0031] When the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 each have a plurality of layers having different filler and / or porous substrate contents, the filler and / or porous substrate contents of the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 refer to the average filler and / or porous substrate contents of each layer.

[0032] (Negative electrode layer) The negative electrode mixture layer 21 essentially contains a negative electrode active material, and may further contain a solid electrolyte, a conductive assistant, a binder, and the like. The negative electrode active material is not particularly limited as long as it is capable of absorbing and releasing lithium ions, and examples thereof include metallic lithium, lithium alloys, metal oxides, metal sulfides, metal nitrides, Si, SiO, and carbon materials. Examples of carbon materials include artificial graphite, natural graphite, hard carbon, and soft carbon.

[0033] The negative electrode current collector 22 is not particularly limited, and examples thereof include metal foils such as copper (Cu) foil and stainless steel (SUS) foil.

[0034] (Positive electrode layer) The positive electrode mixture layer 31 essentially contains a positive electrode active material, and may further contain a solid electrolyte, a conductive assistant, a binder, etc. The positive electrode active material is not particularly limited, and examples thereof include LiCoO2, Li(Ni5 / 10 Co 2 / 10 Mn 3 / 10 )O 2、 Li(Ni) 6 / 10 Co 2 / 10 Mn 2 / 10 )O 2、 Li(Ni) 8 / 10 Co 1 / 10 Mn 1 / 10 )O 2、 Li(Ni) 0.8 Co 0.15 Al 0.05 )O 2、 Li(Ni) 1 / 6 Co 4 / 6 Mn 1 / 6 )O 2、 Li(Ni) 1 / 3 Co 1 / 3 Mn 1 / 3 )O 2、 Examples of the positive electrode composite layer 31 include LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, sulfur, etc. In this embodiment, the positive electrode composite layer 31 is laminated on both sides of the positive electrode current collector 32.

[0035] The positive electrode current collector 32 is not particularly limited, and examples thereof include aluminum (Al) foil, stainless steel (SUS) foil, and the like.

[0036] (Middle class) For example, when the solid-state battery 1 is a lithium metal secondary battery, the intermediate layer 50 has a function of uniformly precipitating Li metal. This stabilizes the interface between the intermediate layer 50 and the negative electrode solid electrolyte layer 42. The material constituting the intermediate layer 50 is not particularly limited, and examples thereof include carbon carrying a metal (e.g., Ag, etc.) capable of being alloyed with Li. Here, the lithium metal secondary battery may be an anode-free battery in which the negative electrode mixture layer 21 does not exist during the initial charge. In this case, a lithium metal layer is formed as the negative electrode mixture layer 21 after the initial charge and discharge.

[0037] 2 and 3, when viewed from the stacking direction Z, the outer peripheral end of the intermediate layer 50 is located outside the outer peripheral end of the negative electrode mixture layer 21, and a part of the intermediate layer 50 is in contact with a part of the outer peripheral side of the negative electrode current collector 22. This suppresses the occurrence of a short circuit.

[0038] (Insulating material) The insulating frame 61 improves the strength of the solid-state battery 1. As shown in Figs. 2 and 3, the insulating frame 61 is provided on the outer periphery in a direction perpendicular to the stacking direction Z of the positive electrode composite layer 31 and the positive electrode current collector 32. The material constituting the insulating frame 61 is not particularly limited as long as it has electronic insulation properties, and examples of the material include insulating oxides such as alumina, resins such as polyvinylidene fluoride (PVDF), and rubbers such as styrene-butadiene rubber (SBR). The insulating frame 61 may have ion conductivity.

[0039] The insulating layer 62 is formed in a region where the positive electrode tab extends from the positive electrode current collector 32. The occurrence of a short circuit is suppressed by the insulating layer 62. The material constituting the insulating layer 62 may be the same as that of the insulating frame 61.

[0040] In addition, the solid-state battery 1 may not have the intermediate layer 50 and / or the insulating member, if necessary.

[0041] [Solid-state battery manufacturing method] The manufacturing method of the solid-state battery 1 is not particularly limited, but may be, for example, the following method. First, the positive electrode composite layer 31 and the insulating layer 62 are formed by a coating method in a predetermined region on both sides of the positive electrode current collector substrate. Next, the positive electrode side solid electrolyte layer 41 is formed by a transfer method or a coating method in a predetermined region of the positive electrode current collector substrate on which the positive electrode composite layer 31 and the insulating layer 62 are formed. Next, after roll pressing, the positive electrode side solid electrolyte layer 41 is punched into a predetermined shape to obtain a positive electrode-solid electrolyte laminate. Therefore, the shape and dimensions of the end of the positive electrode-solid electrolyte laminate can be controlled, and the displacement of the positive electrode composite layer 31 on the front and back of the positive electrode current collector 32 is suppressed. In addition, the adhesion between the positive electrode composite layer 31 and the positive electrode side solid electrolyte layer 41 is improved, and the protrusion of the positive electrode side solid electrolyte layer 41 is suppressed.

[0042] The negative electrode mixture layer 21 is formed by a coating method in a predetermined region on one side of the negative electrode current collector substrate. Next, the intermediate layer 50 is formed by a transfer method or a coating method in the predetermined region of the negative electrode current collector substrate on which the negative electrode mixture layer 21 is formed. Next, the negative electrode side solid electrolyte layer 42 is formed by a transfer method or a coating method in the predetermined region of the negative electrode current collector substrate on which the intermediate layer 50 is formed. Next, after roll pressing, a predetermined shape is punched out to obtain a negative electrode-intermediate layer-solid electrolyte laminate. This suppresses contact between the negative electrode mixture layer 21 and the negative electrode side solid electrolyte layer 42, and suppresses the intermediate layer 50 from falling off. In addition, the adhesion between the negative electrode mixture layer 21, the intermediate layer 50, and the negative electrode side solid electrolyte layer 42 is improved, and the intermediate layer 50 and the negative electrode side solid electrolyte layer 42 are suppressed from popping out.

[0043] An insulating frame 61 is placed at a predetermined position on the anode-intermediate layer-solid electrolyte laminate. Next, the cathode-solid electrolyte laminate is placed at a predetermined position on the anode-intermediate layer-solid electrolyte laminate on which the insulating frame 61 is placed, so that the cathode-side solid electrolyte layer 41 and the anode-side solid electrolyte layer 42 face each other. Next, another anode-intermediate layer-solid electrolyte laminate is placed at a predetermined position on the anode-intermediate layer-solid electrolyte laminate on which the insulating frame 61 and the cathode-solid electrolyte laminate are placed, so that the cathode-side solid electrolyte layer 41 and the anode-side solid electrolyte layer 42 face each other, and then uniaxial pressing is performed to obtain a solid battery 1.

[0044] Here, when the positive electrode-solid electrolyte laminate and the negative electrode-intermediate layer-solid electrolyte laminate are arranged, a solvent capable of dissolving the solid electrolyte constituting the solid electrolyte composite 40 or a slurry containing the solid electrolyte is applied to the interface between the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42. As a result, the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 are bonded together, so that the interface resistance is reduced. In order to remove the solvent used when bonding the positive electrode-side solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 together or the solvent contained in the slurry, the solid electrolyte layer 41 and the negative electrode-side solid electrolyte layer 42 may be heated and dried as necessary. The timing of the heating and drying may be before or after the uniaxial pressing. For example, the solid battery 1 may be restrained by end plates and then heated and dried. This suppresses the occurrence of stacking misalignment and uneven contact of the solid battery 1.

[0045] The method for manufacturing the solid-state battery 1 is not limited to the above, and may be, for example, a method in which the solid electrolyte composite 40 is separately formed and then bonded to other layers or members.

[0046] Next, a description will be given of the configuration of a solid electrolyte composite according to another embodiment of the present invention. Note that the same components as those of the above-mentioned solid electrolyte composite 40 will be denoted by the same reference numerals, and the description thereof will be omitted.

[0047] Second Embodiment As shown in FIG. 5, the solid electrolyte composite 40a according to the present embodiment has a positive electrode side solid electrolyte layer 41a and a negative electrode side solid electrolyte layer 42a. The solid electrolyte composite 40a is provided with a high filler content region R1 in which the content of the filler and / or the porous substrate is higher than other portions. The high filler content region R1 has a stepped shape in which the solid electrolyte composite 40a is reduced. That is, the length of the high filler content region R1 in the Y direction on the positive electrode side solid electrolyte layer 41a side is shorter than the length of the high filler content region R1 in the Y direction on the negative electrode side solid electrolyte layer 42a side. This allows the solid electrolyte composite 40a to have a strength that can withstand impacts during stacking when the θ deviation during stacking is suppressed by the solid electrolyte composite 40a, and the shape of the solid electrolyte composite 40a can be maintained.

[0048] The method for producing the solid electrolyte composite 40a is not particularly limited, but may include a method in which the high filler content region R1 is first formed using a solid electrolyte slurry containing a relatively large amount of filler and / or porous base material in a mold corresponding to the shape of the high filler content region R1, and then the areas other than the high filler content region R1 are coated with a solid electrolyte slurry containing a relatively small amount of filler and / or porous base material.

[0049] Third Embodiment As shown in Fig. 6, the solid electrolyte composite 40b according to this embodiment has a positive electrode side solid electrolyte layer 41b and a negative electrode side solid electrolyte layer 42b. The solid electrolyte composite 40b has a high filler content region R2 having a stepped shape similar to the solid electrolyte composite 40a. Unlike the high filler content region R1, the end of the high filler content region R2 in the direction Y does not reach the outer periphery of the solid electrolyte composite 40b. This reduces the total amount of filler and / or porous substrate, improving the energy density of the solid battery and maintaining the necessary strength.

[0050] The method for producing the solid electrolyte composite 40b is not particularly limited, but may include a method in which the high filler content region R2 is first formed using a solid electrolyte slurry containing a relatively large amount of filler and / or porous base material in a mold corresponding to the shape of the high filler content region R2, and then the high filler content region R2 formed above is immersed in a tank filled with a solid electrolyte slurry containing a relatively small amount of filler and / or porous base material and dried.

[0051] Fourth Embodiment As shown in Fig. 7, the solid electrolyte composite 40c according to this embodiment has a positive electrode side solid electrolyte layer 41c and a negative electrode side solid electrolyte layer 42c. The solid electrolyte composite 40c has a high filler content region R3. The high filler content region R3 is a rib-shaped region that is a further reduced version of the high filler content region R2 having a stepped shape. This allows the total amount of filler and / or porous substrate to be further reduced compared to the solid electrolyte composite 40b, improving the energy density of the solid battery while maintaining the necessary strength.

[0052] The solid electrolyte composite 40c can be manufactured by a method similar to that of the solid electrolyte composite 40b.

[0053] Although the embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and the above embodiment may be modified as appropriate within the scope of the present invention. For example, the arrangement of the positive electrode layer and the negative electrode layer in the solid battery 1 may be reversed. In this case, the arrangement of the positive electrode side solid electrolyte layer and the negative electrode side solid electrolyte layer may also be reversed. [Explanation of symbols]

[0054] 1 solid state battery 21 Negative electrode composite layer (negative electrode layer) 22 Negative electrode current collector (negative electrode layer) 31 Positive electrode mixture layer (positive electrode layer) 32 Positive electrode collector (positive electrode layer) 40, 40a, 40b, 40c solid electrolyte complex 41 Positive electrode solid electrolyte layer 42 Negative electrode side solid electrolyte layer 50 Middle Class 61 Insulating frame (insulating material) 62 Insulating layer (insulating material) R1, R2, R3 high filler content area

Claims

1. A solid electrolyte composite disposed between a positive electrode layer and a negative electrode layer in a solid-state battery, a cathode-side solid electrolyte layer disposed on the cathode layer side and an anode-side solid electrolyte layer disposed on the anode layer side, a stepped shape having a step between the positive electrode-side solid electrolyte layer and the negative electrode-side solid electrolyte layer; a solid electrolyte composite, wherein at least the negative electrode-side solid electrolyte layer contains a filler and / or a porous substrate, and a content of the filler and / or the porous substrate in the negative electrode-side solid electrolyte layer is higher than a content of the filler and / or the porous substrate in the positive electrode-side solid electrolyte layer.

2. the negative electrode-side solid electrolyte layer has a lower content of the filler and / or the porous substrate in the vicinity of the interface on the negative electrode layer side and in the vicinity of the interface on the positive electrode-side solid electrolyte layer side than in other portions; 2. The solid electrolyte composite according to claim 1, wherein the positive electrode-side solid electrolyte layer has a lower content of the filler and / or the porous substrate in a vicinity of an interface on the positive electrode layer side and in a vicinity of an interface on the negative electrode-side solid electrolyte layer side than in other portions.

3. The solid-state battery further includes an insulating member, 3. The solid electrolyte composite according to claim 2, wherein the positive electrode solid electrolyte layer and the negative electrode solid electrolyte layer have a lower content of the filler and / or the porous substrate near an interface with the insulating member than at other portions.

4. A high-filler content region is provided inside the solid electrolyte composite, in which the content of the filler and / or the porous substrate is higher than other portions, 2. The solid electrolyte composite according to claim 1, wherein the filler-rich region has a stepped shape having a step between the positive electrode-side solid electrolyte layer side and the negative electrode-side solid electrolyte layer side.

Citation Information

Patent Citations

  • All-solid battery

    JP2021039876A

  • Manufacturing method of all-solid battery

    JP2022131191A

  • All-solid battery and manufacturing method thereof

    JP2023009988A

  • Non-aqueous electrolyte battery and manufacturing process therefor

    WO2011102027A1

  • All-solid-state secondary battery, production method for same, solid electrolyte film for all-solid-state-electrolyte battery, and production method for same

    WO2018164051A1