Laminate type power storage element and manufacturing method thereof
The laminated power storage element design with a recessed area and protruding resin portion addresses short circuit issues, ensuring precise positioning and consistent dimensions, enhancing performance and yield.
Patent Information
- Application Number
- JP2023058614
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
AI Technical Summary
Existing laminated power storage elements face issues with external short circuits between the positive and negative electrode tabs due to variations in the protrusion of the tab film, leading to inaccurate positioning and reduced performance and yield.
A laminated power storage element design featuring a recessed area along the side of the exterior body where the electrode tabs penetrate, with a protruding insulating resin portion to prevent short circuits and maintain precise positioning.
Prevents external short circuits between electrode tabs while ensuring accurate positioning, maintaining consistent external dimensions and improving yield and performance.
Smart Images

Figure 2024145974000001_ABST
Abstract
Description
[Technical field]
[0001] An embodiment of the present invention relates to a laminate-type energy storage element and a manufacturing method thereof. [Background technology]
[0002] In recent years, devices in which storage elements are mounted have been made thinner, and there is an increasing demand for thinner storage elements mounted in such devices. As shown in Patent Document 1, for example, a laminated storage element is an example of a storage element that has been made thinner, in which an electrode body in which a sheet-shaped positive electrode and a sheet-shaped negative electrode are arranged opposite each other with a separator interposed therebetween is covered with an exterior body made of a laminate film. The exterior body covers the electrode body by sandwiching the electrode body between two laminate films. The exterior body accommodates the electrode body inside by welding the two laminate films together. In the laminated storage element, a part of a positive electrode tab that contacts the positive electrode inside the exterior body and a part of a negative electrode tab that contacts the negative electrode inside the exterior body are exposed to the outside of the exterior body by penetrating between the two laminate films.
[0003] An insulating resin layer is formed on both sides of the laminate film, and even if the laminate film comes into contact with the positive and negative tabs at the portion where the resin layer is formed, no short circuit problem occurs. However, no resin layer is formed on the end face of the laminate film, and if the end face of the laminate film comes into contact with the positive and negative tabs, a short circuit problem occurs. In the laminate type storage element disclosed in Patent Document 1, a seal material (tab film) made of insulating resin is protruded from between two laminate films along one side of the exterior body where the positive and negative tabs are exposed, thereby preventing the positive and negative tabs from coming into contact with the end faces of the laminate film and causing a short circuit. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2018-010751 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, if the tab film protrudes from between the laminate films, the outer dimensions of the laminated-type energy storage element will vary depending on the amount of protrusion of the tab film. For example, the tab film is melted to weld the laminate film, but it is difficult to precisely control the flow of the tab film after melting, and the amount of protrusion of the tab film is likely to vary. Therefore, the outer dimensions of the laminated-type energy storage element are likely to vary.
[0006] The laminated energy storage element may require highly accurate positioning during its manufacturing process, and therefore, if there is variation in the outer dimensions, there is a problem that the performance of the laminated energy storage element may be degraded and the yield may be reduced.
[0007] The disclosed technology has been made in consideration of these points, and aims to obtain a laminate-type storage element that can prevent external short-circuiting of the positive electrode tab and the negative electrode tab without reducing positioning accuracy. [Means for solving the problem]
[0008] A laminated-type energy storage element according to one embodiment of the present disclosure comprises an electrode body in which a sheet-shaped positive electrode and a sheet-shaped negative electrode are stacked with a separator between them, an exterior body having a first sheet-shaped outer casing that covers the electrode body from the positive electrode side and a second sheet-shaped outer casing that covers the electrode body from the negative electrode side, and which houses the electrode body and has a first side, a positive electrode tab in contact with the positive electrode and partially exposed to the outside of the exterior body from the first side, and a negative electrode tab in contact with the negative electrode and partially exposed to the outside of the exterior body from the first side, wherein a recess is formed on the surface of the exterior body extending along the first side, and a second side of the outer periphery of the recess that is on the first side has a separation range that moves away from the first side as it approaches the end. Effect of the Invention
[0009] According to one aspect of the laminated energy storage element disclosed in the present application, it is possible to obtain a laminated energy storage element that can prevent external short-circuiting of the positive electrode tab and the negative electrode tab without reducing positioning accuracy. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a plan view of the laminate type energy storage element in accordance with the first embodiment. [Diagram 2] FIG. 2 is an exploded perspective view of the laminate type energy storage element in accordance with the first embodiment. [Diagram 3] FIG. 3 is a cross-sectional view taken along line III-III shown in FIG. [Figure 4] FIG. 4 is a cross-sectional view taken along the line IV-IV shown in FIG. [Diagram 5] FIG. 5 is a cross-sectional view taken along line VV shown in FIG. [Figure 6] FIG. 6 is a flowchart illustrating a manufacturing process of the laminate type energy storage element according to the first embodiment. [Figure 7] FIG. 7 is a cross-sectional view illustrating the effect of preventing a short circuit in the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of the laminate-type energy storage element and the method for producing the same disclosed in the present application will be described in detail with reference to the accompanying drawings. Note that the battery disclosed in the present application is not limited to the following preferred embodiments.
[0012] (Embodiment 1) Fig. 1 is a plan view of a laminated energy storage element according to embodiment 1. Fig. 2 is an exploded perspective view of the laminated energy storage element according to embodiment 1. The laminated energy storage element 1 includes an electrode assembly 2, an outer casing 3, a positive electrode tab 4, a negative electrode tab 5, and a tab film 6.
[0013] The electrode body 2 includes a positive electrode 21, a negative electrode 22, and a separator 23. The positive electrode 21 is formed in a sheet shape. The positive electrode 21 is formed by disposing a positive electrode material containing a positive electrode active material on one side of a positive electrode collector made of a metal plate or metal foil. The negative electrode 22 is formed in a sheet shape. The negative electrode 22 is formed by disposing a negative electrode material containing a negative electrode active material on one side of a negative electrode collector made of a metal plate or metal foil. The separator 23 is formed in a sheet shape. The separator 23 is formed of an insulator. Examples of the insulator include polyolefin or cellulose. The positive electrode 21 and the negative electrode 22 are laminated with the separator 23 sandwiched therebetween.
[0014] The exterior body 3 has a first exterior body 31 and a second exterior body 32. The exterior body 3 is formed in a quadrangular shape in a plan view. The first exterior body 31 and the second exterior body 32 are aluminum laminate films. In a plan view, the first exterior body 31 and the second exterior body 32 are formed to have a larger outer shape than the electrode body 2. The exterior body 3 sandwiches the electrode body 2 between the first exterior body 31 and the second exterior body 32, and seals the electrode body 2 inside by welding the edges of the first exterior body 31 and the second exterior body 32 to each other. In the following description, the surfaces of the first exterior body 31 and the second exterior body 32 that face each other are referred to as the back surface, and the surface opposite the back surface is referred to as the front surface. An electrolyte is enclosed inside the sealed exterior body 3 together with the electrode body 2. The electrolyte may be an aqueous electrolyte or a non-aqueous organic electrolyte.
[0015] The first exterior body 31 and the second exterior body 32 are provided with resin layers on both sides of the metal foil, which is the base material. More specifically, a resin layer capable of being thermally welded is formed on the back surface of the first exterior body 31 and the second exterior body 32. The resin layer capable of being thermally welded is formed of, for example, polypropylene. A resin layer serving as a protective layer is formed on the front surface of the first exterior body 31 and the second exterior body 32. The resin layer serving as a protective layer is formed of, for example, polyamide resin. Both the resin layers formed on the front surface and the back surface of the first exterior body 31 and the second exterior body 32 are insulating resin layers. The first exterior body 31 and the second exterior body 32 are formed by cutting an aluminum laminate film on both sides of which a resin layer is formed. Therefore, the end surface, which is the cut surface, is not covered with resin and the metal foil, which is the base material, is exposed. In the first embodiment, aluminum foil is exemplified as the metal foil, but the present invention is not limited to this, and may be, for example, stainless steel foil.
[0016] The positive electrode tab 4 is a strip-shaped member made of metal. One end 4a of the positive electrode tab 4 is in contact with the positive electrode 21 inside the exterior body 3. The other end 4b of the positive electrode tab 4 penetrates between the first exterior body 31 and the second exterior body 32 and is exposed to the outside of the exterior body 3.
[0017] The negative electrode tab 5 is a strip-shaped member made of metal. One end 5a of the negative electrode tab 5 is in contact with the negative electrode 22 inside the exterior body 3. The other end 5b of the negative electrode tab 5 penetrates between the first exterior body 31 and the second exterior body 32 and is exposed to the outside of the exterior body 3. Here, the positive electrode tab 4 and the negative electrode tab 5 are exposed from a first side 3a of the exterior body 3 that is quadrangular in plan view. The first side 3a of the exterior body 3 may be formed in a straight line as shown in the figure, or the corners may be chamfered.
[0018] The tab film 6 is provided on the inside of the first exterior body 31 and the inside of the second exterior body 32 along the first side 3a. The tab film 6 is a sealing material made of insulating resin. At the first side 3a, the positive electrode tab 4 and the negative electrode tab 5 penetrate between the first exterior body 31 and the second exterior body 32, so that the gap between the first exterior body 31 and the second exterior body 32 becomes large, and the adhesion may be insufficient by heat welding only the resin layer provided on the inner surface of the first exterior body 31 and the inner surface of the second exterior body 32. Therefore, at the first side 3a, the first exterior body 31 and the second exterior body 32 are more reliably bonded to each other by heat welding using the tab film 6.
[0019] The thermal welding of the tab film 6 is performed by applying heat while pressing a metal mold against the surface of the exterior body 3 against the area where the tab film 6 is provided. A recess 7 is formed in the shape of the metal mold on the surface of the exterior body 3 against which the metal mold is pressed. As the surface of the exterior body 3 is recessed, the tab film 6 melted on the back surface protrudes from between the first exterior body 31 and the second exterior body 32 to the outside of the first side 3a, forming a protruding portion 6a.
[0020] The recess 7 has a shape that extends along the first side 3a. The second side 7a of the outer periphery of the recess 7, which is on the first side 3a side, has a certain range from the end portion as a separation range 7b. In the separation range 7b, the second side 7a becomes more distant from the first side 3a as it approaches the end portion. In the first embodiment, the second side 7a has an R-shape in the separation range 7b. The separation range 7b may be formed in a C-chamfered shape.
[0021] Fig. 3 is a cross-sectional view taken along line III-III shown in Fig. 1. Fig. 4 is a cross-sectional view taken along line IV-IV shown in Fig. 1. Fig. 5 is a cross-sectional view taken along line VV shown in Fig. 1. Figs. 3 to 5 also show a die 10 pressed against the surface of the exterior body 3 in the manufacturing process of the laminated type energy storage element 1.
[0022] 3, in the area where the positive electrode tab 4 is provided, in addition to the exterior body 3 and the tab film 6, the positive electrode tab 4 is also sandwiched between the mold 10, so that the molten tab film 6 protrudes from between the first exterior body 31 and the second exterior body 32 to the outside of the first side 3a. This protruding portion becomes a protruding portion 6a. Although not shown in the figure, a protruding portion 6a is also formed in the area where the negative electrode tab 5 is provided for the same reason.
[0023] As shown in Fig. 4, in the area where the positive electrode tab 4 and the negative electrode tab 5 are not provided, the exterior body 3 and the tab film 6 are sandwiched between the molds 10, but the positive electrode tab 4 and the negative electrode tab 5 are not sandwiched. Therefore, the space that the tab film 6 can occupy between the first exterior body 31 and the second exterior body 32 is wider than the area shown in Fig. 3. This makes it difficult for the molten tab film 6 to protrude.
[0024] A cross section in the separation range 7b is shown in Fig. 5. In the separation range 7b, the positive electrode tab 4 and the negative electrode tab 5 are not sandwiched between the mold 10 as in Fig. 4, and in addition, the distance X between the second side 7a of the recess 7 and the first side 3a of the exterior body 3 is wide, so that the molten tab film 6 is less likely to reach the first side 3a, and protrusion is less likely to occur.
[0025] Next, the manufacturing process of the laminated type energy storage element 1 will be described. FIG. 6 is a flow chart for explaining the manufacturing process of the laminated type energy storage element according to the first embodiment. First, the positive electrode tab 4 is brought into contact with the positive electrode 21 (step S1). Next, the negative electrode tab 5 is brought into contact with the negative electrode 22 (step S2). Next, the positive electrode 21 and the negative electrode 22 are arranged to face each other with the separator 23 interposed therebetween to form the electrode body 2 (step S3). Next, the electrode body 2 is housed in the exterior body 3 while the other ends 4b, 5b of the positive electrode tab 4 and the negative electrode tab 5 are exposed to the outside (step S4). Next, the mold 10 is brought into contact with the exterior body 3, and the tab film 6 and the resin layer are heat-welded and sealed (step S5). Through the above steps, the laminated type energy storage element 1 is manufactured.
[0026] The laminated type energy storage element described above includes an electrode body 2 in which a sheet-shaped positive electrode 21 and a sheet-shaped negative electrode 22 are laminated with a separator 23 sandwiched therebetween, an exterior body 3 having a first sheet-shaped outer casing 31 covering the electrode body 2 from the positive electrode 21 side and a second sheet-shaped outer casing 32 covering the electrode body 2 from the negative electrode 22 side, and housing the electrode body 2 therein and having a first side 3a, a positive electrode tab 4 in contact with the positive electrode 21 and partially exposed from the first side 3a to the outside of the exterior body 3, and a negative electrode tab 5 in contact with the negative electrode 22 and partially exposed from the first side 3a to the outside of the exterior body 3, and a recess 7 extending along the first side 3a is formed on the surface of the exterior body 3, and a second side 7a on the first side 3a side of the outer periphery of the recess 7 has a separation range 7b that becomes more distant from the first side 3a as it approaches the end. This allows a protruding portion 6a made of an insulating resin to be provided at a portion of the first side 3a of the exterior body 3 where the positive electrode tab 4 and the negative electrode tab 5 penetrate. By forming the protruding portion 6a at a portion of the first side 3a of the exterior body 3 where the positive electrode tab 4 and the negative electrode tab 5 penetrate, it is possible to prevent a short circuit between the positive electrode tab 4 and the negative electrode tab 5 and the exterior body 3.
[0027] FIG. 7 is a cross-sectional view illustrating the effect of preventing a short circuit in the first embodiment. Since a resin layer is provided on the front and back surfaces of the first outer casing 31 and the second outer casing 32, a short circuit occurs between the positive electrode tab 4 or the negative electrode tab 5 and the outer casing 3 when the end faces 31a, 32a of the first outer casing 31 or the second outer casing 32 come into contact with the positive electrode tab 4 or the negative electrode tab 5.
[0028] As shown in FIG. 7, by providing the protruding portion 6a protruding from the end faces 31a, 32a, even if the positive electrode tab 4 or the negative electrode tab 5 is bent, the positive electrode tab 4 or the negative electrode tab 5 is unlikely to come into contact with the end faces 31a, 32a, and a short circuit is unlikely to occur.
[0029] Furthermore, since the tab film 6 hardly protrudes from the first side 3a except for the portion of the first side 3a through which the positive electrode tab 4 and the negative electrode tab 5 penetrate, the outer dimensions of the laminated type storage element 1 match the outer dimensions of the exterior body 3. Therefore, the outer dimensions do not vary depending on the amount of protrusion of the tab film 6 except for the portion through which the positive electrode tab 4 and the negative electrode tab 5 penetrate. By using the portion through which the positive electrode tab 4 and the negative electrode tab 5 penetrate as a reference, positioning in the manufacturing process can be performed with high accuracy. This makes it possible to prevent a decrease in performance and a decrease in yield of the laminated type storage element 1 caused by poor positioning.
[0030] In order to make the second side 7a rounded as illustrated in the example in the separation range 17, the mold 10 is also formed in a rounded shape. The mold 10 formed in a rounded shape is less likely to scratch the exterior body 3 than when a mold 10 having a corner shape other than a rounded shape is brought into contact with the exterior body 3.
[0031] Moreover, the recess 7 is formed away from the first side 3a of the exterior body 3, and a gap is provided between the second side 7a of the recess 7 and the first side 3a of the exterior body 3. Since the tab film 6 is hardly melted in the gap, protrusion of the tab film 6 can be more reliably reduced.
[0032] In addition, since the first exterior body 31 and the second exterior body 32 are welded to each other at the first side 3a via the tab film 6, the positive electrode tab 4 and the negative electrode tab 5 can be securely sealed even if they are penetrated. This does not exclude the case where the tab film 6 is not provided and the first exterior body 31 and the second exterior body 32 are welded to each other using a resin layer for the purpose of thermal welding formed on the back surface of the first exterior body 31 and the back surface of the second exterior body 32. In addition, since the tab film 6 only needs to be provided along the first side 3a, the shape of the tab film 6 can be simplified. This allows the tab film 6 to be manufactured at low cost.
[0033] Furthermore, from the viewpoint of making the laminated-type storage element 1 thinner, it is preferable that the thickness of the overlapping portion of the outer casing 3, the positive electrode 21, the negative electrode 22, the separator 23, and the positive electrode tab 4 or the negative electrode tab 5 is 0.6 mm or less.
[0034] Furthermore, by forming the laminated energy storage element 1 as a single layer having one positive electrode 21 and one negative electrode 22, it is possible to reduce the thickness of the laminated energy storage element 1. This does not exclude the laminated energy storage element 1 as a multi-layered element having a plurality of positive electrodes 21 and a plurality of negative electrodes 22.
[0035] Note that the first side 3a may not be provided with the tab film 6, and the first exterior body 31 and the second exterior body 32 may be welded together with a resin layer formed on the back surface of each of them. As in the case where the tab film 6 is provided, the resin layer protrudes around the positive electrode tab 4 and the negative electrode tab 5 to form protruding portions. Furthermore, the molten resin layer hardly protrudes from areas other than the portions where the positive electrode tab 4 and the negative electrode tab 5 penetrate, and the laminated type energy storage element 1 can be positioned with high accuracy. [Explanation of symbols]
[0036] 1. Laminated energy storage element 2 Electrode body 3 Exterior body 3a First side 4 Positive tab 4a one end 4b Other end 5 Negative tab 5a one end 5b Other end 6 Tab Film 6a Protruding part 7 Recess 7a Second Side 7b Distance range 21 Positive electrode 22 Negative electrode 23 Separator 31 First exterior body 31a,32a end face 32 Second exterior body
Claims
1. an electrode assembly in which a sheet-shaped positive electrode and a sheet-shaped negative electrode are stacked with a separator sandwiched therebetween; an exterior body that houses the electrode body and has a first side and includes a sheet-like first exterior body that covers the electrode body from the positive electrode side and a sheet-like second exterior body that covers the electrode body from the negative electrode side; a positive electrode tab in contact with the positive electrode and a portion of which is exposed to the outside of the exterior body from the first side; a negative electrode tab in contact with the negative electrode and a portion of which is exposed to the outside of the exterior body from the first side, a recess extending along the first side is formed on a surface of the exterior body, A laminated energy storage element in which a second side of the outer periphery of the recess that is on the side of the first side has a certain range from the end that becomes increasingly farther away from the first side toward the end.
2. The laminate type energy storage element according to claim 1 , wherein the second side in the spaced range is rounded.
3. The laminate-type energy storage element according to claim 1 , wherein the recess is spaced apart from the first side.
4. The laminate type energy storage element according to claim 1 , wherein the first side of the first exterior body and the second exterior body are welded together via a tab film.
5. 2 . The laminate type energy storage element according to claim 1 , wherein a thickness of an overlapping portion between the exterior body, the positive electrode, the negative electrode, and the positive electrode tab or the negative electrode tab is 0.6 mm or less.
6. 2. The laminate type storage element according to claim 1, comprising one each of the positive electrode and the negative electrode.
7. contacting a positive electrode tab with a sheet-like positive electrode; A step of contacting a negative electrode tab with a sheet-like negative electrode; forming an electrode assembly by disposing the positive electrode and the negative electrode opposite each other with a separator interposed therebetween; a step of housing the electrode assembly in an exterior body while a portion of the positive electrode tab and the negative electrode tab are exposed to the outside; and a step of sealing the surface of the exterior body by contacting a mold with the surface of the exterior body. the exterior body has a first side, and the positive electrode tab and the negative electrode tab are exposed from the first side, The mold has a shape extending along the first side, A manufacturing method for a laminated type energy storage element, in which a second edge on the first edge side of the outer periphery of a recess formed on the surface of the outer casing in the sealing process has a certain range from the end that becomes more distant from the first edge toward the end.
Citation Information
Patent Citations
Laminated battery, its manufacturing method and die for manufacturing laminated battery
JP2005108486A
Electrochemical-cell and its manufacturing method
JP2005243453A
Electrode geometry of galvanicell
JP2012523094A
A method for sealing the side of a pouch-type battery including a two-step sealing process.
JP2020506516A
Pouch-type secondary battery, battery pack, and method for manufacturing pouch-type secondary battery
JP2023500944A