Laminated ceramic electronic component and method for manufacturing the same
The multilayer ceramic electronic component design with a larger first ridgeline curvature and a protective portion effectively addresses the issue of reduced impact resistance by canceling out force propagation, enhancing reliability and durability.
Patent Information
- Application Number
- JP2023059348
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
AI Technical Summary
The side portions of conventional multilayer ceramic electronic components become thinner towards the edges, reducing the impact-reducing effect against external impacts, leading to reduced reliability.
A multilayer ceramic electronic component design featuring a ceramic body with a protective portion including a ridge connecting circumferential surfaces, a base film, and a plating film, where the radius of curvature of the first ridgeline portion is larger than that of the second ridgeline portion, and the internal electrodes are stacked perpendicularly, with a side margin part covering the functional part from a perpendicular direction.
The design enhances the reliability of the component against impact by canceling out the force propagation within the ceramic body, reducing the likelihood of cracks and improving the alignment of internal electrodes, thereby increasing the component's durability.
Smart Images

Figure 2024146448000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a multilayer ceramic electronic component and a method for manufacturing the same. [Background technology]
[0002] A multilayer ceramic electronic component such as a multilayer ceramic capacitor may include a functional section and a protective section provided on a side surface of the functional section. The functional section is formed by alternately laminating a plurality of dielectric layers and a plurality of internal electrodes, and the plurality of internal electrodes are exposed from the side surface of the functional section. The protective section provided on the side surface of the functional section is called a side section or a side margin section, and covers the internal electrodes exposed from the side surface. A configuration has been proposed in the past in which a side section is provided on the side surface of the functional section, and an angle between the side section and an imaginary line connecting the ends of the internal electrodes is 90° or less (see, for example, Patent Document 1). Patent Document 1 claims that such a configuration can provide a multilayer ceramic electronic component with excellent reliability. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-191159 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the configuration described in Patent Document 1, the side portions become thinner toward the edges in the stacking direction of the internal electrodes, which is thought to reduce the impact absorbing effect of the side portions against external impacts.
[0005] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a multilayer ceramic electronic component having high reliability against shocks, and a method for manufacturing the same. [Means for solving the problem]
[0006] In order to achieve the above object, a multilayer ceramic electronic component includes a ceramic body having a protective portion including end faces facing a first direction, a plurality of peripheral surfaces connected to the end faces and extending in the first direction, and a ridge portion having a recess extending along the first direction and connecting between the plurality of peripheral surfaces, and a functional portion disposed inside the protective portion; and an external electrode having an undercoat film covering the end faces and a plating film formed on the undercoat film, wherein the functional portion is made of a plurality of ceramics stacked in a second direction perpendicular to the first direction. The protective portion has an internal electrode, and includes a cover portion stacked along the second direction on the functional portion, and a side margin portion covering the functional portion from a third direction perpendicular to the first direction and the second direction, and the ridge portion includes, separated by the recess, a first ridge portion provided on the cover portion side and a second ridge portion provided on the side margin portion side, and in a cross section including the second direction and the third direction, a radius of curvature R1 of the first ridge portion is greater than a radius of curvature R2 of the second ridge portion.
[0007] In the multilayer ceramic electronic component configured as described above, a dimension of the multilayer ceramic electronic component in the second direction may be larger than a dimension of the multilayer ceramic electronic component in the third direction.
[0008] In the monolithic ceramic electronic component having the above-described configuration, the radius of curvature R1 of the first edge portion may be 15 μm or more and 25 μm or less.
[0009] Furthermore, in the monolithic ceramic electronic component configured as described above, the radius of curvature R2 of the second edge portion may be set to be not less than 0 μm and not more than 20 μm.
[0010] In the laminated ceramic electronic component having the above-mentioned configuration, the base film includes a first covering portion formed on the end face, a plurality of second covering portions formed on each of the plurality of peripheral surfaces, and a third covering portion formed on the recess and spaced apart from at least one of the plurality of second covering portions, and the plating film can be configured to continuously cover the first covering portion, the plurality of second covering portions, and the third covering portion.
[0011] Furthermore, in the multilayer ceramic electronic component having the above-described configuration, the functional section may have a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, and the positions of the ends of the plurality of internal electrodes in a third direction perpendicular to the first and second directions may be aligned with each other within a range of 0.5 μm in the third direction.
[0012] In order to achieve the above object, a method for manufacturing a multilayer ceramic electronic component includes the steps of: producing a ceramic multilayer chip having an end face facing a first direction, a functional section having a plurality of internal electrodes laminated in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed from a side surface facing a third direction perpendicular to the first direction and the second direction; and laminating a cover section on the functional section along the second direction; forming a first ridge section that is continuous with the end face and connects a peripheral surface extending in the first direction to the side surface; and laminating the cover section on the side surface. The process of producing a ceramic body by forming a side margin portion having a second ridge portion extending along a first direction and arranged parallel to the first ridge portion across a recess, firing the ceramic laminated chip and the side margin portion, and forming an external electrode having a base film covering the end face and a plating film formed on the base film includes chamfering to make a radius of curvature R1 of the first ridge portion larger than a radius of curvature R2 of the second ridge portion in a cross section including the second direction and the third direction.
[0013] In the manufacturing method of a multilayer ceramic electronic component having the above-mentioned configuration, the step of forming the external electrode can include forming a conductive base film including a first covering portion formed on the end face of the ceramic body, a plurality of second covering portions formed on a plurality of peripheral surfaces connected to the end face and extending in the first direction, and a third covering portion formed on the recess and spaced apart at an edge from at least one of the plurality of second covering portions, and forming a plating film that continuously covers the first covering portion, the plurality of second covering portions, and the third covering portion.
[0014] Furthermore, in the manufacturing method of the multilayer ceramic electronic component having the above-mentioned configuration, the step of forming the side margin portion may include forming a first side margin portion laminated on the side surface, and a second side margin portion laminated on the first side margin portion and having a larger thermal shrinkage rate than the first side margin portion.
[0015] Furthermore, in the method for manufacturing a multilayer ceramic electronic component having the above-mentioned configuration, the first side margin portion can be formed by attaching a first ceramic sheet onto the side surface, and the second side margin portion can be formed by attaching a second ceramic sheet, the second ceramic sheet having a larger thermal shrinkage rate than the first ceramic sheet, onto the first ceramic sheet. Effect of the Invention
[0016] According to the present invention, it is possible to provide a multilayer ceramic electronic component having high reliability against impacts and a method for manufacturing the same. [Brief description of the drawings]
[0017] [Figure 1] 1 is a perspective view of a multilayer ceramic capacitor according to an embodiment of the present invention; [Diagram 2] 2 is a cross-sectional view taken along line AA' of the multilayer ceramic capacitor. [Diagram 3] 5 is a cross-sectional view taken along line BB' of the multilayer ceramic capacitor. [Figure 4] 3 is a cross-sectional view taken along line CC' of the multilayer ceramic capacitor. [Diagram 5] FIG. 5 is an enlarged cross-sectional view of FIG. [Figure 6] 1A is an explanatory diagram showing positions for measuring the radius of curvature of a first ridgeline portion and a second ridgeline portion in a multilayer ceramic capacitor according to an embodiment, FIG. 1B is a diagram explaining a method for measuring the radius of curvature of the first ridgeline portion and a second ridgeline portion, and FIG. 1C is a diagram explaining another method for measuring the radius of curvature of the first ridgeline portion and a second ridgeline portion. [Figure 7]2A is a partially enlarged cross-sectional view showing a first ridgeline portion and a second ridgeline portion in the multilayer ceramic capacitor of the embodiment, and FIG. 2B is a partially enlarged cross-sectional view showing the first ridgeline portion and the second ridgeline portion in the multilayer ceramic capacitor of the comparative example. [Figure 8] Fig. 1A is a diagram showing an angle θ1 formed by a tangent line connecting the first ridge line and the second ridge line with a line segment extending from the main surface of the ceramic body along the Y-axis direction in a multilayer ceramic capacitor of an embodiment, and a height t1 from the installation surface of the multilayer ceramic capacitor to the second ridge line in a multilayer ceramic capacitor of a comparative example, and Fig. 1B is a diagram showing an angle θ2 formed by a tangent line connecting the first ridge line and the second ridge line with a line segment extending from the main surface of the ceramic body along the Y-axis direction in a multilayer ceramic capacitor of a comparative example, and a height t2 from the installation surface of the multilayer ceramic capacitor to the second ridge line in a multilayer ceramic capacitor of a comparative example. [Figure 9] 4 is a flowchart showing an example of a method for manufacturing the multilayer ceramic capacitor. [Figure 10] 3A to 3C are perspective views illustrating a manufacturing process of the multilayer ceramic capacitor. [Figure 11] 3A to 3C are perspective views illustrating a manufacturing process of the multilayer ceramic capacitor. [Figure 12] 3A to 3C are perspective views illustrating a manufacturing process of the multilayer ceramic capacitor. [Figure 13] 3A to 3C are schematic cross-sectional views showing a manufacturing process of the multilayer ceramic capacitor. [Figure 14] 3A to 3C are schematic cross-sectional views showing a manufacturing process of the multilayer ceramic capacitor. [Figure 15] 3A to 3C are schematic cross-sectional views showing a manufacturing process of the multilayer ceramic capacitor. [Figure 16] 3A to 3C are perspective views illustrating a manufacturing process of the multilayer ceramic capacitor. [Figure 17] 3A to 3C are perspective views illustrating a manufacturing process of the multilayer ceramic capacitor. [Figure 18] 1 is a graph showing the crack occurrence rate in an impact load test for Examples and Comparative Examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings, an X-axis, a Y-axis, and a Z-axis that are mutually orthogonal are shown as appropriate. The X-axis, the Y-axis, and the Z-axis are common to all the drawings. The X-axis direction corresponds to the first direction, the Y-axis direction corresponds to the third direction, and the Z-axis direction corresponds to the second direction.
[0019] [Overall configuration of multilayer ceramic capacitor 10] 1 to 4 are diagrams showing a multilayer ceramic capacitor 10 according to a first embodiment of the present invention. Fig. 1 is a perspective view of the multilayer ceramic capacitor 10. Fig. 2 is a cross-sectional view of the multilayer ceramic capacitor 10 taken along line AA' in Fig. 1. Fig. 3 is a cross-sectional view of the multilayer ceramic capacitor 10 taken along line BB' in Fig. 1. Fig. 4 is a cross-sectional view of the multilayer ceramic capacitor 10 taken along line CC' in Fig. 1.
[0020] The multilayer ceramic capacitor 10 includes a ceramic body 11 and two external electrodes 14a, 14b. The two external electrodes 14a, 14b are formed on the surfaces of the ceramic body 11, respectively.
[0021] The ceramic body 11 has a capacitance forming portion 16 and a protective portion 17. The protective portion 17 constitutes the peripheral portion of the ceramic body 11 and has two end faces 11a facing the X-axis direction, two side faces 11b facing the Y-axis direction, two main faces 11c facing the Z-axis direction, and a ridge portion 11e connecting the main faces 11c and the side faces 11b. The side faces 11b and the main faces 11c constitute a plurality of peripheral surfaces in this embodiment. The end faces 11a, the side faces 11b, and the main faces 11c are, for example, substantially flat surfaces, but may be rounded.
[0022] In detail, the protective portion 17 has a cover portion 18 located outside the capacitance forming portion 16 in the Z-axis direction, a side margin portion 19 located outside the capacitance forming portion 16 in the Y-axis direction, and an end margin portion 20 located outside the capacitance forming portion 16 in the X-axis direction.
[0023] The capacitance forming portion 16 is disposed inside the protective portion 17, and constitutes a functional portion in this embodiment. The capacitance forming portion 16 is formed by stacking a plurality of first internal electrodes 12 and a plurality of second internal electrodes 13 in the Z-axis direction via ceramic layers 15 (see FIG. 2). The internal electrodes 12, 13 are both sheet-shaped extending along the XY plane, and are alternately disposed along the Z-axis direction.
[0024] The internal electrodes 12, 13 are each made of a good electrical conductor and function as internal electrodes of the multilayer ceramic capacitor 10. Examples of good electrical conductors that can be used to form the internal electrodes 12, 13 include metals and alloys containing nickel (Ni), copper (Cu), palladium (Pd), platinum (Pt), silver (Ag), gold (Au), or the like as a main component.
[0025] 2, the first internal electrode 12 is extended to, for example, one end face 11a of the ceramic body 11 and connected to one external electrode 14a. The second internal electrode 13 is extended to the other end face 11a and connected to the other external electrode 14b.
[0026] The ceramic layers 15 are made of dielectric ceramics. In the multilayer ceramic capacitor 10, a dielectric ceramic with a high dielectric constant is used to increase the capacitance of each ceramic layer 15 between the internal electrodes 12 and 13. Examples of dielectric ceramics with a high dielectric constant include materials with a perovskite structure containing barium (Ba) and titanium (Ti), such as barium titanate (BaTiO3).
[0027] In addition, the dielectric ceramics may be based on strontium titanate (SrTiO3), calcium titanate (CaTiO3), magnesium titanate (MgTiO3), calcium zirconate (CaZrO3), calcium zirconate titanate (Ca(Zr,Ti)O3), barium zirconate (BaZrO3), titanium oxide (TiO2), etc., in addition to barium titanate.
[0028] The protective portion 17 is also made of a dielectric ceramic. The material for forming the protective portion 17 may be any insulating ceramic, but by using a material with the same composition as that of the ceramic layer 15, the manufacturing efficiency is improved and the internal stress in the ceramic body 11 is suppressed.
[0029] Each of the external electrodes 14a, 14b has an undercoat film 21 formed so as to cover the end face 11a, and a plating film 22 formed on the undercoat film 21. The undercoat film 21 is formed, for example, of a baked film formed by baking a conductive paste, a sputtered film, or the like. The plating film 22 is a film formed by electrolytic plating. Each of the films of the external electrodes 14a, 14b is formed of a metal or an alloy containing, for example, nickel (Ni), copper (Cu), tin (Sn), palladium (Pd), platinum (Pt), silver (Ag), gold (Au), or the like as a main component.
[0030] The base film 21 of the external electrodes 14a, 14b has an end face covering portion 25 formed on the end face 11a, a main face covering portion 26c formed on the main face 11c, a side face covering portion 26b formed on the side face 11b, and a recess covering portion 27 formed on a recess 23 described below. In this embodiment, the end face covering portion 25 constitutes a first covering portion, the main face covering portion 26c and the side face covering portion 26b constitute a plurality of second covering portions, and the recess covering portion 27 constitutes a third covering portion.
[0031] This embodiment is characterized in that the side surface covering portion 26b and the main surface covering portion 26c of the base film 21 are separated from the recess covering portion 27 at the ridge portion 11e, and this discontinued portion is also covered with the plating film 22. The configuration in the vicinity of the ridge portion 11e will be described in detail below.
[0032] [Detailed structure of multilayer ceramic capacitor 10] Fig. 5 is an enlarged view of Fig. 4, showing the configuration of ridge 11e and its surroundings. Fig. 5 shows one ridge 11e and its surroundings, but the configurations of other ridges 11e and their surroundings are similar.
[0033] The ridge portion 11e has a recess 23 extending along the X-axis direction. An outwardly convex first ridge portion 24a is formed on the outer edge of the recess 23, on the cover portion 18 side, and constitutes a boundary with the main surface 11c. In addition, an outwardly convex second ridge portion 24b is formed on the outer edge of the recess 23, on the side margin portion 19 side, and constitutes a boundary with the side surface 11b. The first ridge portion 24a and the second ridge portion 24b are provided across the recess 23, and both extend along the X-axis direction.
[0034] When a straight line Le is drawn connecting the first ridge line 24a and the second ridge line 24b in a cross section cut in the Z-axis direction, specifically a cross section including the Z-axis direction and the Y-axis direction, the recess 23 is a portion recessed inward from the straight line Le into the ceramic body 11. Small steps or irregularities that do not protrude from the straight line Le may be formed inside the recess 23.
[0035] The first ridge portion 24a has an arc-shaped portion with a radius of curvature R1 in a cross section including the Z-axis direction and the Y-axis direction. The second ridge portion 24b has an arc-shaped portion with a radius of curvature R2 in a cross section including the Z-axis direction and the Y-axis direction. The radius of curvature R1 of the first ridge portion 24a is larger than the radius of curvature R2 of the second ridge portion 24b.
[0036] The radius of curvature R1 of the first ridge portion 24a can be set appropriately within a range of 15 μm to 25 μm. The radius of curvature R2 of the second ridge portion 24b can be set appropriately within a range of 0 μm to 20 μm. Although both ranges include overlapping ranges, the condition that the radius of curvature R1 of the first ridge portion 24a is larger than the radius of curvature R2 of the second ridge portion 24b is applied preferentially, and both values are set within a range that satisfies this condition. Note that the radius of curvature R2 of the second ridge portion 24b being 0 μm means that the second ridge portion 24b is at a right angle in a cross section including the Z-axis direction and the Y-axis direction.
[0037] Here, the measurement positions and the measurement method of the curvature radius R1 and the curvature radius R2 will be described with reference to Fig. 6(A) and Fig. 6(B). With reference to Fig. 6(A), the length of one of the external electrodes 14a in the direction along the X-axis is set to L[14a]. In this embodiment, the measurement positions of the curvature radius R1 and the curvature radius R2 are set to a position L[14a] / 2 from the end face of the external electrode 14a. Therefore, first, the multilayer ceramic capacitor 10 is polished from the end face of the external electrode 14a to a position L[14a] / 2 to expose the cross section. Then, the exposed cross section is photographed using an optical microscope.
[0038] Then, for the first ridgeline portion 24a and the second ridgeline portion 24b that appear in the photograph, the radii of curvature R1 and R2 can be measured using a virtual circle Vc, for example, as shown in FIG. 6B (first method). The radii of curvature R1 and R2 can be measured in a similar manner. Here, the measurement of the radius of curvature R1 of the first ridgeline portion 24a will be described. First, three points, a first point P1, a second point P2, and a third point P3, are set on the contour of the first ridgeline portion 24a that appears in the photograph. The first point P1 is set in the following manner. A virtual line L1 is set that extends in the Y-axis direction along the main surface 11c. The first point P1 is set at a position where the virtual line L1 is separated from the first ridgeline portion 24a. The second point P2 is set at the end of the first ridgeline portion 24a on the opposite side to the first point P1. The third point P3 is set at the vertex of the first ridge portion 24a. The vertex of the first ridge portion 24a (the third point P3) is identified as follows. A virtual line L2 is set that passes through the second point P2 and extends in the Z direction. The virtual lines L1 and L2 are perpendicular to each other. A virtual line L3 is set that passes through the intersection of the virtual lines L1 and L2 and has an angle of θ=45° from the virtual line L1. The intersection of the virtual line L3 and the contour of the first ridge portion 24a is identified as the vertex of the first ridge portion 24a, and the third point P3 is set at this point.
[0039] Then, a virtual circle Vc is set so that the degree of coincidence between the first point P1 to the third point P3 is equal to or greater than a predetermined value, and the radius of the virtual circle Vc is set as the radius of curvature R1. The radius of curvature R2 of the second ridge line portion 24b can be measured in a similar manner. In this case, the virtual line L1 is set so as to extend in the Y-axis direction from the first ridge line portion 24a side, and the second virtual line L2 is set so as to extend in the Z-axis direction along the side surface 11b.
[0040] The radius of curvature R1 and the radius of curvature R2 can also be measured by other methods. For example, as shown in Fig. 6(C), imaginary circles Vc of various radii Rn are superimposed on the contour of the first ridge line portion 24a and the contour of the second ridge line portion 24b. Then, when the degree of coincidence between the contour of the first ridge line portion 24a or the contour of the second ridge line portion 24b and the imaginary circle Vc is equal to or greater than a predetermined value, the radius of the imaginary circle Vc may be determined as the radius of curvature R1 and the radius of curvature R2 (second method).
[0041] The curvature radius R1 and the curvature radius R2 can be measured by either the first method or the second method described above. This embodiment includes both the case where the curvature radius R1 and the curvature radius R2 measured by the first method satisfy the above-mentioned relationship and the case where the curvature radius R1 and the curvature radius R2 measured by the second method satisfy the above-mentioned relationship. In other words, even if the curvature radius R1 and the curvature radius R2 measured by the first method satisfy the above-mentioned relationship but the curvature radius R1 and the curvature radius R2 measured by the second method do not satisfy the above-mentioned relationship, this embodiment is included. Conversely, the case where the curvature radius R1 and the curvature radius R2 measured by the first method do not satisfy the above-mentioned relationship but the curvature radius R1 and the curvature radius R2 measured by the second method satisfy the above-mentioned relationship is also included in this embodiment. Of course, the case where the curvature radius R1 and the curvature radius R2 measured by the first method satisfy the above-mentioned relationship and the curvature radius R1 and the curvature radius R2 measured by the second method satisfy the above-mentioned relationship is included in this embodiment.
[0042] Note that the measurement positions are just an example, and other positions along the X-axis direction may be used as the measurement positions, or multiple positions may be used as the measurement positions. When measurements are taken at multiple positions, the average value may be used.
[0043] As described above, the principal surface covering portion 26c of the base film 21 is formed on the principal surface 11c, and the side surface covering portion 26b of the base film 21 is formed on the side surface 11b. The recess covering portion 27 of the base film 21 is formed on the recess 23. The recess covering portion 27 is separated from at least one of the principal surface covering portion 26c and the side surface covering portion 26b at the ridge portion 11e. In this embodiment, the recess covering portion 27 is separated from both the principal surface covering portion 26c and the side surface covering portion 26b.
[0044] In this embodiment, the plating film 22 has a multi-layer structure. The plating film 22 has an intermediate film 28 formed on the base film 21, and a surface film 29 formed on the intermediate film 28. The intermediate film 28 and the surface film 29 continuously cover the entire end face covering portion 25, the main face covering portion 26c, the side face covering portion 26b, and the recess covering portion 27 of the base film 21. The metal materials constituting the intermediate film 28 and the surface film 29 may be the same or different. The metal material may be selected from, for example, copper, nickel, tin, or an alloy thereof.
[0045] The base film 21 has the main surface covering portion 26c, the side surface covering portion 26b, and the recess covering portion 27 that are spaced apart from one another, so that defects such as cracks in the ceramic body 11 caused by temperature changes can be prevented.
[0046] The electrode material constituting the base film 21 and the ceramic material constituting the ceramic body 11 have different linear expansion coefficients. As a result, when the base film 21 is cooled after baking or after heating after mounting, the base film 21 contracts more than the ceramic body 11, causing tensile stress in the base film 21. Meanwhile, compressive stress due to the tensile stress is caused in the ceramic body 11.
[0047] For example, a tensile stress directed inward in the Y-axis direction is generated in the main surface covering portion 26c of the base film 21. For example, a tensile stress directed inward in the Z-axis direction is generated in the side surface covering portion 26b of the base film 21. As a result, tensile stresses directed in different directions are generated in the base film 21 near the ridge portion 11e.
[0048] In this embodiment, the main surface covering portion 26c and the side surface covering portion 26b are spaced apart from each other. This prevents stress from accumulating in the base film 21 even when the tensile stress is generated. This prevents large compressive stress from being generated in the ceramic body 11, thereby preventing defects such as cracks from occurring in the ceramic body 11.
[0049] Furthermore, in this embodiment, a recess covering portion 27 is formed on the recess 23. The recess covering portion 27 allows the electrode material of the base film 21 to remain within the recess 23, and the separation width between the base films 21 can be minimized.
[0050] In this embodiment, the electrode material remaining in the recess 23 forms the recess covering portion 27. This restricts the distance between the recess covering portion 27 and the main surface covering portion 26c or the side surface covering portion 26b in the base film 21, and allows the plating film 22 to continuously cover the entire base film 21. This prevents gaps from occurring between the external electrodes 14a, 14b and the ceramic body 11, and prevents insulation failure. This improves the reliability of the multilayer ceramic capacitor 10.
[0051] Here, the effect of setting the radius of curvature R1 of the first ridgeline portion 24a larger than the radius of curvature R2 of the second ridgeline portion 24b will be described in comparison with a comparative example. Fig. 7(A) is a partially enlarged cross-sectional view showing the periphery of one first ridgeline portion 24a and one second ridgeline portion 24b, and Fig. 8(A) is a cross-sectional view of the multilayer ceramic capacitor 10 of the embodiment. Fig. 7(B) is a partially enlarged cross-sectional view showing the periphery of one first ridgeline portion 224a and one second ridgeline portion 224b, and Fig. 8(B) is a cross-sectional view of the multilayer ceramic capacitor 50 of the comparative example.
[0052] The laminated ceramic capacitor 50 of the comparative example includes a ridge portion 51e, similar to the laminated ceramic capacitor 10 of the embodiment. The laminated ceramic capacitor 50 also includes a cover portion 58 and a side margin portion 59 around the capacitance forming portion 56. The ridge portion 51e has a recess 53 extending along the X-axis direction. A first ridge portion 224a is provided on the cover portion 58 side at the outer edge of the recess 53, and constitutes a boundary portion with the main surface 51c, and is outwardly convex. A second ridge portion 224b is provided on the side margin portion 59 side at the outer edge of the recess 53, and constitutes a boundary portion with the side surface 51b, and is outwardly convex. The first ridge portion 224a and the second ridge portion 224b are provided across the recess 53, and both extend along the X-axis direction.
[0053] The first ridge portion 224a has an arc-shaped portion in a cross section including the Z-axis direction and the Y-axis direction. The second ridge portion 24b has an arc-shaped portion in a cross section including the Z-axis direction and the Y-axis direction. The radius of curvature of the first ridge portion 24a and the radius of curvature of the second ridge portion 24b are approximately the same. This is different from the multilayer ceramic capacitor 10 of the embodiment.
[0054] 7(A) shows a schematic diagram of the force propagation when an impact force is applied to the ridge 11e of the multilayer ceramic capacitor 10 of the embodiment. The radius of curvature R1 of the first ridge 24a and the radius of curvature R2 of the second ridge 24b are different. Therefore, the first ridge 24a and the second ridge 24b are subjected to impact forces in different directions. Therefore, it is expected that the impact force propagated to the inside of the ceramic body 11 is offset within the ceramic body 11. As a result, the impact force directed toward the capacitance forming portion 16 is mitigated.
[0055] 7(B) is a schematic diagram showing how force is propagated when an impact force is applied to the ridge 51e of the multilayer ceramic capacitor 50 of the comparative example. The radius of curvature R of the first ridge 224a and the second ridge 224b are substantially the same. Therefore, the input direction of the impact force is substantially the same for the first ridge 224a and the second ridge 224b. Therefore, unlike the multilayer ceramic capacitor 10 of the embodiment, it is considered that the effect of canceling out the impact force propagated inside the ceramic body 51 within the ceramic body 51 is low.
[0056] 8A shows an angle θ1 between a tangent line connecting the first ridgeline 24a and the second ridgeline 24b and a line segment extending from the main surface 11c of the ceramic body 11 along the Y-axis direction. Also shown is a height t1 from the main surface 11c, which is the mounting surface of the multilayer ceramic capacitor 10, to the second ridgeline 24b. Referring to FIG. 8B, for the comparative example, an angle θ2 between a tangent line connecting the first ridgeline 224a and the second ridgeline 224b and a line segment extending from the main surface 51c of the ceramic body 51 along the Y-axis direction is also shown. Also shown is a height t2 between the main surface 41c, which is the mounting surface of the multilayer ceramic capacitor 50, and the second ridgeline 224b.
[0057] The angle θ1 is smaller than the angle θ2, and the height t1 is smaller than the height t2. Therefore, the multilayer ceramic capacitor 10 of the embodiment is less likely to tip over during mounting than the multilayer ceramic capacitor 50 of the comparative example.
[0058] In the multilayer ceramic capacitor 10 of this embodiment, the radius of curvature R1 of the first ridge portion 24a is larger than the radius of curvature R of the second ridge portion 24b. If the radius of curvature R2 of the second ridge portion 24b were made larger than the radius of curvature R1 of the first ridge portion 24a, the region in the side margin portion 19 where the thickness is thin would expand. This is because, as the radius of curvature increases, the chamfered region becomes wider and the drawn arc approaches the inside of the ceramic body 11. To avoid this in this embodiment, the radius of curvature R1 is made larger than the radius of curvature R2.
[0059] [Method of manufacturing multilayer ceramic capacitor 10] Fig. 9 is a flowchart showing a method for manufacturing the multilayer ceramic capacitor 10. Figs. 10 to 17 are diagrams that typically show the manufacturing process of the multilayer ceramic capacitor 10. The method for manufacturing the multilayer ceramic capacitor 10 will be described below along Fig. 9 with appropriate reference to Figs. 10 to 17.
[0060] (Step S01: Fabrication of ceramic laminated chip C) In step S01, the ceramic sheets 101 and 102 for forming the capacitance forming portion 16 and the ceramic sheet 103 for forming the cover portion 18 are laminated and cut to produce an unfired ceramic laminated chip (laminated chip) C.
[0061] 10 are configured as unfired dielectric green sheets containing a ceramic material made of dielectric ceramics, an organic binder, and other additives. An unfired first internal electrode 112 corresponding to the first internal electrode 12 is formed on the ceramic sheet 101. An unfired second internal electrode 113 corresponding to the second internal electrode 13 is formed on the ceramic sheet 102. No internal electrodes are formed on the ceramic sheet 103.
[0062] Each of the internal electrodes 112, 113 has a plurality of strip-shaped electrode patterns that cross a cutting line Lx parallel to the X-axis direction and extend along a cutting line Ly parallel to the Y-axis direction. These internal electrodes 112, 113 are formed by applying a conductive paste to the ceramic sheets 101, 102 by a printing method or the like.
[0063] The ceramic sheets 101 and 102 are alternately stacked in the Z-axis direction as shown in Fig. 10. The stack of the ceramic sheets 101 and 102 corresponds to the capacitance forming portion 16 and the end margin portion 20. The ceramic sheet 103 is stacked on the top and bottom surfaces in the Z-axis direction of the stack of the ceramic sheets 101 and 102. The stack of the ceramic sheets 103 corresponds to the cover portion 18. The number of stacked ceramic sheets 101, 102, and 103 can be adjusted as appropriate.
[0064] Next, the laminate of the ceramic sheets 101, 102, and 103 is pressed from the Z-axis direction and cut along the cutting lines Lx and Ly, thereby producing the laminated chip C shown in FIG.
[0065] The laminated chip C has an unsintered capacitance forming portion 116 on which unsintered internal electrodes 112, 113 are formed, an unsintered cover portion 118, and an unsintered end margin portion 120. The laminated chip C has a side surface Cb which is a cut surface corresponding to the cutting line Lx, and an end surface Ca which is a cut surface corresponding to the cutting line Ly. Ends of the unsintered internal electrodes 112, 113 are exposed from the side surface Cb.
[0066] (Step S02: Forming the first ridge line portion 124a) In step S02, a first ridge portion 124a is formed on an edge portion connecting the side surface Cb and the main surface Cc of the laminated chip C. The first ridge portion 124a corresponds to the first ridge portion 24a after firing, and is machined into an arc shape so that the first ridge portion 24a has a radius of curvature R1 after firing. In this embodiment, chamfering is performed by blasting using a nozzle 40 to form the first ridge portion 124a. Note that other conventionally known techniques may be used as long as they can realize the first ridge portion 24a having the desired arc shape.
[0067] (Step S03: Forming side margin portion 119) In step S03, side margin portions 119 are formed on the side surfaces Cb of the stacked chips C. An example of a forming method will be described below.
[0068] First, as shown in Figure 13, a laminated sheet S, which is a laminate of ceramic sheets, is placed on a flat elastic member E, and the other side Cb of a laminated chip C, one side Cb of which is held by tape T, is placed opposite the laminated sheet S.
[0069] In this embodiment, the laminated sheet S has a laminated structure of a first ceramic sheet 104, a second ceramic sheet 105, and a third ceramic sheet 106 for forming side margins. Each of the ceramic sheets 104, 105, and 106 contains a ceramic material, an organic binder, and other additives, similar to the ceramic sheets 101, 102, and 103.
[0070] The second ceramic sheet 105 has a larger thermal shrinkage rate than the first ceramic sheet 104. Furthermore, the third ceramic sheet 106 has a larger thermal shrinkage rate than the second ceramic sheet 105. The thermal shrinkage rate can be adjusted by adjusting the amount of the organic binder and additives.
[0071] Next, as shown in Fig. 14, the laminate sheet S is punched out at the side Cb of the laminate chip C, thereby attaching the laminate sheet S to the side Cb. Specifically, the laminate chip C is strongly pressed in the Y-axis direction against the laminate sheet S. This causes the laminate chip C and the laminate sheet S to locally sink deeply into the elastic member E. At this time, a shear force acts on the laminate sheet S along the outer edge of the side Cb, and when this shear force exceeds the shear strength of the laminate sheet S, the laminate sheet S is punched out.
[0072] 15, a part of the laminated sheet S that has sunk together with the laminated chip C is cut off. As a result, a first side margin portion 119a is formed on the side surface Cb, and a second side margin portion 119b is formed on the first side margin portion 119a. Furthermore, in this embodiment, a third side margin portion 119c is formed on the second side margin portion 119b. As a result, an unfired side margin portion 119 including the first side margin portion 119a, the second side margin portion 119b, and the third side margin portion 119c is formed on the side surface Cb of the laminated chip C.
[0073] Then, a side margin 119 is formed in the same manner on the other side surface Cb. In this manner, the unsintered ceramic body 111 shown in Fig. 16 is produced. At this stage, the recess 23 is not formed in the ridge portion 111e between the main surface 111c and the side surface 111b.
[0074] (Step S04: Firing) In step S04, the ceramic body 111 obtained in step S03 is fired to produce the ceramic body 11 of the multilayer ceramic capacitor 10 shown in Fig. 17 and Figs. 1 to 3. The firing temperature in step S04 can be determined based on the sintering temperature of the ceramic body 111. Furthermore, the firing can be performed, for example, in a reducing atmosphere or a low oxygen partial pressure atmosphere.
[0075] By firing, each of the side margins 119a, 119b, and 119c thermally shrinks at a different rate. Specifically, the second side margin 119b shrinks by a larger amount than the first side margin 119a. The third side margin 119c shrinks by a larger amount than the second side margin 119b.
[0076] 17, a gentle step or slope is formed on ridge portion 11e of the ceramic body 11. The outer edges of each of the side margin portions 119a, 119b, 119c contract inwardly in the Z-axis direction, in this order, to form a recess 23. The outer edge of the third side margin portion 119c forms a second ridge portion 24b.
[0077] By setting the thermal shrinkage rate of the third side margin portion 119c, the radius of curvature R2 of the second ridge portion 24b formed after firing can be adjusted to a desired value. In addition, in order to realize the desired radius of curvature R2, the second ridge portion 24b after firing may be chamfered. The chamfering may be performed by a blasting method or a conventionally known method. When the second ridge portion 24b is processed, the processing may affect the first ridge portion 24a. For this reason, the chamfering of the first ridge portion 24a in step S02 can be performed while taking into consideration the effect of the processing on the second ridge portion 24b. In addition, the chamfering of the second ridge portion 24b may be performed before firing.
[0078] In FIG. 17, the regions of the side margin 19 corresponding to the side margins 119a, 119b, and 119c are indicated by dashed lines, but the boundaries become almost invisible after firing.
[0079] (Step S05: Forming the base film) In step S05, a conductive base film 21 is formed, which includes an end face covering portion 26a formed on the end face 11a, a side face covering portion 26b formed on the side face 11b, a main face covering portion 26c formed on the main face 11c, and a recess covering portion 27 formed on the recess 23 and spaced apart from the side face covering portion 26b and the main face covering portion 26c, respectively.
[0080] Specifically, first, the unsintered electrode material is applied to the end face 11a, and then the unsintered electrode material is also applied to the side face 11b, the main face 11c, and a part of the ridge portion 11e connected to the end face 11a. The application method is, for example, a dipping method. In the dipping method, the end face 11a side of the ceramic body 11 is immersed in a dipping bath containing an electrode material such as a conductive paste. This allows the unsintered electrode material to be applied to the side face 11b, the main face 11c, and the recess 23 almost simultaneously with the end face 11a.
[0081] The unsintered electrode material is applied thinly so that the recess covering portion 27, the side covering portion 26b, and the main surface covering portion 26c are spaced apart from each other after baking. However, they do not have to be spaced apart at the time of application. The thickness of the electrode material application can be adjusted by the immersion time, the pull-up speed, the viscosity of the electrode material, etc.
[0082] The method for forming the undercoat film is not limited to the dipping method, but may be, for example, a printing method, a sputtering method, or a combination of these methods.
[0083] Next, the unsintered electrode material is baked. The baking can be performed, for example, in a reducing atmosphere or a low oxygen partial pressure atmosphere. During baking, the electrode material formed on each surface shrinks due to heat. The shrinkage rate of the electrode material is greater than that of the ceramic body 11. Therefore, the electrode material applied to each surface generates tensile stress in a direction away from the ridge portion 11e. As a result, the recess covering portion 27, the side surface covering portion 26b, and the main surface covering portion 26c are formed to be separated from each other.
[0084] (Step S06: Plating film formation) In step S06, a plating film 22 is formed to continuously cover the end face covering portion 26a, the side face covering portion 26b, the main face covering portion 26c, and the recess covering portion 27. Specifically, the multilayer ceramic capacitor 10 on which the base film 21 has been formed is immersed in plating solutions corresponding to the intermediate film 28 and the surface film 29, respectively, to perform electrolytic plating. As a result, the plating film 22 having multiple layers of the intermediate film 28 and the surface film 29 is formed.
[0085] 1 to 3 is manufactured. In this embodiment, the side margin portion 119 is later attached to the laminated chip C, so that the positions of the ends of the internal electrodes 112, 113 are aligned to within a range of 0.5 μm in the Y-axis direction. This increases the proportion of the volume of the capacitance forming portion 16 in the ceramic body 11, and enables the capacitance to be increased without increasing the size of the laminated ceramic capacitor 10.
[0086] [Other embodiments] Although each embodiment of the present invention has been described above, the present invention is not limited to the above-described embodiments, and it is needless to say that various modifications can be made without departing from the spirit of the present invention.
[0087] The number of ceramic sheets forming each side margin portion 19 is not limited to three. For example, by forming the side margin portion 19 using two or more and four or less ceramic sheets, the recess 23 can be formed in a desired shape and problems such as peeling of the side margin portion 19 after attachment can be prevented.
[0088] For example, in the above embodiment, the unfired side margin portion 119 is formed by attaching the laminated sheet S in which different ceramic sheets are laminated, but a plurality of ceramic sheets may be attached one by one.
[0089] Furthermore, the method of attaching the ceramic sheet is not limited to punching a sheet, and a ceramic sheet that has been pre-cut to a predetermined size may be attached to the side surface Cb.
[0090] Alternatively, the side margin portion 19 may be formed by applying layers of ceramic materials having different thermal shrinkage rates to the side surface Cb of the laminated chip C. This also makes it possible to form a laminated structure of multiple side margin portions having different thermal shrinkage rates.
[0091] Also, the recess can be formed by forming the cover 18 from multiple ceramic sheets with different thermal shrinkage rates. In this case, multiple ceramic sheets with side margins formed around the internal electrodes are stacked, and multiple ceramic sheets with gradually increasing thermal shrinkage rates are stacked above and below in the Z-axis direction. This forms a ridge including a recess on the outer edge of the ceramic sheet for forming the cover.
[0092] Furthermore, the method of forming the recesses is not limited to the thermal contraction of the ceramic material, and the recesses may be formed by grinding the ridges of a ceramic body formed in a rectangular parallelepiped shape.
[0093] Moreover, the multilayer ceramic capacitor can be a so-called tall type, in which the dimension along the Z-axis direction is greater than the dimension along the Y-axis direction. EXAMPLES
[0094] Next, the results of the impact test on the examples will be described together with the comparative examples. The examples correspond to the multilayer ceramic capacitor 10 of the embodiment and have the dimensions shown below. The comparative examples are multilayer ceramic capacitors 50 such as those shown in Fig. 7(B) and Fig. 8(B) and have the dimensions shown below.
[0095] The conditions for the impact test are shown below. Equipment (test equipment): IMY Co., Ltd. i220 Test Method: The test item (multilayer ceramic capacitor) is placed in a specified plastic case and vibrated. Test item dimensions: 0603 (length x width x height = 0.6 mm x 0.3 mm x 0.3 mm) Number of test subjects: 7,000 pieces (assuming 0603 shape) Vibration Frequency: 10Hz Number of cycles: 600 times Evaluation method: Visual evaluation using a stereo microscope (n=100 pieces)
[0096] The test results are shown in Figure 18. The crack occurrence rate in the example was about 3%. In contrast, the crack occurrence rate in the comparative example was about 15%. Thus, the example has higher reliability against impact than the comparative example.
[0097] Each test subject used in the test is subjected to an impact by vibrating. In the comparative example, the direction of the impact force input from the first ridge portion 124a and the second ridge portion 124b is roughly the same. Therefore, it is considered that the impact force is not dispersed but is easily propagated in the direction where the capacitance forming portion 56 exists (see FIG. 8(B)). As a result, it is considered that the crack occurrence rate is high. On the other hand, in the example, the direction of the impact force input from the first ridge portion 24a and the second ridge portion 24b is different. Therefore, it is considered that the impact forces are offset, and the impact force propagated in the direction where the capacitance forming portion 16 exists is mitigated (see FIG. 8(A)). As a result, it is considered that the crack occurrence rate is low.
[0098] Thus, it was confirmed that the embodiment had higher reliability against impact than the comparative example.
[0099] In the above embodiment, the multilayer ceramic capacitor 10 has been described as an example of a multilayer ceramic electronic component, but the present invention is applicable to all multilayer ceramic electronic components in which ceramic layers and internal electrodes are laminated. Examples of such multilayer ceramic electronic components include chip varistors, chip thermistors, and multilayer inductors. [Explanation of symbols]
[0100] 10...Multilayer ceramic capacitor 11…Ceramic body 11a...end face 11b...side 11c…main surface 11e…Ridge 12,13…Internal electrode 14a,14b...External electrode 21...Base film 22...Plating film 23…Recess 24a…First ridgeline part 24b…Second ridgeline part 25...First covering part (end face covering part) 26b, 26c...Second covering part (side covering part, main surface covering part) 27...Third covering portion (recess covering portion)
Claims
1. a ceramic body including a protective portion including an end surface facing a first direction, a plurality of peripheral surfaces connected to the end surface and extending in the first direction, and a ridge portion having a recess extending along the first direction and connecting the plurality of peripheral surfaces, and a functional portion disposed inside the protective portion; an external electrode having an undercoat film covering the end surface and a plating film formed on the undercoat film; Equipped with the functional portion has a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, the protective portion includes a cover portion laminated on the functional portion along the second direction, and a side margin portion covering the functional portion from a third direction perpendicular to the first direction and the second direction, The ridge portion includes a first ridge portion provided on the cover portion side and a second ridge portion provided on the side margin portion side across the recess, In a cross section including the second direction and the third direction, a radius of curvature R1 of the first ridge line portion is larger than a radius of curvature R2 of the second ridge line portion. Multilayer ceramic electronic components.
2. 2. The multilayer ceramic electronic component according to claim 1, a dimension of the multilayer ceramic electronic component in the second direction is larger than a dimension of the multilayer ceramic electronic component in the third direction; Multilayer ceramic electronic components.
3. 2. The multilayer ceramic electronic component according to claim 1, The radius of curvature R1 of the first ridge line portion is 15 μm or more and 25 μm or less. Multilayer ceramic electronic components.
4. 2. The multilayer ceramic electronic component according to claim 1, The radius of curvature R2 of the second ridge line portion is 0 μm or more and 20 μm or less. Multilayer ceramic electronic components.
5. 2. The multilayer ceramic electronic component according to claim 1, The undercoat film is a first covering portion formed on the end surface, a plurality of second covering portions formed on the plurality of peripheral surfaces, respectively, and a third covering portion formed on the recess and spaced apart from at least one of the plurality of second covering portions, The plating film continuously covers the first covering portion, the plurality of second covering portions, and the third covering portion. Multilayer ceramic electronic components.
6. 2. The multilayer ceramic electronic component according to claim 1, the functional portion has a plurality of internal electrodes stacked in a second direction perpendicular to the first direction, The internal electrodes have ends aligned in a third direction perpendicular to the first and second directions, the ends being aligned to within a range of 0.5 μm in the third direction. Multilayer ceramic electronic components.
7. a ceramic laminated chip is fabricated, the ceramic laminated chip having a functional section having an end face facing a first direction, a plurality of internal electrodes laminated in a second direction perpendicular to the first direction, the plurality of internal electrodes being exposed from a side surface facing a third direction perpendicular to the first direction and the second direction, and a cover section laminated on the functional section along the second direction; a first ridge portion is formed to connect a peripheral surface that is connected to the end surface and extends in the first direction and the side surface; forming a side margin portion including a second ridge portion laminated on the side surface, extending along the first direction, and disposed parallel to the first ridge portion across a recess, thereby producing a ceramic body; The ceramic laminated chip and the side margin portion are fired, forming an external electrode having an undercoat film covering the end surface and a plating film formed on the undercoat film; the step of forming the first ridge line portion includes chamfering such that a radius of curvature R1 of the first ridge line portion is larger than a radius of curvature R2 of the second ridge line portion in a cross section including the second direction and the third direction; A method for manufacturing multilayer ceramic electronic components.
8. 8. A method for producing a multilayer ceramic electronic component according to claim 7, comprising the steps of: In the step of forming the external electrode, a conductive base film is formed including a first covering portion formed on the end face of the ceramic body, a plurality of second covering portions formed on a plurality of peripheral surfaces connected to the end face and extending in the first direction, and a third covering portion formed on the recess and spaced apart at an edge from at least one of the plurality of second covering portions; forming a plating film continuously covering the first covering portion, the plurality of second covering portions, and the third covering portion; A method for manufacturing multilayer ceramic electronic components.
9. 8. A method for producing a multilayer ceramic electronic component according to claim 7, comprising the steps of: In the step of forming the side margin portion, a first side margin portion laminated on the side surface and a second side margin portion laminated on the first side margin portion and having a thermal shrinkage rate larger than that of the first side margin portion are formed. A method for manufacturing multilayer ceramic electronic components.
10. 10. A method for producing a multilayer ceramic electronic component according to claim 9, comprising the steps of: the first side margin portion is formed by attaching a first ceramic sheet onto the side surface, The second side margin portion is formed by attaching a second ceramic sheet having a larger thermal shrinkage rate than the first ceramic sheet onto the first ceramic sheet. A method for manufacturing multilayer ceramic electronic components.
Citation Information
Patent Citations
Multilayer ceramic capacitor and manufacturing method for the same
JP2012191159A