Coating method using coating roller

The described coating method using a paint roller with specific fiber composition and paint properties addresses the inefficiencies of existing roller-based paint compositions by achieving a uniform and smooth coating film with improved flatness and finish, enhancing efficiency and reducing environmental impact.

JP2024147905APending Publication Date: 2024-10-17KIKUSUI CHEM IND CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023060640
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-04
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

Existing aqueous paint compositions using a coating roller struggle to form thick coating films efficiently and uniformly, often requiring multiple applications and resulting in an inferior finish compared to spray painting.

Method used

A coating method using a paint roller with a knitted fabric made of cotton-like pile fibers, a specific Ti value range of 2 to 10, and a paint solid content of 10.0 to 80.0% by weight, along with a paint composition containing fillers with a particle size of 1.0 to 800.0 μm, ensures uniform and efficient coating film formation.

Benefits of technology

The method allows for a uniform and smooth coating film with improved flatness and finish, reducing the need for multiple applications and minimizing paint waste, while maintaining environmental cleanliness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147905000001
    Figure 2024147905000001
Patent Text Reader

Abstract

To provide a coating method using a coating roller capable of efficiently obtaining a uniform coated film with ease even when using the coating roller, and also making an underlayer shape flat.SOLUTION: In the case of applying a coating material having a coating material Ti value within a range of 2-10 and a coating material solid portion within a range of 10.0-80.0 weight% to a coating object with a coating roller, a coating part of the coating roller is formed of a knitted fabric obtained by knitting a cotton-like pile which is a fiber aggregate with a backing fabric. The coating roller has a coating material content amount of 0.5-3.0 g / cm3. Since coating is performed by using the coating roller whose bristle length is within a range of 5-32 mm, it is possible to efficiently obtain a uniform film with ease and making an underlayer shape flat even when using the coating roller.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a coating method for the wall surfaces of architectural structures and the like using a coating composition such as a paint or coating material, and in particular to a coating method using a coating roller. [Background technology]

[0002] When painting the walls of buildings and structures, spray painting is often done using a spray gun, which makes it possible to obtain a beautiful painted wall surface that matches the surface shape of the wall, etc. For example, on smooth surfaces, it is possible to form a flat coating of uniform thickness. Spray painting is a method of painting that uses air pressure to spray paint, which makes the painting process quick and produces a good finish. However, because paint tends to scatter, this can have an adverse effect on the working environment and the surrounding area.

[0003] In addition, paint may be wasted. Furthermore, the finish may vary depending on the skill of the painter. Therefore, in recent years, painting with a paint roller has become more common instead of spray painting. This has significantly reduced paint scattering during painting work and greatly reduced paint waste. However, the finish may be inferior to that of spray painting.

[0004] There are many different types of painting rollers available, and they can be selected based on the amount of paint to be applied and the finish of the coating film formed. For this reason, an aqueous paint composition such as that described in Patent Document 1, JP 2019-135282 A, has been proposed.

[0005] Prior Art 1 describes an aqueous coating composition which contains (a) a synthetic resin emulsion, (b) mica having an average particle size of 0.3 to 3 mm, and (c) calcium carbonate having an average particle size of 0.1 to 0.5 mm, in which the content of component (b) is 3 to 30 parts by mass and the content of component (c) is 20 to 100 parts by mass per 100 parts by mass of the solid content in component (a), and which has a viscosity of 1,000 to 100,000 mPa s measured using a B-type viscometer at a rotation speed of 20 rpm and a coating temperature of 25°C, and a Ti value (viscosity at a rotation speed of 2 rpm and a coating temperature of 25°C / viscosity at a rotation speed of 20 rpm and a coating temperature of 25°C) of 2 to 8.

[0006] As a result, by containing a synthetic resin emulsion, mica having a specified average particle size, and calcium carbonate in specified concentrations, it is possible to form a uniform coating film with excellent workability when roller-applied using a medium-pile roller, etc. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2019-135282 A Summary of the Invention [Problem to be solved by the invention]

[0008] However, while the aqueous coating composition in Patent Document 1 provides a good finish by containing mica having a specified average particle size and calcium carbonate at specified concentrations, multiple coats are required to form a thick coating film, which may hinder efficient coating operations. The present disclosure aims to provide a coating method using a coating roller that can easily and efficiently obtain a uniform coating film and can keep the shape of the base flat, even when a coating roller is used. [Means for solving the problem]

[0009] In the case where a paint having a Ti value of 2 to 10 and a paint solid content of 10.0 to 80.0% by weight is applied to an object to be coated with a coating roller, the coating part of the coating roller is made of a knitted fabric in which a cotton-like pile, which is an aggregate of fibers, is woven together with a backing, and the coating amount of the coating roller is 0.5 to 3.0 g / cm 3 The coating is carried out using a coating roller having a bristle length in the range of 5 to 32 mm.

[0010] This makes it possible to easily and efficiently obtain a uniform coating film even when using a painting roller, and to keep the base surface flat. The specific gravity of the paint is in the range of 0.8 to 2.5, the content of fillers contained in the paint is in the range of 10.0 to 70.0 weight %, and the particle size is in the range of 1.0 to 800.0 μm, so that the finish becomes more uniform and smooth.

[0011] By having the coating film formed by painting be in the range of 30 to 1000 μm, a more uniform and smooth coating film can be obtained, resulting in a good finish. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] An embodiment of the present disclosure will be described. The present disclosure relates to a method for coating a substrate with a coating material having a Ti value of 2 to 10 and a coating material solid content of 10.0 to 80.0% by weight using a coating roller, the coating portion of the coating roller being made of a backing having warp and weft threads crossed at right angles and having thread-like pile woven into it, and the coating material load of the coating roller being 0.5 to 3.0 g / cm 3 The coating is performed using a coating roller having a bristle length in the range of 5 to 32 mm.

[0013] First, the paint used in the present disclosure is a paint generally used in painting operations, and is mainly composed of a binder component such as an organic binder, such as synthetic resin, or an inorganic binder, such as cement. Types of paint include topcoat paints such as clear paint, enamel paint, and matte paint, as well as primers and sealers, which are undercoat paints with relatively low paint viscosity.

[0014] There are also paints that form coatings with an average thickness of about 0.5 to 2.0 mm, such as undercoat paints and base conditioners. The present disclosure provides a method for easily and efficiently obtaining a uniform coating film and making it possible to make the base shape flat; in particular, even when using a paint that forms a coating film of a certain thickness, such as an undercoat paint or a base adjuster, a uniform coating film can be easily and efficiently obtained.

[0015] This base conditioner is applied to make the unevenness of the base surface less noticeable. Mid-coat paints are often applied to give a shape to the surface to be painted, and include paints for applying patterns. They are selected appropriately according to the application. Many of the binder components are made of synthetic resins, and paints that contain them as their main component are applied to substrates and other objects to be coated, and then allowed to harden and dry to form a coating film that covers the object.

[0016] Synthetic resins include acrylic resin, silicone resin, acrylic silicone resin, fluororesin, polyurethane resin, styrene resin, epoxy resin, melamine resin, alkyd resin, polyvinyl chloride resin, vinyl acetate resin, polyester resin, polyether resin, phenolic resin, and ketone resin. In many cases, synthetic resin emulsions are used, in which these synthetic resins are dispersed in water. Paints using these synthetic resin emulsions are water-based paints, which use water as a solvent, and are therefore preferred in terms of ease of handling and workability.

[0017] These synthetic resins may be used alone or in combination of two or more kinds. The monomers constituting these resins are generally used alone or in copolymer form. Among the synthetic resin emulsions using these synthetic resins, acrylic synthetic resin emulsions, acrylic styrene synthetic resin emulsions, acrylic silicone synthetic resin emulsions, and urethane synthetic resin emulsions, which have good water resistance, are preferably used.

[0018] In addition to their water resistance, these synthetic resin emulsions are also suitable for use in terms of paint suitability, coating film properties, ease of availability, etc. In addition to synthetic resins, these paints often contain additives, pigment components, fillers, fibers, etc. that are used in regular paints as necessary. These additives include surfactants used as defoamers, dispersants, and wetting agents, high-boiling point solvents used as film-forming aids and antifreeze agents, thickeners for adjusting viscosity, leveling agents, preservatives, anti-algae agents, anti-fungal agents, antibacterial agents, pH adjusters, crosslinking agents, and silane coupling agents.

[0019] The pigment components include white pigments such as titanium oxide and zinc oxide, inorganic pigments such as iron oxide, and color pigments such as organic pigments. Fillers include extender pigments such as calcium carbonate, kaolin, talc, clay, aluminum hydroxide, bentonite, white carbon, and precipitated barium sulfate.

[0020] In addition, aggregates such as silica sand and kansui sand can be added, as well as lightweight aggregates such as zeolite and perlite. In addition to inorganic aggregates, organic aggregates can also be used, and fibers can also be added. These pigment components, fillers and aggregates may be used alone or in combination of two or more kinds.

[0021] It is preferable to incorporate these fillers, and the content is preferably within the range of 10.0 to 70.0% by weight. If the content of these fillers is within the range, the paint will shrink less when it dries, the finish will be more uniform and smooth, an appropriate film thickness can be ensured, and the physical properties of the paint film, such as weather resistance, will be good, making it easy to apply.

[0022] A more preferable range is 10.0 to 50.0% by weight, and within this range, a more uniform and smooth finish can be achieved, an appropriate film thickness can be ensured, and a good coating film can be obtained. In addition, the particle size is preferably in the range of 1.0 to 800.0 μm. If it is smaller than 1.0 μm, the specific surface area of ​​the fillers becomes large, making it difficult to apply the fillers with a painting roller as described below, and it may be difficult to form a flat painted surface.

[0023] If the particle size is larger than 800.0 μm, it may be difficult to obtain a flat coating film due to the influence of the filler, and coating may be difficult because the coating roller described below may become clogged or the coating roller may not be able to hold the coating. The thickness is preferably in the range of 1.0 to 100.0 μm. If a coating material within this range is used, a flat coating film of uniform thickness with few cracks can be formed, and a beautiful coated wall surface can be obtained.

[0024] The paint is composed of the constituent materials as described above, and the Ti value of the paint must be in the range of 2 to 10, and the paint solids content must be in the range of 10.0 to 80.0. The Ti value of this paint indicates the thixotropy, which is the viscosity of the paint, and is calculated by using a B-type viscometer to determine the ratio of apparent viscosities at two rotational speeds. The formula for calculating the Ti value is shown below.

[0025] Ti value = viscosity at low rotation speed / viscosity at 10 times higher rotation speed The measurement conditions were 23° C. and the measurements were taken after rotating for 60 seconds.

[0026] When the Ti value is 1, the paint is a Newtonian fluid, and the degree of thixotropy increases as the Ti value increases above 1. If the Ti value is within this range, there is little dripping of the paint when applied, the evenness of the coating film is not impaired, and the storage stability of the paint is good. By keeping the solids content of the coating material within this range, shrinkage of the coating material during drying is small, and the flatness of the coating film is not impaired.

[0027] It is preferable that this Ti value is in the range of 2 to 7. If it is lower than 2, when applied to a vertical surface, the paint may drip before drying, which may prevent the formation of a uniform coating film, and the coating film may become too thin in some places. If it is higher than 7, it may be difficult to apply the paint and a flat coating may not be obtained.

[0028] When the paint is an undercoat paint or a paint for adjusting the base, the Ti value is preferably in the range of 4 to 7. Within this range, a relatively large amount of paint can be held on the painting roller, making it possible to paint efficiently, and the paint is easy to apply and can keep the base shape flat. The viscosity of the coating material is preferably in the range of 0.5 to 10.0 Pa·s. This viscosity is measured using a B-type viscometer in the same manner as in determining the Ti value, and the measurement conditions are 23° C., No. 3 rotor, 20 rpm, and 60 seconds.

[0029] If the viscosity is lower than 0.5 Pa·s, the paint will be easy to apply, but when applied to a vertical surface, it may be prone to dripping and may not produce a stable finish, such as a flat coating. If the viscosity is higher than 10.0 Pa·s, the paint workability with a paint roller will decrease, the thickness of the paint film will become uneven, and the finish will not be stable.

[0030] In the case of an undercoat paint or a paint for adjusting the base, the paint viscosity is preferably in the range of 0.8 to 10.0 Pa s. If the viscosity is within this range, a large amount of paint can be held on the painting roller, making painting work more efficient and producing a relatively flat, uniform coating. The paint solids content is in the range of 10.0 to 80.0% by weight, and being within this range makes it possible to easily and efficiently obtain a uniform coating film and to keep the base surface in a flat state.

[0031] If the content is lower than 10.0% by weight, the coating film may become thin and show through, depending on the type of object to be coated, whereas if the content is higher than 80.0% by weight, coating may become difficult and a coating film of relatively uniform thickness may not be obtained. Furthermore, in the case of an undercoat paint or a paint for adjusting the base, the range of 30.0 to 80.0% by weight is preferable. Within this range, painting work can be carried out more efficiently, and a relatively flat coating film can be obtained on a smooth surface.

[0032] Furthermore, there is little shrinkage when the paint dries, and the flatness of the coating film is not impaired, making painting easy. When the paint is a topcoat paint containing a pigment component, the content is preferably in the range of 20.0 to 55.0% by weight, and within this range, a relatively uniform and flat coating film can be efficiently obtained on a smooth surface.

[0033] The specific gravity of the paint is preferably in the range of 0.8 to 2.5. When the specific gravity is within this range, the finish becomes more uniform and smooth, an appropriate film thickness can be ensured, and painting becomes easier. If it is lower than 0.8, it will take time to ensure an appropriate film thickness, and if it is higher than 2.5, the paint will be heavy and painting work may become difficult.

[0034] In the case of an undercoat paint or a paint for adjusting the base, a range of 1.0 to 2.0 is preferable. Within this range, the finish will be more uniform and smooth without compromising the flatness of the coating film, an appropriate film thickness can be ensured, and coating will be easier. The paint roller for painting with such properties is made of a cotton-like pile, which is a collection of fibers, woven together with a backing, and the paint content of the roller is 0.5 to 3.0 g / cm 3 The coating is carried out using a coating roller having a bristle length in the range of 5 to 32 mm.

[0035] The painting roller used in this disclosure paints using a painting part made of a cotton-like pile, which is a collection of fibers, woven together with a backing fabric.The roller absorbs paint well, can paint a large area in one go, applies a large amount of paint, and forms a thick coating. In addition, because it adheres well to aggregates, it is effective for applying paints that contain aggregates, or paints with a high pigment content, such as undercoats and base conditioners, and it is also easy to work with.

[0036] Therefore, a uniform coating film can be easily formed efficiently, and the shape of the base can be made flat. The fibers used in this coating are not particularly limited, but synthetic fibers are mainly used, such as acrylic fibers, polyester fibers, and nylon fibers.

[0037] Paint rollers made of acrylic fibers are light and flexible, making them easy to paint with and easy to absorb paint. They are also relatively resistant to acids and alkalis, making them suitable for use with many types of paint. Polyester fiber is often used in high viscosity paints because it is relatively strong, resistant to abrasion, durable, and has excellent elasticity.

[0038] Nylon fiber is strong, has good paint release properties, and is highly elastic. This painting roller has a bristle length in the range of 5 to 32 mm, and the amount of paint contained in the bristle length is 0.5 to 3.0 g / cm 3 The range is as follows:

[0039] This painting roller is composed of a roller portion having a painting part and a handle for supporting the roller portion. The roller has a different inner diameter depending on the type, and the inner diameter is in the range of about 10.0 to 40.0 mm in diameter, and the coating portion is formed from the outer periphery of the inner diameter.

[0040] Typical examples of this inner diameter include a 38 mm one for painting relatively large areas, a 27 mm one that is easy to use, and a 17 mm one that is suitable for painting small details. The paint load is expressed by the weight of paint that can be contained in the volume of the painting roller determined by the length, circumference, and bristles, and this load is 0.5 to 3.0 g / cm. 3 If the amount is less than this range, the amount of paint absorbed will be small, the area that can be painted at one time will be small, and workability will be poor.

[0041] If the thickness is larger than this range, a larger amount of paint can be applied at one time, but it takes time to spread the amount of paint evenly, and in some cases the paint may dry out during the process, making it impossible to form a uniform coating. The paint content is 1.0 to 2.5 g / cm for undercoat paints and paints for base preparation. 3 This range is more preferable, as it allows for more efficient coating work, provides a more uniform and smooth finish without impairing the flatness of the coating film, ensures an appropriate film thickness, and makes coating easier.

[0042] The amount of paint that can be absorbed is affected by the bristle length of the painting roller, and is therefore selected within the range of 5 to 32 mm depending on the type and shape of the surface to be painted and the type of paint, with a bristle length in the range of 5 to 20 mm being preferred. If the bristle length is in the range of 5 to 6 mm, a smoother finish can be achieved, but since the amount of paint absorbed is small, there will be many patchwork areas on the painted surface.

[0043] In addition, brushes with a bristle length of 7 to 8 mm can hold a sufficient amount of paint and expel the contained paint well, providing a good balance between the flatness of the painted surface and ease of use. Those in the 10 to 14 mm range have a relatively high paint content and the paint is discharged well, providing a good balance between the flatness of the painted surface and workability.

[0044] Those in the 15 to 20 mm range can hold a large amount of paint, have good discharge, and are easy to work with. They can also be used to paint slightly uneven surfaces. Painting is performed using the paint and painting roller described above. This painting is often performed mainly on pillars, beams, floors, walls, etc. that constitute buildings, and these buildings may have a large paint area and complex shapes in the details, and in such cases, the effects of the present disclosure are fully exhibited.

[0045] Examples of surfaces that can be painted include mortar, concrete, ALC boards, extruded boards, siding boards, calcium silicate boards, gypsum boards, calcium carbonate foam boards, non-flammable volcanic vitreous laminate boards, fiber-reinforced cement boards, and lightweight cement boards, all of which contain inorganic components such as cement. Other examples include iron products such as steel materials, iron sheets, metal siding, etc. Other examples include tiles, glass, stone, wood, and plastic products.

[0046] It is preferable that the coating film formed by coating is in the range of 30 to 1000 μm. If it is in this range, a more uniform and smooth coating film can be obtained, and a good finish can be obtained. In the case of undercoat paints and paints for adjusting the base, the thickness is preferably in the range of 100 to 1000 μm. Within this range, the film thickness is sufficient to protect the surface to be painted and to allow the painting work to be carried out efficiently.

[0047] Such a coating film is relatively smooth, and this smoothness means that there is no unevenness in color or gloss, and when the coated surface is touched with the hand, there are no agglomerates of the paint components or unnatural unevenness, and it has a consistent feel to the touch. This condition means that the variation in thickness on the cross section of the coating film is within an error range of ±50.0% from the center value of the coating film.

[0048] Within this range, painting can be carried out efficiently, a flat coating film of uniform thickness can be formed, and a clean, smooth painted wall surface that matches the surface shape of the wall, etc. can be obtained. If the error is outside this range, the unevenness of the gloss of the coating film can be confirmed. More preferably, the error is within the range of ±10.0%, and if it is within this range, a flat coating film with a more uniform thickness can be formed, and a smooth painted wall surface can be obtained.

[0049] The above embodiment will now be described in more detail. Various paints were applied to slate boards with a coating film having small bumps using a paint roller, and the workability and finish were confirmed. The specifications and results are shown in Table 1.

[0050] [Table 1]

[0051] The fillers contained in various paints are mainly calcium carbonate, and the particle size is the D50 value calculated from the volume-based particle size distribution measured by laser diffraction method. The viscosity of the paint was measured using a Brookfield viscometer at 20 rpm and 23°C.

[0052] The painting rollers used were a roller generally called a high pile roller, which has a coating part in which cotton-like pile is woven together with the backing, and a roller generally called a woven roller, which has a coating part in which thread-like pile is woven into a woven backing in which warp and weft threads cross at right angles. The amount of paint absorbed is calculated by first weighing the roller, then submerging it in a container of paint, then weighing it again after removing it, and dividing the difference by the volume of the roller.

[0053] To evaluate workability, the ease of spreading various paints using the paint rollers listed in Table 1 and the paint scattering properties were confirmed. The finish was evaluated by checking the workability and visually inspecting the coating film formed. The coating thickness was measured at three random points on the dried coating formed by painting with various specifications.

[0054] The specifications of Examples 1 to 3 allowed the paint to be easily spread and produced a good finish. In particular, the specifications of Examples 1 and 2 allowed the paint to fill in the unevenness of the base, resulting in a smooth appearance. The specifications of Comparative Examples 1 and 2 made it difficult to spread the paint, and the finish was not very nice, as the paint did not easily penetrate into the recesses of the base.

[0055] In the case of the specification of Comparative Example 3, the paint was difficult to spread and there was a lot of splashing of the paint, probably due to the high solid content in the paint. In addition, the formed coating film was uneven. In the specifications of Comparative Example 4, the solid content in the paint was low, and the amount of paint absorbed by the painting roller was high, probably because of this, and there was a lot of paint splashing. In the specification of Comparative Example 5, the bristles of the painting roller used were short, so the amount of paint absorbed was small and it was difficult to spread the paint.

Claims

1. In the case where a paint having a Ti value in the range of 2 to 10 and a paint solid content in the range of 10.0 to 80.0% by weight is applied to an object to be coated with a coating roller, The coating portion of the coating roller is made of a knitted fabric in which a cotton-like pile, which is a collection of fibers, is woven together with a backing, The paint load of the painting roller is 0.5 to 3.0 g / cm 3 It is a painting roller, This coating method uses a coating roller having a bristle length in the range of 5 to 32 mm to coat the paint.

2. 2. The coating method using a coating roller according to claim 1, wherein the specific gravity of the coating material is in the range of 0.8 to 2.5, the content of the fillers contained in the coating material is in the range of 10.0 to 70.0% by weight, and the particle size is in the range of 1.0 to 800.0 μm.

3. 3. A coating method using a coating roller according to claim 1 or 2, wherein the coating film formed by the coating is in the range of 30 to 1000 μm.