Application Number
JP2023063090
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing methods for producing highly saturated clay mineral specimens, such as bentonite, are time-consuming, often taking several months to achieve stable hydraulic conductivity.

Method used

A method involving a charging step and a loading step using a laminate with a sealant between metal plates to apply a load, expelling air and degassing before sealing, ensuring high saturation by preventing leakage.

Benefits of technology

The method significantly reduces the production time of highly saturated clay mineral specimens to about 3 days, achieving a saturation degree of 95% or more.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149294000001_ABST
    Figure 2024149294000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing a clay mineral test piece capable of reducing manufacturing time of a high-saturation clay mineral test piece.SOLUTION: A method for manufacturing a clay mineral test piece includes: an input step S1 for inputting a sample 1 containing clay mineral and water into a metal container 2; and a load step S2 for applying a load to the sample 1 through a laminate 3. The laminate 3 has a sealant 6 between a metal plate 4 and a metal plate 5. The sealant 6 is preferably a plastic plate molded by extrusion molding. The plastic plate is preferably made by molding polyimide using a monomer casting method. The sealant 6 preferably has a compression strength of 10 to 500 MPa and a Young's modulus of 1 to 10 GPa.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a clay mineral specimen. [Background technology]

[0002] Bentonite is one type of clay mineral. Bentonite and bentonite-mixed soils have a low coefficient of permeability, and because of this property, they are used as impermeable layers in industrial waste disposal sites and radioactive waste disposal sites. In order to evaluate the properties of bentonite when it is used, various types of bentonite specimens are manufactured. When considering the use of bentonite as a impermeable layer, since the degree of saturation of these bentonites (see definition below) is high, it is necessary to evaluate the properties of the bentonite specimens at a high degree of saturation. However, it takes a long time to manufacture highly saturated bentonite specimens.

[0003] For example, in the past, water was gradually supplied from the bottom of the specimen. This method was used when the hydraulic conductivity of the specimen was 1×10 -13 In the case of a soil with a permeability of about 10 m / s, it took about 10 months to obtain a stable permeability coefficient. Therefore, efforts are being made to shorten the saturation time of bentonite specimens.

[0004] For example, Non-Patent Document 1 describes the following procedure for shortening the saturation time of a bentonite specimen (see Fig. 5). Note that Fig. 5 illustrates the saturation procedure for a bentonite specimen described in Non-Patent Document 1, which is a conventional example. (1) The sample (bentonite) is placed into a cylindrical mold and compacted by statically loading it from above and below with a hydraulic jack. (2) Insert the sample into the metal cell (ring) for the permeability test, place the cell in a vacuum desiccator, and maintain a vacuum at approximately -98 kPa for approximately two weeks. (3) Place the cell and sample in the permeability test device and keep it under vacuum for about one day. (4) Supply water at atmospheric pressure from the top and bottom of the specimen and leave it for about 10 days. Note that Non-Patent Document 1 also states that a reasonable hydraulic conductivity value can be obtained about 400 hours after water is passed through. In other words, in Non-Patent Document 1, it takes about 25 days to one month to produce a highly saturated bentonite specimen. [Prior art documents] [Non-patent literature]

[0005] [Non-Patent Document 1] Koji Kudo et al., "Study on shortening saturation time by vacuum degassing method for compacted bentonite samples," Proceedings of the 39th Geotechnical Engineering Research Conference, March 5, 2004, Vol. 9, 1105, pp. 2207-2208 Summary of the Invention [Problem to be solved by the invention]

[0006] However, there is a demand in the industry for further shortening the production time for specimens of clay minerals, including highly saturated bentonite.

[0007] The present invention has been made in consideration of the above demands. That is, an object of the present invention is to provide a method for producing a clay mineral specimen that can shorten the production time of a clay mineral specimen having a high degree of saturation. [Means for solving the problem]

[0008] In order to solve the above problems, the present invention has the following means. The present invention is a method for producing a clay mineral specimen, which includes a loading step of loading a sample containing a clay mineral and moisture into a metal container, and a loading step of applying a load to the sample via a laminate, wherein the laminate has a sealing material between the metal plates. In this way, in the present invention, since a load is applied to the sample using a laminate having a sealant between the metal plates in the loading step, the air contained in the sample can be expelled and degassed before the gap between the metal container and the sealant is closed (filled) by deformation of the sealant when the load is applied. In addition, when the load increases, the sealant elastically deforms in the horizontal direction due to the pressure, filling the gap between the sealant and the metal container, preventing the sample from leaking from the gap. Therefore, the present invention can achieve a high degree of saturation of the clay mineral specimen. Due to these actions, the present invention can shorten the manufacturing time of a clay mineral specimen with a high degree of saturation. Here, the degree of saturation refers to the value obtained by dividing the volume of water occupying the gap in the soil by the volume of the gap. The high degree of saturation refers to, for example, a degree of saturation of 95% or more, preferably 100%. In other words, the ratio of the volume of water occupying the gap in the soil to the volume of the gap is 95% or more, preferably 100%.

[0009] In the method for producing a clay mineral specimen according to the present invention, the sealing material is preferably a plastic plate molded by extrusion molding. In the method for producing a clay mineral specimen according to the present invention, it is further preferable that the plastic plate is one molded from polyimide by a monomer casting method. With these plastic plates, there is little distortion in the internal structure, so cracks are unlikely to occur when a load is applied during the loading process. This makes it possible to avoid situations where the gap between the sealing material (plastic plate) and the metal container cannot be filled sufficiently. This makes it possible to more reliably achieve a high degree of saturation for the clay mineral specimen.

[0010] In the method for producing a clay mineral specimen according to the present invention, the sealing material preferably has a compressive strength of 10 to 500 MPa and a Young's modulus of 1 to 10 GPa. With such a sealing material, cracks are less likely to occur when a load is applied in the loading step. This makes it possible to more effectively avoid situations in which the gap between the sealing material (plastic plate) and the metal container cannot be filled sufficiently. This makes it possible to more reliably achieve a high degree of saturation for the clay mineral specimen. Effect of the Invention

[0011] The method for producing a clay mineral specimen according to the present invention can shorten the time required to produce a clay mineral specimen with a high degree of saturation. [Brief description of the drawings]

[0012] [Figure 1] 2 is a flowchart illustrating the details of a method for manufacturing a clay mineral specimen according to this embodiment. [Diagram 2] 1 is a cross-sectional view illustrating the state of a sample 1, a metal container 2 and a laminate 3 immediately before a loading step S2 is performed in a method for producing a clay mineral specimen according to this embodiment. [Diagram 3] These are explanatory diagrams conceptually illustrating the structure of soil. (a) illustrates the state in which water and air are contained in the pores, and (b) illustrates the state in which the pores contain only water (no air, 100% saturation). [Figure 4] FIG. 2 is an enlarged cross-sectional view illustrating the state of a sample 1, a metal container 2 and a laminate 3 during the loading step S2 in the method for producing a clay mineral specimen according to this embodiment. [Diagram 5] 1 illustrates the saturation procedure for a bentonite specimen described in Non-Patent Document 1, which is a conventional example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, one embodiment of the method for producing a clay mineral specimen according to the present invention will be described in detail with reference to the drawings as appropriate. In the drawings, Fig. 1 is a flow chart for explaining the details of the method for producing a clay mineral specimen according to the present embodiment (hereinafter, sometimes referred to as the present production method). Fig. 2 is a cross-sectional view illustrating the state of the sample 1, the metal container 2, and the laminate 3 immediately before the loading step S2 in the present production method.

[0014] (This manufacturing method) 1, the present manufacturing method includes a loading step S1 and a loading step S2. In the loading step S1, a sample 1 containing a clay mineral and moisture is loaded into a metal container 2. In the loading step S2, a load is applied to the sample 1 via a laminate 3. 2, the laminate 3 has a sealing material 6 between the metal plates 4 and 5. Through these steps, the sample 1 becomes a highly saturated clay mineral specimen or a clay mineral mixed soil specimen (hereinafter, these may be collectively referred to simply as specimen 7). In this specification, the term "clay mineral specimen" refers to a specimen consisting of only clay minerals and water, and the term "clay mineral-mixed soil specimen" refers to a specimen consisting of clay minerals, water, and a parent material.

[0015] (Clay Minerals) Soil is composed of soil particles made of clay minerals, water, and air. As shown in FIG. 3, soil has voids, and these voids contain the water and air (FIG. 3(a)). FIG. 3 is an explanatory diagram conceptually illustrating the structure of soil. The voids in soil refer to the parts of the soil that are made up of water and air. When all the voids in the soil are filled with water and there is no air left, the soil is said to have a 100% degree of saturation (FIG. 3(b)). The specimen 7 produced by this production method is highly saturated, so it is most desirable for the saturation to be 100%, but as mentioned above, the saturation should be 95% or more.

[0016] Clay minerals are broadly divided into three groups: kaolinite, montmorillonite, and illite. In this embodiment, any of these can be used as the clay mineral, but it is preferable to use one containing montmorillonite. Montmorillonite is the main constituent mineral of bentonite. In this embodiment, it is more preferable to use bentonite as the clay mineral. In addition to montmorillonite, beidellite and the like are main component minerals of bentonite. Bentonite is a clay that is light gray, light greenish gray, light yellow, etc., and has the properties of swelling by adsorbing water and having high ion exchangeability (cation exchangeability).

[0017] To obtain a highly saturated specimen 7, it is necessary to manufacture it using a sample 1 containing clay minerals and water. The weight of the water to be mixed can be calculated by a known formula described later, assuming the degree of saturation to be 100%. Any clay mineral may be used as long as it is included in the above-mentioned three groups, but it is preferable to use bentonite, for example. Commercially available clay minerals, including bentonite, may be used. Commercially available bentonite products include, for example, Kasaoka bentonite (manufactured by Kasanen Kogyo Co., Ltd.), Kansai bentonite (manufactured by Kasanen Kogyo Co., Ltd.), Izumo bentonite (manufactured by Kasanen Kogyo Co., Ltd.), Shimane bentonite (manufactured by Kasanen Kogyo Co., Ltd.), Kunigel (registered trademark) V1 (manufactured by Kunimine Kogyo Co., Ltd.), Kunigel (registered trademark) V2 (manufactured by Kunimine Kogyo Co., Ltd.), M-1 (manufactured by Nippon Bentonite Kogyo Co., Ltd.), KA-1 (manufactured by Nippon Bentonite Kogyo Co., Ltd.), Aso C (manufactured by Nippon Bentonite Kogyo Co., Ltd.), KG-2 (manufactured by Nippon Bentonite Kogyo Co., Ltd.), and K (manufactured by Nippon Bentonite Kogyo Co., Ltd.), but are not limited thereto.

[0018] When bentonite is used, a specimen consisting of only bentonite and water, i.e., a bentonite specimen, can be prepared. However, since bentonite is expensive, in order to reduce the amount of bentonite used, a bentonite-mixed soil specimen can be prepared by mixing it with locally generated soil or silica sand as a base material. The bentonite-mixed soil specimen refers to a specimen consisting of bentonite, water, and a base material. From the viewpoint of reducing transportation costs, it is preferable to use locally generated soil as the base material. When a base material is mixed, the amount of the base material to be mixed may be such that a permeability coefficient required when using the bentonite-mixed soil as a water shielding layer is obtained. When a bentonite-mixed soil specimen is prepared, for example, the amount of the base material to be mixed is preferably 0 to 2000 parts by weight, more preferably 0 to 1900 parts by weight, even more preferably 0 to 600 parts by weight, and even more preferably 0 to 568 parts by weight, per 100 parts by weight of bentonite.

[0019] The thickness of the specimen 7 is, for example, preferably 10 cm or less, more preferably 5 cm or less. If the thickness of the specimen 7 exceeds 10 cm, it may be difficult to achieve a high degree of saturation even if a press is used. The planar dimensions of the specimen 7 can be large without any restrictions, provided there are no restrictions on the rigidity of the laminate 3 and the metal container 2 and the upper load limit of the press machine. However, taking into consideration the handling of jigs (larger jigs become heavier and work becomes more difficult), it is preferable to keep the dimensions at approximately 30 × 30 cm or less.

[0020] (Metal container) The metal container 2 has a bottomed cylindrical or square tube shape, and serves as a mold for forming the inserted sample 1 into a predetermined shape. The material constituting the metal container 2 is not particularly limited as long as it is a metal, and may be steel, cast iron, or the like. From the viewpoint of durability, the metal container 2 is preferably made of steel. The inner depth of the metal container 2 may be a depth that can accommodate the laminate 3 described below, and may be a depth that exceeds the thickness of the metal plate 4 and the sealing material 6.

[0021] (Laminate) The laminate 3 penetrates into the inside of the metal container 2 and plays a role in transmitting the pressure of the press machine to the entire sample 1. The laminate 3 is constructed by stacking a metal plate 4, a sealing material 6, and a metal plate 5 in this order from the sample 1 side. The metal plate 4, the sealing material 6, and the metal plate 5 have the same shape as the inside shape of the metal container 2 (for example, rectangular or circular in plan view), and preferably have dimensions slightly smaller than the internal dimensions of the metal container 2. Specifically, the gap between the end of the metal plate 4 that contacts the sample 1 and the metal container 2 is about 0.5 mm to 5 mm, particularly preferably 1 to 2 mm, from the viewpoint of preventing leakage of the sample 1. The metal plates 4 and 5 are preferably constructed of a material that does not deform significantly due to the pressure of the press machine. That is, it is preferable that the outer peripheral surfaces of the metal plates 4 and 5 do not contact the inner peripheral surface of the metal container 2 (a gap is secured) until the loading step S2 is completed.

[0022] On the other hand, the metal plate 4 plays a role of securing the area S (see FIG. 4) surrounded by the metal container 2 and the sealing material 6 that contacts the metal container 2 by applying a load. The air in the sample 1 (inside the specimen 7) is released by applying a suitable load press, but after the sealing material 6 contacts the metal container 2, there is no escape route for the air. Therefore, it is considered that the air escapes to this area S. Since air is compressible, it is considered that it accumulates (escapes) in this area S under a fairly high pressure. It is noted that it takes a little time from the start of applying the load until the sealing material 6 deforms and contacts the metal container 2. During this time, it is considered that the sealing effect cannot be expected. Therefore, for example, if the sample 1 is 100% bentonite, it is softer than the bentonite mixed soil with silica sand, so the sample 1 tries to escape from the gap between the metal container 2 and the metal plate 4 even before the sealing effect can be expected. Unless the seal is perfect, it is inevitable that the sample 1 will try to escape. However, it is necessary to prevent the sample 1 from passing through the gap before the sealing material 6 contacts the metal container 2. If the specimen 1 passes through the gap before the sealing material 6 comes into contact with the metallic container 2, the sealing material 6 will deform, and the complete sealing effect achieved by contact with the metallic container 2 cannot be expected. Therefore, while allowing some escape of the specimen 1 by the aforementioned region S, it is possible to buy time for the sealing material 6 and the metallic container 2 to come into direct contact by the thickness of the metal plate 4, thereby avoiding a situation in which the complete sealing effect is lost. Once the sealing material 6 and the metallic container 2 come into contact, a complete sealing effect can be obtained, so pressing is performed with as high a load as possible, and the degree of saturation of the specimen 7 can be increased while an escape route for air is secured by region S.

[0023] The thickness of the metal plate 4 is not particularly limited, but from the above viewpoint and from the viewpoint of durability, it is preferably 20 to 100 mm, and more preferably 30 to 60 mm. The material constituting the metal plate 4 is not particularly limited as long as it is a metal, and may be steel, cast iron, etc. From the viewpoint of durability, the metal plate 4 is preferably steel. The other metal plate 5 not only transmits the pressure of the press to the sealing material 6, but also suppresses the vertical displacement of the sealing material 6. The thickness of the metal plate 5 is not particularly limited, but is preferably 20 to 100 mm, and more preferably 30 to 100 mm, from the viewpoint of durability. The material constituting the metal plate 5 is not particularly limited as long as it is a metal, and may be steel, cast iron, or the like. The metal plate 5 is preferably steel from the viewpoint of durability.

[0024] Here, FIG. 4 is an enlarged cross-sectional view illustrating the state of the sample 1, the metal container 2, and the laminate 3 during the loading step S2 in this manufacturing method. The sealing material 6 is made of a material having a smaller deformation coefficient than the metal plate 5. As shown in FIG. 4, when the loading step S2 is performed, the sealing material 6 elastically deforms in the horizontal direction due to the pressure of the press machine, filling the gap between the sealing material 6 and the metallic container 2 and preventing the sample 1 from leaking from the gap. That is, the sealing material 6 does not contact the inner peripheral surface of the metallic container 2 at the start of the loading step S2, but contacts the inner peripheral surface of the metallic container 2 from the middle to the end of the loading step S2. Note that, during the time until the gap between the sealing material 6 and the metallic container 2 is filled, the pressure of the press machine can expel the air contained in the gap of the sample 1 from the gap, that is, degassing.

[0025] The thickness of the sealing material 6 is not particularly limited, but is preferably 1 to 50 mm, and more preferably 1 to 10 mm. The material of the sealing material 6 is not particularly limited, and may be a thermoplastic resin such as polypropylene, polyethylene, polyacrylic, polyamide, polycarbonate, polyacetal, polyphenylene oxide, or a thermosetting resin such as epoxy resin or phenol resin. The sealing material 6 is preferably a plastic plate with little distortion in the internal structure, since if a crack occurs during compression, the gap between the metal container 2 and the laminate 3 cannot be filled sufficiently. From the above viewpoint, it is preferable that the sealing material 6 is a plastic plate obtained by extrusion molding of a thermoplastic resin or a plastic plate obtained by a monomer casting method of polyimide (nylon).

[0026] The sealing material 6 may be any material that is not broken by the load, and the compressive strength of the sealing material 6 is preferably 10 to 500 MPa. The sealing material 6 may be any material that is softer than metal, and the deformation coefficient (Young's modulus) of the sealing material 6 is preferably 1 to 10 GPa. If the sealing material 6 has such physical properties, cracks are less likely to occur when a load is applied in the loading step S2. Therefore, it is possible to more effectively prevent a situation in which the gap between the sealing material 6 (plastic plate) and the metal container 2 cannot be sufficiently filled. Therefore, it is possible to more reliably increase the degree of saturation of the test piece 7. From the above viewpoint, the compressive strength of the sealing material 6 is more preferably 50 to 300 MPa, and more preferably 100 MPa, for example. From the above viewpoint, the Young's modulus is more preferably 3 to 5 GPa.

[0027] The inserting step S1 and the loading step S2 are as described at the beginning of the description of the embodiment, and an example of a specific operation in each step will be described below. (Input process) In the charging step S1, a clay mineral, preferably bentonite, water, and optionally a base material are mixed in advance to prepare sample 1, which is then charged into a metal container 2. The amount of sample 1 to be charged can be calculated from the dimensions of a specimen 7 to be produced and the target dry density of the specimen 7 using a known formula described below. Here, dry density refers to the value obtained by dividing the weight of soil particles by the volume of the soil. The amounts of clay mineral and base material to be charged can be calculated from the target dry density and the target volume of the test specimen 7. The weight of water to be added can be calculated by calculating the moisture content from the target dry density and soil particle density using the following formula (1), and then adding up the amounts of clay minerals and base material to be added.

[0028] Equation (1): Saturation equation: Sr = (ωρ s ) / (eρ w ) Void ratio formula: e=Vv / Vs=ρ s / ρ d -1 where Sr is the degree of saturation, ω is the water content, and ρ s : soil particle density, e: void ratio, ρ w : density of water, Vv: volume of pores, Vs: volume of soil particles, ρ d : Dry density. The soil particle density is the value obtained by dividing the weight of a soil particle by the volume of the soil particle. The moisture content is the weight of water divided by the weight of dry soil. The void ratio is the value obtained by dividing the volume of the soil voids by the volume of the soil particles.

[0029] (Loading process) In the loading step S2, first, the metal plate 4 is placed on the metal container 2, and a load is applied until the press machine stops displacing. The time for applying this load is about 5 to 10 minutes. In this manner, since the sealing material 6 has not yet been used, the air contained in the gap between the metal plate 4 and the metal container 2 can be expelled from the gap in the sample 1, and degassed. This makes it possible to remove the air that affects the degree of saturation from the sample 1. Next, the application of pressure by the press machine is temporarily stopped, and the sealing material 6 and the metal plate 5 are laminated in this order on the metal plate 4 to form the laminate 3, after which a load is applied by the press machine again. At this time, the sealing material 6, which is one of the components of the laminate 3, undergoes elastic deformation, filling the gap between the sealing material 6 and the metallic container 2. This makes it possible to apply a load by the press machine without the sample 1 leaking from the metallic container 2. The load applied by the press machine is set to 7.5 to 15 t (5 to 10 MPa for the sample 1) and the load is applied for 1 to 3 days.

[0030] According to the present manufacturing method described above, in the loading step S2, a load is applied to the sample 1 using the laminate 3 having the sealing material 6 between the metal plates 4 and 5, so that the air contained in the sample 1 can be expelled and degassed before the gap between the metallic container 2 and the sealing material 6 is closed (filled) by the deformation of the sealing material 6 due to the application of the load. Furthermore, when the load increases, the sealing material 6 elastically deforms in the horizontal direction due to the pressure, filling the gap between the sealing material 6 and the metallic container 2, so that leakage of the sample 1 from the gap can be prevented. Therefore, the present manufacturing method can make the saturation degree of the test piece 7 high. Due to these actions, the present manufacturing method can shorten the manufacturing time of the highly saturated test piece 7. EXAMPLES

[0031] The following examples are given, but the present invention is not limited thereto. The target dimensions of specimen 7 are 15cm x 10cm x 5cm (750cm 3 ) was decided. Bentonite was used as the clay mineral. A base material was used as necessary. Silica sand was used as the base material. The amounts of bentonite and silica sand to be charged were calculated from the target dry density and the target volume of the test specimen 7. The weight of water to be charged was calculated by calculating the water content from the target dry density and soil particle density using the above formula (1) and integrating the amounts of bentonite and silica sand to be charged.

[0032] For example, 100% bentonite (target dry density ρ d =1.6g / cm 3 ), then it is 15cm x 10cm x 5cm (750cm 3 When manufacturing a test piece 7 with a dry weight of 1200 g (= 1.6 × 750), a sample 1 with a dry weight of 1200 g (= 1.6 × 750) is required. s =2.774g / cm 3Then, the water content ω for 100% saturation is specified as ω = 26.5%, and the required weight of the wet sample (dry sample + water) is 1518g (= 1200 × (1 + 0.265)). In other words, if 1518g of sample 1 is placed in a metal container 2 with inner dimensions of 15cm × 10cm and pressed to a height of 5cm, it will become specimen 7 with a dry density of 1.6 and a 100% saturation.

[0033] For example, if the ratio of bentonite and silica sand is 50%:50%, the target dry density ρ d =1.8g / cm 3 So, 15cm x 10cm x 5cm (750cm 3 When manufacturing a test piece 7 with a dry weight of 1350 g (= 1.8 × 750), a sample 1 with a dry weight of 1350 g (= 1.8 × 750) is required. s =2.740g / cm 3 ) (measured from physical property tests), the saturated water content is ω = 19.1%. e=(2.740 / 1.8)-1=0.522 ω=Sr×e / ρ s =100×0.522 / 2.740=19.05≒19.1% The required weight of the wet sample (dry sample + water) is 1608g (=1350×(1+0.191)). In other words, if 1608g of sample 1 is placed in a metal container 2 with inner dimensions of 15cm×10cm and pressed to a height of 5cm, it will become specimen 7 with a dry density of 1.8 and a saturation degree of 100%.

[0034] <Evaluation method> The dry density and the degree of saturation of the specimen 7 were calculated by measuring the dimensions of the obtained specimen 7 and using the above formula (1) and the following formula (2), respectively. In this case, since the moisture content does not change before and after the production of the specimen 7, the value calculated in advance was used. Formula (2): Dry density formula: ρ d =ρ s / (1+ω / 100) Here, ρ d :Dry density, ρ s : soil particle density, ω: water content.

[0035] <Example 1> Bentonite specimen (target dry density 1.6 g / cm 3 ) Bentonite (Kunigel® V1 (Kunimine Industries Co., Ltd.), soil particle density 2.774 g / cm 3 1200g of cellulose acetate and 318g of water were mixed and placed in a metal container 2 with an inner dimension of 15cm x 10cm x 10cm. Then, a metal plate 4 with a thickness of 30mm was placed in the metal container 2, and a load of 7.5t (5MPa for sample 1) was applied at the set value of the device until the displacement of the press machine disappeared (about 5 to 10 minutes). Then, a plastic plate (MC Nylon (registered trademark)) with a thickness of 5mm, i.e., a sealing material 6 and a metal plate 5 with a thickness of 20mm were laminated on the metal plate 4 with a thickness of 30mm, to place the laminate 3 in the metal container 2, and a load of 10t (6.7MPa for sample 1) was applied at the set value of the device by the press machine for three days. Then, the manufactured specimen 7 was taken out of the metal container 2, and the dimensions were measured to calculate the dry density and saturation degree.

[0036] Example 2: Bentonite mixed soil specimen (target dry density 1.8 g / cm 3 ) A mixture containing 50% each of bentonite (Kunigel® V1 (Kunimine Kogyo Co., Ltd.)) and silica sand (soil particle density 2.740 g / cm 3 1350g of cellulose acetate and 258g of water were mixed and placed in a metal container 2 with an inner dimension of 15cm x 10cm x 10cm. Then, a metal plate 4 with a thickness of 30mm was placed in the metal container 2, and a load of 7.5t (5MPa for sample 1) was applied at the set value of the device until the displacement of the press machine disappeared (about 5 to 10 minutes). Then, a plastic plate (MC Nylon (registered trademark)) with a thickness of 5mm, i.e., a sealing material 6 and a metal plate 5 with a thickness of 20mm were laminated on the metal plate 4 with a thickness of 30mm, to place the laminate 3 in the metal container 2, and a load of 10t (6.7MPa for sample 1) was applied at the set value of the device by the press machine for three days. Then, the manufactured specimen 7 was taken out of the metal container 2, and the dimensions were measured to calculate the dry density and saturation degree.

[0037] <Comparative Example 1> Bentonite specimen (target dry density 1.6 g / cm 3 ) Bentonite (Kunigel® V1 (Kunimine Industries Co., Ltd.), soil particle density 2.774 g / cm 3 1,200 g of sintered soybean paste and 318 g of water were mixed and placed in a metal container 2 with inner dimensions of 15 cm x 10 cm x 10 cm. A metal plate 4 with a thickness of 30 mm was then placed in the metal container 2, and a load of 7.5 t (5 MPa for sample 1) was applied at the set value of the press machine until the displacement of the press machine disappeared (about 5 to 10 minutes), and a load of 10 t (6.7 MPa for sample 1) was applied at the set value of the press machine for three days. The manufactured specimen 7 was then removed from the metal container 2, and its dimensions were measured to calculate the dry density and degree of saturation.

[0038] <Comparative Example 2> Bentonite mixed soil specimen (target dry density 1.8g / cm 3 ) A mixture containing 50% each of bentonite (Kunigel® V1 (Kunimine Kogyo Co., Ltd.)) and silica sand (soil particle density 2.740 g / cm 3 1,350 g of sintered soda and 258 g of water were mixed and placed in a metal container 2 with inner dimensions of 15 cm x 10 cm x 10 cm. A metal plate 4 with a thickness of 30 mm was then placed in the metal container 2, and a load of 7.5 t (5 MPa for sample 1) was applied at the set value of the press machine until the displacement of the press machine disappeared (about 5 to 10 minutes), and a load of 10 t (6.7 MPa for sample 1) was applied at the set value of the press machine for three days. The manufactured specimen 7 was then removed from the metal container 2, and its dimensions were measured to calculate the dry density and degree of saturation.

[0039] <Result> The results are shown in Table 1. The values ​​in Table 1 for bentonite, silica sand, and water are in grams (g). Blanks in Table 1 indicate that no water was added. As shown in Table 1, the present invention made it possible to produce highly saturated bentonite specimens and bentonite-mixed soil specimens, i.e., clay mineral specimens and clay mineral-mixed soil specimens, in a short period of about three days. Specifically, in both Examples 1 and 2, the degree of saturation was 95% or higher, reaching approximately 98%.

[0040] [Table 1]

[0041] Although the embodiments and examples of the present invention have been described above, the present invention is not limited to the above-described embodiments and examples, and each of the above-described components can be appropriately modified without departing from the spirit of the present invention. [Explanation of symbols]

[0042] 1. Sample 2. Metal containers 3. Laminate 4 metal plate 5 metal plate 6 Sealing materials 7 Specimen S area S1 Input process S2 Loading process

Claims

1. A step of introducing a sample containing clay minerals and moisture into a metal container; A loading step of applying a load to the sample through the laminate, The laminate is characterized in that it has a sealing material between the metal plates. A method for producing clay mineral specimens.

2. 2. The method for producing a clay mineral specimen according to claim 1, wherein the sealing material is a plastic plate formed by extrusion molding.

3. 3. The method for producing a clay mineral specimen according to claim 2, wherein the plastic plate is formed by molding polyimide by a monomer casting method.

4. 2. The method for producing a clay mineral specimen according to claim 1, wherein the sealing material has a compressive strength of 10 to 500 MPa and a Young's modulus of 1 to 10 GPa.