Manufacturing method for welded member
By designing welded parts to extend in opposite circumferential directions with balanced deformation, the method addresses the issues of increased time and quality deterioration in multi-part welding, enhancing thermal distortion suppression and weld quality.
Patent Information
- Application Number
- JP2023067187
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-17
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2043-04-17
AI Technical Summary
Existing welding methods for multi-part components suffer from increased welding time and varying penetration amounts, leading to deteriorated weld quality due to thermal distortion and overlapping start/end points.
A method involving forming first and second welded parts that extend in opposite circumferential directions around the central axis, with deformation points spaced apart by at least 90 degrees, ensuring equal deformation amounts and opposite contraction forces to offset thermal distortion.
This approach effectively suppresses thermal distortion and maintains weld quality by balancing deformation in multi-part components, reducing the influence of thermal strain on the welded member.
Smart Images

Figure 2024153352000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a welded component. [Background technology]
[0002] Patent Document 1 discloses a welding method for forming a clutch drum by welding a cylindrical drum body having a bottom wall in which a circular fitting hole is formed, and an axial shaft having a fitting portion that is press-fitted into the fitting hole. In this welding method, the joint between the fitting hole and the fitting portion is divided into four ranges (first to fourth ranges) that are equiangular in the circumferential direction centered on the axis of the fitting portion. Then, the joints are welded all around in the order of the first range, the second range facing the first range across the axis, the third range located between the first and second ranges, and the fourth range facing the third range across the axis, so that the start and end points of welding in each range overlap, thereby suppressing thermal distortion of the clutch drum. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2013-103274 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, the above-mentioned welding method requires a longer welding time than a method of welding the entire joint in a single circumferential motion. Also, since the amount of penetration during welding is likely to vary at the start and end points of welding, there is a problem that the quality of the weld is likely to deteriorate if there are many overlapping portions where the start and end points of welding overlap, as in the above-mentioned welding method.
[0005] However, in the case of a welded component formed by welding three or more parts, there are multiple welded parts. Therefore, in a welded component having multiple welded parts, a method is desired that can suppress the influence of thermal distortion of the welded component while suppressing an increase in welding time and a decrease in welding quality.
[0006] One aspect of the present disclosure aims to suppress the effects of thermal distortion in a welded member formed by welding at least three components. [Means for solving the problem]
[0007] One aspect of the present disclosure is a method for manufacturing a welded member in which a first part, a second part, and a third part are welded together. The method for manufacturing the welded member includes welding the first part and the second part together so as to form a first welded part that extends in a circumferential direction centered on an axis of the welded member that extends in a direction in which the first part, the second part, and the third part are aligned. The method for manufacturing the welded member also includes welding the second part and the third part together so as to form a second welded part that extends in the circumferential direction. The first welded part and the second welded part each extend from a welding start point to a welding end point. A position that is located in a range from the welding start point of the first welded part to approximately the center of the first welded part in the circumferential direction and that is the center of deformation that occurs in the first welded part is defined as a first deformation point. A position that is located in a range from the welding start point of the second welded part to approximately the center of the second welded part in the circumferential direction and that is the center of deformation that occurs in the second welded part is defined as a second deformation point. The second deformation point is disposed at least 90° apart from the first deformation point in the circumferential direction.
[0008] In this configuration, the deformation occurring in the first welded portion is easily offset by the deformation occurring in the second welded portion, and therefore the influence of thermal distortion of the welded member formed by welding the three components, the first component, the second component, and the third component, can be suppressed.
[0009] In one aspect of the present disclosure, the circumferential length of the first welded portion and the circumferential length of the second welded portion may be substantially the same. With this configuration, the amount of deformation occurring in the first welded portion and the amount of deformation occurring in the second welded portion tend to be substantially the same, which makes it easier to suppress the effects of thermal distortion of the welded member.
[0010] In one aspect of the present disclosure, the first welded portion and the second welded portion may be formed by full circumference welding. With this configuration, it is possible to suppress the influence of thermal distortion of the welded member having the first welded portion and the second welded portion formed by full circumference welding.
[0011] In one aspect of the present disclosure, the first deformation point may be a welding end point, which is a welding start point and a welding end point of the first welded portion. The second deformation point may be a welding end point, which is a welding start point and a welding end point of the second welded portion. With this configuration, the deformation occurring in the first welded portion is easily offset by the deformation occurring in the second welded portion. Therefore, it is possible to suppress the influence of thermal distortion of the welded member formed by welding three parts, the first part, the second part, and the third part.
[0012] In one aspect of the present disclosure, the welded member may be an on-vehicle part that is mounted on a vehicle. With this configuration, it is possible to suppress the influence of thermal distortion of the on-vehicle part that is formed by welding the first part, the second part, and the third part.
[0013] In one embodiment of the present disclosure, the first welded portion may be formed by welding along a first circumferential direction about the axis. The second welded portion may be formed by welding along a second circumferential direction opposite to the first circumferential direction about the axis. In such a configuration, the welding directions of the welded portions are opposite to each other along the circumferential direction, so that the directions in which the welded portions contract as they cool, i.e., the directions of the forces with which the welded portions pull the respective components in the circumferential direction, are opposite. Therefore, deformation occurring in the first welded portion is more likely to be offset by deformation occurring in the second welded portion. [Brief description of the drawings]
[0014] [Figure 1] FIG. 2 is a cross-sectional view illustrating a welded member. [Diagram 2] 2A is a cross-sectional view taken along line IIA-IIA in FIG. 1, and FIG. 2B is a cross-sectional view taken along line IIB-IIB in FIG. [Diagram 3] 10 is a diagram showing a schematic diagram of positions of welding start and end points of each weld in a modified example of a welded member having three or more welds. FIG. [Figure 4] 10A and 10B are diagrams illustrating the welding directions of the welded portions in a modified example of a welded member having three or more welded portions. [Diagram 5] FIG. 11 is a cross-sectional view showing a schematic position of a deformation point of each weld in a modified example of each weld that is an arc. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, exemplary embodiments of the present disclosure will be described with reference to the drawings. [1. Configuration] 1 is an on-vehicle part that is mounted on a vehicle. An example of the on-vehicle part is an exhaust system part that constitutes at least a part of a flow path for passing exhaust gas from an internal combustion engine mounted on the vehicle.
[0016] 1, the welded member 100 includes a first part 1, a second part 2, a third part 3, a first welded part W1, and a second welded part W2. In this embodiment, the welded member 100 has a central axis A that extends linearly. The welded member 100 is manufactured by welding the first part 1, the second part 2, and the third part 3, which are arranged side by side along the central axis A, by, for example, arc welding.
[0017] The first part 1 and the third part 3 are tubes formed into a cylindrical shape with a constant diameter. The second part 2 is a cylindrical part disposed between the first part 1 and the third part 3. The central axes of the first part 1, the second part 2, and the third part 3 coincide with the central axis A of the welded member 100. The second part 2 has a first end 21 connected to the first part 1 and a second end 22 connected to the third part 3, which are formed in a tapered shape with a diameter decreasing toward the end. In this embodiment, the first part 1, the second part 2, and the third part 3 are connected in a state in which the end of the first part 1 is inserted into the opening on the first end 21 side of the second part 2, and the end of the third part 3 is inserted into the opening on the second end 22 side of the second part 2.
[0018] The first welded portion W1 is formed at a portion where the first part 1 and the second part 2 overlap, extending in a circumferential direction centered on the central axis A, and joins the first part 1 and the second part 2. In this embodiment, as shown in FIG. 2A, the first welded portion W1 is formed by welding along a first circumferential direction centered on the central axis A. That is, the first welded portion W1 is formed by moving a welding machine clockwise along the circumferential direction. That is, the welding direction of the first welded portion W1 is the first circumferential direction (clockwise direction).
[0019] The second welded portion W2 is formed to extend in the circumferential direction in the portion where the second part 2 and the third part 3 overlap, and joins the second part 2 and the third part 3. In this embodiment, as shown in FIG. 2B , the second welded portion W2 is formed by welding along a second circumferential direction opposite to the first circumferential direction, centered on the central axis A. That is, the second welded portion W2 is formed by moving a welding machine counterclockwise along the circumferential direction. That is, the welding direction of the second welded portion W2 is the second circumferential direction (counterclockwise direction).
[0020] In this embodiment, the first welded portion W1 is formed by full circumference welding along a welding path that goes around the outer peripheral surfaces of the first part 1 and the second part 2, and the second welded portion W2 is formed by full circumference welding along a welding path that goes around the outer peripheral surfaces of the second part 2 and the third part 3. In full circumference welding, the welding start point and the welding end point overlap. Hereinafter, the welding start point and the welding end point in the welded portion are referred to as the welding end point. That is, as shown in FIG. 2A and FIG. 2B, in a cross section perpendicular to the central axis A, the shapes of the first welded portion W1 and the second welded portion W2 are circles with the welding path closed. In this embodiment, the circumferential length of the first welded portion W1 and the circumferential length of the second welded portion W2 are approximately the same. Note that the state in which the welding start point and the welding end point overlap each other includes a state in which the welding start point and the welding end point overlap in whole or in part.
[0021] In this embodiment, the first welding end point S1 of the first welded portion W1 shown in Fig. 2A and the second welding end point S2 of the second welded portion W2 shown in Fig. 2B are disposed approximately 180° apart in the circumferential direction when viewed along the central axis A. Specifically, when the second welded portion W2 is moved along the central axis A to overlap with the first welded portion W1, the second welding end point S2 is disposed on an extension of a straight line connecting the first welding end point S1 and the central axis A. In other words, the first welding end point S1 and the second welding end point S2 face each other with the central axis A as the center.
[0022] [2. Manufacturing methods for welding components] 2A and 2B, a method for manufacturing the welded member 100 will be described. Specifically, a method for welding the first component 1 and the second component 2 and a method for welding the second component 2 and the third component 3, which are included in the method for manufacturing the welded member 100, will be described.
[0023] First, the end of the first part 1 is inserted into the opening on the first end 21 side of the second part 2 to connect the first part 1 and the second part 2. Then, as shown in Fig. 2A, the first part 1 and the second part 2 are fully circumferentially welded together in the first circumferential direction to form a first welded part W1.
[0024] Next, the end of the third part 3 is inserted into the opening on the second end 22 side of the second part 2 to connect the second part 2 and the third part 3. Then, as shown in FIG. 2B, the second part 2 and the third part 3 are welded all around along the second circumferential direction to form the second welded part W2. At this time, welding of the second welded part W2 is started from the second welded end point S2 that is disposed approximately 180° apart in the circumferential direction from the first welded end point S1 of the first welded part W1. As a result, when the second welded part W2 is moved along the central axis A to overlap with the first welded part W1, the first welded end point S1 and the second welded end point S2 are disposed in positions that face each other with respect to the central axis A.
[0025] In arc welding, the formation of the welded portion tends to cause deformation due to thermal strain in the welded portion. In addition, in full circumference welding, the welds overlap at points located in the range from the welding start point of the welded portion to approximately the center in the circumferential direction of the welded portion, especially at the welding end point, and the time for the heat of the welding to be transmitted to the welded object is long, so the heat capacity is likely to increase. For this reason, in the first welded portion W1 formed by full circumference welding using arc welding, the position that is the center of deformation occurring in the first welded portion W1 is the first welding end point S1. In addition, in the second welded portion W2 formed by full circumference welding using arc welding, the position that is the center of deformation occurring in the second welded portion W2 is the second welding end point S2. The position that is the center of deformation is, for example, the part of the welded portion that is most deformed by thermal strain.
[0026] The formation of the first weld W1 causes deformation due to thermal strain in a first direction D1 shown in Fig. 2A from the central axis A toward the first weld end point S1. The formation of the first weld W2 causes deformation due to thermal strain in a second direction D2 shown in Fig. 2B from the central axis A toward the second weld end point S2. As described above, the first weld end point S1 and the second weld end point S2 are disposed at opposing positions centered on the central axis A, so the first direction D1 is opposite the second direction D2.
[0027] As described above, the circumferential length of the first welded portion W1 and the circumferential length of the second welded portion W2 are substantially the same, so that the amount of deformation occurring in the first welded portion W1 and the amount of deformation occurring in the second welded portion W2 tend to be substantially the same. Furthermore, as described above, the welding directions of the first welded portion W1 and the second welded portion W2 are opposite to each other along the circumferential direction. Therefore, the direction in which each welded portion W1, W2 contracts as each welded portion W1, W2 cools, that is, the direction of the force of the first welded portion W1 pulling the first component 1 and the second component 2 in the circumferential direction is opposite to the direction of the force of the second welded portion W2 pulling the second component 2 and the third component 3 in the circumferential direction.
[0028] [3. Effects] According to the embodiment described above in detail, the following effects can be obtained. (3a) In this embodiment, the formation of the first welded portion W1 generates thermal distortion in the first direction D1 in the welded member 100, and the formation of the second welded portion W2 generates thermal distortion in the second direction D2. However, the first welded portion W1 and the second welded portion W2 are formed such that the first welding end point S1 and the second welding end point S2 are positioned opposite to each other about the central axis A. In other words, the first direction D1 is opposite to the second direction D2. For this reason, deformation caused by thermal distortion in the first direction D1 in the first welded portion W1 is easily offset by deformation caused by thermal distortion in the second direction D2 in the second welded portion W2.
[0029] Therefore, in a welded member 100 manufactured by welding three parts, the first to third parts 1, 2, and 3, and having two welded parts W1 and W2 formed by full-circumference welding, it is possible to suppress the effects of thermal distortion of the welded member 100 while suppressing an increase in welding time and a decrease in welding quality.
[0030] (3b) In this embodiment, the circumferential length of the first welded portion W1 and the circumferential length of the second welded portion W2 are substantially the same, so that the amount of deformation due to thermal strain occurring in the first welded portion W1 and the amount of deformation due to thermal strain occurring in the second welded portion W2 tend to be substantially the same. Therefore, the influence of thermal strain on the welded member 100 is easily suppressed.
[0031] (3c) In this embodiment, the welding directions of the first welded portion W1 and the second welded portion W2 are opposite to each other along the circumferential direction. As a result, the direction in which each welded portion W1, W2 contracts as it cools, i.e., the direction of the force with which the first welded portion W1 pulls the first component 1 and the second component 2 in the circumferential direction is opposite to the direction of the force with which the second welded portion W2 pulls the second component 2 and the third component 3 in the circumferential direction. For this reason, deformation due to thermal strain occurring in the first welded portion W1 is more likely to be offset by deformation due to thermal strain occurring in the second welded portion W2.
[0032] In this embodiment, the first welding end point S1 corresponds to an example of a first deformation point, the second welding end point S2 corresponds to an example of a second deformation point, and the central axis A corresponds to an example of an axis.
[0033] [4. Other embodiments] Although the embodiments of the present disclosure have been described above, it goes without saying that the present disclosure is not limited to the above-described embodiments and can take various forms.
[0034] (4a) In the above embodiment, the second welding end point S2 of the second welded zone W2 is disposed 180° apart in the circumferential direction from the first welding end point S1 of the first welded zone W1 when viewed along the central axis A. However, the relative positions of the first welding end point S1 and the second welding end point S2 in the circumferential direction are not limited to this.
[0035] For example, the second weld end point S2 of the second welded portion W2 may be disposed circumferentially at least 90° away from the first weld end point S1 of the first welded portion W1. Specifically, when the second welded portion W2 is moved along the central axis A to overlap with the first welded portion W1, the second weld end point S2 may be disposed in a range such that the angle between a line connecting the first weld end point S1 and the central axis A and a line connecting the second weld end point S2 and the central axis A is 90° or more and 270° or less.
[0036] Also, for example, when the welding path in a full circumference welding is divided into four ranges at equal angles in the circumferential direction, the second welding end point S2 may be located in a second range that faces the first range in which the first welding end point S1 is located, with the remaining two ranges (i.e., the third range and the fourth range) in between.
[0037] Even in the case of the above-described relative circumferential positions of the first welding end point S1 and the second welding end point S2, the influence of thermal distortion of the welded member can be suppressed, similarly to the welded member 100 of this embodiment.
[0038] (4b) In the above embodiment, the welded member 100 has two welds, the first welded portion W1 and the second welded portion W2, but for example, the welded member may be formed by welding four or more parts together so as to have three or more welds.
[0039] For example, when a welded member has three or more welds, the welding start and end points of all the welds (i.e., the positions that are the centers of deformation occurring in each weld) of adjacent welds may not be arranged at positions that face each other about the central axis A. Specifically, as in the welded member 100a shown in FIG. 3, when the total number of welding start and end points S1a, S2a, and S5a arranged at the first position is the same as the total number of welding start and end points S3a, S4a, and S6a arranged at the second position, the welding start and end points of some of the adjacent welds may not be arranged at positions that face each other about the central axis A. The second position is a position that is arranged at least 90° apart from the first position in the circumferential direction. That is, the welding start and end points of adjacent welds may be arranged to overlap each other as viewed along the central axis A, such as the welding start and end points S1a and S2a, and the welding start and end points S3a and S4a. In this case, as in the case of the welded member 100 of this embodiment, the influence of thermal distortion of the welded member 100a can be suppressed.
[0040] Also, for example, when the welded member has three or more welds, the welding directions of adjacent welds in all the welds may not be opposite to each other along the circumferential direction. Specifically, as in the welded member 100b shown in FIG. 4, when the total number of the welds W1b, W2b, and W3b formed along the first circumferential direction is the same as the total number of the welds W4b, W5b, and W6b formed along the second circumferential direction, the welding directions of some of the adjacent welds may not be opposite to each other along the circumferential direction. That is, the welding directions of adjacent welds may be the same along the circumferential direction, such as the welded portion W1b and the welded portion W2b, the welded portion W2b and the welded portion W3b, the welded portion W4b and the welded portion W5b, and the welded portion W5b and the welded portion W6b. In this case, as in the welded member 100 of this embodiment, the influence of thermal distortion of the welded member 100b can be suppressed.
[0041] In addition, when the number of welds in the welded member is an even number, the effect of easily canceling out the thermal distortion can be obtained as described above. Even when the number of welds is an odd number, the effect of the thermal distortion can be suppressed compared to when the welding start and end points of all the welds are located at the same position when viewed from the central axis direction, or when all the welds are formed in the same direction along the circumferential direction.
[0042] (4c) In the above embodiment, the first welded portion W1 and the second welded portion W2 are each formed by full circumference welding, but the method of forming the welded portion is not limited to this. For example, the welded portion may be formed by welding a section of a predetermined length of a welding path that goes around the outer circumferential surface of the member. Specifically, as shown in Figs. 5A and 5B, in a cross section perpendicular to the central axis A, the shapes of the first welded portion W1c and the second welded portion W2c may each be an arc whose welding path is not closed. The circumferential length of the first welded portion W1c and the circumferential length of the second welded portion W2c are approximately the same.
[0043] In arc-shaped welding, the time it takes for the heat of welding to be transferred to the welded object is long in the range from the welding start point of the weld to approximately the center of the circumferential direction of the weld, so the heat capacity is likely to increase. In the arc-shaped first weld W1c, the first deformation point T1 located in the range from the welding start point S1c of the first weld W1c to approximately the center of the circumferential direction of the first weld W1c is the position that becomes the center of the deformation that occurs in the first weld W1c. In the arc-shaped second weld W2c, the second deformation point T2 located in the range from the welding start point S2c of the second weld W2c to approximately the center of the circumferential direction of the second weld W2c is the position that becomes the center of the deformation that occurs in the second weld W2c. The range from the welding start point of the first welded portion to approximately the circumferential center of the first welded portion is, for example, a range of approximately 180 degrees from the welding start point when the circumferential angle of the first welded portion is 360 degrees, and a range of approximately 90 degrees from the welding start point when the circumferential angle of the first welded portion is 180 degrees. Note that the range from the welding start point of the second welded portion to approximately the circumferential center of the second welded portion is also similar to that of the first welded portion.
[0044] For convenience, in FIG. 5A, the first deformation point T1 is illustrated at a position that is the center of the first welded portion W1c. However, the first deformation point T1 is not limited to the position that is the center of deformation in the range from the welding start point S1c of the first welded portion W1c to the approximately center in the circumferential direction of the first welded portion W1c. Similarly, in FIG. 5B, the second deformation point T2 is illustrated at a position that is the center of the second welded portion W2c. However, the second deformation point T2 is not limited to the position that is the center of deformation in the range from the welding start point S2c of the second welded portion W2c to the approximately center in the circumferential direction of the second welded portion W2c. In addition, the positions of the welding start point S1c and the welding start point S2c are not limited to the positions illustrated in FIG. 5A and FIG. 5B, and may be any position at either end of the arc.
[0045] The second deformation point T2 of the second welded portion W2c shown in FIG. 5B is disposed approximately 180° apart from the first deformation point T1 of the first welded portion W1c shown in FIG. 5A in the circumferential direction when viewed along the central axis A. Specifically, when the second welded portion W2c is moved along the central axis A and overlapped with the first welded portion W1c, the second deformation point T2 is disposed on an extension line of a straight line connecting the first deformation point T1 and the central axis A. That is, the first deformation point T1 and the second deformation point T2 face each other with the central axis A as the center. The second deformation point T2 of the second welded portion W2c may be disposed at least 90° apart from the first deformation point T1 of the first welded portion W1c in the circumferential direction.
[0046] The first welded portion W1c is deformed by thermal strain in the first direction D1c shown in FIG. 5A from the central axis A toward the first deformation point T1. The second welded portion W2c is deformed by thermal strain in the second direction D2c shown in FIG. 5B from the central axis A toward the second deformation point T2. As described above, the first welded portion W1c and the second welded portion W2c are formed so that the first deformation point T1 and the second deformation point T2 are positioned opposite to each other with the central axis A as the center. That is, the first direction D1c is opposite to the second direction D2c. Therefore, the deformation caused by thermal strain in the first direction D1c in the first welded portion W1c is easily offset by the deformation caused by thermal strain in the second direction D2c in the second welded portion W2c.
[0047] (4d) In the above embodiment, the circumferential length of the first welded portion W1 and the circumferential length of the second welded portion W2 were approximately the same. However, for example, the first welded portion and the second welded portion may be formed so as to have different circumferential lengths.
[0048] (4e) In the above embodiment, the welding directions of the first welded portion W1 and the second welded portion W2 were opposite to each other along the circumferential direction. However, for example, the welding directions of the first welded portion and the second welded portion may be the same along the circumferential direction.
[0049] (4f) In the above embodiment, the first part 1, the second part 2, and the third part 3 are connected in a state in which the end of the first part 1 is inserted into the opening of the first end 21 of the second part 2, and the end of the second part 2 is inserted into the opening of the second end 22 of the second part 2. However, for example, the first part, the second part, and the third part may be connected in a state in which the first end of the second part and the end of the first part are butted together, and the second end of the second part and the end of the second part are butted together. In this case, the first welded part is formed in the part where the first part and the second part are connected, and the second welded part is formed in the part where the second part and the third part are connected.
[0050] Furthermore, the first part 1, the second part 2 and the third part 3 may be arranged such that the first end 21 of the second part 2 is inserted into an opening on one end side of the first part 1, and the second end 22 of the second part 2 is inserted into an opening on one end side of the third part 3.
[0051] (4g) In the above embodiment, the first part 1, the second part 2, and the third part 3 are cylindrical parts, but the shapes of the first part, the second part, and the third part are not limited to this. For example, the first part, the second part, and the third part may be cylindrical parts having a shape other than a circle, or may be solid parts. The solid parts may be plate-shaped, block-shaped, column-shaped, etc.
[0052] (4h) In the above embodiment, the central axis A of the welded member 100 extends linearly. However, for example, the central axis of the welded member may be curved.
[0053] (4i) The function of one component in the above embodiments may be distributed among multiple components, or the functions of multiple components may be integrated into one component. Also, a part of the configuration of the above embodiments may be omitted. Also, at least a part of the configuration of the above embodiments may be added to or substituted for the configuration of another of the above embodiments.
[0054] [5. Technical Concepts Disclosed in This Specification] [Item 1] A method for manufacturing a welded component in which a first part, a second part, and a third part are welded together, comprising the steps of: welding the first part and the second part so as to form a first welded part extending in a circumferential direction about an axis of the welded member extending in a direction in which the first part, the second part, and the third part are arranged; welding the second component and the third component together to form a second weld portion extending in the circumferential direction; Equipped with The first welded portion and the second welded portion each extend from a welding start point to a welding end point, A position that is located in a range from the welding start point of the first welded portion to approximately the center of the first welded portion in the circumferential direction and that is the center of deformation occurring in the first welded portion is defined as a first deformation point; A second deformation point is a position located in a range from the welding start point of the second welded portion to approximately the center of the second welded portion in the circumferential direction and serving as a center of deformation occurring in the second welded portion, A method for manufacturing a welded component, wherein the second deformation point is disposed at least 90° apart from the first deformation point in the circumferential direction.
[0055] [Item 2] A method for producing a welded component according to item 1, A method for manufacturing a welded member, wherein a circumferential length of the first welded portion and a circumferential length of the second welded portion are approximately the same.
[0056] [Item 3] A method for producing a welded member according to item 1 or 2, A method for manufacturing a welded member, wherein the first welded portion and the second welded portion are formed by full circumference welding.
[0057] [Item 4] A method for producing a welded component according to item 3, The first deformation point is a welding end point which is the welding start point and the welding end point of the first welded portion, A method for manufacturing a welded component, wherein the second deformation point is a welding end point which is the welding start point and the welding end point of the second welded portion.
[0058] [Item 5] A method for producing a welded member according to any one of items 1 to 4, The method for manufacturing a welded member, wherein the welded member is an on-vehicle part to be mounted on a vehicle.
[0059] [Item 6] A method for producing a welded member according to any one of items 1 to 5, The first welded portion is formed by welding along a first circumferential direction around the axis, A method for manufacturing a welded member, wherein the second welded portion is formed by welding along a second circumferential direction centered on the axis, the second circumferential direction being opposite to the first circumferential direction. [Explanation of symbols]
[0060] 1...first part, 2...second part, 3...third part, 21...first end, 22...second end, 100, 100a, 100b...welded parts, A...central axis, D1, D1c...first direction, D2, D2c...second direction, S1, S1c...first welding end point, S1a-S6a...welding end points, S2, S2c...second welding end point, T1...first deformation point, T2...second deformation point, W1, W1c...first welded portion, W1b-W6b...welded portion, W2, W2c...second welded portion.
Claims
1. 1. A method for manufacturing a welded component in which a first part, a second part, and a third part are welded together, comprising the steps of: Welding the first part and the second part so as to form a first welded part extending in a circumferential direction about an axis of the weld member extending in a direction in which the first part, the second part, and the third part are arranged; welding the second component and the third component together to form a second weld portion extending in the circumferential direction; Equipped with The first welded portion and the second welded portion each extend from a welding start point to a welding end point, A position that is located in a range from the welding start point of the first welded portion to approximately the center of the first welded portion in the circumferential direction and that is a center of deformation occurring in the first welded portion is defined as a first deformation point; A second deformation point is a position located in a range from the welding start point of the second welded portion to approximately the center of the second welded portion in the circumferential direction and serving as a center of deformation occurring in the second welded portion, The second deformation point is disposed at an angle of at least 90° from the first deformation point in the circumferential direction.
2. A method for manufacturing a welded member according to claim 1, A method for manufacturing a welded member, wherein a circumferential length of the first welded portion and a circumferential length of the second welded portion are substantially the same.
3. A method for manufacturing a welded member according to claim 1, A method for manufacturing a welded member, wherein the first welded portion and the second welded portion are formed by full circumference welding.
4. A method for manufacturing a welded member according to claim 3, The first deformation point is a welding end point which is the welding start point and the welding end point of the first welded portion, A method for manufacturing a welded component, wherein the second deformation point is a welding end point which is the welding start point and the welding end point of the second welded portion.
5. A method for manufacturing a welded member according to any one of claims 1 to 4, The method for manufacturing a welded member, wherein the welded member is an on-vehicle part to be mounted on a vehicle.
6. A method for manufacturing a welded member according to any one of claims 1 to 4, The first welded portion is formed by welding along a first circumferential direction around the axis, A method for manufacturing a welded member, wherein the second welded portion is formed by welding along a second circumferential direction centered on the axis, the second circumferential direction being opposite to the first circumferential direction.
Citation Information
Patent Citations
Welding of long member
JP1984004978A
Welding method of tube
JP2000343218A
Welding apparatus and method
JP2002321077A
Welding apparatus, method, and program
JP2022123412A
Welding method and manufacturing method for combination members and manufacturing method for valve structure
JP3528746B2