Secondary battery and manufacturing method for secondary battery
The secondary battery design with airtightness maintaining and wrinkled portions effectively manages internal pressure, preventing rupture and electrolyte scattering by controlled peeling.
Patent Information
- Application Number
- JP2023067573
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-18
- Publication Date
- 2024-10-30
- Estimated Expiration
- 2043-04-18
AI Technical Summary
Existing secondary batteries face the risk of rupture due to unexpected increases in internal pressure, which can lead to the scattering of electrolyte.
A secondary battery design featuring a laminated electrode body enclosed in an exterior body with a thermally welded laminate sheet, incorporating airtightness maintaining portions and wrinkled portions with lower welding strength, allowing controlled peeling to manage internal pressure.
Prevents the exterior body from bursting by allowing controlled release of pressure through the peeling of the wrinkled portions, maintaining the integrity of the battery casing.
Smart Images

Figure 2024154004000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a secondary battery and a method for manufacturing a secondary battery. [Background technology]
[0002] Patent Document 1 discloses a lithium ion secondary battery in which a battery group, in which a positive electrode, a negative electrode, and a separator layer are laminated, is sealed in a sheet-like exterior body. An opening on the outer periphery of the exterior body is closed by a heat seal part with high peel strength. Furthermore, inside the heat seal part of the exterior body, an easy peel seal part with a peel strength lower than that of the heat seal part is formed. When gas is generated inside the exterior body and the internal pressure of the exterior body increases, the easy peel seal part peels off, thereby increasing the volume of the exterior body and suppressing the increase in internal pressure. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2002-015713 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the above structure, if the internal pressure of the exterior body increases unexpectedly, there is a risk that the exterior body will burst and the electrolyte inside the exterior body will splash out.
[0005] The present disclosure has been completed in light of the above circumstances, and has an object to prevent rupture caused by an increase in internal pressure of an exterior body. [Means for solving the problem]
[0006] The secondary battery of the first disclosure is a laminated electrode body in which a positive electrode plate, a negative electrode plate, and a separator are laminated; and an exterior body having a thermally weldable laminate sheet and sandwiching the laminated electrode body between the laminate sheets to house the laminated electrode body. A thermally welded portion is formed on an outer peripheral edge portion of the laminate sheet that surrounds the laminated electrode body, The thermally welded portion formed on at least one of the multiple sides that constitute the outer peripheral edge portion of the laminate sheet includes an airtightness maintaining portion and a wrinkled portion having a welding strength lower than that of the airtightness maintaining portion.
[0007] In this disclosure, the term "welding strength" is defined as the strength required to peel off a heat-sealed portion. In this disclosure, the term "wrinkle portion" is defined as a linearly extending bent portion such as a crease or a ridge-like protrusion.
[0008] The method for producing a secondary battery according to the second disclosure includes the steps of: a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; a first heat-welding step of forming a first airtightness maintaining portion by heat-welding the laminate sheets together at at least one of a plurality of side portions constituting an outer peripheral edge portion of the laminate sheet; A second thermal welding process is carried out to form a second airtightness maintaining portion and a wrinkled portion having a lower welding strength than the second airtightness maintaining portion by thermally welding an area adjacent to the first airtightness maintaining portion in the at least one side portion. Effect of the Invention
[0009] The portion where the laminate sheet is to be peeled off when the internal pressure of the exterior body increases can be set to a desired region. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a perspective view of a secondary battery according to a first embodiment; [Diagram 2] FIG. 1 is a perspective view showing a state in which a laminated electrode body and a tab are connected to each other; [Diagram 3] Exploded perspective view of a laminated electrode body [Figure 4] Front view of secondary battery [Diagram 5] Partially enlarged front view of a secondary battery [Figure 6] Partially enlarged perspective view of a secondary battery [Figure 7] FIG. 11 is a partially enlarged front view of a secondary battery according to a second embodiment; [Figure 8] FIG. 11 is a partially enlarged front view of a secondary battery according to a third embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Here, preferred embodiment examples of the present disclosure will be described. Any combination of the following embodiment examples without causing any contradiction is also included in the embodiment for carrying out the present invention.
[0012] (1) The secondary battery disclosed herein includes a laminated electrode body obtained by laminating a positive electrode plate, a negative electrode plate, and a separator, and an exterior body having a thermally weldable laminate sheet and sandwiching the laminated electrode body between the laminate sheets, the laminate sheet having a thermally welded portion formed on an outer peripheral edge portion surrounding the laminated electrode body, and the thermally welded portion formed on at least one of a plurality of sides constituting the outer peripheral edge portion of the laminate sheet includes an airtightness maintaining portion and a wrinkled portion having a welding strength lower than that of the airtightness maintaining portion. According to this configuration, when the internal pressure in the exterior body rises to a certain level, the wrinkled portion peels off, causing the internal pressure to drop to atmospheric pressure, thereby preventing the exterior body from bursting due to an excessive rise in internal pressure. Since the thermally welded portion has an airtightness maintaining portion with high welding strength and a wrinkled portion with low welding strength, and the wrinkled portion with low welding strength is formed on a specific side portion, the peeling position of the laminate sheet can be set arbitrarily.
[0013] (2) In (1), a tab connected to the laminated electrode body penetrates the heat-sealed portion and protrudes to the outside of the exterior body, and the wrinkled portion is formed in a region of the laminate sheet that contacts the tab. With this configuration, the heat-sealed portion has a lower welding strength in a welding region where the seal material contacts the tab than in a welding region where the seal materials of the laminate sheet directly contact each other. Therefore, when peeling occurs in the wrinkled portion, the range of peeling is likely to spread in the welding region between the tab and the laminate sheet.
[0014] (3) In (1) or (2), the laminate sheet has a three-dimensionally curved non-welded portion, and the non-welded portion is disposed in a position close to or adjacent to the wrinkled portion. Since stress is likely to concentrate in the three-dimensionally curved non-welded portion when the laminate sheet expands, the wrinkled portion close to or adjacent to the non-welded portion is likely to peel off.
[0015] (4) In (3), the non-welded portion has a ridge portion. The ridge portion has a relatively large curvature, so that it is a portion where stress is more likely to concentrate than a flat portion. Therefore, the wrinkled portion close to or adjacent to the ridge portion is more likely to peel off.
[0016] (5) In (4), the ridge portion has an arc shape when viewed in the direction in which the laminate sheet is pressed when the thermally welded portion is formed.
[0017] (6) A method for manufacturing a secondary battery according to the second disclosure includes a step of enclosing a laminated electrode body, in which a positive electrode plate, a negative electrode plate, and a separator are laminated, in a sandwiched state with laminate sheets constituting an exterior body, a first heat-sealing step of forming an airtightness maintaining portion by heat-sealing the laminate sheets in at least one of a plurality of sides constituting an outer peripheral edge portion of the laminate sheets, and a second heat-sealing step of forming a second airtightness maintaining portion and a wrinkled portion having a lower welding strength than the second airtightness maintaining portion by heat-sealing an area adjacent to the first airtightness maintaining portion in the at least one side. According to this manufacturing method, when the internal pressure in the exterior body rises to a certain level, the wrinkled portion peels off, causing the internal pressure to drop to atmospheric pressure, thereby preventing the exterior body from bursting due to an excessive rise in internal pressure. Since the second airtightness maintaining portion having a high welding strength and the wrinkled portion having a lower welding strength than the second airtightness maintaining portion are formed on the specific side portion, the peeling position of the laminate sheet can be set arbitrarily.
[0018] [Embodiment 1] A first embodiment of the present disclosure will be described with reference to Figs. 1 to 6. Note that the present invention is not limited to these examples, but is defined by the claims, and includes all modifications within the meaning and scope equivalent to the claims. In this first embodiment, with regard to the front-rear direction, the F direction in Figs. 1 to 3 and 6 is defined as the front. With regard to the left-right direction, the R direction in Figs. 1 to 6 is defined as the right. The left-right direction and the width direction are used synonymously. With regard to the up-down direction, the H direction in Figs. 1 to 6 is defined as the up.
[0019] The laminated secondary battery A of the present embodiment 1 is in a form in which the entire laminated electrode body 10 and the base ends of the pair of tabs 16 are liquid-tightly enclosed by an exterior body 20. An electrolyte (not shown) is stored in the exterior body 20. As shown in FIG. 3, the laminated electrode body 10 is configured by stacking a plurality of negative electrode plates 11 (electrode plates) and a plurality of positive electrode plates 12 (electrode plates) in the front-rear direction with a plurality of sheet-like separators 13 (not shown) sandwiched between them. A connection portion 14 consisting of an uncoated portion where no slurry is applied is formed on the right edge portion of the negative electrode plate 11 and the left edge portion of the positive electrode plate 12, respectively. The negative electrode plate 11 and the positive electrode plate 12 are stacked so that the respective connection portions 14 are located on opposite sides to each other in the left-right direction. The portion of the laminated electrode body 10 that is stacked with the separator 13 sandwiched therebetween is defined as an electrode stacking portion 15.
[0020] The tabs 16 are metal members each having a long and narrow plate shape extending in the vertical direction. The pair of tabs 16 are fixed to the front faces of the left and right connection portions 14 with their plate thickness direction facing the front-rear direction. The connection portions 14 and the tabs 16 are arranged along both left and right side edges of the electrode laminated portion 15. The tabs 16 protrude upward beyond the upper end of the connection portions 14. The thickness dimension in the front-rear direction of the overlapping portion where the connection portions 14 and the tabs 16 are overlapped in the front-rear direction is smaller than the thickness dimension in the front-rear direction of the electrode laminated portion 15.
[0021] The exterior body 20 is formed by thermally welding the outer periphery of two rectangular laminate sheets 21. The laminate sheet 21 has an aluminum sheet-like base material (not shown) and a seal material (not shown) made of PP or the like superimposed on the inner surface of the sheet-like base material. The seal material forms the mating surface between the laminate sheets 21. The seal material is made of, for example, a thermoplastic resin such as polypropylene (PP) having a melting point of about 160°C. The two laminate sheets 21 are arranged so that the seal material faces the other laminate sheet 21 and sandwich the laminated electrode body 10 and the tab 16 in the front-rear direction. A heat-welded portion 22 is formed around the entire periphery of the outer periphery of the pair of laminate sheets 21. In a front view of the secondary battery A seen from the front, the heat-welded portion 22 is arranged so as to surround the entire laminated electrode body 10.
[0022] The outer peripheral edge of the laminate sheet 21 is composed of four sides 23, 24L, 24R, and 25, i.e., top, bottom, left and right. The heat-sealed portion 22 of the lower side 23 is composed only of a first airtightness maintaining portion 26 formed by directly contacting and heat-sealing a pair of laminate sheets 21 to each other over the entire area of the lower side 23. The heat-sealed portion 22 of the right side 24R is composed only of a first airtightness maintaining portion 26 formed by directly contacting and heat-sealing a pair of laminate sheets 21 to each other over the entire area of the right side 24R. The heat-sealed portion 22 of the left side 24L is composed only of a first airtightness maintaining portion 26 formed by directly contacting and heat-sealing a pair of laminate sheets 21 to each other over the entire area of the left side 24L.
[0023] At both left and right ends of the upper side portion 25, a tab 16 is sandwiched between the front and rear laminate sheets 21. The tab 16 penetrates the heat-sealed portion 22 of the upper side portion 25 and protrudes upward from the exterior body 20. The heat-sealed portion 22 of the upper side portion 25 is composed of a first airtightness maintaining portion 26, a pair of left and right second airtightness maintaining portions 27, and a wrinkled portion 30. The first airtightness maintaining portion 26 is formed only in the region of the upper side portion 25 between the left and right tabs 16. The first airtightness maintaining portion 26 of the upper side portion 25 is a portion that is heat-sealed with the pair of laminate sheets 21 in direct contact with each other, similar to the first airtightness maintaining portions 26 of the lower side portion 23 and the left and right side portions 24L, 24R.
[0024] The pair of left and right second airtightness maintaining parts 27 are formed by thermally welding the first airtightness maintaining parts 26 formed on the upper side part 25 and the left and right side parts 24L, 24R. The second airtightness maintaining parts 27 are formed in the area of the laminate sheet 21 that contacts the tab 16. The right second airtightness maintaining part 27 is disposed between the upper end of the first airtightness maintaining part 26 formed on the right side part 24R and the right end of the first airtightness maintaining part 26 formed on the upper side part 25. The left second airtightness maintaining part 27 is disposed between the upper end of the first airtightness maintaining part 26 formed on the left side part 24L and the left end of the first airtightness maintaining part 26 formed on the upper side part 25. The second airtightness maintaining part 27 is formed by thermally welding the area of the laminate sheet 21 that contacts the tab 16.
[0025] In a plan view of secondary battery A seen from above, second airtightness maintaining portion 27 is bent to form a trapezoid along the front surface and both left and right side surfaces of tab 16. In a state in which second airtightness maintaining portion 27 is not formed, the outer peripheral edge portion of laminate sheet 21 faces tab 16 with a small clearance between two formed first airtightness maintaining portions 26 located on both the left and right sides of tab 16. The second airtightness maintaining portion 27 and wrinkled portion 30 are formed by closely adhering a portion of laminate sheet 21 facing tab 16 with a clearance therebetween to tab 16 and heat welding it thereto.
[0026] The second airtightness maintaining portion 27 has a front welded portion 28 welded to the front surface of the tab 16, and a pair of left and right side welded portions 29L, 29R welded to both left and right side surfaces of the tab 16. The second airtightness maintaining portion 27 is in close contact with the front surface and both left and right side surfaces of the tab 16 in a face-to-face contact state (parallel state), so the weld strength of the second airtightness maintaining portion 27 is relatively large, similar to the first airtightness maintaining portion 26. In the present embodiment 1, the "weld strength" is defined as the strength required to peel off the thermal welded portion 22.
[0027] The wrinkled portion 30 is a portion formed by an excess portion of the laminate sheet when the second airtightness maintaining portion 27 is formed, and is disposed within the range of the forming area of the second airtightness maintaining portion 27. In the present embodiment 1, the "wrinkled portion 30" is defined as a bent portion having a shape that protrudes like a mountain fold or a ridge line and extends in a straight or curved shape. The wrinkled portion 30 is a portion that is raised higher than a portion of the second airtightness maintaining portion 27 where the wrinkled portion 30 is not formed, and has a lower degree of adhesion to the outer surface of the tab 16. Therefore, the welding strength of the wrinkled portion 30 is lower than that of the first airtightness maintaining portion 26. As shown in Figs. 5 and 6, in the second airtightness maintaining portion 27 on the right side, the wrinkled portion 30 is formed in the front welding portion 28 and the left side welding portion 29L. In the second airtightness maintaining portion 27 on the left side, the wrinkled portion 30 is formed in the front welding portion 28 and the right side welding portion 29R.
[0028] The exterior body 20 (the front laminate sheet 21) has a pair of left and right non-welded parts 32. The non-welded parts 32 are arranged in a region close to or adjacent to the wrinkled parts 30, and are parts for promoting peeling at the wrinkled parts 30. When the internal pressure of the exterior body 20 is maintained at atmospheric pressure or a pressure close to atmospheric pressure, the non-welded parts 32 maintain a three-dimensionally curved shape due to the shape retention of aluminum, which is the material of the laminate sheet 21. The non-welded parts 32 are parts that are not thermally welded to a solid object. Therefore, when the electrolyte contained in the exterior body 20 evaporates and becomes a vaporized gas, and the internal pressure in the exterior body 20 becomes a pressure higher than atmospheric pressure, the non-welded parts 32 are deformed so as to swell as the internal volume of the exterior body 20 increases.
[0029] Next, the non-welded portion 32 located on the right side will be described. The non-welded portion 32 located on the left side has a shape symmetrical to the non-welded portion 32 on the right side, so the description of the shape will be omitted. The non-welded portion 32 on the right side is adjacent to the right end of the first airtightness maintaining portion 26 of the upper side portion 25, the upper end of the first airtightness maintaining portion 26 of the right side portion 24R, and the second airtightness maintaining portion 27 on the right side. The non-welded portion 32 is three-dimensionally curved in accordance with the shapes of the laminated electrode body 10 and the tab 16. In detail, the three-dimensional shape of the non-welded portion 32 is configured to include a first front portion 33, a second front portion 34, a third front portion 35, an upper surface portion 36, a first side portion 37, a first curved surface portion 38, a second curved surface portion 39, a first ridge portion 40, a first valley portion 44, a second ridge portion 47, and a second valley portion 48.
[0030] The first front portion 33 is disposed so as to cover the electrode laminated portion 15 from the front in a front view. The first front portion 33 is located at the front end of the laminate sheet 21 in the front-rear direction. The second front portion 34 is disposed to the right of the first front portion 33 and to the left of the first airtightness maintaining portion 26 of the right side portion 24R in a front view, and is disposed so as to cover the tab 16 from the front. The upper end edge of the second front portion 34 is connected to the lower edge of the front welding portion 28 of the second airtightness maintaining portion 27. The second front portion 34 is disposed behind the first front portion 33. The third front portion 35 is disposed above the first front portion 33 and to the left of the upper end of the second front portion 34 in a front view. The upper edge of the third front portion 35 is connected to the lower edge of the first airtightness maintaining portion 26 of the upper side portion 25.
[0031] The upper surface portion 36 is located so as to connect the upper edge of the first front surface portion 33 and the lower edge of the third front surface portion 35, and faces upward. The first side surface portion 37 is located so as to connect the right edge of the first front surface portion 33 and the left edge of the second front surface portion 34, and faces rightward. The first curved surface portion 38 is located so as to connect the right end of the upper surface portion 36 and the upper end of the first side surface portion 37. The first curved surface portion 38 is curved so as to bulge in a quarter-circular arc in front view, and faces diagonally upward and to the right. The second curved surface portion 39 is located so as to connect the right end of the upper surface portion 36 and the lower end of the left side surface welding portion 29L. The second curved surface portion 39 is curved so as to dent in a quarter-circular arc in front view, and faces diagonally upward and to the left. The upper end of the second curved surface portion 39 is connected to the lower end of the left side surface welding portion 29L of the second airtightness maintaining portion 27.
[0032] The first ridge 40 is located along the outer edge of the first front surface 33. The first ridge 40 has a first horizontal ridge 41, a first vertical ridge 42, and a first arcuate ridge 43. The first horizontal ridge 41 forms a boundary between the upper edge of the first front surface 33 and the front edge of the upper surface 36, and is a portion extending in the left-right direction. The first vertical ridge 42 forms a boundary between the right edge of the first front surface 33 and the front edge of the first side surface 37, and is a portion extending in the up-down direction. The first arcuate ridge 43 forms a boundary between the upper right edge of the first front surface 33 and the front edge of the first curved surface 38. The first arcuate ridge 43 is a portion connected to the right end of the first horizontal ridge 41 and the upper end of the first vertical ridge 42, and curved in a quarter-circular arc shape so as to bulge upward and to the right when viewed from the front.
[0033] The first valley 44 is located along the outer edge of the second front surface 34. The first valley 44 has a first vertical valley 45 and a first arcuate valley 46. The first vertical valley 45 forms the boundary between the left edge of the second front surface 34 and the rear edge of the first side surface 37, and is a portion extending in the vertical direction. The first arcuate valley 46 forms the boundary between the left edge of the second front surface 34 and the rear edge of the first curved surface 38. The first arcuate valley 46 is located along the first arcuate ridge 43 in a front view, and is a portion curved in a quarter-circular arc shape so as to bulge to the upper right. The first arcuate valley 46 is connected to the upper end of the first vertical valley 45.
[0034] The second ridge portion 47 is located along the outer edge of the second front surface portion 34. The second ridge portion 47 forms the boundary between the left edge of the second front surface portion 34 and the front edge of the second curved surface portion 39, and is a portion that curves in a quarter-circular arc so as to be recessed downward and to the right in a front view. In a front view, the lower left end of the second ridge portion 47 is connected to the upper left end of the first arc-shaped valley portion 46 of the first valley portion 44 so as to form an acute angle.
[0035] The second valley 48 is located along the outer edge of the third front surface 35. The second valley 48 has a second horizontal valley 49 and a second arcuate valley 50. The second horizontal valley 49 forms the boundary between the lower edge of the third front surface 35 and the rear edge of the upper surface 36, and is a portion that extends horizontally in a front view. The second arcuate valley 50 forms the boundary between the right edge of the third front surface 35 and the rear edge of the second curved surface 39. The second arcuate valley 50 is located along the second ridge 47 in a front view, and is a portion that curves in a quarter-circular arc shape so as to be recessed downward to the right.
[0036] The manufacturing process of the secondary battery A will be described. The laminated electrode body 10 and the tab 16 are sandwiched between two laminate sheets 21, and among the four sides 23, 24L, 24R, 25 of the outer periphery of the laminate sheet 21, the lower side 23 and both left and right sides 24L, 24R are thermally welded to form the first airtightness maintaining portion 26 on these three sides 23, 24L, 24R. Next, an electrolyte (not shown) is injected into the exterior body 20 from the opening of the upper side 25. Next, the first airtightness maintaining portion 26 is formed in the region of the upper side 25 between the pair of tabs 16. After that, the left and right ends of the upper side 25 are thermally welded to form the second airtightness maintaining portion 27 and the wrinkled portion 30. This completes the manufacturing of the secondary battery A.
[0037] When the secondary battery A is used and part of the electrolyte becomes vaporized gas with an increase in temperature, the internal pressure of the exterior body 20 increases, causing the non-welded portion 32 to swell and deform. The effect of deformation of the upper end of the second front portion 34 and the second curved portion 39 connected to the second airtightness maintaining portion 27 of the non-welded portion 32 extends to the second airtightness maintaining portion 27. As a result, the front and rear laminate sheets 21 peel off from each other at the wrinkled portion 30 of the second airtightness maintaining portion 27, which has a low welding strength. The vaporized gas is released to the outside of the exterior body 20 from an opening (not shown) in the upper side portion 25 caused by the peeling of the laminate sheet 21, so there is no risk of the exterior body 20 bursting. Since the opening is formed only in the upper side portion 25, even if an opening is formed, there is no risk of the electrolyte in the exterior body 20 leaking out.
[0038] The secondary battery A of the first embodiment includes a laminated electrode body 10 and an exterior body 20. The laminated electrode body 10 is formed by laminating a positive electrode plate 12, a negative electrode plate 11, and a separator 13. The exterior body 20 has a laminate sheet 21 that can be heat-sealed, and the laminated electrode body 10 is sandwiched between the laminate sheets 21 and housed therein. A heat-sealed portion 22 is formed on the outer peripheral edge of the laminate sheet 21 that surrounds the laminated electrode body 10. The heat-sealed portion 22 formed on the upper side portion 25 of the multiple sides 23, 24L, 24R, and 25 that constitute the outer peripheral edge of the laminate sheet 21 includes a first airtightness maintaining portion 26, a second airtightness maintaining portion 27, and a wrinkled portion 30 whose welding strength is lower than that of the first airtightness maintaining portion 26 and the second airtightness maintaining portion 27.
[0039] The manufacturing method of the secondary battery A includes a lamination process, a first heat-sealing process, and a second heat-sealing process. In the lamination process, the laminated electrode body 10, which is a laminate of the positive electrode plate 12, the negative electrode plate 11, and the separator 13, is sandwiched and surrounded by the laminate sheet 21 constituting the exterior body 20. In the first heat-sealing process, the laminate sheets 21 are brought into close contact with each other and heat-sealed at a plurality of sides 23, 24L, 24R, and 25 constituting the outer periphery of the laminate sheet 21, thereby forming a first airtightness maintaining portion 26. In the second heat-sealing process, a region adjacent to the first airtightness maintaining portion 26 at the upper side portion 25 is heat-sealed to form a second airtightness maintaining portion 27 and a wrinkled portion 30 having a lower welding strength than the second airtightness maintaining portion 27.
[0040] When the internal pressure in exterior body 20 rises to a certain level, wrinkled portion 30 peels off, causing the internal pressure to drop to atmospheric pressure, so that secondary battery A of this embodiment 1 can prevent rupture of exterior body 20 caused by an excessive rise in internal pressure. Secondary battery A of this embodiment 1 has heat-sealed portion 22 having airtightness maintaining portions (first airtightness maintaining portion 26 and second airtightness maintaining portion 27) with high welding strength and wrinkled portion 30 with low welding strength, and wrinkled portion 30 with low welding strength is formed on a specific side portion (upper side portion 25), so that the peeling position of laminate sheet 21 can be set arbitrarily.
[0041] Tab 16 connected to laminated electrode body 10 penetrates heat-sealed portion 22 and protrudes to the outside of exterior body 20. Wrinkled portion 30 is formed in a region (second airtightness maintaining portion 27) of laminate sheet 21 that contacts tab 16. With this configuration, the weld strength of the welded region (second airtightness maintaining portion 27) where the seal material contacts tab 16 is lower than that of the welded region (first airtightness maintaining portion 26) of heat-sealed portion 22 where the seal materials of laminate sheet 21 directly contact each other. Therefore, when peeling occurs in wrinkled portion 30, the range of peeling is likely to spread in the welded region (second airtightness maintaining portion 27) between tab 16 and laminate sheet 21.
[0042] Laminate sheet 21 has three-dimensionally curved non-welded portion 32. Non-welded portion 32 is disposed in a position close to wrinkled portion 30 or adjacent to wrinkled portion 30. Since stress is likely to concentrate in three-dimensionally curved non-welded portion 32 when laminate sheet 21 expands, wrinkled portion 30 close to or adjacent to non-welded portion 32 is likely to peel off.
[0043] The non-welded portion 32 has a first ridge portion 40 and a second ridge portion 47. The first ridge portion 40 and the second ridge portion 47 are areas where stress is more likely to concentrate than other flat areas (first front portion 33, top surface portion 36, first side surface portion 37, first curved surface portion 38, second front portion 34, second curved surface portion 39). Therefore, the wrinkled portion 30 close to or adjacent to the ridge portion is more likely to peel off. The first ridge portion 40 and the second ridge portion 47 are arc-shaped when viewed in the direction in which the laminate sheet 21 is pressed when the heat-welded portion 22 is formed (front-rear direction).
[0044] <Embodiment 2> Next, a second embodiment of the present disclosure will be described with reference to Fig. 7. In a secondary battery B of the second embodiment, the shape of a portion of a non-welded portion 51 is different from that of the first embodiment. Since the other configurations are the same as those of the first embodiment, the same reference numerals are used for the same configurations, and descriptions of the structures, functions, and effects will be omitted.
[0045] The non-welded portion 51 of the second embodiment is formed by forming a bent surface portion 52, a bent ridge portion 53, and a bent valley portion 54 instead of the second curved surface portion 39, the second ridge portion 47, and the second valley portion 48 of the first embodiment. The bent surface portion 52 has a portion extending upward from the right end of the upper surface portion 36 and a portion extending leftward from the lower end of the left side surface welded portion 29L of the second airtightness maintaining portion 27. The bent surface portion 52 is bent in an L-shape in a front view. The bent ridge portion 53 constitutes a boundary line between the front edge portion of the bent surface portion 52 and the left edge portion of the second front surface portion 34. The bent valley portion 54 constitutes a boundary line between the rear edge portion of the bent surface portion 52 and the right edge portion of the third front surface portion 35 and the right end portion of the first airtightness maintaining portion 26.
[0046] <Embodiment 3> Next, a third embodiment of the present disclosure will be described with reference to Fig. 8. In a secondary battery C of the third embodiment, the shape of a portion of a non-welded portion 55 is different from that of the first embodiment. Since the other configurations are the same as those of the first embodiment, the same reference numerals are used for the same configurations, and descriptions of the structures, functions, and effects will be omitted.
[0047] The non-welded portion 55 of the third embodiment is formed by forming a sloping portion 56, a diagonal ridge portion 57, and a diagonal valley portion 58 instead of the second curved surface portion 39, the second ridge portion 47, and the second valley portion 48 of the first embodiment. The sloping portion 56 is a portion that extends in a straight line from the right end of the upper surface portion diagonally upward to the upper right. The upper end of the sloping portion 56 is connected to the lower end of the left side welded portion 29L of the second airtightness maintaining portion 27. The diagonal ridge portion 57 forms a boundary line between the front edge of the sloping portion 56 and the left edge of the second front surface portion 34. The diagonal valley portion 58 forms a boundary line between the rear edge of the sloping portion 56 and the right edge of the third front surface portion 35 and the right end of the first airtightness maintaining portion 26.
[0048] <Other Examples> The present invention is not limited to the embodiments described above and illustrated in the drawings, and the following embodiments are also included within the technical scope of the present invention.
[0049] In the first to third embodiments, the wrinkled portions and the non-welded portions are formed only on the front laminate sheet, but the wrinkled portions and the non-welded portions may be formed on both the front laminate sheet and the rear laminate sheet. In the first to third embodiments, the wrinkles may be formed in an area that does not contact the tab. In the first to third embodiments, the non-welded portion does not have to be curved three-dimensionally. In the first to third embodiments, the non-welded portion may have a shape that does not have a ridge line portion. In the first to third embodiments, the wrinkles are not limited to being formed on one side, but may be formed on a plurality of sides. In the first to third embodiments, the side portion forming the airtightness maintaining portion and the wrinkled portion is not limited to the upper side portion, and may be a side portion. In the first to third embodiments, the laminated electrode body may be sandwiched between a single laminate sheet folded in half. In this case, heat-sealed portions may be formed on three sides. [Explanation of symbols]
[0050] A…Secondary battery 10...Laminated electrode body 11...Negative electrode plate 12…Positive electrode plate 13…Separator 16…Tab 20…Exterior body 21...Laminate sheet 22…Heat welding part 23…Bottom (edge) 24R…Right side (side) 24L…Left side (side) 25...Top side (edge) 26…First airtightness maintaining unit (airtightness maintaining unit) 27...Second airtightness maintaining section (airtightness maintaining section) 30…Wrinkle area 32…Non-welded part 44…First ridge (ridge) 47…Second ridge (ridge) 51…Non-welded part 53...Bent ridgeline (ridgeline) 55…Non-welded part 56...Diagonal ridgeline (ridgeline)
Claims
1. a laminated electrode body in which a positive electrode plate, a negative electrode plate, and a separator are laminated; and an exterior body having a thermally weldable laminate sheet and sandwiching the laminated electrode body between the laminate sheets to house the laminated electrode body. A thermally welded portion is formed on an outer peripheral edge portion of the laminate sheet that surrounds the laminated electrode body, A secondary battery, wherein the thermal welding portion formed on at least one of the multiple sides constituting the outer peripheral edge portion of the laminate sheet includes an airtightness maintaining portion and a wrinkled portion having a welding strength lower than that of the airtightness maintaining portion.
2. a tab connected to the laminated electrode body penetrates the thermally welded portion and protrudes to the outside of the exterior body; The secondary battery according to claim 1 , wherein the wrinkled portion is formed in an area of the laminate sheet that contacts the tab.
3. The laminate sheet has a three-dimensionally curved non-welded portion, 3. The secondary battery according to claim 1, wherein the non-welded portion is disposed in the vicinity of the wrinkled portion or adjacent to the wrinkled portion.
4. The secondary battery according to claim 3 , wherein the non-welded portion has a ridge portion.
5. The secondary battery according to claim 4 , wherein the ridge portion has an arc shape when viewed in a direction in which the laminate sheet is pressed when the thermally welded portion is formed.
6. a step of sandwiching and enclosing a laminated electrode body obtained by stacking a positive electrode plate, a negative electrode plate, and a separator between laminate sheets constituting an exterior body; a first heat-welding step of heat-welding the laminate sheets together at least one of a plurality of sides constituting an outer peripheral edge of the laminate sheet to form a first airtightness maintaining portion; A method for manufacturing a secondary battery, comprising: carrying out a second thermal welding process in which a region adjacent to the first airtightness maintaining portion is thermally welded in at least one of the sides to form a second airtightness maintaining portion and a wrinkled portion having a lower welding strength than the second airtightness maintaining portion.
Citation Information
Patent Citations
Lithium ion secondary battery
JP2002015713A
Battery and manufacturing device of battery
JP2006185713A
Battery cells with improved safety
JP2010525524A
Laminated battery
JP2016039095A
Pouch-type secondary battery having unsealed portion
US20200358044A1