Power storage device

The power storage device employs a multi-layered current collector foil with varying materials and surface roughness to prevent short circuits and enhance durability, addressing the issue of pinhole-induced damage in conventional designs.

JP2024154302APending Publication Date: 2024-10-30GS YUASA CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023068061
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

Conventional power storage devices are prone to damage and short circuits due to pinholes in the current collector foils, which can occur in the positive or negative metal layers.

Method used

The power storage device is designed with a current collector foil comprising multiple layers, including an opposing layer and a non-opposing layer, where at least one of these layers is formed of different materials or the same material, and the surfaces facing each other have varying roughness to enhance contact area and reduce electrical resistance.

Benefits of technology

This design effectively suppresses damage to the current collector foil, reducing the likelihood of short circuits and improving the device's durability and energy density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154302000001_ABST
    Figure 2024154302000001_ABST
Patent Text Reader

Abstract

To provide a power storage device in which the damage of a current collecting foil can be suppressed.SOLUTION: A power storage device includes a plurality of electrode units 100 that are stacked. Each of the electrode units includes at least a current collecting foil 110 in which a positive electrode metal layer 111 and a negative electrode metal layer 112 are stacked, a positive electrode active material layer 120 formed on the positive electrode metal layer, and a negative electrode active material layer 130 formed on the negative electrode metal layer. At least one metal layer of the positive electrode metal layer and the negative electrode metal layer is formed of a plurality of layers including a counter layer 113, which is a metal foil facing the other metal layer, and a non-counter layer 114, which is a metal foil on the opposite side of the other metal layer.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electricity storage device. [Background technology]

[0002] Patent Document 1 discloses an electricity storage device in which a positive electrode active material layer is disposed on the surface of a positive electrode current collector, and a negative electrode active material layer is disposed on the surface of a negative electrode current collector. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2022-77634 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the above-mentioned conventional electricity storage devices, if a pinhole occurs in at least one of the positive and negative metal layers of the current collecting foil, it may cause a defect such as a short circuit, and therefore it is important to suppress damage to the current collecting foil.

[0005] The present invention was made by the present inventors by focusing on the above-mentioned problem, and has an object to provide an electricity storage device capable of suppressing damage to the current collecting foil. [Means for solving the problem]

[0006] An energy storage device according to one embodiment of the present invention includes a plurality of stacked electrode units, each of which has at least a current collecting foil in which a positive electrode metal layer and a negative electrode metal layer are stacked, a positive electrode active material layer formed on the positive electrode metal layer, and a negative electrode active material layer formed on the negative electrode metal layer, and at least one of the metal layers of the positive electrode metal layer and the negative electrode metal layer is formed of multiple layers having an opposing layer which is a metal foil that faces the other metal layer, and a non-opposing layer which is a metal foil on the opposite side to the other metal layer. Effect of the Invention

[0007] According to the electricity storage device of the present invention, damage to the current collecting foil can be suppressed. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a perspective view showing the appearance of a power storage device according to an embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing an internal configuration of the electricity storage device according to the embodiment. [Diagram 3] FIG. 3 is a perspective view and a cross-sectional view showing a configuration of an electrode unit included in the power storage device according to the embodiment. [Figure 4] FIG. 4 is a cross-sectional view showing the configuration of a current collector foil of an electrode unit according to an embodiment. [Diagram 5] FIG. 5 is a cross-sectional view illustrating a manufacturing process in a manufacturing method for an electricity storage device according to an embodiment. [Figure 6] FIG. 6 is a cross-sectional view showing the configuration of a current collector foil according to the first modification of the embodiment. [Figure 7] FIG. 7 is a cross-sectional view showing the configuration of a current collector foil according to the second modification of the embodiment. [Figure 8] FIG. 8 is a cross-sectional view showing the configuration of a current collector foil according to the third modification of the embodiment. [Figure 9] FIG. 9 is a cross-sectional view showing the configuration of the electricity storage pack. [Figure 10] FIG. 10 is a cross-sectional view showing another configuration of the electricity storage pack. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] (1) An energy storage device according to one embodiment of the present invention includes a plurality of stacked electrode units, each of which has at least a current collecting foil in which a positive electrode metal layer and a negative electrode metal layer are stacked, a positive electrode active material layer formed on the positive electrode metal layer, and a negative electrode active material layer formed on the negative electrode metal layer, and at least one of the metal layers of the positive electrode metal layer and the negative electrode metal layer is formed of multiple layers having an opposing layer that is a metal foil that faces the other metal layer, and a non-opposing layer that is a metal foil on the opposite side to the other metal layer.

[0010] According to this, in the electricity storage device, at least one of the positive and negative metal layers of the current collector foil is formed of multiple layers (multiple metal foils) having an opposing layer that faces the other metal layer and a non-opposing layer on the opposite side to the other metal layer. In this way, by forming the metal layer of the current collector foil from multiple layers, the metal layer can be reinforced, and damage to the current collector foil can be suppressed.

[0011] (2) In the electricity storage device described above in (1), the opposed layer and the other metal layer may be formed of different materials.

[0012] According to this, by forming the opposing layer of one metal layer and the other metal layer from different materials (i.e., they do not have to be formed from the same material), the opposing layer and the other metal layer can each be formed from a suitable material.

[0013] (3) In the power storage device according to (1) or (2) above, the facing layer and the non-facing layer may be formed of the same material.

[0014] According to this, by forming the facing layer and the non-facing layer of the one metal layer from the same material, the one metal layer can be formed from the same material.

[0015] (4) In the electricity storage device according to any one of (1) to (3) above, the positive electrode metal layer may be formed of the multiple layers.

[0016] According to this, since the positive electrode metal layer is generally formed from an easy-to-handle material such as aluminum foil, by forming the positive electrode metal layer as one of the metal layers in multiple layers, the one of the metal layers can be easily formed.

[0017] (5) In the energy storage device described in any one of (1) to (4) above, a surface of the non-opposing layer facing the opposing layer may have a surface roughness greater than a surface of the non-opposing layer opposite to the opposing layer.

[0018] According to this, the surface of the non-facing layer facing the facing layer has a rougher surface than the opposite surface, so that the contact area between the facing layer and the non-facing layer can be increased, thereby reducing the electrical resistance of the multiple layers having the facing layer and the non-facing layer.

[0019] (6) In the energy storage device described in any one of (1) to (5) above, a surface of the opposing layer facing the non-opposing layer may have a surface roughness greater than a surface of the opposing layer opposite the non-opposing layer.

[0020] According to this, the surface of the opposing layer facing the non-opposing layer has a rougher surface than the opposite surface, so that the contact area between the opposing layer and the non-opposing layer can be increased, thereby reducing the electrical resistance of the multiple layers having the opposing layer and the non-opposing layer.

[0021] (7) In the power storage device according to any one of (1) to (6) above, at least one of the facing layer and the non-facing layer may be thicker than the other metal layer.

[0022] According to this, by making at least one of the facing layer and the non-facing layer thicker than the other metal layer, it is possible to suppress the occurrence of pinholes in the metal layer formed of multiple layers.

[0023] Hereinafter, a description will be given of a power storage device according to an embodiment (including modified examples) of the present invention with reference to the drawings. Note that the embodiments described below are all comprehensive or specific examples. The numerical values, shapes, materials, components, the arrangement and connection of the components, manufacturing processes, and the order of the manufacturing processes shown in the following embodiments are merely examples and are not intended to limit the present invention. In each drawing, the dimensions are not strictly shown. In each drawing, the same or similar components are given the same reference numerals.

[0024] In the following description and drawings, the longitudinal direction of the power storage device, or the opposing direction of a pair of short side surfaces of the power storage device, is defined as the X-axis direction. The opposing direction of a pair of long side surfaces of the power storage device is defined as the Y-axis direction. The thickness direction of the power storage device, the stacking direction of the multiple electrode units, the stacking direction of the current collecting foils and active material layers, the arrangement direction of a pair of end members, or the up-down direction is defined as the Z-axis direction. These X-axis, Y-axis, and Z-axis directions intersect with each other (orthogonal in this embodiment). Note that, depending on the mode of use, the Z-axis direction may not be the up-down direction, but for convenience of explanation, the following description will be given assuming that the Z-axis direction is the up-down direction.

[0025] In the following description, the positive X-axis direction refers to the direction of the X-axis arrow, and the negative X-axis direction refers to the opposite direction to the positive X-axis direction. When simply referring to the X-axis direction, it refers to both or either of the positive and negative X-axis directions. The same applies to the Y-axis and Z-axis directions. Expressions indicating relative directions or attitudes, such as parallel and perpendicular, also include cases where the directions or attitudes are not strictly speaking the same. For example, two directions being parallel not only means that the two directions are completely parallel, but also means that the directions are substantially parallel, that is, that there is a difference of, for example, about a few percent. In the following description, when the term "insulation" is used, it means "electrical insulation."

[0026] (Embodiment) [1 General Description of Power Storage Device 10] First, the general description of the energy storage device 10 in this embodiment will be given. FIG. 1 is a perspective view showing the appearance of the energy storage device 10 according to this embodiment. FIG. 2 is a cross-sectional view showing the internal configuration of the energy storage device 10 according to this embodiment. Specifically, FIG. 2 is a cross-sectional view of the energy storage device 10 in FIG. 1 cut along the YZ plane passing through the line II-II. FIG. 2 shows each component included in the energy storage device 10. FIG. 3 is a perspective view and a cross-sectional view showing the configuration of the electrode unit 100 included in the energy storage device 10 according to this embodiment. Specifically, FIG. 3(a) is a perspective view showing the appearance of the electrode unit 100. FIG. 3(b) is a cross-sectional view showing the configuration of the electrode unit 100 in FIG. 3(a) cut along the YZ plane passing through the line IIIb-IIIb. In FIG. 3, for convenience of explanation, the seal portion 210 included in the electrode unit 100 is omitted.

[0027] The power storage device 10 is a device that can charge electricity from an external source and discharge electricity to the outside. The power storage device 10 in this embodiment has a substantially rectangular parallelepiped shape. Specifically, the power storage device 10 is a bipolar battery. The power storage device 10 is used as a battery for driving or starting an engine of a moving body such as an automobile, a motorcycle, a watercraft, a ship, a snowmobile, an agricultural machine, a construction machine, an automatic guided vehicle (AGV), or a railway vehicle for an electric railway. Examples of the above-mentioned automobiles include electric vehicles (EVs), hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), and fossil fuel (gasoline, diesel, liquefied natural gas, etc.) vehicles. Examples of the above-mentioned railway vehicles for an electric railway include electric trains, monorails, linear motor cars, and hybrid trains equipped with both a diesel engine and an electric motor. The power storage device 10 can also be used as a stationary battery for home or business use.

[0028] As shown in FIG. 1 and FIG. 2, the energy storage device 10 includes a plurality of electrode units 100, end units 101 and 102, a plurality of separators 140, and a pair of end members 300. Each of the plurality of electrode units 100, the end units 101, and the end units 102 is a rectangular plate-like portion in a plan view, and is stacked in the Z-axis direction. In the present embodiment, the plan view refers to a view from the stacking direction (Z-axis direction). The direction in which the plurality of electrode units 100, the end units 101, and the end units 102 are stacked (Z-axis direction) is also referred to as the stacking direction. The separator 140 is disposed between each of the plurality of electrode units 100 and the end units 101 and 102. The pair of end members 300 are disposed on both sides of the plurality of electrode units 100 and the end units 101 and 102 in the stacking direction (Z-axis direction). In the present embodiment, two electrode units 100 are stacked in the stacking direction between the end unit 101 and the end unit 102, but the number of stacked electrode units 100 is not particularly limited. The shapes of the electrode unit 100, the end unit 101, the end unit 102, etc. in a plan view are also not particularly limited.

[0029] [1.1 Description of the electrode unit 100] The configuration of the electrode unit 100 will be described in detail below with reference to Fig. 3. The electrode unit 100 is a single unit in which active material layers are formed on both sides of a single current collector foil. Each of the multiple electrode units 100 has at least a current collector foil 110, a positive electrode active material layer 120 formed on one side of the current collector foil 110, a negative electrode active material layer 130 formed on the other side of the current collector foil 110, and a seal portion 210. In this embodiment, the thickness of the electrode unit 100 (thickness in the stacking direction) is about 135 µm to 190 µm.

[0030] The current collecting foil 110 is a plate-like member having a rectangular shape in a plan view. The current collecting foil 110 is a metal foil. As shown in FIG. 3, the current collecting foil 110 has two metal layers 111 and 112 arranged in the stacking direction (Z-axis direction). The metal layers 111 and 112 are plate-like parts having the same size and shape in a plan view. Hereinafter, of the metal layers 111 and 112, the metal layer 111 on which the positive electrode active material layer 120 is formed is also referred to as the positive electrode metal layer 111, and the metal layer 112 on which the negative electrode active material layer 130 is formed is also referred to as the negative electrode metal layer 112. The positive electrode metal layer 111 is a metal layer located in the positive direction of the current collecting foil 110 on the Z-axis, and the negative electrode metal layer 112 is a metal layer located in the negative direction of the current collecting foil 110 on the Z-axis. That is, the current collecting foil 110 is formed by laminating the positive electrode metal layer 111 and the negative electrode metal layer 112 in a lamination direction in a state in which the positive electrode metal layer 111 and the negative electrode metal layer 112 are connected (contacted or joined) to each other. One of the positive electrode metal layer 111 and the negative electrode metal layer 112 may be a metal foil, and the other may be a plated layer plated on the metal foil. Alternatively, both the positive electrode metal layer 111 and the negative electrode metal layer 112 may be metal foils. When both the positive electrode metal layer 111 and the negative electrode metal layer 112 are metal foils, the current collecting foil 110 may be a clad material formed by joining two metal foils together, or may have two metal foils in a state in which the two metal foils are connected (contacted) without being joined to each other.

[0031] The material of the positive electrode metal layer 111 may be a metal such as aluminum, titanium, tantalum, or stainless steel, or an alloy thereof. Among these, from the viewpoint of the balance between the electric potential resistance, the high conductivity, and the cost, the material of the positive electrode metal layer 111 is preferably aluminum or an aluminum alloy. The form of the positive electrode metal layer 111 may be a plated layer, but from the viewpoint of workability and cost, a foil is preferable. That is, the positive electrode metal layer 111 is preferably an aluminum foil. The material of the negative electrode metal layer 112 may be a metal such as copper, nickel, stainless steel, or nickel-plated steel, or an alloy thereof, and among these, it is preferable to use copper or a copper alloy. The form of the negative electrode metal layer 112 may be a plated layer or a foil (copper foil), and examples of the copper foil include rolled copper foil and electrolytic copper foil. The thickness (thickness in the lamination direction) of the current collector foil 110 is about 20 μm to 30 μm. The positive electrode metal layer 111 has a thickness (thickness in the stacking direction) of about 5 μm to 20 μm, and the negative electrode metal layer 112 has a thickness (thickness in the stacking direction) of about 5 μm to 15 μm.

[0032] The positive electrode active material layer 120 is a positive electrode active material layer formed on one surface (surface in the positive direction of the Z axis) of the current collector foil 110. Specifically, the positive electrode active material layer 120 is formed on the positive electrode metal layer 111 (the outer surface (surface in the positive direction of the Z axis) of the positive electrode metal layer 111). The positive electrode active material layer 120 is formed in a rectangular shape smaller in size than the positive electrode metal layer 111 in a planar view according to the shape of the positive electrode metal layer 111. Small size in a planar view means that the area in the XY plane is small. The same applies below. The thickness (thickness in the stacking direction) of the positive electrode active material layer 120 is about 70 μm to 100 μm.

[0033] The positive electrode active material layer 120 contains a positive electrode active material, and optionally contains a conductive agent, a binder, a thickener, a filler, etc. 2 (M1 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.), layered lithium transition metal oxides such as LiM2 2 O 4(M2 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.), spinel-type lithium transition metal oxides such as LiM3PO 4 , LiM3SiO 4 , LiM3BO 3 (M3 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.) and other polyanion compounds. As the positive electrode active material, one of these compounds may be used alone, or two or more may be mixed and used. The conductive agent contained in the positive electrode active material layer 120 is not particularly limited as long as it has conductivity. Examples of the conductive agent include carbon black such as furnace black, acetylene black, and Ketjen black, and natural or artificial graphite. Examples of the binder (binding agent) include fluororesin (polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVDF), etc.), sulfonated EPDM, and styrene butadiene rubber (SBR). Examples of the thickener include polysaccharide polymers such as carboxymethyl cellulose (CMC) and methyl cellulose.

[0034] The negative electrode active material layer 130 is a negative electrode active material layer formed on the other surface (surface in the negative Z-axis direction) of the current collector foil 110. Specifically, the negative electrode active material layer 130 is formed on the negative electrode metal layer 112 (the outer surface (surface in the negative Z-axis direction) of the negative electrode metal layer 112). The negative electrode active material layer 130 is formed in a rectangular shape smaller than the negative electrode metal layer 112 in a planar view according to the shape of the negative electrode metal layer 112. The negative electrode active material layer 130 is formed in a larger size than the positive electrode active material layer 120 in a planar view. The larger size in a planar view means that the area in the XY plane is larger. The same applies below. In other words, the area in the XY plane of the negative electrode active material layer 130 is larger than that of the positive electrode active material layer 120. The thickness (thickness in the stacking direction) of the negative electrode active material layer 130 is about 45 μm to 60 μm.

[0035] The negative electrode active material layer 130 contains a negative electrode active material, and optionally contains optional components such as a conductive agent, a binder, a thickener, and a filler. The optional components such as the conductive agent, the binder, the thickener, and the filler can be the same as those in the positive electrode active material layer 120. As the negative electrode active material, a material capable of absorbing and releasing lithium ions is usually used. As the negative electrode active material, for example, metals or semi-metals such as Si and Sn; metal oxides or semi-metal oxides such as Si oxide and Sn oxide; and carbon materials such as graphite and non-graphitic carbon (easily graphitizable carbon or non-graphitizable carbon) can be used.

[0036] The sealing portion 210 is a portion disposed around the positive electrode active material layer 120 or the negative electrode active material layer 130. In the present embodiment, the sealing portion 210 is an annular portion disposed around the positive electrode active material layer 120 and the negative electrode active material layer 130 over the entire circumference of the positive electrode active material layer 120 and the negative electrode active material layer 130. Specifically, the sealing portion 210 is formed in a quadrangular ring shape along the outer periphery of the current collector foil 110 so as to cover the outer periphery of the current collector foil 110. The sealing portion 210 is formed from an insulating material such as polycarbonate (PC), polypropylene (PP), polyethylene (PE), polystyrene (PS), polyphenylene sulfide resin (PPS), polyphenylene ether (PPE (including modified PPE)), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polyether ether ketone (PEEK), tetrafluoroethylene-perfluoroalkyl vinyl ether (PFA), polytetrafluoroethylene (PTFE), polyethersulfone (PES), polyamide (PA), ABS resin, or a composite material thereof.

[0037] The seal parts 210 of two adjacent electrode units 100 are connected to each other. The seal parts 210 may be connected to each other by being integrally and continuously formed, or may be connected to each other by being joined to each other by heat sealing (thermal welding), ultrasonic welding, laser welding, adhesive, or the like. As a result, the seal part 210 is disposed around the positive electrode active material layer 120 of one of the two electrode units 100 and the negative electrode active material layer 130 of the other of the two electrode units 100, and the seal part 210 is provided between the current collector foils 110 of the two electrode units 100. In other words, the seal part 210 is provided continuously between the current collector foils 110 of the two electrode units 100, and the current collector foils 110 are sealed from each other.

[0038] An electrolyte layer (not shown) is formed on the inside of the seal portion 210 of each of the electrode units 100. In this embodiment, the electrolyte layer is a non-aqueous liquid electrolyte (electrolytic solution), but may be a solid electrolyte (solid electrolyte) or a gel electrolyte. Any known electrolyte may be used as the electrolyte. The electrolyte (non-aqueous electrolyte) may be a non-aqueous solvent in which an electrolyte salt is dissolved. Examples of the non-aqueous solvent include cyclic carbonates such as ethylene carbonate (EC) and propylene carbonate (PC), and chain carbonates such as diethyl carbonate (DEC), dimethyl carbonate (DMC), and ethyl methyl carbonate (EMC). The electrolyte salt is preferably a lithium salt. Examples of the lithium salt include LiPF 6 , LiPO 2 F 2 , LiBF 4 , LiClO 4 , LiN(SO 2 F) 2 , LiN(SO 2 CF 3 ) and other inorganic lithium salts.

[0039] [1.2 Description of end units 101 and 102] Next, the configuration of the end units 101 and 102 will be described in detail. The end unit 101 is disposed at the end of the multiple electrode units 100 in the negative direction of the Z axis. The end unit 102 is disposed at the end of the multiple electrode units 100 in the positive direction of the Z axis. The end units 101 and 102 are portions that sandwich the multiple electrode units 100 in the Z axis direction.

[0040] The end unit 101 has at least a positive electrode metal layer 111, a positive electrode active material layer 120 formed on a surface of the positive electrode metal layer 111 in the Z-axis positive direction, and a seal portion 220. The positive electrode metal layer 111 and the positive electrode active material layer 120 of the end unit 101 have the same configuration as the positive electrode metal layer 111 and the positive electrode active material layer 120 of the current collector foil 110 of the electrode unit 100 described above.

[0041] The sealing portion 220 is a portion disposed around the positive electrode active material layer 120. In the present embodiment, the sealing portion 220 is an annular portion disposed around the positive electrode active material layer 120 over the entire circumference of the positive electrode active material layer 120. Specifically, the sealing portion 220 is formed in a quadrangular ring shape along the outer periphery of the positive electrode metal layer 111 and the end member 300 so as to cover the outer periphery of the positive electrode metal layer 111 and the end member 300. The sealing portion 220 is formed of the same material as the sealing portion 210 of the electrode unit 100.

[0042] The seal portion 220 is connected to the seal portion 210 of the electrode unit 100 adjacent to the end unit 101. The connection between the seal portion 220 and the seal portion 210 is similar to the connection between the seal portions 210 described above, and therefore a detailed description will be omitted. This provides a seal between the positive electrode metal layer 111 of the end unit 101 and the current collecting foil 110 of the electrode unit 100. The above-mentioned electrolyte layer (not shown) is formed inside the seal portion 220.

[0043] The end unit 102 has at least a current collecting foil 110, a negative electrode active material layer 130 arranged on a surface of the current collecting foil 110 in the negative Z-axis direction, and a seal portion 230. The current collecting foil 110 and the negative electrode active material layer 130 of the end unit 102 have the same configuration as the current collecting foil 110 and the negative electrode active material layer 130 of the electrode unit 100 described above.

[0044] The sealing portion 230 is a portion disposed around the negative electrode active material layer 130. In the present embodiment, the sealing portion 230 is an annular portion disposed around the negative electrode active material layer 130 over the entire circumference of the negative electrode active material layer 130. Specifically, the sealing portion 230 is formed in a quadrangular ring shape along the outer periphery of the current collector foil 110 and the end member 300 so as to cover the outer periphery of the current collector foil 110 and the end member 300. The sealing portion 230 is formed of the same material as the sealing portion 210 of the electrode unit 100.

[0045] The seal portion 230 is connected to the seal portion 210 of the electrode unit 100 adjacent to the end unit 102. The connection between the seal portion 230 and the seal portion 210 is similar to the connection between the seal portions 210 described above, and therefore a detailed description will be omitted. This provides a seal between the current collecting foil 110 of the end unit 102 and the current collecting foil 110 of the electrode unit 100. The above-mentioned electrolyte layer (not shown) is formed inside the seal portion 230.

[0046] In this manner, the seal portions 210, 220, and 230 are connected to one another to form the seal member 200. The seal member 200 is a cylindrical (rectangular cylindrical) member that is disposed so as to surround the entire periphery of the positive electrode metal layer 111, the negative electrode metal layer 112, the positive electrode active material layer 120, the negative electrode active material layer 130, the separator 140, and the end member 300, and seals these members from the outside.

[0047] [1.3 Description of the separator 140 and the end member 300] The separator 140 is a microporous sheet made of resin. The separator 140 is disposed between the electrode units 100, between the end unit 101 and the electrode unit 100, and between the end unit 102 and the electrode unit 100. Specifically, the separator 140 is disposed between the positive electrode active material layer 120 and the negative electrode active material layer 130. For example, a woven fabric, a nonwoven fabric, a porous resin film, or the like is used as the material of the separator 140. Among these, a porous resin film is preferable. From the viewpoint of strength, a polyolefin such as polyethylene or polypropylene is preferable as the main component of the porous resin film. The separator 140 may be a multilayer film in which a layer containing a filler is formed on the surface of the porous resin film. The separator 140 is formed in a rectangular shape larger than the negative electrode active material layer 130 in a planar view. In this embodiment, the size of the separator 140 is smaller than that of the current collector foil 110 in a planar view, but may be larger than the current collector foil 110 in a planar view. The thickness of the separator 140 (thickness in the stacking direction) is about 15 μm to 20 μm.

[0048] The end member 300 is a member disposed at an end of the power storage device 10 in the stacking direction (Z-axis direction) relative to the plurality of electrode units 100. In this embodiment, a pair of end members 300 are disposed at the end closest to the negative Z-axis direction and the end closest to the positive Z-axis direction of the power storage device 10. The pair of end members 300 are connected to the end units 101 and 102 (the positive electrode metal layers 111 of the end units 101 and 102). As a result, the pair of end members 300 sandwich the plurality of electrode units 100 and the end units 101 and 102 located therebetween from both sides in the stacking direction (Z-axis direction). The end member 300 is a flat plate-shaped member (end plate). The end member 300 is electrically connected to another end member 300 of another power storage device 10 via another conductive member (bus bar, cooling plate, etc., not shown). The end member 300 is formed of a conductive member made of metal such as aluminum, aluminum alloy, copper, copper alloy, nickel, etc., or a combination thereof, or a conductive member other than metal. Since the end member 300 is connected to the positive electrode metal layer 111, it is preferably formed of the same material as the positive electrode metal layer 111, such as aluminum. The end member 300 has a thickness (thickness in the stacking direction) of about 0.5 mm to 3 mm. The electricity storage device 10 may have another conductive member on the outside of the end member 300 (outside in the Z-axis direction).

[0049] In the above configuration, the separator 140, the positive electrode active material layer 120 and the negative electrode active material layer 130 sandwiching the separator 140 in the Z-axis direction, and the positive electrode metal layer 111 and the negative electrode metal layer 112 sandwiching them in the Z-axis direction may be referred to as one energy storage element. In this case, the energy storage device 10 can also be said to be a group of energy storage elements having a configuration in which a plurality of energy storage elements stacked in the Z-axis direction are sandwiched between a pair of end members 300 in the Z-axis direction and are surrounded by a sealing member 200.

[0050] [2 Explanation of current collecting foil 110] Next, the configuration of the current collecting foil 110 will be described in more detail. Below, the configuration of the current collecting foil 110 of the electrode unit 100 will be described, but the same applies to the configuration of the current collecting foil 110 of the end unit 102. Fig. 4 is a cross-sectional view showing the configuration of the current collecting foil 110 of the electrode unit 100 according to this embodiment. Specifically, Fig. 4(a) shows the electrode unit 100 of Fig. 3(b), and Fig. 4(b) shows an enlarged view of a part (a part surrounded by a dashed line) of the current collecting foil 110 in the electrode unit 100 shown in Fig. 4(a).

[0051] Various configurations of the current collector foil 110 have been described above, and one example of the configurations will be described below in detail. As described above, the current collector foil 110 has a positive electrode metal layer 111 and a negative electrode metal layer 112. At least one of the metal layers of the positive electrode metal layer 111 and the negative electrode metal layer 112 is formed of multiple layers having an opposing layer that is a metal foil facing the other metal layer and a non-opposing layer that is a metal foil on the opposite side to the other metal layer. As shown in FIG. 4, in this embodiment, the positive electrode metal layer 111 is formed of multiple layers. That is, the positive electrode metal layer 111 is formed of multiple layers (two layers, double foil) having an opposing layer 113 that is a metal foil facing the negative electrode metal layer 112 and a non-opposing layer 114 that is a metal foil on the opposite side to the negative electrode metal layer 112.

[0052] The facing layer 113 and the non-facing layer 114 of the positive electrode metal layer 111 may be metal foils of any material used for the positive electrode metal layer 111 described above, but in this embodiment, they are metal foils containing aluminum. Specifically, the facing layer 113 and the non-facing layer 114 are aluminum foils. The negative electrode metal layer 112 is a plating layer plated on the positive electrode metal layer 111 (facing layer 113). The negative electrode metal layer 112 may be a plating layer of any material used for the negative electrode metal layer 112 described above, but in this embodiment, it is a plating layer containing copper. Specifically, the negative electrode metal layer 112 is copper plating. The negative electrode metal layer 112 is formed on the positive electrode metal layer 111 (facing layer 113) by adhesive plating or the like.

[0053] In this manner, the facing layer 113 and the non-facing layer 114 of the positive electrode metal layer 111 (one metal layer) are formed of the same material. The facing layer 113 of the positive electrode metal layer 111 (one metal layer) and the negative electrode metal layer 112 (the other metal layer) are formed of different materials. Similarly, the non-facing layer 114 of the positive electrode metal layer 111 (one metal layer) and the negative electrode metal layer 112 (the other metal layer) are formed of different materials. In this embodiment, the thicknesses (thicknesses in the Z-axis direction) of the facing layer 113 and the non-facing layer 114 are equal to or less than the thickness of the negative electrode metal layer 112, but the thickness of the positive electrode metal layer 111 (the total thickness of the facing layer 113 and the non-facing layer 114) is equal to or more than the thickness of the negative electrode metal layer 112. For example, the thickness of the positive metal layer 111 (the total thickness of the opposing layer 113 and the non-opposing layer 114) is about 10 μm, and the thickness of the negative metal layer 112 is about 5 μm to 10 μm. The opposing layer 113 and the non-opposing layer 114 are formed to have the same size in a plan view.

[0054] The opposing layer 113 and the non-facing layer 114 have mutually opposing surfaces (inner surfaces) with a rougher surface than the opposite surfaces (outer surfaces). In other words, the surface 113a of the opposing layer 113 facing the non-facing layer 114 has a rougher surface roughness than the surface 113b of the opposing layer 113 opposite the non-facing layer 114. The surface 114a of the non-facing layer 114 facing the opposing layer 113 has a rougher surface roughness than the surface 114b of the non-facing layer 114 opposite the opposing layer 113. The surface 113a of the opposing layer 113 has a rougher surface roughness than the surface 114b of the non-facing layer 114. The surface 114a of the non-facing layer 114 has a rougher surface roughness than the surface 113b of the opposing layer 113. The surface 113a of the opposing layer 113 has a rougher surface roughness than the surface 114a of the non-facing layer 114. The surface 113 b of the facing layer 113 has the same surface roughness as the surface 114 b of the non-facing layer 114 .

[0055] The comparison of surface roughness is performed as follows. The negative electrode metal layer 112 is removed from the current collecting foil 110, and tape is applied to both sides of the positive electrode metal layer 111 and pulled to peel off the opposing layer 113 and the non-opposing layer 114. Thereafter, the arithmetic mean roughness Ra of each surface (surface 113a, surface 113b of the opposing layer 113, and surfaces 114a, 114b of the non-opposing layer 114) is measured in accordance with JIS B0601:2013, and the surface roughness of each surface is compared. In this embodiment, in the opposing layer 113, the surface roughness of the surface 113a is about 0.2 μm, and the surface roughness of the surface 113b is about 0.05 μm. In this embodiment, in the non-opposing layer 114, the surface roughness of the surface 114a is about 0.2 μm, and the surface roughness of the surface 114b is about 0.05 μm.

[0056] [3. Description of Manufacturing Method of Electricity Storage Device 10] Next, a method for manufacturing the electricity storage device 10 will be described. Fig. 5 is a cross-sectional view showing manufacturing steps in the manufacturing method for the electricity storage device 10 according to the present embodiment. Fig. 5 shows a manufacturing method for the current collector foil 110 in the manufacturing method for the electricity storage device 10. Specifically, (a) of Fig. 5 shows a step of forming the positive electrode metal layer 111 in the manufacturing method for the current collector foil 110, and (b) of Fig. 5 shows a step of forming the current collector foil 110.

[0057] As shown in FIG. 5(a), first, two metal foils, the facing layer 113 and the non-facing layer 114, are stacked in the Z-axis direction to form the positive electrode metal layer 111. Specifically, the facing layer 113 and the non-facing layer 114 are stacked and roll-pressed (compression-bonded) using a press roll to form the positive electrode metal layer 111. As a result, the surface roughness of the outer surfaces (surfaces 113b and 114b) to be pressed in the facing layer 113 and the non-facing layer 114 is reduced, and as a result, the inner surfaces (surfaces 113a and 114a) have a rougher surface roughness than the outer surfaces (surfaces 113b and 114b). As such, a stack rolling process in which metal foils are stacked and rolled in the rolling process is suitable as a method for forming metal foils with different surface roughnesses. The metal foil thus rolled has a non-glossy surface with large surface roughness at the overlapping surface of the metal foil, and a smooth glossy surface with small surface roughness at the opposite surface. In this embodiment, the opposing layer 113 and the non-facing layer 114 are simply pressed together, and no step of bonding (adhering) the opposing layer 113 and the non-facing layer 114 is performed, but the opposing layer 113 and the non-facing layer 114 may be bonded (adhered) together.

[0058] 5(b), the negative electrode metal layer 112 is formed on the positive electrode metal layer 111. Specifically, the positive electrode metal layer 111 is copper-plated to form the negative electrode metal layer 112, which is a plated layer, on the positive electrode metal layer 111. In this way, the current collecting foil 110 in which the positive electrode metal layer 111 and the negative electrode metal layer 112 are laminated is formed.

[0059] Thereafter, the electrode unit 100 (and the end unit 102) is formed by forming the positive electrode active material layer 120 and the negative electrode active material layer 130 on the current collecting foil 110. Then, the multiple electrode units 100 and the end units 101 and 102 are stacked in the stacking direction with the separator 140 sandwiched between them, and are sandwiched between a pair of end members 300, thereby manufacturing the electricity storage device 10.

[0060] [4. Description of Effects] As described above, in the electricity storage device 10 according to the embodiment of the present invention, at least one of the metal layers of the positive electrode metal layer 111 and the negative electrode metal layer 112 of the current collector foil 110 is formed of multiple layers (multiple metal foils) having an opposing layer 113 opposing the other metal layer, and a non-opposing layer 114 on the opposite side to the other metal layer. In this way, by forming the metal layer of the current collector foil 110 into multiple layers, the metal layer can be reinforced, and damage to the current collector foil 110 can be suppressed.

[0061] Specifically, it is as follows. When a pinhole occurs in the positive electrode metal layer 111 or the negative electrode metal layer 112, the electrolyte may penetrate through the pinhole, and a short circuit due to the electrolyte (a short circuit between the metal layer and the active material of the opposite electrode) may occur. In the pinhole in the positive electrode metal layer 111, the positive electrode active material layer 120 and the negative electrode metal layer 112 are short-circuited via the electrolyte, and further, a pinhole is formed in Cu due to the elution of Cu, and finally, a short circuit occurs between the positive electrode active material layer 120 and the negative electrode active material layer 130. In the pinhole in the negative electrode metal layer 112, the negative electrode active material layer 130 and the positive electrode metal layer 111 are short-circuited via the electrolyte, and further, Li of the negative electrode penetrates into Al to form a Li / Al alloy, and the alloy part forms a crack due to expansion, and finally, a short circuit occurs between the positive electrode active material layer 120 and the negative electrode active material layer 130. The pinhole may occur due to compression of a lubricant or foreign matter during rolling press. For this reason, at least one of the metal layers, the positive electrode metal layer 111 and the negative electrode metal layer 112, is formed of multiple layers. As a result, even if a pinhole occurs in any of the multiple layers, the pinholes in each layer are unlikely to overlap, and the occurrence of a pinhole that penetrates multiple layers can be suppressed, thereby suppressing a short circuit caused by the electrolyte.

[0062] By forming the opposing layer 113 of the one metal layer and the other metal layer from different materials (i.e., they do not have to be formed from the same material), the opposing layer 113 and the other metal layer can each be formed from an appropriate material.

[0063] By forming the facing layer 113 and the non-facing layer 114 of the one metal layer from the same material, the one metal layer can be formed from the same material.

[0064] The positive electrode metal layer 111 is generally formed of an easy-to-handle material such as aluminum foil, and therefore, by forming the positive electrode metal layer 111 as one of the metal layers in multiple layers, the one of the metal layers can be easily formed.

[0065] Since the surface roughness of the surface 114a of the non-facing layer 114 facing the facing layer 113 is greater than the surface 114b on the opposite side, the contact area between the facing layer 113 and the non-facing layer 114 can be increased, and the electrical resistance of the multiple layers having the facing layer 113 and the non-facing layer 114 can be reduced. By rolling and pressing the facing layer 113 and the non-facing layer 114 together, the surface 114b of the non-facing layer 114 opposite the facing layer 113 is made smoother by rolling with the press roll. Therefore, the surface roughness of the surface 114a of the non-facing layer 114 facing the facing layer 113 can be made greater than the surface roughness of the surface 114b of the non-facing layer 114 opposite the facing layer 113.

[0066] The surface roughness of the surface 113a of the facing layer 113 facing the non-facing layer 114 is rougher than that of the surface 113b on the opposite side, and therefore the contact area between the facing layer 113 and the non-facing layer 114 can be increased, and the electrical resistance of the multiple layers having the facing layer 113 and the non-facing layer 114 can be reduced. By rolling and pressing the facing layer 113 and the non-facing layer 114, the surface 113b of the facing layer 113 facing the non-facing layer 114 is made smoother by rolling with a press roll. Even when the other metal layer (negative electrode metal layer 112) is connected to the facing layer 113, the smoothness of the surface 113b is maintained. Therefore, the surface roughness of the surface 113a of the facing layer 113 facing the non-facing layer 114 can be rougher than the surface roughness of the surface 113b of the facing layer 113 facing the non-facing layer 114.

[0067] [5. Explanation of Variations] Although the electricity storage device 10 and the manufacturing method thereof according to the present embodiment have been described above, the present invention is not limited to the above embodiment. The embodiment disclosed herein is illustrative and not restrictive in all respects, and the scope of the present invention includes all modifications within the meaning and scope of the claims.

[0068] In the above-described embodiment, the thickness of the positive electrode metal layer 111 of the current collector foil 110 (the thickness of the opposing layer 113 and the non-opposing layer 114) is not particularly limited. Fig. 6 is a cross-sectional view showing the configuration of a current collector foil 110a according to a first modification of the present embodiment. Fig. 7 is a cross-sectional view showing the configuration of a current collector foil 110b according to a second modification of the present embodiment. Figs. 6 and 7 correspond to (b) of Fig. 4.

[0069] As shown in Fig. 6, the current collector foil 110a in the first modification has a positive electrode metal layer 111a instead of the positive electrode metal layer 111 of the current collector foil 110 in the above embodiment. In the above embodiment, the thicknesses of the facing layer 113 and the non-facing layer 114 of the positive electrode metal layer 111 are both equal to or less than the thickness of the negative electrode metal layer 112, but in this modification, at least one of the facing layer 113 and the non-facing layer 114 of the positive electrode metal layer 111a is thicker than the negative electrode metal layer 112. Specifically, the non-facing layer 114 of the positive electrode metal layer 111a is thicker than the negative electrode metal layer 112. The other configurations of this modification are similar to those of the above embodiment, and therefore detailed description thereof will be omitted.

[0070] In this modification, the facing layer 113 of the positive metal layer 111a may be thicker than the negative metal layer 112, or both the facing layer 113 and the non-facing layer 114 of the positive metal layer 111a may be thicker than the negative metal layer 112. That is, at least one of the facing layer 113 and the non-facing layer 114 of one metal layer (positive metal layer 111a) is thicker than the other metal layer (negative metal layer 112). The configuration of this modification also achieves the same effects as the above embodiment. In particular, in this modification, by making at least one of the facing layer 113 and the non-facing layer 114 of one metal layer (positive metal layer 111a) thicker than the other metal layer (negative metal layer 112), it is possible to suppress the occurrence of pinholes in the metal layer (positive metal layer 111a) formed of multiple layers.

[0071] As shown in FIG. 7, the current collector foil 110b in the second modification has a positive electrode metal layer 111b instead of the positive electrode metal layer 111 of the current collector foil 110 in the above embodiment. In the above embodiment, the thickness of the positive electrode metal layer 111 (the total thickness of the opposing layer 113 and the non-opposing layer 114) is equal to or greater than the thickness of the negative electrode metal layer 112, but in this modification, the thickness of the positive electrode metal layer 111b (the total thickness of the opposing layer 113 and the non-opposing layer 114) is thinner than the thickness of the negative electrode metal layer 112. The other configurations of this modification are the same as those of the above embodiment, and therefore detailed description will be omitted. Even with the configuration of this modification, the positive electrode metal layer 111b is formed of a plurality of metal foils, and therefore damage is suppressed. In particular, since the thickness of the positive electrode metal layer 111b is thin, the thickness of the current collector foil 110b (electrode unit 100) can be thin. This reduces the volume of the power storage device 10 that is occupied by the current collector foil 110b, thereby enabling the energy density of the power storage device 10 to be improved.

[0072] In the above embodiment, the positive electrode metal layer 111 of the current collector foil 110 is a two-layer metal foil, but the positive electrode metal layer 111 may be a three-layer metal foil. FIG. 8 is a cross-sectional view showing the configuration of a current collector foil 110c according to the third modification of the present embodiment. FIG. 8 is a view corresponding to FIG. 4(b). As shown in FIG. 8, the current collector foil 110c according to this modification has a positive electrode metal layer 111c instead of the positive electrode metal layer 111 of the current collector foil 110 in the above embodiment. The positive electrode metal layer 111c is formed of three layers including the facing layer 113, the non-facing layer 114, and the intermediate layer 115. The intermediate layer 115 is a metal foil disposed between the facing layer 113 and the non-facing layer 114. The intermediate layer 115 is formed of the same material and size as the facing layer 113 and the non-facing layer 114.

[0073] In this modification, the surface 113b of the facing layer 113 and the surface 114b of the non-facing layer 114 are also smoothed by rolling with a press roll. Therefore, the surface 113a of the facing layer 113 and the surface 114a of the non-facing layer 114 face the intermediate layer 115, but have a rougher surface than the surface 113b of the facing layer 113 and the surface 114b of the non-facing layer 114. The surface 115a of the intermediate layer 115 facing the facing layer 113 and the surface 115b facing the non-facing layer 114 have the same surface roughness, and are rougher than the surface 113b of the facing layer 113 and the surface 114b of the non-facing layer 114. The other configurations of this modification are the same as those of the above embodiment, so detailed description will be omitted. The configuration of this modification also produces the same effects as those of the above embodiment. In particular, in this modification, the positive metal layer 111c is formed of three layers, which further suppresses damage. In this modification, the positive metal layer 111c may be formed of four or more layers by including a plurality of intermediate layers 115.

[0074] In the above embodiment, the facing layer 113 and the non-facing layer 114 of the positive electrode metal layer 111 are formed of the same material, but they may be formed of different materials. The facing layer 113 and the negative electrode metal layer 112 of the positive electrode metal layer 111 are formed of different materials, but they may be formed of the same material.

[0075] In the above embodiment, in the facing layer 113 of the positive metal layer 111, the surface 113a has a rougher surface than the surface 113b, but the surface roughness may be the same, or the surface 113b may have a rougher surface than the surface 113a. In the non-facing layer 114 of the positive metal layer 111, the surface 114a has a rougher surface than the surface 114b, but the surface roughness may be the same, or the surface 114b may have a rougher surface than the surface 114a. Other than that, the relationship of the surface roughness is not particularly limited.

[0076] In the above embodiment, the current collector foil 110 has been described as being formed by plating the negative electrode metal layer 112 onto multiple positive electrode metal layers 111, but the present invention is not limited to this. The current collector foil 110 may be formed as a clad material in which the negative electrode metal layer 112, which is a metal foil, is bonded to the multiple positive electrode metal layers 111 by rolling press or the like. The current collector foil 110 may be configured such that the negative electrode metal layer 112, which is a metal foil, is connected (contacted) to the multiple positive electrode metal layers 111 without being bonded.

[0077] In the above embodiment, the current collecting foil 110 has the positive electrode metal layer 111 formed in a plurality of layers, but the negative electrode metal layer 112 may also be formed in a plurality of layers. In this case, the current collecting foil 110 may be formed by plating the positive electrode metal layer 111 on the negative electrode metal layer 112 of a plurality of layers. The current collecting foil 110 may be formed as a clad material in which the positive electrode metal layer 111, which is a metal foil, is bonded to the negative electrode metal layer 112 of a plurality of layers by rolling press or the like. The current collecting foil 110 may be configured such that the positive electrode metal layer 111, which is a metal foil, is connected (contacted) to the negative electrode metal layer 112 of a plurality of layers without being bonded thereto. Both the positive electrode metal layer 111 and the negative electrode metal layer 112 may be formed in a plurality of layers.

[0078] In the above embodiment, all of the current collecting foils 110 in all of the electrode units 100 and the end units 102 have the above configuration, but it is not necessary for any of the current collecting foils 110 to have the above configuration. The positive electrode metal layer 111 in the end unit 101 may be formed of multiple layers.

[0079] The electricity storage device 10 may be used in an electricity storage pack 1 as shown in FIG. 9. FIG. 9 is a cross-sectional view showing the configuration of the electricity storage pack 1. In FIG. 9, the internal configuration of the electricity storage device 10 is omitted. As shown in FIG. 9, the electricity storage pack 1 includes an electricity storage device stack 2 in which a plurality of electricity storage devices 10 are stacked, and a conductive member 3. In this case, the technology of the present invention may be applied to at least one electricity storage device 10 included in the electricity storage pack 1. Two adjacent electricity storage devices 10 in the electricity storage device stack 2 are electrically connected by contact or joining (welding, etc.). The conductive member 3 is made of a metal such as stainless steel, and the electricity storage device 10 located at the end in the stacking direction (Z-axis direction) and the conductive member 3 are electrically connected by contact or joining (welding, etc.). An adhesive may be used for the joining. The plurality of electricity storage devices 10 in the electricity storage device stack 2 are connected in series, and charging and discharging are performed via the conductive member 3. The electricity storage pack 1 may be restrained in the stacking direction (Z-axis direction) by using a restraining member such as a screw, a resin band, or a metal band. The electricity storage device stack 2 and the conductive member 3 may be housed in a metal case or a resin case.

[0080] As another example of the electricity storage pack 1, a configuration in which individual electricity storage devices 10 are housed in an exterior body 4 is shown in FIG. 10. FIG. 10 is a cross-sectional view showing the configuration of an electricity storage pack 1a. As shown in FIG. 10, the electricity storage device 10 of this configuration has a connection portion 5 exposed from the exterior body 4. A laminate film or the like can be used as the exterior body 4. The connection portions 5 of adjacent electricity storage devices 10 are electrically connected to each other by contact or bonding (welding, etc.). The connection portion 5 of the electricity storage device 10 located at the end in the stacking direction (Z-axis direction) and the conductive member 3 are electrically connected to each other by contact or bonding (welding, etc.). The other configuration is similar to that of the above-mentioned electricity storage pack 1, so a description thereof will be omitted.

[0081] Any combination of the components included in the above-described embodiment and its modified examples is also included within the scope of the present invention. [Industrial Applicability]

[0082] The present invention can be applied to electricity storage devices such as bipolar batteries. [Explanation of symbols]

[0083] 1, 1a storage pack 2. Electricity storage device laminate 3 Conductive materials 4 Exterior body 5 Connection part 10. Energy storage device 100 electrode units 101, 102 End unit 110, 110a, 110b, 110c current collector foil 111, 111a, 111b, 111c Positive electrode metal layer (metal layer) 112 Negative electrode metal layer (metal layer) 113 Opposing Layer 113a, 113b, 114a, 114b, 115a, 115b side 114 Non-facing layer 115 Middle Class 120 Cathode active material layer 130 Negative electrode active material layer 140 Separator 200 Sealing material 210, 220, 230 Seal part 300 End member

Claims

1. The electrode unit includes a plurality of stacked electrode units, each of the plurality of electrode units includes at least a current collecting foil in which a positive electrode metal layer and a negative electrode metal layer are laminated, a positive electrode active material layer formed on the positive electrode metal layer, and a negative electrode active material layer formed on the negative electrode metal layer; At least one of the positive electrode metal layer and the negative electrode metal layer is formed of a plurality of layers having an opposing layer which is a metal foil facing the other metal layer, and a non-opposing layer which is a metal foil on the opposite side to the other metal layer. Energy storage device.

2. The opposing layer and the other metal layer are formed of different materials. The power storage device according to claim 1 .

3. The facing layer and the non-facing layer are formed of the same material. The power storage device according to claim 1 or 2.

4. The positive electrode metal layer is formed of the multiple layers. The power storage device according to claim 1 or 2.

5. The surface of the non-facing layer facing the facing layer has a surface roughness greater than that of the non-facing layer on the opposite side to the facing layer. The power storage device according to claim 1 or 2.

6. The surface of the opposing layer facing the non-opposing layer has a surface roughness greater than that of the surface of the opposing layer opposite to the non-opposing layer. The power storage device according to claim 1 or 2.

7. At least one of the facing layer and the non-facing layer is thicker than the other metal layer. The power storage device according to claim 1 or 2.

Citation Information

Patent Citations

  • Power storage device

    JP2022077634A