Piezoelectric element
By positioning the second electrode film's outer edge outside the first electrode film and removing the piezoelectric film below the edge, the piezoelectric element addresses leakage current issues, reducing dielectric loss and maintaining performance consistency while simplifying manufacturing.
Patent Information
- Application Number
- JP2023070992
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2024-11-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing piezoelectric elements in microphones suffer from performance deterioration due to increased dielectric loss (tan δ) caused by leakage current between electrode films, which is exacerbated by etching processes, and maintaining consistent manufacturing conditions to prevent this is costly and not always effective.
The piezoelectric element design includes electrode films where the outer edge of the second electrode film is positioned outside the first electrode film, with the piezoelectric film below the edge removed, and optionally includes protective films and slits to minimize the region prone to leakage current.
This configuration reduces dielectric loss and suppresses performance deterioration by minimizing leakage current, maintaining consistent performance without the need for stringent manufacturing control, and enhancing reliability.
Smart Images

Figure 2024156487000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a piezoelectric element. [Background technology]
[0002] Piezoelectric elements used in microphones and the like include a substrate and a lower electrode film, a lower piezoelectric film, an intermediate electrode film, an upper piezoelectric film, and an upper electrode film laminated on the substrate. Each electrode film is patterned according to the required function, and a part of it is removed to form an opening. In this opening, there is a risk of cracks occurring along the crystal orientation of the piezoelectric film.
[0003] For example, in Patent Document 1, in order to suppress this cracking, the in-plane positions of the openings of each electrode film are shifted. That is, the portion where the intermediate electrode film is removed is located above the portion of the substrate covered with the lower electrode film. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] U.S. Pat. No. 10,566,517 Summary of the Invention [Problem to be solved by the invention]
[0005] When patterning the intermediate electrode film, a part of the intermediate electrode film is removed by etching, and then a process such as milling or ashing is usually performed to normalize the surface. If a lower electrode film is present below the part where the intermediate electrode film has been removed, the etching damage may reach the lower electrode film, causing a small amount of leakage current to flow between the lower electrode film and the intermediate electrode film. This small amount of leakage current may increase tan δ, i.e., dielectric loss, and may degrade the performance of the piezoelectric element.
[0006] According to the inventors' intensive research, it has been confirmed that the increase in tan δ can be suppressed by not performing milling or ashing after etching the intermediate electrode film. However, in order to suppress the increase in tan δ using this method, the state of the manufacturing equipment must always be constant, and manufacturing costs increase due to equipment management and advance confirmation, etc. In addition, depending on the surface state after etching, if milling or ashing is not performed, the leakage current cannot be suppressed, and the performance of the piezoelectric element may be degraded.
[0007] In view of the above, an object of the present invention is to provide a piezoelectric element capable of suppressing performance degradation. [Means for solving the problem]
[0008] In order to achieve the above object, the invention described in claim 1 provides a piezoelectric element comprising a support (10), a first electrode film (51, 52) laminated on the support, a piezoelectric film (41, 42) laminated on the first electrode film, and a second electrode film (52, 53) laminated on the piezoelectric film, and in a plane perpendicular to the stacking direction of the first electrode film, the piezoelectric film, and the second electrode film, the outer edge of the second electrode film is outside the outer edge of the first electrode film.
[0009] According to the inventors' intensive research, it is presumed that the region involved in the generation of leakage current and the increase in dielectric loss exists near the outer edge of the second electrode film, and that leakage current occurs when the first electrode film exists below the outer edge of the second electrode film. By forming the outer edge of the second electrode film outside the outer edge of the first electrode film, the region involved in the generation of leakage current becomes small, improving tan δ and suppressing performance degradation.
[0010] In addition, the invention described in claim 4 provides a piezoelectric element comprising a support (10), a first electrode film (51, 52) laminated on the support, a piezoelectric film (41, 42) laminated on the first electrode film, and a second electrode film (52, 53) laminated on the piezoelectric film, in a plane perpendicular to the lamination direction of the first electrode film, the piezoelectric film, and the second electrode film, the outer edge of the second electrode film is inside the outer edge of the first electrode film, and the piezoelectric film is partitioned by a slit (20b) that exposes the upper surface of the first electrode film and the side surface of the second electrode film, and the piezoelectric film located at the lower part of the side surface at the slit is removed.
[0011] According to the inventors' intensive research, it is presumed that the area involved in the generation of leakage current and the increase in dielectric loss exists near the outer edge of the second electrode film, and that leakage current occurs when the first electrode film exists below the outer edge of the second electrode film. By removing the piezoelectric film located below the side surface of the second electrode film in the slit, the area involved in the generation of leakage current becomes smaller, improving tan δ and suppressing the deterioration of performance.
[0012] The reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]
[0013] [Figure 1] FIG. 2 is a top view of the piezoelectric element according to the first embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II of FIG. [Diagram 3] FIG. 2 is a cross-sectional view taken along line III-III of FIG. [Figure 4] FIG. 2 is a top view of a lower electrode film and an intermediate electrode film. [Diagram 5] FIG. 4 is a cross-sectional view of a first comparative example. [Figure 6] FIG. 11 is a cross-sectional view of a second comparative example. [Figure 7] FIG. 11 is a cross-sectional view of a third comparative example. [Figure 8] FIG. 13 is a diagram showing the relationship between the perimeter of an intermediate electrode film and tan δ. [Figure 9] FIG. 13 is a graph showing the relationship between the size of an intermediate electrode film and tan δ. [Figure 10] 5 is a cross-sectional view of a piezoelectric element according to a second embodiment, which corresponds to FIG. 2. FIG. [Figure 11] 5 is a cross-sectional view of a piezoelectric element according to a second embodiment, which corresponds to FIG. 3. FIG. [Figure 12] 10 is a cross-sectional view of a piezoelectric element according to a third embodiment, which corresponds to FIG. [Figure 13] 10 is a cross-sectional view of a piezoelectric element according to a fourth embodiment, which corresponds to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.
[0015] (First embodiment) A first embodiment will be described. The piezoelectric element of this embodiment is suitable for use in a microphone mounted on a smartphone, an AI (artificial intelligence) speaker, etc. The piezoelectric element of this embodiment is also suitable for use in an ultrasonic sensor, etc.
[0016] As shown in Figs. 1 to 3, the piezoelectric element includes a support 10 and a vibration part 20 disposed on the support 10, and has a rectangular planar shape. The support 10 includes a support substrate 11 having one surface 11a, and an insulating film 12 formed on the one surface 11a of the support substrate 11. The support substrate 11 is made of a silicon substrate or the like, and the insulating film 12 is made of an oxide film or the like. The direction parallel to two sides of the rectangle constituting the upper surface of the support 10 is the X direction, and the direction parallel to the other two sides is the Y direction. The direction perpendicular to both the X direction and the Y direction is the Z direction. A piezoelectric film 40 and an electrode film 50, which will be described later, are stacked on the support 10 in the Z direction.
[0017] The support 10 is formed with a recess 10a for floating the inner edge side of the vibration section 20. Therefore, the vibration section 20 has a configuration including a support region 21a arranged on the support 10 and a floating region 21b that is connected to the support region 21a and floats above the recess 10a. The recess 10a in this embodiment has an open end on the vibration section 20 side that is rectangular in plan view. Therefore, the entire floating region 21b is rectangular in plan view.
[0018] Openings 12a, 20a are formed in the outer edge portions of the insulating film 12 and the vibration portion 20 to expose the outer edge portion of the support substrate 11. The openings 12a, 20a facilitate the dicing process when manufacturing the piezoelectric element, and are not necessarily required to be formed.
[0019] In the floating region 21b, a slit 30 is formed penetrating the floating region 21b in the thickness direction. The slit 30 is formed so as to divide the floating region 21b into four. More specifically, two slits 30 are formed so as to pass through the center of the floating region 21b and extend toward opposite corners of the floating region 21b. In other words, the slits 30 are formed so as to extend from each corner of the floating region 21b, which has a rectangular shape in plan view, toward the center, and the slits 30 intersect at the center. As a result, the floating region 21b is divided into first to fourth vibration regions 22a to 22d, which have a substantially triangular shape in plan view.
[0020] Although the slits 30 in this embodiment extend to the support region 21a, they may be formed so as to terminate within the floating region 21b. Also, the slits 30 may be formed so as to terminate at the boundary between the floating region 21b and the support region 21a.
[0021] The first to fourth vibrating regions 22a to 22d are configured as cantilevers having their ends on the support region 21a side as fixed ends and their tips on the opposite side to the support region 21a as free ends.
[0022] The vibration section 20 is configured to have a piezoelectric film 40 and an electrode film 50 connected to the piezoelectric film 40. Specifically, the piezoelectric film 40 has a lower-layer piezoelectric film 41 and an upper-layer piezoelectric film 42 laminated on the lower-layer piezoelectric film 41. The lower-layer piezoelectric film 41 and the upper-layer piezoelectric film 42 are made of lead-free piezoelectric ceramics such as scandium aluminum nitride (ScAlN) and aluminum nitride (AlN). The lower-layer piezoelectric film 41 and the upper-layer piezoelectric film 42 are made of lead zirconate titanate (PZT) or the like.
[0023] The electrode film 50 is formed on each of the vibration regions 22a to 22d so as to be connected to the piezoelectric film 40, and is made of molybdenum (Mo). However, the electrode film 50 may be made of a metal material containing, as a main component, any one of titanium (Ti), platinum (Pt), aluminum (Al), ruthenium (Ru), etc., in addition to molybdenum.
[0024] In this embodiment, the electrode film 50 includes a lower electrode film 51 formed below the lower piezoelectric film 41, an intermediate electrode film 52 formed between the lower piezoelectric film 41 and the upper piezoelectric film 42, and an upper electrode film 53 formed above the upper piezoelectric film 42. The lower electrode film 51 and the intermediate electrode film 52 are arranged to face each other with the lower piezoelectric film 41 in between. The intermediate electrode film 52 and the upper electrode film 53 are arranged to face each other with the upper piezoelectric film 42 in between. The upper electrode film 53 is formed below an interlayer insulating film 81 to a position indicated by a broken line L1 in FIG. 1. The lower electrode film 51 corresponds to a first electrode film, and the intermediate electrode film 52 corresponds to a second electrode film. Although FIG. 1 is not a cross-sectional view, the upper electrode film 53 and the like are hatched to facilitate understanding.
[0025] 4, in this embodiment, in the XY plane, the outer edge of the intermediate electrode film 52 is outside the outer edge of the lower electrode film 51, and the lower electrode film 51 is removed below the outer edge of the intermediate electrode film 52. Specifically, in each of the vibration regions 22a to 22d, the lower electrode film 51, the intermediate electrode film 52, and the upper electrode film 53 are triangular in shape along the upper surface shape of each of the vibration regions 22a to 22d. The lower electrode film 51, the intermediate electrode film 52, and the upper electrode film 53 are similar in shape so that the intermediate electrode film 52 is larger than the lower electrode film 51 and the upper electrode film 53, and the lower electrode film 51 and the upper electrode film 53 are entirely inside the intermediate electrode film 52 in the XY plane. Note that while Figure 5 shows the top surface shapes of the lower electrode film 51 and the intermediate electrode film 52 in the first vibration region 22a, in the second to fourth vibration regions 22b to 22d as well, the entire lower electrode film 51 is similarly arranged inside the outer edge of the intermediate electrode film 52.
[0026] The distance between the outer edge of the intermediate electrode film 52 and the outer edge of the lower electrode film 51 in a direction perpendicular to the Z direction and perpendicular to the outer edges of the lower electrode film 51 and the intermediate electrode film 52 is defined as d1. In this embodiment, the distance d1 is set to 0.2 μm or more.
[0027] At the end faces of each of the vibration regions 22a to 22d, the end face of the intermediate electrode film 52 may be covered by the upper piezoelectric film 42 as shown in FIG. 2, or the end face of the intermediate electrode film 52 may be exposed to the slits 30.
[0028] The electrode films 50 of the first to fourth vibrating regions 22a to 22d are electrically connected in series by the wiring portion 60. Specifically, the lower-layer electrode films 51, the intermediate electrode films 52, and the upper-layer electrode films 53 formed in the respective vibrating regions 22a to 22d are connected in parallel, while the vibrating regions 22a to 22d are connected in series.
[0029] The wiring section 60 includes a first electrode section 61 connected to the lower layer electrode film 51, a second electrode section 62 connected to the middle layer electrode film 52, and a wiring film 63 connecting the first electrode section 61 and the second electrode section 62. The wiring section 60 also includes a third electrode section 64 connected to the upper layer electrode film 53, and the first electrode section 61 and the second electrode section 62 are also connected to the third electrode section 64 by the wiring film 63.
[0030] In the support region 21a, a first hole portion 61a is formed that penetrates the lower layer piezoelectric film 41 and the upper layer piezoelectric film 42 to expose the lower layer electrode film 51, and the first electrode portion 61 has a first through electrode 61b arranged in the first hole portion 61a so as to be electrically connected to the lower layer electrode film 51. In addition, in the support region 21a, a second hole portion 62a is formed that penetrates the upper layer piezoelectric film 42 to expose the middle layer electrode film 52, and the second electrode portion 62 has a second through electrode 62b arranged in the second hole portion 62a so as to be electrically connected to the middle layer electrode film 52.
[0031] In this embodiment, the lower layer piezoelectric film 41 located below the opening of the intermediate electrode film 52 of the first hole portion 61a is removed. Specifically, the first hole portion 61a is formed in a quadrangular prism shape with the Z direction as its axial direction. The lower layer piezoelectric film 41 is removed over the entire lower part of the opening of the intermediate electrode film 52 so that the wall surface of the first hole portion 61a has a flat shape in a cross section parallel to the Z direction.
[0032] As described later, an interlayer insulating film 81 is formed on the wall surface of the first hole portion 61a, the wall surface of the second hole portion 62a, and the upper surface of the upper layer piezoelectric film 42. The first through electrode 61b and the second through electrode 62b are disposed inside the first hole portion 61a and the second hole portion 62a, respectively, so as to be insulated from the piezoelectric film 40 by the interlayer insulating film 81. The wiring film 63 is disposed on the upper surface of the interlayer insulating film 81, and is electrically connected to the first through electrode 61b and the second through electrode 62b at the upper portion of the first hole portion 61a and the second hole portion 62a. Note that FIG. 1 illustrates only a portion of the wiring film 63 that connects the first through electrode 61a and the second through electrode 62b, and a pad portion that is connected to an external circuit.
[0033] The vibration section 20 has a buffer layer 70 on the support 10 side, on which the lower electrode film 51 is disposed. The buffer layer 70 is made of, for example, aluminum nitride (AlN) or the like. The buffer layer 70 is patterned in the same shape as the lower electrode film 51, and the lower electrode film 51 is formed on the upper surface of the buffer layer 70.
[0034] An interlayer insulating film 81 is formed on the wall surfaces of the first hole portion 61a and the second hole portion 62a. The interlayer insulating film 81 is intended to suppress leakage between the electrodes. The interlayer insulating film 81 is also formed on the upper surface of the upper electrode film 53 and on the upper surface of the upper piezoelectric film 42 exposed from the upper electrode film 53, and the first electrode portion 61 and the second electrode portion 62 are connected via a wiring film 63 formed on the upper surface of the interlayer insulating film 81. The interlayer insulating film 81 is made of a photosensitive resin such as polyimide or polybenzoxazole (PBO), or an insulating material such as an oxide film or a nitride film.
[0035] An opening 81a is formed in the interlayer insulating film 81 at the center of the piezoelectric element, and as a result, the upper electrode film 53 of the floating region 21b is exposed from the interlayer insulating film 81.
[0036] The above is the configuration of the piezoelectric element in this embodiment. In such a piezoelectric element, when pressure such as sound pressure is applied to each of the vibration regions 22a-22d, the vibration regions 22a-22d vibrate. For example, when the free end side of each of the vibration regions 22a-22d is displaced upward, a tensile stress is generated in the lower piezoelectric film 41, and a compressive stress is generated in the upper piezoelectric film 42. Therefore, pressure such as sound pressure can be detected by extracting an electric charge from the pad portion of the wiring portion 60.
[0037] A method for manufacturing the piezoelectric element of this embodiment will be described. First, a wafer-shaped support 10 is prepared, in which an insulating film 12 is disposed on a support substrate 11. Next, a buffer layer 70 and a lower electrode film 51 are formed in this order on the support 10 by using a CVD (Chemical Vapor Deposition) method or the like, and are patterned into the shape described above.
[0038] Next, the lower piezoelectric film 41 and the intermediate electrode film 52 are formed by CVD or the like, and the intermediate electrode film 52 is patterned into the shape described above. Similarly, the upper piezoelectric film 42 and the upper electrode film 53 are formed by CVD or the like, and the upper electrode film 53 is patterned into the shape described above.
[0039] After forming the piezoelectric film 40 and the electrode film 50 in this manner, a first hole 61a exposing the lower electrode film 51, a second hole 62a exposing the intermediate electrode film 52, and a slit 30 exposing the insulating film 12 are formed by etching. In addition, the piezoelectric film 40 located at the dicing line is removed to form an opening 20a, and the insulating film 12 is removed to form an opening 12a.
[0040] Thereafter, the interlayer insulating film 81 is formed. When the interlayer insulating film 81 is made of a photosensitive resin, the photosensitive resin is applied to the entire wafer so as to cover the support 10, the piezoelectric film 40, the electrode film 50, and the buffer layer 70, and the photosensitive resin is exposed to light using a mask (not shown). Then, the photosensitive resin in the portions corresponding to the opening 81a, the first hole 61a, and the second hole 62a is removed by development, and the interlayer insulating film 81 is formed. When the interlayer insulating film 81 is made of an insulator such as an oxide film or a nitride film, an insulator is laminated on the entire wafer so as to cover the support 10, the piezoelectric film 40, the electrode film 50, and the buffer layer 70, and then a resist is applied, and the resist is exposed to light using a mask (not shown). Then, the insulator in the portions corresponding to the opening 81a, the first hole 61a, and the second hole 62a is removed by etching, and the interlayer insulating film 81 is formed.
[0041] Next, a metal film is formed so as to fill the first hole 61a and the second hole 62a, thereby forming the first through electrode 61b and the second through electrode 62b. Then, the metal film formed on the interlayer insulating film 81 is patterned to form the wiring film 63. In this way, the wiring section 60 is formed.
[0042] Thereafter, a mask (not shown) is placed as appropriate and etching is performed to form recesses 10a. Then, the substrate is divided into chips along dicing lines. This completes the manufacture of the piezoelectric element having the vibration portion 20 disposed on the support 10.
[0043] The effect of this embodiment will be described. The inventors have investigated the relationship between the shape of the electrode film and tan δ with respect to the leakage current in a piezoelectric element. In a first comparative example shown in FIG. 5, the outer edge of the intermediate electrode film 52 is inside the outer edge of the lower electrode film 51 in the XY plane. In a second comparative example shown in FIG. 6, the intermediate electrode film 52 is divided into two, and the outer edges of the two intermediate electrode films 52 are inside the outer edge of the lower electrode film 51. In a third comparative example shown in FIG. 7, the intermediate electrode film 52 is divided into three, and the outer edges of the three intermediate electrode films 52 are inside the outer edge of the lower electrode film 51.
[0044] With this configuration, the perimeter of the entire intermediate electrode film 52 of the first to third comparative examples is the shortest in the first comparative example and the longest in the third comparative example. When tan δ was measured while changing the perimeter of the intermediate electrode film 52 in this way, as shown in FIG. 8, the longer the perimeter of the intermediate electrode film 52, the larger tan δ became.
[0045] Fig. 9 is a diagram showing the results of measuring tan δ while changing the distance d1. In Fig. 9, the distance d1 is a positive value when the outer edge of the intermediate electrode film 52 is outside the outer edge of the lower electrode film 51 in the XY plane, and is a negative value when the outer edge of the intermediate electrode film 52 is inside the outer edge of the lower electrode film 51. The distance d1 is 0 when the outer edges of the intermediate electrode film 52 and the lower electrode film 51 are aligned in the XY plane.
[0046] 9, when the distance d1 is in the range of 0 or more, tan δ is smaller than when the distance d1 is in the range of -2 μm or less. Moreover, when the distance d1 is in the range of -2 μm or more and less than 0, tan δ changes more greatly with respect to the change in the distance d1 than when the distance d1 is in the range of 0 or more and when the distance d1 is in the range of -2 μm or less.
[0047] From the results shown in Figures 8 and 9, it is believed that the area involved in the generation of leakage current and the increase in dielectric loss is located near the outer edge of the intermediate electrode film 52, and that leakage current occurs when the lower electrode film 51 is located below the outer edge of the intermediate electrode film 52.
[0048] As described above, in this embodiment, in the XY plane, the outer edge of the intermediate electrode film 52 is outside the outer edge of the lower electrode film 51. Therefore, since the lower electrode film 51 is not present below the outer edge of the intermediate electrode film 52, the occurrence of leakage current and an increase in tan δ can be suppressed, and the deterioration of the performance of the piezoelectric element can be suppressed.
[0049] Furthermore, according to the above embodiment, the following effects can be obtained.
[0050] (1) The lower piezoelectric film 41 located below the opening of the intermediate electrode film 52 of the first hole portion 61a is removed. As a result, the lower piezoelectric film 41 that serves as a path for leakage current between the opening end of the first hole portion 61a and the lower electrode film 51 does not exist, so that the occurrence of leakage current in the first hole portion 61a can be suppressed.
[0051] (2) The outer edge of the intermediate electrode film 52 is located 0.2 μm or more outside the outer edge of the lower electrode film 51. This makes it possible to maintain the outer edge of the intermediate electrode film 52 located outside the outer edge of the lower electrode film 51 even if the size varies due to misalignment in photolithography or size reduction in etching.
[0052] Second embodiment The second embodiment will be described. This embodiment is similar to the first embodiment except for the size of the upper-layer electrode film 53, and therefore only the differences from the first embodiment will be described.
[0053] 10 and 11, in the present embodiment, in the XY plane, the outer edge of the upper-layer electrode film 53 is outside the outer edge of the intermediate electrode film 52, and the intermediate electrode film 52 is removed below the outer edge of the upper-layer electrode film 53. In the present embodiment, the lower-layer electrode film 51 and the intermediate electrode film 52 correspond to the first electrode film and the second electrode film, respectively, and the intermediate electrode film 52 and the upper-layer electrode film 53 correspond to the first electrode film and the second electrode film, respectively.
[0054] The distance between the outer edge of the upper electrode film 53 and the outer edge of the intermediate electrode film 52 in a direction perpendicular to the Z direction and perpendicular to the outer edges of the intermediate electrode film 52 and the upper electrode film 53 is defined as d2.
[0055] In this embodiment, the second hole portion 62a penetrates the upper-layer piezoelectric film 42 and the upper-layer electrode film 53, and the upper-layer piezoelectric film 42 located below the opening of the upper-layer electrode film 53 of the second hole portion 62a is removed. Specifically, the second hole portion 62a is formed in a quadrangular prism shape with the Z direction as its axial direction. The upper-layer piezoelectric film 42 is removed over the entire lower part of the opening of the upper-layer electrode film 53 so that the wall surface of the second hole portion 62a has a flat shape in a cross section parallel to the Z direction.
[0056] If the outer edge of the upper electrode film 53 is inside the outer edge of the intermediate electrode film 52, there is a risk of leakage current occurring near the outer edge of the upper electrode film 53 when milling or the like is performed after the formation of the upper electrode film 53. In this embodiment, since the outer edge of the upper electrode film 53 is outside the outer edge of the intermediate electrode film 52, it is possible to suppress the occurrence of this leakage current. Note that, similar to the distance d1, it is desirable to set the distance d2 to 0.2 μm or more in consideration of alignment deviation in photolithography and size reduction in etching.
[0057] Furthermore, the upper piezoelectric film 42 located below the opening in the upper electrode film 53 of the second hole portion 62a is removed, and there is no upper piezoelectric film 42 that can serve as a path for leakage current between the opening end of the second hole portion 62a and the intermediate electrode film 52. Therefore, it is possible to suppress the occurrence of leakage current in the second hole portion 62a.
[0058] This embodiment has the same configuration and operation as the first embodiment, and therefore can obtain the same effects as the first embodiment.
[0059] Third embodiment The third embodiment will be described. This embodiment is similar to the second embodiment except that a protective film is added to the second embodiment, and therefore only the differences from the second embodiment will be described.
[0060] 12, the piezoelectric element of this embodiment includes a lower protective film 91 disposed between the lower piezoelectric film 41 and the intermediate electrode film 52, and an upper protective film 92 disposed between the upper piezoelectric film 42 and the upper electrode film 53. The lower protective film 91 and the upper protective film 92 are made of an oxide or nitride of silicon or the like.
[0061] This embodiment has the same configuration and operation as the first and second embodiments, and therefore can obtain the same effects as the first and second embodiments.
[0062] Furthermore, according to the above embodiment, the following effects can be obtained.
[0063] (1) A lower protective film 91 is provided between the lower piezoelectric film 41 and the intermediate electrode film 52. Also, an upper protective film 92 is provided between the upper piezoelectric film 42 and the upper electrode film 53. This makes it possible to prevent damage caused by etching of the intermediate electrode film 52 from reaching the lower piezoelectric film 41 and the lower electrode film 51, and to prevent damage caused by etching of the upper electrode film 53 from reaching the upper piezoelectric film 42 and the intermediate electrode film 52. This makes it possible to further suppress the occurrence of leakage current.
[0064] (2) The lower protective film 91 and the upper protective film 92 are made of an oxide film or a nitride film, which allows the lower protective film 91 and the upper protective film 92 to be formed in a simple process.
[0065] (Fourth embodiment) The fourth embodiment will be described. This embodiment is different from the third embodiment in that the intermediate electrode film 52 and the upper electrode film 53 are changed in configuration, but the rest is the same as the third embodiment, so only the differences from the third embodiment will be described.
[0066] 13, in this embodiment, slits 20b are formed in each of the vibration regions 22a to 22d, penetrating the lower piezoelectric film 41, the upper piezoelectric film 42, the lower protective film 91, and the upper protective film 92 to expose the upper surface of the lower electrode film 51. The slits 20b are formed inside the outer edge of the lower electrode film 51 in the XY plane, and open in a triangular frame shape similar to the upper surface of the lower electrode film 51. In other words, the lower piezoelectric film 41 and the upper piezoelectric film 42 are partitioned into a triangular region and another region by the slits 20b.
[0067] The intermediate electrode film 52 and the upper electrode film 53 are formed only in the portion of the vibration part 20 surrounded by the slit 20b so that their side surfaces are exposed to the inner wall surface of the slit 20b. That is, in the XY plane, the outer edges of the intermediate electrode film 52 and the upper electrode film 53 are coincident and are inside the outer edge of the lower electrode film 51. In this embodiment, the lower electrode film 51 corresponds to the first electrode film, and the intermediate electrode film 52 corresponds to the second electrode film.
[0068] In the slit 20b, the lower piezoelectric film 41 and the upper piezoelectric film 42 located at the lower part of the side surface of the intermediate electrode film 52 and the upper electrode film 53 are removed. Specifically, the slit 20b is a triangular frame-shaped slit extending in the Z direction. The lower piezoelectric film 41 and the upper piezoelectric film 42 are removed over the entire lower part of the portion from which the intermediate electrode film 52 and the upper electrode film 53 have been removed so that the wall surface of the slit 20b has a flat shape in a cross section parallel to the Z direction.
[0069] The inside of the slit 20b is filled with a buried insulating film 82. The buried insulating film 82 is made of an insulating material. In detail, the buried insulating film 82 is made of the same material as the interlayer insulating film 81, that is, a photosensitive resin such as polyimide or PBO, or an insulating material such as an oxide film or a nitride film. In this embodiment, the slit 20b is formed so as to reach the floating region 21b to the support region 21a, and the slit 20b formed in the support region 21a is filled with the interlayer insulating film 81.
[0070] This embodiment has the same configuration and operation as the first to third embodiments, and therefore can obtain the same effects as the first to third embodiments.
[0071] Furthermore, according to the above embodiment, the following effects can be obtained.
[0072] (1) The lower piezoelectric film 41 and the upper piezoelectric film 42 located below the opening of the slit 20b are removed. As a result, the lower piezoelectric film 41 and the upper piezoelectric film 42 that serve as paths for leakage current do not exist between the lower electrode film 51 and the side surface of the intermediate electrode film 52 and the upper electrode film 53 exposed on the inner wall surface of the slit 20b, and therefore it is possible to suppress the occurrence of leakage current in the slit 20b.
[0073] (2) The inside of the slit 20b is filled with the buried insulating film 82. This can suppress short circuits in the portions where the lower piezoelectric film 41 and the upper piezoelectric film 42 have been removed, improving the reliability of the piezoelectric element.
[0074] (Other embodiments) The present invention is not limited to the above-mentioned embodiment, and can be appropriately modified within the scope of the claims. The above-mentioned embodiments are not unrelated to each other, and can be appropriately combined, except when the combination is clearly impossible. In the above-mentioned embodiments, it goes without saying that the elements constituting the embodiment are not necessarily essential, except when it is specifically stated that they are essential or when it is clearly considered to be essential in principle. In the above-mentioned embodiments, when the numbers, values, amounts, ranges, etc. of the components of the embodiment are mentioned, they are not limited to the specific numbers, except when it is specifically stated that they are essential or when it is clearly limited to a specific number in principle. In the above-mentioned embodiments, when the shapes, positional relationships, etc. of the components are mentioned, they are not limited to the shapes, positional relationships, etc., except when it is specifically stated that they are essential or when it is clearly limited to a specific shape, positional relationship, etc. in principle.
[0075] In the first and second embodiments, the lower electrode film 51, the intermediate electrode film 52, and the upper electrode film 53 do not have to have similar shapes. In this case, in the first embodiment, it is desirable to set the shortest distance between the outer edge of the lower electrode film 51 and the outer edge of the intermediate electrode film 52 in the XY plane to 0.2 μm or more. In the second embodiment, it is desirable to set the shortest distance between the outer edge of the intermediate electrode film 52 and the outer edge of the upper electrode film 53 in the XY plane to 0.2 μm or more.
[0076] In the second embodiment, the outer edge of the intermediate electrode film 52 may be located at the same position as the outer edge of the lower electrode film 51 in the XY plane, or the outer edge of the intermediate electrode film 52 may be located inside the outer edge of the lower electrode film 51. Even in such a configuration, it is possible to suppress leakage current between the intermediate electrode film 52 and the upper electrode film 53. However, since the lower piezoelectric film 41 serves as a base for the upper piezoelectric film 42, it is preferable that the lower electrode film 51 and the intermediate electrode film 52 arranged above and below the lower piezoelectric film 41 are arranged so that the lower electrode film 51 is located inside the outer edge of the intermediate electrode film 52 in the XY plane.
[0077] In the third embodiment, the piezoelectric element may include only one of the lower protective film 91 and the upper protective film 92. The outer edge of the intermediate electrode film 52 may be located at the same position as the outer edge of the lower electrode film 51 in the XY plane, or the outer edge of the intermediate electrode film 52 may be located inside the outer edge of the lower electrode film 51. Even when the outer edge of the intermediate electrode film 52 coincides with the outer edge of the lower electrode film 51 or is located inside the outer edge of the lower electrode film 51, the lower protective film 91 can suppress the leak current. Similarly, the outer edge of the upper electrode film 53 may be located at the same position as the outer edge of the intermediate electrode film 52, or the outer edge of the upper electrode film 53 may be located inside the outer edge of the intermediate electrode film 52.
[0078] In the fourth embodiment, the outer edge of the upper electrode film 53 may be located inside the outer edge of the intermediate electrode film 52 in the XY plane, and the slit 20b may be formed to penetrate the upper piezoelectric film 42 to expose the upper surface of the intermediate electrode film 52. In such a configuration, the intermediate electrode film 52 corresponds to the first electrode film, and the upper electrode film 53 corresponds to the second electrode film. Furthermore, the piezoelectric element may not include the lower protective film 91 and the upper protective film 92. Furthermore, the inside of the slit 20b may not be filled with the interlayer insulating film 81 and the buried insulating film 82.
[0079] Features of the Disclosure [First viewpoint] A piezoelectric element, A support (10); A first electrode film (51, 52) laminated on the support; a piezoelectric film (41, 42) laminated on the first electrode film; A second electrode film (52, 53) laminated on the piezoelectric film, a piezoelectric element in which, in a plane perpendicular to a stacking direction of the first electrode film, the piezoelectric film, and the second electrode film, an outer edge of the second electrode film is located outside an outer edge of the first electrode film. [Second viewpoint] a wiring film (63) disposed on the second electrode film; a through electrode (61b, 62b) connecting the first electrode film and the wiring film; the through electrode is disposed inside a hole portion (61a, 62a) that penetrates the second electrode film and the piezoelectric film to expose the first electrode film, The piezoelectric element according to a first aspect, wherein the piezoelectric film located below an opening in the second electrode film of the hole is removed. [Third Perspective] The piezoelectric element according to the first or second aspect, wherein an outer edge of the second electrode film is located outwardly of an outer edge of the first electrode film by 0.2 μm or more. [Fourth viewpoint] A piezoelectric element, A support (10); A first electrode film (51, 52) laminated on the support; a piezoelectric film (41, 42) laminated on the first electrode film; A second electrode film (52, 53) laminated on the piezoelectric film, an outer edge of the second electrode film is located inside an outer edge of the first electrode film in a plane perpendicular to a stacking direction of the first electrode film, the piezoelectric film, and the second electrode film; the piezoelectric film is partitioned by a slit (20b) that exposes an upper surface of the first electrode film and a side surface of the second electrode film, A piezoelectric element in which the piezoelectric film located at the lower part of the side surface at the slit is removed. [Fifth viewpoint] The piezoelectric element according to a fourth aspect, wherein the inside of the slit is filled with an insulating film (81, 82). [Sixth viewpoint] The piezoelectric element according to any one of the first to fifth aspects, further comprising a protective film (91, 92) disposed between the piezoelectric film and the second electrode film. [Seventh viewpoint] The piezoelectric element according to a sixth aspect, wherein the protective film is made of a nitride or an oxide. [Eighth viewpoint] A lower electrode film (51) laminated on the support; a lower layer piezoelectric film (41) laminated on the lower layer electrode film; an intermediate electrode film (52) laminated on the lower piezoelectric film; an upper layer piezoelectric film (42) laminated on the intermediate electrode film; an upper layer electrode film (53) laminated on the upper layer piezoelectric film, the first electrode film is composed of the lower electrode film, The piezoelectric element according to any one of the first to seventh aspects, wherein the second electrode film is constituted by the intermediate electrode film. [Ninth viewpoint] A lower electrode film (51) laminated on the support; a lower layer piezoelectric film (41) laminated on the lower layer electrode film; an intermediate electrode film (52) laminated on the lower piezoelectric film; an upper layer piezoelectric film (42) laminated on the intermediate electrode film; an upper layer electrode film (53) laminated on the upper layer piezoelectric film, the first electrode film is composed of the intermediate electrode film, The piezoelectric element according to any one of the first to seventh aspects, wherein the second electrode film is constituted by the upper electrode film. [10th viewpoint] The piezoelectric element according to any one of the first to ninth aspects, which is a microphone for detecting a sound pressure applied to the piezoelectric film. [Explanation of symbols]
[0080] 10 Support 41 Lower Piezoelectric Film 42 Upper layer piezoelectric film 51 Lower electrode film 52 Intermediate electrode membrane 53 Upper electrode film
Claims
1. A piezoelectric element, A support (10); A first electrode film (51, 52) laminated on the support; a piezoelectric film (41, 42) laminated on the first electrode film; A second electrode film (52, 53) laminated on the piezoelectric film, A piezoelectric element in which, in a plane perpendicular to a stacking direction of the first electrode film, the piezoelectric film, and the second electrode film, an outer edge of the second electrode film is located outside an outer edge of the first electrode film.
2. A wiring film (63) disposed on the second electrode film; a through electrode (61b, 62b) connecting the first electrode film and the wiring film; the through electrode is disposed inside a hole portion (61 a, 62 a) that penetrates the second electrode film and the piezoelectric film to expose the first electrode film, The piezoelectric element according to claim 1 , wherein the piezoelectric film located below an opening in the second electrode film of the hole is removed.
3. 3. The piezoelectric element according to claim 1, wherein an outer edge of the second electrode film is located 0.2 [mu]m or more outside an outer edge of the first electrode film.
4. A piezoelectric element, A support (10); A first electrode film (51, 52) laminated on the support; a piezoelectric film (41, 42) laminated on the first electrode film; A second electrode film (52, 53) laminated on the piezoelectric film, an outer edge of the second electrode film is located inside an outer edge of the first electrode film in a plane perpendicular to a stacking direction of the first electrode film, the piezoelectric film, and the second electrode film; the piezoelectric film is partitioned by a slit (20b) that exposes an upper surface of the first electrode film and a side surface of the second electrode film; A piezoelectric element in which the piezoelectric film located at the lower part of the side surface at the slit is removed.
5. 5. The piezoelectric element according to claim 4, wherein the inside of the slit is filled with an insulating film (81, 82).
6. 6. The piezoelectric element according to claim 1, further comprising a protective film (91, 92) disposed between the piezoelectric film and the second electrode film.
7. 7. The piezoelectric element according to claim 6, wherein the protective film is made of a nitride or an oxide.
8. A lower electrode film (51) laminated on the support; A lower layer piezoelectric film (41) laminated on the lower layer electrode film; An intermediate electrode film (52) laminated on the lower piezoelectric film; an upper layer piezoelectric film (42) laminated on the intermediate electrode film; an upper layer electrode film (53) laminated on the upper layer piezoelectric film; the first electrode film is formed of the lower electrode film, 8. The piezoelectric element according to claim 1, wherein the second electrode film is formed of the intermediate electrode film.
9. A lower electrode film (51) laminated on the support; A lower layer piezoelectric film (41) laminated on the lower layer electrode film; An intermediate electrode film (52) laminated on the lower piezoelectric film; an upper layer piezoelectric film (42) laminated on the intermediate electrode film; an upper layer electrode film (53) laminated on the upper layer piezoelectric film; the first electrode film is composed of the intermediate electrode film, 8. The piezoelectric element according to claim 1, wherein the second electrode film is formed of the upper electrode film.
10. 10. The piezoelectric element according to claim 1, which is a microphone for detecting a sound pressure applied to the piezoelectric film.
Citation Information
Patent Citations
Single-crystal piezoelectric structure and method for manufacturing same, and electronic device having single-crystal piezoelectric laminated structure
CN111146327A
Multilayer piezoelectric device and manufacturing method for the same
JP2009194226A
Piezoelectric actuator and optical scanner
JP2014082464A
Acoustic transducer having a gap control structure and method for manufacturing an acoustic transducer
JP2014515214A
Piezoelectric device
WO2020235131A1