Crack detection system, and crack detection method

The optical fiber cable-based crack detection system addresses the burdensome and costly nature of conventional methods by allowing permanent installation, reducing maintenance and operational costs while providing accurate crack detection in concrete structures.

JP2024158462APending Publication Date: 2024-11-08TAISEI CORP +4
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023073682
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Conventional crack detection methods for concrete structures, such as those used in concrete-surfaced rockfill dams, are burdensome due to the complexity of installing and removing geophones for each measurement, require multiple receivers for large or densely measured areas, and are costly.

Method used

A crack detection system utilizing an optical fiber cable buried within the concrete structure, which generates vibrations and measures surface waves using an optical fiber cable, allowing for analysis of crack states without the need for repeated installation or removal, and is cheaper than conventional geophones.

Benefits of technology

The system reduces the maintenance burden and cost by allowing the optical fiber cable to remain buried, enabling accurate crack detection with reduced installation and operational costs, and can measure surface waves at closer intervals.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158462000001_ABST
    Figure 2024158462000001_ABST
Patent Text Reader

Abstract

To provide a crack detection system and a crack detection method that can reduce a burden of managing concrete structures.SOLUTION: A crack detection system 1 detecting cracks in a concrete structure (one example is a face slab concrete 4) comprises: an optical fiber cable 5 embedded inside the concrete structure; vibration generating means 6 for applying vibrations to the concrete structure; measuring means 11 for measuring surface waves transmitted through the optical fiber cable 5; and analysis means 13 for analyzing a condition of cracks occurring in the concrete structure based on the measured waveform measured by the measuring means 11.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a system and a method for detecting cracks in a concrete structure. [Background technology]

[0002] One type of dam is a rockfill dam, which is constructed by piling up rocks and soil, and one form of rockfill dam is a concrete-faced impermeable wall type rockfill dam. In a concrete-faced impermeable wall type rockfill dam, the upstream face of the dam is covered with a concrete slab (called "face slab concrete") to impermeable water. As part of the maintenance and management of such dams, it is desirable to understand the condition of cracks that occur in the face slab concrete. Techniques for measuring defects such as cracks in concrete are described, for example, in Patent Documents 1 and 2. As described in Patent Documents 1 and 2, a conventional crack detection method involves installing a receiver on the surface of a concrete structure. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 64-065407 [Patent Document 2] Japanese Patent Application Publication No. 5-113428 Summary of the Invention [Problem to be solved by the invention]

[0004] Conventional crack detection methods require the installation of a receiver (e.g., a geophone) and a cable for signal transmission in the measurement area, which makes the installation work complicated and places a burden on workers. In addition, the installation and removal of the receiver etc. is necessary every time a measurement is made, which is a heavy burden, and is even heavier when measurements are made periodically. In addition, one receiver is required for each observation point, so the larger the measurement area or the more densely the measurements are performed, the more receivers are required, which creates a cost problem. From this perspective, the present invention provides a crack detection system and a crack detection method that can reduce the burden of managing concrete structures. [Means for solving the problem]

[0005] A crack detection system according to the present invention is a system for detecting cracks in a concrete structure, and includes an optical fiber cable, a vibration generating means, a measuring means, and an analyzing means. The optical fiber cable is buried inside the concrete structure. The vibration generating means applies vibrations to the concrete structure. The measuring means measures surface waves transmitted through the optical fiber cable. The analyzing means analyzes the state of cracks occurring in the concrete structure based on the waveform measured by the measuring means. The analysis means, for example, calculates a Fourier spectrum for the measured waveform that reaches directly from the vibration generating means to each of a plurality of measurement points set on the optical fiber cable, and detects the presence or absence of a crack based on the magnitude of the amplitude of the Fourier spectrum.

[0006] In the crack detection system according to the present invention, the optical fiber cable can be left buried, so once the optical fiber cable is installed the first time, there is no need to remove the optical fiber cable or reinstall it a second or subsequent time. In addition, optical fiber cables are cheaper (e.g., several hundred to several thousand yen per meter) than conventional receivers (e.g., geophones), and since they can measure surface waves every tens of centimeters, cost is unlikely to be an issue even if the measurement area becomes large.

[0007] The analysis means may calculate a Fourier spectrum of the waveform that is directly transmitted from the vibration generating means to each of a plurality of measurement points set on the optical fiber cable, and display a contour diagram based on the amplitude of the Fourier spectrum on the display means. In this way, it is easy to identify the location of the crack.

[0008] The concrete structure is, for example, face slab concrete of a concrete-faced impermeable wall type rockfill dam. When the concrete structure is assumed to be a face slab concrete, the optical fiber cable is inserted into the face slab concrete from the top end, turned back at the toe of the slope, and extended from the top end. The vibration generating means applies vibrations to multiple points on the top end. In this way, cracks occurring in the face slab concrete of a concrete-faced impermeable wall type rockfill dam can be detected with high accuracy, and the burden of maintaining and managing the dam is reduced compared to the conventional method.

[0009] When the face slab concrete is composed of a plurality of blocks, the optical fiber cable may be arranged across at least two or more of the blocks. In this way, the number of optical fibers (the number of channels) connected to a measuring means (eg, an interrogator) can be reduced, and therefore the number of measuring means can be reduced.

[0010] A crack detection method according to the present invention is a method for detecting a crack in a concrete structure, and includes an optical fiber installation step, a vibration generation step, a surface wave measurement step, and a crack analysis step. In the optical fiber installation step, an optical fiber cable is installed inside the concrete structure. In the vibration generation step, vibrations are applied to the concrete structure. In the surface wave measurement step, surface waves transmitted through the optical fiber cable are measured. In the crack analysis step, the state of a crack occurring in the concrete structure is analyzed based on the waveform measured in the surface wave measurement step.

[0011] In the crack detection method according to the present invention, the optical fiber cable can be left buried, so once the optical fiber cable is installed the first time, there is no need to remove the optical fiber cable or reinstall it for the second or subsequent times. In addition, optical fiber cables are cheaper (e.g., several hundred to several thousand yen per meter) than conventional receivers (e.g., geophones), and since they can measure surface waves every tens of centimeters, cost is unlikely to be an issue even if the measurement area becomes large.

[0012] The crack detection method may further include a strain measurement step of measuring a strain occurring in the optical fiber cable, and a deformation analysis step of analyzing a deformation occurring in the concrete structure based on the strain measured in the strain measurement step. In the strain measurement step, a measuring means for measuring strain is connected to the optical fiber cable to measure the strain. In the surface wave measurement step, a measuring means for measuring surface waves is connected to the optical fiber cable instead of the measuring means for measuring strain, to measure the surface waves. In this way, the optical fiber cable used to measure the distortion of the concrete structure during construction can also be used for maintenance after construction, which is economical. Effect of the Invention

[0013] According to the present invention, the burden of managing concrete structures can be reduced. [Brief description of the drawings]

[0014] [Figure 1] 1 is a schematic configuration diagram of a crack detection system according to an embodiment of the present invention. [Diagram 2] This is an oblique view of a concrete surface impermeable wall type rockfill dam. [Diagram 3] This is a cross-sectional view of a concrete-faced impermeable wall type rockfill dam. [Figure 4] FIG. 2 is an enlarged view of range A in FIG. [Diagram 5] 1 is an example of a measured waveform. [Figure 6] FIG. 2 is a conceptual diagram of an analysis process executed by an analysis unit. [Figure 7] 13 is an example of a case where contour maps are displayed in chronological order. [Figure 8] This is an example of a method for detecting cracks from measurement results. [Figure 9] 4 is a flowchart showing steps of a crack detection method performed by a crack detection system according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, the embodiment of the present invention will be described in detail with reference to the drawings. Each drawing is merely a schematic illustration to allow a sufficient understanding of the present invention. Therefore, the present invention is not limited to the illustrated examples. In each drawing, common or similar components are denoted by the same reference numerals, and duplicated explanations thereof will be omitted.

[0016] <Configuration of the crack detection system according to the embodiment> The configuration of a crack detection system 1 according to an embodiment will be described with reference to Fig. 1 to Fig. 3. Fig. 1 is a schematic configuration diagram of the crack detection system 1 according to an embodiment. Fig. 2 is a perspective view of a concrete-faced water impermeable wall type rockfill dam, and Fig. 3 is a cross-sectional view of the concrete-faced water impermeable wall type rockfill dam.

[0017] The crack detection system 1 shown in FIG. 1 is a system that detects cracks (fissures) that occur in a concrete structure to be monitored. The concrete structure is, for example, a face slab concrete 4 in a concrete-surface water-impermeable wall-type rockfill dam 2 (hereinafter referred to as "dam 2") shown in FIG. 2 and FIG. 3. The face slab concrete 4 is a concrete slab that covers the upstream face of the dam 2. As shown in FIG. 2, the face slab concrete 4 is composed of a plurality of strip-shaped blocks BK that extend in the vertical direction. The blocks BK are arranged in a line in the width direction of the dam 2. Note that the concrete structure is not limited to the face slab concrete 4, and may be something other than a dam.

[0018] 1, the crack detection system 1 includes an optical fiber cable 5, a vibration generating means 6, a measuring means 11, a recording means 12, an analyzing means 13, and a display means 14. The optical fiber cable 5 and the vibration generating means 6 are installed in a face slab concrete 4, and the measuring means 11, the recording means 12, the analyzing means 13, and the display means 14 are installed in, for example, an administration building 3.

[0019] (optical fiber cable) The optical fiber cable 5 is embedded in the face slab concrete 4. Therefore, the surface of the optical fiber cable 5 is preferably coated with resin. The optical fiber cable 5 is fixed to the reinforcing bars in the concrete using a fixing means such as a binding wire. The optical fiber cable 5 is preferably installed continuously throughout the entire measurement area. If it is difficult to ensure the continuity of the optical fiber cable 5, it is also possible to install the optical fiber cable 5 in each divided area and later connect the optical fiber cables 5 by a dedicated connector or fusion. If the direction of a crack that will occur in the face slab concrete 4 can be predicted in advance, it is preferable to arrange the optical fiber cable 5 so that it intersects with the crack (preferably perpendicular). In other words, it is preferable to arrange the optical fiber cable 5 so that the extension direction of the crack and the optical fiber cable 5 are not parallel to each other.

[0020] An example of the arrangement of the optical fiber cable 5 will be described with reference to Fig. 1. In this embodiment, the entire area of ​​the face slab concrete 4 is assumed to be the measurement area. Therefore, the optical fiber cable 5 is arranged across all the blocks BK. Note that, when the measurement area is a specific block BK, it is sufficient that the optical fiber cable 5 is arranged at least in the block BK to be measured.

[0021] Focusing on each block BK, as shown in FIG. 4, the optical fiber cable 5 is inserted into the face slab concrete 4 from the top end of the face slab concrete 4, turns back at the foot of the slope, and is arranged so as to extend from the top end to the outside. FIG. 4 is an enlarged view of the range A in FIG. 1. The symbol P in FIG. 4 indicates the source of vibration, and the dashed arrow from the source P is an image of vibration propagation. The optical fiber cable 5 extended to the outside is inserted again into the face slab concrete 4 from the top end of the adjacent block BK. In other words, the optical fiber cable 5 inserted from the top end of the block BK1, reaches the foot of the slope, returns, and extends from the top end, and is inserted from the top end of the adjacent block BK2, reaches the foot of the slope, returns, and extends from the top end. In this way, the optical fiber cable 5 that has passed through all the blocks BK is connected to the measurement means 11 (see FIG. 1).

[0022] (Vibration generating means) The vibration generating means 6 shown in FIG. 1 applies vibration to the face slab concrete 4, which is a concrete structure. The vibration generating means 6 is installed on the top end of the face slab concrete 4. The vibration generating means 6 may be, for example, an impulse type vibrator or a sweep type vibrator. As shown in FIG. 4, in this embodiment, since vibration is generated at a plurality of points, it is preferable that the vibration generating means 6 is movable and easy to carry. In this embodiment, as shown in FIG. 4, vibration is generated at a total of five points for each block BK: (1) the left end point P1 of the block BK, (2) the right end point P5 of the block BK, (3) the center point P3 of the block BK, (4) the insertion point P2 of the optical fiber cable 5, and (5) the extension point P4 of the optical fiber cable 5.

[0023] (Method of measurement) The measuring means 11 shown in FIG. 1 is a device for measuring a surface wave (Rayleigh wave) transmitted through the optical fiber cable 5, and the optical fiber cable 5 is connected to the measuring means 11. The measuring means 11 is, for example, an interrogator for measuring a distributed optical fiber sensor (DAS). The interrogator has a function as a light source device for injecting light into the optical fiber cable 5, a function as a sensor for analyzing reflected light from an FBG (Fiber Bragg Grating) arranged in the core of the optical fiber cable 5, and a function for recording a signal obtained from the optical fiber cable 5. The measuring means 11 is a precision instrument and is therefore preferably installed indoors. The measuring means 11 outputs the measured surface wave (referred to as a "measurement waveform") to the analyzing means 13. FIG. 5 shows a measurement waveform measured by the measuring means 11. FIG. 5 shows an example of the measurement waveform.

[0024] (Recording means) 1 is used as an external recording device for the measurement means 11 and the analysis means 13. The recording means 12 is, for example, a hard disk drive (HDD) or a solid state drive (SSD) for storing data. The recording means 12 reads out stored data and records new data in response to instructions from the measurement means 11 and the analysis means 13.

[0025] (Analysis means) The analysis means 13 shown in FIG. 1 analyzes the state of cracks occurring in the face slab concrete 4 based on the measurement waveforms measured by the measurement means 11. The analysis means 13 is a device with a calculation function (e.g., a PC (Personal Computer)), and functions required for analysis are realized by executing an application program for DAS (Distributed Optical Fiber Sensor) measurement in a CPU (Central Processing Unit). The analysis means 13 calculates a Fourier spectrum for a waveform (direct wave) that directly reaches each of a plurality of measurement points set on the optical fiber cable 5 from the vibration generation means 6 among the measurement waveforms measured by the measurement means 11, and detects the presence or absence of a crack based on the magnitude of the amplitude of the Fourier spectrum. The analysis means 13 may display a contour diagram based on the magnitude of the amplitude of the Fourier spectrum on the display means 14 (see FIG. 1).

[0026] An example of the analysis process executed by the analysis means 13 will be described with reference to Fig. 6. Fig. 6 is a conceptual diagram of the analysis process executed by the analysis means 13. The analysis means 13 reads, from the waveform record, time history data of the amplitude of the surface wave that reaches each of a plurality of measurement points Q (only some of which are shown in FIG. 6) set on the optical fiber cable 5. Next, the analysis means 13 extracts the surface wave (reference numeral 91 in FIG. 6) that first arrives at each measurement point Q. That is, reflected waves from cracks and ends of the structure are excluded, and direct waves are extracted. Next, a Fourier transform is performed on the time history data of the extracted waveform to calculate the Fourier spectrum and read the amplitude at any frequency. By comparing the amplitude at adjacent measurement points Q, it is possible to determine whether a reflected wave has occurred. In Figure 6, spectrum attenuation (a decrease in amplitude due to the occurrence of a reflected wave) has occurred in the part indicated by the reference numeral 92, indicating that there is a crack in that part.

[0027] Next, the analysis means 13 creates a contour diagram based on the magnitude of the amplitude of the Fourier spectrum, and causes the display means 14 to display the contour diagram. The worker checks the contour diagram and estimates the presence or absence of a crack and the progress of the crack. In the contour diagram, the crack location is highlighted, for example, as shown by reference numeral 93 in FIG. 6. The presence or absence of a crack can be determined by using an existing technique. For example, a threshold value for determining the presence or absence of a crack is set by referring to the technique described in the following document. Jun Ejima et al., "Vibration Isolation Effect of Ditches and Underground Walls," Soil and Foundations, 28(3), pp.49-55, No.1160, March 25, 1980, Soil and Foundations, Japan Society of Soil and Foundations,

[0028] It is also possible to perform measurements periodically and display the contour diagrams in chronological order as shown in Figure 7. This makes it possible to compare past and present measurement results. This allows workers to easily grasp the occurrence of cracks and their progression.

[0029] Next, an example of a method for detecting cracks is shown in Fig. 8. Fig. 8 shows an example of a method for detecting cracks from measurement results. The time history data of the measured waveform at each measurement point is Fourier transformed to calculate the Fourier spectrum (amplitude distribution for each frequency) as shown by reference numeral 81 in Fig. 8. Based on the calculated amplitude distribution at each measurement point, it is assumed that a crack exists between the measurement points where attenuation is observed (see reference numeral 82 in Fig. 8). Next, the amplitude ratio before and after passing through the crack (the amplitude ratio between adjacent measurement points) is calculated as shown by reference numeral 83 in Fig. 8. For example, at a frequency f = 1.2 [kHz], an amplitude ratio γ = 0.6 is calculated. Next, as shown by reference numeral 84 in FIG. 8, the wavelength λ=v / f=(2.07 / 1.2)=1.73 is calculated from the surface wave velocity v=2.07 [km / s] when the frequency f=1.2 [kHz]. Finally, by substituting the calculated γ and λ into the relational equation between crack depth and surface wave attenuation (amplitude ratio), γ = exp(-2.35d / λ), the crack depth d = 370 [mm] is obtained. Note that the above relational equation is an approximation obtained from the results of a prior experiment.

[0030] <Processes of the crack detection method according to the embodiment> A description will be given of a crack detection method performed by the crack detection system 1 with reference to Fig. 9 (and Figs. 1 to 8 as appropriate). Fig. 9 is a flowchart showing the steps of the crack detection method in this embodiment. (Installation of measuring instruments, etc. "S11") First, a worker buries the optical fiber cable 5 in the face slab concrete 4. The optical fiber cable 5 may be installed during the construction stage of the face slab concrete 4, or may be installed after the construction of the face slab concrete 4 is completed and the maintenance stage begins. In addition, the measurement means 11 is installed indoors (for example, in the management building 3), and the optical fiber cable 5 is connected to the measurement means 11. This completes the measurement preparation.

[0031] The optical fiber cable 5 may be installed at the construction stage of the face slab concrete 4, and the optical fiber cable 5 may be used to analyze the deformation occurring in the face slab concrete 4 during the construction period. For example, a measuring means for measuring strain is connected to the optical fiber cable 5, and the measuring means measures the deformation occurring in the optical fiber cable 5 (strain measuring process). Also, based on the strain measured in the strain measuring process, the deformation occurring in the face slab concrete 4 is analyzed (deformation analysis process). Then, in the maintenance stage, the measuring means 11 for measuring surface waves is connected to the optical fiber cable 5 instead of the measuring means for measuring strain.

[0032] (Start of measurement "S12", excitation of surface waves "S13", reception of surface waves "S14") The measuring means 11 is brought into a state in which it can measure by turning on the power, and the vibration generating means 6 is installed along the measurement line where the first measurement will be performed. For example, the vibration generating means 6 is installed at the left end point P1 (see FIG. 4) of the block BK located at the leftmost position shown in FIG. 1. The vibration generating means 6 is then operated to generate vibrations in the face slab concrete 4, and the measuring means 11 is used to measure surface waves at a plurality of measurement points Q set on the optical fiber cable 5. It is also possible to measure surface waves that propagate across two optical fiber cables 5.

[0033] (Transmission line "S15") Next, the vibration generating means 6 is moved to the measurement line where the next measurement will be performed. For example, the vibration generating means 6 is installed at the insertion point P2 (see FIG. 4) of the optical fiber cable 5 of the block BK located at the leftmost position shown in FIG. 1. Then, similar to the case of the left end point P1, the vibration generating means 6 is operated to generate vibrations in the face slab concrete 4, and the measurement means 11 is used to measure surface waves at multiple measurement points Q set on the optical fiber cable 5. Since it is necessary to receive surface waves with sufficient amplitude throughout the entire measurement target area, multiple measurements are performed while changing the vibration excitation position in this way.

[0034] In this way, within one block BK, measurements are taken by moving the vibration generating means 6 in the order of the left end point P1 of the block BK, the insertion point P2 of the optical fiber cable 5, the center point P3 of the block BK, the extension point P4 of the optical fiber cable 5, and the right end point P5 of the block BK. In other words, multiple measurements are taken for each block BK. Once measurements of one block BK are completed, measurements are taken of the neighboring block BK in the same manner, until measurements have been taken of all blocks BK. Once measurements have been completed for all blocks BK, work on site is finished.

[0035] (Start of analysis "S21", calculation of spectrum of measured waveform "S22", contour plot of amplitude change "S23", analysis completed "S24") Next, an analysis is performed using the method described with reference to FIG. 6, and a contour diagram of the entire face slab concrete 4 is created.

[0036] (Understanding the occurrence and progression of cracks "S25") The worker can ascertain the occurrence of cracks and their progression by checking the contour diagram displayed on the display means 14. The worker may also ascertain the occurrence of cracks and their progression by comparing the contour diagram created in the previous measurement with the current contour diagram. This completes the understanding of the current situation. The measurements and analyses described up to this point are carried out periodically.

[0037] As described above, according to the crack detection system 1 of this embodiment, it is possible to leave the optical fiber cable 5 buried. Therefore, once the optical fiber cable 5 is installed for the first time, there is no need to remove the optical fiber cable 5 or reinstall it for the second or subsequent times. In addition, the optical fiber cable 5 is cheaper (e.g., several hundred to several thousand yen per meter) than conventional receivers (e.g., geophones), and since it can measure surface waves every tens of centimeters, cost is unlikely to be an issue even if the measurement area becomes large. Furthermore, the optical fiber cable 5 used to measure the strain of the concrete structure (face slab concrete 4 in this embodiment) during construction can also be used for maintenance after construction, which is economical. [Explanation of symbols]

[0038] 1. Crack Detection System 2. Concrete-faced impermeable wall type rockfill dam 3 Administration building 4. Face slab concrete 5. Fiber optic cable 6. Means of generating vibration 11 Measurement methods 12 Recording means 13 Analysis methods 14 Display means

Claims

1. A crack detection system for detecting cracks in a concrete structure, comprising: an optical fiber cable buried inside the concrete structure; a vibration generating means for applying vibration to the concrete structure; a measuring means for measuring a surface wave transmitted through the optical fiber cable; and an analysis means for analyzing a state of a crack occurring in the concrete structure based on the measurement waveform measured by the measurement means. A crack detection system comprising:

2. the analysis means calculates a Fourier spectrum for a waveform that is directly transmitted from the vibration generating means to each of a plurality of measurement points set on the optical fiber cable, among the measured waveforms, and detects the presence or absence of a crack based on the magnitude of the amplitude of the Fourier spectrum. The crack detection system of claim 1 .

3. the analysis means calculates a Fourier spectrum for a waveform that has directly reached each of a plurality of measurement points set on the optical fiber cable from the vibration generating means, among the measured waveforms, and causes a display means to display a contour diagram based on the magnitude of the amplitude of the Fourier spectrum; The crack detection system of claim 1 .

4. The concrete structure is a face slab concrete of a concrete surface impermeable wall type rockfill dam; The crack detection system of claim 1 .

5. The optical fiber cable is inserted into the face slab concrete from the top end, turned back at the toe of the slope, and extended from the top end, The vibration generating means applies vibration to a plurality of points on the top end.

5. The crack detection system of claim 4.

6. The face slab concrete is composed of a plurality of blocks, The optical fiber cable is disposed across at least two or more of the blocks.

5. The crack detection system of claim 4.

7. A method for detecting cracks in a concrete structure, comprising: an optical fiber installation step of installing an optical fiber cable inside the concrete structure; a vibration generating step of applying vibration to the concrete structure; a surface wave measuring step of measuring a surface wave transmitted through the optical fiber cable; and a crack analysis step of analyzing a state of a crack occurring in the concrete structure based on the measurement waveform measured in the surface wave measurement step. A crack detection method comprising:

8. a strain measuring step of measuring a strain occurring in the optical fiber cable; and a deformation analysis step of analyzing deformation occurring in the concrete structure based on the strain measured in the strain measurement step. In the strain measuring step, a measuring means for measuring strain is connected to the optical fiber cable to measure the strain, In the surface wave measuring step, a measuring means for measuring a surface wave is connected to the optical fiber cable instead of the measuring means for measuring the strain, and the surface wave is measured. The method of claim 7, wherein the crack is detected by the crack detecting means.

Citation Information

Patent Citations

  • Measuring instrument for thickness of concrete and position of internal cracking

    JP1989065407A

  • Method for detecting defect in concrete wall body

    JP1993113428A