Method for evaluating physical properties of skin surface layer

The method addresses the challenge of inaccurate skin surface layer evaluations by using controlled skin contact movements and force/torque measurements to estimate Young's modulus, providing precise skin property assessments despite external factors and unevenness.

JP2024158942APending Publication Date: 2024-11-08KAO CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023074594
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Existing methods for evaluating the physical properties of the skin surface layer, particularly the stratum corneum, are susceptible to external factors and skin unevenness, leading to inaccurate measurements, especially when liquid cosmetics are applied, and have low resolution in the depth direction.

Method used

A method involving a contact that moves with the skin surface without restraining it, applying changes such as shearing or twisting, and measuring reaction forces or torques to estimate the Young's modulus of the stratum corneum, using a skin physical property measuring device with a six-axis force sensor and controlled movements to minimize skin load and unevenness effects.

Benefits of technology

Enables accurate evaluation of skin surface layer properties, including Young's modulus, with reduced sensitivity to skin irregularities and the presence of liquid cosmetics, allowing for precise estimation of skin characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024158942000001_ABST
    Figure 2024158942000001_ABST
Patent Text Reader

Abstract

To provide a method for evaluating physical properties of a skin surface layer, which is easy to evaluate the physical properties of the skin surface layer and is hardly affected by unevenness of the skin surface.SOLUTION: A method for evaluating physical properties of a skin surface layer comprises: a step of bringing a contactor into contact with a skin surface so that the skin moves together with the contactor; a step of positioning the contactor at least in a vertical direction so that no load is applied to the skin in the vertical direction; and a change imparting step of moving the contactor in a direction along the skin surface or rotating the contactor around an axis perpendicular to the skin surface without restraining the skin around the contactor, to impart a change to the skin in accordance with the movement of the contactor. The method evaluates the physical properties of the surface layer of the skin based on reaction force or reaction torque from the skin generated in the change imparting step.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for evaluating the physical properties of the skin surface layer and a method for estimating Young's modulus of the stratum corneum of the skin. [Background technology]

[0002] It has been reported that the occurrence of irregularities such as fine wrinkles on human skin is related to the physical properties of the skin. For example, non-patent document 1 describes an apparatus that can be used to measure the physical properties of skin, which has a suction hole in the center of the contact surface of a contactor that is placed on the skin, and can suck in a part of the skin located in the center of the area in contact with the contactor through the suction hole and measure changes in the skin. Non-Patent Document 2 describes a method for visualizing the layer structure of the skin by applying ultrasonic vibrations to the skin, measuring the reflected ultrasonic waves, and converting them into acoustic impedance. Non-patent document 3 describes a device that has a rotationally driven rotating part and a peripheral area surrounding the rotating part on the contact surface of a contactor that is placed on the skin, and measures the displacement that occurs in the skin located in the gap between the rotating part and the peripheral area by rotating the rotating part while the peripheral area restrains the skin around the rotating part. [Prior art documents] [Non-patent literature]

[0003] [Non-Patent Document 1] Courage+Khazaka electronic GmbH, "Cutometer(R) Dual MPA 580", [online], [searched on April 28, 2023], Internet <https: / / www.courage-khazaka.de / en / scientific-products / efficacy-tests / skin?view=article&id=266&catid=16> [Non-Patent Document 2] Applied Physics, Vol. 87, No. 12 (2018), p. 932 [Non-Patent Document 3] Dia-Stron Limited., "DTM310 Dermal Torque Meter", [online], [searched on April 28, 2023], Internet<https: / / www.diastron.com / app / uploads / 2017 / 05 / Dia-Stron-DTM310-Brochure.pdf> Summary of the Invention [Problem to be solved by the invention]

[0004] The surface layer of human skin (including the stratum corneum) is susceptible to external factors such as dryness, ultraviolet rays, and atmospheric particles such as PM2.5 and yellow sand. However, it is also susceptible to the effects of skin care. Therefore, measuring the properties of the surface layer of skin and the physical properties that indicate them is useful for verifying the effectiveness of skin care products and for developing skin care agents. However, the device described in Non-Patent Document 1 has low resolution in the depth direction of the skin. Therefore, it is easily affected by the deeper parts of the skin, which is not preferable from the viewpoint of evaluating the physical properties of the skin surface layer. In addition, since the skin sucked through the suction holes is only a small part of the area of ​​the skin that the contactor contacts, if the skin has unevenness, the unevenness of the skin is likely to affect the measured physical properties, such as a difference in the physical properties when the convex parts are sucked and the physical properties when the concave parts are sucked. In the technique described in Non-Patent Document 2, a glass plate is placed on the skin, water is placed between the ultrasound application device and the glass plate, and ultrasound is applied to the skin. Therefore, when a liquid cosmetic is applied to the skin, it becomes difficult to appropriately evaluate the physical properties of the skin. The device described in Non-Patent Document 3 measures the physical properties of skin based on the shear stress of the skin located in the narrow annular gap between a rotating part and the surrounding area. Therefore, the resolution in the depth direction of the skin is low, and when a liquid cosmetic is applied to the skin, it is difficult to appropriately evaluate the physical properties of the skin.

[0005] The present invention relates to providing a method for evaluating the physical properties of the skin surface layer, which can solve the problems inherent to the above-mentioned conventional techniques. The present invention relates to a method for estimating Young's modulus that can efficiently estimate the Young's modulus of the skin surface layer. [Means for solving the problem]

[0006] The present invention (first method) relates to a method for evaluating the physical properties of the skin surface layer. The method preferably includes a step of bringing a contactor into contact with the skin surface so that the skin moves together with the contactor. The method preferably includes a positioning step of positioning the contactor at least in a vertical direction so that a load in the vertical direction is not applied to the skin. The method preferably includes a change imparting step of moving the contactor in a direction along the skin surface or rotating the contactor around an axis perpendicular to the skin surface without restraining the skin around the contactor to impart a change to the skin in accordance with the movement of the contactor. The method preferably includes evaluating the physical properties of the surface layer of the skin based on a reaction force or reaction torque from the skin generated in the change imparting step.

[0007] The present invention (second method) relates to a method for estimating Young's modulus of the stratum corneum of the skin. The method preferably includes a step of contacting a contactor with the skin surface so that the skin moves together with the contactor. The method preferably includes a positioning step of positioning the contactor so that no tangential or perpendicular load is applied to the skin. The method preferably includes a first step of moving the contactor in a direction along the skin surface or rotating it around an axis perpendicular to the skin surface without restraining the skin around the contactor, and measuring a reaction force or counter torque from the skin. The method preferably includes a second step of moving the contactor in a direction perpendicular to the skin before or after the first step, and measuring a reaction force from the skin. The method preferably includes estimating the Young's modulus of the stratum corneum based on the reaction force or counter torque from the skin in the first step and the reaction force from the skin in the second step. Effect of the Invention

[0008] According to the method for evaluating the physical properties of the skin surface layer of the present invention (first method), the physical properties of the skin surface layer can be easily evaluated and are not easily affected by the unevenness of the skin surface. Even when a coating material such as a liquid cosmetic is applied to the skin, the skin physical properties can be appropriately evaluated. According to the method for estimating Young's modulus of the stratum corneum of the present invention (second method), the Young's modulus of the surface layer of the skin can be efficiently estimated. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a perspective view showing an example of a skin property measuring device preferably used in carrying out the method of the present invention. [Diagram 2] FIG. 2 is a side view showing, with a part cut away, the reaction force measuring unit of the skin physical property measuring device shown in FIG. [Diagram 3] FIG. 3 is a block diagram showing an example of a control unit of the skin physical property measuring device. [Figure 4] FIG. 4 is an explanatory diagram of the first embodiment. [Diagram 5] FIG. 5 is an explanatory diagram of the second embodiment. [Figure 6] FIG. 6 is a schematic cross-sectional view showing a state in which a contact is brought into contact with the skin surface and lotion is applied around the contact. [Figure 7] FIG. 7 is a graph showing the compression reaction force, shear reaction force, and rotational reaction torque results measured on a human skin model. [Figure 8] FIG. 8 is a model diagram for analyzing the behavior of the skin when the contact is moved in a direction perpendicular to the skin. [Figure 9] FIG. 9 is a model diagram for analyzing the behavior of the skin when the contact is rotated around an axis perpendicular to the skin surface. [Figure 10] FIG. 10 is a model diagram for analyzing the behavior of the skin when the contact is moved in a direction along the skin surface. [Figure 11] 11(a) and (b) are graphs showing the calculation results of the Young's modulus of the stratum corneum and the Young's modulus of the lower layer for subjects. [Figure 12]12(a) and (b) are graphs showing the results of other calculations of the Young's modulus of the stratum corneum and the Young's modulus of the lower layer for subjects. [Figure 13] 13(a) and (b) are graphs showing further calculation results of the Young's modulus of the stratum corneum and the Young's modulus of the lower layer in subjects. [Figure 14] 14(a), 14(b) and 14(c) are graphs showing the results of a first test in which the reaction force value was measured when the contact was subjected to a reciprocating linear motion. [Figure 15] FIG. 15 is a graph showing the results of a second test in which the counter torque value was measured when the contact was subjected to a reciprocating rotational motion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, the embodiments (modes) of the present invention will be described in detail by way of example with reference to the drawings. However, the configurations, numerical values, process flows, functional elements, etc. described in the following embodiments (modes) are merely examples, and may be freely modified or changed, and are not intended to limit the technical scope of the present invention to the following description.

[0011] [Skin property measuring device] An example of a skin property measuring device preferably used in carrying out the method of the present invention is shown in Figure 1. To explain a skin property measuring device preferably used in carrying out the present invention, taking the skin property measuring device 1 shown in Figure 1 as an example, the skin property measuring device 1 includes a reaction force etc. measuring unit 2 having a contactor 21 to be brought into contact with the skin surface, a position adjustment mechanism 3 that supports the reaction force etc. measuring unit 2 and can adjust the orientation and position of the contactor 21 relative to the skin surface, and an electric displacement mechanism 4 that electrically displaces the contactor 21.

[0012] The reaction force measuring unit 2 has a rod shape extending in one direction and is provided with a contact 21 at its tip. As shown in FIG. 2, the contact 21 is preferably of a removable type that can be easily fixed to and removed from the contact support unit 22 using a fixing means such as a fixing screw 23. The contact 21 shown in FIG. 2 has a disk portion 21a and a rod-shaped portion 21b protruding from the center of one side of the disk portion 21a, and can be fixed to the contact support unit 22 by inserting the rod-shaped portion 21b into an attachment hole 22a provided in the contact support unit 22 and pressing the fixing screw 23 against the rod-shaped portion 21b from the side. It is preferable that the contact 21 is removable from the contact support unit 22 provided in the reaction force measuring unit 2 from the viewpoint of making the contact 21 easily replaceable. The contactor 21 in the present invention is not limited to a detachable type, and for example, a cylindrical contactor having one end that comes into contact with the skin may be provided instead of the contactor 21 and contactor support portion 22 shown in FIG.

[0013] The reaction force measuring unit 2 is provided with a six-axis force sensor 24 on the base end side of the contact 21. The base end side is the side farther from the skin surface. The six-axis force sensor 24 is a sensor capable of measuring the magnitude and direction of forces (Fx, Fy, Fz) and moments (Mx, My, Mz) in the X, Y, and Z axis directions, and detects physical quantities such as strain and displacement generated in the structure it holds by converting them into electrical signals in various ways. Methods for detecting strain and displacement include strain gauge type, piezoelectric type, optical type, and electrostatic capacitance type, and the like, with the use of a strain gauge being preferred. The principle and structure of the six-axis force sensor are described, for example, in the Journal of the Japan Society for Precision Engineering, Vol. 84, No. 4, 2018, pp. 303-306. In the skin property measuring device 1, one end of the six-axis force sensor 24 is connected to the contact support portion 22 so as to move and rotate integrally with the contact 21, and the other end is connected to the shaft 26 via a connecting member 25.

[0014] The position adjustment mechanism 3 includes a gear head or a free head 32 supported on an apparatus support 31 such as a tripod, and a manual XYZ stage 33. The electric displacement mechanism 4 includes a first linear actuator 41 and a second linear actuator . The first linear actuator 41 is fixed to the gear head or the free head 32 and has a first slider 41a that moves in the X direction. The second linear actuator 42 is fixed on the first slider 41a of the first linear actuator 41 and has a second slider 42a that moves in a direction perpendicular to the moving direction of the first slider 41a. The XYZ stage 33 is fixed on the second slider 42a and has a first stage 31a for finely adjusting the position of the contactor 21 in the Z direction, a second stage 31b for finely adjusting the position of the contactor 21 in the X direction perpendicular to the Z direction, and a third stage 31c for finely adjusting the position of the contactor 21 in the Z direction and in the Y direction perpendicular to the X direction. The first stage 31a, the second stage 31b, and the third stage 31c move in both forward and reverse directions by turning the knobs. The Z direction of the XYZ stage 33 , which is the moving direction of the first stage 31 a , coincides with the axial length direction of the reaction force measuring unit 2 and the Z axis direction of the six-axis force sensor 24 .

[0015] The skin physical property measuring device 1 further includes an electric rotation mechanism 5 that rotates the contactor 21, and a control and information processing unit 7. As shown in Fig. 3, the control and information processing unit 7 includes a displacement control unit 71 that controls the displacement of the contactor 21 by the first linear actuator 41 and the second linear actuator 42, a rotation control unit 72 that controls the rotation of the contactor 21 by the electric rotation mechanism 5, a first information processing unit 73 that records the output value of the six-axis force sensor 24 and performs predetermined analysis such as estimating Young's modulus, which will be described later, and the like. The electric rotating mechanism 5 is fixed to the third stage 31c of the XYZ stage 33, and moves integrally with the third stage 31c. The electric rotating mechanism 5 includes a support mechanism that rotatably supports the shaft 26, and a drive mechanism that can rotate the shaft 26 in both forward and reverse directions. The drive mechanism preferably includes an electric motor, such as a stepping motor or a servo motor, that can control the rotation angle and / or rotation angular velocity.

[0016] The control and information processing unit 7 can be configured by incorporating a predetermined program into a computer or the like including a central processing unit such as a CPU, and storage devices such as a ROM and a RAM. The control and information processing unit 7 preferably has a display unit such as a liquid crystal monitor, and an input unit such as a keyboard or a touch panel. The control and information processing unit 7 is electrically connected to the six-axis force sensor 24, the electric displacement mechanism 4, and the electric rotation mechanism 5. For the electrical connection, various connectors, I / O interfaces, etc. are used as necessary.

[0017] [First embodiment] Next, an embodiment of the method of the present invention using the skin physical property measuring device will be described. The first embodiment of the present invention is an embodiment of a method for estimating Young's modulus of the stratum corneum of the skin. [Pre-change process] The method of the first embodiment includes a contacting step of contacting the contactor 21 with the skin surface so that the skin moves together with the contactor, and a positioning step of positioning the contactor 21 so that no vertical load is applied to the skin.

[0018] As a method of contacting the contactor 21 so that the skin moves together with the contactor 21, as shown in Fig. 2, an adhesive tape 21c is attached to the skin-facing surface of the contactor 21, and in this state, the reaction force measuring unit 2 is advanced in the Z-axis direction to bring the contactor 21 into close contact with the skin via the adhesive tape 21c. To advance the reaction force measuring unit 2, a predetermined command is input to the control and information processing unit 7 to advance the second slider 42a of the second linear actuator 42 in the Z-axis direction. In the contact process, care is taken not to apply an excessive load to the skin.

[0019] The positioning step is a step of adjusting the vertical position of the contact 21 so that at least a load in the vertical direction is not applied to the skin. Specifically, the contact 21 is advanced or retreated in the Z-axis direction to adjust so that the load value in the Z-axis direction obtained from the six-axis force sensor 24 approaches zero. Here, "no load in the vertical direction is applied" does not require that the load in the vertical direction is completely zero. In the positioning step, positioning is performed so that the absolute value of the load in the vertical direction is 0.5 N or less, more preferably 0.3 N or less, and even more preferably 0.1 N or less.

[0020] The direction perpendicular to the skin is a direction perpendicular to the surface of the skin. The direction perpendicular to the skin is typically the same as the direction in which the reaction force measuring unit 2 advances or retreats (Z-axis direction), so the direction perpendicular to the skin is also called the Z-axis direction.

[0021] In the positioning step in the first embodiment, the vertical and tangential positions of the contactor 21 are adjusted so that not only a vertical load but also a tangential load is not applied to the skin. Specifically, the contactor 21 is moved in the tangential direction, which is a direction perpendicular to the Z-axis direction, and adjusted so that the tangential load value obtained from the six-axis force sensor 24 approaches zero. Here, the "tangential direction" typically refers to the X-axis direction, which is one direction perpendicular to the Z-axis direction, and the Y-axis direction, which is perpendicular to the one direction. It is preferable that the tangential load on the skin is not applied in either the X-axis direction or the Y-axis direction, which are perpendicular to each other, for example. Even in this case, the load does not need to be completely zero. Positioning is performed so that the absolute value of the tangential load is also 0.5 N or less, more preferably 0.3 N or less, and even more preferably 0.1 N or less. The alignment in the positioning step is preferably performed by the displacement control unit 71 controlling the displacement of the contact 21 by the first linear actuator 41 and the second linear actuator 42 based on the output value of the six-axis force sensor 24. In addition to this, the alignment may be performed by automatic adjustment by the displacement control unit 71, or the operator may perform the alignment by observing the output value of the six-axis force sensor 24.

[0022] [Change imparting step] The change imparting step is carried out after the contacting step and the positioning step. In the first embodiment of the method for estimating Young's modulus, the change imparting step includes a first step of moving the contact 21 in a direction along the skin surface (hereinafter also referred to as "shear") or rotating it around an axis perpendicular to the skin surface (hereinafter also referred to as "torsion") without restraining the skin around the contact, and measuring the reaction force or counter torque from the skin, and a second step of moving the contact 21 toward the skin in a direction perpendicular to the skin (hereinafter also referred to as "compression") and measuring the reaction force from the skin. Instead of this order, the step of moving the contact 21 toward the skin in a direction perpendicular to the skin and measuring the reaction force from the skin may be performed first, and then the step of moving the contact 21 in a direction along the skin surface or rotating it around an axis perpendicular to the skin surface without restraining the skin around the contact may be performed to measure the reaction force or counter torque from the skin. In other words, the second step may be performed before the first step.

[0023] [1st process] In the first step of the first embodiment, as shown in FIG. 4, the contactor 21 is rotated around an axis perpendicular to the skin surface without restraining the skin around the contactor 21. In this specification, "without restraining the skin around the contactor" means that the surroundings of the portion of the skin that the contactor directly abuts on are not prevented from changing in response to the movement of the contactor. By not restraining the skin around the contactor, for example, as shown in FIG. 6, it is possible to apply liquid 9 to the skin around the contactor 21 and examine the change in skin properties due to the presence or absence of application of a liquid cosmetic. In addition, when calculating Young's modulus, which will be described later, a theoretical solution for the case where an external force acts on a semi-infinite elastic body is applied, thereby enabling a highly accurate estimation of Young's modulus.

[0024] FIG. 4 shows a case where a contactor is fixed to the skin of the cheek of the face and the physical properties of the skin are measured, however, the skin to which the contactor is fixed can be selected from any part of the face, such as the skin of the forehead, between the eyebrows, nose, chin, etc. other than the cheek, the skin of the neck, arms, legs, abdomen, chest, back, buttocks, or the top or sole of the foot.

[0025] As shown in FIG. 4, when the contact 21 is rotated clockwise R1 as the positive direction and counterclockwise R2 as the negative direction, it is preferable to rotate the contact 21 in the positive direction and the negative direction at least once each, more preferably multiple times each, from the viewpoint of estimating and measuring physical quantities more objectively. When the position of zero rotation angle before rotating the contact 21 is set as the reference position a, the rotation angle from the reference position a is preferably 90 degrees or less, more preferably 60 degrees or less, in both the positive and negative directions. By suppressing the rotation angle within a predetermined value, it is possible to prevent adverse effects on the skin properties due to the measurement. On the other hand, the rotation angle from the reference position a is preferably 1 degree or more, more preferably 3 degrees or more, even more preferably 10 degrees or more, and more preferably 30 degrees or more, in both the positive and negative directions. By setting the rotation angle to a predetermined value or more, it is possible to expand the area where the skin is deformed, and it is possible to perform more accurate measurement. The contact 21 may rotate only once in the positive or negative direction, and even in this case, the rotation angle from the reference position a is preferably within the above-mentioned range.

[0026] It is preferable that the angular velocity of the contact 21 is constant. In this case, from the viewpoint of enabling not only to determine physical properties such as Young's modulus but also to identify three parameters in a three-element solid model of viscoelasticity from measurements at a plurality of velocities, it is preferable that the angular velocity is independently set to 0.01 deg / sec or more and 90 deg / sec or less in both the positive and negative directions, more preferably 0.05 deg / sec or more and 60 deg / sec or less, and even more preferably 0.1 deg / sec or more and 30 deg / sec or less. In particular, it is preferable that the angular velocity of the contact 21 is the same in both the positive and negative directions, from the viewpoint of estimating the isotropy (symmetry) of the skin physical properties and making the effect on the dynamic viscoelasticity the same.

[0027] The cross section of the contactor 21 is circular, and the radius of the contactor 21 must be a value that ensures an area sufficient for secure fixation to the skin and is sufficient to deform the skin in a relatively wide area. On the other hand, if the radius of the contactor is excessively large, the original shape of the skin is deformed too much, which not only causes initial strain on the skin but also narrows the deformable (measurable) area around the contactor. Furthermore, it is required that the contactor does not cause a sense of discomfort when it is brought into contact with the skin. From these viewpoints, the radius of the contactor 21 is preferably 1 mm or more and 30 mm or less, more preferably 5 mm or more and 25 mm or less, and even more preferably 10 mm or more and 20 mm or less. It is preferable that the center of rotation of the contactor 21 coincides with the center of the circle of the cross section in order to perform accurate measurements.

[0028] In the first step, instead of rotating the contactor 21 around an axis perpendicular to the skin surface (torsion, see FIG. 4) without restraining the skin around the contactor 21, the contactor 21 may be moved in a direction along the skin surface (shear, see FIG. 5) without restraining the skin around the contactor 21. The advantage of not restraining the skin around the contactor 21 is as described above.

[0029] The contact 21 may be moved in only one direction along a straight line, or may be reciprocated along a straight line. When moving the contact 21 in only one direction on a straight line, a decrease in accuracy can be suppressed by setting the moving distance to a certain value or more. Also, by setting the moving distance to a certain value or less, the burden on the skin can be reduced. From these viewpoints, the moving distance of the contact 21 is preferably 1 mm or more and 100 mm or less, more preferably 2 mm or more and 80 mm or less, and even more preferably 3 mm or more and 50 mm or less. In this case, the moving speed is preferably constant. In this case, from the viewpoint of enabling not only to determine physical properties such as Young's modulus but also to identify three parameters in a three-element solid model of viscoelasticity from measurements at a plurality of speeds, the moving speed is preferably 0.01 mm / s or more and 100 mm / s or less, more preferably 0.05 mm / s or more and 80 mm / s or less, and even more preferably 0.1 mm / s or more and 50 mm / s or less. When the contact 21 is reciprocated on a straight line, it is preferable from the viewpoint of more objective estimation and measurement of physical quantities to alternate between forward movement and backward movement at least once each, and more preferably multiple times each, as shown in Fig. 5. Furthermore, when the position before the contact 21 is moved is set as the reference position X, from the viewpoint of reducing the burden on the skin and obtaining high measurement accuracy, the distance from X to the end point X1 in one direction and the distance from X to the end point X2 in the other direction are each independently preferably 0.1 mm or more and 100 mm or less, more preferably 0.5 mm or more and 80 mm or less, and even more preferably 1 mm or more and 50 mm or less. In this case, the moving speed is preferably constant. In this case, from the viewpoint of being able to identify three parameters in a three-element solid model of viscoelasticity from measurements at a plurality of speeds as well as to obtain physical properties such as Young's modulus, the moving speed is preferably 0.01 mm / s or more and 100 mm / s or less in both the forward and backward movements, more preferably 0.05 mm / s or more and 80 mm / s or less, and even more preferably 0.1 mm / s or more and 50 mm / s or less. In particular, it is preferable that the distance from X to the end point X1 in one direction and the distance from X to the end point X2 in the other direction are the same, since this enables estimation of the isotropy (symmetry) of the skin physical properties. For the same reason, it is preferable that the speed of the forward and backward movements is the same.

[0030] During the first step, the output value from the six-axis force sensor 24 is recorded, and preferably the control and information processing unit 7 calculates the reaction torque value or reaction force from the output value.

[0031] [Second process] In the second step, as shown in FIG. 4, the contactor 21 is moved linearly in a direction perpendicular to the skin so that the contactor 21 approaches the skin, and the skin is pressed by the contactor 21, and the reaction force at that time is measured. The amount of depression of the contactor 21, based on the point at which the contactor 21 comes into contact with the skin, is preferably 0.1 mm or more and 30 mm or less, more preferably 0.5 mm or more and 15 mm or less, and even more preferably 1 mm or more and 10 mm or less, from the viewpoint of reducing the burden on the skin and obtaining high measurement accuracy. In this case, it is preferable that the moving speed of the contact 21 is constant. In this case, from the viewpoint of making it possible to not only obtain physical properties such as Young's modulus but also to identify three parameters in a three-element solid model of viscoelasticity from measurements at a plurality of speeds, the moving speed is preferably 0.01 mm / s or more and 100 mm / s or less, more preferably 0.05 mm / s or more and 80 mm / s or less, and even more preferably 0.1 mm / s or more and 50 mm / s or less.

[0032] During the second step, the output value from the six-axis force sensor 24 is recorded, and preferably the control and information processing unit 7 calculates the reaction force from the output value.

[0033] [Calculation of Young's Modulus] The Young's modulus of the stratum corneum is calculated based on the reaction force due to shear or the counter torque due to torsion in the first step and the reaction force due to compression in the second step. This calculation of the Young's modulus may be performed after the first and second steps are completely completed, or may be performed at a stage when the necessary information is obtained even if either or both of the first and second steps are not completely completed. In either case, a calculation based on the reaction force due to compression (calculation 1) is performed first, and then a calculation based on the reaction force due to shear or the counter torque due to torsion (calculation 2) is performed. The calculations should not be performed in the order of calculation 2 and calculation 1.

[0034] Using a gel and a wrap film placed on the gel as a model of human skin, the reaction force due to compression, the reaction force due to shear, and the reaction torque due to torsion were measured in that order. The results are shown in FIG. 7. The results shown in the figure are from a model of human skin made by placing a wrap film on the top surface of a rectangular parallelepiped gel with a length of 150 mm, a width of 100 mm, and a thickness of 20 mm so as to cover the entire top surface without wrinkles. The gel is a model of the tissue located below the stratum corneum in human skin (hereinafter, also referred to as the "lower layer" for convenience), and the wrap film is a model of the stratum corneum. The Young's modulus of the gel used is 0.02 MPa. Two types of wrap films with different thicknesses (6 μm and 25 μm) were used. The Young's modulus of the wrap film with a thickness of 6 μm is 90 MPa, and the Young's modulus of the wrap film with a thickness of 25 μm is 50 MPa. The compression amount was 3 mm, the compression speed was 1 mm / s, the shear travel distance was 3 mm, the compression speed was 1 mm / s, the torsion angle was 3 degrees in both the positive and negative directions, the angular velocity was 1 degree / sec in both the positive and negative directions, and the radius of the cross section of the contact was 8 mm.

[0035] As is clear from the results shown in Fig. 7, the reaction force due to compression is less affected by the presence or absence of a wrap film and the Young's modulus of the wrap film than the reaction force due to shear and the counter torque due to torsion.Therefore, it was found that the Young's modulus of the gel, in other words, the Young's modulus of the tissue (lower layer) located below the stratum corneum can be measured by measuring the reaction force due to compression.Therefore, in the present invention, the reaction force due to compression is first measured, and the Young's modulus of the tissue (lower layer) located below the stratum corneum is estimated based on the result, and then the Young's modulus of the stratum corneum is estimated based on the reaction force due to shear or the counter torque due to torsion and the Young's modulus of the tissue (lower layer) located below the stratum corneum.

[0036] In the specific calculation, the Young's modulus of the stratum corneum and the Young's modulus of the lower layer are set to the same initial value, and the Poisson's ratio and thickness of each layer are given, and the Young's modulus of the lower layer is determined based on the reaction force caused by compression. In detail, since the stratum corneum is thin, it hardly affects the stiffness, but the Young's modulus of the stratum corneum is temporarily fixed at about 5 MPa, and the Young's modulus of other layers is changed to search for a value that is the same as the measured reaction force, and the Young's modulus of other layers is determined. That is, based on the given initial value, the reaction force caused by compression is calculated according to the following theory. The calculated reaction force is compared with the actually measured reaction force, and if the difference between the two exceeds a threshold value, the Young's modulus of the lower layer is changed and the reaction force is calculated again, and compared with the actually measured reaction force. In this case, if the calculated value is greater than the measured value, the Young's modulus of the lower layer is reduced and recalculated. Conversely, if the calculated value is less than the measured value, the Young's modulus of the lower layer is increased and recalculated. This operation is repeated, and when the difference between the two is less than the threshold value, the value at that time is determined as the Young's modulus of the lower layer. After the Young's modulus of the lower layer is determined in this way, the Young's modulus of the stratum corneum is calculated based on the Young's modulus of the lower layer and the reaction force due to shear or the counter torque due to torsion. In detail, an initial value is given to the Young's modulus of the stratum corneum, and a numerical value that is the same as the measured reaction force or counter torque is searched for to determine the Young's modulus of the stratum corneum. The calculated reaction force or counter torque is compared with the actually measured reaction force or counter torque, and if the difference between them exceeds a threshold value, the Young's modulus of the stratum corneum is changed and the reaction force or counter torque is calculated again, and compared with the actually measured reaction force or counter torque. In this case, if the calculated value is greater than the measured value, the Young's modulus of the stratum corneum is reduced and recalculated. Conversely, if the calculated value is less than the measured value, the Young's modulus of the stratum corneum is increased and recalculated. This operation is repeated, and when the difference between them becomes equal to or less than a threshold value, the value at that time is determined as the Young's modulus of the stratum corneum.

[0037] A specific method for calculating the Young's modulus of the lower layer will now be explained. As shown in Figure 8, a semi-infinite body is divided into three layers. From the surface, these are the stratum corneum, the epidermis, the lower layers such as the dermis and subcutaneous tissue (layers below the epidermis, etc.), and bone. Since bone is hard and does not deform, it is possible to set a skin model with an apparent finite thickness. In other words, the skin is defined as having a two-layer structure. The following equations hold for the three layers.

[0038]

number

[0039] These are displayed in a matrix, and the coordinates of the surface and bottom surfaces are assigned in the order of the stratum corneum, lower layers such as the epidermis, and bone.

[0040]

number

[0041]

number

[0042] According to the boundary conditions, in order for the displacement and stress to become zero as z goes to infinity, C3 = D3 = 0 must be true.

[0043]

number

[0044] The deformation (r-direction and z-direction deformation) and stress (normal stress and shear stress) are the same at the bottom surface of the lower layer (2nd layer) such as the epidermis and the surface of the bone (3rd layer), so

[0045]

number

[0046] If the respective matrices are S and T, the constants A2, B2, C2, and D2 for the lower layers such as the epidermis can be calculated as follows.

[0047]

number

[0048] Substituting the above equation with U as the matrix of the second layer surface equation, we get

[0049]

number

[0050] Since the deformation and stress are the same at the bottom of the stratum corneum (first layer) and the surface of the lower layer (second layer) such as the epidermis,

[0051]

number

[0052] The constants A1, B1, C1, and D1 are calculated as follows:

[0053]

number

[0054] Substituting the above equation with W as the matrix of the surface equation of the stratum corneum (first layer), we get:

[0055]

number

[0056] From here, we will calculate the deformation and stress after Hankel transformation as a function of z, starting from the bones. The reason for adopting the Hankel transformation is as follows. The thickness of the stratum corneum is about 0.01 mm, which is very thin compared to other layers in human skin. Therefore, in order to correctly evaluate the stratum corneum, it is necessary to model it using a high-order function in the thickness direction of the skin. The finite element method is a promising method for this purpose, but in the finite element method, if the surface shape of the skin or the thickness of the stratum corneum differs, modeling must be performed each time, which is very cumbersome. In addition, since a normal finite element model uses a low-order function, it is difficult to say that it is suitable for evaluating the stratum corneum. In the theoretical analysis approach, it is necessary to solve simultaneous partial differential equations using harmonic functions or biharmonic functions, and the Hankel transform is a method for solving the equations. When using the Hankel transform, the results can be obtained simply by inputting the values ​​of the stratum corneum thickness and Young's modulus, so it has the advantage of being easy to make into a tool. For these reasons, the Hankel transform is adopted in the present invention.

[0057]

number

[0058]

number

[0059] With the above steps, the displacement and stress after Hankel transformation can be obtained for all layers, including bones, sublayers such as the epidermis, and the stratum corneum. By performing an inverse Hankel transformation on the displacement and stress of the skin (sublayers such as the stratum corneum and epidermis), analytical solutions for these can be obtained.

[0060]

number

[0061] The Young's modulus of the stratum corneum is determined using the Young's modulus of the lower layer thus obtained and the counter torque due to torsion. In detail, based on the initial value of the Young's modulus of the stratum corneum, the counter torque due to torsion is calculated according to the following theory. The calculated counter torque is compared with the actually measured counter torque, and if the difference between the two exceeds a threshold value, the Young's modulus of the stratum corneum is changed and the counter torque is calculated again, and compared with the actually measured counter torque. This operation is repeated, and when the difference between the two becomes equal to or less than the threshold value, the value at that time is determined to be the Young's modulus of the stratum corneum.

[0062] As in Fig. 8, the semi-infinite body is divided into three layers as shown in Fig. 9. From the surface, these are the stratum corneum, the epidermis, the lower layers such as the dermis and subcutaneous tissue (layers below the epidermis, etc.), and bone. Since bone is hard and does not deform, it is possible to set a skin model with an apparent finite thickness. In other words, the skin is defined as having a two-layer structure.

[0063]

number

[0064] From the boundary conditions, when z → ∞, u θ →0, τ zθ →To be 0, A3 must be 0.

[0065]

number

[0066] If the respective matrices are S and T, A2 and B2 are as follows.

[0067]

number

[0068] Let U be the matrix of the second layer surface equation, and substitute the above equation:

[0069]

number

[0070]

number

[0071] If the matrix in the middle of the above equation is V, A1 and B1 become as follows.

[0072]

number

[0073] Substituting the above equation with W as the matrix of the surface equation of the first layer, we get

[0074]

number

[0075] From here, we will calculate the deformation (deformation in the θ direction) and stress (shear stress) after the Hankel transformation as a function of z, starting from the bones.

[0076]

number

[0077] In this way, the displacement and stress after Hankel transformation are obtained for all layers, including bone, lower layers such as the epidermis, and the stratum corneum. Then, by performing an inverse Hankel transformation on the displacement and stress, analytical solutions for these are obtained.

[0078]

number

[0079] The above describes a method for determining the Young's modulus of the stratum corneum using the Young's modulus of the lower layer and the reaction torque due to torsion. Below, a method for determining the Young's modulus of the stratum corneum using the Young's modulus of the lower layer and the reaction force due to shear will be described.

[0080] As in Figure 8, the semi-infinite body is divided into three layers as shown in Figure 10. From the surface, these are the stratum corneum, the epidermis, the lower layers such as the dermis and subcutaneous tissue (layers below the epidermis, etc.), and bone. Since bone is hard and does not deform, it is possible to set a skin model with an apparent finite thickness. In other words, the skin is defined as having a two-layer structure. The following equations hold for the three layers.

[0081]

number

[0082]

number

[0083]

number

[0084]

number

[0085]

number

[0086]

number

[0087]

number

[0088]

number

[0089] According to the boundary conditions, in order for the displacement and stress to be zero when z → infinity, A3 = B3 = E3 = 0 must be true. Under this condition, when z = 0,

[0090]

number

[0091] The deformation and stress are the same at the bottom surface of the lower layer (2nd layer) such as the epidermis and at the surface of the bone layer (3rd layer),

[0092]

number

[0093]

number

[0094] If the matrices of the above equation are S1 and T1, the constants A2, B2, C2, D2, E2, and F2 for layers such as the epidermis can be calculated as follows.

[0095]

number

[0096] Substituting the above equation with U1 as the matrix of the second layer surface equation, we get

[0097]

number

[0098] Let V1 be the matrix of the bottom surface of the stratum corneum (first layer). Since the deformation and stress at the bottom surface of the stratum corneum and the surface of layers such as the epidermis are the same,

[0099]

number

[0100]

number

[0101] If we substitute the above results into the matrix W of the equation for the surface of the stratum corneum (first layer), we get

[0102]

number

[0103]

number

[0104]

number

[0105] From here, we will calculate the deformation and stress after the Hankel transformation as a function of z, starting from the bones.

[0106]

number

[0107]

number

[0108]

number

[0109] With the above steps, the displacement and stress after Hankel transformation can be obtained for all layers, including bones, sublayers such as the epidermis, and the stratum corneum. By performing an inverse Hankel transformation on the displacement and stress of the skin (layers such as the stratum corneum and epidermis), analytical solutions for these can be obtained.

[0110]

number

[0111]

number

[0112] The displacement and stress can be obtained by performing the following calculations for the stratum corneum (i=1) and the lower layers such as the epidermis (i=2).

[0113]

number

[0114]

number

[0115] Now, all the displacements and stresses can be calculated.

[0116] Next, the results of calculating the Young's modulus of the stratum corneum and the lower layer on the inside of the forearm for the subjects shown in Table 1 are shown in Figures 11(a) and (b). In the calculations, the thicknesses of the stratum corneum and the lower layer were set to the values ​​shown in the table, taking into account the age and sex of the subjects. The Poisson's ratio was also set to 0.4. The measurement was carried out by first measuring the reaction force of compression by the contact 21 to obtain the Young's modulus of the subcutaneous tissue, and then applying a torsion as a change to measure the reaction torque, or applying a shear force to measure the reaction force. The contact 21 had a circular cross section with a radius of 16 mm. The absolute value of the load applied to the contact 21 in the vertical direction during the positioning step was set to 0.05 N or less. The amount of compression by the contact 21 was set to 3 mm, and the pressing speed was set to 1 mm / s (constant speed). When a twist was applied as a change, the angle was 10 degrees in both the positive and negative directions, and the angular velocity was 1 degree / sec (constant speed) in both the positive and negative directions. When applying shear force as a change, the movement distance of the contact 21 when it is reciprocated in a straight line from the starting point X to the end point X1 in one direction and to the end point X2 in the other direction is 5 mm, and the speed is 1 mm / s (constant speed) for both the forward movement and the return movement. As is clear from the results shown in Figures 11(a) and (b), the Young's modulus of both the stratum corneum and the dermis tended to decrease as the subjects got older, suggesting that skin elasticity decreases with age. Since the Young's modulus of the dermis is said to be about 0.05 MPa, the result shown in FIG. 11(a) is deemed to be reasonable. As shown in Fig. 11(b), the Young's modulus of the stratum corneum based on the reaction force due to shear was not determined for two subjects, which is believed to be due to the fact that the thickness of the lower layer was set to a large value.

[0117] [Table 1]

[0118] Since the muscles on the inner side of the forearm are hard, if we consider the muscles as bones, the thickness of the lower layer will be smaller than the value used in the above calculation. Therefore, we set the thickness of the lower layer to 5 mm and recalculated. The results are shown in Figure 12 (a) and (b). Among the subjects, those who were judged to have dry skin tended to have a higher Young's modulus of the stratum corneum.In addition, subject Suga is a man in his 60s, and has a habit of applying Vaseline to his arms, which is thought to have caused his stratum corneum's Young's modulus to be lower.

[0119] 13(a) and (b) show the results of recalculation with the lower layer thickness set to 3 mm. The tendency of the calculation results is similar to that when the lower layer thickness was set to 5 mm, but the Young's modulus of the stratum corneum was generally higher.

[0120] Next, an evaluation method according to a second embodiment of the present invention using a skin physical property measuring device will be described. In the second embodiment, a contact step is performed in the same manner as in the first embodiment, in which the contactor 21 is brought into contact with the skin surface so that the skin moves together with the contactor. Also, in the same manner as in the first step in the first embodiment, a positioning step is performed in which the position of the contactor 21 is adjusted so that a load is not applied to the skin in a direction perpendicular to the skin, preferably in both the tangential and perpendicular directions. Then, in the change imparting process, while maintaining the skin free of loads in a direction perpendicular to the skin, preferably in both the tangential and perpendicular directions, the contactor 21 is moved in a direction along the skin surface (shear) or rotated around an axis perpendicular to the skin surface (twist), imparting a change to the skin in accordance with the movement of the contactor. The physical properties of the surface layer of the skin are then evaluated based on the reaction force due to shear or the reaction torque due to torsion obtained in the change imparting step. The evaluation of the physical properties of the surface layer of the skin may be performed after the change imparting step is completely completed, or may be performed at a stage when the necessary information has been obtained even if the change imparting step is not completely completed.

[0121] Next, the evaluation method of the second embodiment will be explained by showing more specific examples (first test and second test). [First test] Fig. 14(a) is a graph showing the change in stress in the longitudinal direction (X-axis direction) when a first test was conducted on two subjects, a man in his 30s and a man in his 50s, in which the contactor 21 was attached to the inside of the forearm with double-sided tape (not shown) as shown in Fig. 5, the loads in the normal and tangential directions to the skin surface were adjusted to zero, and then the contactor 21 was made to perform a reciprocating linear motion multiple times in the longitudinal direction of the forearm. The preferable conditions for the reciprocating linear motion are the same as those in the first embodiment, so a description thereof will be omitted here.

[0122] The first test was conducted before and immediately after adding water to the forearm, and at multiple points after adding water (immediately after adding water, 5 minutes after adding water, 10 minutes after adding water, and 20 minutes after adding water), all in an environment with a temperature of 25°C and a relative humidity of 50%. Water was added after the contactor was fixed to the skin before application. As shown in Figure 6, water, which is liquid 9, was added to a sufficient area around the contactor 21. No water was applied to the skin in the area facing and in contact with the contactor 21. FIG. 14(b) is a graph showing the first peak top value extracted from the results shown in FIG. 14(a), and FIG. 14(c) is a graph showing the moisture content of the skin at each measurement stage. As shown in Figure 14(b), the reaction force value at the first peak top dropped significantly immediately after water was added (labeled "water added" in the graph) compared to before water was added, and then increased over time as the water content decreased. Furthermore, as is clear from the comparison between the two subjects, the male subject in his 30s had a higher reaction force value than the male subject in his 50s. The measurement results of the first test showed a known phenomenon of softening of the stratum corneum by the addition of water as a numerical value (a decrease in the peak top value). Specifically, it was observed that the skin of a man in his 30s was firm and had few wrinkles. Furthermore, the measurement results showed that the reaction force from the skin was large, and that the change in flexibility when water was added was also large. From the above, it can be inferred that the skin of men in their 30s is in a state where it is more susceptible to the moisturizing effects of skin care products. In contrast, the skin of a man in his 50s was loose and had many wrinkles. According to the measurement results, the reaction force from the skin was small, and the change in flexibility when water was added was also small. To summarize the above, it can be said that the first test demonstrates that it is possible to accurately evaluate the skin characteristics of each age group.

[0123] [Second test] As shown in Fig. 4, the contactor was attached to the approximate center of a human cheek with double-sided tape, and the load in the normal and tangential directions relative to the skin surface was adjusted to zero. The contactor was then rotated back and forth several times, with one rotation being a clockwise rotation R1 and one counterclockwise rotation R2. The preferred conditions for the rotational movement are the same as those in the first embodiment, so a description thereof will be omitted here.

[0124] The second test was conducted on two subjects, a man in his 30s and a man in his 60s. The second test was conducted before and after application of lotion, both in an environment with a temperature of 20°C and a relative humidity of 40%. As shown in FIG. 6, lotion, which is liquid 9, was applied to a sufficient area around the contact 21. Lotion was not applied to the skin facing the contact 21. The rotation speed of the contact was 10 degrees / second. The rotation angle of the contact was initially ±5 degrees, and after rotating back and forth several times, the rotation angle was increased to ±10 degrees and ±15 degrees. The measurement results are shown in FIG. 15. As is clear from these results, the male subject in his 30s had a lower counter torque value, regardless of whether he applied lotion or not. In addition, the counter torque after applying lotion was lower than the counter torque before application for both subjects. The degree of decrease was about 40% for the male subject in his 30s, while it was about 50% for the male subject in his 60s, indicating that the degree of decrease in the male subject in his 30s was smaller than the counter torque.

[0125] As is clear from the results shown in Figures 14 and 15, according to the second embodiment of the method of the present invention, the physical properties of the skin surface layer can be easily evaluated and are less susceptible to the effects of unevenness on the skin surface. Furthermore, according to this embodiment, the skin properties can be appropriately evaluated even when a coating material such as a liquid cosmetic is applied to the skin.

[0126] The first and second embodiments of the present invention are useful for evaluating skin softness, skin firmness, skin plumpness and skin suppleness, thereby enabling the determination of dermatological signs such as chronological, solar, hormonal and actinic skin aging.

[0127] Although the present invention has been described above based on its preferred embodiment, the present invention is not limited to the above embodiment. For example, in the reaction force measuring unit 2 shown in Fig. 2, the adhesive tape 21c is attached to the skin-facing surface of the contactor 21, and the adhesive tape 21c is brought into close contact with the skin. However, instead of this, the contactor 21 may have a hollow structure, and a plurality of through holes may be provided on the skin-facing surface of the contactor 21, and the skin may be sucked through the through holes to bring the contactor 21 into close contact with the skin. [Explanation of symbols]

[0128] 1. Skin property measuring device 2. Reaction force measurement section 3 Position adjustment mechanism 4. Electric displacement mechanism 5 Electric rotation mechanism 7 Information Processing Section 21 Contact 21c Adhesive Tape 24 Six-axis force sensor

Claims

1. A method for evaluating a physical property of a skin surface layer, comprising: contacting a contactor with a skin surface such that the skin moves with the contactor; a positioning step of positioning the contact in at least a vertical direction so that a load in the vertical direction is not applied to the skin; a change imparting step of imparting a change to the skin in accordance with the movement of the contactor by moving the contactor in a direction along the skin surface or rotating the contactor around an axis perpendicular to the skin surface without restraining the skin around the contactor; A method for evaluating physical properties of the skin surface layer, comprising evaluating the physical properties of the skin surface layer based on a reaction force or reaction torque from the skin generated in the change imparting step.

2. A method for estimating the Young's modulus of a stratum corneum of skin, comprising: contacting a contactor with a skin surface such that the skin moves with the contactor; a positioning step of positioning the contact so that no load is applied to the skin in a tangential direction or a perpendicular direction; A first step of moving the contactor in a direction along the skin surface or rotating the contactor around an axis perpendicular to the skin surface without restraining the skin around the contactor, and measuring a reaction force or reaction torque from the skin; A second step of moving the contactor in a direction perpendicular to the skin and measuring a reaction force from the skin before or after the first step, A method for estimating the Young's modulus of the stratum corneum of the skin, comprising estimating the Young's modulus of the stratum corneum of the skin based on a reaction force or reaction torque from the skin in a first step and a reaction force from the skin in a second step.

3. setting the Young's modulus of the stratum corneum and the Young's modulus of a tissue located below the stratum corneum to the same initial value, and calculating the Young's modulus of the tissue located below the stratum corneum based on the reaction force from the skin in the second step; The method according to claim 2 , further comprising calculating the Young's modulus of the stratum corneum from the reaction force or reaction torque from the skin in the first step and the Young's modulus of tissue located below the stratum corneum.