Optical member

Non-heat processing with ultra-short pulse lasers is used to mark eyeglass lenses by selectively removing the outermost layer of the anti-reflection film, addressing the issues of peeling and damage in conventional methods, thereby maintaining lens quality.

JP2024160355AInactive Publication Date: 2024-11-13HOYA LENS THAILAND LTD

Patent Information

Application Number
JP2024135536
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-13
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional laser marking methods for eyeglass lenses risk peeling and damaging the thin film layers, leading to potential deterioration of lens quality.

Method used

Non-heat processing using an ultra-short pulse laser to partially remove the low refractive index layer of a multilayer anti-reflection film, exposing the high refractive index layer, while maintaining the integrity of the underlying layers.

Benefits of technology

This method allows for marking decorative patterns on eyeglass lenses without deteriorating the lens quality by minimizing thermal damage and peeling, ensuring the structural integrity of the film layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024160355000001_ABST
    Figure 2024160355000001_ABST
Patent Text Reader

Abstract

To provide a technique by which an optical member is marked without degrading the quality of the optical member.SOLUTION: An antireflection film is formed to cover an optical surface of an optical base material, and has a multilayer structure in which low and high refractive index layers are laminated. An optical member is produced through a removing step (S108, S113) of exposing the high refractive index layer by partially removing the low refractive index layer, which is the outermost layer of the multilayer structure, by performing non-heating processing of the antireflection film through irradiation with an ultrashort pulse laser.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an optical member. [Background technology]

[0002] Some eyeglass lenses are configured such that the optical surface of a lens substrate is coated with a thin film such as a hard coat film, an anti-reflection film, etc. In recent years, it has been proposed to perform marking on eyeglass lenses by partially removing a part of the thin film by irradiating the thin film with a laser (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Special Publication No. 2019-523447 Summary of the Invention [Problem to be solved by the invention]

[0004] In conventional marking by laser irradiation, there is a risk of the thin film peeling off due to partial removal of a part of the thin film, and there is also a risk of damaging the layer below the removed layer. Therefore, there is a concern that the quality will be reduced if this method is applied to eyeglass lens products.

[0005] An object of the present disclosure is to provide a technique that allows marking of an optical member without degrading the quality of the optical member. [Means for solving the problem]

[0006] The first aspect of the present invention is A removal step of performing non-heating processing by irradiating an ultrashort pulse laser on an antireflection film having a multilayer structure in which a low refractive index layer and a high refractive index layer are laminated, the antireflection film being formed so as to cover the optical surface of an optical substrate, to partially remove the low refractive index layer, which is the outermost layer of the multilayer structure, to expose the high refractive index layer. The method for producing an optical member includes the steps of:

[0007] A second aspect of the present invention is The ultrashort pulse laser has a pulse width of 0.1 picoseconds or more and less than 100 picoseconds. A method for producing the optical member according to the first aspect.

[0008] A third aspect of the present invention is The anti-reflection film is irradiated with the ultrashort pulse laser in a defocused setting. A method for producing the optical member according to the first or second subject matter.

[0009] A fourth aspect of the present invention is the outermost layer is a SiO2 layer as the low refractive index layer, The layer exposed by removing the low refractive index layer is a ZrO2 layer as the high refractive index layer. A method for producing the optical member according to any one of the first to third aspects.

[0010] A fifth aspect of the present invention is The optical member is a spectacle lens. A method for producing the optical member according to any one of the first to fourth aspects.

[0011] A sixth aspect of the present invention is a method for producing a composition comprising the steps of: In the removing step, a decorative pattern of the optical member is formed by partially removing the low refractive index layer that is the outermost layer. A method for producing the optical member according to any one of the first to fifth aspects.

[0012] A seventh aspect of the present invention is a method for producing a composition comprising the steps of: an optical substrate having an optical surface; an anti-reflection film covering the optical surface of the optical substrate; The anti-reflection film has a multi-layer structure in which a low refractive index layer and a high refractive index layer are laminated, and the low refractive index layer, which is the outermost layer of the multi-layer structure, is partially removed to expose the high refractive index layer. It is an optical component.

[0013] An eighth aspect of the present invention is a method for producing a composition comprising the steps of: The high refractive index layer exposed by removing the low refractive index layer has a ratio t1 / t2 of a thickness t1 of the removed portion of the low refractive index layer to a thickness t2 of the non-removed portion of the outermost layer, which is in the range of 0.90 to 1.00. The optical member according to claim 7.

[0014] A ninth aspect of the present invention is a method for producing a composition comprising the steps of: the outermost layer is a SiO2 layer as the low refractive index layer, The layer exposed by removing the low refractive index layer is a ZrO2 layer as the high refractive index layer. The optical member according to the seventh or eighth aspect of the present invention.

[0015] A tenth aspect of the present invention is a method for producing a composition comprising the steps of: The optical member is a spectacle lens. The optical member according to any one of the seventh to ninth aspects.

[0016] An eleventh aspect of the present invention is a method for producing a composition comprising the steps of: The removed portion of the outermost low refractive index layer constitutes a decorative pattern of the optical member. The optical member according to any one of the seventh to tenth aspects. Effect of the Invention

[0017] According to the present invention, marking can be performed on an optical member without causing a deterioration in the quality of the optical member. [Brief description of the drawings]

[0018] [Figure 1] 1 is a plan view showing an example of processing of a spectacle lens according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a flow chart showing an example of a procedure for a method of manufacturing a spectacle lens according to an embodiment of the present invention. [Diagram 3] 1 is a side cross-sectional view showing an example of a laminated structure of thin films in a spectacle lens according to an embodiment of the present invention. [Figure 4] 1 is an explanatory diagram showing an example of the schematic configuration of a laser processing device used in a method for manufacturing a spectacle lens according to an embodiment of the present invention; [Diagram 5] 1 is an explanatory diagram showing an example of the configuration of a main part of a spectacle lens according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0020] In this embodiment, the following description will be given taking as an example a case where the optical member is a spectacle lens.

[0021] A spectacle lens has an object-side surface and an eyeball-side surface as optical surfaces. The "object-side surface" is the surface that is located on the object side when a wearer wears spectacles equipped with the spectacle lens. The "eyeball-side surface" is the opposite, that is, the surface that is located on the eyeball side when a wearer wears spectacles equipped with the spectacle lens. The object-side surface is generally a convex surface and the eyeball-side surface is generally a concave surface, that is, a spectacle lens is a meniscus lens.

[0022] FIG. 1 is a plan view showing an example of processing of a spectacle lens according to the present embodiment. In this embodiment, a spectacle lens 1 having a circular shape in a planar view (e.g., outer diameter φ60 to 80 mm) is subjected to a contouring process (frame cutting process) in which the lens outer shape is cut to match the frame shape 2 of the spectacle frame worn by the wearer, and a decorative pattern 3 representing a logo, house mark, etc. is marked on the optical surface so that it is positioned within the lens area after frame cutting.

[0023] The marking of the decorative pattern 3 can be performed, for example, by using a laser irradiation process that can precisely control the irradiation position based on digital data, but it is undesirable that the marking may cause a deterioration in lens quality. Therefore, in this embodiment, the marking of the decorative pattern 3 is performed by the processing procedure described below.

[0024] (1) Manufacturing method of eyeglass lenses Here, the processing procedure of the eyeglass lens including the marking of the decorative pattern, that is, the procedure of the method for manufacturing the eyeglass lens according to this embodiment will be specifically described. FIG. 2 is a flow diagram showing an example of the procedure of the method for manufacturing a spectacle lens according to this embodiment.

[0025] In manufacturing eyeglass lenses, first, a lens substrate, which is an optical base material, is prepared, and the lens substrate is polished according to the prescription information of the eyeglass wearer, and dyed as necessary (step 101, hereinafter step is abbreviated as "S"). As the lens substrate, for example, a resin material having a refractive index (nD) of about 1.50 to 1.74 is used. Specifically, examples of the resin material include allyl diglycol carbonate, urethane resin, polycarbonate, thiourethane resin, and episulfide resin. However, instead of these resin materials, the lens substrate may be made of other resin materials that can obtain a desired refractive index, or may be made of inorganic glass. In addition, the lens substrate has optical surfaces for forming a predetermined lens shape on both the object side surface and the eyeball side surface. The predetermined lens shape may be any of a single-focus lens, a multifocal lens, a progressive power lens, etc., and in any case, each optical surface is made of a curved surface specified based on the prescription information of the eyeglass wearer. The optical surface is formed, for example, by polishing, but may be a cast (molded) product that does not require polishing. The polishing and dyeing of the lens substrate may be performed using known techniques, and detailed description thereof will be omitted here.

[0026] Thereafter, a hard coat film (HC film) is formed on at least one optical surface, and preferably on both optical surfaces, of the lens substrate (S102). The HC film is, for example, made of a curable material containing a silicon compound, and is a film formed to a thickness of about 3 μm to 4 μm. The refractive index (nD) of the HC film is close to the refractive index of the material of the lens substrate described above, for example, about 1.49 to 1.74, and the film configuration is selected according to the material of the lens substrate. By coating with such an HC film, it is possible to improve the durability of the eyeglass lens. The HC film may be formed, for example, by a dipping method using a solution in which a hardening material containing a silicon compound is dissolved.

[0027] After the HC film is formed, an anti-reflection film (AR film) is subsequently formed so as to overlap the HC film (S103). The AR film has a multi-layer structure in which films with different refractive indices are laminated, and prevents light reflection by interference. Specifically, the AR film has a multi-layer structure in which a low refractive index layer and a high refractive index layer are laminated. The low refractive index layer is made of silicon dioxide (SiO2) with a refractive index of about 1.43 to 1.47. The high refractive index layer is made of a material having a higher refractive index than the low refractive index layer, and is made of, for example, zirconium oxide (ZrO2), tin oxide (SnO2), niobium oxide (Nb2O5), tantalum oxide (Ta2O5), titanium oxide (TiO2), yttrium oxide (Y2O3), aluminum oxide (Al2O3), or a mixture thereof (for example, indium tin oxide (ITO)). However, the outermost layer of the AR film of the multi-layer structure is always configured to be a low refractive index layer (for example, a SiO2 layer). By covering with such an AR film, the visibility of an image passing through the eyeglass lens can be improved. The AR film may be formed by, for example, ion-assisted deposition.

[0028] A water-repellent film may be formed on the low refractive index layer, which is the outermost layer of the AR film. The water-repellent film is a film that gives water repellency to the surface, and can be formed by applying a solution of a fluorine-based compound such as metaxylene hexafluoride. The water-repellent film may be formed by, for example, ion-assisted deposition in the same manner as the AR film.

[0029] Through the above-described film formation process, a thin film having a laminated structure as shown in FIG. 3 is formed on the optical surface of the lens substrate. FIG. 3 is a side cross-sectional view showing an example of a laminated structure of thin films according to this embodiment. The laminated structure in the figure is configured by laminating an HC film 12, an AR film 13, and a water-repellent film 14 in this order on the optical surface of a lens substrate 11. The AR film 13 has a multilayer structure in which a low refractive index layer 13a and high refractive index layers SnO2 layer 13b and ZrO2 layer 13c are laminated, with the SiO2 layer 13a being the outermost layer (i.e., the surface layer on the water-repellent film 14 side).

[0030] After the thin film is formed, the eyeglass lens on which the thin film is formed is then subjected to frame cutting and marking of a decorative pattern, as shown in FIG. 2. For example, if the decorative process is performed after the frame cutting (S104: after cutting), first, one optical surface of the eyeglass lens to be processed (specifically, the optical surface not to be decorated, which will be described later) is attached to a dedicated jig (jig blocking) (S105). Then, the blocked eyeglass lens is set in an edge processing machine, and edge processing (frame cutting) is performed on the eyeglass lens, and the outer shape of the eyeglass lens is cut into the frame shape (S106). The jig blocking and frame cutting can be performed using known techniques, so detailed explanations are omitted here.

[0031] After the frame cutting process, the next step is the decoration process (i.e., the marking of the decoration pattern). In the decoration process, first, while still in the blocked state, the lens height of the processing area (i.e., the three-dimensional shape of the processing area on the processing surface) is measured for the processing surface (specifically, the optical surface on the side that is not blocked) of the eyeglass lens to be processed (S107). The measurement method is not particularly limited, but it is possible to use, for example, a non-contact type three-dimensional measuring machine.

[0032] After measuring the lens height in the processing area, laser processing is performed by irradiating the processing area with laser light, and raster scanning is performed by moving the irradiation position of the laser light based on previously prepared pattern data (S108). Vector scanning may be used instead of raster scanning. As a result, the processing area on the processing surface of the eyeglass lens is marked with a decorative pattern. Details of the laser processing for marking the decorative pattern will be described later.

[0033] After the decorative pattern is marked, the spectacle lens is removed from the special jig by deblocking (S109), and the removed spectacle lens is cleaned to remove any residue or foreign matter from the marking process (S110). Then, after a final lens appearance inspection (S111), the production of the spectacle lens is completed.

[0034] On the other hand, for example, in the case of performing frame cutting after decoration processing (S104: before cutting), first, the lens height of the processing area of ​​the processing surface of the eyeglass lens to be processed (i.e., the three-dimensional shape of the processing area on the processing surface) is measured (S112). The measurement method is the same as that in the case of performing decoration processing after frame cutting described above.

[0035] After measuring the lens height in the processing area, laser processing is performed by irradiating the processing area with laser light, and raster scanning is performed by moving the irradiation position of the laser light based on previously prepared pattern data (S113). Vector scanning may be used instead of raster scanning. As a result, the processing area on the processing surface of the eyeglass lens is marked with a decorative pattern. Details of the laser processing for marking the decorative pattern will be described later.

[0036] After the decorative pattern is marked, the eyeglass lens after marking is subjected to frame cutting. In the frame cutting process, first, one optical surface of the eyeglass lens to be processed is mounted on a dedicated jig (S114), and then the blocked eyeglass lens is set in an edging machine to perform edging (frame cutting), and the outer shape of the eyeglass lens is cut into the frame shape (S115). After the frame cutting process, the eyeglass lens is removed from the dedicated jig (S116), and the removed eyeglass lens is cleaned to remove any remaining material or adhering material (foreign matter) from the processing (S117). Then, after a final lens appearance inspection (S118), the manufacture of the eyeglass lens is completed.

[0037] (2) Details of laser processing Next, the laser processing for marking the decorative pattern will be described in more detail.

[0038] In this embodiment, the AR film 13 covering the optical surface of the lens substrate 11 is irradiated with a laser beam, and the SiO2 layer 13a, which is the top layer of the AR film 13, is partially removed, thereby marking the decorative pattern. That is, the SiO2 layer 13a, which is the top layer, is partially removed by laser processing in which a laser beam is irradiated, and the high refractive index layer on the lower layer side is exposed, and then the decorative pattern is marked. The high refractive index layer to be exposed is, for example, the ZrO2 layer 13c. If the ZrO2 layer 13c as the high refractive index layer is exposed, the SnO2 layer 13b, which is the high refractive index layer on the upper layer side, may be removed together with the SiO2 layer 13a, which is the top layer. If the removal of the SnO2 layer 13b is permitted, the SnO2 layer 13b can be formed to a thin thickness (for example, about 5 nm).

[0039] Here, a laser processing device used for the laser processing will be briefly described. FIG. 4 is an explanatory diagram showing a schematic configuration example of a laser processing device used in the method for manufacturing a spectacle lens according to this embodiment.

[0040] As shown in FIG. 4(a), the laser processing apparatus used in this embodiment includes a laser light source unit 21, an AOM (Acousto Optics Modulator) system unit 22, a beam shaper unit 23, a galvanometer scanner unit 24, and an optical system 25, and is configured to irradiate the AR film 13 with laser light via each of these units 21 to 25.

[0041] The laser light source unit 21 emits a laser beam used in laser processing, and is configured to emit an ultrashort pulse laser. In this embodiment, the ultrashort pulse laser refers to, for example, a laser having a pulse width of 0.1 picoseconds or more and less than 100 picoseconds, preferably a laser having a pulse width of 0.1 picoseconds or more and 30 picoseconds or less, and more preferably a laser having a pulse width of 0.1 picoseconds or more and 15 picoseconds or less. The lower limit of the pulse width is not particularly limited as long as it exceeds 0 femtoseconds, but as described above, for example, a laser having a pulse width of 0.1 picoseconds or more (including a laser having a pulse width of 1 picosecond or more) can be preferably used. The wavelength of the ultrashort pulse laser is, for example, 355 nm THG (Third Harmonic Generation) or 532 nm SHG (Second Harmonic Generation). However, it is not limited thereto, and may be, for example, a fundamental wavelength of 1064 nm or 266 nm FHG (Fourth Harmonic Generation). The pulse energy of the ultrashort pulse laser is, for example, 0.1 μJ or more and 30 μJ or less (maximum about 60 μJ) at 50 kHz. The beam diameter of the ultrashort pulse laser is, for example, 10 μm or more and 30 μm or less. As long as the laser light source unit 21 can emit such an ultrashort pulse laser, the specific configuration of the laser light source unit 21 is not particularly limited.

[0042] The AOM system section 22 suppresses excessive irradiation of laser light, which causes uneven processing during laser processing, by canceling the beam output of laser light immediately after the galvano scanner section 24 starts operating and just before its operation ends.

[0043] The beam shaper unit 23 converts the laser light from the laser light source unit 21 from a Gaussian energy distribution to a top-hat energy distribution, thereby making it possible to realize laser processing using laser light with a uniform energy distribution.

[0044] The galvano scanner unit 24 moves the irradiation position of the laser light from the laser light source unit 21 in two or three dimensions, thereby enabling scanning with the laser light to be realized, thereby enabling marking of a desired pattern by laser processing. Note that the scannable range (i.e., maximum laser processing area) 4 of the laser light by the galvano scanner unit 24 is set to a size and shape that can completely encompass the outer shape of the eyeglass lens to be processed (see FIG. 1).

[0045] The optical system 25 is composed of a combination of optical lenses such as telecentric lenses and mirrors, and guides the laser light from the laser light source unit 21 so that the laser light reaches the processing location of the eyeglass lens.

[0046] Moreover, as shown in FIG. 4(b), the laser processing device used in this embodiment is configured to irradiate the AR film 13 with laser light (i.e., ultrashort pulse laser) through the optical system 25 or the like in a defocus setting. The defocus setting means that the focal position F of the irradiated laser light is set at a predetermined defocus distance away from the surface of the AR film 13, which is the part to be processed by the laser light. If the laser light is irradiated in such a defocus setting, the beam energy can be dispersed on the surface of the AR film 13 irradiated with the laser light, thereby making it possible to perform uniform film removal processing. This is particularly useful when the height of the irradiated part may vary due to the influence of the surface shape of the AR film 13. However, it is not necessarily limited to the defocus setting, and the laser light may be irradiated in a focus setting in which the focal position F coincides with the surface of the AR film 13, or in a focus setting in which the focal position F is away in the opposite direction to the defocus setting.

[0047] Next, a procedure for laser processing performed using the laser processing apparatus configured as above will be described.

[0048] In the laser processing, first, the eyeglass lens to be processed is set in the laser processing device. At this time, the eyeglass lens is set so that the optical surface of the eyeglass lens, more specifically, the surface of the AR film 13 on the optical surface, becomes the surface to be processed. The optical surface to be the surface to be processed may be either the surface on the object side or the surface on the eyeball side, but here, for example, the surface on the eyeball side is used as the surface to be processed.

[0049] After the eyeglass lens is set, the laser light source unit 21 and the galvano scanner unit 24 are operated based on the prepared pattern data (i.e., the pattern data specifying the decoration pattern). As a result, the processing area of ​​the processing surface of the eyeglass lens is irradiated with the ultrashort pulse laser in a pattern shape corresponding to the decoration pattern.

[0050] When the ultrashort pulse laser is irradiated, the ultrashort pulse laser passes through the water-repellent film 14 on the processing surface of the eyeglass lens and reaches the AR film 13 on the processing surface. When the ultrashort pulse laser reaches the AR film 13, non-heating processing is performed due to the use of the ultrashort pulse laser.

[0051] Non-heating processing, also known as ablation processing, is a technology that uses the multiphoton absorption phenomenon of an ultrashort pulse laser to perform processing without heating. More specifically, non-heating processing is a removal process that minimizes the effect of heat around the processing area, and instantaneously melts, evaporates, and scatters the irradiated area of ​​the laser light, even in materials that only melt at a fairly high temperature under atmospheric pressure. With this type of non-heating processing, the molten area instantly evaporates, scatters, and is removed, so there is little thermal impact around the processing area, and processing can be performed with reduced thermal damage (such as deformation due to heat).

[0052] When non-heat processing is performed by irradiating an ultrashort pulse laser, the SiO2 layer 13a, which is the outermost layer of the multilayer structure constituting the AR film 13, is partially removed in a pattern shape corresponding to the decorative pattern. In addition, the corresponding portion of the water-repellent film 14 is also removed accordingly. Furthermore, with the removal of the SiO2 layer 13a, the SnO2 layer 13b located on the lower side of the SiO2 layer 13a is also partially removed. As a result, the ZrO2 layer 13c located on the lower side of the SnO2 layer 13b is exposed at the removed portion of the SiO2 layer 13a. At this time, if the ZrO2 layer 13c as a high refractive index layer is exposed, the SnO2 layer 13b as the upper high refractive index layer may be removed together with the outermost SiO2 layer 13a. If the removal of the SnO2 layer 13b is permitted, the SnO2 layer 13b can be formed to a thin thickness (for example, about 5 nm).

[0053] In general, as a laser processing for partially removing a thin film, a heating processing using a laser beam with a pulse width of the order of nanoseconds or more is widely used, instead of the above-mentioned non-heating processing. In the heating processing, the energy of the laser beam is absorbed by the processed portion of the thin film due to the relationship between the transmittance (absorption) of the laser beam and the thin film, and thus the thin film is removed. However, when such a heating processing is applied to the AR film 13, since each layer of the multilayer structure constituting the AR film 13 has the ability to absorb laser beam, not only the outermost layer of the multilayer structure but also multiple layers including the outermost layer are removed. Moreover, there is a risk of thermal damage occurring around the processed portion that has been removed. In particular, there is a concern that damage due to thermal damage will remain on the surface of the lower layer that will be exposed after removal.

[0054] In contrast, the non-heating process described above performs the removal process by the effect of the pulse width rather than the effect of the absorption energy of the laser light, so that it is possible to remove the SiO2 layer 13a, which is the outermost layer of the multi-layer structure constituting the AR film 13. Moreover, because it is a non-heating process, the thermal effect on the periphery of the processed area is small, and the occurrence of thermal damage can be suppressed. Specifically, for example, when the SiO2 layer 13a, which is the outermost layer of the AR film 13, is removed, the SnO2 layer 13b, which is the layer immediately below the SiO2 layer 13a, is also removed, and the ZrO2 layer 13c, which is a high refractive index layer, is exposed, but the occurrence of damage to the exposed surface of the ZrO2 layer 13c can be suppressed.

[0055] By carrying out the above-described laser processing, the SiO2 layer 13a, which is the outermost layer of the AR film 13, is partially removed to expose the ZrO2 layer 13c, which serves as a high refractive index layer, thereby marking the decorative pattern on the processed surface of the eyeglass lens.

[0056] (3) Composition of eyeglass lenses Next, the configuration of the eyeglass lens obtained by the manufacturing method with the procedure described above, that is, the configuration of the eyeglass lens according to this embodiment, will be specifically described. FIG. 5 is an explanatory diagram showing an example of the main configuration of the eyeglass lens according to the present embodiment.

[0057] As shown in Fig. 5(a), the eyeglass lens according to this embodiment is configured by laminating an HC film 12, an AR film 13, and a water-repellent film 14 in this order on the optical surface of a lens substrate 11. The AR film 13 has a multilayer structure in which a low-refractive index layer SiO2 layer 13a and high-refractive index layers SnO2 layer 13b and ZrO2 layer 13c are laminated, and the SiO2 layer 13a, which is the outermost layer of the multilayer structure, is partially removed to expose the ZrO2 layer 13c, which is the high-refractive index layer. Accordingly, the water-repellent film 14 covering the AR film 13 and the SnO2 layer 13b, which is the layer immediately below the SiO2 layer 13a, are also partially removed, similar to the outermost layer SiO2 layer 13a. In other words, the eyeglass lens of this embodiment is configured to include an unprocessed area 15 in which the optical surface of the lens substrate 11 is covered with an HC film 12, an AR film 13 and a water-repellent film 14, and a laser scan area (patterned area) 16 in which the outermost SiO2 layer 13a of the AR film 13, the SnO2 layer 13b directly below it, and the water-repellent film 14 are partially removed to expose the high refractive index layer, ZrO2 layer 13cb.

[0058] One of the non-processed area 15 and the laser scan area 16 is covered with the SiO2 layer 13a, and the other is exposed with the ZrO2 layer 13c, so that the reflectance of light in each area differs depending on the presence or absence of the SiO2 layer 13a. Therefore, when the eyeglass lens is viewed from the outside, the pattern shape formed by the laser scan area 16 can be visually recognized. In other words, if the laser scan area 16 is formed in a pattern shape corresponding to the decorative pattern, the decorative pattern can be visually recognized. In this way, the removed portion of the SiO2 layer 13a, which is the outermost layer of the AR film 13, can be used to form the decorative pattern. In order to make it visible as a decorative pattern, it is sufficient that the high refractive index layer is exposed in the laser scan area 16 from which the SiO2 layer 13a has been removed. Therefore, if the ZrO2 layer 13c as the high refractive index layer is exposed in the laser scan area 16, the SnO2 layer 13b, which is the high refractive index layer on the upper side, may be removed together with the outermost SiO2 layer 13a.

[0059] The laser scan area 16 constituting the decorative pattern is formed by removing the SiO2 layer 13a, which is the outermost layer of the AR film 13, and the SnO2 layer 13b, which is the layer immediately below it. In other words, the removal target is limited to the minimum number of layers including the SiO2 layer 13a. Therefore, it is possible to suppress peeling of each layer of the multilayer structure constituting the AR film 13 due to the formation of the laser scan area 16. For example, when performing laser processing using the absorbency of laser light, not only the outermost layer of the multilayer structure but also multiple layers including the outermost layer are removed, but the more the number of layers increases, that is, the deeper the groove depth of the removal area becomes, the higher the risk of peeling of the film increases. On the other hand, as in the laser scan area 16 in this embodiment, if the removal area is limited to the minimum including the outermost SiO2 layer 13a, there is no effect on the lower layer side, so it is possible to suppress peeling of the film due to the formation of the removal area.

[0060] As described above, the removal of the SiO2 layer 13a, which is the outermost layer of the AR film 13, can be achieved by non-heating processing using ultrashort pulse laser irradiation. This non-heating processing reduces the thermal impact on the periphery of the processed area, and can suppress the occurrence of thermal damage. Therefore, in the laser scan area 16 that constitutes the decorative pattern, the SnO2 layer 13b, which is the layer immediately below the SiO2 layer 13a, is also removed as the SiO2 layer 13a is removed, thereby exposing the ZrO2 layer 13c as a high refractive index layer, but it is possible to suppress the occurrence of damage to the exposed surface of the ZrO2 layer 13c.

[0061] If damage to the exposed surface of the ZrO2 layer 13c can be suppressed, the ZrO2 layer 13c can also be suppressed from reducing its thickness due to the removal processing of the SiO2 layer 13a. The thicknesses of the SiO2 layer 13a, the SnO2 layer 13b, the ZrO2 layer 13c, etc. can be determined by obtaining an electron microscope image of the cross section of the AR film 13 and analyzing the obtained image.

[0062] FIG. 5(b) shows a specific example of the results of observation of the cross section of the AR film 13 by an electron microscope. The example shows an enlarged view of parts A and B in FIG. 5(a), and shows electron microscope images of the laser scan area 16 and the non-processed area 15. In the non-processed area 15, the SiO2 layer 13a, the SnO2 layer 13b, and the ZrO2 layer 13c are laminated, but since the SnO2 layer 13b is thin (for example, about 5 nm), it is difficult to recognize it in the image. On the other hand, in the laser scan area 16, the SiO2 layer 13a and the SnO2 layer 13b have been removed, thereby exposing the ZrO2 layer 13c.

[0063] According to the electron microscope image of the example, in the ZrO2 layer 13c exposed by removing the SiO2 layer 13a, it can be seen that there is no significant difference between the thickness t1 of the laser scan area 16 where the SiO2 layer 13a has been removed and the thickness t2 of the non-processed area 15 covered by the SiO2 layer 13a. More specifically, the ratio t1 / t2 of the thickness t1 of the removed portion of the SiO2 layer 13a to the thickness t2 of the non-removed portion of the SiO2 layer 13a is set to be within a range of, for example, 0.90 to 1.00, preferably 0.95 to 1.00, more preferably 0.99 to 1.00.

[0064] In this way, the exposed high refractive index layer, ZrO2 layer 13c, does not undergo any reduction in thickness due to the removal processing of SiO2 layer 13a, or even if it does, the amount of reduction is suppressed to be extremely small. This is because the laser scan area 16 is formed by non-heating processing by irradiation of ultrashort pulse laser, and no damage is caused to the underlying ZrO2 layer 13c. This means that if the thickness ratio t1 / t2 of the exposed ZrO2 layer 13c falls within the above-mentioned range, the laser scan area 16 is formed without damaging the ZrO2 layer 13c, and it can be assumed that the laser scan area 16 was formed using non-heating processing by ultrashort pulse laser.

[0065] According to the eyeglass lens configured as described above, even if a decorative pattern is marked, peeling of each layer constituting the multi-layered AR film 13 can be suppressed, and the exposed ZrO2 layer 13c is not damaged. Therefore, even if the present invention is applied to eyeglass lens products, it is possible to mark the decorative pattern on the eyeglass lens without causing a deterioration in the quality of the product.

[0066] (4) Effects of this embodiment According to this embodiment, one or more of the following advantages can be obtained.

[0067] (a) In this embodiment, the SiO2 layer 13a, which is the outermost layer of the AR film 13, which is one of the thin films that cover the optical surface of the lens substrate 11, is partially removed to expose the ZrO2 layer 13c, which is a high refractive index layer, thereby marking the eyeglass lens with a decorative pattern. In this way, by removing a minimum number of layers including the SiO2 layer 13a, which is the outermost layer of the AR film 13, it is possible to prevent peeling of each layer of the multilayer structure that constitutes the AR film 13 due to the removal.

[0068] (b) In this embodiment, non-heating processing is performed by irradiating an ultrashort pulse laser to partially remove the SiO2 layer 13a, which is the top layer of the AR film 13, thereby exposing the ZrO2 layer 13c, which is a high refractive index layer, and thus marking the eyeglass lens with a decorative pattern. According to such non-heating processing, the removal processing is performed by the effect of the pulse width rather than the absorption energy effect of the laser light, so it is possible to remove a minimum amount of layers including the SiO2 layer 13a, which is the top layer of the AR film 13. Moreover, because it is non-heating processing, it is possible to suppress thermal damage occurring around the processing location, and therefore it is possible to suppress damage occurring to the exposed surface of the ZrO2 layer 13c exposed by removing the SiO2 layer 13a.

[0069] (c) As described above, in this embodiment, the SiO2 layer 13a, which is the outermost layer of the AR film 13, is removed while using an ultrashort pulse laser, and the ZrO2 layer 13c, which is a high refractive index layer, is exposed, thereby marking the decorative pattern on the eyeglass lens. Therefore, according to this embodiment, peeling of each layer of the AR film 13 can be suppressed, and the exposed ZrO2 layer 13c is not damaged. Therefore, even when applied to eyeglass lens products, it is possible to mark the decorative pattern on the eyeglass lens without causing a deterioration in the quality of the product.

[0070] (d) In this embodiment, the pulse width of the ultrashort pulse laser is 0.1 picoseconds or more and less than 100 picoseconds, preferably 0.1 picoseconds or more and 30 picoseconds or less, more preferably 0.1 picoseconds or more and 15 picoseconds or less. With such a pulse width, non-thermal processing can be performed reliably. In other words, the SiO2 layer 13a is removed by the effect of the pulse width rather than the effect of the absorption energy of the laser light, and as a result, the above-mentioned effect can be reliably obtained.

[0071] (e) In this embodiment, in the non-thermal processing by irradiation with an ultrashort pulse laser, the AR film 13 is irradiated with the ultrashort pulse laser in a defocused setting. By irradiating the laser light in such a defocused setting, the beam energy can be dispersed on the surface of the AR film 13 irradiated with the laser light, thereby making it possible to perform uniform film removal processing. This is particularly useful when the height of the irradiated portion may vary due to the influence of the surface shape of the AR film 13.

[0072] (f) In this embodiment, non-heating processing is performed by irradiating an ultrashort pulse laser, so that damage to the exposed surface of the ZrO2 layer 13c as a high refractive index layer that is exposed by removing the SiO2 layer 13a can be suppressed. Therefore, in the ZrO2 layer 13c, the reduction in film thickness accompanying the removal processing of the SiO2 layer 13a can also be suppressed. Specifically, when the SiO2 layer 13a is partially removed and the SnO2 layer 13b is also removed, the ratio t1 / t2 of the thickness t1 of the ZrO2 layer 13c at the removed portion of the SiO2 layer 13a, etc. to the thickness t2 of the ZrO2 layer 13c at the non-removed portion of the SiO2 layer 13a, etc., falls within a range of, for example, 0.90 to 1.00, preferably 0.95 to 1.00, more preferably 0.99 to 1.00. In this way, in the ZrO2 layer 13c, there is no reduction in the film thickness due to the removal processing of the SiO2 layer 13a, or even if there is a reduction, the reduction amount is suppressed to be extremely small. Therefore, when applied to a spectacle lens product, it is very preferable for marking a decorative pattern on the spectacle lens without causing a deterioration in the quality of the product.

[0073] (5) Modifications, etc. Although the embodiment of the present invention has been described above, the above disclosure shows an exemplary embodiment of the present invention. In other words, the technical scope of the present invention is not limited to the above exemplary embodiment, and various modifications are possible without departing from the gist of the present invention.

[0074] In the above embodiment, the optical member is a spectacle lens, but the present invention is not limited to this. In other words, the present invention can be applied to optical members other than spectacle lenses in the same manner.

[0075] In the above embodiment, a case where a decorative pattern is marked by non-heating processing using an ultrashort pulse laser is taken as an example, but the present invention is not limited to this. In other words, the non-heating processing using an ultrashort pulse laser can be applied in exactly the same way to other purposes besides marking a decorative pattern as long as it is for performing some kind of patterning on the optical surface of an optical component.

[0076] In the above embodiment, the outermost layer of the AR film 13 is the SiO2 layer 13a as a low refractive index layer, and the layers below the SiO2 layer 13a are the SnO2 layer 13b and the ZrO2 layer 13c as high refractive index layers. When the SiO2 layer 13a is partially removed, the SnO2 layer 13b is also removed, and the ZrO2 layer 13c as a high refractive index layer is exposed. However, the present invention is not limited to this. The AR film 13 may be configured by laminating layers other than the SiO2 layer 13a, the SnO2 layer 13b, and the ZrO2 layer 13c. In addition, the outermost layer of the AR film 13 may be a layer other than the SiO2 layer 13a as long as it is a low refractive index layer. Similarly, the layer below it may be a layer other than the SnO2 layer 13b or the ZrO2 layer 13c as long as it is a high refractive index layer. For example, the SnO2 layer 13b that is removed together with the SiO2 layer 13a may be replaced with a thin conductive ITO layer.

[0077] In the above embodiment, the case where the SiO2 layer 13a, which is the outermost layer of the AR film 13, and the SnO2 layer 13b, which is the layer immediately below it, are removed by non-heating processing using an ultrashort pulse laser, as described above. This provides the effect of suppressing film peeling. In this way, non-heating processing using an ultrashort pulse laser can be realized to remove multiple layers including the outermost layer. Even when multiple layers including the outermost layer are removed, non-heating processing using an ultrashort pulse laser can suppress damage to the exposed surface of the layer that will be exposed by the removal, so that the reduction in film thickness associated with the removal processing can also be suppressed. In other words, even when multiple layers including the outermost layer are removed, the ratio t1 / t2 of the thickness t1 of the removed portion to the thickness t2 of the non-removed portion for the layer immediately below the removed layer falls within the range of, for example, 0.90 to 1.00, preferably 0.95 to 1.00, more preferably 0.99 to 1.00. This means that the present disclosure includes the following inventive concept. That is, according to the present disclosure, an optical substrate having an optical surface; an anti-reflection film covering the optical surface of the optical substrate; the anti-reflection film has a multi-layer structure and is configured by partially removing at least one layer constituting the multi-layer structure, The layer immediately below the at least one layer is configured such that the ratio t1 / t2 of the thickness t1 of the removed portion of the at least one layer to the thickness t2 of the non-removed portion of the at least one layer is within the range of 0.90 to 1.00. Optical components. [Explanation of symbols]

[0078] 1... eyeglass lens (optical component), 2... frame shape, 3... decorative pattern, 4... scannable range, 11... lens substrate (optical substrate), 12... HC film, 13... AR film, 13a... SiO2 layer (low refractive index layer), 13b... SnO2 layer (high refractive index layer), 13c... ZrO2 layer (high refractive index layer), 14... water-repellent film, 15... non-processed area, 16... laser scan area (patterned area), 21... laser light source section, 22... AOM system section, 23... beam shaper section, 24... galvano scanner section, 25... optical system

Claims

1. an optical substrate having an optical surface; An optical member comprising: an anti-reflection film covering the optical surface of the optical substrate, the optical member is a spectacle lens, the antireflection film has a multilayer structure in which a low refractive index layer and a high refractive index layer are laminated, and the low refractive index layer, which is an outermost layer of the multilayer structure, is partially removed to expose the high refractive index layer; The high refractive index layer exposed by removing the low refractive index layer has a ratio t1 / t2 of a thickness t1 of the removed portion of the low refractive index layer to a thickness t2 of the non-removed portion of the low refractive index layer in the range of 0.90 to 1.

00. Optical components.

2. The outermost layer is a SiO layer serving as the low refractive index layer. 2 Layer The optical member according to claim 1 .

3. The layer exposed by removing the low refractive index layer is ZrO 2 Layer The optical member according to claim 1 .

4. The removed portion of the outermost low refractive index layer constitutes a decorative pattern of the optical member. The optical member according to claim 1 .

5. The optical member is a lens having a circular shape in a plan view before frame cutting processing, and has the decorative pattern at a position that will become within the lens area after frame cutting processing. The optical member according to claim 4 .

6. The decorative pattern is formed on the eyeball side surface of the optical member. The optical member according to claim 4 or 5.

7. The decorative pattern is formed on the object side surface of the optical member. The optical member according to claim 4 or 5.

8. The t1 / t2 is in the range of 0.95 to 1.

00. The optical member according to claim 1 .

9. The anti-reflection film is formed on a hard coat film. The optical member according to claim 1 .

10. The optical surface is a polished surface based on the eyeglass wearer's prescription. The optical member according to claim 1 .

11. The optical surface is a dyed surface. The optical member according to claim 1 .

12. The optical surface is a cast surface. The optical member according to claim 1 .

13. The optical substrate contains any one of allyl diglycol carbonate, a urethane-based resin, a polycarbonate, a thiourethane-based resin, and an episulfide resin. The optical member according to claim 1 .

14. The antireflection layer is made of tin oxide (SnO 2 ), niobium oxide (Nb 2 O 5 ), tantalum oxide (Ta 2 O 5 ), titanium oxide (TiO 2 ), yttrium oxide (Y 2 O 3 ), aluminum oxide (Al 2 O 3 ), and mixtures thereof, The mixture includes indium tin oxide (ITO). The optical member according to claim 1 .

15. Further has a water-repellent film The optical member according to claim 1 .

16. The removed portion of the low refractive index layer has a different light reflectance than the non-removed portion. The optical member according to claim 1 .

Citation Information

Patent Citations

  • Method for laser marking

    JP2003156667A

  • Marking method to spectacle lens and spectacle lens

    JP2006053227A

  • Optical member, and method of manufacturing the same

    JP2014071166A

  • Marking method for multilayer deposition body and multilayer deposition body

    JP2016007612A

  • Method for permanently visible marking of optical products and marked optical products

    JP2019523447A

Cited By

  • Novel compounds, titanium oxide film-forming materials, and titanium oxide film-forming methods.

    JP2026136027A