Odor sensor and manufacturing method of odor sensor
By minimizing the height difference between the sensor layer and metal electrode in the odor sensor design, the sensor achieves improved detection sensitivity through a uniform and thinner adsorption film, addressing the sensitivity issues in conventional sensors.
Patent Information
- Application Number
- JP2023076371
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-02
- Publication Date
- 2024-11-15
AI Technical Summary
Conventional odor sensors face reduced detection sensitivity due to a significant height difference between the sensor layer and the metal electrode, leading to variations in adsorption film thickness.
The odor sensor design reduces the height difference between the sensor layer and the metal electrode by forming the adsorption film on the surface of a protective layer opposite to the silicon substrate, with the sensor layer and metal electrode positioned on the protective layer surface without being buried, and the metal electrode formed thin enough to maintain uniform adsorption film thickness.
This configuration enhances detection sensitivity by ensuring a uniform and thinner adsorption film, reducing defects and improving the sensor's ability to detect odors effectively.
Smart Images

Figure 2024160879000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an odor sensor and a method for manufacturing an odor sensor, and more particularly to an odor sensor in which the height difference between a sensor layer and a metal electrode is reduced. [Background technology]
[0002] Conventionally, so-called odor detection has been performed by using an odor sensor to detect odor substances contained in surrounding gas (for example, Patent Document 1). If an odor sensor could measure the intensity of an odor and identify the type of odor, it would contribute to reproducing pleasant odors and reducing unpleasant odors, making people's lives more comfortable and enriching.
[0003] An odor sensor has, for example, an adsorption film that adsorbs an odorant, and a sensor layer that detects a change in the adsorption state (adsorption characteristics) caused by the odorant being adsorbed onto the adsorption film.
[0004] As a combination of an adsorption film and a sensor layer, for example, an odor sensor that combines a polyaniline sensitive film and an ion image sensor as described in Patent Document 1 has been proposed. In this odor sensor, it is possible to detect the gas to be measured by monitoring the potential of the sensor layer when a reference voltage is applied to the adsorption film from a reference electrode (hereinafter, metal electrode) disposed in the sensor. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2020-8522 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, in conventional odor sensors, the structure of the sensor results in a large difference in height between the position of the sensor layer and the position of the metal electrode disposed within the sensor. When a difference in height occurs between the sensor layer and the metal electrode, the thickness of the adsorption film formed on the sensor surface varies from place to place, and it becomes difficult to reduce the thickness of the adsorption film. As a result, there is a problem that the detection sensitivity of the odor sensor decreases.
[0007] The present invention has been made in consideration of the above circumstances, and has an exemplary objective of providing an odor sensor and a method for manufacturing an odor sensor that can reduce the difference in height between the sensor layer and the metal electrode in the odor sensor, thereby reducing the variation in the thickness of the adsorption film and achieving a thinner film, thereby improving the detection sensitivity. [Means for solving the problem]
[0008] In order to solve the above problems, an odor sensor as an exemplary aspect of the present invention has the following configuration.
[0009] A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A metal electrode formed on the front surface side of the silicon substrate, the adsorption film is formed on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer, An odor sensor, wherein the sensor layer is formed on the surface side of the protective layer without being embedded in the protective layer.
[0010] A method for producing an odor sensor according to another exemplary aspect of the present invention has the following configuration.
[0011] A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A method for manufacturing an odor sensor having a metal electrode formed on the front surface side of the silicon substrate, comprising the steps of: a protective layer forming step of forming the protective layer on a surface of the silicon substrate; a sensor layer forming step of forming the sensor layer on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer after the protective layer forming step; a metal electrode forming step of forming the metal electrode on a surface side of the protective layer, the metal electrode being located at a position other than the surface of the sensor layer, after the protective layer forming step; a step of forming the adsorption film on the front surface side of the sensor layer, the step being subsequent to the step of forming the sensor layer and subsequent to the step of forming the metal electrode.
[0012] Further objects and other features of the present invention will become apparent from the following description of preferred embodiments with reference to the accompanying drawings. Effect of the Invention
[0013] According to the present invention, it is possible to provide an odor sensor and a method for manufacturing an odor sensor that can reduce variation in the thickness of an adsorption film and make the adsorption film thinner, thereby improving detection sensitivity. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a cross-sectional view showing a schematic structure of an odor sensor according to a first embodiment of the present invention. [Diagram 2] 2 is a plan view showing a schematic configuration of the odor sensor of FIG. 1 as viewed from the front side. [Diagram 3] 2 is a flowchart illustrating a method for manufacturing the odor sensor of FIG. 1. [Figure 4] FIG. 1 is a cross-sectional view showing a schematic structure of a conventional odor sensor. [Diagram 5] 5A and 5B are schematic diagrams illustrating the state in which an adsorption film is formed on the surface of the odor sensor in FIG. 4, where (a) shows the case in which the thickness of the adsorption film is relatively thin, and (b) shows the case in which the thickness of the adsorption film is relatively thick. [Figure 6] 5 is a graph showing the results of a comparison of the sensor sensitivity of the odor sensor in FIG. 4 and the odor sensor in FIG. 1, where (a) shows the sensor sensitivity of the odor sensor in FIG. 4 and (b) shows the sensor sensitivity of the odor sensor in FIG. 1. [Figure 7] Evaluation results of Example 2, where (a) shows a microscopic image and a potential detection image of the adsorption film 6 in a conventional odor sensor 21, and (b) shows a microscopic image and a potential detection image of the adsorption film 6 in the odor sensor 1 of embodiment 1. [Figure 8] 1 shows the evaluation results of Example 3, where (a) is a microscope image of the adsorption film 6 in the odor sensor 1 in accordance with Embodiment 1, and (b) is a graph of the film thickness distribution in the PP cross section. [Figure 9] 1A and 1B are plan views showing a schematic view of an odor sensor according to a second embodiment of the present invention as viewed from the front side, in which (a) shows one vertical row of sensor layers sandwiched between two metal electrodes, and (b) shows three rows of sensor layers sandwiched between two metal electrodes a. [Figure 10] 1A is a plan view showing a schematic view of an odor sensor according to a third embodiment of the present invention as viewed from the front side, in which (a) shows nine sensor layers surrounded by two pairs of metal electrodes in a vertical and horizontal direction, and (b) shows nine sensor layers surrounded by four metal electrodes arranged on the outside of each of the four sensor layers at the four corners of the nine sensor layers. [Figure 11] FIG. 11 is a plan view illustrating a schematic view of an odor sensor according to a fourth embodiment of the present invention as viewed from the front side. [Figure 12]FIG. 1 shows an odor sensor according to a fifth embodiment of the present invention, where (a) is a plan view of the odor sensor, and (b) is a cross-sectional view taken along line AA in (a). [Figure 13] 13A and 13B are diagrams showing another correspondence between the detection unit and the adsorption film in the odor sensor of FIG. 12, where (a) is a plan view of the odor sensor, and (b) is a cross-sectional view taken along line BB in (a). [Figure 14] FIG. 11 is a schematic diagram showing the general configuration of an odor data analysis device according to a fifth embodiment of the present invention. [Figure 15] FIG. 11 is a schematic diagram showing the configuration of an odor sensor unit according to a sixth embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] [Embodiment 1] Hereinafter, the first embodiment of the present invention will be described in detail with reference to the drawings. In the following description, "odor substance" broadly means a substance that can be adsorbed to an adsorption film. Therefore, "odor substance" also includes substances that are not generally considered to be odor-causing substances, substances that are not recognized as odor substances, or unknown odor substances. In addition, "odor substance" includes not only individual odor substances, but also "aggregates of multiple odor substances."
[0016] <Odor sensor> Fig. 1 is a structural diagram showing a schematic structure of an odor sensor 1 according to a first embodiment of the present invention. Fig. 1 is a cross-sectional view of the odor sensor 1 cut along its thickness direction. The odor sensor 1 is roughly composed of a flat substrate (silicon substrate) 2, a protective layer 4, an adsorption film 6, a sensor layer 8, and a metal electrode 10.
[0017] The substrate 2 is a flat plate-like member that constitutes the base portion of the odor sensor 1, and typically has a thickness of about 100 μm to 3000 μm, but is not limited to this. The material of the substrate 2 is typically silicon (Si), but is not limited to this, and various single crystal and polycrystalline semiconductor materials that can be used for the base portion can be used.
[0018] In Fig. 1, the up-down direction is defined as shown in the figure, and is also referred to as the thickness direction. The upper side is also referred to as the front side, the lower side as the back side, the front surface as the front side, and the back surface as the back side. Of course, the up-down direction may be reversed depending on the arrangement direction of the odor sensor 1, but in this embodiment, the up-down direction shown in Fig. 1 is used.
[0019] The protective layer 4 is a layer formed on the front surface 2a, which is one of the front and back surfaces of the substrate 2. Silicon nitride (Si3N4) can be used as the material for the protective layer 4, but since high crystallinity is not required for the protective layer 4, low-crystalline silicon nitride can be used. Silica (SiO2) can also be used for the protective layer 4. Therefore, high temperatures are not required for the formation of the protective layer 4, and the protective layer 4 can be formed at a temperature of, for example, about 500° C. or less. Note that the protective layer 4 can be formed on the substrate 2 by known layer formation methods such as CVD and sputtering.
[0020] The protective layer 4 has a function of protecting, for example, the metal electrode 10a and other internal wiring (not shown) disposed inside the protective layer 4 from various external factors (for example, adverse effects due to gases generated in the process and liquid agents used in the process) that may occur in the process of forming the sensor layer 8 and the adsorption film 6 described below. In addition, the protective layer 4 also exhibits a function of preventing electrical contact between, for example, the adsorption film 6 and the metal electrode 10a inside the protective layer 4 and other internal wiring (not shown).
[0021] The adsorption film 6 is formed on the surface 2a side of the substrate 2, and adsorbs odorous substances contained in the gas present around it. An odorous substance is a substance that causes an odor. A gas containing an odorous substance emits an odor specific to that odorous substance. Examples of odorous substances include acetic acid and ammonia. Components contained in various herbal plants such as eucalyptus, citrus fruits such as lychee, and various spices can also be odorous substances. A gas may contain multiple odorous substances. By containing multiple odorous substances, multiple odors may be blended, and the gas may have an odor different from each odorous substance.
[0022] The adsorption film 6 is formed, for example, by adding an additive (dopant) to a conductive polymer film as a film material. The function of the adsorption film 6 to adsorb odor substances is realized by the additive adsorbing a specific odor substance. The adsorption film 6 is capable of adsorbing different odor substances depending on the type of additive.
[0023] A plurality of different types of adsorption films 6 may be formed on the substrate 2. The different adsorption films 6 may correspond to different additives, and the different additives may selectively adsorb different odor substances. For example, when a plurality of sensor layers 8, which will be described later, are formed on the surface 2a of the substrate 2, different adsorption films 6 may be formed corresponding to each of the sensor layers 8. Also, different adsorption films 6 may be formed corresponding to some of the sensor layers 8. In the odor sensor 1 according to the first embodiment, the thickness of the adsorption film 6 is within a range of about 1 nm to 2 μm, and more preferably within a range of 1 nm to 500 nm. In this odor sensor 1, it is not necessary to expose the sensor layer 8 by a process of removing the protective layer 4 by etching or the like, so that the thickness of the adsorption film 6 can be made thin and relatively uniform.
[0024] The sensor layer 8 is formed on the front surface 2a side of the substrate 2, and detects the odor of the gas in response to the adsorption of the odorant by the adsorption film 6. The sensor layer 8 can detect the amount of odorant adsorbed to the adsorption film 6 in response to changes in the physical properties, chemical properties and / or electrical properties of the adsorption film 6 caused by the odorant being adsorbed to the adsorption film 6. The sensor layer 8 is formed on the front surface side (upper side) of the protective layer 4 after the protective layer 4 is formed on the front surface 2a of the substrate 2.
[0025] FIG. 2 is a plan view showing a schematic configuration of the odor sensor 1 as viewed from the front surface 2a side. The sensor layer 8 is configured as an ISFET type sensor with, for example, tantalum pentoxide (Ta2O5) as a gate material. As shown in FIG. 2, a plurality of sensor layers 8 may be arranged on the front surface 2a side of the substrate 2. In this case, the size of the sensor layer 8 is about several 100 nm to several 100 μm in diameter or one side, or preferably about 100 nm to 30 μm, and more preferably about 100 nm to 3 μm, and the shape is circular, rectangular, or a shape similar thereto. Furthermore, the sensor layers 8 may be arranged vertically and horizontally on the substrate 2 at a pitch (spacing) of several μm to several 10 μm, and at a pitch equal to or greater than the size of the sensor layer 8. In this case, the odor sensor 1 may be referred to as an "odor image sensor" and the sensor layers 8 as "pixels".
[0026] The metal electrode 10 is an electrode formed on the surface 2a side of the substrate 2, and is made of a metal such as aluminum. The material of the metal electrode 10 is not limited to aluminum, and for example, copper or gold can also be used. Reference numeral 12 in FIG. 1 indicates contacts configured in the odor sensor 1, such as a drain, gate, and source. The material of the contacts 12 is, for example, polysilicon, and is disposed on the surface 2a of the substrate 2 via an insulating layer 14 made of silica (SiO2) or the like. The metal electrode 10a of the metal electrode 10 has a function of realizing electrical continuity between the multiple sensor layers 8 and between the sensor layer 8 and the contacts 12.
[0027] As shown in Fig. 1, some of the metal electrodes 10 (metal electrode 10a) are formed before the protective layer 4 is formed on the front surface 2a of the substrate 2, and are consequently disposed inside the protective layer 4. On the other hand, some (metal electrode 10b) are formed on the further front surface (upper side) of the protective layer 4 after the protective layer 4 is formed on the front surface 2a of the substrate 2, or on the further upper side of the sensor layer 8 formed on the front surface of the protective layer 4. Conduction is achieved between the sensor layer 8 and the metal electrode 10b via the adsorption film 6. The metal electrode 10b is for applying a reference voltage to the adsorption film 6 and the sensor layer 8.
[0028] In particular, the metal electrode 10b formed further above the sensor layer 8 is preferably made to have a thickness of 20 times or less than the thickness of the adsorption film 6. Furthermore, the metal electrode 10b is more preferably made to have a thickness equal to or less than the thickness of the adsorption film 6, and may be, for example, 500 nm or less, and more preferably 100 nm or less.
[0029] By reducing the thickness of the metal electrode 10b, the difference in thickness between the surface of the sensor layer 8 and the surface of the metal electrode 10b on the front side of the odor sensor 1, that is, the height difference, can be reduced. The height difference is preferably 2 μm or less, and more preferably 500 nm or less. By reducing the height difference between the surface of the sensor layer 8 and the surface of the metal electrode 10b, the thickness of the adsorption film 6 can be made thin and relatively uniform. This improves the sensitivity of the odor sensor 1.
[0030] <Manufacturing method of odor sensor> Next, a method for manufacturing the odor sensor 1 will be described with reference to the flow chart of Fig. 3. Note that the manufacturing method described here is merely an example, and the manufacturing method for the odor sensor 1 of this embodiment 1 is not limited to the one described here. Ultimately, it is desirable to obtain an odor sensor 1 in which the difference (height difference) in the thickness direction between the metal electrode 10b formed on the surface 2a of the substrate 2 and the sensor layer 8 is small, and as a result, the thickness of the adsorption film 6 formed on the surface side is thin and relatively uniform.
[0031] A protective layer 4 is formed on a surface 2a of a substrate 2 (protective layer forming step: S.1). An N-well 16 may be formed inside the substrate 2 in advance. Furthermore, before the protective layer 4 is formed, contacts 12 such as a drain, gate, and source may be disposed on the surface 2a via an insulating layer. Furthermore, a metal electrode 10a may be formed in electrical conduction with the contacts 12.
[0032] The protective layer forming step can be performed at a temperature of about 500° C. or less when low-crystalline silicon nitride or silica is used as the protective layer 4. Therefore, even if the material of the preformed metal electrode 10a is a metal with a heat resistance temperature of about 500° C. or less, the protective layer forming step does not adversely affect the metal electrode 10a in terms of temperature. Furthermore, by forming the protective layer 4, the metal electrode 10a and other internal wirings inside the protective layer 4 are protected from the effects of the sensor layer forming step and the adsorption film forming step described below, and electrical contact between the metal electrode 10a and other internal wirings and the sensor layer 8 can be prevented.
[0033] After the protective layer forming step, the sensor layer 8 is formed on the front surface side of the protective layer 4 (the side opposite the substrate 2 when viewed from the protective layer 4) (sensor layer forming step: S.2). The sensor layer 8 can be formed using a known film formation technique such as sputtering or CVD. When tantalum pentoxide is used as the sensor layer 8, the sensor layer forming step can be performed at a temperature of about 500° C. or less. Therefore, even if the material of the preformed metal electrode 10a is a metal with a heat-resistant temperature of about 500° C. or less, the protective layer forming step does not adversely affect the metal electrode 10a in terms of temperature.
[0034] After the protective layer forming step, a metal electrode 10b is formed on the surface side of the protective layer 4 (the side opposite the substrate 2 when viewed from the protective layer 4) (metal electrode forming step: S.3). The metal electrode 10b can be formed using a known film formation technique such as sputtering or CVD. Metals such as aluminum, copper, and gold can be used as the metal electrode 10b. It is preferable to form the metal electrode 10b as thin as possible. This can reduce the difference in thickness (height difference) between the surface of the sensor layer 8 and the surface of the metal electrode 10b.
[0035] The metal electrode 10b is formed on the surface side of the protective layer 4 at a position that is not on the surface of the sensor layer 8, i.e., in an area that is not in contact with the sensor layer 8 (see FIG. 1). In this case, the order of the sensor layer formation step (S.2) and the metal electrode formation step (S.3) does not matter. Here, "a position that is not on the surface of the sensor layer 8" means "a position that is not on the surface of the sensor layer 8" or "a position that is not in contact with the sensor layer 8", and means that the sensor layer 8 and the metal electrode 10b are not directly electrically connected (however, electrical connection is only possible via the adsorption film 6).
[0036] After the sensor layer forming step and the metal electrode forming step, an adsorption film 6 is formed on the surface side of the sensor layer 8 (the side opposite the substrate 2 as viewed from the sensor layer 8) (adsorption film forming step: S.4). The adsorption film 6 can be formed by various known methods such as coating, dropping, spray coating, etc. The adsorption film 6 is formed between the sensor layer 8 and the metal electrode 10b so that the sensor layer 8 and the metal electrode 10b are electrically connected via the adsorption film 6.
[0037] By manufacturing the odor sensor 1 based on the above process, it is possible to reduce the unevenness and steps on the surface of the odor sensor 1 before the adsorption film 6 is formed, i.e., the difference (height difference) in the thickness direction between the sensor layer 8 and the metal electrode 10b.
[0038] For example, in the conventional odor sensor 21 shown in Fig. 4, in order to expose the sensor layer 8 formed inside the protective layer 4 to the outside, it is necessary to remove a part of the protective layer 4 by a process such as etching to create an opening. As a result, the unevenness and steps on the surface of the odor sensor 21 before the formation of the adsorption film 6 become large. Fig. 4 shows the difference (height difference) H in the thickness direction between the sensor layer 8 and the metal electrode 10b caused by the unevenness and steps on the surface of the odor sensor 21.
[0039] FIG. 5 is a schematic diagram illustrating the situation in which an adsorption film 6 is formed on the surface of a conventional odor sensor 21, where (a) shows the case in which the adsorption film 6 is relatively thin, and (b) shows the case in which the adsorption film 6 is relatively thick.
[0040] As shown in FIG. 5(a), when the adsorption film 6 is formed relatively thin on a surface with large irregularities or steps, a missing portion 6a in which a part of the adsorption film 6 is missing or an extremely thin portion 6b in which the thickness of the adsorption film 6 is excessively thin may occur. If a missing portion 6a occurs, the sensor sensitivity of that portion may be lost or the conductivity of the adsorption film 6 may be cut off, resulting in a malfunction in which the sensor does not function. If an extremely thin portion 6b occurs, the odorant may not be fully adsorbed, which may result in a decrease in sensitivity, and the adsorption film may break during use due to a decrease in mechanical strength.
[0041] 5(b), when the adsorption film 6 is formed relatively thick on a surface with large irregularities or steps, an extremely thick portion 6c may be generated in which the thickness of the adsorption film 6 is excessively thick. In the extremely thick portion 6c, it becomes difficult for the odor substances adsorbed on the adsorption film 6 to reach the sensor layer 8, which may result in a decrease in sensitivity.
[0042] On the other hand, in the odor sensor 1 of the present embodiment 1, the difference (height difference) in the thickness direction between the sensor layer 8 and the metal electrode 10b is reduced (for example, 1 μm or less), so that the variation in the thickness direction of the adsorption film 6 can be reduced. If the thickness of the adsorption film 6 can be made substantially uniform, the overall thickness of the adsorption film 6 can be thinned, for example, to a range of 1 μm or less. Even if the thickness of the adsorption film 6 is thinned, no missing parts 6a, very thin parts 6b, etc. are generated, and even if the thickness of the adsorption film 6 is thickened, no very thick parts 6c, etc. are generated, so that a decrease in sensor sensitivity due to these factors can be prevented.
[0043] [Example 1] Fig. 6 is a graph showing a comparison result of the sensor sensitivity between the conventional odor sensor 21 shown in Fig. 4 and the odor sensor 1 according to the present embodiment 1 shown in Fig. 1. Fig. 6(a) shows the sensor sensitivity of the conventional odor sensor 21, and Fig. 6(b) shows the sensor sensitivity of the odor sensor 1 according to the present embodiment 1.
[0044] Each graph shows how the output voltage of the odor sensor 21 or odor sensor 1 changes over time when the odor sensor 21 or odor sensor 1 is placed in a gas containing a specific odorant and the odorant is adsorbed by the adsorption film 6. In each graph, the horizontal axis represents the elapsed time T after the odor sensor is placed in the gas, and the vertical axis represents the output voltage V of the odor sensor.
[0045] 6(a) and 6(b) are the same except for the odor sensor 21 and the odor sensor 1. In each figure, graph G1 shows the case where the adsorption film 6 is extremely thick (approximately 800 nm thick), graph G2 shows the case where the adsorption film 6 is thick (approximately 600 nm thick), graph G3 shows the case where the adsorption film 6 is thin (approximately 400 nm thick), and graph G4 shows the case where the adsorption film 6 is extremely thin (approximately 200 nm thick). The thicknesses of the adsorption film 6 are in the order of extremely thick > thick > thin > extremely thin.
[0046] 6(a), in the odor sensor 21, the output voltage at an elapsed time T=200 sec is about 3.8 mV in graph G1, about 17 mV in graph G2, about 39 mV in graph G3, and about 48 mV in graph G4. This indicates that the thicker the adsorption film 6 is, the lower the sensor sensitivity is, and the thinner the adsorption film 6 is, the higher the sensor sensitivity is. Note that a large output voltage from the sensor layer is synonymous with a high sensor sensitivity of the odor sensor, that is, a high detection sensitivity of the odor sensor when an odorant is adsorbed on the adsorption film.
[0047] 6(b), in the odor sensor 1, the output voltage at an elapsed time T=200 sec is about 154 mV in graph G1, about 190 mV in graph G2, about 202 mV in graph G3, and about 346 mV in graph G4. This is similar to the odor sensor 21 in that the thicker the adsorption film 6 is, the lower the sensor sensitivity is, and the thinner the adsorption film 6 is, the higher the sensor sensitivity is.
[0048] However, in the odor sensor 1, the output voltage value itself is about 5 to 40 times higher than in the odor sensor 21. In the odor sensor 1, the difference in thickness (height difference) between the sensor layer 8 and the metal electrode 10b is reduced, and as a result, the adsorption film 6 maintains a constant thickness throughout the odor sensor 1. This results in good sensor sensitivity. In the odor sensor 21, the difference in thickness (height difference) between the sensor layer 8 and the metal electrode 10b is large. If the adsorption film 6 is formed thick, for example, an extremely thick portion 6c (see FIG. 5) or the like may occur, which may cause a decrease in sensitivity. If the adsorption film 6 is formed thin, for example, a missing portion 6a or an extremely thin portion 6b (see FIG. 5) may occur, which may cause a decrease in sensitivity.
[0049] [Example 2] Fig. 7 shows the evaluation results of Example 2. Fig. 7(a) shows a microscope image and a potential detection image of the adsorption film 6 in a conventional odor sensor 21, and Fig. 7(b) shows a microscope image and a potential detection image of the adsorption film 6 in the odor sensor 1 according to embodiment 1. In both cases, the adsorption film 6 is formed on the surface of the sensor layer 8, and the thickness of the adsorption film 6 is controlled to be about 200 nm. Of course, the thickness of the adsorption film 6 may vary to a certain extent in both the odor sensor 21 and the odor sensor 1.
[0050] 7(a) and 7(b), the areas filled in black are areas where potential detection is being performed (i.e., areas that function as an odor sensor), and the areas that are white are areas where potential detection is not being performed (i.e., areas that do not function as an odor sensor). From Fig. 7, it can be seen that even when the adsorption film 6 is formed with a controlled thickness of about 200 nm, in the odor sensor 21, many areas where potential detection is not performed occur even in the area where the adsorption film 6 is formed, while in the odor sensor 1, potential detection is performed in almost the entire area where the adsorption film 6 is formed.
[0051] [Example 3] Fig. 8 shows the evaluation results of Example 3. Fig. 8(a) is a microscope image of the adsorption film 6 in the odor sensor 1 according to embodiment 1, and Fig. 8(b) is a graph of the film thickness distribution in the PP cross section. The adsorption film 6 is formed on the surface of the sensor layer 8, and the film thickness is controlled to be about 200 nm.
[0052] In Fig. 8(b), the horizontal axis X indicates the left-right position (mm) along the PP cross section of the adsorption film 6, and the vertical axis Z indicates the thickness (μm) of the adsorption film 6. As shown in Fig. 8(b), in the odor sensor 1, the adsorption film 6 was formed under control to have a thickness of 200 nm, and as a result, the actual film thickness was within a range of approximately 100 nm to 200 nm. This ensures the approximate thickness of the adsorption film formed in the odor sensor 1 and the odor sensor 21 in Example 2.
[0053] [Embodiment 2] Fig. 9 is a plan view showing a schematic state of an odor sensor 31 according to embodiment 2 as seen from the front surface 2a side. For ease of explanation, Fig. 9 shows the odor sensor 31 without the adsorption film 6. In this odor sensor 31, a plurality of sensor layers 8 are arranged on the front surface 2a side of the substrate 2, above the protective layer 4, and in the example shown in Fig. 9, 20 sensor layers 8 are arranged in four vertical rows and five horizontal rows on the front surface 2a side of the substrate 2.
[0054] In Fig. 9, the metal electrodes 10b are arranged to sandwich the sensor layer 8. In Fig. 9(a), one vertical row of sensor layers 8 is sandwiched between two metal electrodes 10b, and in Fig. 9(b), multiple rows (e.g., three rows) of sensor layers 8 are sandwiched between two metal electrodes 10b. As a result, the distance between the metal electrodes 10b is equal to or greater than the size of the sensor layer 8. By arranging the sensor layer 8 and the metal electrodes 10b in this manner, the sensor sensitivity of the odor sensor 1 can be improved.
[0055] In addition, when multiple metal electrodes 10b are arranged to sandwich multiple sensor layers 8, the sensor sensitivity of the sensor layer 8 arranged at a position that is approximately equidistant from the multiple metal electrodes 10b is the highest. That is, in the example shown in FIG. 9(b), the sensor layer 8 in row B located approximately in the center sandwiched between two metal electrodes 10b has a higher sensor sensitivity than the sensor layers 8 in rows A and C. Even if the number of rows of sensor layers 8 sandwiched between metal electrodes 10b increases, the sensor sensitivity of the sensor layer 8 closer to the center of both metal electrodes 10b is higher than that of the sensor layer 8 closer to one metal electrode 10b. In addition, the narrower the pitch between the two metal electrodes 10b (the distance between the metal electrodes 10b), the higher the output voltage of the sensor layer 8.
[0056] [Embodiment 3] Fig. 10 is a plan view showing a schematic state of an odor sensor 41 according to embodiment 3 as seen from the front surface 2a side. For ease of explanation, Fig. 10 shows the odor sensor 41 without the adsorption film 6. In this odor sensor 41, a plurality of sensor layers 8 are arranged on the front surface 2a side of the substrate 2, above the protective layer 4, and in the example shown in Fig. 10, nine sensor layers 8 are arranged in three vertical rows and three horizontal rows on the front surface 2a side of the substrate 2.
[0057] In Fig. 10, the metal electrodes 10b are arranged so as to surround the sensor layer 8. In Fig. 10(a), the metal electrodes 10b extending lengthwise and widthwise surround the nine sensor layers 8 in the top, bottom, left, and right directions, and in Fig. 10(b), the four metal electrodes 10b arranged on the outside of each of the four sensor layers 8 corresponding to the four corners of the nine sensor layers 8 surround the nine sensor layers 8. As a result, the distance between the metal electrodes 10b is equal to or greater than the size of the sensor layer 8. By arranging the sensor layers 8 and the metal electrodes 10b in this manner, the sensor sensitivity of the odor sensor 1 can be improved.
[0058] Even in this case, the sensor layer 8 arranged at a position that is approximately equidistant from the multiple metal electrodes 10b has the highest sensor sensitivity, as in the case of the second embodiment. The sensor layer 8 that is closer to one of the multiple metal electrodes 10b surrounding the sensor layer 8 has a smaller difference in distance from the multiple metal electrodes 10b, that is, has a higher sensor sensitivity than the sensor layer 8 that is closer to the center of the surrounded area. Also, the narrower the pitch between the multiple metal electrodes 10b (the distance between the metal electrodes 10b), the higher the output voltage of the sensor layer 9.
[0059] [Embodiment 4] Fig. 11 is a plan view showing a schematic state of an odor sensor 51 according to embodiment 4 as seen from the front surface 2a side. For ease of explanation, Fig. 11 shows the odor sensor 51 without the adsorption film 6. In this odor sensor 51, a large number of sensor layers 8 are arranged vertically and horizontally on the front surface 2a side of the substrate 2, above the protective layer 4.
[0060] In Fig. 11, a metal electrode 10b is arranged further on the surface side of the sensor layer 8, i.e., on the upper side so as to overlap the sensor layer 8. In Fig. 11, similar to the arrangement described in the third embodiment, two pairs of metal electrodes 10b vertically and horizontally surround at least one sensor layer 8a. As a result, the distance between the metal electrodes 10b is equal to or greater than the size of the sensor layer 8. The metal electrodes 10b do not necessarily have to be arranged so as to surround the sensor layer 8a as shown in Fig. 11, and may be arranged so as to sandwich the sensor layer 8, similar to the arrangement described in the second embodiment.
[0061] The fourth embodiment is characterized in that the metal electrode 10b is formed further above the sensor layer 8. If the metal electrode 10b is formed to be thin, for example, 500 nm or less, the height difference between the metal electrode 10b and the sensor layer 8 can be 1 μm or less even if the metal electrode 10b is disposed on the upper side of the sensor layer 8. This can reduce variations in the thickness of the adsorption film 6 and make the thickness approximately uniform.
[0062] [Embodiment 5] Hereinafter, a fifth embodiment of the present invention will be described with reference to the drawings.
[0063] <Odor sensor> 12 is a diagram showing an odor sensor 100 of embodiment 5, where (a) is a plan view of the odor sensor 100 and (b) is a cross-sectional view taken along line AA in (a). The odor sensor 100 of embodiment 5 has multiple sensor elements 110 and a substrate (silicon substrate) 120. The sensor element 110 has an adsorption film 112, a detection unit 114, and an electrode 116.
[0064] Here, the odor sensor 100 corresponds to the odor sensor 1 of embodiment 1, the substrate 120 corresponds to the substrate 2 of embodiment 1, the adsorption film 112 corresponds to the adsorption film 6 of embodiment 1, and the detection unit 114 corresponds to the sensor layer 8 of embodiment 1. The electrode 116 does not directly correspond to the metal electrode 10 of embodiment 1, but is electrically connected to one of the multiple metal electrodes 10.
[0065] The odor sensor 100 in Fig. 12 has, for example, nine sensor elements 110a to 110i. Specifically, the sensor element 110a has an adsorption film 112a, a detection unit 114a, and an electrode 116a, the sensor element 110b has an adsorption film 112b, a detection unit 114b, and an electrode 116b, ..., and the sensor element 110i has an adsorption film 112i, a detection unit 114i, and an electrode 116i. Note that when the sensor element (adsorption film, detection unit, electrode) is not specified, the suffixes a to i (including j to l described later) of the reference numerals are omitted. The adsorption film 112 is a film that adsorbs odor substances, and will be described in detail later.
[0066] The detection unit 114 detects a change in the adsorption state (also called the adsorption characteristics) caused by the adsorption of an odorant to the adsorption film 112. Note that the term "adsorption of an odorant to the adsorption film 112" includes not only the adsorption of an odorant to the surface of the adsorption film 112, but also the absorption of an odorant into the interior of the adsorption film 112. Here, the change in the adsorption state caused by the adsorption of an odorant to the adsorption film 112 includes changes in mechanical characteristics, optical characteristics, or electrical characteristics caused by the odorant. The detection unit 114 outputs the change in the adsorption state of the adsorption film 112, for example, as a signal. That is, the detection unit 114 also functions as a signal conversion unit (transducer).
[0067] "Changes in mechanical properties" include, for example, changes in resonance frequency in a quartz crystal oscillator (QCM), changes in the speed of surface acoustic waves, and changes in the expansion / contraction or deflection of a film in a piezoelectric element. "Changes in optical properties" include changes in absorption wavelength, absorbance, fluorescence / luminescence properties, and refractive index in surface plasmon resonance (SPR) elements, etc. "Changes in electrical properties" include, for example, changes in properties such as electrical conductivity, resistance, dielectric constant, and electrochemical impedance in charge-coupled devices, changes in redox potential in oxide semiconductor sensors, and changes in gate voltage, impedance, band gap, etc. in field-effect transistor (FET) sensors.
[0068] Examples of elements used in the detection unit 114 include the following elements (sensors): a quartz crystal oscillator sensor (QCM), a surface acoustic wave sensor, a field effect transistor (FET) sensor, a charge-coupled device sensor, a MOS field effect transistor sensor, an ion-selective field effect transistor (ISFET sensor), a metal oxide semiconductor sensor, an organic conductive polymer sensor, an electrochemical sensor, and the like. The elements used in the detection unit 114 are not particularly limited to these, and various elements can be used as appropriate depending on the purpose of use of the odor sensor 100, and the like. In addition, in the first to fourth embodiments, an ISFET sensor is applied as the odor sensor.
[0069] The "adsorption state of the odorant on the adsorption film 112" also includes, for example, the "amount of the odorant adsorbed on the adsorption film 112." An increase or decrease in the amount of the odorant adsorbed on the adsorption film 112 changes the mechanical, optical, or electrical properties of the adsorption film 112, and the detection unit 114 detects the amount of change to detect the adsorption state of the odorant on the adsorption film 112.
[0070] The electrode 116 can be formed of a predetermined conductive material. For example, an inorganic material or an organic material can be used as the predetermined conductive material. Inorganic materials include, for example, gold, silver, platinum, chromium, titanium, aluminum, nickel, nickel-based alloys, silicon, etc. Organic materials include, for example, nanocarbon materials such as polypyrrole, polyaniline, carbon, carbon nanotubes, and graphene.
[0071] The substrate 120 is, for example, flat and has a surface 120a and a surface 120b, with the sensor element 110 mounted on one surface 120a and the electrode 116 mounted on the other surface 120b (see FIG. 1(b)). For example, a silicon substrate, a substrate made of quartz crystal, a printed wiring substrate, a ceramic substrate, a resin substrate, or the like can be used as the substrate 120. The substrate 120 may also be a multilayer wiring substrate such as an interposer substrate.
[0072] <Sensor element> The odor sensor 100 shown in Fig. 12(a) has nine sensor elements 110a-110i arranged in 3 rows and 3 columns, but the number and arrangement (disposition) of the sensor elements 110 are not limited to this. In addition, the sensor element 110 shown in Fig. 1 has a one-to-one correspondence between the detection unit 114 and the adsorption film 112, but is not limited to this. Fig. 13 is a diagram showing another correspondence between the detection unit 114 and the adsorption film 112, where (a) is a plan view of the odor sensor 100 and (b) is a cross-sectional view taken along line BB in (a).
[0073] As shown in FIG. 13, one adsorption film 112j may correspond to three detection units 114a, 114d, and 114g, forming three sensor elements 110a, 110d, and 110g. Also, one adsorption film 112k may correspond to two detection units 114b and 114c, forming two sensor elements 110b and 110c. Furthermore, one adsorption film 112l may correspond to four detection units 114e, 114f, 114h, and 114i, forming four sensor elements 110e, 110f, 110h, and 110i. That is, one adsorption film 112 may be provided on n detection units 114 to form n sensor elements 110. Here, n is an integer equal to or greater than 1. Furthermore, one or more sensor elements 110 may be used as reference sensor elements 110 without forming an adsorption film 112 on the detection portion 114 .
[0074] <Odor data analysis device> 14 is a schematic diagram showing a schematic configuration of an odor data analysis device 200 of embodiment 5. The odor data analysis device 200 has the odor sensor 100 and an analysis unit 220 described above.
[0075] The analysis unit 220 is for analyzing the odor data F1 output from the odor sensor 100. The analysis unit 220 is mainly configured with a central processing unit (CPU) 220a, and may also have a storage device (memory) 220b. The memory 220b may be provided externally, separate from the analysis unit 220. The analysis unit 220 also has a data input / output port 220c. The input / output port 220c has a function of receiving the odor data F1 from the odor sensor 100, and a function of transmitting the calculated data R as a result of the calculation process performed by the CPU 220a to a control unit (not shown). The control unit (not shown) may be a control unit of an external device, such as a personal computer, to which the odor data analysis device 200 is connected via a known communication means, either wired or wirelessly.
[0076] An analysis program P for analyzing the odor data F1 is stored in the memory 220b. This analysis program P causes the analysis unit 220 as a computer, i.e., the CPU 220a as the main component of the analysis unit 220, to execute known arithmetic processing, thereby analyzing the odor data F1. Note that although the data analysis device 200 in FIG. 3 has one odor sensor 100, it may have multiple odor sensors 100.
[0077] The adsorption film 112 of the fifth embodiment may be made of a material having electrical conductivity, or may be made of an ionically conductive material containing a mixture of a non-conductive material and an ionically conductive material. Here, the plurality of sensor elements 110 may be made of materials having different electrical conductivity. The plurality of sensor elements 110 may each have an adsorption film 112 containing a mixture of different ionically conductive materials. The plurality of sensor elements 110 may each have an adsorption film 112 containing a mixture of different non-conductive materials. The plurality of sensor elements 110 may each have an adsorption film 112 containing a mixture of different non-conductive materials and different ionically conductive materials. Furthermore, the plurality of sensor elements 110 may each have an adsorption film 112 containing the same mixture.
[0078] <Conductive materials> The conductive material may be, for example, a π-electron conjugated polymer. The π-electron conjugated polymer may be, but is not limited to, a polymer material having a so-called π-electron conjugated polymer skeleton, such as polypyrrole and its derivatives, polyacetylene and its derivatives, polyaniline and its derivatives, polythiophene and its derivatives, polyacetylene and its derivatives, polyazulene and its derivatives, or polyimide and its derivatives.
[0079] When the π-electron conjugated polymer is in an oxidized state and the backbone polymer itself is a cation, it is possible to make the polymer conductive by incorporating an anion as a dopant. Note that in the present invention, a neutral π-electron conjugated polymer having no dopant may also be selected as the adsorption film 112.
[0080] When using a π-electron conjugated polymer having a dopant, various substances can be used as the dopant. Examples of the dopant include inorganic ions such as chloride ions, chlorine oxide ions, bromide ions, sulfate ions, nitrate ions, and borate ions, organic acid anions such as alkylsulfonic acid, benzenesulfonic acid, and carboxylic acid, and polymer acid anions such as polyacrylic acid and polystyrenesulfonic acid.
[0081] In addition to the above, a method of doping in a chemical equilibrium manner by coexisting an ionic compound containing both cations and anions, such as an ionic liquid or an inorganic salt, with a neutral π-electron conjugated polymer can also be used. The type of ionic liquid or salt is not particularly limited, but for example, a material consisting of a combination of the following anions and cations can be used.
[0082] Possible anions include halide ions such as chloride ion, bromide ion, and iodide ion, chlorine oxide ion, sulfate ion, nitrate ion, borate ion, tetrachloroferrate(III) ion, tetrafluoroborate ion, hexafluorophosphate ion, hexafluoroantimonate ion, alkylsulfonate ion, alkylphosphate ion, alkylphosphinate ion, alkylphosphonate ion, alkyldithiophosphate ion, thiocyanate ion, alkylsulfate ion, aromatic sulfonate ions such as benzenesulfonic acid, carboxylate ion, bis(perfluoroalkylsulfonyl)imide anion, dicyanamide anion, and tricyanomethanide anion.
[0083] Possible cations include metal ions such as sodium and potassium ions, ammonium ions, alkylammonium ions, alkylphosphonium ions, alkylimidazolium ions, alkylpyridinium ions, alkylpiperidinium ions, alkylpiperazinium ions, alkylmorpholinium ions, alkylpyrrolidinium ions, and alkylsulfonium ions.
[0084] <Ion conductive materials> The non-conductive material used in the ionically conductive material includes a non-conductive (i.e. insulating) solid material. The non-conductive solid material is, for example, a non-conductive material that can contain a different material therein, such as a non-conductive solid matrix base material. The non-conductive solid matrix base material includes, for example, a resin, a porous material, or a low-molecular-weight self-organizing material. The resin includes a general-purpose resin, such as polyvinyl chloride (PVC), polyvinylidene fluoride (PVDF), polymethyl methacrylate (PMMA), cycloolefin polymer (COP), etc.
[0085] Examples of the porous material include microporous materials, mesoporous materials, and macroporous materials. Microporous materials include activated carbon, zeolite, metal organic frameworks (MOFs), etc. Mesoporous materials include silica, etc. Macroporous materials include pumice, etc.
[0086] Furthermore, when referring to a low molecular weight self-organizing material, the term "low molecular weight" refers to a molecule composed of, for example, several to about 100 atoms. A "self-organizing material" refers to a material in which, for example, molecules, atoms, or particles spontaneously assemble to form a regular arrangement. Low molecular weight self-organizing materials include, for example, self-assembled monolayers (SAMs), liquid crystal molecular materials, organic crystals, and the like. SAMs include, for example, organic silane compounds, thiols (R-SH), phosphonic acids (R-PO3H2), and the like.
[0087] The ionic material is a material that allows the movement of ions inside the adsorption film 112. The ionic material is, for example, an ionic liquid or a salt that includes an ionic liquid or a plasticizer in which a salt is dissolved, and is composed of a combination of an anion and a cation as shown below.
[0088] Possible anions include, for example, halide ions such as chloride ions, bromide ions, and iodide ions, chlorine oxide ions, sulfate ions, nitrate ions, borate ions, tetrachloroferrate(III) ions, tetrafluoroborate ions, hexafluorophosphate ions, hexafluoroantimonate ions, alkylsulfonate ions, alkylphosphate ions, alkylphosphinate ions, alkylphosphonate ions, alkyldithiophosphate ions, thiocyanate ions, and alkylsulfate ions; aromatic sulfonate ions such as benzenesulfonic acid; carboxylate ions, bis(perfluoroalkylsulfonyl)imide anions, dicyanamide anions, and tricyanomethanide anions.
[0089] Further, examples of cations that may be considered include metal ions such as sodium and potassium ions, ammonium ions, alkylammonium ions, alkylphosphonium ions, alkylimidazolium ions, alkylpyridinium ions, alkylpiperidinium ions, alkylpiperazinium ions, alkylmorpholinium ions, alkylpyrrolidinium ions, and alkylsulfonium ions.
[0090] The ionically conductive material is an organic liquid material in which the above-mentioned ionic liquid or salt is dissolved. Examples of the organic liquid material include plasticizers such as nitrophenyl alkyl ether, dialkyl phthalate, trialkyl trimellitate, dialkyl sebacate, dialkyl adipate, and trialkyl phosphate. Furthermore, the ionically conductive material may include an ionically conductive inorganic glass material such as lithium orthosilicate.
[0091] The ion-conductive material may include an ion-conductive solid matrix base material. Examples of the ion-conductive solid matrix base material include polymer materials such as Nafion (registered trademark). When an ion-conductive solid matrix base material is used as the ion-conductive material, the adsorption film 112 may not include a mixture with a resin as a non-conductive material. When an ion-conductive solid matrix base material is used as the ion-conductive material, the adsorption film 112 may include a mixture with a non-conductive solid matrix base material.
[0092] An additive (dopant) may be further added to the mixture of the non-conductive material and the ion-conductive material in the adsorption film 112. The additive is not limited to one type, and multiple types of additives may be added to the adsorption film 112. The adsorption state of the odorant of the adsorption film 112 can be changed depending on the type and amount of additive.
[0093] The additive includes, for example, an inorganic ion. The inorganic ion may be selected from the group consisting of, for example, chloride ion, chlorine oxide ion, bromide ion, sulfate ion, nitrate ion, and borate ion. The additive includes an organic acid anion. The organic acid anion may be selected from the group consisting of alkylsulfonic acid, benzenesulfonic acid, and carboxylic acid. The additive includes, for example, a polymer acid anion. The polymer acid anion includes polyacrylic acid or polystyrenesulfonic acid. The additive includes a salt. Other possible additives include host materials such as cyclodextrin and crown ether derivatives, organic base materials such as alkylamines, arylamines, and nitrogen-containing heterocyclic compounds, and hydrogen-bonding materials such as urea derivatives and thiourea derivatives.
[0094] <Adsorption film manufacturing process> The method for producing the adsorption film 112 includes a mixing step, a film forming step, and a drying step. When a conductive material is used as the adsorption film 112, the mixing step includes a first adjustment step of adjusting a solution of a π-electron conjugated polymer or a monomer solution thereof, and a second adjustment step of adjusting a solution of a dopant such as an ionic liquid or a salt. When an ionically conductive material is used as the adsorption film 112, the mixing step includes a first adjustment step of adjusting a solution of a non-conductive material, and a second adjustment step of adjusting a solution of a dopant or an ionically conductive material. The first and second adjustment steps are independent steps. The mixing step includes a third adjustment step of adjusting a mixture solution (hereinafter referred to as a mixture solution) obtained by mixing the solution adjusted in the first adjustment step with the solution adjusted in the second adjustment step. Here, when a conductive material is used as the adsorption film 112, the content of the dopant in the π-electron conjugated polymer may be adjusted to a range of 0.01 to 5, preferably 0.1 to 2, assuming that a state in which one dopant unit (ion) is included per two repeating units constituting the π-electron conjugated polymer is 1. Furthermore, when an ionically conductive material is used as the adsorption film 112, 90 parts by weight of the non-conductive material and 10 parts by weight of the ionically conductive material are mixed, assuming that the mixture solution is 100 parts by weight. The non-conductive material is preferably mixed in the range of 50 to 95 parts by weight, and the ionically conductive material is preferably mixed in the range of 5 to 50 parts by weight.
[0095] The film forming step includes a dropping step of dropping the mixture solution prepared in the mixing step onto the surface of the detection unit 114 using, for example, a microdispenser. Note that the film forming step may include a coating step of coating the mixture solution onto the surface of the detection unit 114 by, for example, inkjet.
[0096] In the drying step, the mixture solution that has been dropped or applied to the surface of the detection unit 114 in the film forming step is dried. In the drying step, the mixture solution is dried in an environment with an atmospheric pressure of 1 bar, a temperature of 25° C., and a humidity of 50%, for example. Note that the atmospheric pressure, temperature, and humidity are not limited to these values.
[0097] When a self-organizing material such as SAM is used as the non-conductive material, a film (SAM) of the self-organizing material may be formed on the surface of the detection unit 114 (film formation step), and the formed film may be made to carry an ion-conductive material (support step). This makes it possible to impart ion conductivity to the adsorption film 112 even when a self-organizing material is used.
[0098] When an additive is added, the third adjustment step of the method for producing the adsorption film 112 includes an addition step of adding the additive to the mixture solution. Here, assuming that the mixture solution is 100 parts by weight, for example, 10 parts by weight of the additive is added. It is preferable that the additive is added in the range of 1 part by weight to 20 parts by weight. The additive may be added in the first adjustment step, or in the second adjustment step. Furthermore, the method for producing the adsorption film 112 may include an addition step after the film formation step, and the additive may be added to the film of the mixture solution formed on the surface of the detection unit 114 in the film formation step.
[0099] [Embodiment 6] The odor sensor according to the sixth embodiment will be described below.
[0100] <Configuration of the odor sensor> In the odor sensor, an adsorption film that adsorbs a specific odor substance is formed on the surface of the base. The adsorption film is formed by adding an additive to a film material such as a conductive polymer film. Note that the base here is a concept that includes the substrate 2 as the base part described in the first embodiment and the sensor layer 8.
[0101] A quartz crystal microbalance sensor (QCM) can also be used as the base. Other examples of sensors that can be used as the base include surface acoustic wave sensors, field effect transistors (FETs), charge-coupled device sensors, MOSFET sensors, ISFET sensors, metal oxide semiconductor sensors, organic conductive polymer sensors, electrochemical sensors, piezoelectric element sensors, and SPR sensors. Depending on the type of sensor used as the base, the physical quantities that make up the odor data F1 can include frequency, electric potential, mass, wavelength and intensity of light or sound, resistance, and current.
[0102] As the film material constituting the adsorption film, for example, conductive polymers such as polyaniline, polypyrrole, polythiophene, etc. can be used. Note that the film material can also be the ionic liquid, general-purpose resin, plasticizer, salt, etc. described in the first embodiment. In addition, inorganic materials such as gold, silver, platinum, chromium, titanium, aluminum, nickel, nickel-based alloys, silicon, etc. can be used for the electrodes. In addition, nanocarbon materials such as carbon, carbon nanotubes, graphene, etc. can be used.
[0103] As the additive, for example, inorganic ions, organic acid anions, and polymeric acid anions can be applied. As the inorganic ions, for example, chloride ions, chlorine oxide ions, bromide ions, sulfate ions, nitrate ions, and borate ions can be considered. As the organic acid anions, for example, alkylsulfonic acid, benzenesulfonic acid, and carboxylic acid can be considered. As the polymeric acid anions, for example, organic acid anions such as alkylsulfonic acid, benzenesulfonic acid, and carboxylic acid, and polymeric acid anions such as polyacrylic acid and polystyrenesulfonic acid can be considered. As the additive, other host materials such as cyclodextrin and crown ether derivatives, organic base materials such as alkylamines, arylamines, and nitrogen-containing heterocyclic compounds, and hydrogen bond materials such as urea derivatives and thiourea derivatives can be considered. In addition, various ionic liquids listed in the fifth embodiment can also be additives.
[0104] <Odor sensor array> The odor sensor can be used by arranging multiple adsorption membranes on the surface of one or multiple bases. In this case, for example, multiple different adsorption membranes each having a specific adsorption property for a different odor substance can be arranged in a line. Also, multiple adsorption membranes can be arranged vertically and horizontally in a planar array.
[0105] By using information on the order in which the adsorption films have the specific adsorption characteristics as an encryption key or passcode, security can be improved in various situations. This odor sensor or the entire system including it can be used as a security system that uses odors.
[0106] <Odor database concealment processing> 15 is a schematic diagram of an odor sensor unit 1010 according to a sixth embodiment. The odor sensor unit 1010 has five odor sensors 1010a to 1010e. The odor sensors 1010a to 1010e use, for example, a quartz crystal microbalance sensor (QCM) as the base 1002. In the second embodiment, the five odor sensors 1010a to 1010e are sequentially arranged in a row. Adsorption films 1004a to 1004e are formed on the surfaces of the five bases 1002, respectively, and the adsorption films 1004a to 1004e correspond to the odor sensors 1010a to 1010e, respectively. The adsorption films 1004a to 1004e are formed by adding additives 1006a to 1006e to a conductive polymer film 1005, respectively. Due to the differences in the properties of the additives 1006a to 1006e, the adsorption films 1004a to 1004e each exhibit the adsorption properties of adsorbing a different odor substance.
[0107] Assume that the odors of three types of gases Ga, Gb, and Gc are detected by this odor sensor 1010 and stored in database DB1. The detection results when the gases Ga, Gb, and Gc are detected by the odor sensors 1010a to 1010e are, for example, as follows. The values in parentheses are the output values of the odor sensors 1010a to 1010e, respectively. Gas Ga: (0,5,10,5,0) Gas Gb: (2,4,6,8,10) Gas Gc: (10, 8, 6, 4, 2) If these output values are stored as is in the odor database DB (not shown), then if the information in the odor database DB is stolen, the detection results of the gases Ga-Gc by the odor sensors 1010a-1010e will be easily revealed to the pirate. However, for example, the arrangement order of the output values of the five odor sensors 1010a-1010e is changed, and the output values from the odor sensors 1010a-1010e are stored in the odor database DB in the changed arrangement order. If the information on the changed order is then managed separately from the odor database DB as an encryption key, then even if the information in the database DB is stolen, the pirate will not be able to easily grasp the detection results of the gases Ga-Gc by the odor sensors 1010a-1010e.
[0108] For example, if the output values of the five odor sensors 1010a to 1010e are arranged in the order of (1, 3, 5, 2, 4), the detection results of the gases Ga to Gc stored in the odor database DB will be as follows. Gas Ga: (0,10,0,5,5) Gas Gb: (2,6,10,4,8) Gas Gc: (10,6,2,8,4) Without the encryption key, the detection results of the gases Ga-Gc by the odor sensors 1010a-1010e cannot be reproduced in the correct sensor order. Here, by using the encryption key (1, 3, 5, 2, 4), the detection results of the gases Ga-Gc in the odor database DB can be decrypted in the correct sensor order of the odor sensors 1010a-1010e. This measure improves the security of the odor data stored in the odor database DB.
[0109] Also, for example, the order of the sensor arrangement in an odor sensor unit for detecting odor data to be stored in the odor database DB and the order of the sensor arrangement in an odor sensor unit to be sold to users can be changed, and the changed content can be used as an encryption key. Furthermore, when multiple odor sensor units are produced, changing the sensor arrangement in the unit for each unit or for each multiple lots, and managing the changed content as an encryption key can further contribute to improving the confidentiality of odor data.
[0110] <Entrance and exit management using scent> By using the odor sensor unit 1010 shown in FIG. 15, for example, it is possible to realize entrance / exit management using odors. Locking and unlocking for entrance / exit is performed using gas that has a specific odor. Here, the odor used for entrance / exit is called an "odor key." The odor key may be, for example, a specific perfume or an individual's body odor. If the odor sensor unit 1010 is linked to an entrance / exit control system that controls the locking and unlocking of a room door, it is possible to unlock the door using the odor key.
[0111] Here, for example, the door cannot be unlocked by the smell key alone, and the sensor array information in the smell sensor unit 1010 must be input as a passcode to finally unlock the door. For example, the detection result that can unlock the door is (2, 4, 6, 8, 10), and this information is stored in a database or the like in the entrance / exit control system or in the cloud. If the detection result of the smell key by the smell sensor unit 1010 is (2, 6, 10, 4, 8), the door cannot be unlocked. However, when the sensor array information (1, 3, 5, 2, 4) in the smell sensor unit 1010 is input, the detection result of (2, 6, 10, 4, 8) is converted to (2, 4, 6, 8, 10). The converted detection result is compared with the detection result stored in the database or the like, and if they match, the door can be unlocked.
[0112] <Industrial Applicability> In addition, by using the odor sensor described in the above embodiment and the method for analyzing odor data detected by the odor sensor, it is possible to quickly and accurately identify the odor substance contained in a gas containing multiple different odor substances. It is also possible to reduce the load on the arithmetic processing device. Even when discriminating between the odor of a specific gas and another gas, it is possible to quickly and accurately discriminate between the two. In addition, even when identifying an odor substance contained in a detected gas by comparing the detected odor data with odor data stored in a database or the like, it is possible to quickly and accurately compare the detected odor data. In addition, the odor sensors 1010a to 1010e of embodiment 2 can be replaced with the odor sensor 100 of embodiment 1.
[0113] Although the preferred embodiments of the present invention have been described above, the present invention is not limited to these, and various modifications and changes are possible within the scope of the gist of the present invention. For example, the present invention includes the following gist.
[0114] [Objective 1] A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A metal electrode formed on the front surface side of the silicon substrate, the adsorption film is formed on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer, An odor sensor, wherein the sensor layer is formed on the surface side of the protective layer without being embedded in the protective layer.
[0115] [Objective 2] The sensor layer may be formed on a surface side of the protective layer, and the metal electrode may be formed on the surface side of the protective layer but not on the surface of the sensor layer.
[0116] [Objective 3] The thickness of the adsorption film may be in the range of 1 nm to 2 μm.
[0117] [Objective 4] The thickness of the metal electrode may be 20 times or less than the thickness of the adsorption film.
[0118] [Objective 5] The metal electrode may have a thickness of 1 μm or less.
[0119] [Objective 6] The difference in thickness between the surface of the sensor layer and the surface of the metal electrode may be 1 μm or less.
[0120] [Objective 7] The sensor layer may be made of tantalum pentoxide.
[0121] [Objective 8] The material of the protective layer may be silicon nitride or glass.
[0122] [Objective 9] The sensor layer is formed on a front surface side of the silicon substrate, The metal electrodes are formed on a front surface side of the silicon substrate, The plurality of metal electrodes may be arranged to sandwich or surround the plurality of sensor layers.
[0123] [Objective 10] The distance between the plurality of metal electrodes may be equal to or greater than the size of the sensor layer.
[0124] [Objective 11] A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A method for manufacturing an odor sensor having a metal electrode formed on the front surface side of the silicon substrate, comprising the steps of: a protective layer forming step of forming the protective layer on a surface of the silicon substrate; a sensor layer forming step of forming the sensor layer on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer after the protective layer forming step; a metal electrode forming step of forming the metal electrode at a position on a surface side of the protective layer, which is not a surface side of the sensor layer, after the sensor protective layer forming step; A method for manufacturing an odor sensor, comprising: forming an adsorption film on the surface side of the sensor layer after the metal electrode forming step. [Explanation of symbols]
[0125] 1, 21, 31, 41, 51, 100: Odor sensor 2, 120: Silicon substrate 2a: surface 4:Protective layer 6, 112, 112a~112l: Adsorption membrane 6a: Defective part 6b: Ultra-thin section 6c: Extra thick part 8, 8a: Sensor layer 10, 10a, 10b: Metal electrode 12: Contact point 14: Insulating layer 16:N well 110, 110a to 110i: sensor elements 114, 114a to 114i: detection unit 116: Electrode 120a, 120b: Surface 200: Data analysis equipment 220: Analysis Department 220b: Storage device (memory) 220c: Input / Output port F1: Scent data Ga~Gc: Gas H: Difference (height difference) P: Analysis program R: Calculated data
Claims
1. A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A metal electrode formed on the front surface side of the silicon substrate, the adsorption film is formed on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer, An odor sensor, wherein the sensor layer is formed on the surface side of the protective layer without being embedded in the protective layer.
2. 2. The odor sensor according to claim 1, wherein the sensor layer is formed on a surface side of the protective layer, and the metal electrode is formed on the surface side of the protective layer but not on the surface of the sensor layer.
3. 3. The odor sensor according to claim 1, wherein the adsorption film has a thickness in the range of 1 nm to 2 μm.
4. 3. The odor sensor according to claim 1, wherein the thickness of the metal electrode is 20 times or less than the thickness of the adsorption film.
5. 3. The odor sensor according to claim 1, wherein the metal electrode has a thickness of 1 μm or less.
6. 3. The odor sensor according to claim 1, wherein a difference in thickness between a surface of the sensor layer and a surface of the metal electrode is 1 μm or less.
7. 3. The odor sensor according to claim 1, wherein the sensor layer is made of tantalum pentoxide.
8. 3. The odor sensor according to claim 1, wherein the protective layer is made of silicon nitride or glass.
9. The sensor layer is formed in plurality on a front surface side of the silicon substrate, The metal electrodes are formed on a front surface side of the silicon substrate, The odor sensor according to claim 1 , wherein the plurality of metal electrodes are arranged to sandwich or surround the plurality of sensor layers.
10. The odor sensor according to claim 9 , wherein the distance between the plurality of metal electrodes is equal to or greater than the size of the sensor layer.
11. A flat silicon substrate; a protective layer formed on one of the front and back surfaces of the silicon substrate; An adsorption film formed on the front surface side of the silicon substrate, which adsorbs odorous substances contained in gas; a sensor layer formed on the front surface side of the silicon substrate, the sensor layer detecting the odor of the gas in response to the odor substance being adsorbed by the adsorption film; A method for manufacturing an odor sensor having a metal electrode formed on the front surface side of the silicon substrate, comprising the steps of: a protective layer forming step of forming the protective layer on a surface of the silicon substrate; a sensor layer forming step of forming the sensor layer on a surface side of the protective layer opposite to the silicon substrate as viewed from the protective layer after the protective layer forming step; a metal electrode forming step of forming the metal electrode on a surface side of the protective layer, the metal electrode being located at a position other than the surface of the sensor layer, after the protective layer forming step; a step of forming the adsorption film on the front surface side of the sensor layer, the step being subsequent to the step of forming the sensor layer and subsequent to the step of forming the metal electrode.
Citation Information
Patent Citations
Smell sensor and method for manufacturing smell sensor
JP2020008522A