Cover member and method for manufacturing the same

A three-layer cover member with adjustable additional layer dielectric constant and thickness maintains consistent radar transmission attenuation, addressing paint color variability and ensuring equipment accuracy.

JP2024162166AActive Publication Date: 2024-11-21TOYOTA JIDOSHA KK
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023077462
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-09
Publication Date
2024-11-21
Estimated Expiration
2043-05-09

AI Technical Summary

Technical Problem

The dielectric constant of a cover member varies with different paint colors, affecting the amount of transmission attenuation for radar equipment, which is inconsistent across vehicles with varying paint colors.

Method used

A cover member composed of three layers: a base material layer, a paint layer, and an additional layer, where the additional layer's dielectric constant and thickness are adjusted to maintain consistent transmission attenuation regardless of paint color.

Benefits of technology

Ensures consistent transmission attenuation across different paint colors, protecting radar equipment accuracy and reducing the need for design changes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162166000001_ABST
    Figure 2024162166000001_ABST
Patent Text Reader

Abstract

To provide a cover member that has the same degree of transmission and attenuation amount regardless of a paint color.SOLUTION: A cover member 10 arranged on a radio emission side of a radar instrument 20 is formed to include three layers of a base material layer 11, a painted layer 12 arranged on the base material layer on the opposite side of the radar instrument, and an addition layer 13. The addition layer is adjusted in its dielectric constant or thickness according to the type of the coated layer so that the amount of transmission and attenuation of radio waves radiated from the radar instrument performed by the cover member falls within a predetermined fixed range.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a cover member and a method for manufacturing the same. [Background technology]

[0002] Conventionally, there has been known a radar system having a millimeter wave radar device and a housing for protecting the millimeter wave radar device, with a part of the housing being formed from a resin sheet (Patent Document 1). In particular, in Patent Document 1, the resin sheet is formed so that the transmittance of the millimeter wave increases or decreases stepwise from both ends toward the center in the thickness direction in order to suppress the reflection of the millimeter wave at the resin sheet and increase the transmittance of the millimeter wave. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2021-162576 A Summary of the Invention [Problem to be solved by the invention]

[0004] In some cases, a cover member that protects a radar device is painted. In such cases, the relative dielectric constant varies depending on the paint color, and therefore the transmission attenuation through the cover member may vary depending on the paint color.

[0005] However, even if the paint color is different, the same radar equipment is basically installed in the same type of vehicle, and therefore, in order to perform accurate measurements using the radar equipment and to eliminate the need to change the design for each paint color, it is preferable that the cover member has the same degree of transmission attenuation regardless of the paint color.

[0006] In view of the above problems, an object of the present disclosure is to provide a cover member having the same degree of transmission attenuation regardless of the paint color, and a manufacturing method thereof. [Means for solving the problem]

[0007] The gist of the present disclosure is as follows.

[0008] (1) A cover member disposed on a radio wave emitting side of a radar device, The radar device is formed so as to include three layers: a base layer, a coating layer disposed on the side of the base layer opposite to the radar device side, and an additional layer; The additional layer is a cover member whose relative dielectric constant or thickness is adjusted according to the type of the paint layer so that the amount of transmission attenuation of the radio waves emitted from the radar device through the cover member falls within a predetermined certain range. (2) The cover member according to (1) above, wherein the additional layer is disposed on the opposite side of the coating layer to the substrate layer. (3) The cover member according to (1) or (2) above, wherein the additional layer is formed as a resin sheet. (4) The cover member according to any one of (1) to (3) above, wherein the radar equipment is provided on a vehicle, and the certain range is the same range for each type of vehicle, regardless of the type of the paint layer. (5) A method for manufacturing a cover member disposed on a radio wave transmitting side of a radar device, comprising the steps of: The cover member is formed to include three layers: a base layer, a coating layer disposed on the side of the base layer opposite to the radar device side, and an additional layer; A manufacturing method in which the dielectric constant or thickness of the additional layer is adjusted according to the type of the paint layer so that the transmission attenuation of the radio waves of the radar device by the cover member falls within a predetermined certain range. Effect of the Invention

[0009] According to the present disclosure, a cover member having the same degree of transmission attenuation regardless of the paint color and a manufacturing method thereof are provided. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic diagram of a vehicle. [Diagram 2]FIG. 2 is a cross-sectional view of the periphery of the front grille taken along line II-II in FIG. [Diagram 3] FIG. 3 is a diagram showing changes in amplitude and wavelength of radio waves emitted from a radar device. [Figure 4] FIG. 4 is a diagram showing an example of parameters of each layer when different types of coating layers are formed on the same base layer. [Diagram 5] FIG. 5 is a diagram showing the relationship between the plate thickness and relative dielectric constant of the base layer and the transmission attenuation of radio waves through the base layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, the embodiments will be described in detail with reference to the drawings. In the following description, like elements are designated by like reference numerals.

[0012] <Vehicle configuration> First, with reference to Fig. 1 and Fig. 2, a vehicle 1 having a cover member 10 for a radar device 20 according to one embodiment will be described. Fig. 1 is a diagram showing a schematic diagram of the vehicle 1. Fig. 1(A) shows a perspective view of the vehicle 1, and Fig. 1(B) shows an enlarged view of a part of the front of the vehicle 1. The vehicle 1 may be an autonomous vehicle that is automatically driven without the driver's operation based on the measurement results by the radar device 20. Alternatively, the vehicle 1 may be a vehicle in which driving assistance is provided to the driver based on the measurement results by the radar device 20.

[0013] The vehicle 1 has a front grille 2 in front of it. As shown in Fig. 1(B), the front grille 2 has a lattice-like portion 3 for taking in air to cool heat-generating equipment (internal combustion engine, motor, etc.) of the vehicle 1, and a plate-like cover member 10 for covering a radar device 20 provided inside.

[0014] Fig. 2 is a cross-sectional view of the periphery of the front grill 2, taken along line II-II in Fig. 1. As shown in Fig. 2, the cover member 10 is disposed in front of the radar device 20 and on the outer side of the vehicle 1 relative to the radar device 20. The cover member 10 is disposed on the side where radio waves are emitted by the radar device 20, that is, on the passage path of the radio waves emitted by the radar device 20. The cover member 10 prevents the radar device 20 from being exposed to wind during travel, thereby protecting the radar device 20.

[0015] The radar device 20 is a device that measures the distance and direction to the surroundings by emitting radio waves to surrounding objects and measuring the reflected waves. The radar device 20 is, for example, a millimeter wave radar device. However, the radar device 20 may be a device using other types of radar, such as a microwave radar device or a LiDAR.

[0016] In this embodiment, the radar device 20 is disposed inside the front grill 2 of the vehicle 1. However, the radar device 20 may be disposed in other locations. Specifically, for example, the radar device 20 may be disposed inside the front bumper. In this case, the front bumper functions as a cover member. Also, for example, the radar device 20 may be disposed inside the rear bumper. In this case, the rear bumper functions as a cover member. In any case, as long as the cover member 10 is provided on the outside of the radar device 20, the radar device 20 may be disposed in any location.

[0017] <Configuration of cover material> Next, the configuration of the cover member 10 will be described with reference to FIG. 2. As can be seen from FIG. 2, the cover member 10 is formed to have at least three layers. In this embodiment, the cover member 10 has a base material layer 11, a paint layer 12, and an additional layer 13. In this embodiment, the base material layer 11, the paint layer 12, and the additional layer 13 are arranged in this order from the inside to the outside of the vehicle 1. Therefore, the paint layer 12 is arranged on the outside of the vehicle 1 relative to the base material layer 11, and the additional layer 13 is arranged on the outside of the vehicle relative to the paint layer 12. Therefore, the additional layer 13 is arranged on the opposite side of the paint layer 12 to the base material layer 11 side.

[0018] The base layer 11 is made of a material that is relatively strong and transmits radio waves radiated from the radar device 20. Specifically, the base layer 11 is made of a resin such as polypropylene or ABS. The base layer 11 is formed to have a thickness of, for example, 1 to 5 mm, or 1.5 to 3 mm. Particularly in this embodiment, the thickness of the base layer 11 is set so that the transmission attenuation of the radio waves radiated from the radar device 20 is small. The base layer 11 is formed by any molding technique such as injection molding.

[0019] The coating layer 12 is a layer of paint used to paint the vehicle 1. Therefore, the coating layer 12 contains pigments, resins, solvents, and additives. The coating layer 12 is formed to have a thickness of, for example, 0.01 to 0.5 mm, or 0.02 to 0.2 mm. The coating layer 12 is formed, for example, by spraying paint, which is the raw material of the coating layer, onto the base layer 11.

[0020] The additional layer 13 is a layer formed as a transparent sheet. The additional layer 13 is formed of a material that has a relatively high strength and transmits radio waves emitted from the radar device 20. Specifically, the additional layer 13 is formed of a resin such as polycarbonate or PET. In this embodiment, the additional layer 13 formed as a transparent sheet is attached onto the surface of the paint layer 12.

[0021] <Additional Layer Configuration> Next, the configuration of the additional layer 13, particularly the thickness and relative dielectric constant of the additional layer 13, will be described with reference to FIG. 3 and FIG.

[0022] Incidentally, the shape and material of the base material layer 11 of the cover member 10 are determined for each type of vehicle 1. Therefore, if the type of vehicle 1 is the same, the shape and material of the base material layer 11 are basically the same. Therefore, if the type of vehicle 1 is the same, the thickness and relative dielectric constant εr of the base material layer 11 are basically the same. On the other hand, the type of the paint layer 12 differs depending on the paint color of the vehicle 1. If the paint color differs, the components such as pigment, resin, solvent, and additives contained in the paint layer 12 differ, and therefore the relative dielectric constant εr of the paint layer 12 also differs. Therefore, if the type of paint layer 12 differs, the transmission attenuation in the portion of the cover member 10 including the base material layer 11 and the paint layer 12 differs.

[0023] In this embodiment, the dielectric constant or thickness of the additional layer 13 is adjusted according to the type of paint layer 12 so that the transmission attenuation of the radio waves emitted from the radar device 20 through the cover member 10 falls within a predetermined certain reference range. In this embodiment, the reference range is determined for each type of vehicle 1, and if the type of vehicle 1 is the same, the reference range is the same regardless of the type of paint layer. In particular, in this embodiment, the dielectric constant or thickness of the additional layer 13 is adjusted according to the type of paint layer 12 so that the transmission attenuation through the cover member 10 becomes a certain reference value determined for each type of vehicle 1 regardless of the type of paint layer 12.

[0024] Fig. 3 is a diagram showing changes in the amplitude and wavelength of radio waves radiated from the radar device 20. In the example shown in Fig. 3, the radar device 20 radiates radio waves with a wavelength λ and an amplitude A. The relative dielectric constant εr in the atmosphere is 1, and the dielectric tangent tanδ is 0. Therefore, the loss coefficient obtained by multiplying these is 0. Therefore, in the atmosphere, the power loss of the radio waves radiated from the radar device 20 is small.

[0025] Thereafter, when the radio waves radiated from the radar device 20 pass through the cover member 10, the wavelength λ' becomes shorter than the wavelength λ in the atmosphere because the relative dielectric constant is higher than that in the atmosphere. In addition, the dielectric tangent tan δ of the cover member 10 is also greater than 0, so the loss factor becomes greater than 0. For this reason, power loss occurs in the cover member 10 due to conversion to thermal energy in the radio waves radiated from the radar device 20, and the amplitude of the radio waves gradually decreases.

[0026] Thereafter, when the radio waves that had passed through the cover member 10 begin to pass through the atmosphere again, the wavelength returns to λ, but because power loss has occurred within the cover member 10, the amplitude A' at this time is smaller than the amplitude A before passing through the cover member 10. In other words, when only the power loss due to conversion to thermal energy within the cover member 10 is taken into consideration, the higher the relative dielectric constant of each layer constituting the cover member 10 and the thicker each layer constituting the cover member 10, the greater the power loss, and therefore the greater the transmission attenuation.

[0027] Fig. 4 is a diagram showing an example of parameters of each layer when different types of coating layers 12 are formed on the same base material layer 11. Fig. 4(A) to Fig. 4(C) show the case where the same base material layer 11 having a thickness of 2.25 mm and a relative dielectric constant εr of 2.7 is used.

[0028] In the example shown in FIG. 4(A), a coating layer 12 made of a first coating material is formed on the surface of a base layer 11. The relative dielectric constant εr of the first coating material is 4, and the thickness of the coating layer 12 is 0.03 mm. In addition, an additional layer 13 formed as a transparent sheet made of polycarbonate is formed on the surface of the coating layer 12. The relative dielectric constant of the additional layer 13 is 2.7, and the thickness of the additional layer 13 is 0.15 mm. As a result, the transmission attenuation of radio waves (millimeter waves) emitted from the radar device 20 by the cover member 10 thus formed coincides with a preset reference value (or falls within a reference range).

[0029] In the example shown in FIG. 4(B), a coating layer 12 made of a second coating material is formed on the surface of the base layer 11. The second coating material has physical properties different from those of the first coating material. In particular, the relative dielectric constant of the second coating material is different from that of the first coating material. Specifically, in this embodiment, the relative dielectric constant of the second coating material is 20. The thickness of the coating layer 12 is 0.03 mm.

[0030] In this embodiment, as described above, the additional layer 13 is configured so that the transmission attenuation of radio waves through the cover member 10 matches a reference value (or falls within a reference range). In particular, in the example shown in FIG. 4(B), the thickness of the additional layer 13 is changed from the thickness of the additional layer 13 in the example shown in FIG. 4(A). Specifically, the thickness of the additional layer 13 is reduced by the amount corresponding to the increase in the relative dielectric constant of the coating layer 12 and the increase in the loss factor. In the example shown in FIG. 4(B), the thickness of the additional layer 13 is set to 0.05 mm, which causes the transmission attenuation of radio waves through the cover member 10 to match the reference value.

[0031] In the example shown in FIG. 4(C), a coating layer 12 made of a second coating material is formed on the surface of the base layer 11, similarly to the example shown in FIG. 4(B). In the example shown in FIG. 4(C), the relative dielectric constant of the additional layer 13 is changed from the relative dielectric constant of the additional layer 13 in the example shown in FIG. 4(A). Specifically, the relative dielectric constant of the coating layer 12 is increased, and the loss factor is increased, so that the relative dielectric constant of the additional layer 13 is reduced accordingly. In the example shown in FIG. 4(C), the relative dielectric constant of the additional layer 13 is set to 2.2, so that the transmission attenuation of radio waves by the cover member 10 coincides with the reference value. The relative dielectric constant of the additional layer 13 is adjusted, for example, by changing the components of the additive mixed into the resin material.

[0032] According to this embodiment, as described above, by adjusting the thickness or relative dielectric constant of the additional layer 13 of the cover member 10, the transmission attenuation of radio waves through the cover member 10 can be made to match a reference value or fall within a reference range even if the type of paint layer 12 is changed. In particular, in this embodiment, the additional layer 13 is configured as a resin tape that is applied after painting of the vehicle 1 is completed, so that the transmission attenuation of radio waves through the cover member 10 can be adjusted simply by changing the resin tape that is applied depending on the type (paint color, etc.) of the paint layer 12.

[0033] In the above embodiment, the relative dielectric constant and the thickness of the additional layer 13 are adjusted so that the transmission attenuation of radio waves through the cover member 10 coincides with a reference value or falls within a reference range. However, other parameters such as the dielectric tangent tan δ may also be adjusted at the same time.

[0034] In the above embodiment, only the attenuation due to conversion to thermal energy when radio waves pass through the cover member 10 is considered. However, when radio waves pass through the cover member 10, the attenuation amount changes due to mutual interference caused by the influence of the reflection of radio waves at interfaces (the interface between the air and the base layer 11, the interface between the base layer 11 and the coating layer 12, the interface between the coating layer 12 and the additional layer 13, and the interface between the additional layer 13 and the air). Specifically, if the phase of the radio waves reflected an even number of times at the interface is close to the same phase, the attenuation is small, and if the phase of the radio waves reflected an even number of times at the interface is close to the opposite phase, the attenuation is large. The phase and strength of the reflected wave at this time change depending on the thickness of each layer and the ratio of the relative dielectric constants at the interface. Therefore, the relative dielectric constant and thickness of the additional layer 13 may be set in consideration of not only the attenuation due to conversion to thermal energy but also the attenuation due to mutual interference caused by reflection.

[0035] According to this embodiment, the additional layer 13 formed as a transparent sheet is disposed on the opposite side of the coating layer 12 from the substrate layer 11, that is, on the outside of the coating layer 12. By providing a transparent sheet on the coating layer 12 in this manner, damage to the coating layer 12 is suppressed. In particular, if the additional layer 13 is not provided, it is assumed that the user will repair the coating layer 12 by themselves if the coating layer 12 is partially peeled off due to chipping or scratches. However, if the user repairs it by himself, the transmission attenuation will change because a material with an appropriate relative dielectric constant is not used, and the measurement accuracy of the radar device 20 will decrease. By providing the additional layer 13, which is a transparent sheet, damage to the coating layer 12 is suppressed, and the change in the transmission attenuation caused by the user's own repair can be suppressed.

[0036] According to the present embodiment, the additional layer 13 is formed as a resin sheet. Therefore, the additional layer 13 is easily produced by attaching a resin sheet onto the surface of the paint layer 12 according to the type (paint color) of the paint layer.

[0037] <Cover member manufacturing procedure> Next, a manufacturing procedure for the cover member 10 will be briefly described.

[0038] In manufacturing the cover member 10, first, the base material layer 11 is produced. The base material layer 11 is produced by a general molding method such as injection molding. FIG. 5 is a diagram showing the relationship between the plate thickness and relative dielectric constant εr of the base material layer 11 and the transmission attenuation of radio waves through the base material layer 11. As shown in FIG. 5, the transmission attenuation of radio waves through the base material layer 11 varies depending on the plate thickness and relative dielectric constant εr of the base material layer 11. For example, in the example shown in FIG. 5, when the base material layer 11 is formed from a material with a relative dielectric constant of 2.7 (broken line in the figure), the plate thickness of the base material layer 11 is set to about 2.4 mm so as to have a small transmission attenuation while maintaining the necessary strength.

[0039] Once the base layer 11 is produced, the front surface of the base layer 11 is painted to form the paint layer 12. The paint layer 12 is formed, for example, by spraying paint onto the surface of the base layer 11. Painting is performed with different paint for each body color of the vehicle 1, and thus different types of paint layers 12 are formed.

[0040] Once the paint layer 12 is formed, the additional layer 13 is formed by attaching a transparent sheet to the paint layer 12. As described above, the thickness and relative dielectric constant of the transparent sheet are selected so that the transmission attenuation of radio waves through the finally formed cover member 10 is a reference value (or within a reference range). The transparent sheet is attached onto the paint layer 12 by any transparent adhesive.

[0041] As described above, according to the present manufacturing method, the cover member 10 is formed to include three layers: the base layer 11, the paint layer 12, and the additional layer 13. In the present manufacturing method, the relative dielectric constant and thickness of the additional layer are adjusted according to the type of paint layer 12 so that the transmission attenuation of the radio waves from the radar device 20 by the cover member 10 falls within a predetermined range.

[0042] Although the preferred embodiments according to the present disclosure have been described above, the present disclosure is not limited to these embodiments, and various modifications and changes can be made within the scope of the claims. [Explanation of symbols]

[0043] 1 vehicle 10 Cover member 11 Base material layer 12 Paint Layer 13 Additional layers 20 Radar Equipment

Claims

1. A cover member disposed on a radio wave emission side of a radar device, The radar device is formed so as to include three layers: a base layer, a coating layer disposed on the side of the base layer opposite to the radar device side, and an additional layer; The additional layer is a cover member whose relative dielectric constant or thickness is adjusted according to the type of the paint layer so that the amount of transmission attenuation of the radio waves emitted from the radar device through the cover member falls within a predetermined certain range.

2. The cover member according to claim 1 , wherein the additional layer is disposed on the opposite side of the coating layer to the substrate layer.

3. The cover member according to claim 1 or 2, wherein the additional layer is formed as a resin sheet.

4. 3. The cover member according to claim 1, wherein the radar device is provided on a vehicle, and the certain range is the same for each type of vehicle, regardless of the type of the paint layer.

5. A method for manufacturing a cover member disposed on a radio wave transmitting side of a radar device, comprising the steps of: The cover member is formed to include three layers: a base layer, a coating layer disposed on the side of the base layer opposite to the radar device side, and an additional layer; A manufacturing method in which the dielectric constant or thickness of the additional layer is adjusted according to the type of the paint layer so that the transmission attenuation of the radio waves of the radar device by the cover member falls within a predetermined certain range.

Citation Information

Patent Citations

  • Radome for radar sensor of motor vehicle and motor vehicle

    CN112751186A

  • Automobile ornament of back-mounted seamless integrated millimeter wave radar

    CN115723684A

  • Pressure-sensitive adhesive tape for coating and coating method using pressure-sensitive adhesive tape for coating

    JP2001011403A

  • Molded product for vehicles

    JP2021113688A

  • Dielectric member, vehicular bumper, radar system, radio wave reflection prevention member and radio wave reflection prevention unit

    JP2021162483A