Power storage module

The power storage module design addresses productivity losses by using joined linear members to form spacer layers, reducing waste and maintaining efficiency in larger modules.

JP2024162815AInactive Publication Date: 2024-11-21TOYOTA INDUSTRIES CORP +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023078727
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-21
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing power storage modules, such as those described in Patent Document 1, suffer from decreased productivity due to high waste material rates when forming rectangular frame-shaped sealing layers by punching out sheet materials, which becomes more significant as the modules increase in size.

Method used

A power storage module design that includes a stacked body of electrodes with rectangular metal current collectors, surrounded by resin seals and spacer layers formed by joining linear members with a joining member, eliminating the need for punching out sheet materials into frame shapes, thereby reducing waste and maintaining productivity.

Benefits of technology

This design suppresses the increase in waste material rates, thereby maintaining or improving the productivity of the power storage module, especially as module size increases, while ensuring consistent sealing performance and reducing material costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162815000001_ABST
    Figure 2024162815000001_ABST
Patent Text Reader

Abstract

To provide a power storage module in which the decrease in productivity can be suppressed.SOLUTION: A power storage module includes a multilayer body in which a plurality of electrodes including a current collector are stacked, and a sealing part provided in a peripheral part of the current collector and made of resin. The sealing part includes a plurality of sealing layers in a rectangular frame shape and a plurality of spacer layers 33 in the rectangular frame shape. The sealing layers are bonded to a first surface and a second surface at the peripheral part of the current collectors in the electrodes. Each of the spacer layers 33 includes a plurality of linear members 41 existing between the sealing layers adjacent to each other in a stacking direction, sealing the inner space formed between the current collectors adjacent to each other in the stacking direction together with the sealing layers, disposed apart from each other when viewed from the stacking direction, and including a region extending linearly, and a bonding member 42 bonded to an edge 41a of the linear member 41 so as to fill the gap between the edges 41a of the adjacent linear members.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an energy storage module. [Background technology]

[0002] Patent Document 1 discloses a bipolar battery. This bipolar battery has a bipolar electrode in which a positive electrode is provided on one side of a current collector and a negative electrode is provided on the other side, a gel electrolyte sandwiched between the positive electrode and the negative electrode, and a seal layer that surrounds the periphery of a unit cell composed of the positive electrode, the negative electrode, and the gel electrolyte and is provided between the current collectors. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2004-158343 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the battery (electricity storage module) disclosed in Patent Document 1, the current collector is made of a rectangular metal foil, and a rectangular frame-shaped sealing layer made of resin is provided on the periphery of this current collector. The rectangular frame-shaped sealing layer is formed, for example, by punching out a long sheet material unwound from a raw material roll into a rectangular frame shape. However, when the sealing layer is formed by punching out the sheet material, the waste rate of the sheet material increases, and the productivity of the electricity storage module decreases. In particular, when the electricity storage module becomes large, the waste rate of the sheet material increases, and the decrease in productivity of the electricity storage module becomes more noticeable.

[0005] An object of the present disclosure is to provide an energy storage module that can suppress a decrease in productivity. [Means for solving the problem]

[0006] An energy storage module according to one embodiment of the present disclosure comprises a stack of multiple electrodes, each having a rectangular current collector, and a resin sealing portion provided on the peripheral portion of the current collector so as to surround the stack when viewed from the stacking direction of the multiple electrodes, each of the multiple electrodes having an active material layer on a first surface and a second surface opposite to the first surface of the current collector, the sealing portion including multiple rectangular frame-shaped sealing layers and multiple rectangular frame-shaped spacer layers, the multiple sealing layers being joined to the first surface and the second surface at the peripheral portion of the current collector of each of the multiple electrodes, each of the multiple spacer layers being located between adjacent sealing layers in the stacking direction and sealing an internal space formed between adjacent current collectors in the stacking direction together with the multiple sealing layers, and having a plurality of straight members arranged spaced apart from each other when viewed from the stacking direction, each having a region extending in a straight line, and a joining member joined to the edges so as to fill the gap between the edges of the adjacent straight members.

[0007] In the above energy storage module, each spacer layer included in the resin sealing portion is formed into a rectangular frame shape by joining the edges of linear members extending in a straight line with a joining member. Therefore, it is not necessary to punch out the long sheet material unwound from the original roll into a rectangular frame shape, and the sheet material can be easily used without waste. Such a spacer layer can prevent an increase in the waste rate of the sheet material. Therefore, a decrease in the productivity of the energy storage module can be prevented.

[0008] The joining member may be an injection molded member, and each of the spacer layers may include a welding layer formed at the joining portion between the joining member and the edge of the straight member, by which the joining member and the straight member melt together.

[0009] The joining member may be an injection molded member, and the melt flow rate of the joining member may be greater than the melt flow rate of the straight member.

[0010] When viewed from the stacking direction, the area of ​​the joint members may be smaller than the area of ​​the straight members.

[0011] The thickness of the joining member may be equal to or less than the thickness of the straight member.

[0012] The multiple straight members may include a pair of rectangular first straight members facing each other in a first direction when viewed from the stacking direction, and a pair of rectangular second straight members facing each other in a second direction perpendicular to the first direction when viewed from the stacking direction, and the joining member may join a region of the edge forming a long side of the first straight member and a region of the edge forming a short side of the second straight member.

[0013] The multiple straight members may include a pair of rectangular first straight members facing each other in a first direction when viewed from the stacking direction, and a pair of rectangular second straight members facing each other in a second direction perpendicular to the first direction when viewed from the stacking direction, and the joining member may join a region of the edge that forms a short side of the first straight member and a region of the edge that forms a short side of the second straight member.

[0014] The plurality of straight members may include a pair of straight members whose longitudinal directions coincide with each other when viewed from the stacking direction and that are adjacent to each other in the longitudinal direction. Effect of the Invention

[0015] According to the present disclosure, it is possible to provide an energy storage module that can suppress a decrease in productivity. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is a schematic plan view showing an example of an electricity storage module. [Diagram 2] FIG. 2 is a schematic cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3 is a schematic plan view showing the spacer layer. [Figure 4] FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. 5 is a flow chart illustrating a method of forming a spacer layer. [Figure 6]FIG. 6 is a schematic plan view for explaining a method of forming a spacer layer. [Figure 7] FIG. 7 is a schematic side view for explaining a method of forming a spacer layer. [Figure 8] FIG. 8 is a schematic plan view showing a spacer layer of a comparative example. [Figure 9] FIG. 9 is a schematic cross-sectional view taken along line IX-IX in FIG. [Figure 10] FIG. 10 is a schematic plan view showing a spacer layer according to a first modified example. [Figure 11] FIG. 11 is a schematic plan view showing a spacer layer according to the second modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, an embodiment of the present disclosure will be described in detail with reference to the accompanying drawings. In the description of the drawings, the same or equivalent elements are designated by the same reference numerals, and duplicated descriptions will be omitted. In the description, a Cartesian coordinate system defined by an X-axis, a Y-axis, and a Z-axis may be referred to.

[0018] (Embodiment) Fig. 1 is a schematic plan view of a power storage module according to this embodiment. The power storage module 11 shown in Fig. 1 can be used as a battery for various vehicles such as a forklift, a hybrid vehicle, and an electric vehicle. The power storage module 11 is a secondary battery such as a nickel-metal hydride secondary battery or a lithium-ion secondary battery. The power storage module 11 may be an electric double layer capacitor or an all-solid-state battery. Here, the case where the power storage module 11 is a lithium-ion secondary battery is shown.

[0019] FIG. 2 is a cross-sectional view taken along line II-II in FIG. 1, and shows a schematic layer configuration of the power storage module 11. The power storage module 11 is a single cell having a rectangular parallelepiped shape that is flattened in the Z-axis direction. In this embodiment, a bipolar lithium-ion secondary battery is shown as an example of the power storage module 11. The power storage module 11 includes an electrode laminate (laminate) 12 in which a plurality of electrodes are laminated, and a resin sealing portion 30. The plurality of electrodes include a plurality of bipolar electrodes 14. The stacking direction of the plurality of electrodes is along the Z-axis direction and coincides with the stacking direction of the power storage modules 11 in the module laminate in which the power storage modules 11 are stacked.

[0020] The bipolar electrode 14 includes a current collector 21, a positive electrode active material layer 22, and a negative electrode active material layer 23. The current collector 21 is a chemically inactive electrical conductor for continuing to pass electric current to the positive electrode active material layer 22 and the negative electrode active material layer 23 during discharging or charging of the lithium ion secondary battery.

[0021] The current collector 21 is a sheet-like conductive member having a rectangular shape in a plan view. The current collector 21 has a first surface 21a and a second surface 21b located on the opposite side of the first surface 21a. The current collector 21 is made of metal and is composed of, for example, a metal foil or an alloy foil. Examples of the metal foil include copper foil, aluminum foil, titanium foil, and nickel foil. Examples of the alloy foil include stainless steel foil (for example, SUS304, SUS316, SUS301, etc., as specified in JIS G 4305:2015), plated steel foil, and stainless steel foil. The alloy foil may be an alloy foil of the metals exemplified as the material of the metal foil. The current collector 21 may be formed by integrating or laminating a plurality of metal foils, or may be formed by plating another metal layer on the surface of one metal foil.

[0022] The current collector 21 in the illustrated example is formed by bonding an aluminum foil 21A and a copper foil 21B together such that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. The current collector 21 may be, for example, a clad foil formed by laminating and rolling an aluminum foil 21A and a copper foil 21B together. The current collector 21 may be a laminated foil. That is, the current collector 21 may be formed by bonding and integrating an aluminum foil 21A and a copper foil 21B together with a conductive adhesive resin (adhesive layer) such that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. The current collector 21 may be formed by copper vapor deposition or copper plating on one side of an aluminum foil such that the first surface 21a is an aluminum layer and the second surface 21b is a copper layer. In addition, the aluminum layer on the first surface 21a of the current collector 21 may be chromate-treated. Furthermore, the copper layer on the second surface 21b of the current collector 21 may be nickel-plated. In this case, the nickel-plated layer may be a roughened surface that is a protruding plated surface having fine protrusions on its surface. The roughened surface may be rougher than the unprocessed metal foil, and may be formed by roughening processing such as etching or electroplating. For example, the thickness of the current collector 21 may be about 30 μm to 150 μm, but is not limited thereto.

[0023] The positive electrode active material layer 22 is provided on a first surface 21a of the current collector 21. The current collector 21 and the positive electrode active material layer 22 provided on the first surface 21a of the current collector 21 constitute the positive electrode of the bipolar electrode 14. The positive electrode active material layer 22 is formed in a rectangular shape in the center of the first surface 21a so that the peripheral portion 21c of the current collector 21 is exposed.

[0024] The positive electrode active material layer 22 as an example is provided on the first surface 21a of the current collector 21 via an adhesive layer. For example, the adhesive layer may be formed of an adhesive such as acetylene black. The adhesive layer as an example may be provided on the entire surface of the first surface 21a of the current collector 21. Furthermore, the edge of the adhesive layer may be formed along the edge of the negative electrode active material layer 23 surrounding the positive electrode active material layer 22 as viewed from the stacking direction.

[0025] The positive electrode active material layer 22 is a layered member including a positive electrode active material, a conductive assistant, and a binder. Examples of the positive electrode active material include a composite oxide, metallic lithium, and sulfur. The composition of the composite oxide includes at least one of iron, manganese, titanium, nickel, cobalt, and aluminum, and lithium. Examples of the composite oxide include olivine-type lithium iron phosphate (LiFePO4), LiCoO2, and LiNiMnCoO2.

[0026] The binder serves to bind the active material or the conductive assistant to the surface of the current collector 21 and maintain the conductive network in the electrode. Examples of the binder include fluorine-containing resins such as polyvinylidene fluoride, polytetrafluoroethylene, and fluorine rubber, thermoplastic resins such as polypropylene and polyethylene, imide resins such as polyimide and polyamideimide, alkoxysilyl group-containing resins, acrylic resins containing monomer units such as acrylic acid and methacrylic acid, styrene-butadiene rubber (SBR), carboxymethyl cellulose, alginates such as sodium alginate and ammonium alginate, water-soluble cellulose ester crosslinked bodies, and starch-acrylic acid graft polymers. These binders can be used alone or in combination. Examples of the conductive assistant include acetylene black, carbon black, and graphite. The positive electrode active material layer 22 may contain a viscosity adjusting solvent such as N-methyl-2-pyrrolidone (NMP).

[0027] The negative electrode active material layer 23 is provided on the second surface 21b of the current collector 21. The current collector 21 and the negative electrode active material layer 23 provided on the second surface 21b of the current collector 21 constitute the negative electrode of the bipolar electrode 14. The negative electrode active material layer 23 is formed in a rectangular shape in the center of the second surface 21b so that the peripheral portion 21c of the current collector 21 is exposed. In one example, the positive electrode active material layer 22 is contained within the region of the negative electrode active material layer 23 when viewed from the stacking direction. In other words, the outer edge of the positive electrode active material layer 22 is slightly smaller than the outer edge of the negative electrode active material layer 23.

[0028] The negative electrode active material layer 23 is a layered member containing a negative electrode active material, a conductive assistant, and a binder. Examples of the negative electrode active material include graphite, artificial graphite, highly oriented graphite, mesocarbon microbeads, hard carbon, soft carbon, and other carbon, metal compounds, elements that can be alloyed with lithium or compounds of such elements, and boron-added carbon. Examples of elements that can be alloyed with lithium include silicon and tin. The conductive assistant and binder may be the same as those used in the positive electrode active material layer 22.

[0029] To form the positive electrode active material layer 22 and the negative electrode active material layer 23 on the current collector 21, a conventionally known method such as roll coating, die coating, dip coating, doctor blade, spray coating, curtain coating, etc. is used. Specifically, an active material, a solvent, and, if necessary, a binder and a conductive assistant are mixed to produce a slurry-like active material layer forming composition, which is then applied to the first surface 21a and the second surface 21b and then dried. Examples of the solvent include N-methyl-2-pyrrolidone, methanol, methyl isobutyl ketone, and water. The dried product may be compressed to increase the electrode density.

[0030] In the electrode stack 12, the bipolar electrodes 14, 14 adjacent in the stacking direction are arranged such that the positive electrode active material layer 22 of one bipolar electrode 14 faces the negative electrode active material layer 23 of the other bipolar electrode 14. A separator 15 is arranged between the bipolar electrodes 14, 14 adjacent in the stacking direction. In this embodiment, the separator 15 is a sheet-like member having a rectangular shape in a plan view, and prevents short circuits between the bipolar electrodes 14, 14 adjacent in the stacking direction.

[0031] The separator 15 has a rectangular shape that is larger than the positive electrode active material layer 22 and the negative electrode active material layer 23 and smaller than the current collector 21 when viewed from the stacking direction. An end portion 15a of the separator 15 is located outside the positive electrode active material layer 22 and the negative electrode active material layer 23 when viewed from the stacking direction. In other words, the end portion 15a of the separator 15 does not overlap either the positive electrode active material layer 22 or the negative electrode active material layer 23 when viewed from the stacking direction.

[0032] The separator 15 is formed, for example, in a sheet shape. The separator 15 is, for example, a porous sheet or nonwoven fabric containing a polymer that absorbs and retains an electrolyte. Examples of materials constituting the separator 15 include polypropylene, polyethylene, polyolefin, and polyester. The separator 15 may have a single-layer structure or a multilayer structure. In the case of a multilayer structure, the separator 15 may include, for example, a base material layer and a pair of adhesive layers, and may be bonded and fixed to the positive electrode active material layer 22 and the negative electrode active material layer 23 by the pair of adhesive layers. The separator 15 may include a ceramic layer that serves as a heat-resistant layer. The separator 15 may be reinforced with a vinylidene fluoride resin compound.

[0033] The separator 15 is formed by stretching a molten resin by a dry process or a wet process. In this case, the separator 15 has a direction in which the amount of shrinkage is large and a direction in which the amount of shrinkage is small, depending on the stretching process. The separator 15 may be rectangular in shape, with the direction in which the amount of shrinkage is large along the short side and the direction in which the amount of shrinkage is small along the long side. An example of the separator 15 is formed by a wet process, with the TD (Transverse Direction) direction in which the amount of shrinkage is large along the short side and the MD (Machine Direction) direction in which the amount of shrinkage is small along the long side.

[0034] Examples of the electrolyte impregnated in the separator 15 include a liquid electrolyte (electrolytic solution) containing a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent, and a polymer gel electrolyte containing an electrolyte held in a polymer matrix. When the separator 15 is impregnated with an electrolyte, known lithium salts such as LiClO4, LiAsF6, LiPF6, LiBF4, LiCF3SO3, LiN(FSO2)2, LiFSi, and LiN(CF3SO2)2 can be used as the electrolyte salt. In addition, known solvents such as cyclic carbonates, cyclic esters, chain carbonates, chain esters, and ethers can be used as the non-aqueous solvent. Two or more of these known solvent materials may be used in combination.

[0035] The electrode laminate 12 has a positive terminal electrode 16 and a negative terminal electrode 17 in addition to the bipolar electrode 14. The positive terminal electrode 16 is composed of a current collector 21 and a positive electrode active material layer 22 provided on a first surface 21a of the current collector 21. The positive terminal electrode 16 is arranged at one end side in the lamination direction of the electrode laminate 12 so that the positive electrode active material layer 22 on the first surface 21a faces the negative electrode active material layer 23 of the terminal bipolar electrode 14. In the positive terminal electrode 16, the positive electrode active material layer 22 and the negative electrode active material layer 23 are not provided on the second surface 21b of the current collector 21, and the second surface 21b is electrically connected to an adjacent conductive plate (not shown). The current collector 21 used in the positive terminal electrode 16 may be composed of aluminum foil.

[0036] The negative terminal electrode 17 is composed of a current collector 21 and a negative active material layer 23 provided on the second surface 21b of the current collector 21. The negative terminal electrode 17 is disposed on the other end side in the stacking direction of the electrode laminate 12 so that the negative active material layer 23 on the second surface 21b faces the positive active material layer 22 of the terminal bipolar electrode 14. In the negative terminal electrode 17, the positive active material layer 22 and the negative active material layer 23 are not provided on the first surface 21a of the current collector 21, and the first surface 21a is electrically connected to an adjacent conductive plate (not shown). The current collector 21 used in the negative terminal electrode 17 may be composed of copper foil.

[0037] The separator 15 is disposed between the bipolar electrodes 14, 14 adjacent to each other in the stacking direction, as well as between the bipolar electrode 14 and the positive terminal electrode 16, and between the bipolar electrode 14 and the negative terminal electrode 17. The separator 15 prevents short circuits between the bipolar electrode 14 and the positive terminal electrode 16, and between the bipolar electrode 14 and the negative terminal electrode 17.

[0038] The sealing portion 30 is a member that seals the internal space S between the current collectors 21 adjacent to each other in the stacking direction. The sealing portion 30 has electrical insulation properties. The sealing portion 30 is bonded (joined) to the edge portion of the current collector 21. The sealing portion 30 is separated from the positive electrode active material layer 22 and the negative electrode active material layer 23 when viewed from the stacking direction. The sealing portion 30 is frame-shaped when viewed from the stacking direction, and is disposed between the current collectors 21 adjacent to each other in the stacking direction so as to surround the periphery of the positive electrode active material layer 22 and the negative electrode active material layer 23. The sealing portion 30 is provided on the peripheral portion 21c of the current collector 21 so as to surround the electrode stack 12 when viewed from the stacking direction. In the electricity storage module 11, the internal space S is defined by the current collectors 21 adjacent to each other in the stacking direction and the sealing portion 30. An electrolyte solution (not shown) containing an electrolyte is accommodated in the internal space S. The sealing portions 30 are disposed between the current collectors 21 adjacent to each other in the stacking direction, and thus also function as spacers that maintain the distance between the adjacent current collectors 21.

[0039] The sealing portion 30 of one example has a plurality of first sealing layers 31, a plurality of second sealing layers 32, and a plurality of spacer layers 33. The first sealing layer 31, the second sealing layer 32, and the spacer layer 33 each have a rectangular frame shape when viewed from the stacking direction. For example, the thickness (length in the stacking direction) of the first sealing layer 31 and the second sealing layer 32 may be about 50 μm to 200 μm. The thickness of the first sealing layer 31 and the thickness of the second sealing layer 32 may be the same as each other. The thickness of the spacer layer 33 may be thicker than the thickness of the first sealing layer 31 and the second sealing layer 32, and may be, for example, about 200 μm to 500 μm. The thickness of the spacer layer 33 is set to a thickness T1 of the straight member 41 described later.

[0040] The first seal layer 31 is bonded to the first surface 21a along the peripheral portion 21c of the current collector 21. In one example, as viewed from the stacking direction, the outer edge 31b of the first seal layer 31 is larger than the edge 21d of the current collector 21 and surrounds the current collector 21. Also, as viewed from the stacking direction, the edge 21d of the current collector 21 is larger than the inner edge 31a of the first seal layer 31 and surrounds the inner edge 31a of the first seal layer 31. The first seal layer 31 and the current collector 21 are bonded to each other in a region where they overlap each other as viewed from the stacking direction. That is, the first seal layer 31 and the current collector 21 are bonded to each other in a region from the inner edge 31a of the first seal layer 31 to the edge 21d of the current collector 21. As viewed from the stacking direction, the inner edge 31a of the first seal layer 31 is spaced apart from the positive electrode active material layer 22. The first sealing layer 31 is joined to the first surface 21a at the peripheral portion 21c of the current collector 21 so as to protrude from the end edge 21d of the current collector 21.

[0041] The second seal layer 32 is bonded to the second surface 21b along the peripheral portion 21c of the current collector 21. In one example, the outer edge 32b of the second seal layer 32 is larger than the edge 21d of the current collector 21 as viewed from the stacking direction, and surrounds the current collector 21. For example, the second seal layer 32 and the current collector 21 are bonded to each other in an overlapping region. That is, the second seal layer 32 and the current collector 21 are bonded to each other in a region from the inner edge 32a of the second seal layer 32 to the edge 21d of the current collector 21. As viewed from the stacking direction, the inner edge 32a of the second seal layer 32 is spaced from the negative electrode active material layer 23. The second seal layer 32 is bonded to the second surface 21b at the peripheral portion 21c of the current collector 21 so as to protrude from the edge 21d of the current collector 21.

[0042] The spacer layer 33 is located between the first seal layer 31 and the second seal layer 32 adjacent to each other in the stacking direction. The spacer layer 33, together with the first seal layer 31 and the second seal layer 32, seals the internal space S formed between the current collectors 21 adjacent to each other in the stacking direction.

[0043] FIG. 3 is a schematic plan view showing the spacer layer. FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. 3. As shown in FIGS. 3 and 4, the spacer layer 33 has a plurality of straight members 41 and a plurality of joining members 42. The plurality of straight members 41 are arranged spaced apart from one another when viewed from the stacking direction. The straight member 41 is a resin member having a region extending linearly. The straight member 41 has a region extending in one direction. A bent portion or a curved portion may be provided at one end or both ends of the region extending in one direction. The straight member 41 may have two straight regions extending in different directions, and a bent portion or a curved portion may be provided at the intersection where the two straight regions intersect.

[0044] The joining members 42 are joined to the edges 41a of the straight members 41 so as to fill the gaps between the edges 41a of the straight members 41 adjacent to each other as viewed from the stacking direction. The joining members 42 join the edges 41a of the straight members 41 adjacent to each other as viewed from the stacking direction. As viewed from the stacking direction, the area of ​​the joining members 42 is smaller than the area of ​​the straight members 41. Since the joining members 42 are formed to fill the gaps between the adjacent straight members 41, the joining members 42 tend to have a smaller shape than the straight members 41. In this embodiment, among the edges 41a, the regions at both ends of the straight members 41 in the longitudinal direction are joined to the joining members 42. In this embodiment, the spacer layer 33 has four straight members 41 and four joining members 42. Each of the four sides of the rectangular frame-shaped spacer layer 33 is composed of one straight member 41.

[0045] The plurality of straight members 41 includes a pair of straight members 43 extending linearly in the Y-axis direction and a pair of straight members 44 extending linearly in the X-axis direction. The plurality of straight members 41 are arranged such that the straight members 43 and the straight members 44 are adjacent to each other. Each of the pair of straight members 43 is rectangular in shape with the Y-axis direction as its longitudinal direction (or long side direction) as viewed from the stacking direction. As viewed from the stacking direction, the edge 41a of the straight member 43 includes a region 43L forming the long side of the straight member 43 and a region 43S forming the short side of the straight member 43. As viewed from the stacking direction, the pair of straight members 43 face each other in the X-axis direction. One straight member 43 constitutes a liquid inlet side described later, and is formed wider than the other straight member 43. That is, the region 43S of one straight member 43 is longer than the region 43S of the other straight member 43.

[0046] Each of the pair of straight members 44 has a rectangular shape with the X-axis direction as the longitudinal direction (or long side direction) when viewed from the stacking direction. That is, in this embodiment, the longitudinal directions of adjacent straight members 41 are perpendicular to each other. When viewed from the stacking direction, the edge 41a of the straight member 44 includes a region 44L that forms the long side of the straight member 44 and a region 44S that forms the short side of the straight member 44. The pair of straight members 44 have the same shape as each other. The region 44S of the pair of straight members 44 has the same length as the region 43S of the other straight member 43, for example. The pair of straight members 44 face each other in the Y-axis direction.

[0047] In this embodiment, the length of the spacer layer 33 in the X-axis direction is longer than the length of the spacer layer 33 in the Y-axis direction. Similarly, the length of the current collector 21 in the X-axis direction is longer than the length of the current collector 21 in the Y-axis direction. It can be said that the X-axis direction is the longitudinal direction (or long side direction) of the spacer layer 33 and the current collector 21. It can be said that the Y-axis direction is the lateral direction (or short side direction) of the spacer layer 33 and the current collector 21. The length of the spacer layer 33 in the X-axis direction may be equal to or shorter than the length of the spacer layer 33 in the Y-axis direction. Similarly, the length of the current collector 21 in the X-axis direction may be equal to or shorter than the length of the current collector 21 in the Y-axis direction.

[0048] The joining member 42 joins a region 43L, which is a side surface of the long side of the straight member 43 in the edge 41a when viewed from the stacking direction, to a region 44S, which is a side surface of the short side of the straight member 44 in the edge 41a. That is, all four corners 33c of the rectangular frame-shaped spacer layer 33 are formed of the straight member 43. As shown by the dashed line in FIG. 3, the corners 33c are rectangular portions where the straight member 43 and a region obtained by extending the straight member 44 in the X-axis direction overlap when viewed from the stacking direction. The length of the corners 33c in the X-axis direction is equal to the length of the straight member 43 in the X-axis direction. The length of the corners 33c in the Y-axis direction is equal to the length of the straight member 44 in the Y-axis direction.

[0049] In this embodiment, the length L2 of the straight member 44 in the longitudinal direction (X-axis direction) is longer than the length L1 of the straight member 43 in the longitudinal direction (Y-axis direction). The thickness T2 of the joining member 42 is less than twice the thickness T1 of the straight member 41. The thickness T2 of the joining member 42 is equal to or smaller than the thickness T1 of the straight member 41. In this embodiment, the thickness T2 of the joining member 42 is equal to the thickness T1 of the straight member 41. The joining member 42 is joined only to the end edge 41a of the straight member 41, and is provided so as not to overlap with the straight member 41 in the stacking direction.

[0050] 4, in this embodiment, between the joining members 42 and the edge 41a of the straight member 41, i.e., at the interface between the joining members 42 and the straight member 41 which are in contact with each other, there is a welding layer 40 where the joining members 42 and the straight member 41 melt together. That is, the spacer layer 33 includes the welding layer 40 formed at the joining portion between the joining members 42 and the edge 41a of the straight member 41, where the joining members 42 and the straight member 41 melt together.

[0051] As shown in FIG. 1 and FIG. 2, the first seal layer 31, the second seal layer 32, and the spacer layer 33 are welded to each other by the end surface welded parts R1. The outer edge 33b of the spacer layer 33 may be at the same position as the outer edge 31b of the first seal layer 31 and the outer edge 32b of the second seal layer 32 when viewed from the stacking direction. The outer edge 33b of the spacer layer 33 may be welded to the outer edge 31b of the first seal layer 31 outside the edge 21d of the current collector 21 when viewed from the stacking direction. The outer edge 33b of the spacer layer 33 may be welded to the outer edge 32b of the second seal layer 32 outside the edge 21d of the current collector 21 when viewed from the stacking direction. That is, the first seal layer 31, the second seal layer 32, and the spacer layer 33 are integrated and welded to each other by the end surface welded parts R1 in the region outside the edge 21d of the current collector 21.

[0052] The end face welded portion R1 is formed by welding and integrating the end portions (outer peripheries) of the plurality of first seal layers 31, the plurality of second seal layers 32, and the plurality of spacer layers 33 on the opposite side to the internal space S. In other words, the first seal layer 31 and the spacer layer 33 are not welded to each other at a portion other than the end face welded portion R1, and are only in contact with each other. Similarly, the second seal layer 32 and the spacer layer 33 are not welded to each other at a portion other than the end face welded portion R1, and are only in contact with each other. In this way, since the spacer layer 33 is connected to the first seal layer 31 and the second seal layer 32 by the end face welded portion R1, the stress due to the expansion and contraction of the spacer layer 33 may affect the current collector 21 to which the first seal layer 31 and the second seal layer 32 are melted and joined.

[0053] The end surface welded portion R1 has a rectangular frame shape surrounding the electrode stack 12 when viewed from the stacking direction. When viewed from the stacking direction, the end surface welded portion R1 is formed outside the edge 21d of the current collector 21. That is, the first seal layer 31, the second seal layer 32, and the spacer layer 33 have an overlapping portion that overlaps with the current collector 21 when viewed from the stacking direction, and an extending portion that extends outside the edge 21d of the current collector 21. The end surface welded portion R1 is provided in the extending portion. The side surface of the end surface welded portion R1 opposite to the internal space S extends along the stacking direction and constitutes the outer side surface of the sealing portion 30. In other words, the sealing portion 30 includes an inner side surface facing the internal space S and an outer side surface opposite to the inner side surface.

[0054] The sealing portion 30 has a communication hole 35 that communicates with each of the multiple internal spaces S. As an example, the communication hole 35 is formed by partially cutting out the spacer layer 33, and penetrates the spacer layer 33 and the end face welding portion R1. The communication hole 35 has one opening in the internal space S and the other opening on the outer surface of the sealing portion 30. In the electricity storage module 11, a cell including one internal space S is formed between a pair of adjacent current collectors 21. Here, one communication hole 35 is formed for one cell. The communication hole 35 can be used as a liquid injection port for injecting an electrolyte into the internal space S. That is, a liquid injection port (opening of the communication hole 35) is provided on the outer surface of the sealing portion 30. In the electricity storage module 11 that is rectangular when viewed from the stacking direction, the side on which the communication hole 35 is provided is called the liquid injection port side.

[0055] When viewed from the stacking direction, the inner edge 33a of the spacer layer 33 at the liquid inlet side is located inside (toward the internal space S) of the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32. In this embodiment, the inner edge 33a of the spacer layer 33 at the liquid inlet side is located, for example, 1 mm or more inside the inner edges 31a, 32a and is exposed from the first seal layer 31 and the second seal layer so as to face the internal space S. When viewed from the stacking direction, the inner edge 33a of the spacer layer 33 at a portion other than the liquid inlet side may be located outside the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32, or may be located inside the inner edge 31a of the first seal layer 31 and the inner edge 32a of the second seal layer 32.

[0056] The end 15a of the separator 15 described above is fixed to the second seal layer 32 between the second seal layer 32 and the spacer layer 33. It is sufficient that the end 15a of the separator 15 is fixed near the inner edge 32a of the second seal layer 32 when viewed from the stacking direction. The end 15a may be partially adhered (welded) to the second seal layer 32 by, for example, spot welding.

[0057] When viewed from the stacking direction, the first sealing layer 31 is spaced apart from the positive electrode active material layer 22, and the inner edge 31a is located outside the positive electrode active material layer 22. When viewed from the stacking direction, the second sealing layer 32 is spaced apart from the negative electrode active material layer 23, and the inner edge 32a is located outside the negative electrode active material layer 23. In this embodiment, when viewed from the stacking direction, the first sealing layer 31 is also spaced apart from the negative electrode active material layer 23, but the first sealing layer 31 may overlap the negative electrode active material layer 23 as long as it is spaced apart from the positive electrode active material layer 22.

[0058] In the stacking direction, the thickness of the first seal layer 31 and the thickness of the second seal layer 32 are, for example, thinner than the thickness of the spacer layer 33. As described above, the thickness of the spacer layer 33 is the thickness T1 of the straight member 41. The thickness of the first seal layer 31 is the thickness of a portion of the first seal layer 31 that is sandwiched between the current collector 21 and the spacer layer 33. The thickness of the second seal layer 32 is the thickness of a portion of the second seal layer 32 that is sandwiched between the current collector 21 and the spacer layer 33.

[0059] The thickness of the spacer layer 33 is the thickness of a portion of the linear member 41 sandwiched between the first seal layer 31 and the second seal layer 32. The thicknesses of the first seal layer 31 and the second seal layer 32 may be, for example, 1 / 10 to 1 / 2 of the thickness of the spacer layer 33, or may be equal to each other. The thicknesses of the first seal layer 31 and the second seal layer 32 may be equal to each other or may be different from each other. The thicknesses of the first seal layer 31 and the second seal layer 32 may be thicker than the thickness of the spacer layer 33.

[0060] The first seal layer 31, the second seal layer 32, and the spacer layer 33 are made of a resin material having electrolyte resistance, such as, for example, acid-modified polyethylene (acid-modified PE), acid-modified polypropylene (acid-modified PP), polyethylene, or polyethylene. The resin materials constituting the first seal layer 31, the second seal layer 32, and the spacer layer 33 may be the same or different from each other. Here, the same resin material means that the type of resin material is the same, such as, for example, acid-modified polyethylene, acid-modified polypropylene, polyethylene, or polyethylene. If the type of resin material is the same, even if the average molecular weight or melt flow rate is different, it is treated as the same resin material.

[0061] The melt flow rate is one of the indicators of the fluidity of molten resin. In JIS K7210, the melt flow rate is divided into two parts: the melt mass flow rate (MFR) expressed in g / 10 min and the melt mass flow rate (MFR) expressed in cm 3 There are two types of melt flow rates: melt volume flow rate (MVR) expressed in units of 1 / 10 min and melt mass flow rate (MFR). The melt flow rate used in this embodiment is melt mass flow rate (MFR). In this embodiment, the first seal layer 31 and the second seal layer 32 are made of acid-modified polyethylene or acid-modified polypropylene. The spacer layer 33 is made of polyethylene or polypropylene.

[0062] The straight member 41 and the joint members 42 are formed so that the MFR of the joint members 42 is greater than the MFR of the straight member 41. The MFR is determined in accordance with JIS K7210. Each MFR is adjusted, for example, by the molecular weight of the constituent materials. The MFR of the straight member 41 is, for example, 0.5 g / 10 min or more at a temperature of 190° C. and a load of 2.16 kgf, and the MFR of the joint members 42 is, for example, 20 g / 10 min or less at a temperature of 190° C. and a load of 2.16 kgf.

[0063] The straight member 41 and the joint member 42 may be made of, for example, the same resin material. That is, both the straight member 41 and the joint member 42 may be made of, for example, polyethylene or polypropylene. In this case, the straight member 41 and the joint member 42 may be formed such that the average molecular weight of the joint member 42 is smaller than the average molecular weight of the straight member 41. This makes it easy to realize a configuration in which the MFR of the joint member 42 is larger than the MFR of the straight member 41.

[0064] The straight member 41 is obtained, for example, by punching or cutting a long sheet material unwound from a raw material roll. The joint member 42 is, for example, an injection molded member, and is formed by injection molding. By forming the joint member 42 between the end edges 41a of the adjacent straight members 41 (in this embodiment, between the region 43L of the straight member 43 and the region 44S of the straight member 44), the straight members 41 are connected to each other, and the spacer layer 33 is formed.

[0065] A method of forming the spacer layer 33 will be described with reference to Fig. 5 to Fig. 7. Fig. 5 is a flowchart showing the method of forming the spacer layer 33. Fig. 6 is a schematic plan view for explaining the method of forming the spacer layer 33. Fig. 7 is a schematic side view for explaining the method of forming the spacer layer 33.

[0066] As shown in FIG. 5, the method for forming the spacer layer 33 includes a first preparation step S1, a placement step S2, a second preparation step S3, a third preparation step S4, an injection molding step S5, and a removal step S6. As shown in FIG. 6, the first preparation step S1 is a step of placing either a first middle mold M3a or a second middle mold M3b at a predetermined position on the lower mold M1. The lower mold M1 is a mold that functions as a mounting table. The first middle mold M3a and the second middle mold M3b are molds having the same thickness as the straight member 41, for example. In this embodiment, the first middle mold M3a is provided with an injection port Mh for injecting a resin. The injection port Mh may be provided in the second middle mold M3b.

[0067] The arrangement step S2 is a step of arranging a plurality of straight members 41 at a predetermined position on the lower mold M1 while aligning with either the first middle mold M3a or the second middle mold M3b arranged in the first preparation step S1. The second preparation step S3 is a step of arranging the remaining mold from the first middle mold M3a or the second middle mold M3b at a predetermined position on the lower mold M1. The third preparation step S4 is a step of arranging the upper mold M2 on the lower mold M1 so as to sandwich the plurality of straight members 41, the first middle mold M3a, and the second middle mold M3b, as shown in FIG.

[0068] The injection molding step S5 is a step of filling the space defined by the plurality of straight members 41, the first intermediate die M3a, the second intermediate die M3b, the lower die M1, and the upper die M2 with resin to form the joint members 42. The resin is injected in a molten state from the injection port Mh. The joint members 42 made of the injected resin are formed so as to join the edges 41a of the plurality of straight members 41 together. In this way, the spacer layer 33 is formed in which the plurality of straight members 41 are joined by the joint members 42. Note that the plurality of joint members 42 may be formed simultaneously or sequentially. The removal step S6 is a step of removing the upper die M2, the first intermediate die M3a, and the second intermediate die M3b, and removing the spacer layer 33.

[0069] The thickness T2 of the joining member 42 can be appropriately set depending on the shape of the lower surface of the upper mold M2. As shown in Fig. 7, by making the lower surface of the upper mold M2 flat, the thickness T2 can be made equal to the thickness T1 of the straight member 41. By providing a convex portion on the lower surface of the upper mold M2, the thickness T2 can be made thinner than the thickness T1. By providing a concave portion on the lower surface of the upper mold M2, the thickness T2 can be made thicker than the thickness T1.

[0070] The method for manufacturing the electricity storage module 11 includes the step of forming the spacer layer 33 as described above.

[0071] As described above, in the electricity storage module 11, each spacer layer 33 included in the resin sealing portion 30 is formed into a rectangular frame shape by joining the edges 41a of the straight members 41 with the joining members 42. The straight members 41 having a linearly extending region are resin members formed by cutting out a long sheet material at regular intervals. When a long sheet material unwound from a roll of raw material is punched into a rectangular frame shape, the punched central sheet material becomes waste. However, when the edges 41a of the straight members 41 are joined with the joining members 42 to form the rectangular frame-shaped spacer layer 33 as in the present embodiment, it is not necessary to punch out the long sheet material into a rectangular frame shape, and waste loss is reduced. In particular, when the size of the electrodes is increased, the effect of reducing waste loss is greater than when punching into a rectangular frame shape. That is, in the present embodiment, the sheet material is easily used without waste. Such a spacer layer 33 can suppress an increase in the waste rate of the sheet material. Therefore, a decrease in the productivity of the electricity storage module 11 can be suppressed.

[0072] A spacer layer 50 of a comparative example will be described with reference to FIG. 8 and FIG. 9. FIG. 8 is a schematic plan view showing the spacer layer of the comparative example. FIG. 9 is a schematic cross-sectional view taken along line IX-IX of FIG. 8. As shown in FIG. 8 and FIG. 9, the spacer layer 50 of the comparative example is formed in a rectangular frame shape by connecting four rectangular resin members 51 with welding parts 52. The welding parts 52 are formed by overlapping and welding the longitudinal ends of adjacent resin members 51. Therefore, the welding parts 52 are thicker than other parts. For this reason, a sealing part including a plurality of stacked spacer layers 50 may have a large thickness variation due to the welding parts 52, and the sealing performance may be deteriorated. In addition, the welding parts 52 may have not only a convex part protruding upward, but also a concave part between the edge of the resin member 51 arranged below and the resin member 51 arranged above.

[0073] In contrast, in the electricity storage module 11 of the present embodiment, each spacer layer 33 included in the sealing portion 30 is not formed by overlapping and fusing the longitudinal ends of the straight members 41, but is formed by joining the end edges 41a of the straight members 41 with the joining members 42. Such a spacer layer 33 can suppress variations in the thickness of the sealing portion 30. Therefore, deterioration of the sealing property of the sealing portion 30 can be suppressed.

[0074] The joining member 42 is an injection molded member, and between the joining member 42 and the edge 41a of the straight member 41 there is a welding layer 40 where the joining member 42 and the straight member 41 are fused to each other. Therefore, regardless of the shape of the edge 41a of the straight member 41, the joining member 42 can be produced by injection molding a resin into the gap between the edges 41a of the straight member 41. Since the joining member 42 and the straight member 41 are fused to each other in the welding layer 40, it is possible to improve the bonding between the straight member 41 and the joining member 42. Therefore, it is possible to suppress defects in the electricity storage module 11 due to insufficient bonding between the straight member 41 and the joining member 42.

[0075] The MFR of the joining members 42 is greater than the MFR of the straight members 41. For this reason, for example, when forming the joining members 42 by pouring resin into the gap between the edges 41a of the adjacent straight members 41 by injection molding or potting, even if the gap between the edges 41a of the adjacent straight members 41 is made small, the MFR of the joining members 42 formed by injection molding is large, so that the joining members 42 easily fill the gap. Therefore, such a spacer layer 33 allows the joining members 42 to be positioned with precision.

[0076] The straight member 41 and the joint member 42 may be made of the same resin material. The average molecular weight of the joint member 42 may be smaller than that of the straight member 41. When the average molecular weight of the joint member 42 is smaller than that of the straight member 41, it is possible to easily realize a configuration in which the MFR of the joint member 42 is larger than that of the straight member 41.

[0077] The thickness T2 of the joining members 42 is equal to or less than the thickness T1 of the straight members 41. Therefore, unlike the spacer layer 50 of the comparative example formed by overlapping and welding the ends of the resin members 51, the spacer layer 33 does not have locally thick portions. This makes it possible to suppress the thickness variation of the sealing portion 30. When the thickness T2 of the joining members 42 is thinner than the thickness T1 of the straight members 41, the amount of resin in the joining members 42 is reduced, and therefore it is expected that the cost increase can be suppressed.

[0078] The plurality of straight members 41 include a pair of straight members 43 and a pair of straight members 44. The joint member 42 joins a region 43L of the end edge 41a that forms the long side of the straight member 43 and a region 44S of the end edge 41a that forms the short side of the straight member 44. Thus, the spacer layer 33 can be formed by four straight members 41 and four joint members 42.

[0079] The length L2 is longer than the length L1. Therefore, the thermal contraction of the straight member 44 in the longitudinal direction (X-axis direction) is greater than the thermal contraction of the straight member 43 in the longitudinal direction (Y-axis direction). The joining member 42 joins the region 43L and the region 44S. Therefore, the corner portion 33c of the rectangular frame-shaped spacer layer 33 is formed by the short straight member 43.

[0080] (First Modification) Fig. 10 is a schematic plan view showing a spacer layer according to a first modified example. In the above embodiment, as shown in Fig. 3, each side of the rectangular frame-shaped spacer layer 33 is composed of one straight member 41. In contrast, in the first modified example, as shown in Fig. 10, each side of the rectangular frame-shaped spacer layer 33A is composed of multiple straight members 41. In this modified example, each side of the spacer layer 33A is composed of a pair of straight members 41. The spacer layer 33A has a total of eight straight members 41.

[0081] The eight straight members 41 include four straight members 45 extending linearly in the Y-axis direction and four straight members 46 extending linearly in the X-axis direction. When viewed from the stacking direction, the straight members 45 are rectangular in shape with their longitudinal direction (or long side direction) in the Y-axis direction. When viewed from the stacking direction, the edge 41a of the straight member 45 includes a region 45L that forms the long side of the straight member 45 and a region 45S that forms the short side of the straight member 45. When viewed from the stacking direction, the straight member 46 is rectangular in shape with their longitudinal direction (or long side direction) in the X-axis direction. When viewed from the stacking direction, the edge 41a of the straight member 46 includes a region 46L that forms the long side of the straight member 46 and a region 46S that forms the short side of the straight member 46.

[0082] Each side of the spacer layer 33A is composed of either a pair of straight line members 45 or a pair of straight line members 46. That is, the plurality of straight line members 41 include two pairs of straight line members 45 whose longitudinal directions (long side directions) coincide with each other when viewed from the stacking direction and are adjacent to each other in the longitudinal direction (long side direction), and two pairs of straight line members 46 whose longitudinal directions (long side directions) coincide with each other when viewed from the stacking direction and are adjacent to each other in the longitudinal direction (long side direction). A pair of straight line members 41 constituting the same side of the spacer layer 33, that is, a pair of straight line members 45 or a pair of straight line members 46, have the same shape. In a pair of straight line members 45 constituting the same side of the spacer layer 33, the regions 45S are joined by a joining member 42. In a pair of straight line members 46 constituting the same side of the spacer layer 33, the regions 46S are joined by a joining member 42. In the adjacent straight members 45 and , the region 45L and the region 46S are joined by the joining member .

[0083] Unlike the above embodiment, in this modification, the longitudinal directions of adjacent straight members 41 may be perpendicular to each other, or may be aligned with each other. According to this modification, a large spacer layer 33A can be formed by joining short straight members 45, 46. Here, the case where each side of the spacer layer 33A is composed of a plurality of straight members 41 has been illustrated, but one side of the spacer layer 33A may be composed of a plurality of straight members 41. In addition, a pair of straight members 41 that compose the same side of the spacer layer 33A may have different shapes.

[0084] (Second Modification) FIG. 11 is a schematic plan view showing a spacer layer according to the second modification. As shown in FIG. 11, the spacer layer 33B according to the second modification is different from the spacer layer 33 (see FIG. 3) in that the joint member 42 constitutes the entire corner 33c of the spacer layer 33. When viewed from the stacking direction, the shape of the joint member 42 matches the shape of the corner 33c. In the spacer layer 33B, the multiple straight members 41 include a pair of straight members 47 and a pair of straight members 48. The straight member 47 is different from the straight member 43 (see FIG. 3) in that it does not constitute the corner 33c. The length L5 of the straight member 47 in the longitudinal direction (Y-axis direction) is shorter than the length L1 of the straight member 43 by the length of the corner 33c. The straight member 48 is different from the straight member 44 (see FIG. 3) in that it reaches the corner 33c. The length L6 of the straight member 48 in the longitudinal direction (X-axis direction) is longer than the length L2 of the straight member 44. The length L6 is longer than the length L5.

[0085] When viewed from the stacking direction, edge 41a of straight member 47 includes region 47L forming the long side of straight member 47 and region 47S forming the short side of straight member 47. When viewed from the stacking direction, edge 41a of straight member 48 includes region 48L forming the long side of straight member 48 and region 48S forming the short side of straight member 48. Joining member 42 joins region 47S of edge 41a forming the short side of straight member 47 and region 48S of edge 41a forming the short side of straight member 48. In this modification as well, the number of straight members 41 is minimized, and therefore the productivity of the electricity storage module 11 can be improved.

[0086] Although an example of the present disclosure has been described in detail above, the present disclosure is not limited to the above-described embodiment and modified examples.

[0087] The joining member 42 may not be an injection molded member, but may be a member formed by a method other than injection molding. For example, as shown in Fig. 6, after the straight member 41 is placed on the lower mold M1 together with the first and second intermediate molds M3a and M3b, the upper mold M2 is not placed, and resin is poured from above into the gap between the edges 41a of the straight member 41 to form the joining member 42. In this case, the first and second intermediate molds M3a and M3b that are not provided with the injection port Mh can be used.

[0088] In the spacer layer 33, the pair of straight members 43 may have the same shape as each other. The length of the region 43S of the pair of straight members 43 may be equal to the length of the region 44S of the pair of straight members 44.

[0089] The number of straight members 41 may be more than one. The joining member 42 may join the region 43S of the straight member 43 and the region 44L of the straight member 44. The length L2 in the longitudinal direction of the straight member 44 may be shorter than the length L1 in the longitudinal direction of the straight member 43. The straight member 41 and the joining member 42 may be made of different resin materials. The straight member 41 may have a region that extends linearly, and may have a shape other than a rectangular shape, such as an L-shape or a U-shape.

[0090] The configuration of the spacer layer 33 is also applicable to the first sealing layer 31 and the second sealing layer 32. That is, each of the first sealing layer 31 and the second sealing layer 32 may include a plurality of straight members arranged spaced apart from each other when viewed from the stacking direction, and a joining member that joins the edges of adjacent straight members.

[0091] An embodiment of the present disclosure can be shown as follows. [1] a laminate including a plurality of electrodes stacked together, each of the electrodes having a rectangular metal current collector; a resin sealing portion provided on a peripheral portion of the current collector so as to surround the stack when viewed from a stacking direction of the plurality of electrodes, each of the plurality of electrodes has an active material layer on a first surface of the current collector and on a second surface opposite to the first surface; the sealing portion includes a plurality of rectangular frame-shaped seal layers and a plurality of rectangular frame-shaped spacer layers, the plurality of sealing layers are joined to the first surface and the second surface at peripheral portions of the current collectors of the plurality of electrodes, Each of the plurality of spacer layers comprises: a plurality of seal layers are disposed between the seal layers adjacent to each other in the stacking direction, and an internal space formed between the current collectors adjacent to each other in the stacking direction is sealed together with the plurality of seal layers; a plurality of linear members arranged apart from each other when viewed from the stacking direction, each having a linearly extending region; and a joining member joined to the edges of the linear members so as to fill a gap between the edges of the adjacent linear members; Energy storage module. [2] The joining member is an injection molded member, The energy storage module described in [1], wherein each of the spacer layers has a welding layer formed at the joint between the joining member and the edge of the straight member, through which the joining member and the straight member are fused to each other. [3] The joining member is an injection molded member, The energy storage module according to [1] or [2], wherein the melt flow rate of the joining members is greater than the melt flow rate of the straight members. [4] The electricity storage module according to any one of [1] to [3], wherein an area of ​​the joint members is smaller than an area of ​​the straight members when viewed from the stacking direction. [5] The electricity storage module according to any one of [1] to [4], wherein the thickness of the joining members is equal to or smaller than the thickness of the straight members. [6] the plurality of straight members include a pair of rectangular first straight members opposed to each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members opposed to each other in a second direction perpendicular to the first direction as viewed from the stacking direction, The energy storage module according to any one of [1] to [5], wherein the joining member joins an edge forming a long side of the first straight member and an edge forming a short side of the second straight member. [7] the plurality of straight members include a pair of rectangular first straight members opposed to each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members opposed to each other in a second direction perpendicular to the first direction as viewed from the stacking direction, The energy storage module according to any one of [1] to [5], wherein the joining member joins a region of the edge that forms a short side of the first straight member and a region of the edge that forms a short side of the second straight member. [8] The plurality of straight members include a pair of straight members whose longitudinal directions coincide with each other when viewed from the stacking direction and that are adjacent to each other in the longitudinal direction. The power storage module according to any one of [1] to [7]. [Explanation of symbols]

[0092] DESCRIPTION OF SYMBOLS 11...energy storage module, 12...electrode laminate (laminate), 14...bipolar electrode, 21...current collector, 21a...first surface, 21b...second surface, 21c...periphery, 22...positive electrode active material layer, 23...negative electrode active material layer, 30...sealing portion, 31...first seal layer, 32...second seal layer, 33, 33A, 33B...spacer layer, 40...welding layer, 41...straight member, 41a... Edge, 42...joint member, 43...straight member, 43L...area, 43S...area, 44...straight member, 44L...area, 44S...area, 45...straight member, 45L...area, 45S...area, 46...straight member, 46L...area, 46S...area, 47...straight member, 47L...area, 47S...area, 48...straight member, 48L...area, 48S...area, S...internal space.

Claims

1. a laminate including a plurality of electrodes stacked together, each of the electrodes having a rectangular metal current collector; a resin sealing portion provided on a peripheral portion of the current collector so as to surround the stack when viewed from a stacking direction of the plurality of electrodes, Each of the plurality of electrodes has an active material layer on a first surface of the current collector and on a second surface opposite to the first surface, the sealing portion includes a plurality of rectangular frame-shaped seal layers and a plurality of rectangular frame-shaped spacer layers, the plurality of sealing layers are joined to the first surface and the second surface at peripheral portions of the current collectors of the plurality of electrodes, Each of the plurality of spacer layers comprises: a plurality of seal layers are disposed between the seal layers adjacent to each other in the stacking direction, and an internal space formed between the current collectors adjacent to each other in the stacking direction is sealed together with the plurality of seal layers; a plurality of linear members arranged apart from each other when viewed from the stacking direction, each having a linearly extending region; and a joining member joined to the edges of the linear members so as to fill a gap between the edges of the adjacent linear members; Energy storage module.

2. The joining member is an injection molded member, The energy storage module according to claim 1 , wherein each of the spacer layers includes a welding layer formed at a joint between the joint member and the end edge of the straight member, the welding layer melting the joint member and the straight member into each other.

3. The joining member is an injection molded member, The energy storage module according to claim 1 , wherein a melt flow rate of the joint members is greater than a melt flow rate of the straight members.

4. The energy storage module according to claim 3 , wherein an area of ​​the joint members is smaller than an area of ​​the straight members when viewed from the stacking direction.

5. The energy storage module according to claim 1 , wherein a thickness of the joint members is equal to or smaller than a thickness of the straight members.

6. the plurality of straight members include a pair of rectangular first straight members opposed to each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members opposed to each other in a second direction perpendicular to the first direction as viewed from the stacking direction, 3 . The energy storage module according to claim 1 , wherein the joining member joins a region of the edge that forms a long side of the first straight member and a region of the edge that forms a short side of the second straight member.

7. the plurality of straight members include a pair of rectangular first straight members opposed to each other in a first direction as viewed from the stacking direction, and a pair of rectangular second straight members opposed to each other in a second direction perpendicular to the first direction as viewed from the stacking direction, 3 . The energy storage module according to claim 1 , wherein the joining member joins a region of the edge that forms a short side of the first straight member and a region of the edge that forms a short side of the second straight member.

8. The plurality of straight members include a pair of straight members whose longitudinal directions coincide with each other when viewed from the stacking direction and that are adjacent to each other in the longitudinal direction. The energy storage module according to claim 1 or 2.

Citation Information

Patent Citations

  • Bipolar battery

    JP2004158343A