Slide member

The sliding member with inclined wear detection grooves on a copper alloy layer addresses the challenge of visual wear detection in tire vulcanizers by enhancing brightness contrast for clear wear indication.

JP2024165979APending Publication Date: 2024-11-28DAIDO METAL IND CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023082628
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-18
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

Conventional sliding members in tire vulcanizers have difficulty in visually confirming the need for replacement due to similar reflection angles of stepped surfaces, making it hard to discern wear levels.

Method used

A flat plate-shaped sliding member with a copper alloy sliding layer featuring wear detection grooves that are inclined relative to the exposed surface, creating distinct brightness differences for easy visual inspection.

Benefits of technology

The inclined wear detection grooves facilitate easy visual confirmation of wear levels by providing distinct brightness differences, allowing timely replacement detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024165979000001_ABST
    Figure 2024165979000001_ABST
Patent Text Reader

Abstract

To provide a slide member for allowing easy and visual confirmation of whether replacement is necessary.SOLUTION: In each first end face part 6 of a slide member 1, a wear detection grove 8 is formed at an exposed surface of a slide layer 3. On the exposed surfaces (an upper side exposed surface 33U and a lower side exposed surface 33L) of the slide layer 3 of the first end face part 6 and in the wear detection grooves 8 (a first groove inner face 81 and a second groove inner face 82), there are light-dark differences of reflected light to be reflected from faces neighboring each other, thus allowing easy and visual confirmation of a shape (a contour) of each face and a structure (a relation between faces).SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sliding member used, for example, in a tire vulcanizer, etc. In particular, the present invention relates to a flat-plate-shaped sliding member including a sliding layer formed on a back metal layer. [Background technology]

[0002] Conventionally, a flat sliding member having a sliding layer formed on a backing metal layer is used in the reciprocating sliding part of a tire vulcanizer. A wear indicator (wear gauge) is formed on such a sliding member so that an operator or manager of the tire vulcanizer can visually detect that the sliding layer has worn down and it is time to replace the sliding member.

[0003] For example, Patent Document 1 proposes a sliding member in which two steps are formed as wear indicators (wear gauges) at the boundary between the sliding surface of the sliding layer and the end face facing the sliding direction of the mating member, for the purpose of easily detecting the time to replace the sliding member by visual inspection without increasing the maintenance workload and running costs (see FIG. 5). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2017-207117 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, in the sliding member proposed in Patent Document 1, two steps are formed on the end surface as a wear indicator (wear gauge). However, since the two step surfaces and the end surface facing the sliding direction are parallel to each other, when visible light is irradiated, the difference in color between the two step surfaces and the surfaces of the sliding layer exposed on the end surface is small, making it difficult to visually check whether replacement is necessary.

[0006] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a sliding member that makes it easy for a person to visually check whether or not replacement is required. [Means for solving the problem]

[0007] In order to achieve the above object, the invention according to claim 1 comprises: A flat-plate-shaped sliding member including a back metal layer having a back surface and a sliding layer having a sliding surface for sliding against a reciprocating counter member, The sliding layer is made of a copper alloy, The interfaces between the back surface, the sliding surface, and the back metal layer of the sliding layer are parallel to each other, the sliding member has a first end surface portion on a leading side in each moving direction of the counter member, the first end surface portion has an exposed surface on which the sliding layer is exposed, At least one of the first end faces has a wear detection groove formed in the exposed surface, The wear detection groove has a constant groove depth and a constant groove width, is parallel to the sliding surface, and extends in a direction perpendicular to the moving direction of the mating member. The surface of the wear detection groove includes a first groove inner surface between a maximum position of a groove depth of the wear detection groove and one end of a groove width, and a second groove inner surface between a maximum position of a groove depth of the wear detection groove and the other end of a groove width, The first groove inner surface and the second groove inner surface are characterized in that the wear detection groove is inclined with respect to the exposed surface adjacent thereto.

[0008] The invention according to claim 2 is the sliding member according to claim 1, wherein the first end surface portion is formed of a vertical surface that is parallel to a virtual plane that is perpendicular to the moving direction of the counter member.

[0009] The invention according to claim 3 is the sliding member according to claim 1, wherein the first end surface portion comprises a vertical surface adjacent to the back surface and parallel to a virtual plane perpendicular to the moving direction of the counter member, and an inclined surface adjacent to the vertical surface and the sliding surface and inclined at a certain angle with respect to the vertical surface.

[0010] A fourth aspect of the present invention is the sliding member according to the third aspect, wherein the wear detection groove is positioned within the inclined surface.

[0011] The invention according to claim 5 is the sliding member according to claim 3, wherein the wear detection groove is positioned within the vertical plane.

[0012] The invention according to claim 6 is the sliding member according to claim 3, wherein the angle θ1 between the inclined surface and the vertical surface is 30° to 60°.

[0013] The invention of claim 7 is characterized in that, in the sliding member described in claim 1, the angle θ2 between the first groove inner surface or the second groove inner surface of the wear detection groove and the exposed surface adjacent to the wear detection groove is 30° to 60°.

[0014] An eighth aspect of the present invention is the sliding member according to the first aspect, wherein the wear detection groove is formed over the entire length of the exposed surface in the width direction.

[0015] The invention according to claim 9 is characterized in that, in the sliding member according to claim 1, the wear detection groove is formed on a part of the length in the width direction of the exposed surface. Effect of the Invention

[0016] In the present invention, a wear detection groove is formed on the exposed surface where the sliding layer is exposed on one or both of the first end faces of the sliding member, and therefore a difference (difference) in brightness of reflected light reflected by each of the adjacent surfaces is generated on the exposed surface of the sliding layer and in the wear detection grooves (the first groove inner surface and the second groove inner surface), making it possible to easily visually check the shape (contour) and structure (relationship between the surfaces) of each surface. [Brief description of the drawings]

[0017] [Figure 1] FIG. 2 is a perspective view showing the relationship between a sliding member of the bearing device and a mating member. [Diagram 2] FIG. 2 is a perspective view showing a sliding member of the first embodiment. [Diagram 3] 3 is an enlarged side view of the sliding member of FIG. 2. [Figure 4] 3 is an enlarged side view of a sliding layer of the sliding member of FIG. 2. [Diagram 5] FIG. 11 is a perspective view showing a sliding member of the second embodiment. [Figure 6] 6 is an enlarged side view of the sliding member of FIG. 5. [Figure 7] FIG. 11 is a perspective view showing a sliding member of a third embodiment. [Figure 8] 8 is an enlarged side view of the sliding member of FIG. 7. [Figure 9] FIG. 11 is a perspective view showing a sliding member of Example 4. [Figure 10] FIG. 1 is an enlarged side view of a sliding member of the prior art. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0019] First, the configuration of a bearing device 11 having a sliding member 1 of the present invention will be described with reference to Fig. 1. As shown in Fig. 1, the bearing device 11 is composed of a sliding member 1 and a mating member 12, and the sliding member 1 and the mating member 12 are adapted to relatively reciprocate in the direction of the X arrow.

[0020] [Example 1] (Configuration of Sliding Member) Next, the configuration of the slide member 1 of Example 1 will be described with reference to Fig. 2 to Fig. 4. Fig. 2 is a perspective view showing the slide member of Example 1, Fig. 3 is an enlarged side view showing the slide member of Fig. 2, and Fig. 4 is an enlarged side view showing the slide layer of the slide member of Fig. 2.

[0021] The slide member 1 of the first embodiment is formed in a flat plate shape by a bimetal in which a sliding layer 3 is bonded to a back metal layer 2. As shown in FIG. 2, the slide member 1 has a sliding surface 4 which is the surface of the sliding layer 3 and supports a mating member 12, an interface 32 between the sliding layer 3 and the back metal layer 2, and a back surface 5 which is the surface of the back metal layer 2 opposite to the side to which the sliding layer 3 is bonded, and the sliding surface 4, the interface 32 between the sliding layer 3 and the back metal layer 2, and the back surface 5 are parallel to each other. Therefore, the thickness T1 of the sliding layer 3 in the direction perpendicular to the sliding surface 4 and the thickness T2 of the back metal layer 2 in the direction perpendicular to the sliding surface 4 are constant. The thickness T1 of the sliding layer 3 can be 0.5 to 5 mm, and the thickness T2 of the back metal layer 2 can be 2 to 5 mm. However, the thickness T1 of the sliding layer 3 and the thickness T2 of the back metal layer 2 may be other dimensions.

[0022] An Fe alloy such as hypoeutectoid steel containing 0.05 to 0.50 mass % of carbon or stainless steel can be used for the back metal layer 2. However, the material of the back metal layer 2 is not limited to this and other materials may be used.

[0023] The sliding layer 3 is made of a colored copper alloy for sliding. The colored copper alloy means a copper alloy that can be visually recognized as a color other than white or black on the surface of the copper alloy when it reflects visible light. The composition of the copper alloy may be one that contains 1 to 12 mass% Sn with the balance being copper and inevitable impurities, or one that contains 1 to 12 mass% Sn and further contains one or more selected components from 0.01 to 1 mass% P, 0.5 to 15 mass% Ni, 0.2 to 5 mass% Fe, 1 to 20 mass% Zn, 0.5 to 20 mass% Pb, and 0.5 to 20 mass% Bi with the balance being copper and inevitable impurities. The copper alloy may further contain 1 to 20 volume% of a solid lubricant selected from Gr, MoS2, and WS2. The copper alloy may further contain 0.5 to 10 volume % of hard materials such as Fe2P, Fe3P, Mo2C, WC, Al2O3, SiO2, etc. However, the composition of the copper alloy 31 is not limited to these, and may be other compositions.

[0024] The sliding member 1 has one first end surface portion 6 at each end in the moving direction X of the mating member 12, and the first end surface portions 6 are parallel to each other. The sliding member 1 has second end surface portions 7 at each end in a direction parallel to the sliding surface 4 and perpendicular to the moving direction X of the mating member 12, and the second end surface portions 7 are parallel to each other. Therefore, the length L2 between the second end surface portions 7 in the direction parallel to the sliding surface 4 and perpendicular to the moving direction X of the mating member 12 is constant. The first end surface portions 6 have a length L2 in the direction parallel to the sliding surface 4 and perpendicular to the moving direction X of the mating member 12.

[0025] 3, each first end surface portion 6 of the sliding member 1 is formed of a vertical surface 61 that is parallel to a virtual plane FP perpendicular to the moving direction X of the counter member 12. This vertical surface 61 is formed of the exposed surface of the back metal layer 2 and the exposed surface 33 of the sliding layer 3.

[0026] As shown in Fig. 4, in each first end surface portion 6 of the sliding member 1, a wear detection groove 8 is formed in an exposed surface 33 of the sliding layer 3. Therefore, the exposed surface 33 is composed of an upper exposed surface 33U between the wear detection groove 8 and the sliding surface 4, and a lower exposed surface 33L between the wear detection groove 8 and the interface 32. The upper exposed surface 33U and the lower exposed surface 33L are located in the same plane (vertical plane 61). The wear detection groove 8 may be formed only in one first end surface portion 6 of the sliding member 1.

[0027] The wear detection groove 8 is not in contact with the sliding surface 4, is spaced from the sliding surface 4 by a constant length L4 in a direction perpendicular to the sliding surface 4, is parallel to the sliding surface 4, and extends in a direction perpendicular to the moving direction X of the mating member 12, and is formed over the entire width direction of the exposed surface 33 of the first end surface portion 6. The width direction of the exposed surface 33 is defined as a direction parallel to the sliding surface 4 and perpendicular to the moving direction X of the mating member 12. The wear detection groove 8 has a constant groove width L1 and a constant groove depth D1 over the entire length in the extension direction. The groove width L1 is defined as the length in a direction parallel to the exposed surface 33 in a cross section perpendicular to the sliding surface 4 and parallel to the moving direction X of the mating member 12. In addition, groove depth D1 is defined as the length in a direction perpendicular to exposed surface 33, between the exposed surface 33 and the deepest part of the wear detection groove 8 (maximum position 81P of groove depth D1) in a cross section perpendicular to the sliding surface 4 and parallel to the moving direction X of the mating member 12.

[0028] The groove width L1 of the wear detection groove 8 may be 0.2 to 2 mm, and the groove depth D1 may be 0.2 to 1 mm. Furthermore, the length L4 from the sliding surface 4 to the wear detection groove 8 in the direction perpendicular to the sliding surface 4 (the length of the upper exposed surface 33U) may be 0.2 to 0.8 mm. However, the groove width L1 and groove depth D1 of the wear detection groove 8, and the length L4 from the sliding surface 4 to the wear detection groove 8 (the length of the upper exposed surface 33U) may be other dimensions.

[0029] The wear detection groove 8 has a V-shaped cross section perpendicular to the sliding surface 4 and parallel to the moving direction X of the mating member 12. The surface of the wear detection groove 8 is composed of a first groove inner surface 81 between a maximum position 81P of the groove depth D1 and one end 81E of the groove width L1, and a second groove inner surface 82 between the maximum position 81P of the groove depth D1 and the other end 82E of the groove width L1. The first groove inner surface 81 and the second groove inner surface 82 are inclined at a certain inclination angle θ1 with respect to the exposed surface 33 adjacent to the wear detection groove 8 (the first groove inner surface 81 and the second groove inner surface 82). The inclination angle θ1 between the first groove inner surface 81 and the exposed surface 33 (the upper exposed surface 33U) of the wear detection groove 8 and the inclination angle θ1 between the second groove inner surface 82 and the exposed surface 33 (the lower exposed surface 33L) can be 30° to 60°. However, the inclination angle θ1 between the first groove inner surface 81 and the exposed surface 33 (upper exposed surface 33U) and the inclination angle θ1 between the second groove inner surface 82 and the exposed surface 33 (lower exposed surface 33L) may be other angles, and although in Example 1 the inclination angle θ1 between the first groove inner surface 81 and the exposed surface 33 (upper exposed surface 33U) and the inclination angle θ1 between the second groove inner surface 82 and the exposed surface 33 (lower exposed surface 33L) are the same, they may be different angles.

[0030] (action) When the sliding member 1 of Example 1 is used in a reciprocating sliding part of a tire vulcanizer, a wear detection groove 8 is formed in the first end surface part 6 so that an operator or a manager can visually detect whether the sliding layer 3 has worn away and the time to replace the sliding member 1 has arrived. In the sliding member 1 of Example 1, wear of the sliding layer 3 progresses due to relative reciprocating sliding with the mating member 12, but it is determined that the time to replace the sliding member 1 has not arrived until (while) an upper exposed surface 33U between the wear detection groove 8 and the sliding surface 4 is lost on the exposed surface 33 of the sliding layer 3 of the first end surface part 6, and when the upper exposed surface 33U is lost, it is determined that the time to replace the sliding member 1 has arrived.

[0031] A worker or manager (hereinafter, referred to as "person") receives visible light irradiated from an indoor light source or the like and reflected by the first end surface portion 6 with his / her eyes, and the visual nerve is stimulated, thereby being able to know the shape of the first end surface portion 6. In detail, in the exposed surface 33 (upper exposed surface 33U, lower exposed surface 33L) of the sliding layer 3 of the first end surface portion 6 and the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82), a difference (difference) in the brightness of the reflected light reflected by each adjacent surface occurs, which makes it easier to visually confirm the shape (contour) and structure (relationship between the surfaces) of each surface. In addition, the first groove inner surface 81 and the second groove inner surface 82 of the wear detection groove 8 are inclined at an inclination angle θ1 with respect to the upper exposed surface 33U and the lower exposed surface 33L, and therefore the reflection angles of visible light differ between the upper exposed surface 33U and the lower exposed surface 33L and the first groove inner surface 81 and the second groove inner surface 82, respectively, resulting in a difference in brightness in the reflected light. On the other hand, the upper exposed surface 33U and the lower exposed surface 33L in the exposed surface 3 of the slide layer 3 of the first end surface portion 6 are located in the same plane (vertical plane 61), and therefore no difference in brightness occurs in the reflected light between the upper exposed surface 33U and the lower exposed surface 33L.

[0032] In the sliding member 1 of Example 1, the sliding layer 3 is made of a colored sliding copper alloy. When visible light is reflected, the copper alloy selectively reflects light (electromagnetic waves) in the red to yellow wavelength range, and thus exhibits a red to yellow (gold) color. When the reflected light is colored (red to yellow (gold) in the case of a copper alloy), the human visual nerve is stimulated, and the shape of each surface (the boundary between each surface (surface outline)) and the difference in brightness of each surface in the exposed surface 33 (upper exposed surface 33U, lower exposed surface 33L) of the sliding layer 3 of the first end surface portion 6 and the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82) become easily visible. Furthermore, when a person visually checks the first end surface portion 6 of the sliding member 1 to check whether the sliding member 1 needs to be replaced, the person can check whether the upper exposed surface 33U of the same color tone (brightness) remains above the wear detection groove 8 while looking at the color tone (brightness) of the lower exposed surface 33L, making it easier to visually check whether the sliding member 1 needs to be replaced.

[0033] In addition, when a sliding layer made of an Al alloy or an Fe alloy for sliding is used instead of the sliding layer 3 made of the copper alloy of the present invention, it becomes difficult for people to visually check whether or not the sliding member needs to be replaced. The Al alloy appears white because it reflects all wavelength regions of visible light evenly, and the Fe alloy appears black (gray) because its reflectance is low in all wavelength regions of visible light. And, when the reflected light is achromatic (white in the case of an Al alloy, black (gray) in the case of an Fe alloy) like the Al alloy or the Fe alloy, the stimulation to the human visual nerve is smaller than that of the colored reflected light of the copper alloy, so that it becomes difficult for people to visually check the shape (contour) and structure (relationship between the surfaces) of each surface in the exposed surface 33 (upper exposed surface 33U, lower exposed surface 33L) of the sliding layer 3 of the first end surface portion 6 and the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82).

[0034] 10 is an enlarged side view of the vicinity of a first end surface portion 106 of a sliding member 101 of the prior art. The sliding member 101 has two steps formed in the first end surface portion 106 on the leading side in the moving direction X of the mating member so that it can be visually determined whether the sliding member 101 needs to be replaced. The exposed surface of the sliding layer 103 is made up of an upper step surface 133U adjacent to the sliding surface 104, a wear detection step surface 108, and a lower exposed surface 133L located at the first end surface portion 106.

[0035] In the sliding member 101 of the conventional technology, wear of the sliding layer 103 progresses due to relative reciprocating sliding with the counter member, and it is determined that the time to replace the sliding member 101 has not yet arrived until the upper step surface 133U of the sliding layer 103 of the first end surface portion 106 is lost (while it exists), and when the upper step surface 133U is lost, it is determined that the time to replace the sliding member 101 has arrived. However, in the sliding member 101 of the conventional technology, the upper step surface 133U, the wear detection step surface 108, and the lower exposed surface 133L are arranged in parallel, and the reflection angles of visible light irradiated to these surfaces are the same, making it difficult for differences in brightness to occur in the reflected light on each surface. For this reason, it is difficult for a person to visually determine whether the upper step surface 133U is lost or not.

[0036] [Example 2] Next, a sliding member 1 according to a second embodiment, which has a first end surface portion 6 having a different configuration from that of the first embodiment, will be described with reference to Fig. 5 and Fig. 6. Fig. 5 is a perspective view of the sliding member 1 according to the second embodiment, and Fig. 6 is an enlarged side view of the sliding member 1 shown in Fig. 5. Note that the same reference numerals are used to designate the same components of the sliding member 1 according to the second embodiment as those of the first embodiment, and description thereof will be omitted.

[0037] 5 and 6, each first end surface portion 6 of the sliding member 1 of Example 2 includes a vertical surface 61 adjacent to the back surface 5 and parallel to an imaginary plane FP perpendicular to the moving direction X of the counterpart member 12, and an inclined surface 62 adjacent to the vertical surface 61 and the sliding surface 4 and inclined at a certain inclination angle θ2 with respect to the vertical surface 61. The inclination angle θ2 between the vertical surface 61 and the inclined surface 62 is preferably 30° to 60°, but is not limited thereto and may be another angle.

[0038] The wear detection groove 8 is formed on the exposed surface 33 of the sliding layer 3 at the inclined surface 62. Therefore, in the exposed surface 33, an upper exposed surface 33U between the wear detection groove 8 and the sliding surface 4, and a lower exposed surface 33L between the wear detection groove 8 and the interface 32 are formed on the inclined surface 62. In addition, the wear detection groove 8 does not contact the sliding surface 4, is separated from the sliding surface 4 by a certain length L4 in a direction perpendicular to the sliding surface 4, is parallel to the sliding surface 4, and extends in a direction perpendicular to the moving direction X of the mating member 12, and is formed over the entire width direction of the exposed surface 33 of the first end surface portion 6.

[0039] In the sliding member 1 of Example 2, a wear detection groove 8 is formed on the exposed surface 33 of the sliding layer 3 at the inclined surface 62. In the exposed surface 33 (upper exposed surface 33U, lower exposed surface 33L) of the sliding layer 3 at the inclined surface 62 and the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82), a difference (difference) in brightness of reflected light reflected by each adjacent surface occurs, making it easier to visually check the shape (contour) and structure (relationship between the surfaces).

[0040] [Example 3] Next, a sliding member 1 according to a third embodiment, which has a first end surface portion 6 having a different configuration from that of the first embodiment, will be described with reference to Figs. 7 and 8. Fig. 7 is a perspective view of the sliding member 1 according to the third embodiment, and Fig. 8 is an enlarged side view of the sliding member 1 shown in Fig. 7. Note that the same reference numerals are used to designate the same components of the sliding member 1 according to the third embodiment as those of the first embodiment, and description thereof will be omitted.

[0041] 7 and 8, each first end surface portion 6 of the sliding member 1 of Example 3 includes a vertical surface 61 adjacent to the back surface 5 and parallel to an imaginary plane FP perpendicular to the moving direction X of the counterpart member 12, and an inclined surface 62 adjacent to the vertical surface 61 and the sliding surface 4 and inclined at a certain inclination angle θ2 with respect to the vertical surface 61. The inclination angle θ2 between the vertical surface 61 and the inclined surface 62 is preferably 30° to 60°, but is not limited thereto and may be another angle.

[0042] The wear detection groove 8 is formed on the exposed surface 33 of the sliding layer 3 on the vertical surface 61. Therefore, on the exposed surface 33, an upper exposed surface 33U between the wear detection groove 8 and the sliding surface 4 is formed on the inclined surface 62 and the vertical surface 61, and a lower exposed surface 33L between the wear detection groove 8 and the interface 32 is formed on the vertical surface 61. In addition, the wear detection groove 8 does not contact the sliding surface 4, is separated from the sliding surface 4 by a certain length L4 in a direction perpendicular to the sliding surface 4, is parallel to the sliding surface 4, and extends in a direction perpendicular to the moving direction X of the mating member 12, and is formed over the entire width direction of the exposed surface 33 of the first end surface portion 6.

[0043] In the sliding member 1 of Example 3, a wear detection groove 8 is formed on the exposed surface 33 of the sliding layer 3 on the vertical surface 61. In the exposed surface 33 (upper exposed surface 33U, lower exposed surface 33L) of the sliding layer 3 on the vertical surface 61 and in the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82), a difference (difference) in brightness of the reflected light reflected by each adjacent surface occurs, making it easier to visually check the shape (contour) and structure (relationship between the surfaces).

[0044] [Example 4] Next, a sliding member 1 according to a fourth embodiment, which has a first end surface portion 6 having a different configuration from that of the first embodiment, will be described with reference to Fig. 9. Fig. 9 is a perspective view of the sliding member 1 according to the fourth embodiment. Note that the same reference numerals are used to designate the same components of the sliding member 1 according to the fourth embodiment as those of the first embodiment, and description thereof will be omitted.

[0045] As shown in FIG. 9, in each first end surface portion 6 of the sliding member 1 of Example 4, a wear detection groove 8 is formed on the exposed surface 33 of the sliding layer 3, but the length L3 of the wear detection groove 8 is smaller than the widthwise length L2 of the exposed surface 33 of the sliding layer 3. In other words, the wear detection groove 8 is formed in a part of the widthwise direction of the exposed surface 33 of the sliding layer 3. The length L3 of the wear detection groove 8 is preferably 60% or more of the widthwise length L2 of the exposed surface 33 of the sliding layer 3, but is not limited thereto and may be other ratios. In addition, when the length L3 of the wear detection groove 8 is formed to be smaller than the widthwise length L2 of the exposed surface 33 of the sliding layer 3, the groove depth D1 and groove width L1 near the end in the lengthwise direction of the wear detection groove 8 may be formed to be gradually smaller toward the end in the lengthwise direction of the wear detection groove 8. In addition, a plurality of wear detection grooves 8 may be formed on the exposed surface 33 of the sliding layer 3.

[0046] In the sliding member 1 of Example 4, a wear detection groove 8 is formed in a part of the width direction of the exposed surface 33 of the sliding layer 3. In the exposed surface 33 of the sliding layer 3 and the wear detection groove 8 (first groove inner surface 81, second groove inner surface 82), a difference (difference) in brightness of the reflected light reflected by each adjacent surface occurs, which makes it easier to visually check the shape (contour) and structure (relationship between the surfaces).

[0047] The sliding member 1 of the present invention is not limited to the first to fourth embodiments and can be modified as follows. The sliding member 1 may have recesses, holes, etc. for fastening the sliding member 1 to a predetermined device with a bolt, or grooves, etc. for holding grease, formed on the sliding surface 4. The second end surface portion 7 of the sliding member 1 may have an inclined surface formed at a position adjacent to the sliding surface 4. [Explanation of symbols]

[0048] 1 Sliding member 2 Backing layer 3. Sliding layer 32 Interface 33 Exposed surfaces 33U upper exposed surface 33L Lower exposed surface 4. Sliding surface 5 Back 6 First end section 61 Vertical plane 62 Slope 7 Second end section 8 Wear detection groove 81 First groove inner surface 82 Second groove inner surface 81E End of groove width (inner surface side of first groove) 82E End of groove width (inner surface side of second groove) 81P Maximum groove depth position 11 Sliding device 12 Counterpart D1 Groove depth L1 groove width L2: The width of the exposed surface of the sliding layer L3 Length of wear detection groove T1 Thickness of the sliding layer T2 Backing layer thickness X: Direction of movement of the mating part FP An imaginary plane perpendicular to the direction of movement of the mating part θ1 Tilt angle θ2 Tilt angle

Claims

1. A flat-plate-shaped sliding member including a back metal layer having a back surface and a sliding layer having a sliding surface for sliding against a reciprocating counter member, The sliding layer is made of a copper alloy, The interfaces between the back surface, the sliding surface, and the back metal layer of the sliding layer are parallel to each other, The sliding member has a first end surface portion on a leading side in each moving direction of the counter member, the first end surface portion has an exposed surface on which the sliding layer is exposed, At least one of the first end faces has a wear detection groove formed in the exposed surface, The wear detection groove has a constant groove depth and a constant groove width, is parallel to the sliding surface, and extends in a direction perpendicular to the moving direction of the mating member. the surface of the wear detection groove includes a first groove inner surface between a maximum position of the groove depth of the wear detection groove and one end of the groove width, and a second groove inner surface between the maximum position of the groove depth of the wear detection groove and the other end of the groove width, A sliding member, wherein the first groove inner surface and the second groove inner surface are inclined with respect to the exposed surface to which the wear detection groove is adjacent.

2. 2. The sliding member according to claim 1, wherein the first end surface portion is formed of a vertical surface that is parallel to an imaginary plane perpendicular to the moving direction of the counter member.

3. 2. The sliding member according to claim 1, wherein the first end surface portion comprises a vertical surface adjacent to the back surface and parallel to a virtual plane perpendicular to a moving direction of the counter member, and an inclined surface adjacent to the vertical surface and the sliding surface and inclined at a certain angle with respect to the vertical surface.

4. 4. The sliding member according to claim 3, wherein the wear detection groove is located within the inclined surface.

5. 4. The sliding member according to claim 3, wherein the wear detection groove is located within the vertical surface.

6. 4. The sliding member according to claim 3, wherein an angle θ1 between said inclined surface and said vertical surface is in the range of 30° to 60°.

7. 2. The sliding member according to claim 1, wherein an angle θ2 between the first groove inner surface or the second groove inner surface of the wear detection groove and the exposed surface adjacent to the wear detection groove is 30° to 60°.

8. 2. The sliding member according to claim 1, wherein the wear detection groove is formed over the entire width of the exposed surface.

9. 2. The sliding member according to claim 1, wherein the wear detection groove is formed on a part of the width of the exposed surface.

Citation Information

Patent Citations

  • Sliding member

    JP2017207117A