Panel molding method

By forming the flange of the outer panel into an uneven shape and using a hemming roller to flatten and crush the unevenness, the method addresses the issue of excessive bending deformation, ensuring improved appearance quality during panel integration.

JP2024166760AInactive Publication Date: 2024-11-29TOYOTA SHATAI KK
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023083083
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 2024166760000001_ABST
    Figure 2024166760000001_ABST
Patent Text Reader

Abstract

To provide a panel molding method that can suppress deflection deformation of an outer panel that occurs when folding a flange of the outer panel to integrate the same with an inner panel.SOLUTION: A panel molding method has: a first step S101 at which a flange 12 is molded so that a flange 12 of an outer panel 10 is in an upright state with respect to a body part 11 and has an uneven shape in a thickness direction; a second step S102 at which an inner panel 20 is superposed on a top face of the body part 11 in the state that the outer panel 10 is located so that the flange 12 extends upward; and a third step S103 at which the flange 12 of the outer panel 10 is so molded as to be bent to the inner panel 20 side by a hemming roller 40 to be integrated with the inner panel 20. At the third step S103, the hemming roller 40 is moved so that the hemming roller 40 rolls along a flange edge while deforming irregularity of the flange 12 of the outer panel 10 into a flat shape and collapsing the same.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a panel forming method. [Background technology]

[0002] The following Patent Document 1 discloses a conventional roller hemming method for folding back the flange of an outer panel of an automobile vehicle door to integrate it with an inner panel. This roller hemming method generally includes a flange erecting process in which the flange of the outer panel on which the inner panel is superimposed is first bent into an upright state, and a hemming forming process in which the flange erected in the flange erecting process is bent toward the inner panel by a hemming roller. In the hemming forming process, a hemming roller held by a teaching / playback type robot is generally used. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 6-91330 Summary of the Invention [Problem to be solved by the invention]

[0004] In the hemming process, the hemming roller is pressed against the flange of the outer panel and rolled in the flange width direction while moving toward the inner panel. At this time, the flange of the outer panel is crushed and deformed toward the inner panel by the hemming roller, and the main body of the outer panel is deflected and deformed due to the deformation stress generated at this time. If the amount of deflection and deformation of the main body of the outer panel becomes large, a problem may occur in that the appearance quality of the outer panel is deteriorated.

[0005] The present invention has been made in consideration of such problems, and aims to provide a panel molding method that can suppress the bending deformation of the outer panel that occurs when the flange of the outer panel is folded back to be integrated with the inner panel. [Means for solving the problem]

[0006] One aspect of the present invention is a flange erecting step of forming a flange of the outer panel so that the flange stands upright relative to the main body and has an uneven shape in a thickness direction; a panel overlapping step of overlapping an inner panel on an upper surface of the main body portion with the outer panel obtained in the flange erecting step disposed so that the flange extends upward; a hemming process for bending the flange of the outer panel toward the inner panel by a hemming roller after the panel overlapping process, thereby integrating the outer panel with the inner panel; having a panel forming method, in which, in the hemming step, the hemming roller is moved so as to roll along an end edge of the flange while deforming and squashing unevenness of the flange of the outer panel into a flat shape; is located. Effect of the Invention

[0007] In the panel forming method of the above aspect, first, in a flange erecting step, the flange of the outer panel is formed so that it stands upright relative to the main body and has an uneven shape in the thickness direction. Next, in a panel overlapping step, the outer panel obtained in the flange erecting step is placed so that the flange extends upward, and an inner panel is overlapped on the top surface of the main body. The inner panel is laid on the outer panel. Finally, in the hemming process, the flange of the outer panel is bent toward the inner panel with a hemming roller to integrate it with the inner panel. In this hemming process, the hemming roller is moved so that it rolls along the flange edge while flattening the unevenness of the flange of the outer panel.

[0008] In the panel forming method of this embodiment, the flange of the outer panel is formed in advance into an uneven shape in the flange erecting process. When the uneven portion of the flange receives a forming load from the hemming roller in the hemming process, the unevenness is eliminated and deformation is permitted so that the flange extends linearly. In other words, the uneven portion of the flange first becomes a deformation allowance for the forming load from the hemming roller, and it is possible to prevent the flange from being stretched until the unevenness is eliminated. Then, after the unevenness is eliminated, the process moves to substantial squashing of the flange. In contrast, in the case of a conventional flat flange without unevenness, it is assumed that the flange will be stretched from the beginning due to the forming load from the hemming roller.

[0009] Therefore, the deformation stress generated when the uneven flange is crushed to the final bending position is smaller than the deformation stress generated when a conventional flat flange without any unevenness is crushed to the final bending position. Therefore, if the flange of the outer panel is made uneven in advance in the standing state, which is the stage before the hemming process, the deformation stress generated during the subsequent hemming can be kept low, and the main body of the outer panel can be prevented from being significantly deflected and deformed due to the deformation stress at this time. As a result, it is possible to prevent a deterioration in the appearance quality of the outer panel.

[0010] As described above, according to the above-mentioned aspect, it is possible to provide a panel forming method that can suppress bending deformation of the outer panel that occurs when the flange of the outer panel is folded back to be integrated with the inner panel. [Brief description of the drawings]

[0011] [Figure 1] FIG. 2 is a perspective view of a molded body molded by the panel molding method of the first embodiment. [Diagram 2] 3 is a flowchart of a panel molding method according to the first embodiment. [Diagram 3] 3 is a side view showing the state when the first step of FIG. 2 is performed. FIG. [Figure 4] A view of Figure 3 from the direction of arrow A. [Diagram 5] 3 is a side view of the outer panel and the inner panel after the first step in FIG. 2 is performed. [Figure 6] A view of Figure 5 from the direction of arrow B. [Figure 7] 6 is a perspective view showing the outer panel of FIG. 5 in a upside-down state. [Figure 8] 3 is a perspective view of the outer panel and the inner panel when the second step in FIG. 2 is performed. FIG. [Figure 9] 3 is a perspective view of the outer panel and the inner panel immediately before the third step in FIG. 2 is performed. [Figure 10] 3 is a perspective view of the outer panel and the inner panel when the third step in FIG. 2 is performed. FIG. [Figure 11] 3 is a perspective view of the outer panel and the inner panel when the third step in FIG. 2 is performed. FIG. [Figure 12] 3 is a side view showing the outer panel and the inner panel when the third step in FIG. 2 is performed, with the flange of the outer panel in a pre-bending position; FIG. [Figure 13] 3 is a side view showing the outer panel and the inner panel when the third step in FIG. 2 is performed, with the flange of the outer panel in a final bending position. FIG. [Figure 14] 2 is a perspective view of a door outer panel and a door inner panel constituting a vehicle door before being molded; FIG. [Figure 15] 13 is a diagram showing a first modified example of the concave and convex shape at the flange end edge of the flange of the outer panel. FIG. [Figure 16] 13 is a diagram showing a second modified example of the concave and convex shape at the flange end edge of the outer panel flange. FIG. [Figure 17] 13 is a diagram showing a third modified example of the concave and convex shape at the flange end edge of the flange of the outer panel. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Preferred embodiments of the above aspects are described below.

[0013] In the panel molding method of the above aspect, it is preferable that in the flange erecting step, a bending blade having a blade surface with an uneven shape is used, and the flange is bent from an initial deployed position to an upright position with the bending blade to obtain the upright state, and that when the flange is bent, the flange is made to have an uneven shape in accordance with the uneven shape of the blade surface.

[0014] According to this panel forming method, the first process of making the flange of the outer panel stand upright using a bending blade with an uneven blade surface and the second process of making the flange uneven can be carried out in parallel, which makes it possible to shorten the time required for the flange erection process compared to carrying out the first and second processes separately.

[0015] In the panel molding method of the above aspect, in the flange setting process, it is preferable to mold the flange so that the boundary line of the concave and convex portions in the flange of the outer panel extends across the rolling direction in which the hemming roller rolls in the hemming forming process.

[0016] According to this panel forming method, the boundary line of the unevenness in the flange of the outer panel extends in a direction intersecting the rolling direction of the hemming roller, so that when the hemming roller hems the unevenness of the flange, the unevenness can be effectively used as a deformation allowance, which makes it possible to suppress the deformation stress generated during hemming.

[0017] In the panel molding method of the above aspect, the outer panel and the inner panel are respectively a door outer panel and a door inner panel of a vehicle door, and it is preferable that the door outer panel has a curved shape with a concave surface on which the door inner panel is overlapped.

[0018] According to this panel forming method, forming the flange of the curved door outer panel into an upright state is a shrink forming in which the flange shrinks in the flange width direction. On the other hand, hemming the flange in the upright state of this door outer panel is an elongation forming in which the flange stretches in the flange width direction. Therefore, if the flange of the curved door outer panel is made uneven in the upright state, which is a stage prior to hemming, the effect of preventing the flange from stretching during the subsequent hemming is particularly remarkable.

[0019] Hereinafter, specific embodiments of the panel molding method according to the above aspect will be described with reference to the drawings.

[0020] In this specification and drawings, unless otherwise specified, the panel width direction is the X-axis direction, the panel up-down direction is the Y-axis direction, and the panel depth direction is the Z-axis direction.

[0021] (Embodiment 1) 1. Structure of Molded Body W As shown in Fig. 1, the formed body W is an integrated outer panel 10 and inner panel 20. This formed body W is used, for example, as various parts that constitute the body of an automobile. The formed body W is formed by folding back the flange 12 in an expanded state with the end portion 21 of the inner panel 20 overlapping the main body portion 11 of the outer panel 10. Both the outer panel 10 and the inner panel 20 are made of steel plates.

[0022] 2.Panel forming method The panel molding method of the first embodiment is a method for forming a molded body W shown in Fig. 1. In this panel molding method, the first step S101 to the third step S103 in Fig. 2 are sequentially performed. If necessary, another step may be added, or each step may be divided into a plurality of steps.

[0023] 2-1. Flange setting process The first step S101 in Fig. 2 is a flange erecting process for forming the flange 12 of the outer panel 10 so that the flange 12 stands upright relative to the main body 11 and has an uneven shape in the thickness direction. In this first step S101, as shown in Figs. 3 to 6, a bending blade 30 having an uneven blade surface 31 is used. The bending blade 30 has a blade surface 31 that is uneven due to convex blade portions 31a and concave blade portions 31b that are alternately provided in the X-axis direction (see Fig. 6). The first step S101 is one form of plastic processing (press processing) that utilizes plastic deformation of the workpiece.

[0024] 3 and 4, in the first step S101, first, the main body 11 of the outer panel 10 is sandwiched between the lower blade 32 and the pad 33. Then, while the bending blade 30 is pressed against the surface (lower surface in the Y-axis direction) of the flange 12 at the initial deployed position P1, the bending blade 30 is moved downward so as to bend the flange 12 in the bending direction D1 (see FIG. 5). At this time, the flange 12 rotates in the bending direction D1 (see FIG. 3) from the initial deployed position P1 to the standing position P2 around the portion to be bent 12b.

[0025] 5, the flange 12 of the outer panel 10 is pushed and bent by the bending blade 30 to an upright position P2, and is plastically deformed to have an uneven shape in the thickness direction in accordance with the uneven shape of the blade surface 31 of the bending blade 30. That is, a convex portion 14 is formed on the flange 12 by the convex blade portion 31a of the blade surface 31, and a concave portion 13 is formed on the flange 12 by the concave blade portion 31b of the blade surface 31.

[0026] 6, in this embodiment, regarding the uneven shape of the flange 12, the portions of the flange 12 that protrude rearward in the bending direction D1 are called recesses 13, and the portions that protrude forward in the bending direction D1 are called protrusions 14. According to the first step S101 of this embodiment, the flange 12 is formed so that the recesses 13 and the protrusions 14 are provided alternately and continuously in the X-axis direction.

[0027] As shown in Fig. 7, the recesses 13 and protrusions 14 of the flange 12 in the standing state are both configured so that the recess depth gradually increases from the intended bending portion 12b side toward the flange end edge 12a side. As shown in Fig. 6, in this embodiment, the recess depth at the flange end edge 12a of the flange 12 in the standing state is approximately the same for the recesses 13 and the protrusions 14. In this way, the flange 12 can be uniformly deformed in the X-axis direction during hemming.

[0028] 7, in this embodiment, when the flange 12 in the upright state is viewed from the Z-axis direction, the imaginary boundary line L between the recessed portion 13 and the protruding portion 14 of the flange 12 is formed in a roughly zigzag shape. This is because, due to the structure of the flange 12, deformation of the portion on the intended bending portion 12b side is restricted compared to the portion on the flange end edge 12a side. At this time, the boundary line L extends so as to cross the rolling direction D2 (see FIG. 9) in which the hemming roller 40 rolls in the third step S103 described later.

[0029] According to the first step S101, the first process of making the flange 12 of the outer panel 10 stand up by using the bending blade 30 having the uneven blade surface 31, and the second process of making the flange 12 uneven can be performed in parallel. This makes it possible to reduce the time required for the first step S101 compared to performing these two processes separately.

[0030] 2-2. Panel stacking process 2 is a panel overlapping step in which the inner panel 20 is overlapped on the outer panel 10. In this second step S102, first, the outer panel 10 in FIG. 5 is turned upside down so that the flange 12 extends upward (see FIG. 7). Then, as shown in FIG. 8, in this second step S102, the folded end 21 of the inner panel 20 is set so as to overlap the upper surface of the main body 11 of the outer panel 10. At this time, the folded end 21 of the inner panel 20 is positioned so that its edge 21a is close to the intended bending portion 12b of the flange 12 of the outer panel 10.

[0031] 2-3. Hemming process 2 is a hemming process that follows the second step S102 and bends the flange 12 of the outer panel 10, formed in the flange setting process in the first step S101, toward the inner panel 20 using a hemming roller 40 to integrate it with the inner panel 20. Although not shown in the figure, the hemming roller 40 is held by a teaching playback type robot, and the position and posture of the hemming roller 40 are controlled by controlling this robot.

[0032] In the third step S103, as shown in Figs. 9 to 12, the hemming roller 40 is moved so as to roll along the flange edge 12a while deforming and squashing the unevenness of the flange 12 of the outer panel 10 into a flat shape. The "rolling" here refers to the action of the hemming roller 40 rolling on the surface of the flange 12 and rotating about the imaginary axis line 41. At this time, the hemming roller 40 is moved in the rolling direction D2 (see Figs. 9 to 11) and in the bending direction D3 (see Fig. 12). The third step S103 is a form of plastic processing (press processing) that utilizes the plastic deformation of the workpiece, similar to the first step S101.

[0033] 10 and 11, according to the third step S103, the unevenness of the flange 12 of the outer panel 10 is successively flattened and deformed by the hemming roller 40. At this time, the line lengths of the curved recesses 13 and protrusions 14 of the flange 12 are the deformation allowances when the recesses 13 and protrusions 14 are flattened and deformed into straight lines by the hemming roller 40. The longer the line lengths of the recesses 13 and protrusions 14 are (the deeper the recesses are), the more the deformation allowance can be increased.

[0034] According to the third step S103, when the flange 12 of the outer panel 10 is viewed from the X-axis direction, as shown in Fig. 12, the flange 12 buckles in the bending direction D3 from the standing position P2 to the preliminary bending position P3 around the intended bending portion 12b. As shown in Fig. 13, the flange 12 further buckles in the bending direction D3 from the preliminary bending position P3 to the main bending position P4. As a result, the end portion 21 of the inner panel 20 is sandwiched between the main body portion 11 of the outer panel 10 and the flange 12 and integrated with them (see Figs. 1 and 13).

[0035] 3. Effects According to the above-mentioned first embodiment, the following advantageous effects can be obtained.

[0036] In the panel forming method of the first embodiment, the flange 12 of the outer panel 10 is formed in advance into an uneven shape in the first step S101 (flange erection step). When the uneven portion of the flange 12 receives a forming load from the hemming roller 40 in the third step (hemming step), the unevenness is eliminated and deformation is permitted so that the flange 12 extends linearly. In other words, the uneven portion of the flange 12 first becomes a deformation margin against the forming load from the hemming roller 40, and it is possible to prevent the flange 12 from being stretched until the unevenness is eliminated. Then, after the unevenness is eliminated, the flange 12 is substantially crushed. In contrast, in the case of a conventional flat flange 12 without unevenness, it is assumed that the flange 12 will be stretched from the beginning due to the forming load from the hemming roller 40.

[0037] Therefore, the deformation stress generated when the uneven flange 12 is crushed to the final bending position is smaller than the deformation stress generated when a conventional flat flange 12 without any unevenness is crushed to the final bending position. Therefore, if the flange 12 of the outer panel 10 is made uneven in advance in the upright state, which is the stage prior to the third step S103 (hemming process), the deformation stress generated during the subsequent hemming can be kept low, and the main body 11 of the outer panel 10 can be prevented from being significantly deflected and deformed due to the deformation stress at this time. As a result, it is possible to prevent the appearance quality of the outer panel 10 from deteriorating.

[0038] In particular, when the boundary line L of the unevenness in the flange 12 of the outer panel 10 extends so as to cut across the rolling direction D2 of the hemming roller 40, the unevenness can be effectively used as a deformation allowance when the hemming roller 40 hems the unevenness of the flange 12. This makes it possible to further reduce the deformation stress that occurs during hemming.

[0039] Therefore, according to the panel molding method of the first embodiment, it is possible to suppress bending deformation of the outer panel 10 that occurs when the flange 12 of the outer panel 10 is folded back and integrated with the inner panel 20.

[0040] The panel molding method of the first embodiment can be used, for example, to mold a vehicle door. As shown in Fig. 14, the outer panel 10 and the inner panel 20 become the door outer panel and the door inner panel of the vehicle door, respectively. The outer panel 10 (door outer panel) has a curved shape with a concave surface on which the inner panel 20 (door inner panel) is laid.

[0041] When forming a vehicle door having the above configuration, forming the flange 12 of the curved outer panel 10 into an upright state is a shrink forming in which the flange 12 shrinks in the flange width direction (X-axis direction). On the other hand, hemming the flange 12 in the upright state of the outer panel 10 is an stretch forming in which the flange 12 stretches in the flange width direction (X-axis direction). Therefore, if the flange 12 of the curved outer panel 10 is made uneven in the upright state, which is a stage prior to hemming, the effect of preventing stretch forming of the flange 12 during the subsequent hemming is particularly prominent.

[0042] The present invention is not limited to the exemplary embodiment described above, and various applications and modifications are possible without departing from the scope of the present invention. For example, the following embodiments can be embodied by applying the above embodiment.

[0043] In the above embodiment, the flange edge 12a of the flange 12 in the standing state has an uneven shape as shown in Fig. 6, but this uneven shape is not limited to that shown in Fig. 6, and any appropriate uneven shape may be adopted as necessary. For example, as shown in Fig. 15, a structure having an uneven shape (first modified example) in which a plurality of recesses 13 of the flange 12 are arranged intermittently and at equal intervals in the X-axis direction with flat portions 15 sandwiched therebetween, as shown in Fig. 16, a structure having an uneven shape (second modified example) in which a plurality of protrusions 14 of the flange 12 are arranged intermittently and at equal intervals in the X-axis direction with flat portions 15 sandwiched therebetween, as shown in Fig. 17, a structure having an uneven shape (third modified example) in which a plurality of recesses 13 and protrusions 14 are arranged alternately in the X-axis direction and intermittently with flat portions 15 sandwiched therebetween, and the like may be adopted.

[0044] In the above embodiment, the process of making the flange 12 of the outer panel 10 stand up and the process of making the flange 12 have an uneven shape are performed in parallel by the bending blade 30, but instead of this, the process of making the flange 12 stand up may be performed after the process of making the flange 12 of the outer panel 10 have an uneven shape. In short, it is sufficient that the flange 12 has been formed to have an uneven shape in the thickness direction prior to the hemming process, which is the third step S103. [Explanation of symbols]

[0045] 10...outer panel, 11...main body, 12...flange, 12a...flange edge, 30...bending blade, 31...blade surface, 40...hemming roller, D2...rolling direction, L...boundary line, P1...initial deployment position, P2...standing position, S101-S103...panel forming method, S101...first step (flange setting process), S102...second step (panel overlapping process), S103...third step (hemming forming process)

Claims

1. a flange erecting step of forming a flange of the outer panel so that the flange stands upright relative to the main body and has an uneven shape in a thickness direction; a panel overlapping step of overlapping an inner panel on an upper surface of the main body portion with the outer panel obtained in the flange erecting step disposed so that the flange extends upward; a hemming process for bending the flange of the outer panel toward the inner panel by a hemming roller after the panel overlapping process, thereby integrating the flange with the inner panel; having In the hemming step, the hemming roller is moved so as to roll along the flange edge while deforming and squashing the unevenness of the flange of the outer panel into a flat shape.

2. 2. The panel molding method according to claim 1, wherein in the flange erecting step, a bending blade having a blade surface with an uneven shape is used, and the flange is pushed and bent by the bending blade from an initial deployed position to an upright position to be in the upright state, and when the flange is pushed and bent, the flange is made to have an uneven shape in accordance with the uneven shape of the blade surface.

3. 3. The panel forming method according to claim 1, wherein in the flange setting process, the flange is formed so that a boundary line of the concave and convex portions in the flange of the outer panel extends across a rolling direction in which the hemming roller rolls in the hemming forming process.

4. The panel molding method according to any one of claims 1 to 3, wherein the outer panel and the inner panel are respectively a door outer panel and a door inner panel of a vehicle door, and the door outer panel has a curved shape with a concave surface on which the door inner panel is overlapped.

Citation Information

Patent Citations

  • JP1988002518U

  • Roller processing method for raising flange and device therefor

    JP1994210358A

  • Multipurpose roller hemming method and device therefor

    JP1995314054A

  • Roller for hemming, roller hemmning apparatus and roller hemming method

    JP2007229723A

  • Hemming apparatus and hemming method

    JP2010194568A