Semiconductor device

The semiconductor device design addresses miniaturization and integration challenges by using a conductor-insulator configuration with IGZO and microwave treatment, achieving improved reliability and reduced power consumption with enhanced transistor performance.

JP2024167372AInactive Publication Date: 2024-12-03SEMICON ENERGY LAB CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024151274
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2019-07-12
Filing Date
2024-09-03
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing semiconductor devices face challenges in miniaturization, integration, storage capacity, reliability, electrical characteristics, and power consumption, with variations in transistor characteristics and on-state current being key issues.

Method used

A semiconductor device design featuring a specific conductor and insulator configuration with overlapping capacitive elements, utilizing indium-gallium-zinc oxide (IGZO) with controlled oxygen vacancies and impurities, and employing microwave treatment to enhance transistor performance.

Benefits of technology

The design enables miniaturization, high integration, large storage capacity, reduced transistor characteristic variations, improved reliability, and low power consumption, with enhanced on-state current and frequency characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024167372000001_ABST
    Figure 2024167372000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor device that can be miniaturized or highly integrated.SOLUTION: A semiconductor device includes: a first conductor positioned over a substrate; an oxide positioned in contact with a top surface of the first conductor; a second conductor, a third conductor and a fourth conductor positioned over the oxide; a first insulator in which a first opening and a second opening are formed, the first insulator being positioned over the second conductor to the fourth conductor; a second insulator positioned in the first opening; a fifth conductor positioned over the second insulator; a third insulator positioned in the second opening: and a sixth conductor positioned over the third insulator. The third conductor is positioned to overlap with the first conductor. The first opening is formed to overlap with a region between the second conductor and the third conductor. The second opening is formed to overlap with a region between the third conductor and the fourth conductor.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] 1. Field of the Invention An embodiment of the present invention relates to a transistor, a semiconductor device, and an electronic device, or to a manufacturing method of a semiconductor device, or to a semiconductor wafer and a module.

[0002] In this specification and the like, a semiconductor device refers to any device that can function by utilizing semiconductor characteristics. Semiconductor elements such as transistors, semiconductor circuits, arithmetic devices, and memory devices are all embodiments of semiconductor devices. Display devices (such as liquid crystal display devices and light-emitting display devices), projection devices, lighting devices, electro-optical devices, power storage devices, memory devices, semiconductor circuits, imaging devices, electronic devices, and the like may be considered to include semiconductor devices.

[0003] Note that one aspect of the present invention is not limited to the above technical field. One aspect of the invention disclosed in the present specification etc. relates to an object, a method, or a manufacturing method. Alternatively, one aspect of the present invention relates to a process, a machine, a manufacture, or a composition of matter. [Background technology]

[0004] In recent years, the development of semiconductor devices has progressed, particularly in LSIs, CPUs, and memories. A CPU is a collection of semiconductor elements that have semiconductor integrated circuits (at least transistors and memories) separated from a semiconductor wafer and on which electrodes that serve as connection terminals are formed.

[0005] Semiconductor circuits (IC chips) such as LSIs, CPUs, and memories are mounted on circuit boards, such as printed wiring boards, and used as components in a variety of electronic devices.

[0006] In addition, a technology for constructing a transistor using a semiconductor thin film formed on a substrate having an insulating surface is attracting attention. Such transistors are widely used in electronic devices such as integrated circuits (ICs) and image display devices (also simply referred to as display devices). Silicon-based semiconductor materials are widely known as semiconductor thin films that can be used in transistors, but oxide semiconductors are also attracting attention as other materials.

[0007] It is also known that a transistor using an oxide semiconductor has an extremely low leakage current in a non-conducting state. For example, a low-power consumption CPU that utilizes the low leakage current characteristic of a transistor using an oxide semiconductor has been disclosed (see Patent Document 1). In addition, a memory device that can retain stored data for a long period of time by utilizing the low leakage current characteristic of a transistor using an oxide semiconductor has been disclosed (see Patent Document 2).

[0008] Furthermore, in recent years, with the trend toward smaller and lighter electronic devices, there is an increasing demand for higher density integrated circuits, and there is also a demand for improved productivity in the manufacture of semiconductor devices including integrated circuits. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2012-257187 A [Patent Document 2] JP 2011-151383 A Summary of the Invention [Problem to be solved by the invention]

[0010] An object of one embodiment of the present invention is to provide a semiconductor device that can be miniaturized or highly integrated. Another object of one embodiment of the present invention is to provide a semiconductor device with a large storage capacity. Another object of one embodiment of the present invention is to provide a semiconductor device with little variation in transistor characteristics. Another object of one embodiment of the present invention is to provide a semiconductor device with high reliability. Another object of one embodiment of the present invention is to provide a semiconductor device with good electrical characteristics. Another object of one embodiment of the present invention is to provide a semiconductor device with high on-state current. Another object of one embodiment of the present invention is to provide a semiconductor device with low power consumption. Another object of one embodiment of the present invention is to provide a novel semiconductor device.

[0011] Note that the description of these problems does not preclude the existence of other problems. Note that one embodiment of the present invention does not necessarily solve all of these problems. Note that problems other than these will become apparent from the description of the specification, drawings, claims, etc., and it is possible to extract problems other than these from the description of the specification, drawings, claims, etc. [Means for solving the problem]

[0012] One embodiment of the present invention is a semiconductor device including a first conductor disposed over a substrate, an oxide disposed in contact with an upper surface of the first conductor, a second conductor, a third conductor, and a fourth conductor disposed on the oxide, a first insulator disposed over the second to fourth conductors and having a first opening and a second opening formed therein, a second insulator disposed in the first opening, a fifth conductor disposed on the second insulator, a third insulator disposed in the second opening, and a sixth conductor disposed on the third insulator, wherein the third conductor is disposed overlapping the first conductor, the first opening is formed overlapping a region between the second conductor and the third conductor, and the second opening is formed overlapping a region between the third conductor and the fourth conductor.

[0013] In the above, the semiconductor device may have a first capacitive element and a second capacitive element, the first capacitive element being electrically connected to the second conductor, and the second capacitive element being electrically connected to the fourth conductor. Also, in the above, it is preferable that the first capacitive element is disposed on the second conductor, and the second capacitive element is disposed on the fourth conductor.

[0014] In the above, it is preferable that the first conductor is connected to a wiring provided below the first conductor, and that the second insulator contacts an upper surface of the oxide and a side surface of the first insulator, and the third insulator contacts an upper surface of the oxide and a side surface of the first insulator.

[0015] In the above, it is preferable that the oxide comprises a first oxide and a second oxide on the first oxide, the first oxide and the second oxide comprise indium, an element M (M is one or more selected from gallium, aluminum, yttrium, and tin), and zinc, and the atomic ratio of indium to the element M in the first oxide is smaller than the atomic ratio of indium to the element M in the second oxide.

[0016] Another embodiment of the present invention includes forming a first conductor on a substrate, forming an oxide film in contact with an upper surface of the first conductor, forming a first conductive film on the oxide film, processing the oxide film and the first conductive film into an island shape to form an oxide and a second conductor, forming a first insulator covering the oxide and the second conductor, removing a portion of the first insulator to form a first opening and a second opening overlapping the second conductor, removing a portion of the second conductor overlapping the first opening and the second opening, and forming a third conductor, a fourth conductor, and a fifth conductor. a fourth conductor is disposed overlapping the first conductor; a region of the oxide that does not overlap with the third to fifth conductors is exposed; a first insulating film is formed in contact with an upper surface of the oxide; microwave treatment is performed in an atmosphere containing oxygen; a second conductive film is formed on the first insulating film; CMP treatment is performed on the first insulating film and the second conductive film until an upper surface of the first insulator is exposed; a second insulator and a sixth conductor are formed in the first opening; and a third insulator and a seventh conductor are formed in the second opening. Effect of the Invention

[0017] According to one embodiment of the present invention, a semiconductor device that can be miniaturized or highly integrated can be provided. According to one embodiment of the present invention, a semiconductor device with large storage capacity can be provided. According to one embodiment of the present invention, a semiconductor device with little variation in transistor characteristics can be provided. According to one embodiment of the present invention, a semiconductor device with high reliability can be provided. According to one embodiment of the present invention, a semiconductor device with good electrical characteristics can be provided. According to one embodiment of the present invention, a semiconductor device with high on-state current can be provided. According to one embodiment of the present invention, a semiconductor device that can be miniaturized or highly integrated can be provided. According to one embodiment of the present invention, a semiconductor device with low power consumption can be provided. According to one embodiment of the present invention, a novel semiconductor device can be provided.

[0018] Note that the description of these effects does not preclude the existence of other effects. Note that one embodiment of the present invention does not need to have all of these effects. Note that effects other than these will become apparent from the description in the specification, drawings, claims, etc., and it is possible to extract effects other than these from the description in the specification, drawings, claims, etc. [Brief description of the drawings]

[0019] [Figure 1] 1A, 1B, 1C, and 1D are a top view and a cross-sectional view of a semiconductor device according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view of a semiconductor device according to one embodiment of the present invention. [Diagram 3] Figure 3A is a diagram for explaining the classification of IGZO crystal structures, Figure 3B is a diagram for explaining the XRD spectrum of a CAAC-IGZO film, and Figure 3C is a diagram for explaining the ultrafine electron beam diffraction pattern of a CAAC-IGZO film. [Figure 4] 4A, 4B, 4C, and 4D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Diagram 5] 5A, 5B, 5C, and 5D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 6] 6A, 6B, 6C, and 6D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 7] 7A, 7B, 7C, and 7D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 8] 8A, 8B, 8C, and 8D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 9] 9A, 9B, 9C, and 9D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 10]10A, 10B, 10C, and 10D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 11] 11A, 11B, 11C, and 11D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 12] 12A, 12B, 12C, and 12D are top views and cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 13] FIG. 13 is a top view illustrating a microwave processing apparatus according to one embodiment of the present invention. [Figure 14] FIG. 14 is a cross-sectional view illustrating a microwave processing apparatus according to one embodiment of the present invention. [Figure 15] FIG. 15 is a cross-sectional view illustrating a microwave processing apparatus according to one embodiment of the present invention. [Figure 16] 16A, 16B, 16C, and 16D are a top view and a cross-sectional view of a semiconductor device according to one embodiment of the present invention. [Figure 17] 17A and 17B are cross-sectional views of a semiconductor device according to one embodiment of the present invention. [Figure 18] FIG. 18 is a cross-sectional view illustrating a configuration of a memory device according to one embodiment of the present invention. [Figure 19] FIG. 19 is a cross-sectional view illustrating a configuration of a memory device according to one embodiment of the present invention. [Figure 20] 20A and 20B are cross-sectional views of a semiconductor device according to one embodiment of the present invention. [Figure 21] FIG. 21 is a cross-sectional view of a semiconductor device according to one embodiment of the present invention. [Figure 22] FIG. 22 is a cross-sectional view of a semiconductor device according to one embodiment of the present invention. [Figure 23] 23A and 23B are block diagrams illustrating configuration examples of a memory device according to one embodiment of the present invention. [Figure 24] 24A, 24B, and 24C are circuit diagrams illustrating configuration examples of a memory device according to one embodiment of the present invention. [Diagram 25]25A and 25B are schematic diagrams of a semiconductor device according to one embodiment of the present invention. [Figure 26] 26A and 26B are diagrams illustrating an example of an electronic component according to one embodiment of the present invention. [Figure 27] 27A and 27B are schematic diagrams of a memory device according to one embodiment of the present invention. [Figure 28] 28A, 28B, 28C, 28D, 28E, 28F, 28G, and 28H are diagrams illustrating electronic devices according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] Hereinafter, the embodiments will be described with reference to the drawings. However, it will be easily understood by those skilled in the art that the embodiments can be implemented in many different ways, and that the modes and details can be changed in various ways without departing from the spirit and scope of the present invention. Therefore, the present invention should not be interpreted as being limited to the description of the following embodiments.

[0021] In addition, in the drawings, the size, thickness of layers, or areas may be exaggerated for clarity. Therefore, the drawings are not necessarily limited to the scale. The drawings are schematic illustrations of ideal examples, and are not limited to the shapes or values ​​shown in the drawings. For example, in an actual manufacturing process, layers, resist masks, etc. may be unintentionally thinned by etching or other processes, but this may not be reflected in the drawings to facilitate understanding. In addition, in the drawings, the same reference numerals are used in common between different drawings for the same parts or parts having similar functions, and repeated explanations may be omitted. In addition, when referring to similar functions, the same hatch pattern may be used and no particular reference numeral may be attached.

[0022] In order to facilitate understanding of the invention, particularly in top views (also called "plan views") and perspective views, some components may be omitted from the drawings. Also, some hidden lines may be omitted from the drawings.

[0023] In addition, in this specification, ordinal numbers such as first, second, etc. are used for convenience and do not indicate the order of steps or stacking. Therefore, for example, "first" can be appropriately replaced with "second" or "third" for explanation. In addition, the ordinal numbers described in this specification and the like may not match the ordinal numbers used to specify one embodiment of the present invention.

[0024] In addition, in this specification, the terms "above" and "below" indicating the arrangement are used for convenience in order to explain the positional relationship between the components with reference to the drawings. In addition, the positional relationship between the components changes as appropriate depending on the direction in which each component is depicted. Therefore, the terms are not limited to those described in the specification, and can be rephrased appropriately depending on the situation.

[0025] For example, when it is explicitly stated in this specification that X and Y are connected, the case where X and Y are electrically connected, the case where X and Y are functionally connected, and the case where X and Y are directly connected are considered to be disclosed in this specification. Therefore, it is not limited to a specific connection relationship, for example, a connection relationship shown in a figure or text, and a connection relationship other than that shown in a figure or text is also considered to be disclosed in the figure or text. Here, X and Y are objects (for example, a device, an element, a circuit, wiring, an electrode, a terminal, a conductive film, a layer, etc.).

[0026] In this specification, a transistor is an element having at least three terminals including a gate, a drain, and a source. A region where a channel is formed between the drain (drain terminal, drain region, or drain electrode) and the source (source terminal, source region, or source electrode) (hereinafter, also referred to as a channel formation region) is provided, and a current can flow between the source and the drain through the channel formation region. In this specification, a channel formation region refers to a region through which a current mainly flows.

[0027] Furthermore, the functions of the source and drain may be interchanged when transistors of different polarities are used, when the direction of current changes during circuit operation, etc. For this reason, in this specification and the like, the terms source and drain may be used interchangeably.

[0028] The channel length refers to, for example, a region where the semiconductor (or a portion in the semiconductor through which current flows when the transistor is on) and the gate electrode overlap in a top view of a transistor, or a distance between the source (source region or source electrode) and the drain (drain region or drain electrode) in a channel formation region. Note that the channel length of one transistor does not necessarily have the same value in all regions. That is, the channel length of one transistor may not be fixed to one value. Therefore, in this specification, the channel length is defined as any one value, maximum value, minimum value, or average value in the channel formation region.

[0029] The channel width refers to, for example, the length of a channel formation region in a vertical direction based on the channel length direction in a region where a semiconductor (or a portion in the semiconductor through which current flows when the transistor is on) and a gate electrode overlap in a top view of a transistor, or in a channel formation region. Note that the channel width does not necessarily have the same value in all regions in one transistor. In other words, the channel width of one transistor may not be determined to a single value. Therefore, in this specification, the channel width is defined as any one value, maximum value, minimum value, or average value in the channel formation region.

[0030] In this specification and the like, depending on the structure of a transistor, the channel width in a region where a channel is actually formed (hereinafter also referred to as an "effective channel width") may differ from the channel width shown in a top view of the transistor (hereinafter also referred to as an "apparent channel width"). For example, when a gate electrode covers a side surface of a semiconductor, the effective channel width may be larger than the apparent channel width, and the influence of this may not be negligible. For example, in a fine transistor in which a gate electrode covers a side surface of a semiconductor, the proportion of a channel formation region formed on the side surface of the semiconductor may be large. In that case, the effective channel width is larger than the apparent channel width.

[0031] In such a case, it may be difficult to estimate the effective channel width by actual measurement. For example, in order to estimate the effective channel width from the design value, it is necessary to assume that the shape of the semiconductor is known. Therefore, if the shape of the semiconductor is not precisely known, it is difficult to accurately measure the effective channel width.

[0032] In this specification, when simply described as a channel width, it may refer to an apparent channel width. Alternatively, when simply described as a channel width, it may refer to an effective channel width. Note that the values ​​of the channel length, channel width, effective channel width, apparent channel width, etc. can be determined by analyzing a cross-sectional TEM image, etc.

[0033] Note that impurities in a semiconductor refer to, for example, anything other than the main components constituting the semiconductor. For example, an element with a concentration of less than 0.1 atomic % can be considered an impurity. The inclusion of impurities can, for example, increase the density of defect states in the semiconductor or reduce the crystallinity. When the semiconductor is an oxide semiconductor, impurities that change the characteristics of the semiconductor include, for example, Group 1 elements, Group 2 elements, Group 13 elements, Group 14 elements, Group 15 elements, and transition metals other than the main components of the oxide semiconductor, such as hydrogen, lithium, sodium, silicon, boron, phosphorus, carbon, and nitrogen. Note that water can also function as an impurity. For example, the inclusion of impurities can cause oxygen deficiencies (V O :oxygen vacancy) may be formed.

[0034] In this specification and the like, silicon oxynitride refers to a material having a composition that contains more oxygen than nitrogen, and silicon nitride oxide refers to a material having a composition that contains more nitrogen than oxygen.

[0035] In this specification and the like, the term "insulator" can be replaced with an insulating film or an insulating layer, the term "conductor" can be replaced with a conductive film or a conductive layer, and the term "semiconductor" can be replaced with a semiconductor film or a semiconductor layer.

[0036] In addition, in this specification, "parallel" refers to a state in which two straight lines are arranged at an angle of -10 degrees or more and 10 degrees or less. Therefore, it also includes the case of -5 degrees or more and 5 degrees or less. "Approximately parallel" refers to a state in which two straight lines are arranged at an angle of -30 degrees or more and 30 degrees or less. "Perpendicular" refers to a state in which two straight lines are arranged at an angle of 80 degrees or more and 100 degrees or less. Therefore, it also includes the case of 85 degrees or more and 95 degrees or less. "Approximately perpendicular" refers to a state in which two straight lines are arranged at an angle of 60 degrees or more and 120 degrees or less.

[0037] In this specification and the like, the term "metal oxide" refers to an oxide of a metal in a broad sense. Metal oxides are classified into oxide insulators, oxide conductors (including transparent oxide conductors), oxide semiconductors (also referred to as oxide semiconductors or simply OS), and the like. For example, when a metal oxide is used for a semiconductor layer of a transistor, the metal oxide may be referred to as an oxide semiconductor. In other words, an OS transistor can be rephrased as a transistor having a metal oxide or an oxide semiconductor.

[0038] In this specification and the like, normally-off means that when no potential is applied to the gate or when a ground potential is applied to the gate, the drain current flowing through the transistor per 1 μm of channel width is 1×10 -20 A or less, 1×10 at 85℃ -18 A or less, or 1×10 at 125°C -16 This means that it is A or lower.

[0039] (Embodiment 1) 1 to 17, an example of a semiconductor device including a transistor 200a and a transistor 200b according to one embodiment of the present invention and a manufacturing method thereof will be described. Note that hereinafter, the transistors 200a and 200b may be collectively referred to as the transistors 200.

[0040] <Example of semiconductor device configuration> A configuration of a semiconductor device having a transistor 200a and a transistor 200b will be described with reference to FIGS. 1A to 1D. FIG. 1A is a top view of the semiconductor device. FIGS. 1B to 1D are cross-sectional views of the semiconductor device. FIG. 1B is a cross-sectional view of a portion indicated by a dashed line A1-A2 in FIG. 1A, and is also a cross-sectional view of the transistors 200a and 200b in the channel length direction. FIG. 1C is a cross-sectional view of a portion indicated by a dashed line A3-A4 in FIG. 1A, and is also a cross-sectional view of the transistor 200a in the channel width direction. FIG. 1D is a cross-sectional view of a portion indicated by a dashed line A5-A6 in FIG. 1A. Note that some elements are omitted from the top view of FIG. 1A for clarity.

[0041] A semiconductor device according to one embodiment of the present invention includes an insulator 212 on a substrate (not shown), an insulator 214 on the insulator 212, a transistor 200 on the insulator 214, an insulator 280 on the transistor 200, an insulator 282 on the insulator 280, and an insulator 283 on the insulator 282. The insulators 212, 214, 280, 282, and 283 function as interlayer films. A conductor 248 (conductor 248a and conductor 248b) is provided so as to be embedded between the insulator 212, the insulator 214, and the transistors 200a and 200b. The conductor 248 is electrically connected to the transistors 200a and 200b and functions as a plug. Note that an insulator 249 is preferably provided in contact with a side surface of the conductor 248 functioning as a plug.

[0042] [Transistor 200] As shown in Figures 1A to 1D, transistor 200a has an insulator 216 on insulator 214, conductor 205 (conductor 205a, conductor 205b, and conductor 205c) arranged so as to be embedded in insulator 216, an insulator 222 on insulator 216 and on conductor 205, an insulator 224 on insulator 222, an oxide 230a on insulator 224, an oxide 230b on oxide 230a, oxide 243a and oxide 243b on oxide 230b, a conductor 242a on oxide 243a, a conductor 242b on oxide 243b, an insulator 250 on oxide 230b, and a conductor 260 (conductor 260a and conductor 260b) located on insulator 250 and overlapping with a portion of oxide 230b.

[0043] Also, as shown in Figures 1A to 1D, transistor 200b has an insulator 216 on insulator 214, a conductor 205 arranged so as to be embedded in insulator 214 or insulator 216, an insulator 222 on insulator 216 and on conductor 205, an insulator 224 on insulator 222, an oxide 230a on insulator 224, an oxide 230b on oxide 230a, oxide 243b and oxide 243c on oxide 230b, a conductor 242b on oxide 243b, a conductor 242c on oxide 243c, an insulator 250 on oxide 230b, and a conductor 260 located on insulator 250 and overlapping with a portion of oxide 230b.

[0044] In the following, the oxide 230a and the oxide 230b may be collectively referred to as the oxide 230. Furthermore, the oxide 243a, the oxide 243b, and the oxide 243c may be collectively referred to as the oxide 243. Furthermore, the conductor 242a, the conductor 242b, and the conductor 242c may be collectively referred to as the conductor 242.

[0045] 1B and 1C, an insulator 275 is provided to cover the insulator 224, the oxide 230, the oxide 243, and the conductor 242. The upper surface of the conductor 260 is disposed so as to substantially coincide with the upper surface of the insulator 250 and the upper surface of the insulator 280. The insulator 282 contacts the upper surfaces of the conductor 260 and the insulator 280, as well as the uppermost part of the insulator 250.

[0046] As shown in FIGS. 1A to 1D, the transistor 200b is provided on the opposite side of the transistor 200a with the conductor 248 interposed therebetween, and has the same structure as the transistor 200a except for the conductor 242 and the oxide 243.

[0047] In the transistor 200a and the transistor 200b, the insulator 212, the insulator 214, the insulator 216, the insulator 222, the insulator 224, the oxide 230a, the oxide 230b, the insulator 275, the insulator 280, the insulator 282, and the insulator 283 are used in common. On the other hand, the conductor 205, the insulator 250, and the conductor 260 are provided in each of the transistor 200a and the transistor 200b. Note that in the transistor 200b, the conductor 205, the insulator 250, and the conductor 260 each have the same structure as the transistor 200a, and are therefore denoted by the same reference numerals.

[0048] Moreover, the conductors 242a to 242c and the oxides 243a to 243c are arranged linearly in the channel length direction (A1-A2 direction) over the oxide 230. Here, the conductor 242b is arranged overlapping with the conductor 248. Also, openings are provided overlapping with a region between the conductors 242a and 242b and a region between the conductors 242b and 242c. An insulator 250 and a conductor 260 arranged on the insulator 250 are provided in each opening.

[0049] Two openings reaching the oxide 230b are provided in the insulator 280 and the insulator 275, and the insulator 250 and the conductor 260 are disposed in the openings. That is, in the transistor 200a, the insulator 250 is provided in contact with the upper surface of the oxide 230b, the side surfaces of the oxide 243a and the oxide 243b, the side surfaces of the conductor 242a and the conductor 242b, the side surface of the insulator 275, and the side surface of the insulator 280. In the transistor 200b, the insulator 250 is provided in contact with the upper surface of the oxide 230b, the side surfaces of the oxide 243b and the oxide 243c, the side surfaces of the conductor 242b and the conductor 242c, the side surface of the insulator 275, and the side surface of the insulator 280. In the transistors 200a and 200b, each of the conductors 260 is provided in contact with the upper surface and the side surface of each of the insulators 250.

[0050] In each of the transistors 200a and 200b, the conductor 260 functions as a first gate (also referred to as a top gate) electrode, and the conductor 205 functions as a second gate (also referred to as a back gate) electrode. In each of the transistors 200a and 200b, the insulator 250 functions as a first gate insulator, and the insulators 222 and 224 function as second gate insulators.

[0051] The conductor 242a functions as one of the source and drain of the transistor 200a. The conductor 242b functions as the other of the source and drain of the transistor 200a and one of the source and drain of the transistor 200b. The conductor 242c functions as the other of the source and drain of the transistor 200b. At least a part of the region of the oxide 230 that overlaps with the conductor 260 functions as a channel formation region of the transistor 200a or the transistor 200b.

[0052] Here, an enlarged view of the vicinity of the channel formation region in Fig. 1B is shown in Fig. 2. As shown in Fig. 2, the oxide 230 has a region 232d that functions as a channel formation region of the transistor 200a, regions 232a and 232b that are provided to sandwich the region 232d and function as a source region or drain region of the transistor 200a, a region 232e that functions as a channel formation region of the transistor 200b, and a region 232c that is provided together with the region 232b and sandwiches the region 232e and functions as a source region or drain region of the transistor 200b.

[0053] Region 232d and region 232e at least partially overlap with conductor 260. In other words, region 232d is provided overlapping with the region between conductor 242a and conductor 242b, and region 232e is provided overlapping with the region between conductor 242b and conductor 242c. Region 232a is provided overlapping with conductor 242a, region 232b is provided overlapping with conductor 242b, and region 232c is provided overlapping with conductor 242c.

[0054] The regions 232d and 232e functioning as channel formation regions have fewer oxygen vacancies or lower impurity concentrations than the regions 232a, 232b, and 232c, and are therefore high-resistance regions with lower carrier concentrations. Therefore, the regions 232d and 232e can be said to be i-type (intrinsic) or substantially i-type.

[0055] Moreover, the regions 232a, 232b, and 232c that function as source and drain regions have many oxygen vacancies or high concentrations of impurities such as hydrogen, nitrogen, and metal elements, which increases the carrier concentration and reduces resistance. That is, the regions 232a, 232b, and 232c are n-type regions with a high carrier concentration and low resistance compared to the regions 232d and 232e.

[0056] Here, the carrier concentration of the region 232d and the region 232e functioning as channel formation regions is 1×1018 cm -3 It is preferable that the value is less than 1×10 17 cm -3 More preferably, it is less than 1×10 16 cm -3 More preferably, it is less than 1×10 13 cm -3 More preferably, it is less than 1×10 12 cm -3 The lower limit of the carrier concentration of the region 232d and the region 232e functioning as a channel formation region is not particularly limited, but may be, for example, 1×10 -9 cm -3 It can be said that:

[0057] Furthermore, between the region 232d and the region 232a or the region 232b, or between the region 232e and the region 232b or the region 232c, a region may be formed in which the carrier concentration is equal to or lower than the carrier concentration of the region 232a, the region 232b, and the region 232c, and equal to or higher than the carrier concentration of the region 232d and the region 232e. In other words, the region functions as a junction region between the region 232d or the region 232e and the region 232a, the region 232b, or the region 232c. The hydrogen concentration of the junction region may be equal to or lower than the hydrogen concentration of the region 232a, the region 232b, and the region 232c, and equal to or higher than the hydrogen concentration of the region 232d and the region 232e. Furthermore, the junction region may have oxygen vacancies equal to or less than the oxygen vacancies in regions 232a, 232b, and 232c, and equal to or more than the oxygen vacancies in regions 232d and 232e.

[0058] In addition, it may be difficult to clearly detect the boundaries between the regions in the oxide 230. The concentrations of metal elements, hydrogen, nitrogen, and other impurity elements detected in each region may not only vary stepwise from region to region, but may also vary continuously within each region. In other words, it is sufficient that the concentrations of metal elements, hydrogen, nitrogen, and other impurity elements decrease in the region closer to the channel formation region.

[0059] Here, the region 232b functions as a source region or a drain region for both the transistor 200a and the transistor 200b, and can be said to be shared by the transistors 200a and 200b. In this manner, the transistors 200a and 200b have a structure in which the source and the drain are connected in series.

[0060] 1B and 1D, the oxide 230 contacts at least a portion of the top surface of the conductor 248 in the region 232b. By connecting the region 232b of the oxide 230 to the conductor 248 in this manner, the electrical resistance between the source or drain of the transistor 200a and the conductor 248 and the conductor 248 can be reduced. Furthermore, since the region 232b is formed overlapping the conductor 242b, the conductor 242b is disposed overlapping at least a portion of the conductor 248.

[0061] Moreover, the conductor 248 is disposed so as to be exposed from the upper surface of the insulator 224. For example, the conductor 248 may be disposed so as to be embedded in openings formed in the insulators 212, 214, 216, 222, and 224. At least a portion of the upper surface of the conductor 248 is exposed from the insulator 224, and it is preferable that the upper surface of the conductor 248 and the upper surface of the insulator 224 approximately coincide with each other.

[0062] Here, the conductor 248 functions as a plug for electrically connecting the transistor 200a and the transistor 200b to a wiring, an electrode, a terminal, or a circuit element (such as a switch, a transistor, a capacitor, an inductor, a resistor, or a diode) provided below the insulator 212. For example, the conductor 248 may be configured to be connected to a wiring provided below the insulator 212.

[0063] For example, when the transistor 200 is used as a memory cell of a memory device and the memory cell is disposed on a peripheral circuit formed on a substrate, the conductor 248 and the wiring provided in contact with the conductor 248 correspond to a bit line, and the conductor 260 of the transistor 200 corresponds to a word line. As shown in FIG. 1B and other figures, when the conductor 248 is provided under the oxide 230, the parasitic capacitance generated in the conductor 248 and the conductor 260 can be reduced compared to when the conductor 248 is provided on the oxide 230. That is, in the memory device, the parasitic capacitance generated in the word line and the bit line can be reduced. Furthermore, when the conductor 248 is provided under the oxide 230, the bit line can be shortened compared to when the conductor 248 is provided on the oxide 230. Thus, the parasitic capacitance generated in the bit line can be reduced.

[0064] In this way, by reducing the parasitic capacitance of the bit lines of the memory device, the design value of the capacitance required for the capacitive element of the memory cell can be reduced, which allows the capacitive element to be made smaller, thereby enabling the memory device to be miniaturized or highly integrated.

[0065] Furthermore, it is preferable that at least a portion of a wiring, an electrode, a terminal, or a circuit element (such as a switch, a transistor, a capacitor, an inductor, a resistor, or a diode) electrically connected to the conductor 248 overlaps with the oxide 230. This can reduce the area occupied by the transistor 200, the wiring, the electrode, the terminal, or the circuit element in a top view, thereby enabling miniaturization or high integration of the semiconductor device according to this embodiment.

[0066] 1A, 1B, and 1D, the conductor 248 is provided in contact with the lower surface of the region 232b, but the present invention is not limited to this. For example, the conductor 248 may be provided in contact with the lower surface of the region 232a, or the conductor 248 may be provided in contact with the lower surface of the region 232c.

[0067] In the transistor 200, a metal oxide functioning as a semiconductor (hereinafter also referred to as an oxide semiconductor) is preferably used for the oxide 230 including the channel formation region. The oxide 230 preferably includes an oxide 230a disposed over the insulator 224 and an oxide 230b disposed over the oxide 230a.

[0068] In addition, it is preferable to use a metal oxide that functions as a semiconductor having a band gap of 2 eV or more, preferably 2.5 eV or more. By using a metal oxide having a wide band gap in this way, the off-current of the transistor can be reduced. By using a metal oxide having a wide band gap, the off-current of the transistor 200 can be reduced. By reducing the off-current of the transistor 200 in this way, when the transistor 200 is used as a memory cell of a storage device, stored contents can be retained for a long period of time. That is, the storage device does not require a refresh operation or the frequency of the refresh operation may be extremely low. This also allows the power consumption of the storage device to be sufficiently reduced.

[0069] As the oxide 230, for example, a metal oxide such as an In-M-Zn oxide having indium, element M, and zinc (element M is one or more selected from aluminum, gallium, yttrium, tin, copper, vanadium, beryllium, boron, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium, etc.) may be used. For example, as the oxide 230, an In-Ga-Zn oxide may be used, or an oxide obtained by adding tin to the In-Ga-Zn oxide may be used. Also, as the oxide 230, an In-Ga oxide, an In-Zn oxide, or an indium oxide may be used.

[0070] The metal oxide can be formed on a substrate by sputtering or the like. Thus, the transistor 200 can be provided overlapping on a peripheral circuit such as a driver circuit formed on a silicon substrate. Thus, when the transistor 200 is used as a memory cell of a storage device, the area occupied by a memory cell array that can be provided on one chip can be increased, and the storage capacity of the storage device can be increased. Furthermore, by forming a plurality of layers of the metal oxide, the memory cell array can be provided in a stacked manner. This allows cells to be integrated and arranged without increasing the area occupied by the memory cell array. That is, a stacked structure of the memory cell array (hereinafter, sometimes referred to as a 3D cell array) can be configured. As described above, a semiconductor device with a large storage capacity can be provided by achieving high integration of memory cells.

[0071] Furthermore, semiconductor devices using the above metal oxides, particularly In-Ga-Zn oxides, have very good heat resistance, with the temperature range in which the semiconductor device can operate normally being from -40° C. to 190° C. This is better heat resistance than the heat resistance of phase change memory (PCM) (-40° C. to 150° C.), resistance random access memory (ReRAM) (-40° C. to 125° C.), magnetoresistive random access memory (MRAM) (-40° C. to 105° C.), etc.

[0072] Here, it is preferable that the atomic ratio of In to element M in the metal oxide used for oxide 230b is greater than the atomic ratio of In to element M in the metal oxide used for oxide 230a.

[0073] By disposing the oxide 230a below the oxide 230b, it is possible to suppress the diffusion of impurities and oxygen from structures formed below the oxide 230a into the oxide 230b.

[0074] However, the oxide 230 is not limited to a structure in which two layers of the oxide 230a and the oxide 230b are laminated. For example, the oxide 230 may be a single layer of the oxide 230b, or a laminate structure of three or more layers, or each of the oxides 230a and 230b may have a laminate structure. For example, the oxide 230 may be a single layer of the oxide 230b, and the region 232b may be easily formed up to the bottom surface of the oxide 230.

[0075] In addition, since the oxide 230a and the oxide 230b have a common element other than oxygen (as a main component), the defect state density at the interface between the oxide 230a and the oxide 230b can be reduced. Since the defect state density at the interface between the oxide 230a and the oxide 230b can be reduced, the effect of interface scattering on carrier conduction is small, and a high on-current can be obtained.

[0076] It is preferable that the oxide 230b has crystallinity, and it is particularly preferable to use c-axis aligned crystalline oxide semiconductor (CAAC-OS) as the oxide 230b.

[0077] CAAC-OS has a highly crystalline and dense structure and is free of impurities and defects (e.g., oxygen vacancies (V O ) is a metal oxide having a small amount of impurities. In particular, by performing heat treatment at a temperature at which the metal oxide does not become polycrystallized (for example, 400° C. or higher and 600° C. or lower) after the formation of the metal oxide, the CAAC-OS can have a dense structure with higher crystallinity. In this way, the density of the CAAC-OS can be increased, and the diffusion of impurities or oxygen in the CAAC-OS can be reduced.

[0078] On the other hand, it is difficult to identify clear grain boundaries in CAAC-OS, so it is unlikely that the electron mobility will decrease due to grain boundaries. Therefore, metal oxides with CAAC-OS have stable physical properties. Therefore, metal oxides with CAAC-OS are resistant to heat and highly reliable.

[0079] In a transistor using an oxide semiconductor, if impurities and oxygen vacancies exist in a region in which a channel is formed in the oxide semiconductor, the electrical characteristics are likely to fluctuate and the reliability may be reduced. In addition, hydrogen near the oxygen vacancies is called a defect in which hydrogen enters the oxygen vacancy (hereinafter referred to as V O H.) and may generate electrons that serve as carriers even when no voltage is applied to the gate electrode of the transistor. For this reason, if oxygen vacancies are present in the region in the oxide semiconductor in which a channel is formed, the transistor is likely to have normally-on characteristics (a channel exists even when no voltage is applied to the gate electrode, and current flows through the transistor). Therefore, in the region in the oxide semiconductor in which a channel is formed, impurities, oxygen vacancies, and V OIt is preferable that H is reduced as much as possible. In other words, it is preferable that a region in the oxide semiconductor where a channel is formed has a reduced carrier concentration in a state where no voltage is applied to the gate electrode of the transistor, and is i-type (intrinsic) or substantially i-type.

[0080] In response to this problem, an insulator containing oxygen that is released by heating (hereinafter may be referred to as excess oxygen) is provided near the oxide semiconductor and heat treatment is performed. In this way, oxygen is supplied from the insulator to the oxide semiconductor, and oxygen vacancies and V O H can be reduced. However, if an excessive amount of oxygen is supplied to the source region or drain region, this may cause a decrease in the on-current or a decrease in the field effect mobility of the transistor 200. Furthermore, if the oxygen supplied to the source region or drain region varies within the substrate surface, the characteristics of the semiconductor device having the transistor will vary.

[0081] Therefore, in the oxide semiconductor, the regions 232d and 232e functioning as channel formation regions preferably have a reduced carrier concentration and are i-type or substantially i-type, whereas the regions 232a, 232b, and 232c functioning as source and drain regions preferably have a high carrier concentration and are n-type. O It is preferable to reduce H so that an excessive amount of oxygen is not provided to regions 232a, 232b, and 232c.

[0082] Therefore, in the present embodiment, in a state where the conductor 242a, the conductor 242b, and the conductor 242c are provided on the oxide 230b, a microwave treatment is performed in an atmosphere containing oxygen, and oxygen vacancies in the regions 232d and 232e and V O The microwave treatment herein refers to a treatment using an apparatus having a power source that generates high-density plasma using microwaves, for example.

[0083] By performing microwave processing in an atmosphere containing oxygen, oxygen gas can be turned into plasma using microwaves or high frequency waves such as RF, and the oxygen plasma can be made to work. At this time, microwaves or high frequency waves such as RF can also be irradiated onto the regions 232d and 232e. The V of the regions 232d and 232e can be increased by the action of the plasma, microwaves, etc. O H is split off, hydrogen H is removed from the region 232d and the region 232e, and oxygen vacancies V O can be supplemented with oxygen. That is, in the region 232d and the region 232e, O H→H+V O " occurs, and the hydrogen concentration in the regions 232d and 232e can be reduced. Therefore, oxygen vacancies and V O H can be reduced, lowering the carrier concentration.

[0084] Furthermore, when microwave processing is performed in an atmosphere containing oxygen, the effects of microwaves, high frequency waves such as RF, oxygen plasma, and the like are shielded by conductor 242a, conductor 242b, and conductor 242c and do not reach region 232a, region 232b, and region 232c. Furthermore, the effects of oxygen plasma can be reduced by insulators 275 and 280 that are provided to cover oxide 230b and conductor 242. As a result, during microwave processing, V O Since there is no reduction in H and no excessive supply of oxygen, a decrease in the carrier concentration can be prevented.

[0085] In this manner, oxygen vacancies and V OBy removing H, the region 232d and the region 232e can be made i-type or substantially i-type. Furthermore, the supply of excess oxygen to the region 232a, the region 232b, and the region 232c that function as the source region or the drain region can be suppressed, and the n-type can be maintained. This can suppress the fluctuation of the electrical characteristics of the transistor 200, and can suppress the electrical characteristics of the transistor 200 from varying within the substrate surface. Furthermore, the region 232b becomes a low-resistance n-type region, and therefore a good contact with the conductor 248 can be formed.

[0086] By adopting the above-mentioned configuration, it is possible to provide a semiconductor device with less variation in transistor characteristics, a semiconductor device having good electrical characteristics, and a semiconductor device with good reliability.

[0087] In FIG. 1 and other figures, the side of the opening in which the conductor 260 and the like are embedded is approximately perpendicular to the surface on which the oxide 230b is formed, including the groove of the oxide 230b, but this embodiment is not limited to this. For example, the bottom of the opening may be U-shaped with a gentle curve. Also, for example, the side of the opening may be inclined with respect to the surface on which the oxide 230b is formed.

[0088] 1C, in a cross-sectional view in the channel width direction of the transistor 200, a curved surface may be formed between the side surface of the oxide 230b and the top surface of the oxide 230b. In other words, the end of the side surface and the end of the top surface may be curved (hereinafter also referred to as rounded).

[0089] The radius of curvature of the curved surface is preferably greater than 0 nm and smaller than the film thickness of the oxide 230b in the region overlapping with the conductor 242, or smaller than half the length of the region not having the curved surface. Specifically, the radius of curvature of the curved surface is greater than 0 nm and less than 20 nm, preferably greater than 1 nm and less than 15 nm, and more preferably greater than 2 nm and less than 10 nm. By forming the curved surface in this manner, the coverage of the oxide 230b by the insulator 250 and the conductor 260 can be improved.

[0090] The oxide 230 preferably has a laminated structure of a plurality of oxide layers with different chemical compositions. Specifically, in the metal oxide used for the oxide 230a, the atomic ratio of element M to the metal element that is the main component is preferably greater than the atomic ratio of element M to the metal element that is the main component in the metal oxide used for the oxide 230b. In addition, in the metal oxide used for the oxide 230a, the atomic ratio of element M to In is preferably greater than the atomic ratio of element M to In in the metal oxide used for the oxide 230b. In addition, in the metal oxide used for the oxide 230b, the atomic ratio of In to element M is preferably greater than the atomic ratio of In to element M in the metal oxide used for the oxide 230a.

[0091] Moreover, the oxide 230b is preferably a crystalline oxide such as CAAC-OS. A crystalline oxide such as CAAC-OS has few impurities and defects (such as oxygen vacancies) and has a dense structure with high crystallinity. This can suppress the extraction of oxygen from the oxide 230b by the source electrode or drain electrode. As a result, even when a heat treatment is performed, the extraction of oxygen from the oxide 230b can be reduced, so that the transistor 200 is stable against high temperatures (so-called thermal budget) in the manufacturing process.

[0092] Here, the conduction band minimum changes gradually at the junction between the oxide 230a and the oxide 230b. In other words, the conduction band minimum at the junction between the oxide 230a and the oxide 230b can be said to change continuously or to be a continuous junction. To achieve this, it is preferable to reduce the defect level density of the mixed layer formed at the interface between the oxide 230a and the oxide 230b.

[0093] Specifically, the oxide 230a and the oxide 230b have a common element other than oxygen as a main component, so that a mixed layer with a low density of defect states can be formed. For example, when the oxide 230b is an In-M-Zn oxide, the oxide 230a may be an In-M-Zn oxide, an M-Zn oxide, an oxide of element M, an In-Zn oxide, an indium oxide, or the like.

[0094] Specifically, the oxide 230a may be a metal oxide having a composition of In:M:Zn=1:3:4 [atomic ratio] or a composition close thereto, or In:M:Zn=1:1:0.5 [atomic ratio] or a composition close thereto. The oxide 230b may be a metal oxide having a composition of In:M:Zn=1:1:1 [atomic ratio] or a composition close thereto, or In:M:Zn=4:2:3 [atomic ratio] or a composition close thereto. The composition close thereto includes a range of ±30% of the desired atomic ratio. The element M is preferably gallium.

[0095] In addition, when a metal oxide film is formed by a sputtering method, the above atomic ratio is not limited to the atomic ratio of the formed metal oxide film, but may be the atomic ratio of a sputtering target used to form the metal oxide film.

[0096] By configuring the oxide 230a and the oxide 230b as described above, the defect state density at the interface between the oxide 230a and the oxide 230b can be reduced, so that the effect of interface scattering on carrier conduction is reduced, and the transistor 200 can obtain a large on-current and high frequency characteristics.

[0097] At least one of the insulators 212, 214, 275, 282, and 283 preferably functions as a barrier insulating film that suppresses diffusion of impurities such as water and hydrogen from the substrate side or from above the transistor 200 to the transistor 200. Therefore, at least one of the insulators 212, 214, 275, 282, and 283 is preferably made of an insulating material that has a function of suppressing diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules (NO, NO, NO, etc.), and copper atoms (through which the above impurities are unlikely to permeate). Alternatively, it is preferable to use an insulating material that has a function of suppressing diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.) (through which the above oxygen is unlikely to permeate).

[0098] In this specification, a barrier insulating film refers to an insulating film having a barrier property. In this specification, the barrier property refers to a function of suppressing the diffusion of a corresponding substance (also referred to as low permeability) or a function of capturing and fixing a corresponding substance (also referred to as gettering).

[0099] For example, aluminum oxide, hafnium oxide, gallium oxide, indium gallium zinc oxide, silicon nitride, or silicon nitride oxide can be used as the insulator 212, the insulator 214, the insulator 275, the insulator 282, and the insulator 283. For example, it is preferable to use silicon nitride or the like, which has a higher hydrogen barrier property, as the insulator 212 and the insulator 283. For example, it is preferable to use aluminum oxide or the like, which has a high function of capturing and fixing hydrogen and has a high oxygen barrier property, as the insulator 214, the insulator 275, and the insulator 282. This can suppress impurities such as water and hydrogen from diffusing from the substrate side to the transistor 200 side through the insulator 212 and the insulator 214. Alternatively, it can suppress impurities such as water and hydrogen from diffusing from an interlayer insulating film or the like disposed outside the insulator 283 to the transistor 200 side. Alternatively, it can suppress oxygen contained in the insulator 224 or the like from diffusing to the substrate side through the insulator 212 and the insulator 214. Alternatively, oxygen contained in the insulator 280 or the like can be prevented from diffusing upward from the transistor 200 through the insulator 282 or the like. In this manner, it is preferable to have a structure in which the transistor 200 is surrounded by the insulators 212, 214, 275, 282, and 283, which have a function of suppressing the diffusion of impurities such as water and hydrogen, and oxygen.

[0100] The insulators 212, 214, 275, 282, and 283 may be formed by, for example, a sputtering method. Since the sputtering method does not require the use of hydrogen as a film formation gas, the hydrogen concentration of the insulators 212, 214, 275, 282, and 283 can be reduced. Note that the film formation method is not limited to the sputtering method, and a chemical vapor deposition (CVD) method, a molecular beam epitaxy (MBE) method, a pulsed laser deposition (PLD) method, an atomic layer deposition (ALD) method, or the like may be used as appropriate.

[0101] In addition, it may be preferable to reduce the resistivity of the insulator 212 and the insulator 283. For example, it is preferable to reduce the resistivity of the insulator 212 and the insulator 283 to approximately 1×10 13 By setting the resistivity at Ωcm, the insulator 212 and the insulator 283 may be able to reduce charge-up of the conductor 205, the conductor 242, or the conductor 260 in a process using plasma or the like in a semiconductor device manufacturing process. 10 Ωcm or more 1×10 15 Ωcm or less.

[0102] The insulator 216 and the insulator 280 preferably have a lower dielectric constant than the insulator 214. By using a material with a low dielectric constant as an interlayer film, the parasitic capacitance generated between wirings can be reduced. For example, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide to which fluorine has been added, silicon oxide to which carbon has been added, silicon oxide to which carbon and nitrogen have been added, silicon oxide having vacancies, or the like may be used as the insulator 216 and the insulator 280 as appropriate.

[0103] In the transistor 200a and the transistor 200b, the conductor 205 is arranged to overlap with the oxide 230 and the conductor 260. The conductor 205 may be provided to extend in the A3-A4 direction as shown in FIG. 1A. Here, the conductor 205 is preferably provided to be embedded in an opening formed in the insulator 216. Note that a part of the conductor 205 may be provided to be embedded in the insulator 214.

[0104] The conductor 205 includes conductor 205a, conductor 205b, and conductor 205c. The conductor 205a is provided in contact with the bottom surface and side wall of the opening. The conductor 205b is provided so as to be embedded in a recess formed in the conductor 205a. Here, the upper surface of the conductor 205b is lower than the upper surface of the conductor 205a and the upper surface of the insulator 216. The conductor 205c is provided in contact with the upper surface of the conductor 205b and the side surface of the conductor 205a. Here, the height of the upper surface of the conductor 205c is approximately the same as the height of the upper surface of the conductor 205a and the height of the upper surface of the insulator 216. In other words, the conductor 205b is configured to be wrapped in the conductor 205a and the conductor 205c.

[0105] Here, the conductor 205a and the conductor 205c are preferably made of a conductive material having a function of suppressing the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules (NO, NO, NO, etc.), copper atoms, etc. Alternatively, it is preferable to use a conductive material having a function of suppressing the diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.).

[0106] By using a conductive material having a function of reducing hydrogen diffusion for the conductor 205a and the conductor 205c, it is possible to prevent impurities such as hydrogen contained in the conductor 205b from diffusing into the oxide 230 via the insulator 224 and the like. In addition, by using a conductive material having a function of suppressing oxygen diffusion for the conductor 205a and the conductor 205c, it is possible to suppress the conductor 205b from being oxidized and its conductivity from decreasing. As the conductive material having a function of suppressing oxygen diffusion, it is preferable to use, for example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, or the like. Therefore, the conductor 205a and the conductor 205c may be formed of the above-mentioned conductive material in a single layer or a multilayer structure. For example, the conductor 205a and the conductor 205c may be made of titanium nitride.

[0107] The conductor 205b is preferably made of a conductive material containing tungsten, copper, or aluminum as a main component, for example, tungsten.

[0108] The conductor 205 may function as a second gate electrode. In this case, the threshold voltage (Vth) of the transistor 200 can be controlled by changing the potential applied to the conductor 205 independently of the potential applied to the conductor 260. In particular, applying a negative potential to the conductor 205 can increase the Vth of the transistor 200 and reduce the off-current. Therefore, applying a negative potential to the conductor 205 can reduce the drain current when the potential applied to the conductor 260 is 0 V, compared to not applying a negative potential.

[0109] The electrical resistivity of the conductor 205 is designed in consideration of the potential applied to the conductor 205, and the film thickness of the conductor 205 is set according to the electrical resistivity. The film thickness of the insulator 216 is approximately the same as that of the conductor 205. Here, it is preferable to make the film thicknesses of the conductor 205 and the insulator 216 thin within the range permitted by the design of the conductor 205. By making the film thickness of the insulator 216 thin, the absolute amount of impurities such as hydrogen contained in the insulator 216 can be reduced, and therefore the diffusion of the impurities into the oxide 230 can be reduced.

[0110] As shown in FIG. 1A, the conductor 205 is preferably provided larger than the size of the region of the oxide 230 that does not overlap with the conductor 242a and the conductor 242b. In particular, as shown in FIG. 1C, the conductor 205 preferably extends in a region outside the end of the oxide 230a and the oxide 230b that intersects with the channel width direction. In other words, outside the side surface of the oxide 230 in the channel width direction, the conductor 205 and the conductor 260 preferably overlap with each other via an insulator. With this configuration, the channel formation region of the oxide 230 can be electrically surrounded by the electric field of the conductor 260 that functions as the first gate electrode and the electric field of the conductor 205 that functions as the second gate electrode. In this specification, a structure of a transistor in which the channel formation region is electrically surrounded by the electric fields of the first gate and the second gate is called a surrounded channel (S-channel) structure.

[0111] In this specification and the like, a transistor with an S-channel structure refers to a transistor structure in which a channel formation region is electrically surrounded by the electric fields of one and the other of a pair of gate electrodes. The S-channel structure disclosed in this specification and the like is different from a fin type structure and a planar type structure. By adopting the S-channel structure, it is possible to improve resistance to the short channel effect, in other words, to make a transistor in which the short channel effect is unlikely to occur.

[0112] 1C, the conductor 205 is extended to function as wiring. However, the present invention is not limited to this, and a conductor functioning as wiring may be provided below the conductor 205. Also, it is not necessary to provide one conductor 205 for each transistor. For example, the conductor 205 may be shared by multiple transistors.

[0113] Although the conductor 205 is shown as being a laminate of conductor 205a, conductor 205b, and conductor 205c, the present invention is not limited to this. The conductor 205 may be configured as a single layer, a two-layer, or a laminated structure of four or more layers. For example, when the conductor 205 is configured as a two-layer laminated structure, the conductor 205c is not required, and the upper surface of the conductor 205a and the upper surface of the conductor 205b may be aligned.

[0114] The conductor 248 may have a configuration including a conductor 248a and a conductor 248b disposed inside the conductor 248a, similar to the conductor 205. The conductor 248a may be a conductor that can be used for the conductor 205a, and is preferably a conductor that reduces the permeation of impurities such as water or hydrogen and oxygen. For example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, etc. may be used. The conductor 248a may be a conductor that has good adhesion to the conductor 248b. The conductor 248b may be a conductor that can be used for the conductor 205b, and is preferably a conductive material mainly composed of tungsten, copper, or aluminum.

[0115] 1A, the shape of the conductor 248 is circular when viewed from above, but is not limited thereto. For example, the conductor 248 may be substantially circular, such as an ellipse, polygonal, such as a rectangle, or polygonal, such as a rectangle, with rounded corners, when viewed from above.

[0116] Although the conductor 248 is shown as having a stacked structure of the conductor 248a and the conductor 248b, the present invention is not limited to this. The conductor 248 may be configured as a single layer or a stacked structure of three or more layers. For example, a conductor similar to the conductor 205a may be disposed between the top surface of the conductor 248b and the oxide 230, similar to the conductor 205c.

[0117] Further, an insulator 249 is provided in contact with the inner walls of the openings of the insulators 212, 214, 216, 222, and 224, and a conductor 248 is provided in contact with the side surface of the insulator 249. As the insulator 249, it is preferable to use an insulator that reduces the diffusion of impurities such as hydrogen and water and oxygen, and for example, an insulator such as silicon nitride, aluminum oxide, or silicon nitride oxide may be used. This can prevent impurities such as water and hydrogen contained in the insulator 216 from being mixed into the oxide 230 through the conductor 248. In particular, silicon nitride is preferable because it has high barrier properties against hydrogen. Also, it can prevent oxygen contained in the insulator 216 from being absorbed by the conductor 248. Note that the above is not limited, and a configuration without the insulator 249 may be used.

[0118] Insulator 222 and insulator 224 function as gate insulators.

[0119] The insulator 222 preferably has a function of suppressing the diffusion of hydrogen (e.g., at least one of hydrogen atoms, hydrogen molecules, etc.). The insulator 222 preferably has a function of suppressing the diffusion of oxygen (e.g., at least one of oxygen atoms, oxygen molecules, etc.). For example, the insulator 222 preferably has a function of suppressing the diffusion of one or both of hydrogen and oxygen more than the insulator 224.

[0120] The insulator 222 may be an insulator containing an oxide of one or both of aluminum and hafnium, which are insulating materials. As the insulator, it is preferable to use aluminum oxide, hafnium oxide, an oxide containing aluminum and hafnium (hafnium aluminate), or the like. When the insulator 222 is formed using such a material, the insulator 222 functions as a layer that suppresses the release of oxygen from the oxide 230 to the substrate side and the diffusion of impurities such as hydrogen from the periphery of the transistor 200 to the oxide 230. Thus, by providing the insulator 222, it is possible to suppress the diffusion of impurities such as hydrogen into the inside of the transistor 200 and the generation of oxygen vacancies in the oxide 230. In addition, it is possible to suppress the reaction of the conductor 205 with the insulator 224 and the oxygen contained in the oxide 230.

[0121] Alternatively, for example, aluminum oxide, bismuth oxide, germanium oxide, niobium oxide, silicon oxide, titanium oxide, tungsten oxide, yttrium oxide, or zirconium oxide may be added to the insulator. Alternatively, these insulators may be nitrided. The insulator 222 may be formed by stacking silicon oxide, silicon oxynitride, or silicon nitride on these insulators.

[0122] The insulator 222 may be a single layer or a multilayer of insulators containing so-called high-k materials, such as aluminum oxide, hafnium oxide, tantalum oxide, zirconium oxide, lead zirconate titanate (PZT), strontium titanate (SrTiO3), (Ba,Sr)TiO3 (BST), etc. As transistors become smaller and more highly integrated, problems such as leakage current may occur due to the thinning of the gate insulator. By using a high-k material for the insulator that functions as the gate insulator, it is possible to reduce the gate potential during transistor operation while maintaining the physical film thickness.

[0123] The insulator 224 in contact with the oxide 230 preferably contains excess oxygen (oxygen is released by heating). For example, the insulator 224 may be made of silicon oxide, silicon oxynitride, or the like as appropriate. By providing an insulator containing oxygen in contact with the oxide 230, oxygen vacancies in the oxide 230 can be reduced and the reliability of the transistor 200 can be improved.

[0124] Specifically, it is preferable to use an oxide material from which some oxygen is released by heating, in other words, an insulator material having an excess oxygen region, as the insulator 224. An oxide material from which oxygen is released by heating is an oxide material from which the amount of released oxygen molecules is 1.0×10 18 molecules / cm 3 More than 1.0×10 19 molecules / cm 3 More preferably, 2.0×10 19 molecules / cm 3 or more, or 3.0×10 20 molecules / cm 3 The oxide film is one having the above-mentioned properties. The surface temperature of the film during the TDS analysis is preferably in the range of 100° C. or more and 700° C. or less, or 100° C. or more and 400° C. or less.

[0125] In addition, in the manufacturing process of the transistor 200, it is preferable to perform heat treatment while the surface of the oxide 230 is exposed. The heat treatment may be performed, for example, at a temperature of 100° C. or higher and 600° C. or lower, more preferably 350° C. or higher and 550° C. or lower. Note that the heat treatment is performed in an atmosphere of nitrogen gas or an inert gas, or an atmosphere containing an oxidizing gas at 10 ppm or higher, 1% or higher, or 10% or higher. For example, the heat treatment is preferably performed in an oxygen atmosphere. This supplies oxygen to the oxide 230 to reduce oxygen deficiencies (V O) can be reduced. The heat treatment may be performed under reduced pressure. Alternatively, the heat treatment may be performed in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas in order to compensate for the desorbed oxygen after the heat treatment in a nitrogen gas or inert gas atmosphere. Alternatively, the heat treatment may be performed in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas in order to compensate for the desorbed oxygen. Alternatively, the heat treatment may be performed in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas in succession to a heat treatment in a nitrogen gas or inert gas atmosphere.

[0126] In addition, by subjecting the oxide 230 to an oxygen addition treatment, the oxygen vacancies in the oxide 230 are repaired by the supplied oxygen. In other words, O In addition, the reaction of the hydrogen remaining in the oxide 230 with the oxygen supplied can be promoted, and the hydrogen can be removed as H2O (dehydrated). As a result, the hydrogen remaining in the oxide 230 recombines with the oxygen vacancies to form V O The formation of H can be suppressed.

[0127] The insulator 222 and the insulator 224 may have a laminated structure of two or more layers. In this case, the laminated structure is not limited to being made of the same material, and may be made of different materials. The insulator 224 may be formed in an island shape by overlapping with the oxide 230a. In this case, the insulator 275 is configured to contact the side surface of the insulator 224 and the upper surface of the insulator 222.

[0128] The oxide 243a, the oxide 243b, and the oxide 243c are provided on the oxide 230b. The oxide 243a, the oxide 243b, and the oxide 243c are arranged in the A1-A2 direction and are provided separately with the conductor 260 therebetween.

[0129] The oxide 243 (oxide 243a, oxide 243b, and oxide 243c) preferably has a function of suppressing oxygen permeation. By disposing the oxide 243 having a function of suppressing oxygen permeation between the conductor 242 functioning as a source electrode or a drain electrode and the oxide 230b, the electrical resistance between the conductor 242 and the oxide 230b is reduced, which is preferable. With such a structure, the electrical characteristics and reliability of the transistor 200 can be improved. Note that if the electrical resistance between the conductor 242 and the oxide 230b can be sufficiently reduced, the oxide 243 may not be provided.

[0130] A metal oxide having element M may be used as the oxide 243. In particular, the element M may be aluminum, gallium, yttrium, or tin. The oxide 243 preferably has a higher concentration of element M than the oxide 230b. Gallium oxide may be used as the oxide 243. A metal oxide such as In-M-Zn oxide may be used as the oxide 243. Specifically, in the metal oxide used for the oxide 243, the atomic ratio of element M to In is preferably greater than the atomic ratio of element M to In in the metal oxide used for the oxide 230b. The film thickness of the oxide 243 is preferably 0.5 nm or more and 5 nm or less, more preferably 1 nm or more and 3 nm or less, and even more preferably 1 nm or more and 2 nm or less. The oxide 243 is preferably crystalline. When the oxide 243 is crystalline, the release of oxygen in the oxide 230 can be suitably suppressed. For example, if the oxide 243 has a crystal structure such as a hexagonal crystal structure, the release of oxygen in the oxide 230 may be suppressed.

[0131] It is preferable that the conductor 242a is provided in contact with the upper surface of the oxide 243a, the conductor 242b is provided in contact with the upper surface of the oxide 243b, and the conductor 242c is provided in contact with the upper surface of the oxide 243c. The conductors 242a, 242b, and 242c are arranged in the A1-A2 direction and are spaced apart from each other with the conductor 260 sandwiched therebetween. The conductors 242a, 242b, and 242c function as source electrodes and drain electrodes of the transistor 200a or the transistor 200b, respectively.

[0132] As the conductor 242 (conductor 242a, conductor 242b, and conductor 242c), it is preferable to use, for example, a nitride containing tantalum, a nitride containing titanium, a nitride containing molybdenum, a nitride containing tungsten, a nitride containing tantalum and aluminum, or a nitride containing titanium and aluminum. In one embodiment of the present invention, a nitride containing tantalum is particularly preferable. In addition, for example, ruthenium oxide, ruthenium nitride, an oxide containing strontium and ruthenium, an oxide containing lanthanum and nickel, or the like may be used. These materials are preferable because they are conductive materials that are difficult to oxidize, or materials that maintain their conductivity even when they absorb oxygen.

[0133] Note that hydrogen contained in the oxide 230b and the like may diffuse into the conductor 242a, the conductor 242b, and the conductor 242c. In particular, by using a nitride containing tantalum for the conductors 242a, 242b, and 242c, hydrogen contained in the oxide 230b and the like is likely to diffuse into the conductors 242a, 242b, and 242c, and the diffused hydrogen may bond with nitrogen contained in the conductors 242a, 242b, and 242c. In other words, hydrogen contained in the oxide 230b and the like may be absorbed by the conductors 242a, 242b, and 242c.

[0134] Moreover, a configuration may be adopted in which no curved surface is formed between the side surface of the conductor 242 and the top surface of the conductor 242. By forming the conductor 242 such that no curved surface is formed, it is possible to increase the cross-sectional area of ​​the conductor 242 in the cross section in the channel width direction as shown in Fig. 1D. This increases the conductivity of the conductor 242, and therefore the on-current of the transistor 200.

[0135] The insulator 275 is provided to cover the insulator 224, the oxide 230, the oxide 243, and the conductor 242, and an opening is formed in the region where the insulator 250 and the conductor 260 are provided. The insulator 275 is preferably provided in contact with the top surface of the insulator 224, the side surface of the oxide 230, the side surface of the oxide 243, the side surface of the conductor 242, and the top surface of the conductor 242. The insulator 275 preferably functions as a barrier insulating film that suppresses oxygen permeation. The insulator 275 preferably functions as a barrier insulating film that suppresses impurities such as water and hydrogen from diffusing from above to the insulator 224 or the oxide 230, and preferably has a function of capturing impurities such as hydrogen. As the insulator 275, for example, an insulator such as aluminum oxide or silicon nitride may be used.

[0136] By providing insulator 275, which is in contact with insulator 280 and insulator 224 and has a function of capturing impurities such as hydrogen, in the region between insulator 212 and insulator 283, impurities such as hydrogen contained in insulator 280 and insulator 224 can be captured and the amount of hydrogen in the region can be kept constant. In this case, it is preferable to use aluminum oxide or the like as insulator 275.

[0137] As shown in FIG. 1A, the insulator 250 is provided extending in the A3-A4 direction and functions as a gate insulator for the transistor 200a and the transistor 200b. In the transistor 200a and the transistor 200b, the insulator 250 is preferably disposed in contact with the top surface and the side surface of the oxide 230b, respectively. The insulator 250 can be made of silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide to which fluorine has been added, silicon oxide to which carbon has been added, silicon oxide to which carbon and nitrogen have been added, silicon oxide having vacancies, or the like. In particular, silicon oxide and silicon oxynitride are preferable because they are stable against heat.

[0138] The insulator 250 preferably has a reduced concentration of impurities such as water and hydrogen in the insulator 250, similar to the insulator 224. The thickness of the insulator 250 is preferably 1 nm or more and 20 nm or less.

[0139] In addition, although the insulator 250 is illustrated as a single layer in FIG. 1B and FIG. 1C, it may be a laminated structure of two or more layers. When the insulator 250 is a laminated structure of two layers, it is preferable that the lower layer of the insulator 250 is formed using an insulator that releases oxygen when heated, and the upper layer of the insulator 250 is formed using an insulator that has a function of suppressing the diffusion of oxygen. By adopting such a configuration, it is possible to suppress the diffusion of oxygen contained in the lower layer of the insulator 250 to the conductor 260. In other words, it is possible to suppress the decrease in the amount of oxygen supplied to the oxide 230. In addition, it is possible to suppress the oxidation of the conductor 260 due to the oxygen contained in the lower layer of the insulator 250. For example, the lower layer of the insulator 250 can be provided using a material that can be used for the insulator 250 described above, and the upper layer of the insulator 250 can be provided using a material similar to that of the insulator 222.

[0140] When silicon oxide or silicon oxynitride is used for the lower layer of the insulator 250, the upper layer of the insulator 250 may be made of an insulating material that is a high-k material with a high dielectric constant. By forming the gate insulator into a laminated structure of the lower layer of the insulator 250 and the upper layer of the insulator 250, it is possible to obtain a laminated structure that is stable against heat and has a high dielectric constant. Therefore, it is possible to reduce the gate potential applied during transistor operation while maintaining the physical film thickness of the gate insulator. In addition, it is possible to reduce the equivalent oxide thickness (EOT) of the insulator that functions as the gate insulator.

[0141] Specifically, the upper layer of the insulator 250 may be a metal oxide containing one or more of hafnium, aluminum, gallium, yttrium, zirconium, tungsten, titanium, tantalum, nickel, germanium, magnesium, etc., or a metal oxide that can be used as the oxide 230. In particular, it is preferable to use an insulator containing an oxide of one or both of aluminum and hafnium. For example, hafnium oxide may be used as the upper layer of the insulator 250.

[0142] Furthermore, a metal oxide may be provided between the insulator 250 and the conductor 260. The metal oxide preferably suppresses the diffusion of oxygen from the insulator 250 to the conductor 260. By providing a metal oxide that suppresses the diffusion of oxygen, the diffusion of oxygen from the insulator 250 to the conductor 260 is suppressed. In other words, a decrease in the amount of oxygen supplied to the oxide 230 can be suppressed. Furthermore, oxidation of the conductor 260 due to oxygen from the insulator 250 can be suppressed.

[0143] The metal oxide may be configured to function as a part of the first gate electrode. For example, the metal oxide that can be used as the oxide 230 may be used as the metal oxide. In this case, the electric resistance value of the metal oxide can be reduced to make it a conductor by forming the conductor 260a by a sputtering method. This can be called an OC (Oxide Conductor) electrode.

[0144] By including the metal oxide, the on-current of the transistor 200 can be improved without weakening the effect of the electric field from the conductor 260. Furthermore, by maintaining a distance between the conductor 260 and the oxide 230 due to the physical thickness of the insulator 250 and the metal oxide, it is possible to suppress leakage current between the conductor 260 and the oxide 230. Furthermore, by providing a stacked structure of the insulator 250 and the metal oxide, it is possible to easily and appropriately adjust the physical distance between the conductor 260 and the oxide 230 and the electric field strength applied from the conductor 260 to the oxide 230.

[0145] As shown in FIG. 1A, the conductor 260 is provided extending in the A3-A4 direction, and functions as a first gate electrode of the transistor 200a and the transistor 200b. In the transistor 200a and the transistor 200b, the conductor 260 preferably includes a conductor 260a and a conductor 260b disposed on the conductor 260a. For example, the conductor 260a is preferably disposed so as to surround the bottom and side surfaces of the conductor 260b. As shown in FIG. 1B and FIG. 1C, the upper surface of the conductor 260 is substantially aligned with the upper surface of the insulator 250. Note that, in FIG. 1B and FIG. 1C, the conductor 260 is shown as a two-layer structure of the conductor 260a and the conductor 260b, but may be a single-layer structure or a laminated structure of three or more layers.

[0146] The conductor 260a is preferably made of a conductive material having a function of suppressing the diffusion of impurities such as hydrogen atoms, hydrogen molecules, water molecules, nitrogen atoms, nitrogen molecules, nitrogen oxide molecules, copper atoms, etc. Alternatively, it is preferably made of a conductive material having a function of suppressing the diffusion of oxygen (for example, at least one of oxygen atoms, oxygen molecules, etc.).

[0147] Furthermore, since the conductor 260a has a function of suppressing oxygen diffusion, it is possible to suppress a decrease in conductivity due to oxidation of the conductor 260b caused by oxygen contained in the insulator 250. As a conductive material having a function of suppressing oxygen diffusion, it is preferable to use, for example, titanium, titanium nitride, tantalum, tantalum nitride, ruthenium, ruthenium oxide, or the like.

[0148] In addition, since the conductor 260 also functions as wiring, it is preferable to use a conductor with high conductivity. For example, the conductor 260b can be a conductive material mainly composed of tungsten, copper, or aluminum. The conductor 260b may also have a laminated structure, for example, a laminated structure of titanium or titanium nitride and the above conductive material.

[0149] Moreover, in the transistor 200, the conductor 260 is formed in a self-aligned manner so as to fill an opening formed in the insulator 280 or the like. By forming the conductor 260 in this manner, the conductor 260 can be disposed in the region between the conductor 242a and the conductor 242b and in the region between the conductor 242b and the conductor 242c without the need for alignment.

[0150] As shown in FIG. 1C, in the channel width direction of the transistor 200, the height of the bottom surface of the conductor 260 in the region where the conductor 260 and the oxide 230b do not overlap is preferably lower than the height of the bottom surface of the oxide 230b when the bottom surface of the insulator 222 is used as a reference. The conductor 260, which functions as a gate electrode, is configured to cover the side and upper surfaces of the channel formation region of the oxide 230b via the insulator 250, so that the electric field of the conductor 260 can be easily applied to the entire channel formation region of the oxide 230b. This can increase the on-current of the transistor 200 and improve the frequency characteristics. When the bottom surface of the insulator 222 is used as a reference, the difference between the height of the bottom surface of the conductor 260 in the region where the oxide 230a and the oxide 230b do not overlap with the conductor 260 and the height of the bottom surface of the oxide 230b is 0 nm or more and 100 nm or less, preferably 3 nm or more and 50 nm or less, and more preferably 5 nm or more and 20 nm or less.

[0151] The insulator 280 is provided on the insulator 275, and has openings formed in the areas where the insulator 250 and the conductor 260 are provided. The upper surface of the insulator 280 may be flattened.

[0152] The insulator 280 that functions as an interlayer film preferably has a low dielectric constant. By using a material with a low dielectric constant as the interlayer film, the parasitic capacitance that occurs between wirings can be reduced. The insulator 280 is preferably formed using, for example, the same material as the insulator 216. In particular, silicon oxide and silicon oxynitride are preferable because they are thermally stable. In particular, materials such as silicon oxide, silicon oxynitride, and silicon oxide having vacancies are preferable because they can easily form a region containing oxygen that is desorbed by heating.

[0153] Like the insulator 224, the insulator 280 preferably has an excess oxygen region or excess oxygen. The concentrations of impurities such as water and hydrogen in the insulator 280 are preferably reduced. For example, the insulator 280 may be an oxide containing silicon, such as silicon oxide or silicon oxynitride, as appropriate. By providing an insulator having excess oxygen in contact with the oxide 230, oxygen vacancies in the oxide 230 can be reduced and the reliability of the transistor 200 can be improved.

[0154] The insulator 282 is disposed in contact with the upper surfaces of the conductor 260 and the insulator 280, and with the uppermost portion of the insulator 250. The insulator 282 preferably functions as a barrier insulating film that suppresses the diffusion of impurities such as water and hydrogen from above into the insulator 280, and preferably has a function of capturing impurities such as hydrogen. The insulator 282 preferably functions as a barrier insulating film that suppresses the transmission of oxygen. For example, an insulator such as aluminum oxide may be used as the insulator 282. By providing the insulator 282 in contact with the insulator 280 in the region sandwiched between the insulator 212 and the insulator 283 and having a function of capturing impurities such as hydrogen, it is possible to capture impurities such as hydrogen contained in the insulator 280 and to keep the amount of hydrogen in the region constant.

[0155] The insulator 283 functions as a barrier insulating film that suppresses diffusion of impurities such as water and hydrogen from above into the insulator 280. The insulator 283 is disposed on the insulator 282. It is preferable to use a nitride containing silicon, such as silicon nitride or silicon nitride oxide, as the insulator 283. For example, silicon nitride formed by a sputtering method may be used as the insulator 283. By forming the insulator 283 by a sputtering method, a silicon nitride film that is high in density and unlikely to form voids can be formed. Alternatively, the insulator 283 may be formed by stacking a silicon nitride film formed by a CVD method on a silicon nitride film formed by a sputtering method.

[0156] <Materials for semiconductor devices> The following describes constituent materials that can be used in the semiconductor device.

[0157] <<Substrate>> The substrate on which the transistor 200 is formed may be, for example, an insulating substrate, a semiconductor substrate, or a conductive substrate. Examples of insulating substrates include a glass substrate, a quartz substrate, a sapphire substrate, a stabilized zirconia substrate (such as an yttria stabilized zirconia substrate), and a resin substrate. Examples of semiconductor substrates include a semiconductor substrate made of silicon or germanium, or a compound semiconductor substrate made of silicon carbide, silicon germanium, gallium arsenide, indium phosphide, zinc oxide, and gallium oxide. Examples of semiconductor substrates include a semiconductor substrate having an insulating region inside the semiconductor substrate, such as an SOI (Silicon On Insulator) substrate. Examples of conductive substrates include a graphite substrate, a metal substrate, an alloy substrate, and a conductive resin substrate. Examples of substrates include a substrate having a metal nitride, a substrate having a metal oxide, and the like. Examples of substrates include a substrate having a conductor or semiconductor provided on an insulating substrate, a substrate having a conductor or insulator provided on a semiconductor substrate, and a substrate having a semiconductor or insulator provided on a conductive substrate. Alternatively, a substrate provided with elements may be used. The elements provided on the substrate include a capacitor element, a resistor element, a switch element, a light-emitting element, a memory element, and the like.

[0158] <<Insulators>> Examples of the insulator include oxides, nitrides, oxynitrides, nitride oxides, metal oxides, metal oxynitrides, and metal nitride oxides, each of which has insulating properties.

[0159] For example, as transistors become smaller and more highly integrated, problems such as leakage current can occur due to thinner gate insulators. By using a high-k material for the insulator that functions as the gate insulator, it is possible to reduce the voltage required for transistor operation while maintaining the physical film thickness. On the other hand, by using a material with a low dielectric constant for the insulator that functions as the interlayer film, it is possible to reduce the parasitic capacitance that occurs between wiring. Therefore, it is best to select materials according to the function of the insulator.

[0160] Further, examples of insulators with a high relative dielectric constant include gallium oxide, hafnium oxide, zirconium oxide, oxides having aluminum and hafnium, oxynitrides having aluminum and hafnium, oxides having silicon and hafnium, oxynitrides having silicon and hafnium, and nitrides having silicon and hafnium.

[0161] Examples of insulators with a low dielectric constant include silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide with fluorine added, silicon oxide with carbon added, silicon oxide with carbon and nitrogen added, silicon oxide with voids, or resin.

[0162] In addition, the transistor using metal oxide can have stable electrical characteristics by being surrounded by an insulator having a function of suppressing the permeation of impurities such as hydrogen and oxygen. As the insulator having a function of suppressing the permeation of impurities such as hydrogen and oxygen, for example, an insulator containing boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium, or tantalum may be used in a single layer or a stacked layer. Specifically, as the insulator having a function of suppressing the permeation of impurities such as hydrogen and oxygen, metal oxides such as aluminum oxide, magnesium oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide, and tantalum oxide, and metal nitrides such as aluminum nitride, silicon nitride oxide, and silicon nitride can be used.

[0163] The insulator that functions as the gate insulator is preferably an insulator having a region containing oxygen that is released by heating. For example, by using a structure in which silicon oxide or silicon oxynitride having a region containing oxygen that is released by heating is in contact with the oxide 230, oxygen vacancies in the oxide 230 can be compensated for.

[0164] <<Conductors>> As the conductor, it is preferable to use a metal element selected from aluminum, chromium, copper, silver, gold, platinum, tantalum, nickel, titanium, molybdenum, tungsten, hafnium, vanadium, niobium, manganese, magnesium, zirconium, beryllium, indium, ruthenium, iridium, strontium, lanthanum, etc., or an alloy containing the above-mentioned metal elements as a component, or an alloy combining the above-mentioned metal elements. For example, it is preferable to use tantalum nitride, titanium nitride, tungsten, nitride containing titanium and aluminum, nitride containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, oxide containing strontium and ruthenium, oxide containing lanthanum and nickel, etc. In addition, tantalum nitride, titanium nitride, nitride containing titanium and aluminum, nitride containing tantalum and aluminum, ruthenium oxide, ruthenium nitride, oxide containing strontium and ruthenium, oxide containing lanthanum and nickel are conductive materials that are difficult to oxidize, or materials that maintain conductivity even when oxygen is absorbed, so they are preferable. Furthermore, a semiconductor having high electrical conductivity, typified by polycrystalline silicon containing an impurity element such as phosphorus, or a silicide such as nickel silicide may be used.

[0165] A plurality of conductive layers formed of the above-mentioned materials may be stacked. For example, a stacked structure may be formed by combining the above-mentioned material containing a metal element and a conductive material containing oxygen. A stacked structure may be formed by combining the above-mentioned material containing a metal element and a conductive material containing nitrogen. A stacked structure may be formed by combining the above-mentioned material containing a metal element, a conductive material containing oxygen, and a conductive material containing nitrogen.

[0166] In addition, when an oxide is used for the channel formation region of a transistor, a conductor functioning as a gate electrode preferably has a stacked structure in which a material containing a metal element and a conductive material containing oxygen are combined. In this case, the conductive material containing oxygen is preferably provided on the channel formation region side. By providing the conductive material containing oxygen on the channel formation region side, oxygen released from the conductive material is easily supplied to the channel formation region.

[0167] In particular, it is preferable to use a conductive material containing oxygen and a metal element contained in the metal oxide in which the channel is formed as a conductor functioning as a gate electrode. The conductive material containing the metal element and nitrogen described above may also be used. For example, a conductive material containing nitrogen, such as titanium nitride or tantalum nitride, may also be used. Indium tin oxide, indium oxide containing tungsten oxide, indium zinc oxide containing tungsten oxide, indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc oxide, and indium tin oxide to which silicon is added may also be used. Indium gallium zinc oxide containing nitrogen may also be used. By using such a material, hydrogen contained in the metal oxide in which the channel is formed may be captured. Alternatively, hydrogen mixed in from an external insulator may be captured.

[0168] <<Metal oxides>> It is preferable to use a metal oxide that functions as a semiconductor (oxide semiconductor) as the oxide 230. Hereinafter, metal oxides that can be applied to the oxide 230 according to the present invention will be described.

[0169] The metal oxide preferably contains at least indium or zinc. In particular, it is preferable that the metal oxide contains indium and zinc. In addition to these, it is preferable that the metal oxide contains aluminum, gallium, yttrium, tin, etc. In addition, it may contain one or more elements selected from boron, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium, cobalt, etc.

[0170] Here, the case where the metal oxide is an In-M-Zn oxide having indium, element M, and zinc is considered. The element M is one or more selected from aluminum, gallium, yttrium, and tin. Other elements applicable to the element M include boron, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum, cerium, neodymium, hafnium, tantalum, tungsten, magnesium, and cobalt. However, there are cases where the element M may be a combination of multiple elements mentioned above.

[0171] In this specification and the like, metal oxides containing nitrogen may also be collectively referred to as metal oxides. Furthermore, metal oxides containing nitrogen may also be referred to as metal oxynitrides.

[0172] <Classification of crystal structures> First, classification of crystal structures in oxide semiconductors will be described with reference to Fig. 3A. Fig. 3A is a diagram for explaining classification of crystal structures of oxide semiconductors, typically IGZO (metal oxide containing In, Ga, and Zn).

[0173] As shown in FIG. 3A, oxide semiconductors are broadly classified into "Amorphous", "Crystalline", and "Crystal". "Amorphous" includes completely amorphous. "Crystalline" includes c-axis-aligned crystalline (CAAC), nanocrystalline (nc), and cloud-aligned composite (CAC) (excluding single crystal and poly crystal). "Crystalline" excludes single crystal, poly crystal, and completely amorphous. "Crystal" includes single crystal and poly crystal.

[0174] The structure in the bold frame shown in Fig. 3A is an intermediate state between "Amorphous" and "Crystal" and belongs to a new boundary region (New crystalline phase). In other words, this structure is completely different from the energetically unstable "Amorphous" and "Crystal".

[0175] The crystal structure of the film or substrate can be evaluated using an X-ray diffraction (XRD) spectrum. Figure 3B shows an XRD spectrum obtained by GIXD (Grazing-Incidence XRD) measurement of the CAAC-IGZO film classified as "Crystalline". The GIXD method is also called the thin film method or the Seemann-Bohlin method. Hereinafter, the XRD spectrum obtained by the GIXD measurement shown in Figure 3B will be simply referred to as the XRD spectrum. The composition of the CAAC-IGZO film shown in Figure 3B is approximately In:Ga:Zn=4:2:3 [atomic ratio]. The thickness of the CAAC-IGZO film shown in Figure 3B is 500 nm.

[0176] As shown in Figure 3B, a clear peak indicating crystallinity is detected in the XRD spectrum of the CAAC-IGZO film. Specifically, a peak indicating c-axis orientation is detected near 2θ=31° in the XRD spectrum of the CAAC-IGZO film. Note that, as shown in Figure 3B, the peak near 2θ=31° is asymmetric with respect to the angle at which the peak intensity is detected.

[0177] The crystal structure of the film or substrate can be evaluated from the diffraction pattern (also called the nanobeam electron diffraction pattern) observed by nanobeam electron diffraction (NBED). The diffraction pattern of the CAAC-IGZO film is shown in Figure 3C. Figure 3C shows a diffraction pattern observed by NBED, which causes an electron beam to be incident parallel to the substrate. The composition of the CAAC-IGZO film shown in Figure 3C is approximately In:Ga:Zn=4:2:3 [atomic ratio]. In the nanobeam electron diffraction method, electron diffraction is performed with a probe diameter of 1 nm.

[0178] As shown in Figure 3C, multiple spots indicating c-axis orientation are observed in the diffraction pattern of the CAAC-IGZO film.

[0179] <<Structure of oxide semiconductor>> In addition, when focusing on the crystal structure, oxide semiconductors may be classified differently from that shown in FIG. 3A. For example, oxide semiconductors are divided into single-crystal oxide semiconductors and other non-single-crystal oxide semiconductors. Examples of non-single-crystal oxide semiconductors include the above-mentioned CAAC-OS and nc-OS. In addition, non-single-crystal oxide semiconductors include polycrystalline oxide semiconductors, pseudo-amorphous-like oxide semiconductors (a-like OS), amorphous oxide semiconductors, and the like.

[0180] Here, the above-mentioned CAAC-OS, nc-OS, and a-like OS will be described in detail.

[0181] [CAAC-OS] CAAC-OS is an oxide semiconductor having a plurality of crystalline regions, each of which has a c-axis aligned in a specific direction. The specific direction is the thickness direction of the CAAC-OS film, the normal direction of the surface on which the CAAC-OS film is formed, or the normal direction of the surface of the CAAC-OS film. The crystalline region is a region having periodic atomic arrangement. If the atomic arrangement is considered as a lattice arrangement, the crystalline region is also a region with a uniform lattice arrangement. CAAC-OS has a region in which a plurality of crystalline regions are connected in the ab-plane direction, and the region may have distortion. The distortion refers to a portion in which the direction of the lattice arrangement changes between a region with a uniform lattice arrangement and another region with a uniform lattice arrangement in the region in which the plurality of crystalline regions are connected. In other words, CAAC-OS is an oxide semiconductor having a c-axis aligned and no clear orientation in the ab-plane direction.

[0182] Each of the multiple crystalline regions is composed of one or more minute crystals (crystals with a maximum diameter of less than 10 nm). When a crystalline region is composed of one minute crystal, the maximum diameter of the crystalline region is less than 10 nm. When a crystalline region is composed of many minute crystals, the size of the crystalline region may be about several tens of nm.

[0183] In addition, in an In-M-Zn oxide (wherein element M is one or more elements selected from aluminum, gallium, yttrium, tin, titanium, etc.), the CAAC-OS tends to have a layered crystal structure (also referred to as a layered structure) in which a layer containing indium (In) and oxygen (hereinafter, In layer) and a layer containing element M, zinc (Zn), and oxygen (hereinafter, (M, Zn) layer) are stacked. Note that indium and element M are mutually substituted. Thus, the (M, Zn) layer may contain indium. Also, the In layer may contain element M. Note that the In layer may contain Zn. The layered structure is observed as a lattice image in a high-resolution TEM image, for example.

[0184] When the CAAC-OS film is subjected to structural analysis using, for example, an XRD device, a peak indicating c-axis orientation is detected at or near 2θ=31° in out-of-plane XRD measurement using θ / 2θ scan. Note that the position of the peak indicating c-axis orientation (2θ value) may vary depending on the type and composition of the metal elements constituting the CAAC-OS.

[0185] For example, a plurality of bright points (spots) are observed in the electron diffraction pattern of the CAAC-OS film, and the two spots are observed at positions symmetrical to each other with respect to the spot of the incident electron beam that has passed through the sample (also called the direct spot).

[0186] When the crystal region is observed from the specific direction, the lattice arrangement in the crystal region is based on a hexagonal lattice, but the unit cell is not necessarily a regular hexagon and may be a non-regular hexagon. The above distortion may have a pentagonal or heptagonal lattice arrangement. In addition, no clear grain boundary can be confirmed in the CAAC-OS even in the vicinity of the distortion. That is, it is found that the formation of grain boundaries is suppressed by the distortion of the lattice arrangement. This is considered to be because the CAAC-OS can tolerate distortion due to the fact that the arrangement of oxygen atoms is not dense in the ab-plane direction and the bond distance between atoms changes due to the substitution of metal atoms.

[0187] A crystal structure in which clear grain boundaries are observed is called a polycrystal. The grain boundaries are likely to become recombination centers, trap carriers, and cause a decrease in the on-current of a transistor and a decrease in field effect mobility. Therefore, CAAC-OS in which clear grain boundaries are not observed is one of the crystalline oxides having a crystal structure suitable for a semiconductor layer of a transistor. In order to form a CAAC-OS, a structure containing Zn is preferable. For example, In-Zn oxide and In-Ga-Zn oxide are suitable because they can suppress the occurrence of grain boundaries more than In oxide.

[0188] The CAAC-OS is an oxide semiconductor with high crystallinity and no clear crystal grain boundaries. Therefore, it can be said that the CAAC-OS is less susceptible to a decrease in electron mobility due to crystal grain boundaries. In addition, since the crystallinity of an oxide semiconductor can be decreased by the inclusion of impurities or the generation of defects, the CAAC-OS can be said to be an oxide semiconductor with few impurities and defects (such as oxygen vacancies). Therefore, the physical properties of an oxide semiconductor having the CAAC-OS are stable. Therefore, an oxide semiconductor having the CAAC-OS is resistant to heat and has high reliability. In addition, the CAAC-OS is stable against high temperatures (so-called thermal budget) in the manufacturing process. Therefore, the use of the CAAC-OS in an OS transistor can increase the degree of freedom in the manufacturing process.

[0189] [nc-OS] The nc-OS has periodic atomic arrangement in a minute region (for example, a region of 1 nm to 10 nm, particularly a region of 1 nm to 3 nm). In other words, the nc-OS has minute crystals. Note that the size of the minute crystals is, for example, 1 nm to 10 nm, particularly 1 nm to 3 nm, and therefore the minute crystals are also called nanocrystals. In addition, the nc-OS does not show regularity in the crystal orientation between different nanocrystals. Therefore, no orientation is seen in the entire film. Therefore, depending on the analysis method, the nc-OS may be indistinguishable from an a-like OS or an amorphous oxide semiconductor. For example, when a structure analysis is performed on an nc-OS film using an XRD device, no peak indicating crystallinity is detected in out-of-plane XRD measurement using θ / 2θ scan. In addition, when an nc-OS film is subjected to electron diffraction (also called selected area electron diffraction) using an electron beam with a probe diameter larger than that of nanocrystals (for example, 50 nm or more), a diffraction pattern like a halo pattern is observed. On the other hand, when electron diffraction (also called nanobeam electron diffraction) is performed on an nc-OS film using an electron beam with a probe diameter (e.g., 1 nm to 30 nm) that is close to the size of a nanocrystal or smaller than the nanocrystal, an electron diffraction pattern in which multiple spots are observed within a ring-shaped region centered on the direct spot may be obtained.

[0190] [a-like OS] The a-like OS is an oxide semiconductor having a structure between the nc-OS and an amorphous oxide semiconductor. The a-like OS has a void or low-density region. That is, the a-like OS has lower crystallinity than the nc-OS and CAAC-OS. Moreover, the a-like OS has a higher hydrogen concentration in the film than the nc-OS and CAAC-OS.

[0191] <<Oxide semiconductor structure>> Next, the above-mentioned CAC-OS will be described in detail, with reference to its material composition.

[0192] [CAC-OS] CAC-OS is, for example, a material configuration in which elements constituting a metal oxide are unevenly distributed in a size range of 0.5 nm to 10 nm, preferably 1 nm to 3 nm, or in the vicinity thereof. In the following, a state in which one or more metal elements are unevenly distributed in a metal oxide and the regions having the metal elements are mixed in a size range of 0.5 nm to 10 nm, preferably 1 nm to 3 nm, or in the vicinity thereof, is also referred to as a mosaic or patch state.

[0193] Furthermore, CAC-OS is a composite metal oxide in which the material is separated into a first region and a second region, forming a mosaic structure, and the first region is distributed throughout the film (hereinafter, also referred to as a cloud structure). In other words, CAC-OS is a composite metal oxide in which the first region and the second region are mixed together.

[0194] Here, the atomic ratios of In, Ga, and Zn to the metal elements constituting the CAC-OS in the In-Ga-Zn oxide are represented as [In], [Ga], and [Zn], respectively. For example, in the CAC-OS in the In-Ga-Zn oxide, the first region is a region where [In] is larger than [In] in the composition of the CAC-OS film. Also, the second region is a region where [Ga] is larger than [Ga] in the composition of the CAC-OS film. Alternatively, for example, the first region is a region where [In] is larger than [In] in the second region and [Ga] is smaller than [Ga] in the second region. Also, the second region is a region where [Ga] is larger than [Ga] in the first region and [In] is smaller than [In] in the first region.

[0195] Specifically, the first region is a region mainly composed of indium oxide, indium zinc oxide, etc., and the second region is a region mainly composed of gallium oxide, gallium zinc oxide, etc. In other words, the first region can be rephrased as a region mainly composed of In, and the second region can be rephrased as a region mainly composed of Ga.

[0196] In addition, there are cases where a clear boundary between the first region and the second region cannot be observed.

[0197] For example, in the case of a CAC-OS of an In-Ga-Zn oxide, EDX mapping obtained using EDX (Energy Dispersive X-ray spectroscopy) has confirmed that the CAC-OS has a structure in which a region mainly composed of In (first region) and a region mainly composed of Ga (second region) are unevenly distributed and mixed.

[0198] When CAC-OS is used in a transistor, the conductivity due to the first region and the insulating property due to the second region act in a complementary manner, giving the CAC-OS a switching function (On / Off function). In other words, CAC-OS has a conductive function in part of the material and an insulating function in other parts of the material, and the material as a whole functions as a semiconductor. By separating the conductive function from the insulating function, it is possible to maximize both functions. Therefore, by using CAC-OS in a transistor, it is possible to achieve a high on-current (I on ), high field effect mobility (μ), and good switching behavior can be achieved.

[0199] Oxide semiconductors have a variety of structures and have different characteristics. The oxide semiconductor of one embodiment of the present invention may include two or more of an amorphous oxide semiconductor, a polycrystalline oxide semiconductor, an a-like OS, a CAC-OS, an nc-OS, and a CAAC-OS.

[0200] <Transistor Having Oxide Semiconductor> Next, the case where the oxide semiconductor is used for a transistor will be described.

[0201] By using the oxide semiconductor for a transistor, a transistor with high field-effect mobility and high reliability can be realized.

[0202] It is preferable to use an oxide semiconductor having a low carrier concentration for a channel formation region of a transistor. For example, the carrier concentration of the channel formation region of an oxide semiconductor is 1×10 18 cm -3 It is preferable that the value is less than 1×10 17 cm -3 More preferably, it is less than 1×10 16 cm -3 More preferably, it is less than 1×10 13 cm -3 More preferably, it is less than 1×10 12 cm-3 It is more preferable that the carrier concentration in the oxide semiconductor film is less than 100%. In order to reduce the carrier concentration in the oxide semiconductor film, the impurity concentration in the oxide semiconductor film may be reduced to reduce the density of defect states. In this specification and the like, an oxide semiconductor having a low impurity concentration and a low density of defect states is referred to as a high-purity intrinsic or substantially high-purity intrinsic oxide semiconductor. An oxide semiconductor having a low carrier concentration may be referred to as a high-purity intrinsic or substantially high-purity intrinsic oxide semiconductor.

[0203] Furthermore, a highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film has a low density of defect states, and therefore the density of trap states might also be low.

[0204] In addition, charges trapped in the trap states of an oxide semiconductor take a long time to disappear and may behave as if they are fixed charges. Therefore, a transistor in which a channel formation region is formed in an oxide semiconductor with a high density of trap states may have unstable electrical characteristics.

[0205] Therefore, in order to stabilize the electrical characteristics of a transistor, it is effective to reduce the impurity concentration in the oxide semiconductor. In order to reduce the impurity concentration in the oxide semiconductor, it is preferable to also reduce the impurity concentration in a nearby film. Examples of impurities include hydrogen, nitrogen, alkali metals, alkaline earth metals, iron, nickel, silicon, and the like.

[0206] <Impurities> Here, the influence of each impurity in an oxide semiconductor will be described.

[0207] When an oxide semiconductor contains silicon or carbon, which is one of the group 14 elements, defect levels are formed in the oxide semiconductor. For this reason, the concentrations of silicon and carbon in the channel formation region of the oxide semiconductor and the vicinity of the interface with the channel formation region of the oxide semiconductor (concentrations obtained by secondary ion mass spectrometry (SIMS)) are set to 2×10 18 atoms / cm 3Less than or equal to 2 x 10 17 atoms / cm 3 The following applies.

[0208] In addition, when an oxide semiconductor contains an alkali metal or an alkaline earth metal, defect levels are formed and carriers are generated in some cases. Therefore, a transistor using an oxide semiconductor containing an alkali metal or an alkaline earth metal is likely to have normally-on characteristics. For this reason, when the concentration of the alkali metal or the alkaline earth metal in the channel formation region of the oxide semiconductor obtained by SIMS is set to 1×10 18 atoms / cm 3 Less than or equal to 2 x 10 16 atoms / cm 3 To the following:

[0209] Furthermore, when nitrogen is contained in an oxide semiconductor, electrons serving as carriers are generated, the carrier concentration increases, and the semiconductor is likely to become n-type. As a result, a transistor using an oxide semiconductor containing nitrogen as a semiconductor is likely to have normally-on characteristics. Alternatively, when nitrogen is contained in an oxide semiconductor, trap states may be formed. As a result, the electrical characteristics of the transistor may become unstable. For this reason, the nitrogen concentration in the channel formation region of the oxide semiconductor obtained by SIMS is set to 5×10 19 atoms / cm 3 Less than 5 x 10 18 atoms / cm 3 Less than or equal to 1×10 18 atoms / cm 3 Less than 5×10, more preferably 17 atoms / cm 3 To the following:

[0210] Furthermore, hydrogen contained in the oxide semiconductor reacts with oxygen bonded to a metal atom to form water, which may form an oxygen vacancy. When hydrogen enters the oxygen vacancy, electrons serving as carriers may be generated. In addition, some of the hydrogen may bond with oxygen bonded to a metal atom to generate electrons serving as carriers. Therefore, a transistor using an oxide semiconductor containing hydrogen is likely to have normally-on characteristics. For this reason, it is preferable to reduce hydrogen in the channel formation region of the oxide semiconductor as much as possible. Specifically, the hydrogen concentration measured by SIMS in the channel formation region of the oxide semiconductor is 1×10 20 atoms / cm 3 Less than 5 x 10 19 atoms / cm 3 less than 1×10 19 atoms / cm 3 less than 5×10 18 atoms / cm 3 less than 1×10 18 atoms / cm 3 Make it less than.

[0211] When an oxide semiconductor in which impurities are sufficiently reduced is used for a channel formation region of a transistor, stable electrical characteristics can be obtained.

[0212] <<Other semiconductor materials>> The semiconductor material that can be used for the oxide 230 is not limited to the above-mentioned metal oxides. A semiconductor material having a band gap (a semiconductor material that is not a zero-gap semiconductor) may be used for the oxide 230. For example, a semiconductor of a single element such as silicon, a compound semiconductor such as gallium arsenide, or a layered material (also called an atomic layer material, a two-dimensional material, etc.) that functions as a semiconductor is preferably used for the semiconductor material. In particular, it is preferable to use a layered material that functions as a semiconductor for the semiconductor material.

[0213] Here, in this specification and the like, the layered material is a general term for a group of materials having a layered crystal structure. The layered crystal structure is a structure in which layers formed by covalent bonds or ionic bonds are stacked via bonds weaker than covalent bonds or ionic bonds, such as van der Waals forces. The layered material has high electrical conductivity within a unit layer, that is, high two-dimensional electrical conductivity. By using a material that functions as a semiconductor and has high two-dimensional electrical conductivity in the channel formation region, a transistor with a large on-current can be provided.

[0214] Layered materials include graphene, silicene, and chalcogenides. Chalcogenides are compounds that contain chalcogen. Chalcogen is a general term for elements in group 16, including oxygen, sulfur, selenium, tellurium, polonium, and livermorium. Chalcogenides include transition metal chalcogenides and group 13 chalcogenides.

[0215] It is preferable to use, for example, a transition metal chalcogenide that functions as a semiconductor as the oxide 230. Specific examples of transition metal chalcogenides that can be used as the oxide 230 include molybdenum sulfide (representatively MoS2), molybdenum selenide (representatively MoSe2), molybdenum tellurium (representatively MoTe2), tungsten sulfide (representatively WS2), tungsten selenide (representatively WSe2), tungsten tellurium (representatively WTe2), hafnium sulfide (representatively HfS2), hafnium selenide (representatively HfSe2), zirconium sulfide (representatively ZrS2), and zirconium selenide (representatively ZrSe2).

[0216] <Method for manufacturing semiconductor device> Next, a manufacturing method of the semiconductor device of one embodiment of the present invention shown in FIGS. 1A to 1D will be described with reference to FIGS. 4A to 12A, 4B to 12B, 4C to 12C, and 4D to 12D.

[0217] Each of Fig. 4A to Fig. 12A shows a top view. Each of Fig. 4B to Fig. 12B is a cross-sectional view corresponding to a portion indicated by a dashed line A1-A2 in Fig. 4A to Fig. 12A, and is also a cross-sectional view in the channel length direction of the transistor 200a and the transistor 200b. Each of Fig. 4C to Fig. 12C is a cross-sectional view corresponding to a portion indicated by a dashed line A3-A4 in Fig. 4A to Fig. 12A, and is also a cross-sectional view in the channel width direction of the transistor 200a. Each of Fig. 4D to Fig. 12D is a cross-sectional view of a portion indicated by a dashed line A5-A6 in Fig. 4A to Fig. 12A. Note that some elements are omitted in each of the top views in Fig. 4A to Fig. 12A for clarity.

[0218] In the following, insulating materials for forming insulators, conductive materials for forming conductors, or semiconductor materials for forming semiconductors can be formed as films by appropriately using a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like.

[0219] There are three types of sputtering: RF sputtering, which uses a high-frequency power source for the sputtering power supply, DC sputtering, which uses a direct current power source, and pulsed DC sputtering, which changes the voltage applied to the electrode in a pulsed manner. RF sputtering is mainly used when depositing insulating films, while DC sputtering is mainly used when depositing metal conductive films. Pulsed DC sputtering is mainly used when depositing compounds such as oxides, nitrides, and carbides using reactive sputtering.

[0220] CVD methods can be classified into plasma enhanced CVD (PECVD), which uses plasma, thermal CVD (TCVD), which uses heat, photo CVD (Photo CVD), etc. They can also be further divided into metal CVD (MCVD) and metal organic CVD (MOCVD), depending on the source gas used.

[0221] The plasma CVD method can obtain a high-quality film at a relatively low temperature. Moreover, the thermal CVD method is a film formation method that can reduce plasma damage to the object to be processed because it does not use plasma. For example, wiring, electrodes, elements (transistors, capacitive elements, etc.) included in a semiconductor device may be charged up by receiving electric charge from plasma. At this time, the wiring, electrodes, elements, etc. included in the semiconductor device may be destroyed by the accumulated electric charge. On the other hand, in the case of the thermal CVD method that does not use plasma, such plasma damage does not occur, so the yield of the semiconductor device can be increased. Furthermore, in the thermal CVD method, plasma damage does not occur during film formation, so a film with few defects can be obtained.

[0222] As the ALD method, a thermal ALD method in which a reaction between a precursor and a reactant is carried out using only thermal energy, a plasma enhanced ALD method in which a plasma excited reactant is used, or the like can be used.

[0223] In addition, the ALD method utilizes the self-regulating nature of atoms to deposit atoms one layer at a time, and thus has the following advantages: extremely thin films can be formed; films can be formed on structures with high aspect ratios; films can be formed with fewer defects such as pinholes; films can be formed with excellent coverage; and films can be formed at low temperatures. In the PEALD method, the use of plasma can be preferable because it allows films to be formed at lower temperatures. Note that some precursors used in the ALD method contain impurities such as carbon. For this reason, films formed by the ALD method may contain more impurities such as carbon than films formed by other film formation methods. Note that the amount of impurities can be quantified using X-ray photoelectron spectroscopy (XPS).

[0224] The CVD method and the ALD method are different from the film formation method in which particles emitted from a target or the like are deposited, and are film formation methods in which a film is formed by a reaction on the surface of a workpiece. Therefore, they are film formation methods that are not easily affected by the shape of the workpiece and have good step coverage. In particular, the ALD method has excellent step coverage and excellent thickness uniformity, so it is suitable for coating the surface of an opening with a high aspect ratio. However, since the ALD method has a relatively slow film formation speed, it may be preferable to use it in combination with other film formation methods such as the CVD method, which has a fast film formation speed.

[0225] In the CVD method and the ALD method, the composition of the film obtained can be controlled by the flow rate ratio of the raw material gases. For example, in the CVD method and the ALD method, a film of any composition can be formed by changing the flow rate ratio of the raw material gases. In addition, for example, in the CVD method and the ALD method, a film whose composition changes continuously can be formed by changing the flow rate ratio of the raw material gases while forming the film. When forming a film while changing the flow rate ratio of the raw material gases, the time required for film formation can be shortened compared to the case of forming a film using multiple film formation chambers because no time is required for transportation and pressure adjustment. Therefore, the productivity of semiconductor devices can be increased in some cases.

[0226] First, a substrate (not shown) is prepared, and the insulator 212 is formed on the substrate (see FIGS. 4A to 4D). The insulator 212 is preferably formed by a sputtering method. By using a sputtering method that does not require hydrogen as a deposition gas, the hydrogen concentration in the insulator 212 can be reduced. However, the method for forming the insulator 212 is not limited to the sputtering method, and a CVD method, an MBE method, a PLD method, an ALD method, or the like may be used as appropriate.

[0227] In this embodiment, a silicon nitride film is formed as the insulator 212 by pulsed DC sputtering using a silicon target in an atmosphere containing nitrogen gas. By using pulsed DC sputtering, the generation of particles due to arcing on the target surface can be suppressed, making the film thickness distribution more uniform. In addition, by using a pulsed voltage, the rise and fall of the discharge can be made steeper than with a high-frequency voltage. This allows power to be supplied to the electrodes more efficiently, improving the sputtering rate and film quality.

[0228] By using an insulator such as silicon nitride through which impurities such as water and hydrogen do not easily permeate, it is possible to suppress the diffusion of impurities such as water and hydrogen contained in layers below the insulator 212. Furthermore, by using an insulator such as silicon nitride through which copper does not easily permeate as the insulator 212, even if a metal that easily diffuses, such as copper, is used for a conductor in a layer (not shown) below the insulator 212, it is possible to suppress the diffusion of the metal upward through the insulator 212.

[0229] Next, the insulator 214 is deposited on the insulator 212 (see FIGS. 4A to 4D). The insulator 214 is preferably deposited by a sputtering method. By using a sputtering method that does not require hydrogen as a deposition gas, the hydrogen concentration in the insulator 214 can be reduced. However, the deposition of the insulator 214 is not limited to the sputtering method, and a CVD method, an MBE method, a PLD method, an ALD method, or the like may also be used as appropriate.

[0230] In this embodiment, an aluminum oxide film is formed by pulse DC sputtering using an aluminum target in an atmosphere containing oxygen gas as the insulator 214. By using the pulse DC sputtering method, the film thickness distribution can be made more uniform, and the sputtering rate and film quality can be improved.

[0231] By using aluminum oxide, which has a high ability to capture and fix hydrogen, as the insulator 214, it is possible to capture or fix hydrogen contained in the insulator 216 and the like, and prevent the hydrogen from diffusing into the oxide 230.

[0232] Next, the insulator 216 is deposited over the insulator 214. The insulator 216 is preferably deposited by a sputtering method. By using a sputtering method that does not require hydrogen as a deposition gas, the hydrogen concentration in the insulator 216 can be reduced. However, the deposition of the insulator 216 is not limited to the sputtering method, and a CVD method, an MBE method, a PLD method, an ALD method, or the like may also be used as appropriate.

[0233] In this embodiment, a silicon oxide film is formed by pulsed DC sputtering using a silicon target in an atmosphere containing oxygen gas as the insulator 216. By using the pulsed DC sputtering method, the film thickness distribution can be made more uniform, and the sputtering rate and film quality can be improved.

[0234] It is preferable that the insulators 212, 214, and 216 are successively formed without exposure to the air. For example, a multi-chamber film formation apparatus can be used. This allows the insulators 212, 214, and 216 to be formed with reduced hydrogen in the films, and further reduces the incorporation of hydrogen into the films between each film formation process.

[0235] Next, two openings reaching the insulator 214 are formed in the insulator 216 by extending in the A3-A4 direction. The openings may be, for example, grooves or slits. The openings may be referred to as the openings. The openings may be formed by wet etching, but dry etching is preferable for fine processing. For the insulator 214, it is preferable to select an insulator that functions as an etching stopper film when the insulator 216 is etched to form the grooves. For example, when silicon oxide or silicon oxynitride is used for the insulator 216 that forms the grooves, the insulator 214 may be silicon nitride, aluminum oxide, or hafnium oxide.

[0236] As the dry etching apparatus, a capacitively coupled plasma (CCP) etching apparatus having parallel plate electrodes can be used. The capacitively coupled plasma etching apparatus having parallel plate electrodes can be configured to apply a high frequency voltage to one of the parallel plate electrodes. Alternatively, it can be configured to apply a plurality of different high frequency voltages to one of the parallel plate electrodes. Alternatively, it can be configured to apply a high frequency voltage of the same frequency to each of the parallel plate electrodes. Alternatively, it can be configured to apply high frequency voltages of different frequencies to each of the parallel plate electrodes. Alternatively, a dry etching apparatus having a high density plasma source can be used. As the dry etching apparatus having a high density plasma source, for example, an inductively coupled plasma (ICP) etching apparatus or the like can be used.

[0237] After the opening is formed, a conductive film that becomes the conductor 205a is formed. The conductive film that becomes the conductor 205a preferably contains a conductor that has a function of suppressing oxygen permeation. For example, tantalum nitride, tungsten nitride, titanium nitride, or the like can be used. Alternatively, it can be a laminated film of a conductor that has a function of suppressing oxygen permeation and tantalum, tungsten, titanium, molybdenum, aluminum, copper, or a molybdenum-tungsten alloy. The conductive film that becomes the conductor 205a can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like.

[0238] In this embodiment, titanium nitride is formed as the conductive film that becomes the conductor 205a. By using such a metal nitride as the lower layer of the conductor 205b, it is possible to prevent the conductor 205b from being oxidized by the insulator 216 or the like. Even if a metal that easily diffuses, such as copper, is used as the conductor 205b, it is possible to prevent the metal from diffusing out of the conductor 205a.

[0239] Next, a conductive film to be the conductor 205b is formed. As the conductive film to be the conductor 205b, tantalum, tungsten, titanium, molybdenum, aluminum, copper, a molybdenum-tungsten alloy, or the like can be used. The conductive film can be formed by a plating method, a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. In this embodiment, tungsten is formed as the conductive film to be the conductor 205b.

[0240] Next, a CMP process is performed to remove a portion of the conductive film that will become the conductor 205a and a portion of the conductive film that will become the conductor 205b, thereby exposing the insulator 216. As a result, the conductor 205a and the conductor 205b remain only in the openings. Note that the CMP process may remove a portion of the insulator 216.

[0241] Next, the upper portion of the conductor 205b is removed by etching, so that the upper surface of the conductor 205b is lower than the upper surfaces of the conductor 205a and the insulator 216. The conductor 205b may be etched by dry etching or wet etching, but dry etching is preferable for fine processing.

[0242] Next, a conductive film to be the conductor 205c is formed over the insulator 216, the conductor 205a, and the conductor 205b. The conductive film to be the conductor 205c preferably contains a conductor having a function of suppressing oxygen permeation, similar to the conductive film to be the conductor 205a.

[0243] In this embodiment, titanium nitride is formed as the conductive film that becomes the conductor 205c. By using such a metal nitride as the upper layer of the conductor 205b, it is possible to prevent the conductor 205b from being oxidized by the insulator 222 or the like. Even if a metal that easily diffuses, such as copper, is used as the conductor 205b, it is possible to prevent the metal from diffusing out of the conductor 205c.

[0244] Next, a part of the conductive film that becomes the conductor 205c is removed by performing CMP processing, and the insulator 216 is exposed (see FIG. 4A to FIG. 4D). As a result, the conductor 205a, the conductor 205b, and the conductor 205c remain only in the opening. This allows the conductor 205 with a flat upper surface to be formed. Furthermore, the conductor 205b is configured to be surrounded by the conductor 205a and the conductor 205c. This prevents impurities such as hydrogen from the conductor 205b from diffusing out of the conductor 205a and the conductor 205c, and prevents oxygen from entering from outside the conductor 205a and the conductor 205c and oxidizing the conductor 205b. Note that the CMP processing may remove a part of the insulator 216.

[0245] Next, the insulator 222 is formed on the insulator 216 and the conductor 205. As the insulator 222, an insulator containing one or both of an oxide of aluminum and hafnium may be formed. Note that as the insulator containing one or both of an oxide of aluminum and hafnium, it is preferable to use aluminum oxide, hafnium oxide, an oxide containing aluminum and hafnium (hafnium aluminate), or the like. The insulator containing one or both of an oxide of aluminum and hafnium has a barrier property against oxygen, hydrogen, and water. When the insulator 222 has a barrier property against hydrogen and water, the hydrogen and water contained in the structure provided around the transistor 200 are prevented from diffusing into the inside of the transistor 200 through the insulator 222, and the generation of oxygen vacancies in the oxide 230 can be suppressed.

[0246] The insulator 222 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. In this embodiment, a hafnium oxide film is formed by a sputtering method as the insulator 222. By using a sputtering method in which hydrogen is not required as a deposition gas, the hydrogen concentration in the insulator 222 can be reduced.

[0247] It is preferable to carry out a heat treatment subsequently. The heat treatment may be carried out at 250°C or higher and 650°C or lower, preferably 300°C or higher and 500°C or lower, and more preferably 320°C or higher and 450°C or lower. The heat treatment may be carried out in an atmosphere of nitrogen gas or an inert gas, or an atmosphere containing 10 ppm or higher, 1% or higher, or 10% or higher of an oxidizing gas. For example, when the heat treatment is carried out in a mixed atmosphere of nitrogen gas and oxygen gas, the oxygen gas may be about 20%. The heat treatment may be carried out under reduced pressure. Alternatively, the heat treatment may be carried out in an atmosphere of nitrogen gas or an inert gas, and then in an atmosphere containing 10 ppm or higher, 1% or higher, or 10% or higher of an oxidizing gas to compensate for the desorbed oxygen.

[0248] In addition, it is preferable that the gas used in the heat treatment is highly purified. For example, the amount of moisture contained in the gas used in the heat treatment is 1 ppb or less, preferably 0.1 ppb or less, and more preferably 0.05 ppb or less. By performing the heat treatment using a highly purified gas, it is possible to prevent moisture and the like from being taken into the insulator 222 as much as possible.

[0249] In this embodiment, after the insulator 222 is formed, heat treatment is performed at a flow rate ratio of nitrogen gas and oxygen gas of 4 slm:1 slm at a temperature of 400° C. for one hour. The heat treatment can remove impurities such as water and hydrogen contained in the insulator 222. When an oxide containing hafnium is used as the insulator 222, the heat treatment can improve the crystallinity of the insulator 222. The heat treatment can also be performed at a timing such as after the insulator 224 is formed.

[0250] Next, the insulator 224 is formed on the insulator 222. The insulator 224 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. In this embodiment, a silicon oxide film is formed as the insulator 224 by a sputtering method. By using a sputtering method that does not require hydrogen as a deposition gas, the hydrogen concentration in the insulator 224 can be reduced. Since the insulator 224 comes into contact with the oxide 230a in a later process, it is preferable that the hydrogen concentration be reduced in this manner.

[0251] Next, openings are formed in the insulators 224, 222, 216, 214, and 212. The openings are formed between two conductors 205. The openings may be formed by wet etching, but dry etching is preferable for fine processing. Note that the shape of the openings is circular in top view in FIG. 5A, but is not limited thereto. For example, the openings may be substantially circular such as an ellipse, polygonal such as a rectangle, or polygonal such as a rectangle with rounded corners in top view.

[0252] Next, an insulating film that will become the insulator 249 is formed, and the insulating film is anisotropically etched to form the insulator 249. The insulating film that will become the insulator 249 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. As the insulating film that will become the insulator 249, it is preferable to use an insulating film that has a function of reducing oxygen permeation. For example, it is preferable to form an aluminum oxide film by the ALD method. Alternatively, it is preferable to form a silicon nitride film by the PEALD method. Silicon nitride is preferable because it has a high barrier property against hydrogen.

[0253] For example, a dry etching method may be used for the anisotropic etching of the insulating film that becomes the insulator 249. By providing the insulator 249 on the sidewall of the opening, it is possible to reduce the permeation of oxygen from the outside and prevent the oxidation of the conductor 248 to be formed next. It is also possible to prevent impurities such as water and hydrogen from entering the conductor 248 from the outside.

[0254] After the openings are formed, a conductive film that becomes the conductor 248 is formed. The conductive film that becomes the conductor 248 can be formed by sputtering, CVD, MBE, PLD, ALD, or the like. In this embodiment, the conductor 248 is formed to have the same structure as the conductor 205. Therefore, the conductive film that becomes the conductor 248a may be formed by the same method as the conductive film that becomes the conductor 205a, and the conductive film that becomes the conductor 248b may be formed by the same method as the conductive film that becomes the conductor 205b.

[0255] Next, a CMP process is performed to remove a portion of the conductive film that will become the conductor 248, exposing the insulator 224. As a result, the conductive film that will become the conductor 248 remains only in the opening. This makes it possible to form the conductor 248 (conductor 248a and conductor 248b) with a flat upper surface (see FIGS. 5A to 5D). Note that the CMP process may remove a portion of the insulator 224.

[0256] Here, in order to form an excess oxygen region in the insulator 224, a plasma treatment including oxygen may be performed under reduced pressure. For the plasma treatment including oxygen, it is preferable to use an apparatus having a power source that generates high density plasma using, for example, microwaves. Alternatively, the apparatus may have a power source that applies RF (Radio Frequency) to the substrate side. By using high density plasma, high density oxygen radicals can be generated, and by applying RF to the substrate side, the oxygen radicals generated by the high density plasma can be efficiently guided into the insulator 224. Alternatively, after performing a plasma treatment including an inert gas using this apparatus, a plasma treatment including oxygen may be performed to compensate for the desorbed oxygen. Note that impurities such as water and hydrogen contained in the insulator 224 can be removed by appropriately selecting the conditions for the plasma treatment. In that case, heat treatment does not need to be performed.

[0257] Here, after forming an aluminum oxide film on the insulator 224 by, for example, a sputtering method, a CMP process may be performed until the insulator 224 is reached. The CMP process can planarize and smooth the surface of the insulator 224. By disposing the aluminum oxide on the insulator 224 and performing the CMP process, it becomes easy to detect the end point of the CMP process. In addition, the CMP process may polish a part of the insulator 224, and the thickness of the insulator 224 may become thin, but the thickness may be adjusted when the insulator 224 is formed. By planarizing and smoothing the surface of the insulator 224, it may be possible to prevent a deterioration in the coverage rate of the oxide to be formed later and to prevent a decrease in the yield of the semiconductor device. In addition, it is preferable to form an aluminum oxide film on the insulator 224 by a sputtering method, since oxygen can be added to the insulator 224.

[0258] Next, oxide film 230A and oxide film 230B are sequentially formed on insulator 224 and conductor 248 (see FIGS. 6A to 6D). Note that oxide film 230A and oxide film 230B are preferably formed successively without exposure to the air environment. By forming the films without exposure to the air, it is possible to prevent impurities or moisture from the air environment from adhering to oxide film 230A and oxide film 230B, and it is possible to keep the vicinity of the interface between oxide film 230A and oxide film 230B clean.

[0259] The oxide film 230A and the oxide film 230B can be formed by using a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like.

[0260] For example, when the oxide film 230A and the oxide film 230B are formed by sputtering, oxygen or a mixed gas of oxygen and a rare gas is used as the sputtering gas. By increasing the ratio of oxygen contained in the sputtering gas, the excess oxygen in the oxide film to be formed can be increased. In addition, when the oxide film is formed by sputtering, the above-mentioned In-M-Zn oxide target can be used.

[0261] In particular, during the formation of the oxide film 230A, a portion of the oxygen contained in the sputtering gas may be supplied to the insulator 224. Therefore, the ratio of oxygen contained in the sputtering gas may be 70% or more, preferably 80% or more, and more preferably 100%.

[0262] When the oxide film 230B is formed by a sputtering method, an oxygen-excessive oxide semiconductor is formed when the ratio of oxygen contained in the sputtering gas is more than 30% and less than or equal to 100%, preferably 70% to 100%. A transistor using an oxygen-excessive oxide semiconductor for a channel formation region can have relatively high reliability. However, one embodiment of the present invention is not limited thereto. When the oxide film 230B is formed by a sputtering method, an oxygen-deficient oxide semiconductor is formed when the ratio of oxygen contained in the sputtering gas is more than or equal to 1% and less than or equal to 30%, preferably 5% to 20%,. A transistor using an oxygen-deficient oxide semiconductor for a channel formation region can have relatively high field-effect mobility. When the oxide film is formed while the substrate is heated, the crystallinity of the oxide film can be improved.

[0263] In this embodiment, the oxide film 230A is formed by sputtering using an oxide target with an atomic ratio of In:Ga:Zn=1:3:4. The oxide film 230B is formed by sputtering using an oxide target with an atomic ratio of In:Ga:Zn=4:2:4.1. Each oxide film may be formed according to the characteristics required for the oxide 230a and the oxide 230b by appropriately selecting the film formation conditions and atomic ratio.

[0264] Next, the oxide film 243A is formed on the oxide film 230B (see FIGS. 6A to 6D). The oxide film 243A can be formed by sputtering, CVD, MBE, PLD, ALD, or the like. The atomic ratio of Ga to In in the oxide film 243A is preferably greater than the atomic ratio of Ga to In in the oxide film 230B. In this embodiment, the oxide film 243A is formed by sputtering using an oxide target with an atomic ratio of In:Ga:Zn=1:3:4.

[0265] It is preferable to form the insulator 222, the insulator 224, the oxide film 230A, the oxide film 230B, and the oxide film 243A by a sputtering method without exposing them to the atmosphere. For example, a multi-chamber film forming apparatus may be used. This allows the insulator 222, the insulator 224, the oxide film 230A, the oxide film 230B, and the oxide film 243A to be formed with reduced hydrogen in the films, and further reduces the inclusion of hydrogen in the films between each film forming process.

[0266] Next, it is preferable to perform a heat treatment. The heat treatment may be performed in a temperature range in which the oxide film 230A, the oxide film 230B, and the oxide film 243A are not polycrystallized, and may be performed at 250°C to 650°C, preferably 400°C to 600°C. The heat treatment is performed in an atmosphere of nitrogen gas or an inert gas, or an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas. For example, when the heat treatment is performed in a mixed atmosphere of nitrogen gas and oxygen gas, the oxygen gas may be about 20%. The heat treatment may be performed under reduced pressure. Alternatively, the heat treatment may be performed in an atmosphere of nitrogen gas or an inert gas, and then in an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas to compensate for the desorbed oxygen.

[0267] In addition, the gas used in the heat treatment is preferably highly purified. For example, the amount of moisture contained in the gas used in the heat treatment may be 1 ppb or less, preferably 0.1 ppb or less, and more preferably 0.05 ppb or less. By using a highly purified gas to perform the heat treatment, it is possible to prevent moisture and the like from being taken into the oxide film 230A, the oxide film 230B, and the oxide film 243A as much as possible.

[0268] In this embodiment, the heat treatment is performed in a nitrogen atmosphere at 550° C. for 1 hour, followed by another heat treatment in an oxygen atmosphere at 550° C. for 1 hour. This heat treatment can remove impurities such as water and hydrogen from the oxide film 230A, the oxide film 230B, and the oxide film 243A. Furthermore, this heat treatment can improve the crystallinity of the oxide film 230B, resulting in a denser and more compact structure. This can reduce the diffusion of oxygen or impurities in the oxide film 230B.

[0269] Next, the conductive film 242A is formed on the oxide film 243A (see FIGS. 6A to 6D). The conductive film 242A can be formed by sputtering, CVD, MBE, PLD, ALD, or the like. For example, tantalum nitride may be formed as the conductive film 242A by sputtering. Note that heat treatment may be performed before the conductive film 242A is formed. The heat treatment may be performed under reduced pressure, and the conductive film 242A may be formed continuously without exposure to the air. By performing such treatment, moisture and hydrogen adsorbed on the surface of the oxide film 243A can be removed, and the moisture concentration and hydrogen concentration in the oxide film 230A, the oxide film 230B, and the oxide film 243A can be further reduced. The temperature of the heat treatment is preferably 100° C. or higher and 400° C. or lower. In this embodiment, the temperature of the heat treatment is set to 200° C.

[0270] Next, the oxide film 230A, the oxide film 230B, the oxide film 243A, and the conductive film 242A are processed into an island shape by using a lithography method to form the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B (see FIGS. 7A to 7D). This processing can be performed by a dry etching method or a wet etching method. Processing by the dry etching method is suitable for fine processing. The oxide film 230A, the oxide film 230B, the oxide film 243A, and the conductive film 242A may be processed under different conditions. In this process, the thickness of the region of the insulator 224 that does not overlap with the oxide 230a may become thin. In this process, the insulator 224 may be processed into an island shape by overlapping with the oxide 230a.

[0271] In the lithography method, first, the resist is exposed through a mask. Next, the exposed area is removed or left using a developer to form a resist mask. Next, a conductor, a semiconductor, an insulator, or the like can be processed into a desired shape by etching through the resist mask. For example, a resist mask may be formed by exposing the resist using KrF excimer laser light, ArF excimer laser light, EUV (Extreme Ultraviolet) light, or the like. Also, a liquid immersion technique may be used in which a liquid (e.g., water) is filled between the substrate and the projection lens and exposure is performed. Also, an electron beam or an ion beam may be used instead of the light described above. When an electron beam or an ion beam is used, a mask is not required. The resist mask can be removed by performing a dry etching process such as ashing, a wet etching process, a wet etching process after a dry etching process, or a dry etching process after a wet etching process.

[0272] Furthermore, a hard mask made of an insulator or a conductor may be used under the resist mask. When using a hard mask, an insulating film or a conductive film that will be the hard mask material is formed on the conductive film 242A, a resist mask is formed thereon, and the hard mask material is etched to form a hard mask of a desired shape. Etching of the conductive film 242A and the like may be performed after removing the resist mask, or may be performed while leaving the resist mask. In the latter case, the resist mask may disappear during etching. After etching of the conductive film 242A and the like, the hard mask may be removed by etching. On the other hand, if the material of the hard mask does not affect the subsequent process or can be used in the subsequent process, it is not necessarily necessary to remove the hard mask. For example, when the hard mask is formed of an insulating film, the hard mask may be left and used as a barrier insulating film.

[0273] Moreover, the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B are formed so that at least a part of them overlap with the conductor 248 and the two conductors 205. Moreover, it is preferable that the side surfaces of the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B are approximately perpendicular to the upper surface of the insulator 222. When the side surfaces of the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B are approximately perpendicular to the upper surface of the insulator 222, it is possible to reduce the area and increase the density when providing a plurality of transistors 200. Alternatively, a configuration may be used in which the angle between the side surfaces of the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B and the upper surface of the insulator 222 is low. In this case, the angle between the side surfaces of the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B and the upper surface of the insulator 222 is preferably 60 degrees or more and less than 70 degrees. By forming the shape in this way, the coverage of the insulator 275 and the like can be improved in the subsequent steps, and defects such as voids can be reduced.

[0274] In addition, by-products generated in the above etching process may be formed in layers on the side surfaces of the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B. In this case, the layered by-products are formed between the oxide 230a, the oxide 230b, the oxide 243, and the conductor 242 and the insulator 275. Similarly, layered by-products may be formed on the insulator 224. Even if the insulator 275 is formed in a state in which the layered by-products are formed on the insulator 224, the layered by-products will prevent oxygen from being added to the insulator 224. Therefore, it is preferable to remove the layered by-products formed in contact with the upper surface of the insulator 224.

[0275] Next, the insulator 275 is formed over the insulator 224, the oxide 230a, the oxide 230b, the oxide layer 243B, and the conductive layer 242B (see FIGS. 8A to 8D). The insulator 275 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. It is preferable that the insulator 275 is an insulating film having a function of suppressing oxygen permeation. For example, the insulator 275 may be formed of aluminum oxide by an ALD method or a sputtering method. The insulator 275 may also be formed of silicon nitride by a sputtering method.

[0276] Note that oxygen can be added to the insulator 224 by forming the insulator 275 by a sputtering method.

[0277] Next, an insulating film to be the insulator 280 is formed on the insulator 275. The insulating film can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. For example, a silicon oxide film may be formed by a sputtering method as the insulating film. The insulating film to be the insulator 280 can be formed by a sputtering method in an atmosphere containing oxygen, thereby forming the insulator 280 containing excess oxygen. In addition, the hydrogen concentration in the insulator 280 can be reduced by using a sputtering method that does not require hydrogen as a deposition gas. Note that a heat treatment may be performed before the insulating film is formed. The heat treatment may be performed under reduced pressure, and the insulating film may be formed continuously without exposure to the atmosphere. By performing such a treatment, moisture and hydrogen adsorbed on the surface of the insulator 275 and the like can be removed, and the moisture concentration and hydrogen concentration in the oxide 230a, the oxide 230b, the oxide layer 243B, and the insulator 224 can be further reduced. The heat treatment conditions described above can be used for the heat treatment.

[0278] Next, the insulating film that becomes the insulator 280 is subjected to CMP processing to form the insulator 280 with a flat upper surface (see FIGS. 8A to 8D). Note that a silicon nitride film may be formed on the insulator 280 by, for example, a sputtering method, and the silicon nitride may be subjected to CMP processing until it reaches the insulator 280.

[0279] Next, a part of the insulator 280, a part of the insulator 275, a part of the conductive layer 242B, a part of the oxide layer 243B, and a part of the oxide 230b are removed to form two openings reaching the oxide 230b. The two openings are preferably formed so as to overlap the conductor 205. By forming the openings, the conductor 242a, the conductor 242b, the conductor 242c, the oxide 243a, the oxide 243b, and the oxide 243c are formed (see FIGS. 9A to 9D). Here, the conductor 242b is preferably formed so as to overlap the conductor 248. In addition, the regions of the oxide 230b that do not overlap the conductor 242a, the conductor 242b, and the conductor 242c are exposed.

[0280] When forming the opening, the upper part of the oxide 230b is removed. By removing a part of the oxide 230b, a groove is formed in the oxide 230b. Depending on the depth of the groove, the groove may be formed in the process of forming the opening, or may be formed in a process different from the process of forming the opening.

[0281] In addition, a part of the insulator 280, a part of the insulator 275, a part of the conductive layer 242B, a part of the oxide layer 243B, and a part of the oxide 230b can be processed by dry etching or wet etching. Processing by the dry etching method is suitable for fine processing. In addition, the processing may be performed under different conditions. For example, a part of the insulator 280 may be processed by dry etching, a part of the insulator 275 may be processed by wet etching, and a part of the oxide layer 243B, a part of the conductive layer 242B, and a part of the oxide 230b may be processed by dry etching. In this case, first, two openings are formed in the insulator 280, and openings are formed in the insulator 275, the oxide layer 243B, and the conductive layer 242B so as to overlap the two openings. In addition, processing of a part of the oxide layer 243B and a part of the conductive layer 242B and processing of a part of the oxide 230b may be performed under different conditions.

[0282] Here, it is preferable to remove impurities attached to the surfaces of the oxide 230a, the oxide 230b, etc. or diffused therein. It is also preferable to remove damaged areas formed on the surface of the oxide 230b by the dry etching. The impurities include those originating from components contained in the insulator 280, the insulator 275, and the conductive layer 242B, components contained in the members used in the device used to form the opening, and components contained in the gas or liquid used in the etching. The impurities include, for example, aluminum, silicon, tantalum, fluorine, and chlorine.

[0283] In particular, impurities such as aluminum or silicon inhibit the oxide 230b from becoming a CAAC-OS. Therefore, it is preferable that impurity elements such as aluminum or silicon that inhibit the CAAC-OS formation are reduced or removed. For example, the concentration of aluminum atoms in the oxide 230b and its vicinity may be 5.0 atomic % or less, preferably 2.0 atomic % or less, more preferably 1.5 atomic % or less, even more preferably 1.0 atomic % or less, and even more preferably less than 0.3 atomic %.

[0284] In addition, the region of the metal oxide in which the CAAC-OS formation is inhibited by impurities such as aluminum or silicon and which becomes an amorphous-like oxide semiconductor (a-like OS) is sometimes called a non-CAAC region. In the non-CAAC region, the density of the crystal structure is reduced, so the V O A large amount of H is formed, which makes the transistor more likely to be normally on. Therefore, it is preferable that the non-CAAC region of the oxide 230b is reduced or removed.

[0285] In contrast, it is preferable that the oxide 230b has a layered CAAC structure. In particular, it is preferable that the oxide 230b has the CAAC structure up to the drain lower end. Here, in the transistor 200, the conductor 242a, the conductor 242b, or the conductor 242c and the vicinity thereof function as the drain. In other words, it is preferable that the oxide 230b near the lower end of the conductor 242a, the conductor 242b, or the conductor 242c has the CAAC structure. In this way, even at the drain end, which significantly affects the drain breakdown voltage, the damaged region of the oxide 230b is removed, and by having the CAAC structure, the fluctuation in the electrical characteristics of the transistor 200 can be further suppressed. In addition, the reliability of the transistor 200 can be improved.

[0286] In order to remove the above-mentioned impurities, a cleaning process is performed. The cleaning method includes wet cleaning using a cleaning solution, plasma processing using plasma, cleaning by heat treatment, and the like, and the above cleaning methods may be combined appropriately. Note that the above-mentioned grooves may become deeper due to the cleaning process.

[0287] For wet cleaning, a cleaning process may be performed using an aqueous solution of ammonia water, oxalic acid, phosphoric acid, hydrofluoric acid, or the like diluted with carbonated water or pure water, pure water, carbonated water, or the like. Alternatively, ultrasonic cleaning may be performed using these aqueous solutions, pure water, or carbonated water. Alternatively, these cleaning methods may be combined as appropriate.

[0288] In this specification, an aqueous solution obtained by diluting commercially available hydrofluoric acid with pure water may be called diluted hydrofluoric acid, and an aqueous solution obtained by diluting commercially available ammonia water with pure water may be called diluted ammonia water. The concentration and temperature of the aqueous solution may be appropriately adjusted depending on the impurities to be removed and the configuration of the semiconductor device to be cleaned. The ammonia concentration of the diluted ammonia water may be 0.01% or more and 5% or less, preferably 0.1% or more and 0.5% or less. The hydrogen fluoride concentration of the diluted hydrofluoric acid may be 0.01 ppm or more and 100 ppm or less, preferably 0.1 ppm or more and 10 ppm or less.

[0289] In addition, it is preferable to use a frequency of 200 kHz or more, and more preferably 900 kHz or more, for ultrasonic cleaning. By using such a frequency, damage to the oxide 230b and the like can be reduced.

[0290] The above cleaning process may be performed multiple times, and the cleaning solution may be changed for each cleaning process. For example, a first cleaning process may be performed using diluted hydrofluoric acid or diluted ammonia water, and a second cleaning process may be performed using pure water or carbonated water.

[0291] In the present embodiment, as the cleaning process, wet cleaning is performed using diluted hydrofluoric acid, followed by wet cleaning using pure water or carbonated water. By performing this cleaning process, impurities attached to the surfaces of the oxide 230a, the oxide 230b, etc. or diffused inside can be removed. Furthermore, the crystallinity of the oxide 230b can be improved.

[0292] In the past, processing such as dry etching or the above-mentioned cleaning process may result in the thickness of insulator 224 in the area that overlaps with the opening but does not overlap with oxide 230b being thinner than the thickness of insulator 224 in the area that overlaps with oxide 230b.

[0293] After the etching or cleaning, a heat treatment may be performed. The heat treatment may be performed at a temperature of 100° C. to 450° C., preferably 350° C. to 400° C. The heat treatment is performed in an atmosphere of nitrogen gas or an inert gas, or an atmosphere containing 10 ppm or more, 1% or more, or 10% or more of an oxidizing gas. For example, the heat treatment is preferably performed in an oxygen atmosphere. This supplies oxygen to the oxide 230a and the oxide 230b, thereby reducing the oxygen vacancy V. O In addition, by performing such a heat treatment, the crystallinity of the oxide 230b can be improved. The heat treatment may be performed under reduced pressure. Alternatively, after the heat treatment in an oxygen atmosphere, the heat treatment may be performed in a nitrogen atmosphere without exposure to the air.

[0294] Next, the insulating film 250A is formed (see FIGS. 10A to 10D). A heat treatment may be performed before the formation of the insulating film 250A, and the heat treatment may be performed under reduced pressure, and the insulating film 250A may be formed continuously without exposure to the atmosphere. The heat treatment is preferably performed in an atmosphere containing oxygen. By performing such a treatment, moisture and hydrogen adsorbed on the surface of the oxide 230b can be removed, and the moisture concentration and hydrogen concentration in the oxide 230a and the oxide 230b can be further reduced. The temperature of the heat treatment is preferably 100° C. or higher and 400° C. or lower.

[0295] The insulating film 250A can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. The insulating film 250A is preferably formed by a film formation method using a gas in which hydrogen atoms are reduced or removed. This allows the hydrogen concentration of the insulating film 250A to be reduced. Since the insulating film 250A becomes the insulator 250 that contacts the oxide 230b in a later process, it is preferable that the hydrogen concentration is reduced in this manner.

[0296] In addition, it is preferable to form the insulating film 250A by using the ALD method. The thickness of the insulator 250 functioning as the gate insulating film of the miniaturized transistor 200 must be extremely thin (for example, about 5 nm to 30 nm) and have small variations. In contrast, the ALD method is a film formation method in which a precursor and a reactant (oxidizer) are alternately introduced, and the thickness can be adjusted by the number of times this cycle is repeated, so that precise thickness adjustment is possible. Therefore, the precision of the thickness of the gate insulating film required by the miniaturized transistor 200 can be achieved. In addition, as shown in FIG. 10B and FIG. 10C, the insulating film 250A must be formed with good coverage on the bottom and side of the opening formed by the insulator 280, etc. Since layers of atoms can be deposited one by one on the bottom and side of the opening, the insulating film 250A can be formed with good coverage on the opening.

[0297] In addition, for example, when the insulating film 250A is formed by using the PECVD method, the film formation gas containing hydrogen is decomposed in the plasma, and a large amount of hydrogen radicals is generated. The oxygen in the oxide 230b is extracted by the reduction reaction of the hydrogen radicals, and V OWhen H is formed, the hydrogen concentration in the oxide 230b increases. However, when the insulating film 250A is formed using the ALD method, the generation of hydrogen radicals can be suppressed both when the precursor and the reactant are introduced. Therefore, by forming the insulating film 250A using the ALD method, it is possible to prevent the hydrogen concentration in the oxide 230b from increasing. For example, a silicon oxide film such as silicon oxide may be formed as the insulating film 250A using the ALD method.

[0298] In addition, in FIG. 10B, FIG. 10C, and FIG. 10D, the insulating film 250A is illustrated as a single layer, but it may have a laminated structure of two or more layers. When the insulating film 250A has a laminated structure of two layers, it is preferable that the lower layer of the insulating film 250A is formed using an insulator that releases oxygen when heated, and the upper layer of the insulating film 250A is formed using an insulator that has a function of suppressing the diffusion of oxygen. With such a configuration, it is possible to suppress the diffusion of oxygen contained in the lower layer of the insulator 250 to the conductor 260. In other words, it is possible to suppress the decrease in the amount of oxygen supplied to the oxide 230. In addition, it is possible to suppress the oxidation of the conductor 260 due to the oxygen contained in the lower layer of the insulator 250. For example, the lower layer of the insulating film 250A is provided using a material that can be used for the insulator 250 described above, and the upper layer of the insulating film 250A can be provided using a material similar to that of the insulator 222.

[0299] Specifically, the upper layer of the insulating film 250A may be a metal oxide containing one or more elements selected from hafnium, aluminum, gallium, yttrium, zirconium, tungsten, titanium, tantalum, nickel, germanium, magnesium, etc., or a metal oxide that can be used as the oxide 230. In particular, it is preferable to use an insulator containing an oxide of one or both of aluminum and hafnium.

[0300] In this embodiment, the insulating film 250A has a two-layer laminate structure, with a lower layer of silicon oxide formed by the PEALD method and an upper layer of hafnium oxide formed by the thermal ALD method.

[0301] In addition, when the insulating film 250A has a two-layer laminated structure, it is preferable to continuously deposit the insulating film that is the lower layer of the insulating film 250A and the insulating film that is the upper layer of the insulating film 250A without exposing them to the air environment. By depositing the films without exposing them to the air, it is possible to prevent impurities such as hydrogen or moisture from the air environment from adhering to the insulating film that is the lower layer of the insulating film 250A and the insulating film that is the upper layer of the insulating film 250A, and it is possible to keep the vicinity of the interface between the insulating film that is the lower layer of the insulating film 250A and the insulating film that is the upper layer of the insulating film 250A clean.

[0302] Next, microwave processing is performed in an atmosphere containing oxygen (see Figs. 10A to 10D). Here, the dotted lines shown in Figs. 10B, 10C, and 10D indicate microwaves, high frequency such as RF, oxygen plasma, or oxygen radicals. For the microwave processing, it is preferable to use a microwave processing device having a power source that generates high density plasma using microwaves. The microwave processing device may also have a power source that applies RF to the substrate side. By using high density plasma, high density oxygen radicals can be generated. By applying RF to the substrate side, oxygen ions generated by high density plasma can be efficiently introduced into the oxide 230b. The microwave processing is preferably performed under reduced pressure, with the pressure being 60 Pa or more, preferably 133 Pa or more, more preferably 200 Pa or more, and even more preferably 400 Pa or more. The oxygen flow rate ratio (O2 / O2+Ar) is preferably 50% or less, and preferably 10% to 30%. The treatment temperature may be 750° C. or less, preferably 500° C. or less, for example, about 400° C. After the oxygen plasma treatment, a heat treatment may be performed continuously without exposure to the outside air.

[0303] As shown in Figures 10B, 10C, and 10D, by performing microwave processing in an atmosphere containing oxygen, oxygen gas can be turned into plasma using microwaves or high frequency waves such as RF, and the oxygen plasma can be applied to the region between conductor 242a and conductor 242b of oxide 230b, and to the region between conductor 242b and conductor 242c. At this time, microwaves or high frequency waves such as RF can also be irradiated. In other words, microwaves, high frequency waves such as RF, oxygen plasma, etc. can be applied to region 232d and region 232e shown in Figure 2. The action of plasma, microwaves, etc. increases the V of region 232d and region 232e. O H can be split off and hydrogen H can be removed from the regions 232d and 232e. O H→H+V O " occurs, and the hydrogen concentration in the regions 232d and 232e can be reduced. Therefore, oxygen vacancies and V O By supplying oxygen radicals generated by the oxygen plasma or oxygen contained in the insulator 250 to the oxygen vacancies formed in the regions 232d and 232e, the oxygen vacancies in the regions 232d and 232e can be further reduced, and the carrier concentration can be reduced.

[0304] On the other hand, conductors 242a, 242b, and 242c are provided on regions 232a, 232b, and 232c. As shown in Fig. 10B, 10C, and 10D, conductors 242a, 242b, and 242c shield the effects of microwaves, high frequency waves such as RF, oxygen plasma, and the like, so that these effects do not reach regions 232a, 232b, and 232c. As a result, V O Since there is no reduction in H and no excessive supply of oxygen, a decrease in the carrier concentration can be prevented.

[0305] In this manner, oxygen vacancies and V O By removing H, the region 232d and the region 232e can be made i-type or substantially i-type. Furthermore, the supply of excess oxygen to the region 232a, the region 232b, and the region 232c that function as the source region or the drain region can be suppressed, and the n-type can be maintained. This can suppress the fluctuation of the electrical characteristics of the transistor 200, and can suppress the variation of the electrical characteristics of the transistor 200 in the substrate surface. In addition, since the conductor 248 is provided so as to overlap the conductor 242b, the upper surface of the conductor 248 contacts the region 232b in a self-aligned manner, and therefore the transistors 200a and 200b and the conductor 248 can form good contacts.

[0306] In this manner, a semiconductor device with less variation in transistor characteristics can be provided, a semiconductor device with good electrical characteristics can be provided, and a semiconductor device with good reliability can be provided.

[0307] 10, the microwave treatment is performed after the insulating film 250A is formed, but the present invention is not limited to this. For example, the microwave treatment may be performed before the insulating film 250A is formed, or may be performed both before and after the insulating film 250A is formed.

[0308] For example, when the insulating film 250A has the above-mentioned two-layer structure, a microwave process is performed, silicon oxide is formed as the lower layer of the insulating film 250A by the PEALD method, and hafnium oxide is formed as the upper layer of the insulating film 250A by the thermal ALD method. Here, it is preferable to perform the microwave process, the PEALD formation of silicon oxide, and the thermal ALD formation of hafnium oxide successively without exposure to the atmosphere. For example, a multi-chamber processing device may be used. The microwave process may be replaced by a process using a plasma-excited reactant (oxidant) in a PEALD device. Here, oxygen gas may be used as the reactant (oxidant).

[0309] Moreover, a heat treatment may be performed while maintaining the reduced pressure state after the microwave treatment. By performing such a treatment, hydrogen in the insulating film 250A, the oxide 230b, and the oxide 230a can be efficiently removed. A part of the hydrogen may be gettered to the conductor 242 (the conductor 242a and the conductor 242b). Alternatively, a step of performing a heat treatment may be repeated multiple times while maintaining the reduced pressure state after the microwave treatment. By repeatedly performing the heat treatment, hydrogen in the insulating film 250A, the oxide 230b, and the oxide 230a can be more efficiently removed. The heat treatment temperature is preferably 300° C. or more and 500° C. or less.

[0310] Moreover, by modifying the film quality of the insulating film 250A by microwave processing, it is possible to suppress the diffusion of hydrogen, water, impurities, etc. Therefore, it is possible to suppress the diffusion of hydrogen, water, impurities, etc. into the oxide 230b, the oxide 230a, etc. through the insulator 250 by a post-process such as film formation of a conductive film that becomes the conductor 260, or a post-process such as heat treatment.

[0311] Next, a conductive film that becomes the conductor 260a and a conductive film that becomes the conductor 260b are formed in this order. The conductive film that becomes the conductor 260a and the conductive film that becomes the conductor 260b can be formed using a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. In this embodiment, the conductive film that becomes the conductor 260a is formed using the ALD method, and the conductive film that becomes the conductor 260b is formed using the CVD method.

[0312] Next, the insulating film 250A, the conductive film to be the conductor 260a, and the conductive film to be the conductor 260b are polished by CMP until the insulator 280 is exposed, thereby forming the insulator 250 and the conductor 260 (the conductor 260a and the conductor 260b) corresponding to the transistor 200a and the transistor 200b, respectively (see FIGS. 11A to 11D). As a result, the insulator 250 of the transistor 200a and the transistor 200b is arranged so as to cover the two openings reaching the oxide 230b and the inner walls (side walls and bottom surface) of the groove of the oxide 230b. Also, the conductor 260 of the transistor 200a and the transistor 200b is arranged so as to fill the two openings and the groove through the insulator 250.

[0313] Next, heat treatment may be performed under the same conditions as the above heat treatment. In this embodiment, the treatment is performed in a nitrogen atmosphere at a temperature of 400° C. for 1 hour. The heat treatment can reduce the moisture and hydrogen concentrations in the insulators 250 and 280. Note that after the heat treatment, the insulator 282 may be formed without exposure to the air.

[0314] Next, the insulator 282 is formed over the insulator 250, the conductor 260, and the insulator 280 (see FIGS. 12A to 12D). The insulator 282 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. The insulator 282 is preferably formed by a sputtering method. By using a sputtering method that does not require the use of hydrogen in the film formation gas, the hydrogen concentration in the insulator 282 can be reduced. In addition, by forming the insulator 282 in an atmosphere containing oxygen by using a sputtering method, oxygen can be added to the insulator 280 while forming the film. This allows the insulator 280 to contain excess oxygen. At this time, the insulator 282 is preferably formed while heating the substrate.

[0315] In this embodiment, an aluminum oxide film is formed by pulse DC sputtering using an aluminum target in an atmosphere containing oxygen gas as the insulator 282. By using the pulse DC sputtering method, the film thickness distribution can be made more uniform, and the sputtering rate and film quality can be improved.

[0316] Next, the insulator 283 is formed over the insulator 282 (see FIGS. 1A to 1D). The insulator 283 can be formed by a sputtering method, a CVD method, an MBE method, a PLD method, an ALD method, or the like. The insulator 283 is preferably formed by a sputtering method. By using a sputtering method that does not require hydrogen as a deposition gas, the hydrogen concentration in the insulator 283 can be reduced. The insulator 283 may have a multilayer structure. For example, a silicon nitride film may be formed by a sputtering method, and a silicon nitride film may be formed on the silicon nitride by a CVD method. By enclosing the transistor 200 with the insulator 283 and the insulator 212 that have high barrier properties, it is possible to prevent moisture and hydrogen from entering from the outside.

[0317] Next, heat treatment may be performed. In this embodiment, the treatment is performed in a nitrogen atmosphere at a temperature of 400° C. for one hour. By this heat treatment, as shown in FIG. 2, oxygen added by the formation of the insulator 282 can be diffused to the insulators 280 and 250 and selectively supplied to the channel formation region of the oxide 230. Note that the heat treatment may be performed not only after the formation of the insulator 283 but also after the formation of the insulator 282.

[0318] Through the above steps, a semiconductor device including the transistor 200 illustrated in Figures 1A to 1D can be manufactured. As illustrated in Figures 4A to 12A, 4B to 12B, 4C to 12C, and 4D to 12D, the transistor 200 can be manufactured by the method for manufacturing a semiconductor device described in this embodiment.

[0319] <Microwave processing equipment> A microwave processing apparatus that can be used in the above-described method for manufacturing a semiconductor device will be described below.

[0320] First, the configuration of a manufacturing apparatus that reduces the inclusion of impurities during the manufacture of semiconductor devices and the like will be described with reference to FIGS.

[0321] 13 is a schematic top view of a single-wafer multi-chamber manufacturing apparatus 2700. The manufacturing apparatus 2700 includes an atmosphere-side substrate supply chamber 2701 having a cassette port 2761 for accommodating a substrate and an alignment port 2762 for aligning the substrate, an atmosphere-side substrate transfer chamber 2702 for transferring the substrate from the atmosphere-side substrate supply chamber 2701, a load lock chamber 2703a for loading the substrate and for reducing the pressure in the chamber from atmospheric pressure or for switching the pressure from reduced pressure to atmospheric pressure, an unload lock chamber 2703b for unloading the substrate and for switching the pressure in the chamber from reduced pressure to atmospheric pressure or for switching the pressure from atmospheric pressure to reduced pressure, a transfer chamber 2704 for transferring the substrate in a vacuum, a chamber 2706a, a chamber 2706b, a chamber 2706c, and a chamber 2706d.

[0322] The atmospheric side substrate transfer chamber 2702 is connected to a load lock chamber 2703a and an unload lock chamber 2703b, the load lock chamber 2703a and the unload lock chamber 2703b are connected to a transfer chamber 2704, and the transfer chamber 2704 is connected to a chamber 2706a, a chamber 2706b, a chamber 2706c, and a chamber 2706d.

[0323] A gate valve GV is provided at the connection between each chamber, and each chamber can be independently maintained in a vacuum state, except for the atmosphere side substrate supply chamber 2701 and the atmosphere side substrate transfer chamber 2702. A transfer robot 2763a is provided in the atmosphere side substrate transfer chamber 2702, and a transfer robot 2763b is provided in the transfer chamber 2704. Substrates can be transferred within the manufacturing apparatus 2700 by the transfer robot 2763a and the transfer robot 2763b.

[0324] The back pressure (total pressure) of the transfer chamber 2704 and each chamber is, for example, 1×10 -4 Pa or less, preferably 3×10 -5 Pa or less, more preferably 1×10 -5 The partial pressure of gas molecules (atoms) with a mass-to-charge ratio (m / z) of 18 in the transfer chamber 2704 and each chamber is, for example, 3×10 -5 Pa or less, preferably 1×10 -5 Pa or less, more preferably 3×10 -6 The partial pressure of gas molecules (atoms) with m / z of 28 in the transfer chamber 2704 and each chamber is, for example, 3×10 -5 Pa or less, preferably 1×10 -5 Pa or less, more preferably 3×10 -6 The partial pressure of gas molecules (atoms) with m / z of 44 in the transfer chamber 2704 and each chamber is, for example, 3×10 -5 Pa or less, preferably 1×10 -5 Pa or less, more preferably 3×10 -6 Pa or less.

[0325] The total pressure and partial pressure in the transfer chamber 2704 and each chamber can be measured using a mass spectrometer. For example, a quadrupole mass spectrometer (also called Q-mass) Qulee CGM-051 manufactured by ULVAC, Inc. may be used.

[0326] In addition, it is desirable that the transfer chamber 2704 and each chamber have a configuration with little external or internal leakage. For example, the leak rate of the transfer chamber 2704 and each chamber is 3×10 -6 Pa·m 3 / s or less, preferably 1×10 -6 Pa·m 3 / s or less. For example, the leak rate of a gas molecule (atom) with m / z of 18 is 1×10 -7 Pa·m 3 / s or less, preferably 3×10 -8 Pa·m 3 / s or less. For example, the leak rate of a gas molecule (atom) with m / z of 28 is 1×10 -5 Pa·m 3 / s or less, preferably 1×10 -6 Pa·m 3 / s or less. For example, the leak rate of a gas molecule (atom) with m / z of 44 is 3×10 -6 Pa·m 3 / s or less, preferably 1×10 -6 Pa·m 3 / s or less.

[0327] The leak rate can be derived from the total pressure and partial pressure measured using the mass spectrometer mentioned above. The leak rate depends on external and internal leaks. External leaks are gases that flow in from outside the vacuum system due to tiny holes or poor seals. Internal leaks are caused by leaks from partitions such as valves in the vacuum system and gases released from internal components. To keep the leak rate below the above values, measures must be taken to prevent both external and internal leaks.

[0328] For example, the opening and closing parts of the transfer chamber 2704 and each chamber may be sealed with a metal gasket. The metal gasket is preferably made of a metal coated with iron fluoride, aluminum oxide, or chromium oxide. Metal gaskets have higher adhesion than O-rings and can reduce external leakage. In addition, by using a passivated metal coated with iron fluoride, aluminum oxide, chromium oxide, or the like, the release of gas containing impurities from the metal gasket is suppressed, and internal leakage can be reduced.

[0329] In addition, aluminum, chromium, titanium, zirconium, nickel, or vanadium, which emits less gas containing impurities, is used as the members constituting the manufacturing apparatus 2700. The above-mentioned members may be coated with an alloy containing iron, chromium, nickel, etc. The alloy containing iron, chromium, nickel, etc. is rigid, heat-resistant, and suitable for processing. Here, if the surface irregularities of the members are reduced by polishing or the like in order to reduce the surface area, the amount of emitted gas can be reduced.

[0330] Alternatively, the components of the manufacturing apparatus 2700 described above may be coated with iron fluoride, aluminum oxide, chromium oxide, or the like.

[0331] It is preferable that the components of the manufacturing apparatus 2700 are constructed solely from metal as much as possible. For example, even if a viewing window made of quartz or the like is installed, it is advisable to thinly coat the surface with iron fluoride, aluminum oxide, chromium oxide, or the like to suppress outgassing.

[0332] The adsorbed matter present in the transfer chamber 2704 and each chamber does not affect the pressure of the transfer chamber 2704 and each chamber because it is adsorbed to the inner walls, but it causes gas emission when the transfer chamber 2704 and each chamber are evacuated. Therefore, although there is no correlation between the leak rate and the exhaust speed, it is important to use a pump with high exhaust capacity to desorb as much of the adsorbed matter present in the transfer chamber 2704 and each chamber and evacuate them in advance. In addition, the transfer chamber 2704 and each chamber may be baked to promote the desorption of the adsorbed matter. By baking, the desorption speed of the adsorbed matter can be increased by about 10 times. Baking may be performed at 100°C or higher and 450°C or lower. At this time, if the adsorbed matter is removed while introducing an inert gas into the transfer chamber 2704 and each chamber, the desorption speed of water and the like that is difficult to desorb by only exhausting can be further increased. In addition, the desorption speed of the adsorbed matter can be further increased by heating the inert gas introduced to the same temperature as the baking temperature. Here, it is preferable to use a rare gas as the inert gas.

[0333] Alternatively, it is preferable to increase the pressure in the transfer chamber 2704 and each chamber by introducing an inert gas such as a heated rare gas or oxygen, and then evacuate the transfer chamber 2704 and each chamber again after a certain time has passed. By introducing a heated gas, it is possible to desorb adsorbed substances in the transfer chamber 2704 and each chamber, and it is possible to reduce impurities present in the transfer chamber 2704 and each chamber. It is effective to repeat this process 2 to 30 times, preferably 5 to 15 times. Specifically, by introducing an inert gas or oxygen having a temperature of 40° C. to 400° C., preferably 50° C. to 200° C., the pressure in the transfer chamber 2704 and each chamber is set to 0.1 Pa to 10 kPa, preferably 1 Pa to 1 kPa, and more preferably 5 Pa to 100 Pa, and the period for maintaining the pressure is 1 minute to 300 minutes, preferably 5 minutes to 120 minutes. Thereafter, the transfer chamber 2704 and each chamber are evacuated for a period of 5 to 300 minutes, preferably 10 to 120 minutes.

[0334] Next, chamber 2706b and chamber 2706c will be described with reference to the schematic cross-sectional view shown in FIG.

[0335] The chamber 2706b and the chamber 2706c are chambers capable of performing microwave processing on an object to be processed, for example. The chamber 2706b and the chamber 2706c differ only in the atmosphere during microwave processing. Since the other configurations are common, they will be described together below.

[0336] The chamber 2706b and the chamber 2706c have a slot antenna plate 2808, a dielectric plate 2809, a substrate holder 2812, and an exhaust port 2819. In addition, outside the chamber 2706b and the chamber 2706c, a gas supply source 2801, a valve 2802, a high frequency generator 2803, a waveguide 2804, a mode converter 2805, a gas pipe 2806, a waveguide 2807, a matching box 2815, a high frequency power supply 2816, a vacuum pump 2817, and a valve 2818 are provided.

[0337] The high frequency generator 2803 is connected to the mode converter 2805 via a waveguide 2804. The mode converter 2805 is connected to a slot antenna plate 2808 via a waveguide 2807. The slot antenna plate 2808 is disposed in contact with a dielectric plate 2809. The gas supply source 2801 is connected to the mode converter 2805 via a valve 2802. Gas is sent to the chambers 2706b and 2706c through a gas pipe 2806 passing through the mode converter 2805, the waveguide 2807, and the dielectric plate 2809. The vacuum pump 2817 has a function of exhausting gas and the like from the chambers 2706b and 2706c via a valve 2818 and an exhaust port 2819. The high frequency power supply 2816 is connected to the substrate holder 2812 via a matching box 2815.

[0338] The substrate holder 2812 has a function of holding the substrate 2811. For example, the substrate holder 2812 has a function of electrostatically or mechanically chucking the substrate 2811. The substrate holder 2812 also has a function as an electrode to which power is supplied from a high frequency power supply 2816. The substrate holder 2812 also has an internal heating mechanism 2813 and has a function of heating the substrate 2811.

[0339] For example, a dry pump, a mechanical booster pump, an ion pump, a titanium sublimation pump, a cryopump, or a turbo molecular pump can be used as the vacuum pump 2817. A cryotrap may be used in addition to the vacuum pump 2817. The use of a cryopump and a cryotrap is particularly preferable because water can be efficiently exhausted.

[0340] The heating mechanism 2813 may be, for example, a heating mechanism that uses a resistance heating element or the like for heating. Alternatively, it may be a heating mechanism that uses heat conduction or heat radiation from a medium such as a heated gas for heating. For example, RTA (Rapid Thermal Annealing) such as GRTA (Gas Rapid Thermal Annealing) or LRTA (Lamp Rapid Thermal Annealing) can be used. GRTA performs heating processing using high-temperature gas. An inert gas is used as the gas.

[0341] The gas supply source 2801 may be connected to a refiner via a mass flow controller. It is preferable to use a gas with a dew point of -80° C. or less, preferably -100° C. or less. For example, oxygen gas, nitrogen gas, and rare gas (such as argon gas) may be used.

[0342] The dielectric plate 2809 may be made of, for example, silicon oxide (quartz), aluminum oxide (alumina), or yttrium oxide (yttria). A separate protective layer may be formed on the surface of the dielectric plate 2809. The protective layer may be made of magnesium oxide, titanium oxide, chromium oxide, zirconium oxide, hafnium oxide, tantalum oxide, silicon oxide, aluminum oxide, or yttrium oxide. The dielectric plate 2809 is exposed to a particularly high-density region of the high-density plasma 2810 described later, and thus damage to the dielectric plate 2809 can be mitigated by providing a protective layer. As a result, an increase in particles during processing can be suppressed.

[0343] The high frequency generator 2803 has a function of generating microwaves of, for example, 0.3 GHz to 3.0 GHz, 0.7 GHz to 1.1 GHz, or 2.2 GHz to 2.8 GHz. The microwaves generated by the high frequency generator 2803 are transmitted to the mode converter 2805 via the waveguide 2804. In the mode converter 2805, the microwaves transmitted as TE mode are converted to TEM mode. Then, the microwaves are transmitted to the slot antenna plate 2808 via the waveguide 2807. The slot antenna plate 2808 is provided with a plurality of slot holes, and the microwaves pass through the slot holes and the dielectric plate 2809. Then, an electric field is generated below the dielectric plate 2809, and a high density plasma 2810 can be generated. In the high density plasma 2810, ions and radicals according to the gas species supplied from the gas supply source 2801 exist. For example, oxygen radicals and the like exist.

[0344] At this time, the film on the substrate 2811 can be modified by the ions and radicals generated by the high density plasma 2810. It may be preferable to apply a bias to the substrate 2811 side using a high frequency power supply 2816. For the high frequency power supply 2816, an RF (Radio Frequency) power supply with a frequency of, for example, 13.56 MHz or 27.12 MHz may be used. By applying a bias to the substrate side, the ions in the high density plasma 2810 can be efficiently delivered to the depths of the openings of the film on the substrate 2811.

[0345] For example, oxygen can be introduced from a gas supply source 2801 into the chamber 2706b or the chamber 2706c to perform oxygen radical treatment using a high density plasma 2810.

[0346] Next, chamber 2706a and chamber 2706d will be described with reference to the schematic cross-sectional view shown in FIG.

[0347] The chamber 2706a and the chamber 2706d are chambers capable of irradiating the object to be treated with electromagnetic waves, for example. The only difference between the chamber 2706a and the chamber 2706d is the type of electromagnetic waves. As the other configurations are largely common, they will be described together below.

[0348] The chamber 2706a and the chamber 2706d each have one or more lamps 2820, a substrate holder 2825, a gas inlet 2823, and an exhaust port 2830. In addition, a gas supply source 2821, a valve 2822, a vacuum pump 2828, and a valve 2829 are provided outside the chamber 2706a and the chamber 2706d.

[0349] The gas supply source 2821 is connected to a gas inlet 2823 via a valve 2822. The vacuum pump 2828 is connected to an exhaust port 2830 via a valve 2829. The lamp 2820 is disposed facing a substrate holder 2825. The substrate holder 2825 has a function of holding a substrate 2824. The substrate holder 2825 also has an internal heating mechanism 2826 and has a function of heating the substrate 2824.

[0350] A light source having a function of emitting electromagnetic waves such as visible light or ultraviolet light may be used as the lamp 2820. For example, a light source having a function of emitting electromagnetic waves having a peak wavelength of 10 nm to 2500 nm, 500 nm to 2000 nm, or 40 nm to 340 nm may be used.

[0351] For example, lamp 2820 may be a light source such as a halogen lamp, a metal halide lamp, a xenon arc lamp, a carbon arc lamp, a high pressure sodium lamp, or a high pressure mercury lamp.

[0352] For example, the electromagnetic waves emitted from the lamps 2820 can be absorbed in part or in whole by the substrate 2824 to modify a film on the substrate 2824. For example, defects can be generated or reduced, or impurities can be removed. If the process is performed while the substrate 2824 is heated, defects can be generated or reduced, or impurities can be removed efficiently.

[0353] Alternatively, for example, the substrate holder 2825 may be heated by electromagnetic waves emitted from the lamps 2820, thereby heating the substrate 2824. In that case, the substrate holder 2825 does not need to have the heating mechanism 2826 inside.

[0354] For the vacuum pump 2828, refer to the description of the vacuum pump 2817. For the heating mechanism 2826, refer to the description of the heating mechanism 2813. For the gas supply source 2821, refer to the description of the gas supply source 2801.

[0355] By using the above manufacturing apparatus, it is possible to modify the film while suppressing the inclusion of impurities in the processed object.

[0356] <Modifications of the semiconductor device> An example of a semiconductor device which is one embodiment of the present invention will be described below with reference to FIGS. 16A to 16D.

[0357] Fig. 16A shows a top view of the semiconductor device. Fig. 16B is a cross-sectional view corresponding to the portion indicated by the dashed line A1-A2 in Fig. 16A. Fig. 16C is a cross-sectional view corresponding to the portion indicated by the dashed line A3-A4 in Fig. 16A. Fig. 16D is a cross-sectional view corresponding to the portion indicated by the dashed line A5-A6 in Fig. 16A. In the top view of Fig. 16A, some elements are omitted for clarity.

[0358] 16A to 16D, structures having the same functions as those of the structures constituting the semiconductor device shown in <Configuration example of semiconductor device> are denoted by the same reference numerals. Note that, in this section, the materials described in detail in <Configuration example of semiconductor device> can be used as the materials constituting the semiconductor device.

[0359] The semiconductor device shown in Figures 16A to 16D is a modified example of the semiconductor device shown in Figures 1A to 1D. The semiconductor device shown in Figures 16A to 16D differs from the semiconductor device shown in Figures 1A to 1D in that it has an oxide 230c and an oxide 230d. It also differs in that it has an insulator 271, an insulator 272, and an insulator 273.

[0360] In the semiconductor device shown in FIGS. 16A to 16D, the transistor 200a and the transistor 200b each have an oxide 230c on the oxide 230b and an oxide 230d on the oxide 230c. The oxide 230c and the oxide 230d are provided in openings formed in the insulator 280 and the insulator 275. The oxide 230c is in contact with the top surface of the insulator 224, the side of the oxide 230a, the top surface and side of the oxide 230b, the side of the oxide 243, the side of the conductor 242, the side of the insulator 271, the side of the insulator 273, the side of the insulator 275, and the side of the insulator 280. The top of the oxide 230c and the top of the oxide 230d are in contact with the insulator 282.

[0361] By disposing the oxide 230d on the oxide 230c, it is possible to suppress the diffusion of impurities from a structure formed above the oxide 230d to the oxide 230b or the oxide 230c. Also, by disposing the oxide 230d on the oxide 230c, it is possible to suppress the upward diffusion of oxygen from the oxide 230b or the oxide 230c.

[0362] In addition, in a cross-sectional view in the channel length direction of the transistor, a groove is preferably provided in the oxide 230b, and the oxide 230c is preferably embedded in the groove. In this case, the oxide 230c is disposed so as to cover the inner wall (side wall and bottom surface) of the groove. In addition, the thickness of the oxide 230c is preferably approximately the same as the depth of the groove. With this configuration, even if a damaged region is formed on the surface of the oxide 230b at the bottom of the opening when forming an opening for embedding the conductor 260 or the like, the damaged region can be removed. This makes it possible to suppress defects in the electrical characteristics of the transistor 200 caused by the damaged region.

[0363] Here, it is preferable that the atomic ratio of In to element M in the metal oxide used for oxide 230c is greater than the atomic ratio of In to element M in the metal oxide used for oxide 230a or oxide 230d.

[0364] In addition, when the oxide 230c is used as the main path of the carriers, the atomic ratio of indium to the main metal element in the oxide 230c is preferably greater than the atomic ratio of indium to the main metal element in the oxide 230b. In addition, the atomic ratio of In to the element M in the oxide 230c is preferably greater than the atomic ratio of In to the element M in the oxide 230b. By using a metal oxide with a high indium content in the channel formation region, the on-current of the transistor can be increased. Therefore, by making the atomic ratio of indium to the main metal element in the oxide 230c greater than the atomic ratio of indium to the main metal element in the oxide 230b, the oxide 230c can be used as the main path of the carriers. In addition, the conduction band minimum of the oxide 230c is preferably farther from the vacuum level than the conduction band minimums of the oxide 230a and the oxide 230b. In other words, it is preferable that the electron affinity of the oxide 230c is larger than those of the oxide 230a and the oxide 230b. At this time, the main path of carriers is the oxide 230c.

[0365] Specifically, the oxide 230c may be a metal oxide or indium oxide having a composition of In:M:Zn=4:2:3 (atomic ratio) or a composition close thereto, In:M:Zn=5:1:3 (atomic ratio) or a composition close thereto, or In:M:Zn=10:1:3 (atomic ratio) or a composition close thereto.

[0366] In addition, it is preferable to use a CAAC-OS as the oxide 230c, and it is preferable that the c-axis of the crystal of the oxide 230c is oriented in a direction approximately perpendicular to the surface on which the oxide 230c is formed or the upper surface of the oxide 230c. The CAAC-OS has a property of easily moving oxygen in a direction perpendicular to the c-axis. Therefore, oxygen in the oxide 230c can be efficiently supplied to the oxide 230b.

[0367] Moreover, the oxide 230d preferably contains at least one of the metal elements constituting the metal oxide used in the oxide 230c, and more preferably contains all of the metal elements. For example, the oxide 230c may be In-M-Zn oxide, In-Zn oxide, or indium oxide, and the oxide 230d may be In-M-Zn oxide, M-Zn oxide, or an oxide of element M. This can reduce the defect state density at the interface between the oxide 230c and the oxide 230d.

[0368] In addition, the conduction band minimum of the oxide 230d is preferably closer to the vacuum level than the conduction band minimum of the oxide 230c. In other words, the electron affinity of the oxide 230d is preferably smaller than that of the oxide 230c. In this case, the oxide 230d is preferably made of a metal oxide that can be used for the oxide 230a or the oxide 230b. In this case, the main carrier path is the oxide 230c.

[0369] Specifically, the oxide 230c may be a metal oxide having a composition of In:M:Zn=4:2:3 [atomic ratio] or a composition close thereto, In:M:Zn=5:1:3 [atomic ratio] or a composition close thereto, or In:M:Zn=10:1:3 [atomic ratio] or a composition close thereto, or an indium oxide. The oxide 230d may be a metal oxide having a composition of In:M:Zn=1:3:4 [atomic ratio] or a composition close thereto, M:Zn=2:1 [atomic ratio] or a composition close thereto, or M:Zn=2:5 [atomic ratio] or a composition close thereto, or an oxide of element M. The composition close thereto includes a range of ±30% of the desired atomic ratio. It is preferable to use gallium as the element M.

[0370] In addition, the oxide 230d is preferably a metal oxide that suppresses the diffusion or permeation of oxygen more than the oxide 230c. By providing the oxide 230d between the insulator 250 and the oxide 230c, oxygen can be efficiently supplied to the oxide 230b through the oxide 230c.

[0371] In addition, in the metal oxide used for the oxide 230d, the atomic ratio of In to the metal element that is the main component is made smaller than the atomic ratio of In to the metal element that is the main component in the metal oxide used for the oxide 230c, so that the diffusion of In to the insulator 250 side can be suppressed. For example, in the oxide 230d, the atomic ratio of In to the element M may be made smaller than the atomic ratio of In to the element M in the oxide 230c. Since the insulator 250 functions as a gate insulator, if In is mixed into the insulator 250, etc., the characteristics of the transistor will be defective. Therefore, by providing the oxide 230d between the oxide 230c and the insulator 250, it is possible to provide a highly reliable semiconductor device.

[0372] Note that the oxide 230c may be provided for each transistor 200. That is, the oxide 230c of one transistor 200 may not be in contact with the oxide 230c of another transistor 200 adjacent to the transistor 200 in the channel width direction. The oxide 230c of one transistor 200 may be separated from the oxide 230c of another transistor 200 adjacent to the transistor 200 in the channel width direction. In other words, the oxide 230c may not be disposed between the transistor 200 and the transistor 200 adjacent to the transistor 200 in the channel width direction.

[0373] In a semiconductor device in which a plurality of transistors 200 are arranged in the channel width direction, the above configuration allows the oxide 230c to be provided independently in each of the transistors 200. This makes it possible to prevent a parasitic transistor from being generated between a transistor 200 and a transistor 200 adjacent to the transistor 200 in the channel width direction, thereby preventing the above-mentioned leakage path from being generated. This makes it possible to provide a semiconductor device that has favorable electrical characteristics and can be miniaturized or highly integrated.

[0374] In addition, the semiconductor device shown in Figures 16A to 16D has an insulator 271 on the conductor 242, an insulator 273 on the insulator 271, and an insulator 272 in contact with the side of the oxide 230b, the side of the oxide 243, and the side of the conductor 242.

[0375] The insulator 271 preferably functions as at least a barrier insulating film against oxygen. Therefore, the insulator 271 preferably has a function of suppressing oxygen diffusion. For example, the insulator 271 preferably has a function of suppressing oxygen diffusion more than the insulator 280. As the insulator 271, for example, a nitride containing silicon, such as silicon nitride, may be used.

[0376] Like the insulator 224, the insulator 273 preferably has an excess oxygen region or excess oxygen. The insulator 273 also preferably has a reduced concentration of impurities such as water and hydrogen. For example, the insulator 273 may be an oxide containing silicon, such as silicon oxide or silicon oxynitride, as appropriate. By providing an insulator having excess oxygen in contact with the insulator 250, oxygen diffused to the oxide 230 through the insulator 250 can reduce oxygen vacancies in the oxide 230 and improve the reliability of the transistor 200.

[0377] The insulator 272 preferably functions as at least a barrier insulating film against oxygen. Therefore, the insulator 272 preferably has a function of suppressing oxygen diffusion. For example, the insulator 272 preferably has a function of suppressing oxygen diffusion more than the insulator 280. As the insulator 272, for example, a nitride containing silicon, such as silicon nitride, may be used.

[0378] By providing the insulators 271 and 272 as described above, the conductor 242 can be wrapped in an insulator having a barrier property against oxygen. In other words, it is possible to prevent oxygen added when the insulator 275 is formed or oxygen contained in the insulator 273 from diffusing into the conductor 242. This makes it possible to suppress a situation in which the conductor 242 is directly oxidized by oxygen added when the insulator 275 is formed or oxygen contained in the insulator 273, which would increase the resistivity and reduce the on-current.

[0379] 1B and other figures show a configuration in which the insulator 272 is in contact with the side surfaces of the oxide 230a, the oxide 230b, the oxide 243, the conductor 242, the insulator 271, and the insulator 273, but it is sufficient that the insulator 272 is in contact with at least the side surfaces of the insulator 271 and the conductor 242. For example, there may be a configuration in which the insulator 272 is in contact with the side surfaces of the oxide 230a, the oxide 230b, the oxide 243, the conductor 242, and the insulator 271, but is not in contact with the insulator 273. In this case, the side surface of the insulator 273 is in contact with the insulator 275.

[0380] According to one embodiment of the present invention, a semiconductor device that can be miniaturized or highly integrated can be provided. According to one embodiment of the present invention, a semiconductor device with large storage capacity can be provided. According to one embodiment of the present invention, a semiconductor device with little variation in transistor characteristics can be provided. According to one embodiment of the present invention, a semiconductor device with high reliability can be provided. According to one embodiment of the present invention, a semiconductor device with good electrical characteristics can be provided. According to one embodiment of the present invention, a semiconductor device with high on-state current can be provided. According to one embodiment of the present invention, a semiconductor device that can be miniaturized or highly integrated can be provided. According to one embodiment of the present invention, a semiconductor device with low power consumption can be provided. According to one embodiment of the present invention, a novel semiconductor device can be provided.

[0381] The structures and methods described in this embodiment can be used in appropriate combination with other structures and methods described in this embodiment or structures and methods described in other embodiments.

[0382] (Embodiment 2) In this embodiment mode, one mode of a semiconductor device that can be used as a memory device will be described with reference to FIGS.

[0383] [Storage device 1] 17A illustrates an example of a semiconductor device (memory device) according to one embodiment of the present invention. In the semiconductor device illustrated in FIG. 17A, a capacitor 100a is disposed over a transistor 200a, and a capacitor 100b is disposed over a transistor 200b. Note that hereinafter, the capacitors 100a and 100b may be collectively referred to as capacitors 100.

[0384] The transistors 200a and 200b described in the above embodiment can be used as the transistors 200a and 200b. That is, the semiconductor device illustrated in FIG 17A has a structure in which the capacitors 100a and 100b are provided over the semiconductor device illustrated in FIG 1. Note that the structures of the transistors 200a and 200b can be referred to in the description of the transistors 200a and 200b described in the above embodiment.

[0385] Here, one of the source and drain of the transistor 200a is electrically connected to the first electrode of the capacitor 100a, the other of the source and drain of the transistor 200a is electrically connected to one of the source and drain of the transistor 200b, and the other of the source and drain of the transistor 200b is electrically connected to the first electrode of the capacitor 100b. The transistor 200a and the capacitor 100a, and the transistor 200b and the capacitor 100b connected in this manner can each function as a memory cell of a storage device. Therefore, hereinafter, a semiconductor device having the transistor 200a, the transistor 200b, the capacitor 100a, and the capacitor 100b as shown in FIG. 17A may be referred to as a memory unit 400.

[0386] In the memory unit 400, by providing the conductor 248 under the oxide 230, the parasitic capacitance of the conductor 248 and the bit line provided in contact with the conductor 248 can be reduced. This reduces the capacitance required for the capacitor 100, and the capacitor 100 can be miniaturized. For example, the capacitor 100a may overlap the transistor 200a, and the capacitor 100b may overlap the transistor 200b. In this way, by miniaturizing the capacitor 100, the memory unit 400 can be miniaturized or highly integrated. Furthermore, by miniaturizing or highly integrating the memory unit 400, a semiconductor device with a large storage capacity can be provided.

[0387] Furthermore, in the memory unit 400, by providing the conductor 248 under the oxide 230, it is possible to prevent interference between the capacitive element 100a and the capacitive element 100b and the extraction plug of the memory unit 400. This allows the capacitance of the capacitive element 100a and the capacitive element 100b to be increased without increasing the area occupied by the memory unit 400.

[0388] The capacitor 100 is provided over an insulator 283. The capacitor 100 has a conductor 110 functioning as a first electrode, a conductor 120 functioning as a second electrode, and an insulator 130 functioning as a dielectric.

[0389] Conductor 110 and conductor 120 may be any conductor that can be used for conductor 205, etc. Note that, although a single-layer structure is shown for conductor 110 and conductor 120 in Fig. 17, the present invention is not limited to this configuration and may be a laminated structure of two or more layers. For example, a conductor having barrier properties and a conductor having high adhesion to the conductor having high conductivity may be formed between a conductor having barrier properties and a conductor having high conductivity.

[0390] The insulator 130 can be made of, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, aluminum oxide, aluminum oxynitride, aluminum nitride oxide, aluminum nitride, hafnium oxide, hafnium oxynitride, hafnium nitride oxide, hafnium nitride, or the like, and can be provided as a stacked layer or a single layer.

[0391] For example, it is preferable to use a laminated structure of a material with high dielectric strength, such as silicon oxynitride, and a high dielectric constant (high-k) material for the insulator 130. With this configuration, the capacitance element 100 can ensure sufficient capacitance by having an insulator with high dielectric constant (high-k), and the capacitance element 100 can have improved dielectric strength by having an insulator with high dielectric strength, thereby suppressing electrostatic breakdown of the capacitance element 100.

[0392] Examples of high dielectric constant (high-k) material insulators (materials with a high relative dielectric constant) include gallium oxide, hafnium oxide, zirconium oxide, oxides having aluminum and hafnium, oxynitrides having aluminum and hafnium, oxides having silicon and hafnium, oxynitrides having silicon and hafnium, and nitrides having silicon and hafnium.

[0393] On the other hand, materials with high dielectric strength (materials with low dielectric constant) include silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide with added fluorine, silicon oxide with added carbon, silicon oxide with added carbon and nitrogen, silicon oxide or resin with voids, etc.

[0394] In addition, a conductor 240 is provided that functions as a plug that electrically connects the transistor 200a and the capacitor 100a and a plug that electrically connects the transistor 200b and the capacitor 100b.

[0395] 17A, the conductor 240 provided between the transistor 200a and the capacitor 100a has a bottom surface in contact with the conductor 242a and a top surface in contact with the conductor 110 of the capacitor 100a. The conductor 240 provided between the transistor 200b and the capacitor 100b has a bottom surface in contact with the conductor 242c and a top surface in contact with the conductor 110 of the capacitor 100b. Furthermore, an insulator 241 is preferably provided in contact with a side surface of the conductor 240 functioning as a plug.

[0396] Insulator 241 is provided in contact with the inner walls of the openings of insulators 275, 280, 282, and 283, a first conductor of conductor 240 is provided in contact with the side surface of insulator 241, and a second conductor of conductor 240 is provided further inside. Note that, although Fig. 17 shows a configuration in which the first conductor of conductor 240 and the second conductor of conductor 240 are laminated, the present invention is not limited to this. For example, conductor 240 may be provided as a single layer or a laminated structure of three or more layers.

[0397] The conductor 240 is preferably made of a conductive material mainly composed of tungsten, copper, or aluminum. The conductor 240 may have a laminated structure. When the conductor 240 has a laminated structure, the conductor in contact with the insulator 283, the insulator 282, the insulator 280, and the insulator 275 is preferably made of a conductive material having a function of suppressing the permeation of impurities such as water and hydrogen. For example, tantalum, tantalum nitride, titanium, titanium nitride, ruthenium, ruthenium oxide, etc. are preferably used. The conductive material having a function of suppressing the permeation of impurities such as water and hydrogen may be used in a single layer or a laminated layer. This makes it possible to suppress impurities such as water and hydrogen contained in layers above the insulator 283 from being mixed into the oxide 230 through the conductor 240.

[0398] As the insulator 241, for example, an insulator such as silicon nitride, aluminum oxide, or silicon nitride oxide may be used. Since the insulator 241 is provided in contact with the insulator 283, the insulator 282, and the insulator 275, it is possible to prevent impurities such as water and hydrogen contained in the insulator 280 from being mixed into the oxide 230 through the conductor 240. In particular, silicon nitride is preferable because it has high barrier properties against hydrogen. In addition, it is possible to prevent oxygen contained in the insulator 280 from being absorbed by the conductor 240.

[0399] Furthermore, as shown in FIG. 17B, a memory unit 400 and a memory unit 401 having a similar configuration to the memory unit 400 may be arranged in the channel length direction.

[0400] 17B, ​​an insulator 210 is provided under an insulator 212, and a conductor 288 is provided under the insulator 210. An upper surface of the conductor 288 contacts a lower surface of the conductor 248 of the memory unit 400 and the memory unit 401. Here, the insulator 212 may be made of an insulator that can be used for the insulator 280. The conductor 288 may be made of a conductor that can be used for the conductor 205.

[0401] The conductor 288 functions as a wiring. That is, the memory unit 400 and the memory unit 401 are electrically connected to the conductor 288, which functions as a wiring, via the conductor 248.

[0402] Here, the conductor 288 functioning as the bit line and the conductor 260 functioning as the word line are preferably arranged perpendicular to each other. The transistor 200 and the capacitor 100 are formed in the region where the conductor 288 and the conductor 260 intersect, and memory cells each including the transistor 200 and the capacitor 100 are arranged in a matrix.

[0403] In this way, a cell array (also called a memory unit layer) can be configured by arranging memory units in a matrix on the same layer. By configuring the cell array in this way, the distance between adjacent cells can be reduced, so the projection area of ​​the cell array can be reduced, enabling high integration.

[0404] [Storage device 2] Next, an example of a semiconductor device (memory device) according to one embodiment of the present invention is shown in FIG. In the semiconductor device of one embodiment of the present invention, the memory unit 400 shown in FIG. 17A is provided above the transistor 300. That is, the transistors 200a and 200b are provided above the transistor 300, and the capacitors 100a and 100b are provided above the transistors 200a and 200b. Note that the capacitor 100 and the transistor 200 described above can be used as the capacitor 100 and the transistor 200, and the detailed structures thereof can be referred to.

[0405] The transistor 200 is a transistor in which a channel is formed in a semiconductor layer including an oxide semiconductor. Since the off-state current of the transistor 200 is small, stored data can be retained for a long time by using the transistor 200 in a memory device. In other words, a refresh operation is not required or the frequency of the refresh operation is extremely low, so that the power consumption of the memory device can be sufficiently reduced.

[0406] As described in the previous embodiment, a metal oxide such as In-M-Zn oxide can be formed on a substrate by sputtering or the like. Therefore, a memory unit 400 formed of a transistor 200 and a capacitor element 100 can be provided on a driving circuit formed of a transistor 300 or the like formed on a silicon substrate. This reduces the area occupied by the peripheral circuits provided on one chip and increases the area occupied by the memory cell array, thereby increasing the storage capacity of the semiconductor device.

[0407] Moreover, the memory device shown in FIG. 18 can be arranged in a matrix to form a memory cell array.

[0408] <Transistor 300> The transistor 300 is provided on a substrate 311 and includes a conductor 316 functioning as a gate, an insulator 315 functioning as a gate insulator, a semiconductor region 313 formed of a part of the substrate 311, and a low-resistance region 314a and a low-resistance region 314b functioning as a source region or a drain region. The transistor 300 may be either a p-channel type or an n-channel type.

[0409] Here, in the transistor 300 shown in FIG. 18, a semiconductor region 313 (a part of a substrate 311) in which a channel is formed has a convex shape. A conductor 316 is provided so as to cover the side and top surface of the semiconductor region 313 via an insulator 315. Note that the conductor 316 may be made of a material that adjusts the work function. Such a transistor 300 is also called a FIN type transistor because it uses a convex portion of a semiconductor substrate. Note that an insulator that contacts the upper portion of the convex portion and functions as a mask for forming the convex portion may be provided. Note that, although a case where a convex portion is formed by processing a part of a semiconductor substrate has been shown here, a semiconductor film having a convex shape may be formed by processing an SOI substrate.

[0410] Note that the transistor 300 illustrated in FIG. 18 is just an example, and the present invention is not limited to this structure. An appropriate transistor may be used depending on the circuit configuration and driving method.

[0411] <Wiring layer> Between each structure, a wiring layer having an interlayer film, wiring, plugs, etc. may be provided. Also, a plurality of wiring layers may be provided according to the design. Here, a conductor having a function as a plug or wiring may be collectively given the same symbol as a plurality of structures. Also, in this specification, the wiring and the plug electrically connected to the wiring may be integrated. That is, there are cases where a part of the conductor functions as the wiring, and cases where a part of the conductor functions as the plug.

[0412] For example, an insulator 320, an insulator 322, an insulator 324, and an insulator 326 are stacked in this order as an interlayer film over the transistor 300. A conductor 328, a conductor 330, and the like that are electrically connected to the capacitor 100 or the transistor 200 are embedded in the insulator 320, the insulator 322, the insulator 324, and the insulator 326. The conductor 328 and the conductor 330 function as plugs or wirings.

[0413] The insulator functioning as an interlayer film may also function as a planarizing film that covers the uneven shape underneath. For example, the top surface of the insulator 322 may be planarized by a planarization process using a chemical mechanical polishing (CMP) method or the like to enhance flatness.

[0414] A wiring layer may be provided on the insulator 326 and the conductor 330. For example, in Fig. 18, an insulator 350, an insulator 352, and an insulator 354 are stacked in this order. A conductor 356 is formed in the insulator 350, the insulator 352, and the insulator 354. The conductor 356 functions as a plug or a wiring.

[0415] An insulator 358 is provided over the insulator 354 and the conductor 356, and a conductor 288 functioning as wiring is provided over the insulator 358. Furthermore, an insulator 210 is provided over the conductor 288. The insulators 212, 214, 216, 222, 224, 280, 282, and 283 shown in the above embodiments are provided over the insulator 210, and the transistors 200a and 200b are formed in these insulators.

[0416] Conductor 248 and insulator 249 are embedded in insulator 210, insulator 212, insulator 214, insulator 216, insulator 222, and insulator 224. Here, conductor 248 is provided in contact with conductor 288 on the upper surface.

[0417] As described above, the conductor 240 functioning as a plug is provided in contact with the top surface of the conductor 242. An insulator 241 is provided in contact with the side surface of the conductor 240 functioning as a plug. A conductor 110 is provided in contact with the conductor 240 on the insulator 283 and on the conductor 240. An insulator 274 is provided on the insulator 283 in a region not overlapping with the insulator 280.

[0418] The above-described capacitor 100a and capacitor 100b are formed on the insulator 283. Furthermore, on the conductor 120 and the insulator 130 which form the capacitor 100, an insulator 150 is provided.

[0419] Examples of insulators that can be used as the interlayer film include insulating oxides, nitrides, oxynitrides, nitride oxides, metal oxides, metal oxynitrides, and metal nitride oxides.

[0420] For example, by using a material with a low dielectric constant for the insulator that functions as an interlayer film, the parasitic capacitance generated between wirings can be reduced. Therefore, it is advisable to select a material according to the function of the insulator.

[0421] For example, the insulator 150, the insulator 274, the insulator 210, the insulator 358, the insulator 352, the insulator 354, and the like preferably have an insulator with a low relative dielectric constant. For example, the insulator preferably has silicon oxynitride, silicon nitride, silicon oxide to which fluorine has been added, silicon oxide to which carbon has been added, silicon oxide to which carbon and nitrogen have been added, silicon oxide having voids, or resin. Alternatively, the insulator preferably has a laminated structure of silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide to which fluorine has been added, silicon oxide to which carbon has been added, silicon oxide to which carbon and nitrogen has been added, or silicon oxide having voids, and resin. Silicon oxide and silicon oxynitride are thermally stable, and therefore can be combined with a resin to form a laminated structure that is thermally stable and has a low relative dielectric constant. Examples of the resin include polyester, polyolefin, polyamide (nylon, aramid, and the like), polyimide, polycarbonate, and acrylic.

[0422] Furthermore, when a transistor using an oxide semiconductor is surrounded by an insulator that has a function of suppressing the permeation of impurities such as hydrogen and oxygen, the electrical characteristics of the transistor can be stabilized. Therefore, the insulators 283, 282, 214, 212, and 350 can be made of insulators that have a function of suppressing the permeation of impurities such as hydrogen and oxygen.

[0423] As an insulator having a function of suppressing the permeation of impurities such as hydrogen and oxygen, for example, an insulator containing boron, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zirconium, lanthanum, neodymium, hafnium, or tantalum may be used in a single layer or a stacked layer. Specifically, as an insulator having a function of suppressing the permeation of impurities such as hydrogen and oxygen, metal oxides such as aluminum oxide, magnesium oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide, or tantalum oxide, silicon nitride oxide, or silicon nitride may be used.

[0424] Conductors that can be used for wiring and plugs include materials containing one or more metal elements selected from aluminum, chromium, copper, silver, gold, platinum, tantalum, nickel, titanium, molybdenum, tungsten, hafnium, vanadium, niobium, manganese, magnesium, zirconium, beryllium, indium, ruthenium, etc. Also, semiconductors with high electrical conductivity, typified by polycrystalline silicon containing impurity elements such as phosphorus, and silicides such as nickel silicide may be used.

[0425] For example, the conductor 328, the conductor 330, the conductor 356, the conductor 288, the conductor 110, and the conductor 120 can be formed of a single layer or a stack of conductive materials such as metal materials, alloy materials, metal nitride materials, or metal oxide materials formed from the above materials. It is preferable to use a high melting point material such as tungsten or molybdenum that has both heat resistance and conductivity, and it is preferable to use tungsten. Alternatively, it is preferable to form the conductor from a low resistance conductive material such as aluminum or copper. By using a low resistance conductive material, the wiring resistance can be reduced.

[0426] <Wiring or plug of layer provided with oxide semiconductor> Note that when an oxide semiconductor is used for the transistor 200, an insulator having an excess oxygen region may be provided near the oxide semiconductor. In that case, an insulator having a barrier property is preferably provided between the insulator having the excess oxygen region and a conductor provided in the insulator having the excess oxygen region.

[0427] 18, for example, an insulator 241 may be provided between the insulator 280 having excess oxygen and the conductor 240. By providing the insulator 241 in contact with the insulator 275, the insulator 282, and the insulator 283, the insulator 224 and the transistor 200 can be sealed with an insulator having a barrier property.

[0428] In other words, the insulator 241 can prevent excess oxygen in the insulator 280 from being absorbed by the conductor 240. Furthermore, the insulator 241 can prevent hydrogen, which is an impurity, from diffusing into the transistor 200 through the conductor 240.

[0429] As the insulator 241, an insulating material having a function of suppressing the diffusion of impurities such as water or hydrogen, and oxygen, may be used. For example, it is preferable to use silicon nitride, silicon nitride oxide, aluminum oxide, or hafnium oxide. In particular, silicon nitride is preferable because it has high barrier properties against hydrogen. In addition, other metal oxides such as magnesium oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, or tantalum oxide may be used.

[0430] 18, the insulator 280 may be patterned, and the insulator 212 may be in contact with the insulator 283. That is, the transistor 200 may be sealed with the insulators 212, 214, 282, and 283. With such a configuration, it is possible to reduce the intrusion of hydrogen contained in the insulators 274, 150, and the like into the insulator 280 and the like.

[0431] Here, the conductor 240 penetrates the insulator 283 and the insulator 282, and as described above, the insulator 241 is provided in contact with the conductor 240. This makes it possible to reduce hydrogen that is mixed into the inside of the insulators 212, 214, 282, and 283 through the conductor 240. In this way, the transistor 200 is sealed with the insulators 212, 214, 282, 283, and 241, making it possible to reduce the mixing of impurities such as hydrogen contained in the insulator 274, etc. from the outside.

[0432] <Dicing line> In the following, a dicing line (sometimes called a scribe line, a dividing line, or a cutting line) that is provided when a large-area substrate is divided into individual semiconductor elements to extract multiple semiconductor devices in chip form will be described. As a dividing method, for example, first, grooves (dicing lines) for dividing the semiconductor elements are formed in the substrate, and then the substrate is cut along the dicing lines to divide (split) the substrate into multiple semiconductor devices.

[0433] 18, for example, it is preferable to design the area where the insulator 283 and the insulator 212 contact each other so as to overlap the dicing line. That is, in the vicinity of the area that becomes the dicing line provided on the outer edge of the multiple memory units 400, openings are provided in the insulators 282, 280, 275, 224, 222, 216, and 214.

[0434] That is, the insulator 212 and the insulator 283 are in contact with each other at the openings provided in the insulators 282, 280, 275, 224, 222, 216, and 214. For example, the insulators 212 and 283 may be formed using the same material and the same method. By providing the insulators 212 and 283 using the same material and the same method, adhesion can be improved. For example, it is preferable to use silicon nitride.

[0435] With this structure, the transistor 200 can be surrounded by the insulator 212, the insulator 214, the insulator 282, and the insulator 283. At least one of the insulator 212, the insulator 214, the insulator 282, and the insulator 283 has a function of suppressing diffusion of oxygen, hydrogen, and water, and therefore, even if the substrate is divided into a plurality of chips by dividing the substrate into each circuit region in which the semiconductor element described in this embodiment is formed, impurities such as hydrogen or water can be prevented from entering from the side direction of the divided substrate and diffusing into the transistor 200.

[0436] This structure can prevent excess oxygen in the insulator 280 and the insulator 224 from diffusing to the outside. Therefore, the excess oxygen in the insulator 280 and the insulator 224 is efficiently supplied to the oxide in which a channel is formed in the transistor 200. The oxygen can reduce oxygen vacancies in the oxide in which a channel is formed in the transistor 200. As a result, the oxide in which a channel is formed in the transistor 200 can be an oxide semiconductor with low density of defect states and stable characteristics. That is, fluctuations in the electrical characteristics of the transistor 200 can be suppressed and reliability can be improved.

[0437] In the memory device shown in Fig. 17 and Fig. 18, the shape of the capacitor element 100a and the capacitor element 100b is a planar type, but the memory device shown in this embodiment is not limited to this. For example, as shown in Fig. 19, the shape of the capacitor element 100a and the capacitor element 100b may be a cylindrical type. In the memory device shown in Fig. 19, the configuration below the insulator 150 is the same as that of the semiconductor device shown in Fig. 18.

[0438] The capacitance element 100a and the capacitance element 100b shown in FIG. 19 each include an insulator 150 on the insulator 130, an insulator 142 on the insulator 150, a conductor 115 arranged in an opening formed in the insulator 150 and the insulator 142, an insulator 145 on the conductor 115 and the insulator 142, a conductor 125 on the insulator 145, and an insulator 152 on the conductor 125 and the insulator 145. Here, at least a part of the conductor 115, the insulator 145, and the conductor 125 are arranged in two openings formed in the insulator 150 and the insulator 142. Also, an insulator 154 is arranged on the insulator 152, and a conductor 153 and an insulator 156 are arranged on the insulator 154. Also, a conductor 140 is provided in an opening formed in the insulator 152 and the insulator 154.

[0439] The conductor 115 functions as the lower electrode of the capacitance element 100, the conductor 125 functions as the upper electrode of the capacitance element 100, and the insulator 145 functions as the dielectric of the capacitance element 100. The capacitance element 100 has a configuration in which the upper electrode and the lower electrode face each other across the dielectric not only on the bottom surface but also on the side surface in the openings of the insulators 150 and 142, and the capacitance per unit area can be increased. Therefore, the deeper the opening is, the larger the capacitance of the capacitance element 100 can be. Increasing the capacitance per unit area of ​​the capacitance element 100 in this way can promote miniaturization or high integration of semiconductor devices.

[0440] The insulator 152 may be made of an insulator that can be used for the insulator 280. The insulator 142 preferably functions as an etching stopper when forming an opening in the insulator 150, and may be made of an insulator that can be used for the insulator 214.

[0441] The shape of the openings formed in the insulator 150 and the insulator 142 when viewed from above may be a rectangle, a polygon other than a rectangle, a polygon with curved corners, or a circle including an ellipse. Here, it is preferable that the area of ​​the opening overlapping with the transistor 200 is large when viewed from above. With such a configuration, the occupation area of ​​a semiconductor device including the capacitor 100 and the transistor 200 can be reduced.

[0442] The conductor 115 is disposed in contact with the insulator 142 and an opening formed in the insulator 150. The upper surface of the conductor 115 preferably approximately coincides with the upper surface of the insulator 142. The lower surface of the conductor 115 is in contact with the conductor 110 through the opening of the insulator 130. The conductor 115 is preferably formed by an ALD method, a CVD method, or the like, and may be, for example, a conductor that can be used for the conductor 205.

[0443] The insulator 145 is disposed so as to cover the conductor 115 and the insulator 142. For example, the insulator 145 is preferably formed by an ALD method, a CVD method, or the like. The insulator 145 may be formed using, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, zirconium oxide, aluminum oxide, aluminum oxynitride, aluminum nitride oxide, aluminum nitride, hafnium oxide, hafnium oxynitride, hafnium nitride oxide, hafnium nitride, or the like, and can be provided as a stacked layer or a single layer. For example, the insulator 145 can be an insulating film stacked in this order of zirconium oxide, aluminum oxide, and zirconium oxide.

[0444] Moreover, it is preferable to use a material with high dielectric strength, such as silicon oxynitride, or a high dielectric constant (high-k) material for the insulator 145. Alternatively, a laminated structure of a material with high dielectric strength and a material with high dielectric constant (high-k) may be used.

[0445] Examples of insulators made of high dielectric constant (high-k) materials (materials with high relative dielectric constant) include gallium oxide, hafnium oxide, zirconium oxide, oxides having aluminum and hafnium, oxynitrides having aluminum and hafnium, oxides having silicon and hafnium, oxynitrides having silicon and hafnium, and nitrides having silicon and hafnium. By using such high-k materials, the capacitance of the capacitance element 100 can be sufficiently secured even if the insulator 145 is made thick. By making the insulator 145 thick, the leakage current occurring between the conductor 115 and the conductor 125 can be suppressed.

[0446] On the other hand, materials with high dielectric strength include silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, silicon oxide with added fluorine, silicon oxide with added carbon, silicon oxide with added carbon and nitrogen, silicon oxide with vacancies, and resin. For example, silicon nitride (SiN x ), silicon oxide (SiO x), and silicon nitride (SiN x ) in that order can be used. By using such an insulator having a high dielectric strength, the dielectric strength is improved, and electrostatic breakdown of the capacitor 100 can be suppressed.

[0447] The conductor 125 is arranged to fill the openings formed in the insulator 142 and the insulator 150. The conductor 125 is also electrically connected to the conductor 153 functioning as a wiring via the conductor 140. The conductor 125 is preferably formed by an ALD method, a CVD method, or the like, and may be a conductor that can be used for the conductor 205, for example.

[0448] The conductor 153 is provided over the insulator 154 and is covered with the insulator 156. The conductor 153 may be any of the conductors that can be used for the conductor 110, and the insulator 156 may be any of the insulators that can be used for the insulator 152. Here, the conductor 153 is in contact with the top surface of the conductor 140.

[0449] [Storage device 3] An example of a semiconductor device (memory device) according to one embodiment of the present invention is illustrated in FIGS.

[0450] The memory unit 400 shown in FIG. 20A differs from the memory unit 400 shown in FIG. 17A in the shapes of the capacitive elements 100a and 100b.

[0451] The capacitance element 100a has a conductor 242a, an insulator 275 provided to cover the conductor 242a, and a conductor 294a on the insulator 275. The capacitance element 100b has a conductor 242c, an insulator 275 provided to cover the conductor 242c, and a conductor 294b on the insulator 275. That is, the capacitance elements 100a and 100b configure a MIM (Metal-Insulator-Metal) capacitance.

[0452] Here, one of a pair of electrodes included in the capacitor 100, that is, the conductor 242, can also serve as a source electrode or a drain electrode of the transistor 200. A dielectric layer included in the capacitor 100 can also serve as a protective layer provided in the transistor 200, that is, the insulator 275. Thus, part of a manufacturing process of the transistor can be used in a manufacturing process of the capacitor 100, and thus a semiconductor device with high productivity can be obtained. Furthermore, one of a pair of electrodes included in the capacitor 100, that is, the conductor 242, also serves as a source electrode or a drain electrode of the transistor 200, and thus an area in which the transistor 200 and the capacitor 100 are arranged can be reduced.

[0453] The conductor 294a and the conductor 294b may be made of a material that can be used for the conductor 242, for example.

[0454] Also, for example, as shown in FIG 20B, a memory unit 400 and a memory unit 401 having a similar configuration to the memory unit 400 may be connected via a capacitance part. Here, the memory unit 400 and the memory unit 401 shown in FIG 20B have the same structure as the memory unit 400 shown in FIG 20A. Therefore, for details of the structure of the memory unit 400 and the memory unit 401 shown in FIG 20B, the description of the memory unit 400 shown in FIG 20A can be referred to.

[0455] FIG. 20B is a cross-sectional view in which a memory unit 400 including a transistor 200a, a transistor 200b, a capacitor 100a, and a capacitor 100b is connected to a memory unit 401 having a similar configuration to the memory unit 400 via a capacitance portion.

[0456] As shown in Fig. 20B, the conductor 294b functioning as one electrode of the capacitance element 100b of the memory unit 400 is configured to also serve as one electrode of a capacitance device of a memory unit 401 having a similar configuration to the memory unit 400. Although not shown, the conductor 294a functioning as one electrode of the capacitance element 100a of the memory unit 400 also serves as one electrode of a capacitance device of a semiconductor device adjacent to the left side of the memory unit 400, that is, in the A1 direction in Fig. 20B. The same configuration is also applied to the right side of the memory unit 401, that is, the cell in the A2 direction in Fig. 20B.

[0457] In this way, a cell array can be configured by arranging memory units in a matrix on the same layer. This type of cell array configuration allows the spacing between adjacent cells to be reduced, which in turn reduces the projection area of ​​the cell array and enables high integration.

[0458] 17B, ​​the semiconductor device shown in FIG. 20B also has an insulator 210 provided below the insulator 212, and a conductor 288 provided below the insulator 210. The upper surface of the conductor 288 contacts the lower surfaces of the conductors 248 of the memory units 400 and 401. Thus, the memory units 400 and 401 are electrically connected to the conductors 288 functioning as wiring via the conductors 248. The conductors 288 functioning as bit lines and the conductors 260 functioning as word lines are preferably arranged orthogonal to each other.

[0459] Also, the cell array having the memory unit 400 having the structure shown in FIG. 20A and FIG. 20B may be stacked instead of being formed in one layer. FIG. 21 shows a cross-sectional view of a structure in which n layers of cell arrays 610 having memory units 400 are stacked. As shown in FIG. 21, by stacking a plurality of cell arrays (cell arrays 610_1 to 610_n), cells can be integrated and arranged without increasing the occupied area of ​​the cell arrays. That is, a 3D cell array can be configured. Also, since the capacitive element 100 having the structure shown in FIG. 20A and FIG. 20B can be formed at a position lower than the upper surface of the conductor 260, the height of each cell array can be lowered compared to the case where a capacitive element having a cylinder structure is used. This allows a plurality of cell arrays to be stacked relatively easily. In this way, a semiconductor device having a large memory capacity can be provided by achieving high integration of memory cells.

[0460] [Storage device 4] An example of a semiconductor device (memory device) according to one embodiment of the present invention is illustrated in FIG.

[0461] 22 illustrates an example of a memory 470 including a transistor layer 413 including a transistor 200T and four memory unit layers 415 (memory unit layers 415_1 to 415_4). Note that the transistor 200T has a structure similar to that of the transistor 200 described in the above embodiment.

[0462] Each of the memory unit layers 415_1 to 415_4 includes a plurality of memory units 400. The memory units 400 included in the memory unit layers 415_1 to 415_4 have the same structure as the memory unit 400 shown in Fig. 20A. Therefore, the details of the memory unit 400 can be referred to the description of Fig. 20A.

[0463] Here, the conductor 248_1 provided in the memory unit layer 415_1 is electrically connected to the transistor 200T, the conductor 248_2 provided in the memory unit layer 415_2 is connected to the conductor 242b provided in the memory unit layer 415_1, the conductor 248_3 provided in the memory unit layer 415_3 is connected to the conductor 242b provided in the memory unit layer 415_2, and the conductor 248_4 provided in the memory unit layer 415_4 is connected to the conductor 242b provided in the memory unit layer 415_3. Note that in FIG. 22, the conductor 248_1 is connected to the gate electrode of the transistor 200T, but the present invention is not limited to this, and the connection of the conductor 248_1 may be appropriately set according to the circuit configuration of the memory 470, etc.

[0464] As described in the previous embodiment, the region 232b of the oxide 230b overlaps with the conductor 242b, and thus has a high carrier concentration and electrical conductivity. Therefore, with the above structure, the region 232b of the memory unit 400 provided in each memory unit layer 415 can be electrically connected to the transistor 200T through the conductor 248.

[0465] In this way, since a plurality of memory unit layers can be stacked, memory cells can be integrated and arranged without increasing the occupied area of ​​the cell array, thereby achieving high integration of memory cells and providing a semiconductor device with a large storage capacity.

[0466] The memory 470 is sealed by the insulator 212, the insulator 214, the insulator 282, and the insulator 283 (hereinafter, for convenience, this is referred to as a sealing structure). The insulator 274 is provided around the insulator 283. Furthermore, the conductor 440 is provided on the insulator 274, the insulator 283, and the insulator 212, and is electrically connected to the element layer 411.

[0467] Further, an insulator 280 is provided inside the sealing structure. The insulator 280 has a function of releasing oxygen when heated. Alternatively, the insulator 280 has an excess oxygen region.

[0468] Note that the insulators 212 and 283 are preferably made of a material having a high barrier property against hydrogen. The insulators 214 and 282 are preferably made of a material having a function of capturing hydrogen or fixing hydrogen.

[0469] For example, the material having a high barrier property against hydrogen includes silicon nitride, silicon nitride oxide, etc. Furthermore, the material having a function of capturing or fixing hydrogen includes aluminum oxide, hafnium oxide, and oxide containing aluminum and hafnium (hafnium aluminate), etc.

[0470] Note that the crystal structure of the materials used for the insulators 212, 214, 282, and 283 is not particularly limited, and may be an amorphous or crystalline structure. For example, an amorphous aluminum oxide film is preferably used as a material having a function of trapping or fixing hydrogen. Amorphous aluminum oxide may trap and fix a larger amount of hydrogen than aluminum oxide with high crystallinity.

[0471] The insulator 282 and the insulator 214 are preferably provided between the transistor layer 413 and the memory unit layer 415 or between each memory unit layer 415. The insulator 296 is preferably provided between the insulator 282 and the insulator 214. The insulator 296 can be made of a material similar to that of the insulator 283. Alternatively, silicon oxide or silicon oxynitride can be used. Alternatively, a known insulating material can be used.

[0472] Here, the following model can be considered for the diffusion of excess oxygen in the insulator 280 and hydrogen in the oxide semiconductor in contact with the insulator 280.

[0473] Hydrogen present in the oxide semiconductor diffuses to other structures through the insulator 280 in contact with the oxide semiconductor. Due to the diffusion of hydrogen, excess oxygen in the insulator 280 reacts with hydrogen in the oxide semiconductor to form OH bonds, and diffuses through the insulator 280. When the hydrogen atom having the OH bond reaches a material (typically the insulator 282) having a function of capturing or fixing hydrogen, the hydrogen atom reacts with an oxygen atom bonded to an atom (e.g., a metal atom, etc.) in the insulator 282, and is captured or fixed in the insulator 282. On the other hand, it is presumed that the oxygen atom of the excess oxygen having the OH bond remains in the insulator 280 as excess oxygen. In other words, there is a high probability that the excess oxygen in the insulator 280 plays a bridging role in the diffusion of hydrogen.

[0474] In order to satisfy the above model, the manufacturing process of the semiconductor device is one of the important factors.

[0475] As an example, the insulator 280 containing excess oxygen is formed in an oxide semiconductor, and then the insulator 282 is formed. After that, heat treatment is preferably performed. Specifically, the heat treatment is performed in an atmosphere containing oxygen, an atmosphere containing nitrogen, or an atmosphere containing a mixture of oxygen and nitrogen at a temperature of 350° C. or higher, preferably 400° C. or higher. The heat treatment time is 1 hour or longer, preferably 4 hours or longer, and more preferably 8 hours or longer.

[0476] By the above heat treatment, hydrogen in the oxide semiconductor can diffuse outward through the insulator 280 and the insulator 282. That is, the absolute amount of hydrogen present in the oxide semiconductor and in the vicinity of the oxide semiconductor can be reduced.

[0477] After the heat treatment, the insulator 283 is formed. The insulator 283 is a material having a high barrier property against hydrogen, and therefore can prevent hydrogen diffused to the outside or hydrogen present on the outside from entering the inside, specifically, the oxide semiconductor or the insulator 280 side.

[0478] Note that the above heat treatment is performed after the insulator 282 is formed, but is not limited thereto. For example, the heat treatment may be performed after the transistor layer 413 is formed or after the memory unit layers 415_1 to 415_3 are formed. When hydrogen is diffused outward by the heat treatment, hydrogen is diffused upward or laterally of the transistor layer 413. Similarly, when the heat treatment is performed after the memory unit layers 415_1 to 415_3 are formed, hydrogen is diffused upward or laterally.

[0479] By using the above manufacturing process, the insulator 212 and the insulator 283 are bonded to each other, and the above-described sealing structure is formed.

[0480] As described above, by using the above structure and manufacturing process, a semiconductor device including an oxide semiconductor in which the hydrogen concentration is reduced can be provided. Therefore, a semiconductor device with high reliability can be provided. According to one embodiment of the present invention, a semiconductor device with good electrical characteristics can be provided.

[0481] The structure, the method, and the like described in this embodiment can be used in appropriate combination with the structure, the method, and the like described in other embodiments.

[0482] (Embodiment 3) 23A, 23B, and 24A to 24C will be used to describe a transistor using an oxide as a semiconductor (hereinafter may be referred to as an OS transistor) and a memory device including a capacitor (hereinafter may be referred to as an OS memory device) according to one embodiment of the present invention. The OS memory device is a memory device including at least a capacitor and an OS transistor that controls charging and discharging of the capacitor. Since the off-state current of the OS transistor is extremely small, the OS memory device has excellent retention characteristics and can function as a nonvolatile memory.

[0483] <Storage device configuration example> 23A shows an example of the configuration of an OS memory device. The memory device 1400 includes a peripheral circuit 1411 and a memory cell array 1470. The peripheral circuit 1411 includes a row circuit 1420, a column circuit 1430, an output circuit 1440, and a control logic circuit 1460.

[0484] The column circuit 1430 includes, for example, a column decoder, a precharge circuit, a sense amplifier, a write circuit, and the like. The precharge circuit has a function of precharging the wiring. The sense amplifier has a function of amplifying a data signal read from a memory cell. Note that the above wiring is a wiring connected to a memory cell included in the memory cell array 1470, and will be described in detail later. The amplified data signal is output to the outside of the memory device 1400 as a data signal RDATA via the output circuit 1440. The row circuit 1420 includes, for example, a row decoder, a word line driver circuit, and the like, and can select a row to be accessed.

[0485] A low power supply voltage (VSS), a high power supply voltage (VDD) for the peripheral circuit 1411, and a high power supply voltage (VIL) for the memory cell array 1470 are supplied to the memory device 1400 from the outside as power supply voltages. In addition, control signals (CE, WE, RE), an address signal ADDR, and a data signal WDATA are input from the outside to the memory device 1400. The address signal ADDR is input to a row decoder and a column decoder, and the data signal WDATA is input to a write circuit.

[0486] The control logic circuit 1460 processes control signals (CE, WE, RE) input from the outside to generate control signals for the row decoder and column decoder. The control signal CE is a chip enable signal, the control signal WE is a write enable signal, and the control signal RE is a read enable signal. The signals processed by the control logic circuit 1460 are not limited to these, and other control signals may be input as necessary.

[0487] The memory cell array 1470 has a plurality of memory cells MCa and memory cells MCb arranged in a matrix, and a plurality of wirings. In the memory device shown in this embodiment, as shown in FIG. 23A, a memory cell MCa and a memory cell MCb are paired to form one memory unit. In the following, the memory cells MCa and the memory cells MCb may be collectively referred to as memory cells MC. The number of wirings connecting the memory cell array 1470 and the row circuit 1420 is determined by the configuration of the memory cells MC, the number of memory cells MC in one column, and the like. The number of wirings connecting the memory cell array 1470 and the column circuit 1430 is determined by the configuration of the memory cells MC, the number of memory cells MC in one row, and the like.

[0488] 23A shows an example in which the peripheral circuit 1411 and the memory cell array 1470 are formed on the same plane, but the present embodiment is not limited to this. For example, as shown in FIG. 23B, the memory cell array 1470 may be provided so as to overlap a part of the peripheral circuit 1411. For example, a sense amplifier may be provided so as to overlap the memory cell array 1470 below.

[0489] As described in the previous embodiment, a metal oxide such as In-M-Zn oxide can be formed on a substrate by sputtering or the like. Therefore, the memory cell array 1470 can be provided on the peripheral circuit 1411 formed on a silicon substrate. This increases the area occupied by the memory cell array that can be provided on one chip, thereby increasing the storage capacity of the semiconductor device.

[0490] Moreover, a configuration in which a plurality of memory cell arrays 1470 are stacked may be used. By stacking a plurality of memory cell arrays 1470, memory cells can be integrated and arranged without increasing the area occupied by the memory cell array 1470. In other words, a 3D cell array can be configured. In this way, a semiconductor device with a large memory capacity can be provided by achieving high integration of memory cells.

[0491] 24A to 24C will be used to explain examples of the configuration of memory cells that can be applied to the above-mentioned memory cells MCa and memory cells MCb.

[0492] [DOSRAM] 24A to 24C show an example of a circuit configuration of a memory cell of a DRAM. In this specification and the like, a DRAM using a memory cell of a one-OS transistor, one-capacitor type may be called a DOSRAM (Dynamic Oxide Semiconductor Random Access Memory). A memory unit 1471 shown in FIG. 24A has a memory cell MCa and a memory cell MCb. Here, the memory cell MCa has a transistor M1a and a capacitative element CAa, and the memory cell MCb has a transistor M1b and a capacitative element CAb. The transistor M1a and the transistor M1b have a gate (sometimes called a top gate) and a back gate.

[0493] The first terminal of the transistor M1a is connected to the first terminal of the capacitance element CAa, the second terminal of the transistor M1a is connected to the wiring BIL, the gate of the transistor M1a is connected to the wiring WOLa, and the back gate of the transistor M1a is connected to the wiring BGLa. The second terminal of the capacitance element CAa is connected to the wiring CAL. Similarly, the first terminal of the transistor M1b is connected to the first terminal of the capacitance element CAb, the second terminal of the transistor M1b is connected to the wiring BIL, the gate of the transistor M1b is connected to the wiring WOLb, and the back gate of the transistor M1b is connected to the wiring BGLb. The second terminal of the capacitance element CAb is connected to the wiring CAL.

[0494] The wiring BIL functions as a bit line, and the wirings WOLa and WOLb function as word lines. The wiring CAL functions as a wiring for applying a predetermined potential to the second terminals of the capacitance elements CAa and CAb. When writing and reading data, it is preferable to apply a low-level potential to the wiring CAL. The wiring BGLa functions as a wiring for applying a potential to the back gate of the transistor M1a, and the wiring BGLb functions as a wiring for applying a potential to the back gate of the transistor M1b. By applying an arbitrary potential to the wiring BGLa (wiring BGLb), the threshold voltage of the transistor M1a (transistor M1b) can be increased or decreased.

[0495] 24A corresponds to the memory unit 400 shown in FIG. 17A etc. In other words, the transistor M1a corresponds to the transistor 200a, the capacitor CAa corresponds to the capacitor 100a, the transistor M1b corresponds to the transistor 200b, and the capacitor CAb corresponds to the capacitor 100b. The wiring WOLa corresponds to the conductor 260 of the transistor 200a, the wiring WOLb corresponds to the conductor 260 of the transistor 200b, and the wiring BIL corresponds to the conductor 248 and the conductor 288.

[0496] Furthermore, the memory device according to this embodiment is not limited to the memory unit 1471, and the circuit configuration can be changed. For example, the memory device according to this embodiment may be configured as in memory unit 1472 shown in FIG. 24B, in which the back gate of transistor M1a is connected to wiring WOLa instead of wiring BGLa, and the back gate of transistor M1b is connected to wiring WOLb instead of wiring BGLb. For example, the memory device according to this embodiment may be configured as in memory unit 1473 shown in FIG. 24C, in which transistors M1a and M1b have a single-gate structure, that is, transistors without a back gate.

[0497] When the semiconductor device described in the above embodiment is used for the memory unit 1471 or the like, the transistor 200a can be used as the transistor M1a, the transistor 200b can be used as the transistor M1b, the capacitor 100a can be used as the capacitor CAa, and the capacitor 100b can be used as the capacitor CAb. By using OS transistors as the transistors M1a and M1b, the leakage current of the transistors M1a and M1b can be made very small. That is, written data can be held for a long time by the transistors M1a and M1b, so that the frequency of refreshing the memory cells can be reduced. Furthermore, the refresh operation of the memory cells can be made unnecessary. Furthermore, since the leakage current is very small, multi-valued data or analog data can be held in the memory unit 1471, the memory unit 1472, and the memory unit 1473.

[0498] Furthermore, in the DOSRAM, if a sense amplifier is provided so as to overlap under the memory cell array 1470 as described above, the bit line can be shortened. In particular, by providing the conductor 248 under the oxide 230 as shown in the previous embodiment, the bit line can be shortened more than by providing the conductor 248 on the oxide 230. This reduces the bit line capacitance and the storage capacitance of the memory cell.

[0499] Note that the configurations of the peripheral circuit 1411, the memory cell array 1470, and the like shown in this embodiment are not limited to those described above. The arrangement or functions of these circuits, wirings connected to the circuits, circuit elements, and the like may be changed, deleted, or added as necessary.

[0500] The structure described in this embodiment mode can be used in appropriate combination with structures described in other embodiment modes.

[0501] (Embodiment 4) In this embodiment, an example of a chip 1200 on which the semiconductor device of the present invention is mounted is shown with reference to Figures 25A and 25B. A plurality of circuits (systems) are mounted on the chip 1200. A technology for integrating a plurality of circuits (systems) on a single chip in this manner is sometimes called a system on chip (SoC).

[0502] As shown in FIG. 25A, the chip 1200 includes a CPU 1211, a GPU 1212, one or more analog computing units 1213, one or more memory controllers 1214, one or more interfaces 1215, one or more network circuits 1216, and the like.

[0503] Chip 1200 is provided with bumps (not shown) and is connected to a first surface of a printed circuit board (PCB) 1201 as shown in Fig. 25B. In addition, a plurality of bumps 1202 are provided on the back side of the first surface of PCB 1201 and are connected to a motherboard 1203.

[0504] The motherboard 1203 may be provided with a storage device such as a DRAM 1221 and a flash memory 1222. For example, the DOSRAM described in the above embodiment may be used for the DRAM 1221. By using the DOSRAM described in the above embodiment for the DRAM 1221, the storage capacity of the DRAM 1221 can be increased.

[0505] The CPU 1211 preferably has a plurality of CPU cores. The GPU 1212 preferably has a plurality of GPU cores. The CPU 1211 and the GPU 1212 may each have a memory for temporarily storing data. Alternatively, a memory common to the CPU 1211 and the GPU 1212 may be provided in the chip 1200. The memory may be the above-mentioned DOSRAM or the like. The GPU 1212 is suitable for parallel calculation of a large amount of data, and may be used for image processing and multiplication and accumulation. By providing the GPU 1212 with an image processing circuit or a multiplication and accumulation circuit using the oxide semiconductor according to the present invention, it becomes possible to perform image processing and multiplication and accumulation with low power consumption.

[0506] In addition, by providing the CPU 1211 and GPU 1212 on the same chip, the wiring between the CPU 1211 and GPU 1212 can be shortened, and data transfer from the CPU 1211 to the GPU 1212, data transfer between the memories of the CPU 1211 and GPU 1212, and transfer of calculation results from the GPU 1212 to the CPU 1211 after calculation in the GPU 1212 can be performed quickly.

[0507] The analog calculation unit 1213 has one or both of an A / D (analog / digital) conversion circuit and a D / A (digital / analog) conversion circuit. The analog calculation unit 1213 may also be provided with the above-mentioned product-sum calculation circuit.

[0508] The memory controller 1214 has a circuit that functions as a controller for the DRAM 1221 and a circuit that functions as an interface for the flash memory 1222 .

[0509] The interface 1215 has an interface circuit with externally connected devices such as a display device, a speaker, a microphone, a camera, and a controller. The controller includes a mouse, a keyboard, a game controller, etc. As such an interface, a USB (Universal Serial Bus), an HDMI (registered trademark) (High-Definition Multimedia Interface), etc. can be used.

[0510] The network circuit 1216 has a function of controlling connections with a LAN (Local Area Network), etc. In addition, it may have a circuit for network security.

[0511] The above circuits (systems) can be formed in the same manufacturing process in the chip 1200. Therefore, even if the number of circuits required for the chip 1200 increases, there is no need to increase the manufacturing process, and the chip 1200 can be manufactured at low cost.

[0512] A PCB 1201 on which a chip 1200 having a GPU 1212 is provided, a motherboard 1203 on which a DRAM 1221 and a flash memory 1222 are provided can be referred to as a GPU module 1204.

[0513] The GPU module 1204 has the chip 1200 using SoC technology, so that its size can be reduced. In addition, since it excels in image processing, it is suitable for use in portable electronic devices such as smartphones, tablet terminals, laptop PCs, and portable (portable) game consoles. In addition, a multiply-and-accumulate circuit using the GPU 1212 can execute techniques such as deep neural networks (DNN), convolutional neural networks (CNN), recurrent neural networks (RNN), autoencoders, deep Boltzmann machines (DBM), and deep belief networks (DBN), so that the chip 1200 can be used as an AI chip, and the GPU module 1204 can be used as an AI system module.

[0514] The structure described in this embodiment mode can be used in appropriate combination with structures described in other embodiment modes.

[0515] (Embodiment 5) This embodiment mode describes an example of an electronic component or electronic device in which the memory device or the like described in the above embodiment mode is incorporated.

[0516] <Electronic components> First, an example of an electronic component incorporating a memory device 720 will be described with reference to FIGS. 26A and 26B.

[0517] Fig. 26A shows a perspective view of electronic component 700 and a substrate (mounting substrate 704) on which electronic component 700 is mounted. Electronic component 700 shown in Fig. 26A has memory device 720 in mold 711. Part of electronic component 700 is omitted in Fig. 26A to show the inside of electronic component 700. Electronic component 700 has lands 712 on the outside of mold 711. Lands 712 are electrically connected to electrode pads 713, and electrode pads 713 are electrically connected to memory device 720 by wires 714. Electronic component 700 is mounted on, for example, a printed circuit board 702. A plurality of such electronic components are combined and electrically connected on printed circuit board 702 to complete mounting substrate 704.

[0518] The memory device 720 includes a driver circuit layer 721 and a memory circuit layer 722. For example, the memory circuit layer 722 can be formed using the 3D cell array described in the above embodiment.

[0519] 26B shows a perspective view of electronic component 730. Electronic component 730 is an example of a SiP (System in package) or MCM (Multi Chip Module). Electronic component 730 has an interposer 731 provided on a package substrate 732 (printed circuit board), and a semiconductor device 735 and a plurality of memory devices 720 provided on interposer 731.

[0520] In the electronic component 730, an example is shown in which the storage device 720 is used as a high bandwidth memory (HBM). Also, the semiconductor device 735 can be an integrated circuit (semiconductor device) such as a CPU, a GPU, or an FPGA.

[0521] The package substrate 732 may be a ceramic substrate, a plastic substrate, a glass epoxy substrate, etc. The interposer 731 may be a silicon interposer, a resin interposer, etc.

[0522] The interposer 731 has a plurality of wirings and functions to electrically connect a plurality of integrated circuits having different terminal pitches. The plurality of wirings are provided in a single layer or multiple layers. The interposer 731 also functions to electrically connect the integrated circuits provided on the interposer 731 to electrodes provided on the package substrate 732. For these reasons, the interposer may be called a "rewiring substrate" or an "intermediate substrate." In addition, a through electrode may be provided in the interposer 731, and the integrated circuits and the package substrate 732 may be electrically connected using the through electrode. In addition, in a silicon interposer, a TSV (Through Silicon Via) may be used as the through electrode.

[0523] It is preferable to use a silicon interposer as the interposer 731. Since a silicon interposer does not require an active element, it can be manufactured at a lower cost than an integrated circuit. On the other hand, since the wiring of the silicon interposer can be formed by a semiconductor process, it is easy to form fine wiring, which is difficult to form with a resin interposer.

[0524] In HBM, many wirings need to be connected to realize a wide memory bandwidth. For this reason, the interposer that implements HBM requires fine and high-density wiring. Therefore, it is preferable to use a silicon interposer for the interposer that implements HBM.

[0525] In addition, in SiPs and MCMs that use silicon interposers, reliability is less likely to decrease due to differences in the expansion coefficient between the integrated circuit and the interposer. In addition, because the surface of the silicon interposer is highly flat, connection defects are less likely to occur between the integrated circuit mounted on the silicon interposer and the silicon interposer. In particular, it is preferable to use silicon interposers in 2.5D packages (2.5-dimensional mounting) in which multiple integrated circuits are arranged side by side on the interposer.

[0526] A heat sink (heat dissipation plate) may be provided so as to overlap the electronic component 730. When providing a heat sink, it is preferable to align the height of an integrated circuit provided on the interposer 731. For example, in the electronic component 730 shown in this embodiment, it is preferable to align the height of the memory device 720 and the height of the semiconductor device 735.

[0527] In order to mount the electronic component 730 on another substrate, electrodes 733 may be provided on the bottom of the package substrate 732. Fig. 26B shows an example in which the electrodes 733 are formed of solder balls. By providing solder balls in a matrix on the bottom of the package substrate 732, BGA (Ball Grid Array) mounting can be realized. The electrodes 733 may also be formed of conductive pins. By providing conductive pins in a matrix on the bottom of the package substrate 732, PGA (Pin Grid Array) mounting can be realized.

[0528] The electronic component 730 can be mounted on other substrates using various mounting methods, including but not limited to BGA and PGA, such as Staggered Pin Grid Array (SPGA), Land Grid Array (LGA), Quad Flat Package (QFP), Quad Flat J-leaded package (QFJ), and Quad Flat Non-leaded package (QFN).

[0529] This embodiment mode can be implemented in appropriate combination with structures described in other embodiment modes.

[0530] (Embodiment 6) In this embodiment, an application example of a storage device using the semiconductor device described in the previous embodiment will be described. The semiconductor device described in the previous embodiment can be applied to storage devices of various electronic devices (for example, information terminals, computers, smartphones, electronic book terminals, digital cameras (including video cameras), recording and reproducing devices, navigation systems, and the like). Note that the computer here includes a large computer such as a server system, in addition to tablet computers, notebook computers, and desktop computers. Alternatively, the semiconductor device described in the previous embodiment can be applied to various removable storage devices such as SSDs (solid state drives). FIG. 27A and FIG. 27B are schematic diagrams illustrating configuration examples of a removable storage device. For example, the semiconductor device described in the previous embodiment can be processed into a packaged memory chip and used in various storage devices and removable memories.

[0531] FIG. 27A is a schematic diagram of the appearance of an SSD, and FIG. 27B is a schematic diagram of the internal structure of the SSD. SSD 1150 has a housing 1151, a connector 1152, and a board 1153. Board 1153 is housed in housing 1151. For example, memory chip 1154, memory chip 1155, and controller chip 1156 are attached to board 1153. Memory chip 1155 is a work memory for controller chip 1156, and for example, the DOSRAM chip shown in the previous embodiment may be used. By providing memory chip 1154 on the back side of board 1153 as well, the capacity of SSD 1150 can be increased.

[0532] This embodiment mode can be implemented in appropriate combination with structures described in other embodiment modes.

[0533] (Embodiment 7) A semiconductor device according to one embodiment of the present invention can be used in a processor such as a CPU or a GPU, or a chip. Specific examples of electronic devices including a processor such as a CPU or a GPU, or a chip according to one embodiment of the present invention are shown in FIG. 28A to FIG. 28H.

[0534] <Electronic equipment and systems> The GPU or chip according to one embodiment of the present invention can be mounted on various electronic devices. Examples of electronic devices include electronic devices with relatively large screens, such as television devices, monitors for desktop or notebook information terminals, digital signage, large game machines such as pachinko machines, digital cameras, digital video cameras, digital photo frames, electronic book readers, mobile phones, portable game machines, portable information terminals, and audio playback devices. Moreover, by providing the GPU or chip according to one embodiment of the present invention in an electronic device, it is possible to mount artificial intelligence on the electronic device.

[0535] The electronic device of one embodiment of the present invention may have an antenna. By receiving a signal through the antenna, images, information, and the like can be displayed on a display portion. In addition, when the electronic device has an antenna and a secondary battery, the antenna may be used for contactless power transmission.

[0536] An electronic device according to one embodiment of the present invention may have a sensor (including a function of measuring force, displacement, position, velocity, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical substances, sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, odor, or infrared rays).

[0537] An electronic device according to one embodiment of the present invention can have various functions. For example, the electronic device can have a function of displaying various information (still images, videos, text images, etc.) on a display unit, a touch panel function, a function of displaying a calendar, date, or time, a function of executing various software (programs), a wireless communication function, a function of reading out a program or data recorded in a recording medium, etc. Examples of electronic devices are shown in FIGS. 28A to 28H.

[0538] [Information terminal] 28A illustrates a mobile phone (smartphone), which is a type of information terminal. The information terminal 5100 includes a housing 5101 and a display unit 5102. As an input interface, a touch panel is provided on the display unit 5102, and buttons are provided on the housing 5101.

[0539] By applying the chip of one embodiment of the present invention, the information terminal 5100 can execute applications using artificial intelligence. Examples of applications using artificial intelligence include an application that recognizes a conversation and displays the conversation content on the display unit 5102, an application that recognizes characters, figures, and the like input by a user to a touch panel provided in the display unit 5102 and displays them on the display unit 5102, and an application that performs biometric authentication such as fingerprints and voiceprints.

[0540] 28B illustrates a notebook type information terminal 5200. The notebook type information terminal 5200 includes a main body 5201 of the information terminal, a display unit 5202, and a keyboard 5203.

[0541] The notebook type information terminal 5200 can execute an application using artificial intelligence by applying a chip according to one embodiment of the present invention, similar to the above-described information terminal 5100. Examples of applications using artificial intelligence include design support software, text correction software, and automatic menu generation software. In addition, the notebook type information terminal 5200 can be used to develop new artificial intelligence.

[0542] In the above description, a smartphone and a notebook type information terminal are illustrated in Fig. 28A and Fig. 28B as examples of electronic devices, but information terminals other than smartphones and notebook type information terminals can also be applied. Examples of information terminals other than smartphones and notebook type information terminals include PDAs (Personal Digital Assistants), desktop type information terminals, and workstations.

[0543] [Game consoles] FIG. 28C illustrates a portable game machine 5300 which is an example of a game machine. The portable game machine 5300 includes a housing 5301, a housing 5302, a housing 5303, a display unit 5304, a connection unit 5305, an operation key 5306, and the like. The housing 5302 and the housing 5303 can be detached from the housing 5301. When the connection unit 5305 of the housing 5301 is attached to another housing (not shown), a video displayed on the display unit 5304 can be displayed on another video device (not shown). In this case, the housing 5302 and the housing 5303 can each function as an operation unit. This allows a plurality of players to play a game at the same time. The chips described in the above embodiments can be incorporated in the chips provided on the substrates of the housings 5301, 5302, and 5303.

[0544] 28D shows a stationary game machine 5400, which is an example of a game machine. A controller 5402 is connected to the stationary game machine 5400 wirelessly or by wire.

[0545] A game machine with low power consumption can be realized by applying a GPU or a chip of one embodiment of the present invention to a game machine such as a portable game machine 5300 or a stationary game machine 5400. Furthermore, low power consumption can reduce heat generation from a circuit, and therefore the influence of heat generation on the circuit itself, peripheral circuits, and modules can be reduced.

[0546] Furthermore, by applying a GPU or a chip of one embodiment of the present invention to the portable game console 5300, the portable game console 5300 can have artificial intelligence.

[0547] Originally, the expression of the progress of a game, the behavior of creatures appearing in the game, and phenomena occurring in the game are determined by the program of the game, but by applying artificial intelligence to the portable game device 5300, it becomes possible to express things that are not limited to the program of the game. For example, it becomes possible to express things such as changes in the questions asked by the player, the progress of the game, the time, and the behavior of people appearing in the game.

[0548] In addition, when playing a game on the portable game console 5300 that requires multiple players, the game players can be personified using artificial intelligence, so that the game can be played by one person by making the opponent a game player based on artificial intelligence.

[0549] 28C and 28D show a portable game machine and a stationary game machine as examples of game machines, but the game machine to which the GPU or chip of one embodiment of the present invention is applied is not limited to this. Examples of game machines to which the GPU or chip of one embodiment of the present invention is applied include arcade game machines installed in entertainment facilities (game centers, amusement parks, etc.) and pitching machines for batting practice installed in sports facilities.

[0550] [Mainframe computers] The GPU or chip of one embodiment of the present invention can be applied to a large computer.

[0551] 28E is a diagram showing a supercomputer 5500, which is an example of a large computer. FIG. 28F is a diagram showing a rack-mounted calculator 5502 included in the supercomputer 5500.

[0552] A supercomputer 5500 includes a rack 5501 and a plurality of rack-mounted computers 5502. The plurality of computers 5502 are stored in the rack 5501. The computer 5502 is provided with a plurality of boards 5504, and the GPU or chip described in the above embodiment can be mounted on the board.

[0553] The supercomputer 5500 is a large-scale computer mainly used for scientific and technological calculations. In scientific and technological calculations, huge amounts of calculations need to be processed at high speed, and therefore power consumption is high and chips generate a lot of heat. By applying a GPU or chip according to one embodiment of the present invention to the supercomputer 5500, a supercomputer with low power consumption can be realized. Furthermore, low power consumption can reduce heat generation from a circuit, and therefore the influence of heat generation on the circuit itself, peripheral circuits, and modules can be reduced.

[0554] 28E and 28F show a supercomputer as an example of a large computer, but the large computer to which the GPU or chip of one embodiment of the present invention is applied is not limited to this. Examples of large computers to which the GPU or chip of one embodiment of the present invention is applied include computers that provide services (servers) and large general-purpose computers (mainframes).

[0555] [Mobile object] The GPU or chip according to one embodiment of the present invention can be applied to automobiles, which are moving objects, and to the area around the driver's seat of an automobile.

[0556] Fig. 28G is a diagram showing the periphery of the windshield in the interior of an automobile, which is an example of a moving body, Fig. 28G shows display panel 5701, display panel 5702, and display panel 5703 attached to the dashboard, as well as display panel 5704 attached to a pillar.

[0557] The display panels 5701 to 5703 can provide various information by displaying a speedometer, a tachometer, a mileage, a fuel gauge, a gear state, an air conditioner setting, and the like. In addition, the display items and layouts displayed on the display panels can be changed as appropriate according to the user's preferences, and the design can be improved. The display panels 5701 to 5703 can also be used as lighting devices.

[0558] The display panel 5704 can complement the field of view (blind spot) blocked by the pillar by displaying an image from an imaging device (not shown) installed in the vehicle. That is, by displaying an image from an imaging device installed outside the vehicle, blind spots can be complemented and safety can be improved. In addition, by displaying an image that complements the invisible part, safety can be confirmed more naturally and without discomfort. The display panel 5704 can also be used as a lighting device.

[0559] Since the GPU or chip of one embodiment of the present invention can be used as a component of artificial intelligence, the chip can be used, for example, in an automatic driving system for an automobile. The chip can also be used in a system that performs road guidance, risk prediction, etc. The display panels 5701 to 5704 may be configured to display information such as road guidance and risk prediction.

[0560] In the above description, an automobile is described as an example of a moving object, but the moving object is not limited to an automobile. For example, the moving object may be a train, a monorail, a ship, an aircraft (helicopter, unmanned aerial vehicle (drone), airplane, rocket), etc., and the chip of one embodiment of the present invention may be applied to these moving objects to provide a system using artificial intelligence.

[0561] [electric appliances] 28H shows an example of an electric appliance, an electric refrigerator-freezer 5800. The electric refrigerator-freezer 5800 has a housing 5801, a refrigerator door 5802, a freezer door 5803, and the like.

[0562] An electric refrigerator-freezer 5800 having artificial intelligence can be realized by applying the chip of one embodiment of the present invention to the electric refrigerator-freezer 5800. By using artificial intelligence, the electric refrigerator-freezer 5800 can have a function of automatically generating a menu based on ingredients stored in the electric refrigerator-freezer 5800 and the expiration dates of the ingredients, a function of automatically adjusting the temperature to match the ingredients stored in the electric refrigerator-freezer 5800, and the like.

[0563] Although an electric refrig...

Claims

1. a first conductor disposed on a substrate; a metal oxide disposed on an upper surface of the first conductor; a second conductor, a third conductor, and a fourth conductor disposed on the metal oxide; a first insulator disposed on the second conductor to the fourth conductor and having a first opening and a second opening formed therein; a second insulator disposed within the first opening; a fifth conductor disposed on the second insulator; and a third insulator disposed in the second opening; and a sixth conductor disposed on the third insulator; the third conductor is disposed so as to overlap the first conductor; the first opening is formed to overlap a region between the second conductor and the third conductor; the second opening is formed to overlap a region between the third conductor and the fourth conductor; The metal oxide comprises indium oxide.

2. In claim 1, A first capacitance element and a second capacitance element, the first capacitive element is electrically connected to the second conductor; the second capacitive element is electrically connected to the fourth conductor.

Citation Information

Patent Citations

  • Semiconductor memory device

    JP2016213487A

  • Semiconductor device, circuit board, and electronic equipment

    JP2017028237A

  • Semiconductor device, circuit board, and electronic equipment

    JP2017034249A

  • Semiconductor device and semiconductor device manufacturing method

    JP2019047101A

  • Semiconductor device, and method for manufacturing semiconductor device

    WO2019025911A1