Display device
A protective film formed via atomic layer deposition stabilizes peripheral circuits in display devices, enabling a larger display area with a narrower frame and improved reliability.
Patent Information
- Application Number
- JP2024159791
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2015-05-28
- Filing Date
- 2024-09-17
- Publication Date
- 2024-12-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing display devices face challenges in expanding the display area while maintaining high operational stability and reliability of peripheral circuits due to the proximity of drive circuits to the edge, which can lead to reduced transistor characteristics and unstable circuit operation.
The implementation of a protective film formed using atomic layer deposition (ALD) on the substrate, which includes insulating layers and a protective film to isolate the peripheral circuit from atmospheric components, thereby maintaining stability and reducing the frame width.
This approach enhances the operational stability and reliability of peripheral circuits, allows for a narrower frame, and increases the display area, resulting in a high-definition, lightweight, and reliable display device.
Smart Images

Figure 2024169511000001_ABST
Abstract
Description
[Technical field]
[0001] One embodiment of the present invention relates to a display device and an electronic device.
[0002] Note that one embodiment of the present invention is not limited to the above technical field. The technical field relates to an article, a method, or a manufacturing method. is a process, machine, manufacture, or composition of matter. Therefore, one aspect of the present invention disclosed in the present specification more specifically relates to a The technical fields of the present invention include semiconductor devices, display devices, light-emitting devices, power storage devices, memory devices, and input devices. , an input / output device, a driving method thereof, or a manufacturing method thereof, as examples. can be done.
[0003] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. This refers to semiconductor devices in general, including semiconductor elements such as transistors, semiconductor circuits, arithmetic units, and memory devices. The device is one aspect of a semiconductor device. Optical devices, power generation devices (including thin-film solar cells, organic thin-film solar cells, etc.), and electronic devices are all semiconductor devices. The semiconductor device may include a conductor device. [Background technology]
[0004] Displays using thin-film transistors have become widespread around the world and indispensable in people's lives. In addition, these displays are thin and lightweight, making them suitable for use in portable information terminals and other devices. It has become indispensable in various situations.
[0005] In addition, display devices that have a display area (pixel section) and peripheral circuits (drive section) on the same substrate have become widespread. For example, Patent Document 1 discloses a transistor using an oxide semiconductor for a display region and a The technology used for the peripheral circuits is disclosed. By forming the display area and the peripheral circuits simultaneously, The manufacturing cost can be reduced. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2007-123861 A Summary of the Invention [Problem to be solved by the invention]
[0007] When manufacturing a display device, ensure that the display area is as large as possible on the viewing side (display surface side). In order to expand the display area, it is necessary to increase the area from the edge of the display area to the edge of the substrate. It is necessary to make the frame, which is the area of the image, as narrow as possible.
[0008] On the other hand, the driving circuits around the display area are located in the frame area, making it difficult to expand the display area. In addition, if the frame is narrowed, the drive circuit will be closer to the edge of the substrate, and the influence of atmospheric components will be reduced. The reliability of the transistor characteristics of the driver circuit decreases due to intrusion, etc., causing the circuit operation to become unstable. There is a risk.
[0009] One object of one embodiment of the present invention is to provide a display device having a peripheral circuit portion with high operational stability. Let us assume that.
[0010] Another object of one embodiment of the present invention is to provide a display device with a narrow frame.
[0011] Another object of one embodiment of the present invention is to provide a lightweight display device.
[0012] Another object of one embodiment of the present invention is to provide a high-definition display device.
[0013] Another object of one embodiment of the present invention is to provide a highly reliable display device.
[0014] Another object of one embodiment of the present invention is to provide a large-area display device.
[0015] Another object of one embodiment of the present invention is to provide a display device that can reduce power consumption. This is one of the topics.
[0016] Another object is to provide a novel display device or the like.
[0017] Another object is to provide a manufacturing method of the display device.
[0018] The description of these problems does not preclude the existence of other problems. It is not necessary for the embodiment to solve all of these problems. The above will become apparent from the description in the specification, drawings, claims, etc. It is possible to extract other issues from the descriptions in the patent, claims, etc. [Means for solving the problem]
[0019] One aspect of the present invention is a method for manufacturing a semiconductor device comprising the steps of: forming a semiconductor device on a first surface of the first substrate; a first insulating layer is provided on the first surface of the second substrate, a second insulating layer is provided on the first surface of the second substrate, The first surface of the first substrate and the first surface of the second substrate have the same area. The first surfaces of the plates face each other, and an adhesive layer is provided between the first insulating layer and the second insulating layer; The protective film is in contact with the first substrate, the first insulating layer, the adhesive layer, the second insulating layer, and the second substrate. A display device having an area.
[0020] One aspect of the present invention is a method for manufacturing a semiconductor device comprising the steps of: forming a semiconductor device on a first surface of the first substrate; A first insulating layer is provided on the first surface of the second substrate, and a second insulating layer is provided on the first surface of the second substrate. The first surface of the first substrate has an area smaller than that of the first substrate, and the first surface of the first substrate and the first substrate have an area smaller than that of the first substrate. The first surfaces of the plates face each other, and an adhesive layer is provided between the first insulating layer and the second insulating layer; The protective film is in contact with the first substrate, the first insulating layer, the adhesive layer, the second insulating layer, and the second substrate. A display device having an area.
[0021] In addition, a transistor, a capacitance element, and a The display device may include a display element, a light-shielding layer, a colored layer, and a spacer.
[0022] The protective film may be made of an oxide, nitride or metal.
[0023] In addition, aluminum oxide, hafnium oxide, zirconium oxide, titanium oxide, etc. can be used as protective films. Zinc oxide, indium oxide, tin oxide, indium tin oxide, tantalum oxide, silicon oxide Silicon oxide, manganese oxide, nickel oxide, erbium oxide, cobalt oxide, tellurium oxide, titanium oxide Barium tantalate, titanium nitride, tantalum nitride, aluminum nitride, tungsten nitride, nitrogen Cobalt nitride, silicon nitride, manganese nitride, hafnium nitride, ruthenium, platinum, nickel For example, nickel, cobalt, manganese, or copper may be used.
[0024] The protective film may also contain fluorine, carbon, or hydrogen.
[0025] The fluorine concentration in the protective film is 1×10 18 atoms / cm 3 More than 1×10 22 at oms / cm 3 It is desirable that it be less than this.
[0026] The carbon concentration in the protective film is 1×10 17 atoms / cm 3 More than 1×10 22 ato ms / cm 3 It is desirable that it be less than this.
[0027] The hydrogen concentration in the protective film is 1×10 19 atoms / cm 3 More than 1×10 22 ato ms / cm 3 It is desirable that it be less than this.
[0028] The display device may also include a liquid crystal element.
[0029] The display device may also include an organic EL element.
[0030] Moreover, a configuration using a display device, a microphone, and a speaker is also possible.
[0031] Other aspects of the present invention will be described in the following embodiments and As shown in the drawings. Effect of the Invention
[0032] According to one embodiment of the present invention, a display device in which the peripheral circuit portion has high operational stability can be provided.
[0033] Alternatively, one embodiment of the present invention can provide a display device with a narrow frame.
[0034] Alternatively, one embodiment of the present invention can provide a lightweight display device.
[0035] Alternatively, according to one embodiment of the present invention, a high-definition display device can be provided.
[0036] Alternatively, according to one embodiment of the present invention, a highly reliable display device can be provided.
[0037] Alternatively, one embodiment of the present invention can provide a large-area display device.
[0038] Another embodiment of the present invention can provide a display device that can reduce power consumption. Cut.
[0039] Alternatively, one embodiment of the present invention can provide a novel display device or the like.
[0040] Alternatively, a method for manufacturing the above display device can be provided.
[0041] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have to have all of these effects. Effects other than these may also be included. The above is self-evident from the description, drawings, claims, etc. Other effects can be extracted from the claims and other descriptions. [Brief description of the drawings]
[0042] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating a display device of one embodiment of the present invention. [Diagram 2] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 3] 1 is a cross-sectional view illustrating a method for manufacturing a display device according to one embodiment of the present invention; [Figure 4] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 5] 1A and 1B are a top view and a cross-sectional view illustrating a display device of one embodiment of the present invention. [Figure 6] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 7] 1A to 1C are cross-sectional views illustrating a manufacturing method of a display device according to one embodiment of the present invention. [Figure 8] FIG. 1 is a schematic cross-sectional view for explaining a film formation principle. [Figure 9] 1A is a schematic cross-sectional view of a film-forming apparatus and a schematic top view of a manufacturing apparatus including a chamber for the film-forming apparatus. [Figure 10] FIG. [Figure 11] 1A and 1B are a top view and a cross-sectional view illustrating a display device of one embodiment of the present invention. [Figure 12] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 13] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 14] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 15] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 16] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 17] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 18] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 19] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 20] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 21] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 22] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 23] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 24] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 25] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 26] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 27] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 28] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Figure 29] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 30] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 31] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 32] FIG. 1 is a cross-sectional view illustrating a display device according to one embodiment of the present invention. [Diagram 33] 1A and 1B are cross-sectional views illustrating a transistor of one embodiment of the present invention. [Diagram 34] 1A and 1B are cross-sectional views illustrating a transistor of one embodiment of the present invention. [Diagram 35] 1A and 1B are a top view and a cross-sectional view illustrating a transistor of one embodiment of the present invention. [Diagram 36] 1A and 1B are a top view and a circuit diagram illustrating a display device of one embodiment of the present invention. [Figure 37] FIG. 2 is a top view showing the positional relationship between pixels, transistors, and wiring of a touch sensor. [Figure 38] FIG. 1 is a top view illustrating an input device of one embodiment of the present invention. [Figure 39] FIG. 1 is a top view illustrating an input device of one embodiment of the present invention. [Diagram 40] FIG. 1 is a top view illustrating an input device of one embodiment of the present invention. [Diagram 41] FIG. 1 is a top view illustrating an input device of one embodiment of the present invention. [Diagram 42] 1 is a circuit diagram illustrating an input device of one embodiment of the present invention. [Diagram 43] 1 is a circuit diagram illustrating an input device of one embodiment of the present invention. [Diagram 44]1A to 1C are diagrams illustrating a method for forming a CAAC-OS film. [Diagram 45] A diagram explaining the InMZnO4 crystal. [Figure 46] 1A to 1C are diagrams illustrating a method for forming a CAAC-OS film. [Figure 47] 1A to 1C are diagrams illustrating a method for forming a CAAC-OS film. [Figure 48] A diagram explaining the method for forming nc-OS. [Figure 49] FIG. 1 is a top view of a display module to which a semiconductor device of one embodiment of the present invention is applied. [Figure 50] 1A to 1C are diagrams illustrating electronic devices according to one embodiment of the present invention. [Figure 51] 1A to 1C are diagrams illustrating electronic devices according to one embodiment of the present invention. [Figure 52] Ca test measurement results with and without a protective film formed by the ALD method. [Diagram 53] 13 shows the results of measuring the voltage holding ratio of a sample using an embodiment of the present invention and a positive liquid crystal. [Figure 54] 13 shows the results of measuring the voltage holding ratio of a sample using one embodiment of the present invention and using a negative type liquid crystal as the liquid crystal. [Figure 55] 13 shows a display result of a display device manufactured using one embodiment of the present invention. [Figure 56] 3A to 3C are schematic cross-sectional views of a display panel and a schematic cross-sectional view of an SEM observation area. [Figure 57] Cross-sectional SEM photograph of the side of the display panel, and EDX mapping analysis results. [Figure 58] Cross-sectional SEM photograph of the side of the display panel, and EDX mapping analysis results. [Figure 59] SIMS analysis results of aluminum oxide films formed by the ALD method or the sputtering method. [Figure 60] 1A and 1B are top views of a sample for measuring light transmittance and a diagram showing a method for driving a display. [Figure 61] Voltage-light transmittance characteristics at intermediate tones. [Figure 62] Measurement results of light transmittance at various times after storage in a 60℃, 90% humidity environment. [Figure 63] Density evaluation results of aluminum oxide film. [Figure 64] Ca test measurement results with and without a protective film formed by the ALD method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0043] The embodiment will be described in detail with reference to the drawings. However, the present invention is not limited to the following description. The present invention is not limited to the above embodiment, and various changes and modifications may be made in the form and details without departing from the spirit and scope of the present invention. It will be easily understood by those skilled in the art that the above-mentioned invention can be obtained by the following embodiments. The present invention should not be construed as being limited to the contents described below. The same reference numerals are used in different drawings to indicate the same parts or parts having similar functions. A repeated explanation thereof will be omitted.
[0044] <Notes on the description explaining the drawings> In this specification, the terms "above" and "below" that indicate the positional relationship between components are used. The above is used for convenience in describing the drawings. The meaning of the term varies depending on the direction in which the configuration is depicted. It is not limited to this and can be rephrased appropriately depending on the situation.
[0045] In addition, the terms "above" and "below" refer to the positional relationship of components directly above or below each other and directly adjacent to each other. For example, if the expression is "electrode B on insulating layer A," It is not necessary for electrode B to be formed directly on insulating layer A. This does not exclude the inclusion of other components.
[0046] In this specification, "parallel" means that two straight lines are arranged at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Line" refers to the state in which two straight lines are arranged at an angle between -30° and 30°. "Perpendicular" means that two straight lines are arranged at an angle of 80° or more and 100° or less. Therefore, the angle may be between 85° and 95°. This refers to a state in which two straight lines are arranged at an angle of 60° or more and 120° or less.
[0047] In addition, in this specification, when the crystal is a trigonal or rhombohedral crystal, it is represented as a hexagonal crystal system. .
[0048] In addition, in the drawings, the size, layer thickness, and area are shown arbitrarily for convenience of explanation. Therefore, the drawings are not necessarily limited to the scale. The drawings are merely schematic illustrations for illustrative purposes only, and are not limited to the shapes or values shown in the drawings.
[0049] In addition, in the drawings, in top views (also called plan views or layout views) and perspective views, In order to clarify the drawings, some components may be omitted.
[0050] In addition, "the same" may mean having the same area or the same shape. Due to the manufacturing process, it is expected that the shapes will not be completely identical. In other words, they are the same.
[0051] <Notes on possible alternative descriptions> In this specification, when describing the connection relationship of a transistor, "the other of the source or drain" (or the first electrode, or the first terminal), "the other of the source or drain" (or the second electrode, The source and drain of a transistor are written as the first terminal and the second terminal. This is because it varies depending on the structure or operating conditions of the transistor. The name of the input may be changed depending on the situation, such as source (drain) terminal or source (drain) electrode. It can be rephrased appropriately accordingly.
[0052] In addition, the terms "electrode" and "wiring" used in this specification and the like do not limit the functionality of these components. For example, an "electrode" may be used as part of a "wire." In addition, the term "electrode" or "wiring" may be used to refer to the plural "electrodes" or "wirings". This also includes cases where the "line" is formed as a single unit.
[0053] In this specification, a transistor includes a gate, a drain, and a source. It is an element that has at least three terminals. And the drain (drain terminal, drain A channel is formed between the source (source terminal, source region or drain electrode) and the source (source terminal, source region or source electrode). The transistor has a channel region and allows current to flow through the drain, the channel region, and the source. It is possible.
[0054] Here, the source and drain vary depending on the structure or operating conditions of the transistor. Therefore, it is difficult to determine which is the source and which is the drain. The part that functions as a source and the part that functions as a drain are not called a source or a drain. One of the source and the drain is referred to as a first electrode, and the other of the source and the drain is referred to as a second electrode. It may be indicated.
[0055] In this specification, the ordinal numbers "first," "second," and "third" are used to avoid confusion of the elements. It should be noted that the numbers are added to avoid confusion and are not intended to be limiting.
[0056] In the present specification, the substrate of the display panel is provided with, for example, an FPC (Flexible Printed Circuit). Integrated Circuits) or TCP (Tape Carrier Packa ge) or COG (Chip On Glass) on the board Devices in which ICs (integrated circuits) are directly mounted using this method are sometimes called display devices.
[0057] In addition, the words "membrane" and "layer" may be interchangeable depending on the situation. For example, the term "conductive layer" can be used interchangeably with the term "conductive film." ". Alternatively, for example, the term "insulating film" may be used. It may be possible to change the term to "insulating layer."
[0058] <Notes on definitions of terms> The following provides definitions of terms not mentioned in the above embodiments.
[0059] <About connection> In this specification, "A and B are connected" does not mean that A and B are directly connected. In addition to the above, it includes those that are electrically connected. Here, A and B are electrically connected. Being connected means that there is an object between A and B that has some electrical effect. A communication line is a line that enables the transmission of electrical signals between A and B.
[0060] Note that these expression methods are merely examples, and the present invention is not limited to these expression methods. , Y, Z1, and Z2 are objects (e.g., devices, elements, circuits, wiring, electrodes, terminals, conductive films, layer, etc.).
[0061] In addition, the contents (or even a part of the contents) described in one embodiment may be used in the embodiment. Another subject matter (or a part of the subject matter) described in the above and / or one or more other embodiments The contents (or a part of the contents) described in the embodiments may be applied, combined, or replaced. It is possible to do things like drawing.
[0062] The contents described in the embodiments are explained in detail with reference to various figures in each embodiment. This refers to the content that is stated or stated using the text in the specification.
[0063] In addition, a figure (or a part thereof) described in one embodiment may be different from another part of the figure, Another figure (or a part thereof) described in the embodiment, and / or one or more By combining the figures (or a part of them) described in the other embodiments of the present invention, This allows even more diagrams to be constructed.
[0064] (Embodiment 1) In this embodiment, a configuration example of a display panel will be described.
[0065] <Protection of the Surface and Side Parts of the Substrate by the Protective Film 23> FIG. 1 shows a top view and a cross-sectional view of a display device. In FIG. 1(A), a display device 10 includes: A display panel 20 having a display area 21 and a peripheral circuit 22, and an FPC 42 are used. In one embodiment of the present invention, a protective film 23 is provided on the display panel 20. The protective film 23 is formed by atomic layer deposition (ALD). It is preferable to form the film by the Micro-Layer Deposition method. The protective film such as the protective film 23 can protect, for example, a display element or a transistor. In addition, the protective film such as the protective film 23 has a function of preventing the display element and the transistor from being damaged. In some cases, the product may have other functions, such as the addition of one or more ingredients. A protective film such as the protective film 23 may be simply referred to as a film. may be referred to as the first membrane, the second membrane, etc.
[0066] FIG. 1B shows a cross-sectional view of the display panel taken along dashed line A1-A2, which indicates the substrate edge of the display panel. indicates the end of the area having the adhesive layer 370, and A4 indicates the end of the peripheral circuit area. The module is formed with transistors, capacitance elements, display elements, etc., and has a protective layer at the edge of the substrate. Substrate 100 covered with film 23, substrate 300, insulating layer 130, insulating layer 131, insulating layer 170 , insulating layer 180, insulating layer 181, insulating layer 182, light shielding layer 18, insulating layer 330, spacer 2 1B, the substrate 100 and the substrate 370 are shown. 300 and 301 can overlap and have approximately the same area. This improves the controllability of alignment during lamination.
[0067] The thickness of the protective film 23 is preferably 3 nm to 200 nm, more preferably 5 nm to 15 nm. It is desirable to make the thickness less than 0 nm. This improves the barrier properties and prevents the film from penetrating into the display panel. This can prevent the infiltration of atmospheric components.
[0068] Alternatively, the hydrogen concentration in the protective film 23 is 1×10 19 atoms / cm 3 1x or more 10 22 atoms / cm 3 Less than 1 x 10 19 atoms / cm 3 1x or more 10 21 atoms / cm 3 It is preferable that the protective film 23 has a large amount of hydrogen. In this case, hydrogen may penetrate through the protective film 23 to the display panel side, causing a deterioration in the characteristics of the peripheral circuits. Therefore, by having the above-mentioned hydrogen concentration in the protective film, high purity The protective film 23 can be provided to suppress the intrusion of hydrogen from the protective film to the display panel side, and the peripheral circuit This can improve the operational stability and reliability of the road.
[0069] Alternatively, the carbon concentration in the protective film 23 is 1×10 17 atoms / cm 3 1x or more 10 22 atoms / cm 3 Less than 1 x 10 17 atoms / cm 3 1x or more 10 21 atoms / cm 3 less than 1×10 17 atoms / cm 3 Below Top 1×10 20 atoms / cm 3 It is preferable that the carbon concentration in the protective film 23 is less than 1000 nm. By having the above concentration, the protective film can be made denser and the barrier properties can be further improved. can be increased to.
[0070] Alternatively, the fluorine concentration in the protective film 23 is 1×10 18 atoms / cm 3 1 more ×10 22 atoms / cm 3 Less than 1 x 10 18atoms / cm 3 1 more ×10 21 atoms / cm 3 It is preferable that the fluorine concentration in the protective film 23 is less than 100%. By having the above concentration, the protective film can be made denser and the barrier properties can be further improved. It can be improved.
[0071] <Method of forming protective film 23 on display panel by ALD method> Using Figures 3(A), 3(B), and 3(C), we will explain how to fabricate a protective film for a display panel using the ALD method. The method for forming the film 23 will now be described.
[0072] A transistor, a capacitor, a part of a display element, etc. are provided on a substrate 100 to form a region 11. In addition, a light-shielding layer, a colored layer, an insulating layer, a part of a display element, etc. are provided on the substrate 300, and a region 12 (See FIG. 3(A)).
[0073] Next, the region 11 of the substrate 100 and the region 12 of the substrate 300 are placed face to face, and the adhesive layer 370 is By bonding the substrate 100 and the substrate 300 using the adhesive, the display panel 20 can be formed. (See Figure 3(B)).
[0074] The temperature at which the protective film 23 is formed by the ALD method is from room temperature to less than 200° C., and preferably from 5 It can be greater than or equal to 0 degrees and less than 150 degrees.
[0075] The ALD method can form a film extremely uniformly on the surface to be formed. For example, aluminum oxide, hafnium oxide, zirconium oxide, titanium oxide, Zinc oxide, indium oxide, tin oxide, indium tin oxide (ITO), tantalum oxide, Silicon oxide, manganese oxide, nickel oxide, erbium oxide, cobalt oxide, terbium oxide barium titanate, titanium nitride, tantalum nitride, aluminum nitride, tungsten nitride The protective film is made of silicon nitride, cobalt nitride, silicon nitride, manganese nitride, hafnium nitride, etc. The protective film is not limited to an insulating film, and a conductive film may be formed. For example, ruthenium, platinum, nickel, cobalt, manganese, copper, etc. can be deposited. It is possible.
[0076] In addition, the protective film 23 is not formed on the portion electrically connected to the FPC 42, etc. As a method of masking, organic films, inorganic films, For example, silicon oxide, silicon oxynitride, gallium oxide, etc. can be used. , gallium oxide nitride, yttrium oxide, yttrium oxide nitride, hafnium oxide, Oxide insulating film such as hafnium oxide nitride, nitride insulating film such as silicon nitride, aluminum nitride Film, photoresist, polyimide resin, acrylic resin, polyimide amide resin, benzosilane Organic materials such as clobutene resin, polyamide resin, and epoxy resin can be used. When these films are used as a mask, the protective film 23 can be removed after the film is formed.
[0077] In addition, the area where the film is to be formed by the ALD method may be masked with a metal mask. Lumask is made of iron, chromium, nickel, cobalt, tungsten, molybdenum, aluminum, A metal element selected from aluminum, copper, tantalum, titanium, or a material containing the above-mentioned metal elements as a component. The metal may be an alloy of any of the above metal elements or a combination of the above metal elements. The mask may be placed close to or in contact with the display panel.
[0078] In addition, by using the ALD method, a dense film can be formed. By forming a protective film 23 on the surface by the ALD method, the intrusion of external components such as moisture is suppressed. As a result, the variation in transistor characteristics can be suppressed, and the peripheral circuits can be This allows for stable operation. In addition, narrowing the frame allows for an expansion of the pixel area, Furthermore, the display device can have a higher resolution.
[0079] In addition, by providing the protective film 23, the distance A1-A4 between the end of the peripheral circuit 22 and the end of the substrate Even if the gap is narrowed, the barrier properties are high, so the transistor characteristics are stable, i.e. the operation of the peripheral circuits is stable. The stability is improved. Therefore, the presence of the protective film 23 makes it possible to narrow the frame of the display panel. For example, the distance from the end of the peripheral circuit 22 to the end of the substrate (the cut portion for processing the panel) can be The distance A1-A4 can be set to 300 μm or less, preferably 200 μm or less. The structure at the end portion can also be made smooth as shown in FIG. 1(C).
[0080] By forming the protective film 23 on the insulating layer, the metal components in the protective film 23 are absorbed into the insulating layer. For example, when forming the protective film 23 on the insulating layer 330, When the insulating layer is formed by heating, and is made of organic resin, the resin softens and the protective film 23 The metal components therein can also be diffused into the insulating layer.
[0081] Also, a resin film may be provided on the outside of the protective film 23. This allows various stresses to be mitigated. This allows the insulation layer to be prevented from being destroyed due to stress concentration. This makes it possible to provide a highly reliable display device.
[0082] <Another example of the display panel periphery configuration 1> FIG. 2(A) and FIG. 2(B) show another example of the configuration of FIG. 1(B). In this case, the protective film 23 is placed on the back as shown in FIG. It can be wrapped around slightly to the front side, or to the back side (area 14) as shown in Figure 2(B). This also makes it possible to suppress the formation of the protective film 23.
[0083] <Another example of the display panel periphery configuration 2> 4(A) and 4(B) show another example of the configuration of FIG. 1(B). By using the protective film 23, This can prevent moisture from entering the material, and reduce the number of insulating layers. In FIG. 4(B), the insulating layer 182 used in FIG. 1(B) and FIG. 1(C) is not included. It is possible.
[0084] <Another example of the display panel periphery configuration 3> FIG. 5(A) shows a configuration example different from those shown in FIG. 4(A) and FIG. 4(B). FIG. 5(A) shows a display panel. 5(B) is a top view of the filter 20 as viewed from the substrate 300 side, and FIG. 5(B) is a cross-sectional view taken along dashed line A1-A2. In FIG. 5(A), each layer is omitted for ease of viewing. In the configuration example shown in FIG. 4B, an insulating layer 182 is added to the structure of FIG. 1B in the same manner as in FIG. 4A. In addition, in FIG. 5(A) and FIG. 5(B), the upper surface of the substrate 100 may be a structure that does not have the above-mentioned structure. The area of the upper surface of the substrate 300 can be made smaller than the area of the upper surface. As shown in FIG. 5A, when the peripheral portion of the substrate 100 is viewed from the front side (substrate 300 side), Since the side surface of the adhesive layer 370 is exposed and has an inclined shape, the protective film 23 is more It can be formed uniformly.
[0085] As a configuration example different from that shown in FIG. 5(A), as shown in FIG. 5(C), The substrate 300 has a smaller area than the substrate 100. As shown in FIG. 5(D), a protective film 2 may be provided on the substrate 100 side and the substrate 300 side. 3 may be hardly formed.
[0086] <Another configuration example 4 of the display panel periphery> Figures 6(A), 6(B), 6(C), 6(D), and 6(E) show different patterns from those in Figure 1(B). A configuration example is shown. By using the protective film 23, it is possible to prevent the intrusion of moisture and the like, and the insulating layer The number of can be further reduced. Figure 6(A), Figure 6(B), Figure 6(C), Figure 6(D), In the configuration example shown in FIG. 6(E), the insulating layer used in the configuration examples shown in FIG. 1(B) and FIG. 1(C) is The structure of the peripheral portion may be one not including the insulating layer 181 and the insulating layer 182. As shown in FIG. 6(B), the surface may have irregularities, or may have almost no irregularities. As shown in FIG. 6(B) and FIG. 6(C), the spacer 240 may be omitted. As shown in FIG. 6(D), the substrate 100 side and the substrate 300 side Alternatively, the protective film 23 may be omitted in the region 14 as shown in FIG. A structure not having this may also be used.
[0087] Note that one embodiment of the present invention has been described in this embodiment. An embodiment of the present invention will be described below. However, the embodiment of the present invention is not limited to these. That is, various inventive aspects are described in this and other embodiments. Therefore, one embodiment of the present invention is not limited to a specific embodiment. In the above, an example of film formation using the ALD method has been described, but one embodiment of the present invention is not limited thereto. In some cases or depending on the situation, various film formation methods according to an embodiment of the present invention may be used. For example, in some cases or depending on the circumstances, one of the methods of the present invention may be used to form a film. In the embodiment, the CVD method, the plasma CVD method, the MOCVD method, the PVD method, the sputtering method, the deposition method At least one method such as spin coating, ink jet, printing, or coating. Alternatively, for example, optionally or depending on the situation, In one embodiment of the present invention, the film may be formed without using the ALD method.
[0088] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0089] (Embodiment 2) In this embodiment, a plurality of display panels having the protective film 23 described in the first embodiment are manufactured. This article explains how to do this.
[0090] A method for manufacturing the display panel 20 is shown in FIG. 7(A), FIG. 7(B), FIG. 7(C), and FIG. FIG. 7 is a schematic diagram showing a liquid crystal element 80 and an adhesive layer 370 as a display element. The panel includes an element substrate having transistors, capacitance elements, etc., on a substrate 100, and a substrate 30 The opposing substrate, which has a light-shielding layer, a colored layer, etc., on the liquid crystal display, is bonded in such a way that the liquid crystal is sealed. Note that the same steps as those in the manufacturing method shown in FIG. 3 will be omitted.
[0091] In a configuration having a plurality of display panels 20 (see FIG. 7A), the substrate 300 (upper surface side) By cutting, the groove portion 30 can be formed (see FIG. 7(B)). After that, a protective film 23 is formed from the upper side by the ALD method (see FIG. 7(C)). By cutting the 0 side, multiple display panels can be manufactured (see FIG. 7(D)). In this case, the formation of the protective film 23 on the back surface can be suppressed.
[0092] After cutting, a protective film may be formed again using the ALD method.
[0093] In FIG. 7D, when the substrate 100 is cut, the substrate edge or the vicinity of the substrate edge is Damaged areas with tiny cracks (also called microcracks) may form in the film. Specifically, a marking is made (also called a scribe) and the stress is concentrated on the marking. In addition, microcracks may form on the edges of the broken glass. In such a case, if a protective film is formed using the ALD method, the protective film will not be able to penetrate the damaged area. The film is formed even inside the cracks, so the damaged area can be covered. This can suppress embrittlement and cracking of the substrate or film in the subsequent manufacturing steps.
[0094] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0095] (Embodiment 3) <Description of the film formation method> The following describes a method for forming a semiconductor layer, an insulating layer, a conductive layer, and the like that can be applied to one embodiment of the present invention. A film forming apparatus will be described.
[0096] <CVD and ALD Film Deposition> Conventional CVD deposition equipment requires a precursor gas for the reaction during deposition. One or more of the above are simultaneously supplied to the chamber. Precursors for the reaction are introduced into the chamber in sequence, and the sequence of gas introduction is repeated. For example, each switching valve (also called a high-speed valve) is turned on and off. Two or more precursors are supplied to the chamber in sequence by switching between them, and multiple precursors are mixed. To avoid dust, an inert gas (such as argon or nitrogen) is placed after the first precursor. In addition, instead of introducing an inert gas, the first precursor is introduced. Thus, after the first precursor is evacuated, the second precursor can be introduced.
[0097] FIG. 8(A), FIG. 8(B), FIG. 8(C), and FIG. 8(D) show the film formation process by the ALD method. The precursor 601 is adsorbed onto the surface of the substrate (see FIG. 8(A)) and a first monolayer is formed. (See FIG. 8(B)). At this time, metal atoms contained in the precursor are present on the substrate surface. The metal atom can bond with the hydroxyl group. The second precursor introduced after the first precursor 601 is pumped out may be 8C), the second monolayer is laminated onto the first monolayer to form a thin layer. A film is formed (see Figure 8(D)). For example, if the second precursor contains an oxidizing agent, In the case of the first precursor, the metal atom or the alkyl group bonded to the metal atom is present in the first precursor. A chemical reaction occurs between the metal and the oxidizing agent, forming an oxide film.
[0098] In addition, the ALD method is a film formation method based on surface chemical reactions, and the precursor is absorbed on the film formation surface. The self-limiting mechanism works by adhering to the surface of the metal, and the metal is formed into a single layer. For example, trimethylaluminum The precursor reacts with the hydroxyl group (OH group) present on the surface to be coated. Since only surface reactions occur due to heat, the precursors come into contact with the surface to be deposited and transfer thermal energy. Using this gas, metal atoms in the precursor can be adsorbed onto the surface to be filmed. The precursor has a high vapor pressure, is thermally stable before film formation, and does not self-decompose. It has the characteristics of rapid chemical adsorption to the substrate. In addition, the precursor is introduced as a gas, Therefore, the first precursor and the second precursor, which are introduced alternately, have time to diffuse sufficiently. If this could be achieved, it would be possible to form a film with good coverage even in areas with high aspect ratio unevenness. It is possible.
[0099] In addition, in the ALD method, the gas introduction order is controlled and repeated multiple times until the desired thickness is achieved. By repeating the process, a thin film with excellent step coverage can be formed. Since the number of times can be adjusted, precise film thickness adjustment is possible. By increasing the temperature, the film formation speed can be increased and the impurity concentration in the film can be reduced. can.
[0100] There are two types of ALD: ALD using heat (thermal ALD) and ALD using plasma (plasma ALD). In the thermal ALD method, the precursor reacts using thermal energy. In the plasma ALD method, the precursor reaction is carried out in a radical state.
[0101] The ALD method can deposit extremely thin films with high precision. Surface coating can be achieved even on uneven surfaces. The rate is high and the film density is high.
[0102] In addition, the thermal ALD method is free of plasma damage, so it is possible to suppress the occurrence of defects in the film. This can be done.
[0103] Plasma ALD In addition, by forming a film using the plasma ALD method, compared to the ALD method using heat (thermal ALD method), The plasma ALD method can form films at temperatures even lower than 100 degrees. The deposition rate can be maintained without decreasing. Because the plasma can generate radicals, it is possible to form films of not only oxides but also nitrides. can be done.
[0104] In addition, the plasma ALD method can increase the oxidizing power of the oxidizing agent. This increases the oxidizing power of the oxidizing agent. When performing the above, the precursor remaining in the film or the organic components desorbed from the precursor are reduced. It is also possible to reduce the amount of carbon, chlorine, hydrogen, etc. in the film, and the impurity concentration It is possible to have a film with a low
[0105] In addition, when a light-emitting element (such as an organic EL element) is used as a display element, if the process temperature is high, However, there is a risk that the deterioration of the light-emitting element will be accelerated. Since the process temperature can be lowered, deterioration of the light emitting element can be suppressed.
[0106] In addition, when performing plasma ALD, inductively coupled plasma (ICP) is used to generate radical species. This uses a physically coupled plasma. It can be generated in a state separate from the substrate, and can be applied to the substrate or the film on which the protective film is formed. It can reduce the plasma damage.
[0107] As a result of the above, by using the plasma ALD method, the process temperature can be lowered compared to other film formation methods. The surface coverage can be increased, and the side surface of the substrate can be easily coated with the This film can be formed, which can prevent water from entering from the outside. This improves the reliability of the driver operation of the peripheral circuits at the edge of the panel (transistor To improve the reliability of the display characteristics, stable operation is possible even with a narrow frame. do.
[0108] <<Explanation about ALD equipment>> FIG. 9(A) shows an example of a film formation apparatus using the ALD method. A film forming chamber (chamber 1701), a raw material supply unit 1711a, a raw material supply unit 1711b, High-speed valves 1712a and 1712b, which are flow rate controllers, and a raw material inlet 1713 a, a raw material inlet 1713b, a raw material outlet 1714, and an exhaust device 1715. The raw material inlet 1713a and the raw material inlet 1713b installed in the member 1701 are connected to a supply pipe or The raw material supply unit 1711a and the raw material supply unit 1711b are connected to each other via valves. The raw material discharge port 1714 is connected to an exhaust device 1715 via a discharge pipe, a valve, and a pressure regulator. It has been done.
[0109] Inside the chamber is a substrate holder 1716 equipped with a heater. A substrate 1700 is provided on which the film is to be deposited.
[0110] In the raw material supply units 1711a and 1711b, solid A precursor is formed from a solid or liquid raw material. Supply unit 1711b may be configured to supply a gas precursor.
[0111] In addition, although an example in which two raw material supply units 1711a and 1711b are provided is shown, There is no particular limitation, and three or more valves may be provided. 12b can be precisely controlled in time and can supply either a precursor or an inert gas. The high-speed valve 1712a and the high-speed valve 1712b supply the precursor. It can also be said to be a flow rate controller for an inert gas.
[0112] In the film forming apparatus shown in FIG. 9(A), a substrate 1700 is loaded onto a substrate holder 1716. After the bar 1701 is sealed, the substrate 1700 is heated by the heater of the substrate holder 1716. is set to a desired temperature (for example, 100° C. or higher or 150° C. or higher), a precursor is supplied, and Exhaust by the exhaust device 1715, supply of inert gas, and exhaust by the exhaust device 1715 By repeating this process, a thin film is formed on the substrate surface.
[0113] In the film forming apparatus shown in FIG. 9(A), the raw material supply units 1711a and 1711b are provided with By appropriately selecting the raw materials (volatile organometallic compounds, etc.), hafnium, aluminum, Oxides containing one or more elements selected from the group consisting of tungsten, tantalum, zirconium, etc. (composite oxides) Specifically, an insulating layer containing hafnium oxide can be formed. an insulating layer including aluminum oxide; and hafnium silicate. or an insulating layer comprising aluminum silicate. In addition, the raw materials provided in the raw material supply units 1711a and 1711b can be By appropriately selecting the material (volatile organometallic compound, etc.), the tungsten layer, titanium layer It is also possible to deposit thin films such as metal layers, or nitride layers, such as titanium nitride layers.
[0114] For example, when a hafnium oxide layer is formed using a deposition apparatus that uses the ALD method, a solvent and liquids containing hafnium precursor compounds (hafnium alkoxides, tetrakisdimethyl A precursor made by vaporizing hafnium amide (such as TDMAH), Two types of gases are used: oxidant and ozone (O3). The first precursor supplied from the raw material supply unit 1711b is TDMAH. The second precursor is ozone. The chemical formula for tetrakisdimethylamidohafnium is The material is Hf[N(CH3)2]4. Other materials include tetrakis(ethylmethyl) Nitrogen has the function of eliminating the charge trapping level. Therefore, the precursor containing nitrogen can produce hafnium oxide with a low charge trapping state density. A film can be formed.
[0115] When forming an aluminum oxide layer using a deposition system that uses the ALD method, the solvent and the aluminum The precursor is a vaporized liquid containing a tritium precursor compound (e.g., TMA) and an oxidizer. In this case, two types of gases, H2O and H2O, are used. The precursor is TMA, and the second precursor supplied from the raw material supply unit 1711b is H2 O. The chemical formula for trimethylaluminum is Al(CH3)3. The material liquid is tris(dimethylamido)aluminum, triisobutylaluminum, Aluminum tris(2,2,6,6-tetramethyl-3,5-heptanedionate) ) etc.
[0116] <Multi-chamber manufacturing equipment> Also, a multi-chamber manufacturing apparatus having at least one film forming apparatus shown in FIG. An example is shown in FIG.
[0117] The manufacturing apparatus shown in FIG. 9(B) can continuously form a laminated film without exposing it to the air. The aim is to prevent impurities from being mixed in and improve throughput.
[0118] The manufacturing apparatus shown in FIG. 9(B) includes a load chamber 1702, a transfer chamber 1720, a processing chamber 1703, and a forming chamber 1704. The device has at least a chamber 1701 which is a membrane chamber, and an unloading chamber 1706. The chambers of the equipment (including the load chamber, processing chamber, transfer chamber, deposition chamber, unload chamber, etc.) In order to prevent moisture from adhering, the container is filled with an inert gas (such as nitrogen gas) with a controlled dew point. It is preferable to reduce the pressure and desirably maintain the reduced pressure.
[0119] Additionally, chambers 1704 and 1705 utilize the same ALD method as chamber 1701. It may be a film forming apparatus, a film forming apparatus using a plasma CVD method, or a sp The deposition apparatus may be a deposition apparatus using a deposition method, or a metal organic chemical vapor deposition (MOCVD) method. Organic Chemical Vapor Deposition (TCCVD) method The deposition apparatus may be a deposition apparatus that uses the same.
[0120] For example, the chamber 1704 may be a film forming device that uses a plasma CVD method. The following is an example of a deposition system using the MOCVD method to deposit a multilayer film. show.
[0121] In FIG. 9B, the top view of the transfer chamber 1720 is shown as an example of a hexagon. If necessary, a manufacturing device having a polygonal shape or more and connected to more chambers may be used. In addition, in FIG. 9B, the top surface shape of the substrate is shown as a rectangle, but this is not particularly limited. Although FIG. 9B shows an example of a single-wafer type, a batch type in which a film is formed on multiple substrates at once may also be used. The deposition apparatus may be a deposition apparatus as described above.
[0122] 《Large area ALD film deposition equipment》 In addition, the use of plasma ALD makes it possible to form films on large-area substrates. 1(A) and (B) are schematic diagrams of another configuration of the ALD deposition apparatus. The case is introduced into the chamber 820 from the inlet 810 and is then heated through the plasma source 830. Thus, film formation can be performed on the substrate 800 by the ALD method from above and below. The source 830 may be located inside the chamber or outside the chamber. As a deposition method, the film can be deposited by fixing it in a chamber as shown in Figure 10(A). As shown in Figure 10(B), the film can be formed while the substrate is moving in an in-line system. By using the plasma ALD method, it is possible to form films over large areas with high throughput.
[0123] In order to form a uniform film on the side surface of the display panel, the display panel is provided with a susceptor or the like. Alternatively, the display panel substrate 100 and the cassette jig may be brought into point contact or line contact. Alternatively, surface contact may be made.
[0124] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0125] (Embodiment 4) In this embodiment, the display devices described in the first and second embodiments will be described in detail with reference to the drawings. explain.
[0126] 11A and 11B are a top view and a cross-sectional view of a display device. 1(A) shows a display panel 20, a display area 21, a peripheral circuit 22, and an FPC 42. A representative configuration is shown.
[0127] In Fig. 11(B), the dashed lines A-A', B-B', C-C', and DD in Fig. 11(A) are shown. A-A' shows the peripheral part of the display device, and B-B' shows the peripheral circuit part. The area between CC' indicates the display area, and the area between D and D' indicates the connection part with the FPC.
[0128] "Transistors 50 and 52" The transistor 50 includes a conductive layer 120, an insulating layer 130, an insulating layer 131, a semiconductor layer 140, and a conductive The conductive layer 150, the conductive layer 160, and the insulating layer 170 may be included. The transistor 52 can be configured in a similar manner. An edge layer 181 or an insulating layer 182 may be added.
[0129] Dual gate structure In addition, a modified transistor 55 may be used instead of the transistor 50. 5. The transistor 55 shown in FIG. 35 has a dual gate structure. It is characterized by:
[0130] 35A, 35B, and 35C are a top view and a cross-sectional view of a transistor 55. FIG. 35A is a top view of the transistor 55, and FIG. FIG. 35(C) is a cross-sectional view taken along the dashed line YY in FIG. 35(A). 35(A) is a cross-sectional view of the substrate 100 and the insulating layer 11 for clarity. 0, insulating layer 130, insulating layer 170, insulating layer 180, etc. are omitted.
[0131] The transistor 55 shown in FIGS. 35(A) to 35(C) has the same structure as the transistor 50. In addition, the conductive layer 120 includes the insulating layer 130, the insulating layer 170, and the insulating layer 1 It is also possible to adopt a configuration in which the conductive layer 520 is connected to the opening 530 of the insulating film 80 .
[0132] Conductive layer 520 The conductive layer 520 is a conductive film that is transparent to visible light or a conductive film that is reflective to visible light. As the conductive film having a visible light transmitting property, the following conductive film can be used. The same material as the conductive layer 190 can be used, for example, indium (In), zinc (Z It is recommended to use a material containing one of the following elements: tin (Sn), tin (Tn), and tin (Sn). As a light-transmitting conductive film, typically, indium tin oxide or tungsten oxide is used. Indium oxide containing tungsten oxide, indium zinc oxide containing titanium oxide Indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc oxide, Conductive oxides such as indium tin oxide containing silicon dioxide can be used.
[0133] Alternatively, the conductive layer 520 may be a conductive film having a reflectivity to visible light, as described below. The same materials as those in 220 can be used.
[0134] As shown in FIG. 35C, the side surface of the semiconductor layer 140 and the conductive layer 142 are in contact with each other in the channel width direction. The insulating layer 170 and the insulating layer 130 face each other in the semiconductor layer 140. Since carriers flow not only at the interface of the semiconductor layer 140 but also inside the semiconductor layer 140, Therefore, the amount of carrier movement in the transistor 55 increases. As the on-current of the conductive layer 520 increases, the field effect mobility also increases. Since the semiconductor layer 140 is affected by the side surface or the edge portion including the side surface and the vicinity thereof, This can suppress the occurrence of parasitic channels at the sides or ends of 140.
[0135] In addition, the transistor shown in FIG. 35 can be used for a large display device or a high-definition display device by providing the transistor in a pixel portion. Even if the number of wirings increases in such a display device, it is possible to reduce the signal delay in each wiring. It is possible to suppress display defects such as display unevenness.
[0136] The transistors 52 in the peripheral circuits (gate drivers, etc.) all have the same structure. In addition, the pixel portion may have a plurality of transistors. The rotors 50 may all have the same structure, or may have two or more different structures.
[0137] Alternatively, the transistor described in this embodiment may be a transistor including an oxide semiconductor. However, one embodiment of the present invention is not limited to this. Alternatively, depending on the situation, one embodiment of the present invention may be a semiconductor device using a semiconductor material other than an oxide semiconductor. A transistor may also be used.
[0138] <Reflective LCD panel> As a display panel mounted on the display device, a reflective liquid crystal panel as shown in FIG. 11(B) is used. The display device 10 shown in FIG. 11B uses liquid crystal elements as display elements. The display device 10 includes a polarizing plate 103, a polarizing plate 303, a protective group Plate 105, protection substrate 302, adhesive layer 373, adhesive layer 374, adhesive layer 375, and adhesive layer 3 76. In order to realize a reflective liquid crystal panel, a part or all of the pixel electrodes In this case, it is sufficient if the electrode functions as a reflective electrode (as will be described later). In this case, it is possible to provide a memory circuit such as an SRAM under the reflective electrode. , and power consumption can be further reduced.
[0139] Other examples of LCD panels include transmissive (described below), semi-transmissive, direct-view, and projection types. You can also be there.
[0140] <<Substrate 100>> There is no particular restriction on the material of the substrate 100, but it should be at least strong enough to withstand the subsequent heat treatment. The substrate 100 must be heat resistant. It is also preferable that the substrate 100 has high light transmittance.
[0141] The substrate 100 may be made of an organic material, an inorganic material, or a composite material of an organic material and an inorganic material. For example, inorganic materials such as glass, ceramics, and metals can be used for the substrate 100. can be done.
[0142] Specifically, non-alkali glass, soda-lime glass, potash glass, or crystal glass. etc. can be used for the substrate 100. An inorganic oxide film, an inorganic nitride film, or an inorganic oxynitride film can be used. A film or the like can be used for the substrate 100. For example, silicon oxide, silicon nitride, oxide, Silicon nitride, alumina, etc. can be used for the substrate 100. Also, stainless steel or Alternatively, the substrate 100 may be made of a material such as silicon or aluminum.
[0143] Additionally, the substrate 100 may be a single layer material or a multi-layer laminate material. For example, a material that is laminated with a base material and an insulating film that prevents the diffusion of impurities contained in the base material is called a substrate. Specifically, it can be used to prevent the diffusion of impurities contained in glass. A silicon oxide layer, a silicon nitride layer, a silicon oxynitride layer, or the like is preferably formed. A material in which several films are laminated can be applied to the substrate 100. Alternatively, a material made of resin and an impermeable material that is permeable to the resin can be applied. A silicon oxide film, a silicon nitride film, a silicon oxynitride film, or the like is laminated to prevent the diffusion of impurities. The resulting material can be applied to a substrate 100 .
[0144] The above-mentioned substrates that can be applied to the substrate 100 can also be applied to the substrate 300.
[0145] Insulating layer 110 The insulating layer 110 having a function as a base film is made of silicon oxide, silicon oxynitride, Silicon nitride, silicon oxide nitride, gallium oxide, hafnium oxide, yttrium oxide, The insulating layer 110 is formed using aluminum oxide, aluminum oxynitride, or the like. Silicon nitride, gallium oxide, hafnium oxide, yttrium oxide, aluminum oxide By using ammonium hydrate or the like, impurities, typically alkali metals, water, hydrogen, etc., can be removed from the substrate 100. The diffusion into the semiconductor layer 140 can be suppressed. The insulating layer 110 is formed on the substrate 100. Moreover, the insulating layer 110 does not necessarily have to be formed.
[0146] Conductive layer 120 The conductive layer 120 having the function of a gate electrode is made of aluminum, chromium, copper, tantalum, or the like. , a metal element selected from titanium, molybdenum, nickel, iron, cobalt, and tungsten; Or an alloy containing the above-mentioned metal elements or an alloy combining the above-mentioned metal elements. In addition, the alloy is formed using one or more selected from manganese and zirconium. The conductive layer 120 may be formed using a single layer structure or a multi-layer structure. For example, a single layer structure of an aluminum film containing silicon, a manganese film, a single-layer structure of a copper film containing the above-mentioned, a two-layer structure of a titanium film laminated on an aluminum film, a titanium nitride film Two-layer structure with a titanium film laminated on top, and two-layer structure with a tungsten film laminated on a titanium nitride film , a two-layer structure in which a tungsten film is laminated on a tantalum nitride film or a tungsten nitride film, A two-layer structure is formed by laminating a copper film on a copper film containing fluorine, and a titanium film and an aluminum film on the titanium film. A three-layer structure is formed by laminating a copper film and then forming a titanium film on top of that, and then forming a manganese-containing copper film on top of that. There is also a three-layer structure in which a copper film is laminated and a manganese-containing copper film is formed on top of that. Aluminum, titanium, tantalum, tungsten, molybdenum, chromium, neodymium, steel Using an alloy film or a nitride film made of one or more selected from candium Good too.
[0147] Insulating layer 130 The insulating layer 130 also functions as a gate insulating film. , aluminum oxide, magnesium oxide, silicon oxide, silicon oxynitride, silicon nitride oxide Silicon, silicon nitride, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide One or more of lanthanum oxide, neodymium oxide, hafnium oxide and tantalum oxide. The insulating layer 130 may contain lanthanum (La), nitrogen, or di- The insulating layer 130 may contain impurities such as zirconium (Zr). For example, silicon oxynitride can be used.
[0148] Insulating layer 131 The gate insulating film can be formed by laminating an insulating layer 130 and an insulating layer 131 . The insulating layer 131 can be made of the same material as the insulating layer 130. For example, silicon nitride can be used for the insulating layer 131. The intrusion of hydrogen, water, and the like into the semiconductor layer 140 can be prevented.
[0149] Semiconductor layer 140 The semiconductor layer 140 is made of a metal oxide containing at least In or Zn. The area of the top surface of layer 140 is preferably equal to or smaller than the area of the top surface of conductive layer 120. It is.
[0150] <Oxide Semiconductor> The oxide semiconductor used for the semiconductor layer 140 is, for example, an In-Ga-Zn oxide. In-Al-Zn oxides, In-Sn-Zn oxides, In-Hf-Zn oxides , In-La-Zn oxide, In-Ce-Zn oxide, In-Pr-Zn oxide, In-Nd-Zn oxide, In-Sm-Zn oxide, In-Eu-Zn oxide, I n-Gd-Zn oxide, In-Tb-Zn oxide, In-Dy-Zn oxide, In -Ho-Zn oxide, In-Er-Zn oxide, In-Tm-Zn oxide, In- Yb-Zn oxide, In-Lu-Zn oxide, In-Sn-Ga-Zn oxide, I n-Hf-Ga-Zn oxide, In-Al-Ga-Zn oxide, In-Sn-Al- Zn-based oxide, In-Sn-Hf-Zn-based oxide, In-Hf-Al-Zn-based oxide, I An n-Ga-based oxide can be used.
[0151] In this case, the In-Ga-Zn oxide is an oxide having In, Ga, and Zn as main components. It means oxide, and the ratio of In, Ga, and Zn does not matter. Also, In, Ga, and Zn Metal elements other than those may be included.
[0152] When the semiconductor layer 140 is made of an In-M-Zn oxide, the sum of In and M is 1 When the atomic percentage of In is 0.00, the atomic percentage of In and M is preferably 25. atomic %, M is less than 75 atomic %, and more preferably In is 34 atomic %. tomic%, and M is less than 66 atomic%.
[0153] The semiconductor layer 140 has an energy gap of 2 eV or more, preferably 2.5 eV or more. The energy gap is preferably 3 eV or more. This allows the off-state current of the transistor 50 to be reduced.
[0154] The thickness of the semiconductor layer 140 is 3 nm to 200 nm, preferably 3 nm to 100 nm. It is more preferable to set the thickness to 3 nm or more and 50 nm or less.
[0155] The semiconductor layer 140 is an In-M-Zn oxide (wherein M is Al, Ga, Y, Zr, La, Ce, Ti , Ge, or Nd) to form In-M-Zn oxide. The atomic ratio of the metal elements in the sputtering target to be used may be a natural number, or M may be a natural number. For example, the atomic ratio of the metal elements in the target is In:M:Zn=1. :1:1, In:M:Zn=1:1:1.2, In:M:Zn=1:1:1.5, In: M:Zn=2:1:3, In:M:Zn=3:1:2, In:M:Zn=4:2:4.1 The atomic ratio of the metal elements in the semiconductor layer 140 is preferably The error is the atomic ratio of the metal elements contained in the sputtering target. Including a minus 40% variation. In addition, the target containing In-Ga-Zn oxide, preferably By using a polycrystalline target containing In-Ga-Zn oxide, the CAAC -OS(C Axis Aligned Crystalline Oxide Sem It is possible to form a silicon oxide semiconductor film and a microcrystalline oxide semiconductor film.
[0156] The hydrogen contained in the semiconductor layer 140 reacts with the oxygen that bonds with the metal atoms to form water, and Oxygen vacancies are formed in the lattice from which oxygen has been removed (or in the portion from which oxygen has been removed). When hydrogen enters the electron carrier, it can generate electrons. When it bonds with oxygen, which bonds with a metal atom, it may generate electrons, which act as carriers. Therefore, a transistor using an oxide semiconductor containing hydrogen has normally-on characteristics. It's easy to become.
[0157] For this reason, it is preferable that the semiconductor layer 140 has as little oxygen vacancy as possible and as little hydrogen as possible. Specifically, in the semiconductor layer 140, secondary ion mass spectrometry (SIMS:Se Hydrogen concentration obtained by condary ion mass spectrometry Degrees, 5 x 10 19atoms / cm 3 Less than or equal to 1×10 19 atoms / cm 3 Less than or equal to 5×10 18 atoms / cm 3 Less than or equal to 1× 10 18 atoms / cm 3 Less than or equal to 5×10 17 atoms / cm 3 below , and more preferably 1×10 16 atoms / cm 3 As a result, the transistor The transistor 50 has electrical characteristics in which the threshold voltage is positive (also called normally-off characteristics). do.
[0158] In addition, when the semiconductor layer 140 contains silicon or carbon, which is one of the Group 14 elements, As a result, oxygen vacancies increase in the semiconductor layer 140, causing the semiconductor layer 140 to become n-type. The concentrations of silicon and carbon at 40 (obtained by secondary ion mass spectrometry) were ×10 18 atoms / cm 3 Less than or equal to 2×10 17 atoms / cm 3 Below and As a result, the transistor 50 has electrical characteristics in which the threshold voltage is positive (normal This is also called the turn-off characteristic.
[0159] In addition, in the semiconductor layer 140, an alkali metal or is the concentration of alkaline earth metals, 1×10 18 atoms / cm 3 Below, preferably 2 x 1 0 16 atoms / cm 3 Alkali metals and alkaline earth metals are oxide semiconductors. When it bonds with a conductor, it can generate carriers, which increases the off-state current of the transistor. For this reason, the concentration of the alkali metal or alkaline earth metal in the semiconductor layer 140 As a result, transistor 50 has a positive threshold voltage. The semiconductor device has electrical characteristics (also called normally-off characteristics).
[0160] Furthermore, when the semiconductor layer 140 contains nitrogen, electrons that act as carriers are generated, and the carrier density increases. As a result, the transistor tends to have normally-on characteristics. Therefore, it is preferable that the nitrogen content in the semiconductor layer 140 is reduced as much as possible. For example, the nitrogen concentration obtained by secondary ion mass spectrometry is 5×10 18 atoms / cm 3 It is preferable to do the following:
[0161] By reducing the impurities in the semiconductor layer 140, the carrier density of the semiconductor layer 140 can be reduced. Therefore, the semiconductor layer 140 has a carrier density of 1×10 15 pieces / cm 3 below , preferably 1 x 10 13 pieces / cm 3 Less than 8×10, more preferably 11 pieces / cm 3 Not yet More preferably, 1×10 11 pieces / cm 3 less than 1×10 10 pieces / cm 3 Less than 1 x 10 -9 pieces / cm 3 That is all.
[0162] The semiconductor layer 140 is formed using an oxide semiconductor having a low impurity concentration and a low density of defect states. By using the above-mentioned method, a transistor having better electrical characteristics can be manufactured. The low impurity concentration and low defect level density (low oxygen vacancies) are called high purity intrinsic or real In terms of quality, it is called high-purity intrinsic. A high-purity intrinsic or substantially high-purity intrinsic oxide semiconductor is Since there are few carrier generation sources, it may be possible to reduce the carrier density. A transistor in which a channel region is formed in the semiconductor layer 140 formed using the oxide semiconductor. Transistors have electrical characteristics in which the threshold voltage is positive (also called normally-off characteristics). In addition, a highly pure intrinsic or substantially highly pure intrinsic oxide semiconductor is prone to defect formation. The trap level density may also be low due to the low level density. A transistor in which the semiconductor layer 140 is formed using a qualitatively high-purity intrinsic oxide semiconductor. The off-state current is extremely small, and the voltage between the source and drain electrodes (drain voltage) is 1 In the range from V to 10 V, the off-state current is below the measurement limit of the semiconductor parameter analyzer. , i.e. 1 × 10 -13 A characteristic of less than A can be obtained, and the characteristic fluctuation can be suppressed. It is possible.
[0163] Note that the transistor 50 using an oxide semiconductor for the semiconductor layer 140 has a When the voltage between the transistor and the drain is set to about 0.1V, 5V, or 10V, The off-current normalized by the channel width of the semiconductor device can be reduced to several yA / μm to several zA / μm. This becomes possible.
[0164] In the off state, the transistor 50 connected to the display element (for example, the liquid crystal element 80) By using transistors with extremely low leakage current, image signals can be retained. For example, the image signal writing rate can be increased to 11.6 μHz (1 day). A frequency of 0.28mHz (1 Hz) or more and less than 0.1Hz (0.1 times per second) is preferable. Images can be retained even if the frequency is more than 1Hz (once per hour) and less than 1Hz (once per second). This reduces the frequency of writing image signals. This can reduce the power consumption of the panel 20. Preferably, the frequency is 30 Hz (30 times per second) or more, and more preferably, 60 Hz (6 times per second). The frequency can be greater than or equal to 960Hz (960 times per second) and less than 960Hz (960 times per second).
[0165] For the above reasons, by using a transistor including an oxide semiconductor, it is possible to realize high reliability and low power consumption. A display panel with reduced power consumption can be manufactured.
[0166] In the case of a transistor using an oxide semiconductor, the semiconductor layer 140 is formed by sputtering or MOCVD (M etal Organic Chemical Vapor Deposition) method The film can be formed by the PLD (Pulse Laser Deposition) method, etc. When the semiconductor layer 140 is formed by sputtering, a large-area display device can be manufactured. It is possible.
[0167] The semiconductor layer 140 is a semiconductor layer made of silicon or silicon germanium. A semiconductor layer made of silicon or silicon germanium may be used as appropriate. The structure may be a crystalline structure, a polycrystalline structure, or a single crystal structure.
[0168] <Conductive layer 150, conductive layer 160> The conductive layer 150 and the conductive layer 160 are a source electrode, a drain electrode, or The conductive layer 150 and the conductive layer 160 function as electrodes of a capacitor. Chromium, copper, tantalum, titanium, molybdenum, nickel, iron, cobalt, tungsten or an alloy containing the above-mentioned metal elements or the above-mentioned metal elements. It is formed by using an alloy of manganese and zirconium. The conductive layer 150 may be formed using a metal element selected from a plurality of metal elements. The layer 160 may be a single layer structure or a laminated structure of two or more layers. Single layer structure of aluminum film, single layer structure of copper film containing manganese, titanium on aluminum film A two-layer structure in which a titanium film is laminated on a titanium nitride film, a two-layer structure in which a titanium film is laminated on a titanium nitride film, A two-layer structure in which a tungsten film is laminated on a tantalum nitride film or a tungsten nitride film is laminated on a tantalum nitride film. A two-layer structure in which a copper film is laminated on a manganese-containing copper film; A titanium film is laminated on the titanium film, an aluminum film is laminated on the aluminum film, and a titanium film is formed on the aluminum film. A three-layer structure is formed by laminating a copper film on a copper film containing manganese, and then laminating a copper film containing manganese on top of that. There are also three-layer structures that form aluminium, titanium, tantalum, tungsten, etc. , molybdenum, chromium, neodymium, and scandium. Alternatively, an alloy film or a nitride film may be used.
[0169] Insulating layer 170 The insulating layer 170 has a function of protecting the channel region of the transistor. , silicon oxide, silicon oxynitride, aluminum oxide, aluminum oxynitride, gas oxide Lithium, Gallium Oxide Nitride, Yttrium Oxide, Yttrium Oxide Nitride, Hafnium Oxide oxide insulating films such as hafnium oxide nitride; nitride insulating films such as silicon nitride and aluminum nitride; The insulating layer 170 may be a single layer or a laminated layer. .
[0170] Also, the insulating layer 170 is an oxide insulating layer containing more oxygen than the oxygen required for the stoichiometric composition. It is preferable to form the film by using a method that contains more oxygen than the stoichiometric composition. When the oxide insulating film containing oxygen is heated, some of the oxygen is released. The oxide insulating film containing more oxygen than the TDS (Thermal Desorption Spectroscopy analysis shows that the surface temperature of the film is between 100℃ and 700℃. or the amount of oxygen atoms released in the range of 100°C to 500°C is 1.0×10 18 atoms / cm 3 More than 3.0×10 20 atoms / cm 3 Acid that is greater than or equal to The oxygen contained in the insulating layer 170 is transferred to the semiconductor layer 140 by heat treatment. As a result, oxygen vacancies in the semiconductor layer 140 can be reduced.
[0171] Insulating layer 180 As the insulating layer 180, an insulating film having a blocking effect against oxygen, hydrogen, water, etc. is provided. The diffusion of oxygen from the semiconductor layer 140 to the outside and the diffusion of hydrogen and water from the outside to the semiconductor layer 140 For example, aluminum oxide, magnesium oxide, silicon oxide, etc. can be prevented from entering. Con, silicon oxide nitride, silicon nitride oxide, silicon nitride, gallium oxide, germanium oxide tungsten oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide, hafnium oxide An insulating film containing one or more of tungsten oxide and tantalum oxide can be used. The insulating layer 80 may be a laminate of the above materials. , zirconium (Zr), etc. may be contained as impurities.
[0172] Insulating layer 181 The insulating layer 181 has a flattening function. The insulating layer 181 is made of an inorganic material or an organic material. For example, silicon oxide, silicon oxynitride, aluminum oxide, etc. nium, aluminum oxide nitride, gallium oxide, gallium oxide nitride, yttrium oxide, Oxide insulating films such as yttrium oxide nitride, hafnium oxide, and hafnium oxide nitride, silicon nitride Silicon, aluminum nitride and other nitride insulating films, polyimide resin, acrylic resin, polyimide Resins with heat resistance such as amide resins, benzocyclobutene resins, polyamide resins, and epoxy resins. The insulating layer is formed using an organic material that has a high insulating property.
[0173] Insulating layer 182 As the insulating layer 182, an insulating film having a blocking effect against oxygen, hydrogen, water, etc. is provided. In addition to the insulating layer 180, oxygen diffuses from the semiconductor layer 140 to the outside, and oxygen diffuses from the outside to the semiconductor layer 140. It is possible to further prevent hydrogen, water, etc. from penetrating into the layer 140. For example, aluminum oxide, Magnesium oxide, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride , gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide The insulating film may include one or more of tantalum oxide, neodymium oxide, hafnium oxide, and tantalum oxide. The insulating layer 182 may be a laminate of the above materials. Even if it contains impurities such as lanthanum (La), nitrogen, and zirconium (Zr), good.
[0174] Liquid crystal element 80 The liquid crystal element 80 is driven in, for example, a Twisted Nematic (TN) mode. The liquid crystal element 80 includes a liquid crystal layer 390, a conductive layer 220, and a conductive layer 380. do.
[0175] Although not shown in FIG. 11, the conductive layers 220 and 380 are provided on the side in contact with the liquid crystal layer 390. , and an alignment film may be provided on each of them.
[0176] The liquid crystal layer 390 is sandwiched between the conductive layer 220 and the conductive layer 380. The orientation of the liquid crystal molecules can be controlled by the electric field generated. The method may be, for example, STN mode, VA mode, ASM (Axially Symmetry Mode), etc. etic Aligned Micro-cell) mode, OCB(Optical ly Compensated Birefringence mode, FLC (Fer ferroelectric Liquid Crystal) mode, AFLC (AntiF erroelectric Liquid Crystal) mode, MVA mode, P VA(Patterned Vertical Alignment) mode, IPS( In plane Switching mode or TBA (Transverse A display device driving method such as a bend alignment mode may also be used. In addition to the above mentioned driving method, ECB (Electrically Controlled Bias Circuit) LED Birefringence mode, PDLC (Polymer Dispersion) rsed Liquid Crystal) mode, PNLC (Polymer Net There are various modes such as the Liquid Crystal mode and the guest host mode. However, the present invention is not limited to this, and various liquid crystal elements and driving methods thereof can be used. Cut.
[0177] In addition, the liquid crystal element 80 is made of a liquid crystal composition containing a liquid crystal exhibiting a nematic phase and a chiral agent. In this case, a cholesteric phase or a blue phase e) Liquid crystals that exhibit a blue phase have a short response time of 1 msec or less, and are optically Since it is isotropic, no alignment treatment is required and the viewing angle dependency is small.
[0178] Conductive layer 220 The conductive layer 220 that reflects visible light may be made of, for example, aluminum, gold, platinum, silver, or nickel. tungsten, chromium, molybdenum, iron, cobalt, copper, or gold such as palladium Metallic materials or alloys containing these metallic materials can be used. Lanthanum, neodymium, germanium, etc. may be added to gold. Aluminum and titanium alloys, aluminum and nickel alloys, aluminum and neodymium alloys , aluminum, nickel, and lanthanum alloys (Al-Ni-La) Alloys containing palladium (aluminum alloys), silver and copper alloys, silver, palladium and copper alloys (Ag- Pd-Cu, also written as APC), formed using an alloy containing silver, such as an alloy of silver and magnesium An alloy containing silver and copper is preferable because of its high heat resistance. By laminating a metal film or a metal oxide film in contact with the aluminum alloy film, the oxidation of the aluminum alloy film can be prevented. The metal film and the metal oxide film can be made of titanium, titanium oxide, or the like. In addition, a conductive film that transmits visible light and a film made of a metal material are laminated. For example, a laminated film of silver and ITO, a laminated film of an alloy of silver and magnesium and ITO, etc. can be used.
[0179] <<Capacitive element 60, capacitive element 62>> The capacitance element 60 includes a conductive layer 120, an insulating layer 130, an insulating layer 131, a conductive layer 160, The conductive layer 120 can function as one electrode of the capacitor 60. The conductive layer 160 functions as the other electrode of the capacitor 60. Between the conductive layer 160 and the insulating layer 130, an insulating layer 131 is provided. The capacitance element 62 can be configured in the same manner as the capacitance element 60.
[0180] Conductive layer 380 The conductive layer 380 is formed using a conductive film that transmits visible light. Examples of the conductive film having transparency include indium (In), zinc (Zn), and tin (Sn It is preferable to use a material containing one selected from the group consisting of those having transparency to visible light. The conductive film is typically made of indium tin oxide or indium containing tungsten oxide. Oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide Indium tin oxide containing titanium oxide, indium zinc oxide, silicon oxide A conductive oxide such as indium tin oxide can be used.
[0181] Insulating layer 330 The insulating layer 330 has a planarizing function. The insulating layer 330 is made of an inorganic material or an organic material. For example, silicon oxide, silicon oxynitride, aluminum oxide, etc. nium, aluminum oxide nitride, gallium oxide, gallium oxide nitride, yttrium oxide, Oxide insulating films such as yttrium oxide nitride, hafnium oxide, and hafnium oxide nitride, silicon nitride Silicon, aluminum nitride and other nitride insulating films, polyimide resin, acrylic resin, polyimide Resins with heat resistance such as amide resins, benzocyclobutene resins, polyamide resins, and epoxy resins. The insulating layer is formed using an organic material that has a high insulating property.
[0182] 《Colored layer 360》 The colored layer 360 is a colored layer that transmits light of a specific wavelength band. For example, red, green, and blue A color filter that transmits light in the yellow or red wavelength band can be used. The color layers are made of various materials using printing, inkjet, and photolithography methods. The white pixels are formed at the desired positions by etching or other methods. A transparent or white resin may be disposed on top of the electrode.
[0183] 《Light blocking layer 18》 A material having a light-shielding property can be used for the light-shielding layer 18. For example, a resin in which a pigment is dispersed, In addition to resin containing dye, inorganic films such as black chrome films can be used for the light-shielding layer 18. The light-shielding layer 18 is made of a composite oxide containing a solid solution of inorganic oxides, inorganic oxides, or a mixture of inorganic oxides. can be used.
[0184] "Spacer 240" An insulating material can be used for the spacer 240. For example, an inorganic material, an organic material, or For example, a laminate of inorganic and organic materials can be used. Films containing silicon or silicon nitride, acrylic, polyimide, or photosensitive resin etc. can be applied.
[0185] 《Adhesive layer 370》 The adhesive layer 370 may be made of an inorganic material, an organic material, or a composite material of an inorganic material and an organic material. can be done.
[0186] For example, photocurable adhesives, reaction curable adhesives, heat curable adhesives or / and anaerobic adhesives. The adhesive layer 370 may be made of an organic material such as a fluorine-containing adhesive. or in combination.
[0187] The photocurable adhesive is, for example, an adhesive that is cured by ultraviolet light, electron beams, visible light, infrared light, etc. say.
[0188] Specifically, epoxy resin, acrylic resin, silicone resin, phenolic resin, polyimide resin, etc. resin, imide resin, PVC (polyvinyl chloride) resin, PVB (polyvinyl butyrate) Adhesives containing resin, EVA (ethylene vinyl acetate) resin, silica, etc. are used for the adhesive layer. It can be used for 370.
[0189] In particular, when using a light-curing adhesive, the material hardens quickly, shortening the work time. In addition, since curing starts by irradiating light, the effect of the film formation process is suppressed. In addition, it can be cured at low temperatures, making it easy to control the working environment. As described above, by using a light-curing adhesive, the process can be shortened and processing can be performed at low cost. .
[0190] FPC42 The FPC 42 is electrically connected to the conductive layer 160 via the anisotropic conductive film 510. The signals are supplied from the FPC 42 to a driving circuit having a transistor 52 and a capacitance element 62. It is possible.
[0191] <Insulating layer 181 and insulating layer 182 having unevenness> The insulating layer 181 and the insulating layer 182 may have irregularities in the pixel region. When external light is incident on the conductive layer 220, the reflected light can be scattered. It can prevent shots.
[0192] <Insulating layer 181 with no unevenness, insulating layer 182, and scattering film 304> Alternatively, the insulating layer 181 and the insulating layer 182 may not have unevenness. 1 shows a cross-sectional view of another configuration of the display device. In this case, the visible side of the substrate 300 (the front side of the display device) 11.) By using a scattering film 304 and an adhesive layer 377, the same effect as that shown in FIG. can.
[0193] <Another configuration 1 of the shape of the substrate edge of the display device> FIG. 13 shows a cross-sectional view of a display device having a different structure from that shown in FIG. 11(B). ) the substrate edge is formed without any irregularities, and the protective film 23 can be formed by the ALD method. can.
[0194] <Another configuration 2 of the shape of the substrate edge of the display device> In addition, when forming the protective film 23 on the display device 10, it is possible to selectively form it on the front and side surfaces. 14 and 15 show cross-sectional views of the display device.
[0195] In FIG. 14, the protective film 23 is formed on the back surface side (the substrate 100 side) as shown in FIG. For example, in the configuration shown in FIG. It is possible to suppress the formation of the protective film 23 on the back surface and the upper surface side of the FPC 42. In this case, the protective film is formed in a wraparound manner, as in the region 13 at the edge of the substrate 100 or 300. Alternatively, as shown in FIG. 15, a protective film may be formed on the back side by using the method shown in FIG. It is possible to provide a region 14 that is not exposed to the light.
[0196] <Another configuration of the display device substrate edge shape 3> 16, 17, and 18 show examples of the display device 10 having a configuration different from that described above. The configuration example of FIG. 16 is a structure using the configuration of FIG. 4(A), and the configuration example of FIG. 17 is a structure using the configuration of FIG. 18 is a structure using the configuration of FIG. 5(A). In either case, the provision of the protective film 23 can prevent the intrusion of atmospheric components such as water, and provides insulation. The structure may not have layer 182 .
[0197] In addition, the structure of FIG. 18 has a smaller area for the substrate 300 than for the substrate 100, so that the protection The film 23 can be formed more uniformly.
[0198] <Alternative configuration 4 of the shape of the substrate edge of the display device> FIG. 19 shows another example of the configuration of the display device 10. FIG. 19 shows a structure using FIG. By providing the protective film 23, a structure without the insulating layer 181 and the insulating layer 182 can be obtained. can.
[0199] <Combination with a display device's touch sensor> The display device 10 can be combined with a touch sensor to form a touch panel. 20 and 21 show cross-sectional views of a touch panel. As shown in FIG. 20, the electrodes for the touch sensor The conductive layers 410 and 430 can be used as wirings. The conductive layer 380 used in the display panel can be used for the wiring of the touch sensor. By combining these, an in-cell type touch panel can be formed. The electrodes may be formed on the visible side (front side) of the substrate 300 or on the inside (display element side). This is also fine.
[0200] <Conductive Layer 410, Conductive Layer 430> The conductive layer 410 may be made of aluminum, chromium, copper, tantalum, titanium, molybdenum, or nickel. A metal element selected from the group consisting of iron, cobalt, and tungsten, or a metal element containing the above-mentioned metal elements. It is formed by using an alloy of the above-mentioned metal elements or an alloy combining the above-mentioned metal elements. The present invention may be formed using one or more metal elements selected from the group consisting of tungsten, fluorine, zirconium, and tungsten. good.
[0201] The conductive layer may have a single layer structure or a laminated structure of two or more layers. A single layer structure of an aluminum film containing manganese, a single layer structure of a copper film containing manganese, and a single layer structure of a copper film on an aluminum film. Two-layer structure with titanium film laminated on titanium nitride film, two-layer structure with titanium film laminated on titanium nitride film, titanium nitride Two-layer structure with tungsten film laminated on the film, tantalum nitride film or tungsten nitride film Two-layer structure with a tungsten film laminated on top, and two-layer structure with a copper film laminated on a manganese-containing copper film A titanium film is laminated on the titanium film, an aluminum film is laminated on the titanium film, and a titanium film is formed on the aluminum film. A three-layer structure consisting of a copper film containing manganese, a copper film is laminated on top of the manganese-containing copper film, and a manganese-containing There are three-layer structures in which a copper film is formed. In addition, titanium, tantalum, and tungsten are added to aluminum. One or more of the following elements may be combined: zinc, molybdenum, chromium, neodymium, and scandium. A combined alloy film or a nitride film may also be used.
[0202] Alternatively, it may be used for conductive films such as the conductive layer 410, that is, wiring and electrodes constituting a touch panel. Examples of materials that can be used include transparent conductive films containing indium oxide, tin oxide, zinc oxide, etc. (For example, ITO, etc.) are also used for wiring and electrodes that make up touch panels. For example, it is preferable that the material has a low resistance. Aluminum, carbon nanotubes, graphene, metal halides (silver halides, etc.) In addition, a plurality of very thin (e.g., a diameter of a few nanometers) Metal nanowires made of a conductor may be used. Metal meshes in a shape of a nanowire may be used. Examples include Ag nanowires and Cu nanowires. , Al nanowires, Ag mesh, Cu mesh, Al mesh, etc. may also be used. For example, when Ag nanowires are used for the wiring and electrodes that make up a touch panel, The transmittance can be set to 89% or more, and the sheet resistance can be set to 40Ω / □ or more and 100Ω / □ or less. Cut.
[0203] It is also an example of a material that can be used for the wiring and electrodes that make up the above-mentioned touch panel. Metal nanowires, metal meshes, carbon nanotubes, graphene, etc., which are used for visible light Since the transmittance is high in the Also, a similar film may be used for the conductive layer 430. do.
[0204] <Insulating layer 420, insulating layer 440> The insulating layer 420 can be made of an inorganic material or an organic material. Silicon oxide, silicon oxynitride, aluminum oxide, aluminum oxynitride, gallium oxide , gallium oxide nitride, yttrium oxide, yttrium oxide nitride, hafnium oxide, Oxide insulating film such as hafnium nitride, silicon nitride, aluminum nitride, etc. , polyimide resin, acrylic resin, polyimide amide resin, benzocyclobutene resin, It is made of heat-resistant organic materials such as polyamide resin and epoxy resin. The edge layer 440 may be a film similar to that used for 420 .
[0205] <Transmissive LCD panel> In addition, a transmissive liquid crystal panel is used as the display panel mounted on the display device as shown in FIG. The display device shown in FIG. 22 uses a liquid crystal element 81 as a display element. The display device includes a polarizing plate 103, a polarizing plate 303, a backlight 104, and an adhesive. The polarizing plate 303 has a protective substrate 30 on the viewing side. 2 is provided and bonded with an adhesive layer 376. Also, a reflective type such as a transistor The parts that are shared with the liquid crystal panel can be formed in the same manner as the reflective liquid crystal panel. .
[0206] Liquid crystal element 81 The liquid crystal element 81 is driven in FFS (Fringe Field Switching) mode. The liquid crystal element 81 includes a liquid crystal layer 390 and a conductive layer 190. When the liquid crystal layer 390 receives a lateral electric field from the conductive layer 190, the liquid crystal layer 390 The orientation of the molecules can be controlled.
[0207] Conductive layer 190 The conductive layer 190 is formed using a conductive film that transmits visible light. Examples of the conductive film having transparency include indium (In), zinc (Zn), and tin (Sn It is preferable to use a material containing one selected from the group consisting of those having transparency to visible light. The conductive film is typically made of indium tin oxide or indium containing tungsten oxide. Oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide oxide, indium tin oxide, indium zinc oxide, silicon or oxide A conductive oxide such as indium tin oxide containing silicon can be used.
[0208] <<Capacitive element 61, Capacitive element 63>> The capacitance element 61 includes a conductive layer 400, an insulating layer 180, and a conductive layer 190. The conductive layer 400 functions as one electrode of the capacitor 61. The conductive layer 400 has a function as the other electrode of the conductive layer 61. The capacitive element 63 is configured in the same manner as the capacitive element 61. can be done.
[0209] Conductive layer 400 The transistor 50 may be a transistor in which an oxide semiconductor is used for the semiconductor layer 140. By doing so, the conductive layer 400 can be formed of the same material as the semiconductor layer 140. In this case, the conductive layer 400 is formed by processing a film that is formed simultaneously with the semiconductor layer 140. , the conductive layer 400 may have a similar crystal structure to the semiconductor layer 140 or a different crystal structure. In addition, the film formed simultaneously with the semiconductor layer 140 may have impurities or oxygen vacancies. Thus, the conductive layer 400 is formed. Representative examples of impurities contained in the layer 400 include rare gases, hydrogen, boron, nitrogen, fluorine, and arsenic. Examples of noble gases are helium, neon, argon, and aluminium. In addition, examples of the conductive layer 400 having conductivity include However, one aspect of the present invention is not limited thereto. Therefore, the conductive layer 400 does not necessarily have to be conductive. may have similar properties as the semiconductor layer 140.
[0210] From the above, the semiconductor layer 140 and the conductive layer 400 are both formed on the insulating layer 130. The impurity concentration is different. Specifically, the impurity concentration of the conductive layer 400 is different from that of the semiconductor layer 140. For example, in the semiconductor layer 140, the hydrogen concentration obtained by secondary ion mass spectrometry is Degrees are 5 x 10 19 atoms / cm 3 Less than or equal to 5×10 18 atoms / cm 3 Less than or equal to 1×10 18 atoms / cm 3 Less than or equal to 5×10 17 at oms / cm 3 Less than or equal to 1×10 16 atoms / cm 3 On the other hand, In the electrode layer 400, the hydrogen concentration obtained by secondary ion mass spectrometry is 8×10 19 a toms / cm 3 More than 1×10 20 atoms / cm 3 More than 5, preferably ×10 20atoms / cm 3 The above is the case. In addition, compared to the semiconductor layer 140, the conductive layer 4 00 contains twice as much hydrogen, or 10 times more.
[0211] In addition, the oxide semiconductor film formed simultaneously with the semiconductor layer 140 is exposed to plasma. The oxide semiconductor film can be damaged and oxygen vacancies can be formed. When a film is formed on the conductive film by plasma CVD or sputtering, an oxide semiconductor The film is exposed to a plasma to generate oxygen vacancies or to form openings in the insulating layer 170. In the etching treatment for forming the oxide semiconductor film, the oxide semiconductor film is exposed to plasma, and oxygen deficiency is reduced. Alternatively, when the oxide semiconductor film is heated in a mixed gas of oxygen and hydrogen, hydrogen, a rare gas, or Exposure to plasma such as ammonia creates oxygen vacancies. By adding impurities to the oxide semiconductor film, oxygen vacancies are formed. The method of adding impurities includes ion doping, ion implantation, and plating. In the case of plasma processing, the plasma is heated in a gas atmosphere containing the impurities to be added. By generating a plasma and performing plasma processing, the accelerated impurity ions are converted into oxides. By colliding with the semiconductor film, oxygen vacancies can be formed in the oxide semiconductor film.
[0212] An impurity, for example, hydrogen, is added to an oxide semiconductor film in which oxygen vacancies are formed by the addition of an impurity element. When oxygen is present, hydrogen enters the oxygen vacancy site and a donor level is formed near the conduction band. As a result, the conductivity of the oxide semiconductor film is increased and the oxide semiconductor film becomes a conductor. The semiconductor layer 140 can be called an oxide conductor film. It can be said that the conductive layer 400 is formed of an oxide conductor film. It can be said that the conductive layer 400 is formed using an oxide semiconductor film having high conductivity. It can also be said that it is formed of a high-temperature metal oxide film.
[0213] The insulating layer 180 preferably contains hydrogen. Therefore, when the insulating layer 180 contains hydrogen, the hydrogen in the insulating layer 180 is absorbed by the semiconductor layer 14. The oxide semiconductor film formed at the same time as the semiconductor layer 10 can be diffused. Impurities can be added to the oxide semiconductor film formed at the same time as the conductive layer 400. The electrical conductivity can be increased.
[0214] By the above method, the conductive layer 400 is formed simultaneously with the semiconductor layer 140, and is made conductive after the formation. By adopting this configuration, it is possible to reduce the manufacturing cost.
[0215] In general, an oxide semiconductor film is transparent to visible light because of its large energy gap. On the other hand, the oxide conductor film is an oxide semiconductor having a donor level in the vicinity of the conduction band. Therefore, the effect of absorption due to the donor level is small, and the oxide film is It has the same degree of light transmittance as a semiconductor film.
[0216] As described above, the conductive layer 190 and the conductive layer 400 have a light-transmitting property. The capacitor element may be configured as a light-transmitting element as a whole.
[0217] <Another configuration of transmissive LCD panel> In addition, in transmissive LCD panels, as in reflective LCD panels, there are various peripheral shapes. 2 and can have a corresponding protective coating 23.
[0218] 23, 24, and 25 show cross-sectional views of a transmission type liquid crystal panel. The LCD panel can have a structure with no irregularities on the periphery as shown in FIG. As shown in FIG. 24, the rear surface of the display device (the substrate 100 having the transistor 50 and the liquid crystal element 81) is It is possible to provide a structure in which the protective film 23 is hardly present on the side (the side not covered with the protective film 23). As shown in FIG. 1, the front surface of the display device (the side of the substrate 300 that does not have a liquid crystal element) and the rear surface of the display device (the side of the substrate 300 that does not have a liquid crystal element) are 100 (the side not having the transistor 50 and the liquid crystal element 81) does not have the protective film 23. In both of FIG. 24 and FIG. 25, the protective film 23 is partially wrapped around the substrate. As shown in FIG. 26, a protective film is provided in the area 14 (the back and side of the display device). The structure may be one without the membrane 23 .
[0219] In addition, in the case of a transmissive liquid crystal panel, a touch panel is formed by combining it with a touch sensor. The cross-sectional views of the touch panel are shown in Fig. 27, Fig. 28, and Fig. 29. is an example of an in-cell type touch panel, and FIG. 27 shows a case where the protective film 23 is formed over the entire area except for the FPC portion. FIG. 28 shows a configuration example in which the formation of a protective film 23 on the substrate 100 side is suppressed. FIG. 29 shows a configuration example having an on-cell type touch panel.
[0220] <Organic EL panel> Moreover, the display device 10 can be manufactured using the light-emitting element 70 as a display element.
[0221] 30, 31, and 32 are cross-sectional views of a display device using a light-emitting element. The portion shared with the liquid crystal panel can be formed in the same manner.
[0222] "Light Emitting Element 70" The light emitting element 70 may be a self-emitting element, which can be turned on or off by a current or voltage. The category includes devices whose brightness can be controlled. For example, light-emitting diodes (LEDs), For example, the lower electrode, the upper electrode, and the A layer containing a light-emitting organic compound (hereinafter, also referred to as an EL layer 250) is disposed between the lower electrode and the upper electrode. ) can be used as the light-emitting element 70.
[0223] The light-emitting elements are top emission type, bottom emission type, and dual emission type. The electrode from which light is extracted is made of a conductive material that is transparent to visible light. In addition, a conductive film that reflects visible light is used for the electrode on the side from which light is not extracted.
[0224] A light emitting element is disposed between a lower electrode made of the conductive layer 220 and an upper electrode made of the conductive layer 260. When a voltage higher than the threshold voltage is applied, holes are injected into the EL layer 250 from the anode side, and the cathode The injected electrons and holes recombine in the EL layer 250, forming an EL The luminescent material contained in layer 250 emits light.
[0225] The EL layer 250 has at least a light-emitting layer. The EL layer 250 has a positive electrode as a layer other than the light-emitting layer. Materials with high hole injection properties, materials with high hole transport properties, hole blocking materials, materials with high electron transport properties , a substance with high electron injection properties, or a bipolar substance (a substance with high electron transport properties and hole transport properties) The film may further include a layer containing a polymer (such as a polymeric material).
[0226] The EL layer 250 can be made of either a low molecular weight compound or a high molecular weight compound. The layers constituting the EL layer 250 may each be formed by deposition (vacuum deposition) The method may include a transfer method, a printing method, an inkjet method, a coating method, etc. .
[0227] The light-emitting element may contain two or more light-emitting materials, which may result in, for example, white light emission. For example, two or more luminescent materials emit light of complementary colors. White light can be obtained by selecting the luminescent material so that ), G (green), B (blue), Y (yellow), or O (orange) light-emitting materials, A luminescent material that emits light containing spectral components of two or more of the colors of B can be used. For example, a light-emitting material that emits blue light and a light-emitting material that emits yellow light may be used. The emission spectrum of a luminescent material exhibiting yellow emission may contain green and red spectral components. The emission spectrum of the light emitting element 70 is preferably in the visible region (e.g., 350 nm or 750 nm or less, or 400 nm or more, or 800 nm or less) It is preferable that the .alpha.-amino acid has a .alpha.-amino acid.
[0228] The EL layer 250 may have multiple light-emitting layers. The layers may be stacked in contact with each other or with a separating layer interposed therebetween. For example, a separation layer may be provided between the fluorescent light-emitting layer and the phosphorescent light-emitting layer.
[0229] The separation layer is, for example, a layer for converting the excited state of a phosphorescent material generated in the phosphorescent-emitting layer into the fluorescent material in the fluorescent-emitting layer. Preventing energy transfer (especially triplet energy transfer) to optical materials through the Dexter mechanism The separation layer only needs to be a few nm thick. Specifically, it is 0. 1nm to 20nm, or 1nm to 10nm, or 1nm to 5nm The separation layer may be a single material (preferably a bipolar material) or a plurality of materials. (preferably a hole transporting material and an electron transporting material).
[0230] The separation layer may be formed using a material contained in the light-emitting layer that is in contact with the separation layer. This facilitates the fabrication of the light-emitting device and reduces the driving voltage. When the separation layer is made of a host material, an assist material, and a phosphorescent material (guest material), In other words, the separation layer may be formed of a phosphorescent material and an assist material. The phosphorescent layer has a region that does not contain a phosphorescent material, and the phosphorescent layer has a region that contains a phosphorescent material. It is possible to deposit the separation layer and the phosphorescent light-emitting layer with or without the phosphorescent material. By forming the separation layer and the phosphorescent layer in the same chamber, it becomes possible to form the separation layer and the phosphorescent layer in the same chamber. This makes it possible to reduce manufacturing costs.
[0231] <Layer 230 for adjusting optical distance> The light-emitting device 70 in FIG. 30 is an example in which a microcavity structure is combined with a light-emitting device. For example, A microcavity structure is formed using the lower electrode and the upper electrode of the light-emitting element 70, and A specific light may be extracted efficiently.
[0232] Specifically, a reflective film that reflects visible light is used as the lower electrode, allowing some of the visible light to pass through and some to be reflected. A semi-transmissive / semi-reflective film that reflects light of a specific wavelength is used as the upper electrode. An upper electrode is disposed relative to the lower electrode so as to be extracted.
[0233] For example, the lower electrode functions as a lower electrode or an anode of a light-emitting element. The outer electrode is arranged to resonate the desired light from the light emitting layer and intensify its wavelength. The layer 230 for adjusting the optical path is not limited to the lower electrode. The optical path can be adjusted by at least one layer constituting the light emitting element. The layer 230 for adjusting the separation may be, for example, indium oxide, indium tin oxide (ITO) :Indium Tin Oxide), Indium Zinc Oxide, Zinc Oxide (ZnO), It can be formed using zinc oxide doped with gallium, or the like.
[0234] When combining a microcavity structure, a semi-transmissive / semi-reflective electrode is used for the upper electrode of the light-emitting element. The semi-transmissive / semi-reflective electrode can be made of a conductive material having reflectivity and a transparent material having The conductive material has a visible light reflectance of 20% or more and 80% or less. % or less, preferably 40% to 70%, and the resistivity is 1×10 -2 Ω·c Examples of semi-transparent and semi-reflective electrodes include conductive materials with a thickness of 100 nm or less. The material may be formed by using one or more of alloys, conductive compounds, etc. It is preferable to use a material with a small electron transport potential (3.8 eV or less). For example, Elements belonging to group 1 or group 2 (alkali metals such as lithium and cesium, calcium, strontium, etc.) Alkaline earth metals such as nickel, magnesium, etc.), alloys containing these elements (e.g., A g-Mg, Al-Li), europium, ytterbium, and other rare earth metals, An alloy containing a metal, aluminum, silver, etc. can be used.
[0235] The electrodes may be formed by vapor deposition or sputtering. , a discharge method such as an inkjet method, a printing method such as a screen printing method, or a plating method. It can be formed by:
[0236] It should be noted that the organic EL structure may be other than the microcavity structure. For example, a method of painting different colors of light emitting elements, a method of using a material that emits white light, A white EL method can be used.
[0237] 《Bulkhead 245》 An insulating material can be used for the partition 245. For example, an inorganic material, an organic material, or an inorganic material can be used. Materials in which organic materials and inorganic materials are laminated can be used. A film containing silicon or silicon nitride, acrylic, polyimide, or photosensitive resin, etc. Applicable.
[0238] Conductive layer 200 The conductive layer 200 may be made of any of a variety of materials, including aluminum, chromium, copper, tantalum, titanium, molybdenum, and nickel. A metal element selected from the group consisting of iron, cobalt, and tungsten, or a metal element containing the above-mentioned metal elements. It is formed by using an alloy of the above-mentioned metal elements or an alloy combining the above-mentioned metal elements. The present invention may be formed using one or more metal elements selected from the group consisting of tungsten, fluorine, zirconium, and tungsten. The conductive layer 200 may have a single-layer structure or a laminated structure of two or more layers. For example, , a single layer structure of aluminum film containing silicon, a single layer structure of copper film containing manganese, Two-layer structure with titanium film laminated on titanium nitride film, two-layer structure with titanium film laminated on titanium nitride film A two-layer structure in which a tungsten film is laminated on a titanium nitride film, a tantalum nitride film or a tungsten nitride film Two-layer structure with tungsten film laminated on tungsten film, and copper film laminated on copper film containing manganese A two-layer structure is used, a titanium film and an aluminum film are laminated on the titanium film, and then A three-layer structure in which a titanium film is formed, a copper film is laminated on a copper film containing manganese, and a manganese film is further laminated on top of that. There are three-layer structures in which a copper film containing fluorine is formed. One or more of the following materials are selected from the group consisting of zinc, tungsten, molybdenum, chromium, neodymium, and scandium. Alternatively, an alloy film made by combining a plurality of layers or a nitride film may be used.
[0239] Insulating layer 210 The insulating layer 210 has a planarizing function. The insulating layer 210 is made of an inorganic material or an organic material. For example, silicon oxide, silicon oxynitride, aluminum oxide, etc. nium, aluminum oxide nitride, gallium oxide, gallium oxide nitride, yttrium oxide, Oxide insulating films such as yttrium oxide nitride, hafnium oxide, and hafnium oxide nitride, silicon nitride Silicon, aluminum nitride and other nitride insulating films, polyimide resin, acrylic resin, polyimide Resins with heat resistance such as amide resins, benzocyclobutene resins, polyamide resins, and epoxy resins. The insulating layer is formed using an organic material that has a high insulating property.
[0240] Conductive layer 260 The conductive layer 260 that transmits visible light may be made of, for example, indium oxide or indium tin oxide. (ITO: Indium Tin Oxide), Indium Zinc Oxide, Zinc Oxide (Z nO), zinc oxide doped with gallium, etc. Also, gold, silver, , platinum, magnesium, nickel, tungsten, chromium, molybdenum, iron, cobalt, Metallic materials such as copper, palladium, or titanium, alloys containing these metallic materials, or Nitrides of metal materials (for example, titanium nitride) can also be formed thin enough to have light transmission properties. Also, a laminated film of the above materials can be used as the conductive layer. For example, the use of a laminated film of an alloy of silver and magnesium and ITO can increase the electrical conductivity. In addition, graphene or the like may be used.
[0241] <Color-coded OLED panel> In addition, organic EL elements can also be produced using a color-coded method, as shown in Figure 31. 30 in that the EL layer 250 is formed on the conductive layer 220 by a color-coded method. become.
[0242] <Flexible display device> The display device is fabricated on flexible substrates 101 and 301 as shown in FIG. It is also possible to attach the flexible substrate and the display device using an adhesive layer 370. This allows the touch panel to have flexibility and bendable or curved. It is possible to realize a touch panel. Furthermore, the thickness of the substrate can be made thinner. This makes it possible to reduce the weight of the touch panel.
[0243] <Example of a method for manufacturing a flexible display device> Here, a method for manufacturing a flexible display device will be described.
[0244] For the sake of convenience, the term "structure including pixels and circuits," "structure including optical members such as color filters," or "structure including optical members such as color filters" will be used herein. The structure including the touch sensor is called an element layer. The element layer includes, for example, a display element. In addition to the display element, wiring electrically connected to the display element, transistors used in pixels and circuits, etc. The device may include an element.
[0245] Also, in this embodiment, a support (e.g., a substrate 101 or The substrate 301) is referred to as a base material.
[0246] As a method for forming an element layer on a substrate having a flexible insulating surface, A method of directly forming an element layer and a method of forming an element layer on a supporting substrate and then bonding the element layer and the supporting substrate. and a method of peeling off the element layer and transferring it to a base material.
[0247] In the case where the material constituting the base material has heat resistance against the heat applied in the process of forming the element layer, It is preferable to form the element layer directly on the substrate, since the process is simplified. When the element layer is formed in a state where it is fixed to a supporting substrate, it is easy to transport it within and between devices. This is preferable because
[0248] In addition, when a method is used in which an element layer is formed on a supporting substrate and then transferred to the substrate, the supporting substrate is first A release layer and an insulating layer are laminated on a substrate, and an element layer is formed on the insulating layer. The element layer is peeled off and transferred to a substrate. Materials may be selected such that release occurs at the layer interface or within the release layer.
[0249] For example, a layer containing a high melting point metal material such as tungsten as a peeling layer and an oxidized layer of the metal material A layer including a substance is laminated, and a layer in which silicon nitride or silicon oxynitride is laminated on a peeling layer It is preferable to use a high melting point metal material. This is preferable.
[0250] Peeling can be achieved by applying mechanical force, etching the peeling layer, or by splitting one of the peeling interfaces. The peeling may be performed by dropping a liquid on the portion and allowing it to penetrate into the entire peeling interface. Alternatively, the peeling may be performed by applying heat to the peeling interface, taking advantage of the difference in thermal expansion.
[0251] In addition, if peeling is possible at the interface between the support substrate and the insulating layer, it is not necessary to provide a peeling layer. For example, glass is used as the support substrate, and an organic resin such as polyimide is used as the insulating layer. A part of the organic resin is locally heated using a laser beam or the like to form a peeling starting point, The separation may be performed at the interface between the glass and the insulating layer. A metal layer is provided between the layers, and the metal layer is heated by passing an electric current through the metal layer. In this case, the insulating layer made of an organic resin may be peeled off at the interface between the metal layer and the insulating layer. The border layer can be used as a substrate.
[0252] Examples of flexible substrates include polyethylene terephthalate (PET), polyethylene terephthalate (PE ... Polyester resins such as ethylene naphthalate (PEN), polyacrylonitrile resins, poly Imide resin, polymethyl methacrylate resin, polycarbonate (PC) resin, polyethylene Tersulfone (PES) resin, polyamide resin, cycloolefin resin, polystyrene resin Examples of such materials include resins with low thermal expansion coefficients, such as polyamide-imide resins and polyvinyl chloride resins. It is preferable to use a material with a low thermal expansion coefficient, for example, 30×10 -6 / K or less Preferably, a triamide-imide resin, a polyimide resin, PET, etc. can be used. A substrate made of resin-impregnated fiber (also called prepreg) or a substrate made of inorganic filler mixed with organic resin. Substrates with reduced thermal expansion coefficients may also be used.
[0253] When the material contains fibrous material, the fibrous material is a high strength material made of organic or inorganic compounds. High-strength fibers are specifically fibers with high tensile modulus or Young's modulus. Representative examples are polyvinyl alcohol fibers, polyester fibers, polyamide fibers, etc. Fibers based on cellulose, polyethylene fibers, aramid fibers, polyparaphenylene benzobisoxa Examples of the fiberglass include sol fiber, glass fiber, and carbon fiber. The glass fiber is E-glass. Examples of glass fibers include those made of S glass, D glass, Q glass, etc. The fiber is used in the form of a nonwoven fabric, and the resin is impregnated into the fiber and hardened to form a flexible structure. As a substrate having flexibility, a substrate having a structure made of a fiber body and a resin may be used. The use of a structure is preferable because it improves reliability against damage caused by bending or local pressure. .
[0254] Alternatively, a thin glass or metal having flexibility may be used as the substrate. Alternatively, a composite material in which glass and a resin material are bonded together may be used.
[0255] For example, in the case of the configuration shown in FIG. 32, a first release layer and an insulating layer 112 are sequentially formed on a first support base material. After forming the first supporting substrate, the upper layer structure is formed. A second release layer and an insulating layer 312 are formed on the material in this order, and then the upper layer structure is formed. Next, the first supporting substrate and the second supporting substrate are bonded together with an adhesive layer 370. Thereafter, the second release layer is peeled off at the interface between the second release layer and the insulating layer 312 to form the second support substrate and the second The release layer is removed, and the insulating layer 312 and the substrate 301 are bonded together with the adhesive layer 372. The first release layer is peeled off at the interface between the first release layer and the insulating layer 112, so that the first support base and the first release layer are separated. The insulating layer 112 and the substrate 101 are bonded together with an adhesive layer 371. The separation and bonding may be performed on either side first.
[0256] The above is a description of the method for manufacturing a flexible display device.
[0257] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0258] (Embodiment 5) In the fifth embodiment, a modification of the transistor structure described in the fourth embodiment will be described.
[0259] 《Stacked oxide semiconductor》 The semiconductor layer 140 is formed by stacking a plurality of oxide semiconductor films having different atomic ratios of metal elements. For example, in the transistor 51, as shown in FIG. 30, oxide semiconductor layers 141 and 142 may be stacked in this order. As shown in FIG. 1, an oxide semiconductor layer 142, an oxide semiconductor layer 141, and an oxide The oxide semiconductor layer 142 and the oxide semiconductor layer 143 may be stacked in this order. The oxide semiconductor layer 141 has a different atomic ratio of metal elements than the oxide semiconductor layer 141.
[0260] <Channel protection type and top gate structure> The transistor 50 shown in FIG. 12 illustrates a transistor having a bottom gate structure. As a modification of the transistor 50, a transistor shown in FIG. In FIG. 11B, transistor 50 is shown. In FIG. 34B, transistor 54 is shown. 34(A) shows a channel etch type, but the insulating layer 165 Alternatively, a channel protection transistor 53 having a channel protection layer may be used as shown in the cross-sectional view of FIG. Alternatively, the transistor 54 may have a top gate structure as shown in FIG.
[0261] The transistors 52 in the peripheral circuits (gate drivers, etc.) all have the same structure. The pixel section may have a structure having two or more types of transistors. The rotors 50 may all be of the same structure, or may be of two or more different structures.
[0262] Alternatively, the transistor described in this embodiment may be a transistor including an oxide semiconductor. However, one embodiment of the present invention is not limited to this. Alternatively, depending on the situation, one embodiment of the present invention may be a semiconductor device using a semiconductor material other than an oxide semiconductor. A transistor may also be used.
[0263] For example, the semiconductor layer 140 may be made of a group 14 element, a compound semiconductor, or an oxide semiconductor. Specifically, a semiconductor containing silicon, a semiconductor containing gallium arsenide, etc. Transistors using conductors or organic semiconductors can be used.
[0264] For example, single crystal silicon, polysilicon, or amorphous silicon is used for the transistor. The present invention can be applied to the semiconductor layer of
[0265] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0266] (Embodiment 6) In this embodiment, a structural example of a display panel according to one embodiment of the present invention will be described with reference to FIGS. do.
[0267] [Configuration example] FIG. 36A is a top view of a display device of one embodiment of the present invention, and FIG. A pixel circuit that can be used when a liquid crystal element is applied to a pixel of a display device of one embodiment will be described. FIG 36C is a circuit diagram showing a configuration of a pixel of a display device according to one embodiment of the present invention. FIG. 1 is a circuit diagram illustrating a pixel circuit that can be used when an organic EL element is applied. .
[0268] The transistors disposed in the pixel portion can be formed according to the above-described embodiment. Since the transistor can be easily made into an n-channel type, the n-channel transistor in the driver circuit can be easily made into an n-channel type. A part of the driver circuit can be configured with a transistor of the same type as the transistor of the pixel part. In this manner, the transistor shown in the above embodiment is formed in the pixel portion or the driver circuit. By using the above, a highly reliable display device can be provided.
[0269] An example of a top view of an active matrix display device is shown in FIG. On the upper surface of the display 700, there are a pixel portion 701, a scanning line driving circuit 702, a scanning line driving circuit 703, a signal line driving circuit 704, a signal line driving circuit 705, a signal line driving circuit 706, a signal line driving circuit 707, a signal line driving circuit 708, a signal line driving circuit 709, a signal line driving circuit 701, a signal line driving circuit 702, a signal line driving circuit The pixel portion 701 has a signal line driver circuit 704. A plurality of scanning lines are connected to a scanning line driving circuit 702 and a scanning line driving circuit 703. The scanning lines and the signal lines are arranged in such a manner that they extend from each other. The display device has a substrate 700 that is connected to an FPC or the like. It is connected to a timing control circuit (also called a controller or control IC) via a connection part. do.
[0270] In FIG. 36A, a scanning line driver circuit 702, a scanning line driver circuit 703, a signal line driver circuit The path 704 is formed on the same substrate 700 as the pixel section 701. Since the number of components such as the operating circuit is reduced, the cost can be reduced. If a drive circuit is provided in the sensor section, the wiring must be extended, and the number of connections between the wiring increases. When the driving circuit is provided on the same substrate 700, the number of connections between the wirings can be reduced, and reliability can be improved. It is possible to improve the efficiency or yield.
[0271] <Liquid crystal display device> An example of the circuit configuration of a pixel is shown in FIG. 36(B). 4 shows a pixel circuit that can be applied to a pixel of a display device.
[0272] This pixel circuit can be applied to a configuration in which one pixel has multiple pixel electrode layers. The pixel electrode layer is connected to different transistors, and each transistor is driven by a different gate signal. This allows individual pixels of a multi-domain pixel to be The signals applied to the electrode layers can be independently controlled.
[0273] The gate wiring 712 of the transistor 716 and the gate wiring 713 of the transistor 717 are , are separated so that different gate signals can be applied. On the other hand, the data line 714 is used in common for the transistor 716 and the transistor 717. The transistors 16 and 717 may be appropriately selected from the transistors described in the above embodiment modes. This makes it possible to provide a highly reliable liquid crystal display device.
[0274] The transistor 716 is electrically connected to a first pixel electrode. The second pixel electrode is electrically connected to the first pixel electrode 7. The first pixel electrode and the second pixel electrode are The first pixel electrode and the second pixel electrode are separated from each other. For example, the first pixel electrode may be V-shaped.
[0275] The gate electrode of the transistor 716 is connected to the gate wiring 712. The gate electrode is connected to the gate wiring 713. By applying different gate signals to the transistors 716 and 717, the operation timing of the transistors 716 and 717 is By varying the polarity, the alignment of the liquid crystal can be controlled.
[0276] In addition, the capacitance wiring 710, the gate insulating film functioning as a dielectric, and the first pixel electrode layer or A storage capacitor may be formed by a capacitor electrode electrically connected to the second pixel electrode layer.
[0277] The multi-domain structure includes a first liquid crystal element 718 and a second liquid crystal element 719 in one pixel. The first liquid crystal element 718 is composed of a first pixel electrode layer, a counter electrode layer, and a liquid crystal layer therebetween. The second liquid crystal element 719 is composed of a second pixel electrode layer, a counter electrode layer, and a liquid crystal layer therebetween. do.
[0278] Note that the pixel circuit shown in FIG. 36(B) is not limited to this. The pixel circuit is newly equipped with switches, resistors, capacitors, transistors, sensors, or logic Circuits etc. may be added.
[0279] <Organic EL display device> Another example of the circuit configuration of a pixel is shown in FIG. 36(C). 3 shows the pixel structure of the device.
[0280] In an organic EL element, when a voltage is applied to the light-emitting element, electrons are emitted from one of a pair of electrodes. Holes are injected from the other side into the layer containing the light-emitting organic compound, causing a current to flow. The electrons and holes recombine to form an excited state in the light-emitting organic compound, which When the excited state of the electron returns to the ground state, light is emitted. The element is called a current-excited light-emitting element.
[0281] FIG. 36C is a diagram showing an example of an applicable pixel circuit. The metal oxide film of one embodiment of the present invention is The film can be used for the channel formation region of an n-channel transistor. The pixel circuit can apply digital time gray scale driving.
[0282] Regarding the configuration of an applicable pixel circuit and the operation of a pixel when digital time gray scale driving is applied, I will explain this in more detail.
[0283] The pixel 720 includes a switching transistor 721, a driving transistor 722, and a light-emitting element The switching transistor 721 has a gate electrode 724 and a capacitor element 723. The gate electrode layer is connected to the scanning line 726, and the first electrode (the source electrode layer and the drain electrode layer) One of the electrodes (the source electrode layer and the drain electrode layer) is connected to a signal line 725, and the second electrode (the other of the source electrode layer and the drain electrode layer) is connected to a signal line 725. ) is connected to the gate electrode layer of the driving transistor 722. In the semiconductor device 22, the gate electrode layer is connected to a power supply line 727 through a capacitor element 723, and the first electrode is The second electrode is connected to the first electrode (pixel electrode) of the light-emitting element 724. The second electrode of the light emitting element 724 corresponds to a common electrode 728. It is electrically connected to a common potential line formed on the substrate.
[0284] The switching transistor 721 and the driving transistor 722 may have other embodiments. This allows the transistors described in 2. to be used appropriately. A display device can be provided.
[0285] The potential of the second electrode (common electrode 728) of the light-emitting element 724 is set to a low power supply potential. The power supply potential is a potential lower than the high power supply potential supplied to the power supply line 727, for example, GND , 0V, etc. can be set as the low power supply potential. The high power supply potential and the low power supply potential are set so that the potential difference is equal to or greater than the threshold voltage. By applying a voltage to the light emitting element 724, a current flows through the light emitting element 724, causing it to emit light. The forward voltage in 4 refers to the voltage required to achieve the desired brightness, and must be at least the forward threshold. Includes low-value voltages.
[0286] The capacitance element 723 can be omitted by substituting the gate capacitance of the driving transistor 722. The gate capacitance of the driving transistor 722 can be omitted. A capacitance may be formed between the first electrode layer and the second electrode layer.
[0287] Next, a signal input to the driving transistor 722 will be described. In this case, the driving transistor 722 is in two states: fully on or fully off. A video signal such as the above is input to the driving transistor 722. In order to operate the driving transistor 722 in a linear region, a voltage higher than the voltage of the power supply line 727 is applied to the driving transistor 722. A signal line 725 is connected to the gate electrode layer of the transistor 722. A voltage equal to or greater than the threshold voltage Vth of the input transistor 722 is applied.
[0288] When analog gradation driving is performed, the gate electrode layer of the driving transistor 722 is connected to the light emitting element 72 A voltage equal to or greater than the sum of the forward voltage of the transistor 724 and the threshold voltage Vth of the driving transistor 722 is applied. In addition, a video signal is input so that the driving transistor 722 operates in the saturation region. A current flows through the light emitting element 724. In addition, the driving transistor 722 is operated in a saturation region. In order to achieve this, the potential of the power supply line 727 is set higher than the gate potential of the driving transistor 722. By converting the video signal into an analog signal, a current corresponding to the video signal is passed through the light emitting element 724. , analog gray scale driving can be performed.
[0289] The configuration of the pixel circuit is not limited to the pixel configuration shown in FIG. A switch, a resistor, a capacitor, a sensor, a transistor or a logic A logic circuit or the like may be added.
[0290] When the transistor illustrated in the above embodiment is applied to the circuit illustrated in FIG. The source electrode (first electrode) is on the low potential side, and the drain electrode (second electrode) is on the high potential side. Furthermore, the potential of the first gate electrode is controlled by a control circuit or the like. The second gate electrode is connected to a wiring (not shown) so as to have a potential lower than that applied to the source electrode. Any of the above-mentioned potentials may be input.
[0291] For example, in this specification and the like, the term "display element," "display device having a display element," "light-emitting element," A light-emitting device, which is a device having a light-emitting element and a light-emitting element, can be used in various forms or in various The display element, the display device, the light-emitting element, or the light-emitting device may include, for example, For example, EL (electroluminescence) elements (EL elements containing organic and inorganic materials, organic EL elements, inorganic EL elements), LEDs (white LEDs, red LEDs, green LEDs, blue LEDs) etc.), transistors (transistors that emit light according to electric current), electron-emitting devices, liquid crystal devices , electronic ink, electrophoretic element, grating light valve (GLV), plasma display Using MEMS (Micro-Electro-Mechanical Systems) Display element, Digital Micromirror Device (DMD), DMS (Digital Micromirror Shutter), MIRASOL (registered trademark), IMOD (Interference Module duction element, shutter type MEMS display element, optical interference type MEMS display element , electrowetting element, piezoelectric ceramic display, carbon nanotube In addition to these, the device has at least one electric or magnetic display element. The display medium has contrast, brightness, reflectance, transmittance, etc. that change due to electrochemical effects. An example of a display device using an EL element is an EL display. An example of a display device using electron-emitting elements is a field emission display ( FED) or SED type flat panel display (SED: Surface-conductive Liquid crystal elements An example of a display device using the liquid crystal display (transmissive liquid crystal display, semi-transmissive liquid crystal display, LCD display, reflective LCD display, direct-view LCD display, projection LCD display Electronic ink, electronic powder, or electrophoretic elements are used. An example of the display device used is electronic paper. In order to realize a reflective LCD, some or all of the pixel electrodes must be For example, a part or the whole of the pixel electrode may be made to have a function as a reflective electrode. The portion may be made of aluminum, silver, or the like. In this case, the reflective electrode It is also possible to provide a memory circuit such as an SRAM under the It is possible to reduce power consumption. When using LEDs, the electrodes of the LEDs and the nitride semiconductors Graphene or graphite may be placed under the A multi-layer film may be formed by stacking several layers. By this, a nitride semiconductor, for example, a crystal-containing n-type GaN semiconductor layer, etc., can be formed thereon. It is easy to form a film. Furthermore, a p-type GaN semiconductor layer having crystals can be formed on it. By providing a crystalline material, an LED can be constructed. An AlN layer may be provided between the n-type GaN semiconductor layer and the LED. The aN semiconductor layer may be formed by MOCVD. However, by providing graphene, The GaN semiconductor layer of the LED can also be formed by sputtering.
[0292] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0293] (Embodiment 7) In this embodiment, a configuration example of a touch panel according to one embodiment of the present invention will be described with reference to FIGS. do.
[0294] <Positional relationship between transistor and touch sensor wiring> Figure 37 shows a top view showing the positional relationship of the pixels, transistors, and touch sensor wiring. The conductive layer 410, which is an electrode for the touch sensor, overlaps, for example, the source line 91 and the gate line 92. They can be arranged in a parallel manner without overlapping. The conductive layer 410, which is the wiring of the touch sensor, does not overlap with the transistor 50 and the capacitance element 61. Although an example is shown, they may be arranged overlapping each other. Also, the conductive layer 410 overlaps the pixel 24. Although they are arranged side by side, they can also be arranged overlapping each other. The conductive layer 430 and the conductive layer 380, which can play a role in the above-mentioned embodiment, are arranged in a similar manner. This can be done.
[0295] <Examples of sensor electrode configurations> In the following, a more specific configuration example of the input device 90 having a function as a touch sensor will be described. The following description will be given with reference to the drawings.
[0296] 38A shows a top view of an input device 90. The input device 90 has a plurality of electrodes on a substrate 930. The substrate includes an electrode 931, a plurality of electrodes 932, a plurality of wirings 941, and a plurality of wirings 942. The plate 930 includes an FPC that is electrically connected to each of the plurality of wirings 941 and the plurality of wirings 942. In FIG. 38(A), an IC 951 is provided on the FPC 950. The following shows an example of how this is being done.
[0297] FIG. 38B shows an enlarged view of the area surrounded by the dashed line in FIG. 38A. The electrode 931 is A plurality of diamond-shaped electrode patterns are arranged in a line in the horizontal direction of the paper. The diamond-shaped electrode patterns are electrically connected to each other. Similarly, the electrode 932 is also The diamond-shaped electrode pattern has a shape that is connected vertically on the paper surface, and the diamond-shaped electrodes are arranged in a row. The patterns are electrically connected to each other. Also, the electrodes 931 and 932 are At this intersection, the electrodes 931 and 932 An insulator is sandwiched between the wires to prevent electrical short circuits.
[0298] As shown in FIG. 38(C), the electrode 932 is connected to a plurality of diamond-shaped electrodes 933. , and may be composed of a bridge electrode 934. The island-shaped electrode 933 is arranged in the vertical direction of the drawing. The electrodes 933 are arranged side by side, and two adjacent electrodes 933 are electrically connected by a bridge electrode 934. With this structure, the electrode 933 and the electrode 931 are formed of the same conductive film. By processing the layers, they can be formed simultaneously. This makes it possible to suppress variations in the resistance and light transmittance of each electrode depending on the location. In this embodiment, the electrode 932 has a bridge electrode 934. 1 may have such a configuration.
[0299] As shown in FIG. 38(D), the diamond-shaped electrodes 931 and 932 shown in FIG. 38(B) are The inside of the electrode pattern may be hollowed out to leave only the outline. In the case where the width of the electrodes 931 and 932 is thin enough not to be visually recognized by the user, As described later, the electrodes 931 and 932 may be made of a light-shielding material such as a metal or an alloy. In addition, the electrode 931 or the electrode 932 shown in FIG. 38(D) connects the bridge electrode 934. The configuration may include the above.
[0300] One electrode 931 is electrically connected to one wiring 941. The electrodes 931 and 932 are electrically connected to one wiring 942. One of them corresponds to a row wiring, and the other corresponds to a column wiring.
[0301] As an example, in FIG. 39(A), FIG. 39(B), FIG. 39(C), and FIG. 39(D), an electrode 931 9 shows a schematic diagram of an enlarged portion of the electrode 932. The electrodes may have various shapes. can be done.
[0302] In FIG. 40(A), FIG. 40(B), and FIG. 40(C), instead of the electrode 931 and the electrode 932, This shows an example in which electrodes 936 and 937 having a thin-line top surface shape are used. In FIG. 40(A), linear electrodes 936 and 937 are arranged in a lattice pattern. In FIG. 40B and FIG. 40C, the electrodes 936 and 937 are arranged in a zigzag pattern. The sensors are arranged in a grid pattern.
[0303] Enlarged views of the area enclosed by the dashed line in FIG. 40(B) are shown in FIG. 41(A), FIG. 41(B), and FIG. FIG. 41(D) and FIG. 41(E) are enlarged views of the area enclosed by the dashed line in FIG. 40(C). 41(F) and 41(G). Also, in each figure, an electrode 936, an electrode 937, and As shown in FIG. 41(B) and FIG. 41(E), 41(A) and 41(D), the straight line portions of the electrodes 936 and 937 have corners. As shown in Figs. 41(C) and 41(F), the shape may be a meandering shape. The line may have a meandering shape so as to be continuous.
[0304] <Example of in-cell touch panel configuration> Below is an example of a touch panel configuration in which a touch sensor is incorporated into a display unit having multiple pixels. Here, an example in which a liquid crystal element is used as a display element provided in a pixel will be described. Shows.
[0305] FIG. 42(A) shows a part of a pixel circuit provided in a display unit of a touch panel exemplified in this configuration example. FIG.
[0306] One pixel has at least a transistor 3503 and a liquid crystal element 3504. A wiring 3501 is connected to the gate of the transistor 3503, and a wiring 350 is connected to either the source or drain. 2 are electrically connected to each other.
[0307] The pixel circuit includes a plurality of wirings (for example, wiring 3510_1, wiring 3510_ 2) and a plurality of wirings (for example, wiring 3511) extending in the Y direction, which are mutually The electrodes are arranged to cross each other to form a capacitance therebetween.
[0308] In addition, among the pixels provided in the pixel circuit, some of the adjacent pixels are provided The electrodes of the liquid crystal elements are electrically connected to each other to form one block. The blocks are divided into island-like blocks (e.g., block 3515_1, block 3515_2) and Linear blocks extending in the Y direction (e.g., block 3516) are classified into two types. In addition, although FIG. 42 shows only a part of the pixel circuit, these two types of The blocks are arranged repeatedly in the X and Y directions.
[0309] The wiring 3510_1 (or 3510_2) extending in the X direction is arranged in an island-shaped block 3515 _1 (or block 3515_2). The wiring 3510_1 extending in the X direction is discontinuously arranged along the X direction via a line-shaped block. The island-shaped blocks 3515_1 are electrically connected to each other. The wiring 3511 is electrically connected to a line-shaped block 3516 .
[0310] FIG. 42B shows a plurality of wirings 3510 extending in the X direction and a plurality of wirings 3510 extending in the Y direction. 3511. Each of the wirings 3510 extending in the X direction is An input voltage or a common potential can be input to the wiring 35 extending in the Y direction. A ground potential is input to each of the terminals 11, or the wiring 3511 is electrically connected to the detection circuit. It is possible.
[0311] The operation of the above-mentioned touch panel will be described below with reference to FIG. 43(A) and FIG. 43(B). do.
[0312] Here, one frame period is divided into a writing period and a detection period. This is the period in which the image data is written, and the wiring 3510 (also called the gate line) is sequentially selected. On the other hand, the detection period is the period during which sensing is performed by the touch sensor, and the X-direction The wiring 3510 extending to is selected in sequence, and an input voltage is input.
[0313] 43A is an equivalent circuit diagram during the writing period. A common potential is input to both the wiring 3510 extending in the Y direction and the wiring 3511 extending in the Y direction. do.
[0314] FIG. 43(B) is an equivalent circuit diagram at a certain point in the detection period. Each of the wirings 3511 extending in the X direction is electrically connected to a detection circuit. Of the wirings 3510, the input voltage is input to the selected one, and the other ones are connected to the common A conducting potential is input.
[0315] The driving method exemplified here can be applied not only to the in-cell type but also to the touch panel exemplified above. It can also be applied to the above-mentioned driving method example and can be used in combination with the method. do.
[0316] In this way, the image writing period and the touch sensor sensing period are separated. This prevents touch sensitivity caused by noise when writing to the pixel. This can suppress the decrease in the sensitivity of the sensor.
[0317] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination.
[0318] (Embodiment 8) In this embodiment, a structure of an oxide semiconductor film will be described.
[0319] <Film formation method> An example of a method for forming a CAAC-OS film will be described below.
[0320] FIG. 44(A) is a schematic diagram of the inside of the film formation chamber. CAAC-OS is formed by sputtering. A film can be formed.
[0321] As shown in FIG. 44(A), a substrate 5220 and a target 5230 are arranged to face each other. Between the substrate 5220 and the target 5230 there is a plasma 5240. In addition, a heating mechanism 5260 is provided below the substrate 5220. The pad 5230 is bonded to the backing plate. A number of magnets are arranged facing the target 5230. The sputtering method that uses a magnetic field to increase the deposition rate is called magnetron sputtering. Called.
[0322] The distance d between the substrate 5220 and the target 5230 (target-substrate distance (TS distance ) is 0.01m or more and 1m or less, preferably 0.02m or more and 0.5m or less. In the deposition chamber, most of the deposition gas (e.g., oxygen, argon, or oxygen at 5% by volume) is The pressure is preferably 0.01 Pa to 100 Pa. The pressure is controlled to 0.1 Pa or more and 10 Pa or less. By applying pressure, discharge starts and plasma 5240 is observed. A high-density plasma region is formed near 5230 by the magnetic field. In the deposition region, the deposition gas is ionized to generate ions 5201. The ions 5201 are For example, the oxygen cation (O +) and argon cations (Ar + ) etc.
[0323] The target 5230 has a polycrystalline structure having a plurality of crystal grains, and each of the crystal grains has As an example, FIG. 45 shows a target 5230 containing InMZnO 4 (wherein element M is, for example, aluminum, gallium, yttrium or tin) Figure 45 shows the crystal structure of InMZnO4 when observed from a direction parallel to the b axis. In the InMZnO4 crystal, the oxygen atoms have a negative charge, so that adjacent There is a repulsive force between the two M-Zn-O layers. Therefore, the InMZnO4 crystal is There is a cleavage plane between two adjacent M-Zn-O layers.
[0324] Ions 5201 generated in the high-density plasma region are applied to the target 5230 side by the electric field. The cleavage plane is accelerated and eventually collides with the target 5230. At this time, flat or pellet-like particles are generated from the cleavage plane. Pellets 5200, which are pellet-shaped sputtered particles, are peeled off (see FIG. 44(A)). The pellet 5200 is a portion sandwiched between the two cleavage planes shown in FIG. When only 200 is extracted, its cross section looks like Figure 44(B) and its top surface looks like Figure 44(C). It can be seen that the pellet 5200 is formed by the impact of the ion 5201. In addition, the target may become distorted due to the peeling of pellet 5200. Particle 5203 is also ejected from 5230. Particle 5203 is one atom or a few atoms in size. Therefore, the particle 5203 is called an atomic particle. It can also be called es.
[0325] The pellet 5200 is a flat or pellet-shaped pellet having a triangular, for example equilateral, plane. The pellet 5200 is a sputtered particle. Alternatively, the pellet 5200 has a hexagonal, e.g., regular hexagonal, planar surface. The sputtered particles are in the form of a plate or pellet. However, the shape of the pellet 5200 is The shape is not limited to a triangle or a hexagon, but may be, for example, a shape made up of multiple triangles. For example, a quadrilateral (such as a rhombus) made up of two triangles (such as an equilateral triangle) In some cases, this may be the case.
[0326] The thickness of the pellet 5200 is determined depending on the type of deposition gas. 200 has a thickness of 0.4 nm or more and 1 nm or less, preferably 0.6 nm or more and 0.8 nm or less For example, the pellet 5200 has a width of 1 nm or more and 3 nm or less, preferably 1 For example, a target having an In-M-Zn oxide Ions 5201 are bombarded onto 5230. Then, the M-Zn-O layer, the In-O layer and The pellet 5200 having three layers, the M-Zn-O layer, and the M-Zn-O layer, is peeled off. As the target 5230 is peeled off, the particle 5203 is also ejected from the target 5230. It has an aggregate of one atom or several atoms. Therefore, the particle 5203 is called an atomic particle (at They can also be called omic particles.
[0327] When the pellet 5200 passes through the plasma 5240, the surface may become negatively or positively charged. For example, when a pellet 5200 is in a plasma 5240, 2- negative charge from As a result, the oxygen atoms on the surface of the pellet 5200 may become negatively charged. In addition, when the pellet 5200 passes through the plasma 5240, the pellet 5200 is It may grow by combining with indium, element M, zinc, or oxygen in 0.
[0328] The pellets 5200 and particles 5203 that have passed through the plasma 5240 adhere to the surface of the substrate 5220. Some of the particles 5203 are small in mass and can be removed by a vacuum pump or other device. may be discharged into the area.
[0329] Next, regarding the deposition of pellets 5200 and particles 5203 on the surface of the substrate 5220, This will be explained using Figure 46.
[0330] First, the first pellet 5200 is deposited on the substrate 5220. The pellet 5200 has a flat shape. Therefore, the flat side is deposited facing the surface of the substrate 5220 (see FIG. 46(A)). At this time, the charge on the surface of the pellet 5200 facing the substrate 5220 is discharged through the substrate 5220. do.
[0331] Next, the second pellet 5200 reaches the substrate 5220. The surface of the first pellet 5200 and the surface of the second pellet 5200 are charged, so A repulsive force is generated between the two (see Figure 46(B)).
[0332] As a result, the second pellet 5200 avoids the first pellet 5200 and falls on the substrate 52 The particles are deposited at a location slightly away from the surface of 20 (see Figure 46(C)). By repeating this process, On the surface of the substrate 5220, countless pellets 5200 are deposited to a thickness equivalent to one layer. Between the pellets 5200, there is a pile of pellets 5200. There will be areas where this is not the case.
[0333] Next, the particles 5203 reach the surface of the substrate 5220 (see FIG. 46(D)).
[0334] Particles 5203 cannot accumulate in active areas such as the surface of pellet 5200. Therefore, the pellets 5200 are deposited so as to fill the areas where the pellets 5200 are not deposited. The particles 5203 grow sideways between the pellets 5200 (also called lateral growth). In this way, the pellets 5200 are connected to each other. Particles 5203 are deposited until they fill the area. This mechanism is the deposition mechanism of the ALD method. Similar to .
[0335] There are several possible mechanisms for the lateral growth of particles 5203 between pellets 5200. For example, as shown in FIG. 46(E), In this case, after the first M-Zn-O layer is formed, the In-O layer Then, the first M-Zn-O layer is connected to the second M-Zn-O layer (first mechanism).
[0336] Alternatively, for example, as shown in FIG. 47(A), first, one side of the first M-Zn-O layer is Next, one of the In-O layers is bonded to the In-O particles 5203 as shown in FIG. Next, as shown in FIG. 47(C), the second layer MZ In some cases, the nO layers are connected by bonding one particle 5203 to one side of the layer (second (The mechanism of the above) Note that Figure 47(A), Figure 47(B) and Figure 47(C) may occur simultaneously. In some cases, they may be linked by means of a single link (third mechanism).
[0337] As described above, the mechanism of lateral growth of the particles 5203 between the pellets 5200 However, there are other mechanisms that may affect the There is also a possibility that particles 5203 may grow laterally between the nuclei 5200.
[0338] Therefore, even if multiple pellets 5200 are facing in different directions, multiple The grains 5203 grow laterally and fill the gaps between the pellets 5200. In addition, the particles 5203 smoothly connect the pellets 5200. The resulting crystal structure is different from that of single crystals and polycrystals. A crystal structure having distortion between the uniform crystal regions (pellets 5200) is thus formed. The regions between the crystalline regions are distorted crystalline regions, and are therefore referred to as amorphous structures. It is considered inappropriate to
[0339] When the particles 5203 finish filling the gaps between the pellets 5200, the thickness of the pellets 5200 becomes approximately the same as that of the pellets 5200. A new pellet 5200 is piled up on the first layer. Then, a second layer is formed. This process is repeated to form a laminate. A thin film structure having the above structure is formed (see FIG. 44(D)).
[0340] The deposition of the pellets 5200 may vary depending on the surface temperature of the substrate 5220. For example, if the surface temperature of the substrate 5220 is high, the pellet 5200 may adhere to the surface of the substrate 5220. As a result, the pellet 5200 and another pellet 5200 The ratio of connections not passing through the particle 5203 increases, resulting in highly oriented CAAC-OS. The surface temperature of the substrate 5220 during the formation of the CAAC-OS film is 100° C. or higher and 500° C. or lower. less than 140°C and less than 450°C, and more preferably 170°C and less than 400°C. Therefore, even if a large-area substrate of the 8th generation or later is used as the substrate 5220, It can be seen that almost no warping or other defects occur.
[0341] On the other hand, when the surface temperature of the substrate 5220 is low, the pellet 5200 is microscopically attached to the surface of the substrate 5220. As a result, pellets 5200 pile up on each other. Low-oriented nc-OS (nanocrystalline oxide semiconductor) In nc-OS, pellet 5200 is the load. The pellets 5200 may accumulate at regular intervals due to the charge on the surface. Therefore, although the orientation is low, the amorphous oxide semiconductor has a slight degree of regularity. It has a denser structure than a conductor.
[0342] In addition, in CAAC-OS, the gap between pellets is extremely small, so that one Large pellets may be formed. The inside of one large pellet has a single crystal structure. For example, the size of the pellet is 10 nm to 200 nm, 15 nm to 200 nm, as viewed from the top. It may be m or more and 100 nm or less, or 20 nm or more and 50 nm or less.
[0343] Based on the above model, it is assumed that the pellets 5200 are deposited on the surface of the substrate 5220. CAAC-OS can be deposited even on a surface that does not have a crystalline structure. This indicates that the growth mechanism is different from epitaxial growth. AAC-OS and nc-OS enable uniform deposition even on large glass substrates. For example, if the structure of the surface (formation surface) of the substrate 5220 is an amorphous structure (e.g., an amorphous oxide It is possible to form a CAAC-OS film even on a substrate made of silicon dioxide.
[0344] In addition, even if the surface of the substrate 5220 on which the material is to be formed is uneven, the pellets are formed according to the shape of the uneven surface. It can be seen that 5200 bits are arranged.
[0345] (Embodiment 9) <module> A display module to which the semiconductor device of one embodiment of the present invention is applied will be described below with reference to FIG. Explanations will be given.
[0346] The display module 8000 shown in FIG. 49 is made up of an upper cover 8001 and a lower cover 8002. In between, the touch sensor 8004 connected to the FPC 8003 and the touch sensor 8005 connected to the FPC 8005 Display device 8006, backlight unit 8007, frame 8009, printed circuit board 8 8010 and a battery 8011. In some cases, the input / output terminal 8003 may not have the input / output terminal 8011 or the touch sensor 8004.
[0347] The semiconductor device of one embodiment of the present invention can be used for the display device 8006, for example.
[0348] The upper cover 8001 and the lower cover 8002 are provided with a touch sensor 8004 and a display device. The shape and dimensions can be changed as appropriate to match the size of 8006.
[0349] The touch sensor 8004 is a resistive or capacitive touch panel that is connected to the display device 80 8006. It is also possible to provide a touch panel function. It is also possible to provide an optical sensor in each pixel to make an optical touch panel. A touch sensor electrode is provided in each pixel of the display device 8006 to form a capacitive touch panel. It is also possible.
[0350] The backlight unit 8007 includes a light source 8008. It may be provided at the end of the unit 8007 and may be configured to use a light diffusion plate.
[0351] The frame 8009 protects the display device 8006 and also functions to protect the printed circuit board 8010. The film may also have a function as an electromagnetic shield to block electromagnetic waves generated by the film. The frame 8009 may function as a heat sink.
[0352] The printed circuit board 8010 includes a power supply circuit, a signal circuit for outputting a video signal, and a clock signal. The power supply circuit is provided with a signal processing circuit. Alternatively, the power source may be a battery 8011 provided separately. In some cases, the battery 8011 may not be required.
[0353] In addition, the display module 8000 includes components such as a polarizing plate, a retardation plate, and a prism sheet. It may be added.
[0354] (Embodiment 10)
[0355] <Electronic equipment> In this embodiment, one of electronic devices to which a display device according to one embodiment of the present invention can be applied will be described. An example will be described with reference to FIGS. 50 and 51.
[0356] As an example of an electronic device to which a display device is applied, a television device (television or television (also called television receivers), computer monitors, digital cameras, digital video Cameras, digital photo frames, mobile phones (also called mobile phones or mobile phone devices), mobile phones These include portable game machines, mobile information terminals, audio playback devices, and large game machines such as pachinko machines. Specific examples of these electronic devices are shown in Figures 50 and 51.
[0357] FIG. 50A shows a portable game machine. The portable game machine includes a housing 7101, a housing 7102, a display portion 7103, Display unit 7104, microphone 7105, speaker 7106, operation keys 7107, stylus The display device according to one embodiment of the present invention includes the display portion 7103 or the display portion 7 The display portion 7103 or the display portion 7104 can be used as a display device according to one embodiment of the present invention. By using such a display device, a mobile phone that is excellent in usability and is unlikely to experience deterioration in quality can be provided. It is possible to provide a portable game machine. The display unit 7103 and the display unit 7104 are included in the portable game machine. The number is not limited to this.
[0358] FIG. 50B shows a smart watch. The smart watch includes a housing 7302, a display unit 7304, and operation buttons. 7311, 7312, a connection terminal 7313, a band 7321, a clasp 7322, etc. A display device or a touch panel according to one embodiment of the present invention can be used for the display portion 7304. Cut.
[0359] FIG. 50C shows a portable information terminal. In addition to a display portion 7502 incorporated in a housing 7501, , operation button 7503, external connection port 7504, speaker 7505, microphone 7506 The display device according to one embodiment of the present invention can be used for the display portion 7502. Note that the display portion 7502 can be of very high resolution and therefore can be small or medium in size. It is possible to display 8k images while maintaining the resolution, resulting in extremely clear images.
[0360] FIG. 50D shows a video camera, which includes a first housing 7701, a second housing 7702, and a display unit 77 03, operation keys 7704, a lens 7705, a connection part 7706, etc. 4 and a lens 7705 are provided in a first housing 7701, and a display unit 7703 is provided in a second housing. The first housing 7701 and the second housing 7702 are connected to each other. The first housing 7701 and the second housing 7702 are connected by a connector 7706. The angle between the first housing 7701 and the second housing 7702 is The connection portion 7706 can change the image on the display portion 7703. 6, the switch is configured according to the angle between the first housing 7701 and the second housing 7702. The imaging device of one embodiment of the present invention may be provided at the focal position of the lens 7705. The display device according to one embodiment of the present invention can be used for the display portion 7703.
[0361] FIG. 50(E) shows a curved display. The display unit 7802 is built into a housing 7801. In addition, the device is provided with an operation button 7803, a speaker 7804, etc. Such a display device can be used for the display portion 7802.
[0362] FIG. 50(F) shows a digital signage. A display unit 7922 is installed on a utility pole 7921. The display device according to one embodiment of the present invention can be used for the display portion 7922. .
[0363] FIG. 51A shows a notebook personal computer, which includes a housing 8121 and a display unit 8122. , a keyboard 8123, a pointing device 8124, etc. Such a display device can be applied to the display portion 8122. Because it can always maintain high resolution, it can display 8K even though it is small to medium sized. It is possible to obtain very clear images.
[0364] FIG. 51(B) shows the exterior of the automobile 9700. FIG. 51(C) shows the driver's seat of the automobile 9700. The automobile 9700 includes a body 9701, wheels 9702, a dashboard 9703, and a lighter. The display device or the input / output device of one embodiment of the present invention includes an automobile 970 For example, the display units 9710 to 9711 shown in FIG. The display device, the input / output device, or the touch panel according to one embodiment of the present invention is provided in the display portion 9715. It is possible.
[0365] The display portion 9710 and the display portion 9711 are a display device provided on a windshield of an automobile, The display device or the input / output device according to one embodiment of the present invention is a display device or By forming the electrodes of the input / output device from a light-transmitting conductive material, The device is a so-called see-through display device or input / output device that allows the opposite side to be seen through. If it is a see-through display device or an input / output device, the operation of the car 9700 can be Therefore, the display device or input / output device according to one embodiment of the present invention can be used without obstructing the view even when the display device is turned on. The display device can be installed on the windshield of the automobile 9700. A display device or an input / output device is provided with transistors for driving the display device or the input / output device. In this case, organic transistors using organic semiconductor materials and transistors using oxide semiconductors are used. For example, a light-transmitting transistor such as a transistor having a light-transmitting property may be used.
[0366] The display unit 9712 is a display device provided on a pillar part. By displaying an image from the imaging means on the display unit 9712, the view blocked by the pillars can be compensated for. The display unit 9713 is a display device provided in the dashboard. For example, an image captured by an imaging means provided on the vehicle body is displayed on the display unit 9713. This can complement the view obstructed by the dashboard. By projecting images from the installed imaging means, blind spots can be filled and safety can be improved. In addition, by projecting an image that complements the invisible parts, it is possible to make the sense of discomfort more natural. Safety checks can be performed without any hassle.
[0367] FIG. 51(D) shows the interior of a car with bench seats for the driver and passenger. The display unit 9721 is a display device or an input / output device provided in the door section. For example, the driver can view the vehicle by displaying an image captured by an imaging means provided on the vehicle body on the display unit 9721. The display unit 9722 can complement the view blocked by the steering wheel. The display unit 9723 is a display device provided in the center of the seat surface of the bench seat. The display device is installed on the seat or backrest, and the display device is The heat generated by the display device can also be used as a seat heater.
[0368] The display unit 9714, the display unit 9715, or the display unit 9722 displays navigation information, odometer, tachometer, mileage, fuel level, gear status, air conditioning settings, etc. It is possible to provide various information. In addition, the display items and layout displayed on the display unit can be The above information can be displayed on the display unit 9. 710 to 9713, the display unit 9721, and the display unit 9723. In addition, the display units 9710 to 9715 and the display units 9721 to 9723 are illuminated. The display units 9710 to 9715 and the display unit The display portion 9721 to the display portion 9723 can also be used as a heating device.
[0369] The display unit to which the display device according to one embodiment of the present invention is applied may be flat. The display device of this embodiment may not have a curved surface or flexibility.
[0370] Note that the structures and methods described in this embodiment may be different from the structures and methods described in other embodiments. can be used in appropriate combination. EXAMPLES
[0371] In this example, in order to evaluate the moisture barrier property of the protective film 23 according to one embodiment of the present invention, We ran a test and will explain the results.
[0372] The sample was prepared by vacuum-depositing calcium on a glass substrate to a thickness of 80 nm, and then The adhesive for the Drop Fill is applied to the glass substrate, and the substrate is bonded to another glass substrate in a vacuum. The adhesive was then cured. The bonded width at this point was about 1 mm. A protective film 23 was formed to prepare a sample.
[0373] The protective film 23 was an aluminum oxide film formed by the ALD method. MA (Trimethyl Aluminum) and ozone are used for thermal ALD. An aluminum oxide film was then formed to a thickness of 100 nm.
[0374] Figure 52 shows the Ca test measurement results with and without a protective film formed by the ALD method. The vertical axis shows the light transmittance at 60℃ and 90% humidity. The higher the light transmittance, the more moisture there is. Indicates infiltration.
[0375] FIG. 52 shows that when the protective film 23 is not present, the light transmittance tends to increase due to the intrusion of moisture. On the other hand, in the sample having the protective film 23 formed by the ALD method according to one embodiment of the present invention, Therefore, by carrying out one embodiment of the present invention, it is possible to prevent the moisture This has the effect of suppressing intrusion. EXAMPLES
[0376] In this embodiment, a test cell in which a liquid crystal is sealed and in which a protective film 23 according to one embodiment of the present invention is formed is The voltage holding ratio characteristics were evaluated using the following method. The results are described below.
[0377] Table 1 shows an overview of the test cell, and Table 2 shows the measurement conditions.
[0378] [Table 1]
[0379] [Table 2]
[0380] The test cell has a structure in which liquid crystal is sandwiched between transparent electrodes (ITO electrodes), and is an ODF printer. Then, an aluminum oxide film was formed as a protective film 23. The aluminum film was formed by thermal ALD using TMA and ozone as precursors. The temperature was set at 80° C. by the method. The thickness of the aluminum oxide film was 70 nm and 110 nm. In addition, evaluation was performed using two types of liquid crystal: a positive type and a negative type.
[0381] FIG. 53 shows a sample in which a protective film 23 according to one embodiment of the present invention is formed and a positive type liquid crystal is used as the liquid crystal. The voltage holding ratio measurement results of the pull are shown in FIG. 54. The graph shows the results of voltage retention. The horizontal axis shows the storage time at 60°C and 90% humidity, and the vertical axis shows the voltage retention. show.
[0382] 53 and 54, by having the protective film 23, which is one embodiment of the present invention, the positive type liquid crystal, Negative type liquid crystal, none of the liquid crystals showed any change from the start of the storage test. It can be seen that the long-term reliability of the voltage holding ratio is improved. The same effect was obtained at both 100 nm and 110 nm. By providing the protective film 23 in this manner, it becomes possible to hold the voltage more stably, and writing It is possible to improve operational reliability even when driving the device with a reduced number of write operations. EXAMPLES
[0383] In this example, a display device using a liquid crystal element according to one embodiment of the present invention was manufactured. The display results of the position will now be explained.
[0384] Table 3 shows the specifications of the display device using the liquid crystal element. The display device is a high-definition liquid crystal panel. be.
[0385] [Table 3]
[0386] For the display device, an aluminum oxide film is formed as a protective film 23 by the ALD method. The precursors were TMA (Trimethyl Aluminum) and ozone. Using this, an aluminum oxide film was formed to a thickness of about 100 nm at 80° C. by thermal ALD.
[0387] FIG. 55 shows the display result of a display device manufactured using one embodiment of the present invention. As shown in FIG. 55, the side and peripheral parts are sealed using the protective film 23 formed by the ALD method. By suppressing the spread of light, it is possible to realize a display device that has high display quality and high reliability even with a narrow frame. can be obtained. EXAMPLES
[0388] In this embodiment, the side surface of the display panel 20 used in the third embodiment was examined using a scanning electron microscope (S Cross-sectional observation using a scanning electron microscope (SEM), and Energy Dispersive X-ray Spectroscopy The results of elemental mapping analysis using EDX (Energy Dispersion X-ray spectroscopy) He explains.
[0389] For SEM observation, Hitachi High-Technologies Corporation's SU8030 was used. For EDX analysis, The side of the board was made of resin 37 8, and then observation was performed. A schematic cross-sectional view of the observed display panel 20 is shown in FIG. For ease of explanation, transistors, capacitor elements, insulating layers, conductive layers, etc. The regions where are formed are shown as regions 15 and 16. The observation regions are shown in FIG. FIG. 56B shows a schematic diagram of the region 17. The region 17 is a region of the substrate 100. Substrate 300, insulating layer 131, insulating layer 180, protective film 23, insulating layer 330, conductive layer 380, It has an adhesive layer 370 and a resin 378 .
[0390] Figure 57(A) shows a cross-sectional SEM photograph of region 17, and Figure 57(B) shows the EDX image of aluminum. The results of the mapping analysis of oxygen by the EDX method are shown in FIG. 57(C).
[0391] As shown in FIG. 57(A), the region 17 includes the substrate 100, the insulating layer 131, the insulating layer 180, and the adhesive layer 37. 57(B), 57(C), and 57(D). From (C), aluminum and oxygen are connected to the conductive layer 380 and the side surface of the display device. The protective film 23 formed by the ALD method is detected along the deposition layer 370 and the insulating layer 180. It can be seen that the aluminum oxide film having the above thickness is uniformly formed.
[0392] In addition, the upper and lower parts of region 17 were magnified and cross-sectional SEM observations were performed. Further EDX analysis was performed. Figure 58(A) shows an SEM image of the upper part of region 17, and Figure 58(B) shows ) shows the aluminum mapping analysis results by EDX method for the upper part of region 17, and Fig. 58(C) shows The cross-sectional SEM observation result of the lower part of the region 17 is shown.
[0393] 58(A) and 58(B), the insulating layer 330, the adhesive layer 370, the resin 378, the conductive layer 3 In addition to 80, the presence of aluminum was confirmed, and the aluminum oxide film, which is the protective film 23, was attached. The conductive layer 370 and the conductive layer 380 are formed uniformly on the side surface of the display device. Also, from FIG. 58(C), it can be seen that the aluminum oxide protective film 23 is also used in the lower region. It can be seen that the silicon film is formed uniformly.
[0394] From the above, Fig. 57(A), Fig. 57(B), Fig. 57(C), Fig. 58(A), Fig. 58(B), FIG. 58(C) reflects the configuration of FIG. 56(B), and it is confirmed that the present invention can be implemented. It has been confirmed that a display device using one embodiment of the present invention can improve barrier properties and reduce the frame. Even if the number of the wirings is reduced, the reliability can be improved. EXAMPLES
[0395] In this example, the results of evaluating the impurity concentration contained in the protective film 23 will be described. .
[0396] The impurity concentration was evaluated by secondary ion mass spectrometry. The analysis was performed using SIMS (Simulation Imaging Spectrometry) and an ULVAC-PHI Corporation The dynamic SIMS instrument PHI ADEPT-1010 was used. The samples for analysis were A thermal oxide film is formed on the silicon wafer by hydrochloric acid oxidation, and a protective film 23 is formed on the thermal oxide film. Aluminum oxide (AlOx) films formed by the ALD method that can be used as a The aluminum oxide film was formed by deposition using a sputtering method.
[0397] Figure 59 shows the results of SIMS analysis of hydrogen, carbon, and fluorine in an aluminum oxide film.
[0398] As shown in Figure 59, the hydrogen concentration in the aluminum oxide film formed by the ALD method is 1×10 21 a toms / cm 3 About 1×10 carbon concentration 20 atoms / cm 3 degree, fluoride concentration 1×10 20 atoms / cm 3 In addition, the sputtering method The aluminum oxide film formed by the method has different element concentrations, In addition, the difference in the thickness of the aluminum oxide film formed by the ALD method was The impurity concentration can be further reduced, and the reliability of the display device can be improved. This can be done. EXAMPLES
[0399] In this example, the results of measuring the light transmittance after a high-temperature, high-humidity storage test will be described.
[0400] The sample was fabricated with the same specifications as the liquid crystal display shown in Example 3, and was fabricated by the ALD method. The aluminum oxide film and the aluminum oxide film were separately formed. A few pieces of each were prepared. These samples were subjected to high temperature and high humidity storage tests at 60℃ and 90%. Then, the idle stop (IDS) operation was performed at a frame frequency of 0.1 Hz. The light transmittance was measured when the sample was heated. The measurement point was 5 mm inside from the edge of the sample (Figure 60). A)). In addition, when measuring, the halftones (grays) are the areas most likely to experience a difference in light transmittance before and after rewriting. ) was displayed (see Figure 61).
[0401] In addition, the idle stop (IDS) operation is performed after the data writing process is completed. As shown in FIG. 60(B), in the conventional In the case of the driving method of FIG. 60(C), rewriting is required about 60 times per second. By using S drive, the number of rewrites can be reduced, reducing power consumption. can be done.
[0402] Figure 62 shows the results of measuring the light transmittance at various times after storage in a 60°C, 90% humidity environment. In Figure 62, the difference in light transmittance is converted to a difference in gray scale. Aluminum oxide film The sample with the film (Figure 62(A)) had a grayscale difference of about 4 levels before and after writing, On the other hand, the sample without the aluminum oxide film (FIG. 62(B)) has a gradation difference of about 13 gradations. This was a great result.
[0403] Therefore, by using the present invention, it is possible to suppress the change in gray scale, and the liquid crystal display This can improve the long-term reliability of the device. EXAMPLES
[0404] In this example, the temperature at which the aluminum oxide film was formed by the ALD method was changed and each evaluation was performed. The results of this study will be explained below.
[0405] <Aluminum oxide film density> The aluminum oxide film density measurement sample was prepared by oxidizing a silicon wafer using the ALD method. An aluminum film was formed to a thickness of 100 nm. The aluminum oxide film was formed at a temperature of 80° C. The temperatures used were 100° C. and 120° C. The precursors were the same as those in Example 3.
[0406] The density of the aluminum oxide film was measured using X-ray reflectometry. The TRXV-SMX manufactured by Technos was used.
[0407] Figure 63 shows the density of the aluminum oxide film formed at each temperature. The higher the value, the higher the density tends to be.
[0408] <Water permeability of aluminum oxide film> Using the aluminum oxide film formed by the above method, a Ca test measurement similar to that in Example 1 was performed. The measurement results are shown in Figure 64. The horizontal axis represents the storage time at 60°C and 90% humidity, and the vertical axis represents This is light transmittance. The higher the light transmittance, the more moisture has penetrated.
[0409] As shown in Figure 64, the light transmittance is low for the samples with film formation temperatures of 80°C and 100°C. In addition, the sample with the film deposition temperature of 100°C had a low light transmittance. In other words, the aluminum oxide film, which is the protective film, is easily resistant to moisture. It can be said that it acts as a barrier against the penetration of
[0410] As described above, by using one embodiment of the present invention, a highly reliable display device can be provided. can. [Explanation of symbols]
[0411] 10 Display device 11 areas 12 areas 13 areas 14 areas 15 areas 16 areas 17 areas 18 Light blocking layer 20 Display Panel 21 Display area 22 Peripheral circuits 23 Protective film 24 pixels 30 Groove 42 FPC 50 Transistors 51 Transistor 52 Transistor 53 Transistor 54 Transistor 55 Transistor 60 Capacitive element 61 Capacitive element 62 Capacitive element 63 Capacitive element 70 Light emitting element 80 Liquid crystal element 81 Liquid crystal element 90 Input Devices 91 Source Line 92 Gate Line 100 Substrates 101 Substrate 103 Polarizing plate 104 Backlight 105 Protection Board 110 Insulating layer 112 Insulating layer 120 Conductive layer 130 Insulating layer 131 Insulating layer 140 Semiconductor layer 141 Oxide semiconductor layer 142 Oxide semiconductor layer 143 Oxide Semiconductor Layer 150 Conductive layer 160 Conductive layer 165 Insulating Layer 170 Insulating layer 180 Insulating layer 181 Insulating Layer 182 Insulating Layer 190 Conductive Layer 200 Conductive layer 210 Insulating layer 220 Conductive layer 230 layers 240 Spacer 245 Bulkhead 250 EL layer 260 Conductive Layer 300 Substrates 301 Substrate 302 Protection Board 303 Polarizing plate 304 Scattering Film 312 Insulating layer 330 Insulating layer 360 colored layer 370 Adhesive layer 371 Adhesive layer 372 Adhesive layer 373 Adhesive layer 374 Adhesive layer 375 Adhesive layer 376 Adhesive layer 377 Adhesive layer 378 Resin 380 Conductive Layer 390 Liquid crystal layer 400 Conductive Layer 410 Conductive layer 420 Insulating layer 430 Conductive layer 440 Insulating layer 510 Anisotropic conductive film 520 Conductive layer 530 Opening 601 Precursor 602 Precursor 700 Substrates 701 Pixel section 702 Scanning line driver circuit 703 Scanning line driver circuit 704 Signal Line Driver Circuit 710 Capacitance wiring 712 Gate wiring 713 Gate wiring 714 Data Line 716 Transistor 717 Transistor 718 Liquid crystal element 719 Liquid crystal element 720 pixels 721 Switching Transistors 722 Driving Transistor 723 Capacitive element 724 Light emitting element 725 Signal Line 726 scan lines 727 Power line 728 Common electrode 800 boards 810 Introduction 820 Inside the chamber 830 Plasma Source 930 Substrate 931 Electrode 932 Electrode 933 Electrode 934 Bridge Electrode 936 Electrode 937 Electrode 938 Intersection 941 Wiring 942 Wiring 950 FPC 951 IC 1700 Board 1701 Chamber 1702 Road Room 1703 Processing Room 1704 Chamber 1705 Chamber 1706 Unloading Room 1711a Raw material supply section 1711b Raw material supply section 1712a High Speed Valve 1712b High Speed Valve 1713a Raw material inlet 1713b Raw material inlet 1714 Raw material discharge port 1715 Exhaust system 1716 PCB Holder 1720 Delivery Room 3501 Wiring 3502 Wiring 3503 Transistor 3504 Liquid crystal elements 3510 Wiring 3510_1 Wiring 3510_2 Wiring 3511 Wiring 3515_1 Block 3515_2 Block 3516 Block 5200 pellets 5201 AEON 5203 particles 5220 PCB 5230 Target 5240 Plasma 5260 Heating mechanism 7101 Case 7102 Case 7103 Display section 7104 Display section 7105 Microphone 7106 Speaker 7107 Operation key 7108 Stylus 7302 Case 7304 Display section 7311 Operation button 7312 Operation button 7313 Connection terminal 7321 Band 7322 Gold 7501 Case 7502 Display section 7503 Operation button 7504 External connection port 7505 Speaker 7506 Microphone 7701 Case 7702 Case 7703 Display section 7704 Operation key 7705 Lens 7706 Connection 7801 Case 7802 Display section 7803 Operation button 7804 Speaker 7921 Electric pole 7922 Display section 8000 Display Module 8001 Top cover 8002 Lower cover 8003 FPC 8004 Touch Sensor 8005 FPC 8006 Display device 8007 Backlight unit 8008 light source 8009 Frame 8010 Printed Circuit Board 8011 Battery 8121 Case 8122 Display section 8123 Keyboard 8124 Pointing Device 9700 Automobiles 9701 Body 9702 wheels 9703 Dashboard 9704 Light 9710 Display section 9711 Display section 9712 Display section 9713 Display section 9714 Display section 9715 Display section 9721 Display section 9722 Display section 9723 Display section
Claims
[Claim 1] A first substrate and a second substrate, a first insulating layer provided on a first surface of the first substrate; a second insulating layer provided on a first surface of the second substrate; the first surface of the second substrate has an area smaller than that of the first surface of the first substrate; a first surface of the first substrate and a first surface of the second substrate face each other; an adhesive layer is provided between the first insulating layer and the second insulating layer; A display device, wherein a protective film has an area in contact with the first substrate, the first insulating layer, the adhesive layer, the second insulating layer, and the second substrate.
Citation Information
Patent Citations
Display system and electric appliance
JP2001272968A
Semiconductor device and method for manufacturing the same
JP2001290439A
Display device
JP2010282183A
Display device having a moisture barrier layer and method of manufacturing the same
US20140063424A1
Semiconductor device and its manufacturing method
JP2007123861A