Capacitor and manufacturing method thereof
The capacitor design addresses the issues of load and damage on long capacitors by securing the element with a compression element portion, improving vibration resistance and durability, and expanding its applications.
Patent Information
- Application Number
- JP2023086926
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-26
- Publication Date
- 2024-12-06
AI Technical Summary
Long capacitors exceeding 60 mm in length face challenges with increased weight, leading to higher loads on the tab, potential damage, and reduced vibration resistance, which are not adequately addressed by existing technologies.
A capacitor design that includes an outer case with a sealing plate, where the external terminal or tab is pushed into the capacitor element, forming a compression element portion with a specific compression amount to secure the element, enhancing fixation and reducing load on the tab.
The design effectively suppresses movement and load on the tab, improves vibration resistance and durability, and expands the applications of long capacitors by preventing damage and enhancing connection stability.
Smart Images

Figure 2024170016000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a capacitor and a method for manufacturing the same. [Background technology]
[0002] A capacitor such as an electrolytic capacitor includes, for example, a capacitor element housed in an exterior case and a sealing plate that seals the opening of the exterior case. An external terminal attached to the sealing plate is connected to a lead (tab) drawn out from the capacitor element (for example, Patent Document 1). The connection between the external terminal and the lead makes it possible to store electricity in the capacitor element and to extract electricity from the capacitor element. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-44068 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in recent years, there has been a demand for a capacitor with a higher capacity. In addition, the electric and electronic devices and information and communication devices in which capacitors are used are being actively promoted to have higher performance, smaller size, and lighter weight, and there is a demand for smaller and more efficient power supplies for these devices and devices. Therefore, not only is there a demand for a capacitor with a higher capacity, but there is also a tendency for the mounting area of the capacitor on the board to become smaller, and the space for arranging the capacitor tends to be limited due to the arrangement of other electronic components on the board. In order to meet such demands, for example, the capacitor has been made elongated. By placing a capacitor having an elongated external shape upright so that the bottom surface of the outer case is separated from the board, it is possible to reduce the diameter of the mounting area. In addition, by placing the capacitor lying down so that the side of the outer case is parallel to the board, the capacitor can be mounted in the elongated space of the board. However, if an attempt is made to realize a high capacitance of a capacitor in an elongated capacitor, the capacitor element also becomes longer and the weight of the capacitor element also becomes larger. If the capacitor element moves inside the outer case, a load is applied to the lead (tab). The load on the lead increases with the weight of the capacitor element, etc. Therefore, for long capacitors, for example those with a length exceeding 60 millimeters (hereafter referred to as "mm"), measures to reduce the load on the lead (tab) are required that differ from those used for short, normal capacitors.
[0005] Patent Document 1 does not disclose or suggest such a problem, and the configuration disclosed in Patent Document 1 cannot solve such a problem.
[0006] Therefore, a first object of the present disclosure is to suppress the load on the tabs of a long-dimension capacitor having a length exceeding, for example, 60 mm.
[0007] A second object of the present disclosure is to suppress damage to the tabs of, for example, long-dimension capacitors.
[0008] A third object of the present disclosure is to provide a vibration-resistant structure that can withstand an increase in element weight of a long capacitor, for example, and to improve the vibration resistance or durability of the long capacitor.
[0009] A fourth object of the present disclosure is to expand the applications of long-dimension capacitors, for example. [Means for solving the problem]
[0010] In order to achieve the above-mentioned object, according to a first aspect of the present disclosure, a capacitor includes an outer case having a length of more than 60 mm, a sealing plate having an external terminal and fixed to an opening of the outer case, and a capacitor element housed in the outer case and including a tab connected to the external terminal, the capacitor element being fixed between a bottom of the outer case and the sealing plate by pushing in the external terminal or the tab overlapping the external terminal.
[0011] In the capacitor, a compressed element portion may be formed in the capacitor element by pressing in the external terminal or the tab overlapping the external terminal, and the amount of compression in the compressed element portion may be 1.06 mm or more. In the capacitor, the amount of compression may be 1.15 mm or more. In the capacitor, the amount of compression may be 1.81 mm or more. In the capacitor, the amount of compression may be less than 2.82 mm or 2.66 mm or less.
[0012] In the above capacitor, the capacitor element may include a cathode foil having a carbon layer.
[0013] In order to achieve the above object, according to a second aspect of the present disclosure, a method for manufacturing a capacitor includes the steps of: connecting a tab of a capacitor element and an external terminal attached to a sealing plate, inserting the capacitor element into a bottomed cylindrical exterior case, arranging the sealing plate at an opening of the exterior case, bending an end of the opening to fix the sealing plate to the opening, and pushing the external terminal or the tab overlapping the external terminal into the capacitor element to fix the capacitor element by the bottom of the exterior case and the sealing plate. The exterior case has a length exceeding 60 mm after bending the end of the opening.
[0014] The method for manufacturing the capacitor includes the steps of: determining a position for forming a side crimping portion on a side surface of the exterior case based on the following formula so that a compression amount of a compressed element portion of the capacitor element formed by pushing in the external terminal or the tab overlapping the external terminal is 1.06 mm or more: Compression amount=S1-S2=S1-(L2-ABC) S1: The length of the capacitor element before the external terminal or the tab overlapping the external terminal is pressed in. S2: The length of the compression element portion L2: The length of the outer case before bending the edge of the opening A: The distance from the tip of the opening side of the exterior case to the side crimping portion before bending the edge of the opening B: Protruding distance of the external terminal and the tab C: The thickness of the bottom of the outer case The method may further include forming the side crimping portion at the determined formation position. Effect of the Invention
[0015] According to the present disclosure, the following effects can be obtained.
[0016] (1) The capacitor element is fixed in place by pressing in the external terminals. This limits movement of the capacitor element and the load on the tab, thereby preventing damage to the tab.
[0017] (2) The vibration resistance or durability of a long capacitor can be improved.
[0018] (3) The improved vibration resistance and durability can expand the applications of long capacitors. [Brief description of the drawings]
[0019] [Figure 1] FIG. 2 is a diagram illustrating an example of a capacitor according to an embodiment. [Diagram 2] 1A to 1C are diagrams illustrating an example of a manufacturing process for a capacitor. [Diagram 3] FIG. 13 is a diagram showing an example of an experimental result of a capacitor. [Figure 4] FIG. 2 is a diagram illustrating an example of a capacitor element. [Diagram 5] 11A and 11B are diagrams for explaining protrusions of external terminals. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] Fig. 1 shows an example of a capacitor according to an embodiment. In Fig. 1, an outer case 4 and a sealing plate 6 are shown in cross section at the center. In Fig. 1, an end of the outer case 4 before the end crimping portion 14 is formed is shown by a dashed line. The configuration shown in Fig. 1 is only an example, and the technology of the present disclosure is not limited to the configuration shown in Fig. 1.
[0021] The capacitor 2 is, for example, an electrolytic capacitor. The capacitor 2 includes, for example, an exterior case 4, a sealing plate 6, and a capacitor element 8 having a tab 32. The capacitor element 8 is housed inside the exterior case 4, and the sealing plate 6 is disposed and fixed in the opening 10 of the exterior case 4. In addition, the tab 32 pressed against at least the external terminal 22 of the sealing plate 6 is pressed into the capacitor element 8. Therefore, the element end surface 8-1 and the element end surface 8-2 of the capacitor element 8 are in contact with the sealing plate 6 under pressure via the bottom 16 of the exterior case 4, the tab 32, and the external terminal 22, respectively, and the capacitor element 8 is fixed by the bottom 16 of the exterior case 4 and the sealing plate 6. The capacitor 2 has a length L1 that exceeds, for example, 60 mm. The length L1 of the capacitor 2 is equal to the length from the bottom 16 of the exterior case 4 to the apex of the end crimping portion 14 after the end crimping.
[0022] The outer case 4 is, for example, a metal case such as an aluminum case, and is a cylindrical container with a bottom. The outer case 4 has a side crimping portion 12 on the side facing the opening 10, and an end crimping portion 14 on the end facing the opening 10. The side crimping portion 12 determines the position of the sealing plate 6, and the end crimping portion 14 presses the sealing plate 6 against the side crimping portion 12. The outer case 4 may have a fragile portion 18 on a bottom 16 of the outer case 4. The fragile portion 18 breaks when the internal pressure of the outer case 4 rises above a set value, thereby reducing the internal pressure of the outer case 4. The fragile portion 18 prevents the capacitor 2 from bursting.
[0023] The sealing plate 6 is disposed inside the opening 10 of the outer case 4, between the side crimping portion 12 and the end crimping portion 14. The sealing plate 6 is pressed against the side crimping portion 12 by the end crimping portion 14, and is thereby fixed to the opening 10 of the outer case 4. The sealing plate 6 seals the opening 10 of the outer case 4. The sealing plate 6 has a shape corresponding to the shape of the opening 10 of the outer case 4, and for example, has a disk shape with a diameter equal to or close to that of the circular opening 10. The sealing plate 6 may have a shape and size corresponding to the polygonal opening 10. The sealing plate 6 includes, for example, a laminate 20 in which a plurality of members with different functions are laminated, and, for example, two external terminals 22. The laminate 20 includes, for example, a rubber layer 24 and a resin layer 26. The rubber layer 24 has a function of allowing gas to pass through but blocking liquid. The rubber layer 24 is made of a rubber material such as ethylene propylene rubber, butyl rubber, or silicone rubber. The resin layer 26 has a higher rigidity than the rubber layer 24, and is, for example, a paper phenolic resin. The paper phenolic resin is a synthetic material in which a paper base material is impregnated with a phenolic resin. The resin layer 26 may be a single structure made of paper phenolic resin, or may be a laminate structure in which other materials (not shown) are superimposed. The rubber layer 24 is disposed on the outer side of the sealing plate 6 (i.e., on the side of the end crimping portion 14 of the exterior case 4) and forms the outer surface of the sealing plate 6. The resin layer 26 is disposed on the inner side of the sealing plate 6 (i.e., on the side of the capacitor element 8) and forms the inner surface of the sealing plate 6. The laminate 20 has a through hole 27 through which the rivet 30 of the external terminal 22 passes.
[0024] The external terminal 22 includes an electrode terminal 28 and a rivet 30. The electrode terminal 28 is disposed on the outer surface of the sealing plate 6, and functions as an anode terminal or a cathode terminal of the capacitor 2. The electrode terminal 28 has, for example, an L-shape, and has an upright portion that stands upright on the laminate 20 and is for connecting to an external component, and a flat portion that is disposed parallel to the surface of the laminate 20. The flat portion forms a through hole through which the rivet 30 passes.
[0025] The rivet 30 penetrates the laminate 20 and protrudes from the outer surface and the inner surface of the laminate 20. The rivet 30 has flanges 34-1, 34-2, 34-3 and a cylindrical portion 36. The flange 34-1 is disposed on the outer surface side of the sealing plate 6, and the flanges 34-2, 34-3 are disposed on the inner surface side of the sealing plate 6. The cylindrical portion 36 is disposed between the flanges 34-1, 34-2 and between the flanges 34-2, 34-3, and is integrated with the flanges 34-1, 34-2, 34-3. The cylindrical portion 36 penetrates the flat portion of the electrode terminal 28 and the laminate 20, and the flanges 34-1, 34-2 sandwich the flat portion of the electrode terminal 28 and the laminate 20. Therefore, the electrode terminal 28 is fixed to the laminate 20. The cylindrical portion 36 passes through the through hole of the tab 32, and the flange portions 34-2 and 34-3 sandwich the tab 32. Therefore, the tab 32 is fixed to the external terminal 22. That is, the rivet 30 is connected to the tab 32 of the capacitor element 8 by, for example, pressure welding or sandwiching. The connection portion of the tab 32 to the rivet 30 is integrated with the rivet 30 to form the external terminal 22. In this application, the external terminal 22 is defined to include the connection portion of the tab 32 to the rivet 30. The rivet 30 is made of a conductive metal material or has a metal-plated surface, and is electrically connected to the electrode terminal 28 and the tab 32.
[0026] A part of the external terminal 22 is pressed into the element end face 8-2 of the capacitor element 8. The capacitor element 8 is fixed to the bottom 16 of the exterior case 4 and the sealing plate 6 by the pressing of the external terminal 22. The pressing of the external terminal 22 generates a pressure P1 from the sealing plate 6 to the capacitor element 8 and a pressure P2 from the bottom 16 of the exterior case 4 to the capacitor element 8, as shown in FIG. 1. The pressure P2 is a repulsive force of the pressure P1. When the pressing amount of the external terminal 22 is smaller than the protruding distance B of the external terminal 22, the element end face 8-2 is separated from the sealing plate 6 in the portion other than the external terminal 22, as shown in FIG. 1. However, the pressing amount of the external terminal 22 may be larger than the protruding distance B of the external terminal 22, and the element end face 8-2 may contact the sealing plate 6 in the portion other than the external terminal 22.
[0027] A compressed element portion 9 is formed in the capacitor element 8 by pressing in the external terminal 22. The compressed element portion 9 is a capacitor element portion sandwiched between the external terminal 22 and the bottom portion 16, and has a length S2 that is shorter than the length S1 of the capacitor element 8 before the external terminal 22 is pressed in. The compression amount α of the compressed element portion 9 is a distance represented by the difference between the length S1 and the length S2 of the compressed element portion 9 (i.e., the compressed distance), and is represented by the following formula (1): α=S1-S2=S1-(L2-ABC) ···(1) L2: Length of the outer case 4 before the end crimping portion 14 is formed A: Distance from the tip of the opening 10 side of the outer case 4 to the side crimped portion 12 before the end crimped portion 14 is formed B: Protruding distance of the external terminal 22 from the resin layer 26 C: Thickness of the bottom 16 of the outer case 4
[0028] When the compression amount α is large, the pressures P1 and P2 are large, and the fixing force of the capacitor element 8 can be increased. However, when the pressures P1 and P2 are excessively large, the sealing plate 6 is deformed. Specifically, the force generated by the law of action and reaction against the pressure P1 (i.e., the force pressing the sealing plate 6 to the outside) is increased as the pressure P1 is increased. Then, the sealing plate 6 may be warped toward the outside, and the flange portion 34-1 may protrude from the end crimping portion 14. When the flange portion 34-1 protrudes from the end crimping portion 14, a gap may be generated between the end crimping portion 14 and the substrate when the capacitor element 8 is mounted on the substrate, and the substrate mountability may be deteriorated. Therefore, the compression amount α is preferably set within a certain range so that the long-dimension capacitor element 8 for the long-dimension capacitor 2 is sufficiently fixed without being excessively fixed, and is set, for example, in a range of 1.06 mm or more and less than 2.82 mm, or 1.06 mm or more and less than 2.82 mm.
[0029] As shown in Figures 4A and 4B, the capacitor element 8 includes a cathode foil 42, an anode foil 44, and a separator 46. The cathode foil 42, the anode foil 44, and the separator 46 are stacked and wound to form a wound element such that the separator 46 is disposed between the cathode foil 42 and the anode foil 44. This wound element forms the capacitor element 8. The capacitor element 8 has two tabs 32 protruding from the element end surface 8-2. The tabs 32 are connected to the anode foil 44 or the cathode foil 42, and the protruding portions of the tabs 32 are connected to the external terminals 22.
[0030] Cathode foil 42 is an example of an electrode foil, and constitutes the cathode of capacitor 2. Cathode foil 42 is, for example, a strip-shaped foil, and has a base foil and a carbon layer.
[0031] The base foil is the base metal of the cathode foil 42, and is, for example, a valve metal foil such as aluminum foil, tantalum foil, niobium foil, titanium foil, hafnium foil, zirconium foil, zinc foil, tungsten foil, bismuth foil, or antimony foil. The surface of the base foil has irregularities formed, for example, by etching, and the surface area of the base foil is enlarged. The surface of the base foil may include, for example, tunnel-shaped or spongy etching pits, and the tunnel-shaped or spongy etching pits may form the irregularities.
[0032] The carbon layer is disposed, for example, on both sides or one side of the base foil. The carbon layer partially penetrates into the interior of the unevenness, and therefore adheres closely to and engages with the unevenness of the base foil, thereby increasing the strength of the cathode foil 42. The carbon layer contains, for example, a carbon material as a main material, and a binder and a dispersant as additives.
[0033] Carbon materials include activated carbon, carbon black, carbon nanohorns, amorphous carbon, natural graphite, artificial graphite, graphitized Ketjen black, mesoporous carbon, and fibrous carbon. Activated carbon is produced from, for example, natural plant tissue such as coconut shells, synthetic resins such as phenol, and fossil fuels such as coal, coke, and pitch. Carbon black includes Ketjen black, acetylene black, channel black, and thermal black. Fibrous carbon includes carbon nanotubes and carbon nanofibers. Carbon nanotubes may be single-walled carbon nanotubes, which have one graphene sheet, or multi-walled carbon nanotubes (MWCNTs), which have two or more graphene sheets rolled coaxially to form multiple tube walls.
[0034] The binder is a resin-based binder such as styrene butadiene rubber, polyvinylidene fluoride, or polytetrafluoroethylene, which binds the carbon material together. The dispersant is, for example, sodium carboxymethylcellulose.
[0035] The anode foil 44 is an example of an electrode foil and constitutes the anode of the capacitor 2. The anode foil 44 is, for example, the valve metal foil described above, and is a strip-shaped foil. An expanded surface portion having a porous structure is formed on the surface of the anode foil 44. The porous structure is formed, for example, by tunnel-like pits, spongy pits, or voids between densely packed powder particles formed by etching. The surface of the expanded surface portion includes a dielectric oxide film formed by chemical conversion treatment.
[0036] Separator 46 is disposed between anode foil 44 and cathode foil 42 to prevent short circuit between anode foil 44 and cathode foil 42. Separator 46 is an insulating material and includes kraft as a separator material, and may include other separator materials such as manila, esparto, hemp, rayon, cellulose, mixtures thereof, and the like.
[0037] The electrolyte is an electrolytic solution, a gel electrolyte, a solid electrolyte containing a conductive polymer, etc. The electrolyte may include an electrolytic solution or a gel electrolyte, and a solid electrolyte containing a conductive polymer to form a so-called hybrid electrolytic capacitor.
[0038] Fig. 2 shows an example of a manufacturing process for a capacitor. The configuration shown in Fig. 2 is just an example, and the technology of the present disclosure is not limited to the configuration shown in Fig. 2.
[0039] The manufacturing process of capacitor 2 is an example of a manufacturing method of capacitor 2 of the present disclosure, and includes, for example, a process of making outer case 4, a process of making sealing plate 6, a process of making capacitor element 8, a process of connecting sealing plate 6 and tab 32 of capacitor element 8, a process of encapsulating capacitor element 8, and a crimping process.
[0040] In the process of manufacturing the outer case 4, a metal material such as aluminum is, for example, formed into a bottomed cylindrical shape to manufacture the outer case 4 before forming the side crimped portions 12 and the end crimped portions 14. In the process of manufacturing the outer case 4, the outer case 4 before forming the side crimped portions 12 and the end crimped portions 14 may be prepared, for example, by purchase.
[0041] The process of producing the sealing plate 6 includes a step of producing the laminate 20 and a step of attaching the external terminals 22 to the laminate 20.
[0042] In the process of producing the laminate 20, the above-mentioned rubber material for forming the rubber layer 24 is layered on, for example, a paper phenolic resin for forming the resin layer 26, and the rubber material and the paper phenolic resin are heated and pressed to produce a laminate. The produced laminate is punched into the shape and dimensions of the sealing plate 6 by, for example, a press process to produce the laminate 20. In the press process, the laminate is cut by, for example, a shear blade of a press machine. Through holes 27 for passing the external terminals 22 are formed in the laminate 20 by a hole-making device such as a drill or a punching device.
[0043] In the process of attaching the external terminal 22 to the laminate 20, the columnar portion 36 of the rivet 30, which has a columnar portion 36 and a flange portion 34-2 before being crushed, is inserted into the through-hole 27 of the laminate 20 from the resin layer 26 side, and is also inserted into the through-hole in the flat portion of the electrode terminal 28. With the flange portion 34-2 in contact with the resin layer 26, the columnar portion 36 protruding from the flat portion of the electrode terminal 28 is crushed to form the flange portion 34-1. The electrode terminal 28, the rivet 30, and the laminate 20 are integrated by sandwiching the flange portions 34-1 and 34-2. In the state in which the external terminal 22 is attached to the laminate 20, the rivet 30 is made to protrude from the surface of the resin layer 26 so that the tab 32 of the capacitor element 8 can be attached. In the process of producing the sealing plate 6, the sealing plate 6, the laminate 20, the external terminal 22, the rubber layer 24, the resin layer 26, the electrode terminal 28, or the rivet 30 may be prepared, for example, by purchase.
[0044] The process of producing capacitor element 8 includes a step of producing anode foil 44, a step of producing cathode foil 42, a step of producing separator 46, and a lamination step.
[0045] In the process of producing the anode foil 44, for example, an enlarged surface portion having a porous structure is formed on the surface of the valve metal foil described above, and a dielectric oxide film is formed on the surface of the valve metal foil on which the enlarged surface portion is formed by chemical conversion treatment. The enlarged surface portion is formed by direct current etching, alternating current etching, or by vapor deposition or sintering of metal particles on the valve metal foil. In direct current etching or alternating current etching, a direct current or alternating current is typically applied to the valve metal foil immersed in an acidic aqueous solution containing halogen ions such as hydrochloric acid. The valve metal foil on which the dielectric oxide film is formed is cut to produce the anode foil 44.
[0046] In the process of producing the cathode foil 42, a base foil is produced by, for example, forming irregularities on the surface of the valve action metal foil described above by etching. The etching of the cathode foil 42 may be the same as or different from the etching of the anode foil 44. The cathode foil 42 is produced by forming a carbon layer on the base foil, and cutting the base foil and the carbon layer into strips.
[0047] The carbon layer is formed, for example, as follows: The carbon material, binder, and dispersant described above are added to a diluent, and mixed by a dispersion process such as a mixer, jet mixing (jet collision), ultracentrifugation, or ultrasonic treatment to form a slurry. The diluent is, for example, alcohol, a hydrocarbon solvent, an aromatic solvent, an amide solvent, water, or a mixture thereof. The alcohol is, for example, methanol, ethanol, or 2-propanol. The amide solvent is, for example, N-methyl-2-pyrrolidone (NMP) or N,N-dimethylformamide (DMF).
[0048] The slurry is applied to the base foil, the solvent is evaporated to form a carbon layer, and the carbon layer is pressed. The pressing can, for example, force the carbon material into the pores of the unevenness, or, if the carbon material is larger than the pores of the unevenness, can deform the carbon material along the uneven surface of the unevenness. For example, the adhesion and fixation between the carbon layer and the base foil can be improved by forcing the carbon material into the pores of the unevenness or by deforming the carbon material along the uneven surface of the unevenness.
[0049] In the process of producing the separator 46, the separator member described above is cut to produce the separator 46.
[0050] In the lamination process, the anode foil 44, the cathode foil 42, and the separator 46 are stacked so that the separator 46 is disposed between the anode foil 44 and the cathode foil 42, and the anode foil 44, the cathode foil 42, and the separator 46 are wound to produce the capacitor element 8. Before or during the winding, the anode foil 44 and the cathode foil 42 are each connected to a tab 32, and the tab 32 protrudes from the element end surface 8-2. In the process of producing the capacitor element 8, the cathode foil 42, the anode foil 44, the separator 46, or the capacitor element 8 may be prepared, for example, by purchase.
[0051] In the process of connecting the sealing plate 6 and the tab 32 of the capacitor element 8, the columnar portion 36 protruding from the inner surface of the sealing plate 6 is inserted into the through hole of the tab 32. With the flange portion 34-2 in contact with the tab 32, the columnar portion 36 protruding from the tab 32 is crushed to form the flange portion 34-3. The tab 32 and the external terminal 22 are integrated by being sandwiched between the flange portions 34-2 and 34-3.
[0052] 2A, in the process of encapsulating capacitor element 8, capacitor element 8 impregnated with an electrolyte such as an electrolytic solution is inserted into exterior case 4, and sealing plate 6 is placed at opening 10 of exterior case 4. At this time, tab 32 may be folded into the gap between sealing plate 6 and capacitor element 8 for storage.
[0053] In the crimping process, the mounting position of the sealing plate 6 and the formation position of the side crimping portion 12 are determined so that the external terminal 22 or the tab 32 overlapping with the external terminal 22 to form the external terminal 22 is pressed into the capacitor element 8. The mounting position and the formation position may be determined by calculation processing, or may be determined from the relationship between the mounting position and the formation position of the previously manufactured capacitor 2 and the compression amount α of the capacitor element 8. When determining by calculation processing, for example, the mounting position and the formation position are determined by the following formula (2) or formula (3). The length S1, the protruding distance B, and the thickness C are the same as those in formula (1). The distance M is the distance from the outer end of the bottom 16 of the exterior case 4 to the position Po, and is the same as the distance obtained by subtracting the distance A from the length L2 in formula (1). The position Po is the contact position between the sealing plate 6 and the side crimping portion 12, and represents the mounting position on the inner surface of the sealing plate 6 and the formation position of the side crimping portion 12. M <S1+B+C ···(2) M = S1 + B + C - α (3)
[0054] When the position Po is determined so as to satisfy the formula (2), the external terminal 22 can be pressed into the capacitor element 8. Furthermore, when the compression amount α is set to any value within a range of, for example, not less than 1.06 mm and less than 2.82 mm, or not less than 1.06 mm and less than 2.82 mm, and the position Po is determined so as to satisfy the formula (1) or (3), the compression amount α of the capacitor element 8 can be controlled to the set value or a value close to the set value.
[0055] In the crimping step, as shown in B of Fig. 2, side crimping portion 12 is formed at position Po by crimping. Also, as shown in C of Fig. 2, the end of opening 10 of exterior case 4 is bent to form end crimping portion 14. By forming end crimping portion 14, sealing plate 6 is pressed against and fixed to side crimping portion 12, and external terminals 22 are pressed into capacitor element 8, so that capacitor element 8 is fixed between bottom 16 of exterior case 4 and sealing plate 6.
[0056] Fig. 3 shows the experimental results of the capacitor. The experimental results shown in Fig. 3 are merely an example, and the technology of the present disclosure is not limited to such experimental results.
[0057] In order to confirm the action or effect of pushing in external terminal 22, capacitors 2 according to experiment numbers 1 to 19 were fabricated.
[0058] The basic structure of the capacitor 2 according to the experiment numbers 1 to 19 is the same as that of the capacitor 2 already described. The capacitor 2 according to the experiment numbers 1 to 19 has a product diameter of 35 mm and an element diameter of 33.5 mm, and has the product height, element length, anode foil width x, cathode foil width y, separator width z, cathode margin distance w1, element structure, and compression amount α shown in FIG. 3. The product diameter is the diameter of the capacitor 2, and the element diameter is the diameter of the capacitor element 8. The product height is the already-mentioned length L1, and the element length is the already-mentioned length S1. The cathode margin distance w1 is the position difference between the side end 42-1 of the cathode foil 42 and the side end 46-1 of the separator 46 on the element end surface 8-1 side of the capacitor element 8. Regarding the element structure, the cathode foil 42 included in the capacitor element 8 according to the "structure A" has the same or almost the same width as the anode foil 44, as shown in A of FIG. 4. As shown in FIG. 4B, the cathode foil 42 included in the capacitor element 8 according to the "structure B" has a side end 42-1 that overlaps or nearly overlaps the side end 46-1 of the separator 46 on the element end face 8-1 side, and has a width larger than that of the anode foil 44. In the capacitor element 8 according to the "structure B", the cathode foil 42 protrudes from the side end 44-1 of the anode foil 44 on the element end face 8-1 side, and the protruding cathode foil 42 increases the rigidity of the capacitor element 8 in the vicinity of the element end face 8-1. That is, the capacitor element 8 according to the "structure B" has a higher rigidity as a whole than the capacitor element 8 according to the "structure A". On the other hand, in the capacitor element 8 according to the "structure A", the vicinity of the element end face 8-1 is formed only by the separator 46. Therefore, the element portion formed only by the separator 46 absorbs the pressure P1, and the pressure P2, which is the repulsive force of the pressure P1, becomes smaller. Therefore, when capacitor 2 relating to "Structure B" is the same as capacitor 2 relating to "Structure A" except for cathode margin distance w1, capacitor 2 relating to "Structure B" can obtain greater pressures P1 and P2 than capacitor 2 relating to "Structure A", and the fixing force of capacitor element 8 is higher.
[0059] In the element structures of "Structure A" and "Structure B," for example, the cathode margin distance w2 and the anode margin distance v2 are greater than the cathode margin distance w1 and the anode margin distance v1. The anode margin distance v1 is the positional difference between the side end 44-1 of the anode foil 44 and the side end 46-1 of the separator 46 on the element end face 8-1 side. The cathode margin distance w2 is the positional difference between the side end 42-2 of the cathode foil 42 and the side end 46-2 of the separator 46 on the element end face 8-2 side of the capacitor element 8. The anode margin distance v2 is the positional difference between the side end 44-2 of the anode foil 44 and the side end 46-2 of the separator 46 on the element end face 8-2 side. The relatively narrow cathode margin distance w1 and anode margin distance v1 reduce the product height, while the relatively wide cathode margin distance w2 and anode margin distance v2 reduce short circuits between the pressed-in external terminal 22 and the electrode foil.
[0060] In the capacitors 2 according to the experiment numbers 1 to 19, the anode foil 44 has the tunnel-shaped pits described above, and the separator 46 has a density of 0.70 g / cm 3 The electrolyte contains ethylene glycol as a solvent.
[0061] Capacitors 2 according to experiment numbers 1 to 19 were evaluated by vibration tests (standard vibration tests or modified vibration tests). Capacitors 2 according to experiment numbers with an amplitude of "1.0 times" in Fig. 3 were evaluated by the standard vibration test. Capacitors 2 according to experiment numbers with an amplitude of "1.5 times" or "2.0 times" in Fig. 3 were evaluated by the modified vibration test.
[0062] The standard vibration test is a vibration test that complies with "4.8 Vibration" of the Japanese Industrial Standards (JIS) C5101-4:2019 "Fixed capacitors for electronic equipment - Part 4: General rules by type - Fixed aluminum solid (MnO2) and non-solid electrolytic capacitors" and "4.17 Vibration" of JIS C5101-1:2019 "Fixed capacitors for electronic equipment - Part 1: General rules by type". The conditions for the standard vibration test are as follows. The X, Y, and Z directions are as shown in Figure 1. Frequency: 10~55Hz Amplitude or acceleration: Single amplitude 0.75mm or 100m / s 2 (Whichever is looser) Sweep rate: 10Hz-55Hz-10Hz (approximately 1 minute) Sweep direction and test time: (sweep direction) first X direction, then Y direction, and finally Z direction (Test time) 2 hours for each direction (total 6 hours)
[0063] The modified vibration test is the same as the standard vibration test except for the amplitude. In the modified vibration test with an amplitude of "1.5 times", a single amplitude of 1.125 mm is used, and in the modified vibration test with an amplitude of "2.0 times", a single amplitude of 1.50 mm is used. As the amplitude increases, the vibration energy applied to the capacitor 2 increases. In other words, the modified vibration test with an amplitude of "1.5 times" is a stricter test than the standard vibration test, and the modified vibration test with an amplitude of "2.0 times" is a stricter test than the modified vibration test with an amplitude of "1.5 times".
[0064] 3, "Tab damage" is an evaluation item for the capacitor 2. The evaluation result of "Tab damage" indicates the presence or absence of damage to the tab 32 after the vibration test, with the evaluation result "OK" indicating that the tab 32 was not damaged and the evaluation result "NG" indicating that the tab 32 was damaged.
[0065] From the evaluation results of capacitor 2 related to experiment numbers 6 and 8, where standard vibration testing was performed, it was found that when the compression amount α was 1.06 mm or more, the evaluation result for tab damage was "OK". From the evaluation results of capacitor 2 related to experiment numbers 11 to 16, where modified vibration testing (amplitude "2.0 times") was performed, it was found that when the compression amount α was 1.15 mm or more, the evaluation result for tab damage was "OK". From the evaluation results of capacitor 2 related to experiment number 19, where modified vibration testing (amplitude "2.0 times") was performed, it was found that when the compression amount α was 1.81 mm or more, the evaluation result for tab damage was "OK" for capacitor 2 with a product height of 90 mm.
[0066] "Terminal protrusion" in FIG. 3 is an evaluation item for the capacitor 2. The evaluation result of "terminal protrusion" indicates whether or not the flange 34-1 of the rivet 30 protrudes from the case front end 50. The flange 34-1 is a portion that faces or contacts the case front end 50 when the capacitor 2 is connected to, for example, a board. The evaluation result "OK" indicates that the flange 34-1 does not protrude from the case front end 50 as shown in FIG. 5A, and the evaluation result "NG" indicates that the flange 34-1 protrudes from the case front end 50 as shown in FIG. 5B. As shown in FIG. 5A, when the sealing plate 6 is flat (i.e., in a non-curved state), the recession distance R of the flange 34-1 from the case front end 50 is, for example, 0.2 to 0.3 mm. The flange 34-1 protrudes due to the curvature of the sealing plate 6 that receives pressure from the capacitor element 8.
[0067] From the evaluation results of the capacitors 2 according to the experiments 4 to 16, it was found that when the compression amount α was less than 2.82 mm or 2.66 mm or less, the evaluation result for the terminal protrusion was "OK." The protrusion of the flange 34-1 causes the case tip 50 to come into contact with the board when the capacitor 2 is connected to the board, for example, and the connection stability of the capacitor 2 is reduced. In contrast, the non-protrusion of the flange 34-1 causes the case tip 50 to come into contact with the board when the capacitor 2 is connected to the board, for example, and produces the remarkable effect of increasing the connection stability of the capacitor 2.
[0068] The compression amount α is not limited to a range of 1.06 mm or more and less than 2.82 mm. Even if the compression amount α is less than 1.06 mm or is 2.82 mm or more, a certain fixing effect can be obtained by pressing in the external terminal 22 or the tab 32 overlapping with the external terminal 22. Protrusion of the flange portion 34-1 from the case front end portion 50 may be prevented, for example, by increasing the rigidity of the sealing plate 6. Protrusion of the flange portion 34-1 that does not impair the performance of the capacitor 2 may be ignored.
[0069] According to the embodiment, for example, the following effects can be obtained.
[0070] (1) Capacitor element 8 is fixed by pressing in external terminal 22 or tab 32 overlapping external terminal 22. The load on tab 32 due to vibration of capacitor element 8 is suppressed, and damage to tab 32 (e.g., breakage of tab 32) can be suppressed.
[0071] (2) As capacitor element 8 becomes larger, the load on tab 32 increases, for example, when capacitor element 8 vibrates. Pressing in external terminal 22 or tab 32 overlapping external terminal 22 can improve the vibration resistance or durability of long capacitor 2 having a length exceeding 60 mm, and can resolve issues specific to long capacitors.
[0072] (3) By pushing in the external terminal 22 or the tab 32 overlapping the external terminal 22, the vibration state of the tab 32 and the vibration state of the capacitor element 8 can be made as close as possible. Damage to the tab 32 occurs when stress is applied to the tab 32. The application of stress to the tab 32 may be caused by the tab 32 and the capacitor element 8 vibrating separately. Vibration of the capacitor 2 may cause the tab 32 and the capacitor element 8 to vibrate separately or cause vibration resonance. When the tab 32 is exposed to such swinging or vibration resonance, excessive vibration stress is concentrated on the tab 32. As a result, there is a risk of damaging the tab 32. However, by integrating the tab 32 and the capacitor element 8 by pushing in the external terminal 22 or the tab 32 overlapping the external terminal 22, vibration resonance can be suppressed and the stress on the tab 32 can be reduced.
[0073] (4) The improved vibration resistance and durability of the long capacitor 2 can expand the range of uses.
[0074] (5) When flange portion 34-1 of rivet 30 does not protrude from front end portion 50 of the case, contact occurs between front end portion 50 of the case and the board, improving the connection stability of capacitor 2.
[0075] (6) When cathode foil 42 includes a carbon layer, the strength of cathode foil 42 and capacitor element 8 is improved. Therefore, the pressure resistance of capacitor element 8 against pressures P1 and P2 is improved.
[0076] (7) When the cathode margin distance w2 and the anode margin distance v2 are wider than the cathode margin distance w1 and the anode margin distance v1, the product height is reduced and short circuits between the pressed-in external terminal 22 and the electrode foil are reduced.
[0077] The features and modifications of the above-described embodiment will be listed below.
[0078] (1) The outer case 4, the sealing plate 6, the capacitor element 8, the electrolyte, etc. are not limited to those described in the embodiment. These materials may be other materials used in aluminum electrolytic capacitors or similar capacitors. The capacitor element 8 may be, for example, a laminated element in which a plurality of flat cathode foils 42, anode foils 44, and separators 46 are laminated. The material of the carbon layer is not limited to those described in the embodiment. The material forming the carbon layer may be any conductive material containing carbon. The state of adhesion or engagement of the carbon layer with the base foil is not limited to those described in the embodiment. The cathode foil 42 may not include a carbon layer, and may be made, for example, only of the valve action metal foil already described.
[0079] (2) Pressing of the external terminals 22 may be applied to short normal capacitors.
[0080] (3) Capacitor element 8 may be capacitor element 8 according to the already described “Structure A” or capacitor element 8 according to the already described “Structure B”. Capacitor 2 including capacitor element 8 according to “Structure B” can obtain greater pressures P1, P2 than capacitor 2 including capacitor element 8 according to “Structure A”.
[0081] (4) In the embodiment, as shown in FIG. 1, the bottom 16 of the outer case 4 is flat. However, a protrusion may be formed on the bottom 16 of the outer case 4, and the protrusion of the bottom 16 may press the element end surface 8-1 of the capacitor element 8. When the protrusion of the bottom 16 is pressed into the compressed element portion 9, the compression amount α is defined as the compression amount due to both the pressing by the external terminal 22 or the tab 32 overlapping with the external terminal 22 and the pressing by the protrusion of the bottom 16, and is expressed by the above-mentioned formula (1). However, the thickness C of the bottom 16 of the outer case 4 is defined as the thickness of the portion where the protrusion is formed. In the embodiment, the compressed element portion 9 is formed by pressing the external terminal 22 or the tab 32 overlapping with the external terminal 22. However, the compressed element portion 9 may be formed by pressing the external terminal 22 or the tab 32 overlapping with the external terminal 22, together with other elements such as pressing by the protrusion of the bottom 16. The protrusion of the bottom 16 can suppress the pushing load caused by the external terminals 22 or the tabs 32 overlapping with the external terminals 22 .
[0082] (5) Exterior case 4 may have ribs on the inner surface of exterior case 4. The ribs reduce the distance between the inner surface of exterior case 4 and the side of capacitor element 8. As a result, the ribs can suppress movement of capacitor element 8 in the X and Y directions, and improve the vibration resistance of capacitor 2.
[0083] As described above, the most preferred embodiment of the present disclosure has been described. The technology of the present disclosure is not limited to the above description. Based on the gist of the invention described in the claims or disclosed in the specification, those skilled in the art can make various modifications and changes. It goes without saying that such modifications and changes are included in the scope of the present disclosure. [Industrial Applicability]
[0084] INDUSTRIAL APPLICABILITY The technology of the present disclosure is useful in that it can provide a capacitor having vibration resistance or durability. [Explanation of symbols]
[0085] 2. Capacitor 4 Outer case 6 Sealing plate 8 Capacitor elements 8-1, 8-2 Element end face 9 Compression element section 10 Opening 12 Side crimping part 14 End crimping part 16 Bottom 18 Weakened Part 20 Laminate 22 External terminal 24 Rubber layer 26 Resin layer 27 Through hole 28 Electrode terminal 30 Rivet 32 Tabs 34-1, 34-2, 34-3 Flange 36 Cylinder section 42 Cathode foil 44 Anode foil 46 Separator 42-1, 42-2, 44-1, 44-2, 46-1, 46-2 side end 50 Case tip
Claims
1. An outer case having a length exceeding 60 mm; a sealing plate having an external terminal and fixed to an opening of the exterior case; a capacitor element that is housed in the exterior case, includes a tab connected to the external terminal, and is fixed between a bottom of the exterior case and the sealing plate by pressing in the external terminal or the tab that overlaps the external terminal; A capacitor comprising:
2. a compression element portion is formed in the capacitor element by pressing the external terminal or the tab overlapping the external terminal, 2. The capacitor according to claim 1, wherein the compression amount of the compression element portion is 1.06 mm or more.
3. 3. The capacitor according to claim 2, wherein the compression amount is 1.15 mm or more.
4. 4. The capacitor according to claim 3, wherein the compression amount is 1.81 mm or more.
5. 3. The capacitor of claim 2, wherein the compression amount is less than 2.82 mm or equal to or less than 2.66 mm.
6. 6. The capacitor of claim 1, wherein the capacitor element comprises a cathode foil having a carbon layer.
7. a step of connecting a tab of the capacitor element to an external terminal attached to a sealing plate; inserting the capacitor element into a bottomed cylindrical exterior case; placing the sealing plate in an opening of the exterior case; a step of bending an end of the opening to fix the sealing plate to the opening, and pressing the external terminal or the tab overlapping the external terminal into the capacitor element, thereby fixing the capacitor element by a bottom of the exterior case and the sealing plate; Equipped with A method for manufacturing a capacitor, wherein the exterior case has a length exceeding 60 mm after bending the end of the opening.
8. determining a position for forming a side crimping portion on a side surface of the exterior case based on the following formula so that a compression amount of a compression element portion of the capacitor element formed by pressing the external terminal or the tab overlapping the external terminal is 1.06 mm or more; Compression amount = S1-S2 = S1-(L2-A-B-C) S1: Length of the capacitor element before the external terminal or the tab overlapping the external terminal is pushed in S2: Length of the compression element portion L2: The length of the outer case before bending the end of the opening A: Distance from the tip of the outer case on the opening side to the side crimping portion before bending the end of the opening B: Protruding distance of the external terminal and the tab C: Thickness of the bottom of the exterior case forming the side crimping portion at the determined formation position; The method for manufacturing a capacitor according to claim 7, further comprising:
Citation Information
Patent Citations
Electrolytic capacitor
JP2012044068A