Manufacturing device of metal container
The use of a laser-based manufacturing apparatus for metal containers addresses the challenge of producing clear and durable identification marks by discoloring the coating layer, ensuring high visibility and resistance to wear while maintaining efficiency and precision.
Patent Information
- Application Number
- JP2024160732
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2043-04-13
AI Technical Summary
The existing methods for marking metal containers, such as drums, face challenges in producing clear and durable identification marks within a short takt time, as printing techniques like spraying paint or silk screen printing can result in blurred markings and limited expressiveness, and the marks may peel off during use.
A manufacturing apparatus that uses a laser beam in the visible or UV wavelength range to discolor a portion of the metal container's coating layer, forming identification marks within a range of 0.3 μm to 10 μm from the surface, ensuring high durability and precision.
The laser-marked identification marks on metal containers provide excellent durability, visibility, and resistance to rust and rubbing, without affecting the base material, and can be applied efficiently on large surfaces with multiple heads, reducing takt time.
Smart Images

Figure 2024170334000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus for manufacturing metal containers, and more particularly to an apparatus for marking the surface with an identification mark using a laser beam. [Background technology]
[0002] Conventionally, metal containers such as drums and pails are painted in a variety of colors and further have surface identification marks to classify them into different types. There are many combinations of paint colors and surface identification marks, but drums are manufactured while controlling the type of drum according to manufacturing instructions, etc. Surface identification marks are, for example, sprayed with paint, silk screen printed, printed with a stamp, or attached with a sticker. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2003-285811 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the manufacturing process of metal containers such as drums, it is necessary to put complex identification markings on them in a short takt time because it is necessary to put drums of many different colors on one production line. When printing is done on the surface of metal containers by spraying paint, silk screen printing, stamping, etc., there are problems such as the printing being faint and unclear, and there being a limit to expressing complex characters or symbols. In addition, the printing can peel off when the metal container is in use, and there are problems with the durability of the identification markings.
[0005] The present invention is intended to solve the above problems, and has an object to provide an apparatus for manufacturing metal containers having clear and durable identification marks. [Means for solving the problem]
[0006] The metal container manufacturing apparatus of the present invention is an apparatus for manufacturing metal containers that includes a head that emits laser light in the visible or UV wavelength range to be printed on a metal container, and the head irradiates the laser light with a light energy hν greater than the band gap of at least one type of pigment contained in a paint layer, and the metal container includes a main body made of metal and having a cylindrical portion and lid portions attached to close both ends of the cylindrical portion, the main body is formed with the paint layer that constitutes the outer surface of the main body, and includes a discolored portion formed by discoloring a portion including the surface of the paint layer with the laser light of a visible or UV wavelength, and the discolored portion is formed in a range of 0.3 μm to 10 μm from the surface of the paint layer. Effect of the Invention
[0007] According to the present invention, a printing portion is provided by discoloring a portion, including the surface, of a coating layer using laser light of a visible or UV wavelength, thereby obtaining a manufacturing apparatus for metal containers having an identification mark with excellent durability. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is an external perspective view showing an example of a metal container 100 according to a first embodiment. [Diagram 2] 1 is an enlarged view of a cross-sectional structure of a print section 10 of a metal container 100 according to embodiment 1. FIG. [Diagram 3] 1 is a schematic diagram of a laser beam 30 irradiated onto a metal container 100 according to the first embodiment. [Figure 4] 1 is a schematic diagram of a part of an apparatus 90 for manufacturing a metal container 100 according to a first embodiment. [Diagram 5] 1 is a diagram showing an example of a functional configuration related to control of a laser marking process of an apparatus 90 for manufacturing a metal container 100 according to the first embodiment. [Figure 6] 1 is an example of a flowchart of control of a laser marking process of the manufacturing apparatus 90 for the metal container 100 according to the first embodiment. [Figure 7]1 shows examples of the paint colors, paints and components of the metal container 100 according to the first embodiment, and the coloring of the printed portion 10 with each paint color. [Figure 8] 1 shows an example of the appearance of a printing portion 10 of a metal container 100. [Figure 9] FIG. 13 is a diagram showing examples in which laser marking was performed on each paint color and the evaluation results thereof. [Figure 10] FIG. 1 is a diagram showing examples and comparative examples in which printing such as laser marking is applied to each coating color, and the evaluation results thereof. [Figure 11] 1 shows an example of the results of a composition analysis by X-ray diffraction method of a discolored portion of the printed portion 10 of the metallic container 100 according to the first embodiment. [Figure 12] 1 shows an example of the results of a composition analysis by X-ray diffraction method of a discolored portion of the printed portion 10 of the metallic container 100 according to the first embodiment. [Figure 13] 1 is a schematic diagram of a reduction reaction of Fe2O3 caused by irradiation of laser light to the printed portion 10 of the metal container 100 according to the first embodiment. FIG. [Figure 14] 2 shows an example of a laser beam irradiated onto the metal container 100 according to the first embodiment. [Figure 15] 1 shows the band gap of the material contained in the coating layer 21 of the metallic container 100 according to the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The following describes the embodiments based on the drawings. In each drawing, the same reference numerals are used to denote the same or equivalent parts, and this is common throughout the specification. Furthermore, the forms of the components shown in the specification are merely examples and are not limited to these descriptions.
[0010] Embodiment 1 <Configuration of Metal Container 100> FIG. 1 is an external perspective view showing an example of a metal container 100 according to the first embodiment. The metal container 100 according to the first embodiment is, for example, a metal drum, and is exemplified by a drum having a capacity of about 200 L as specified in JIS Z 1601:2017. However, the metal container 100 is not limited to this, and the concept also includes metal containers such as drums, pails, one-gallon cans, and tanks having a capacity of more than 200 L. In addition, drums include not only closed types (tight head drums) in which a base plate and a top plate are joined to a body by rolling and joining, but also open types in which a top plate is detachable from a body.
[0011] 1 is a drum can, and includes a cylindrical portion 101, which is a cylindrical portion called a body, and lid portions 102 at both ends in the central axis direction of the cylindrical portion 101. The lid portion 102 is composed of a lid portion 102A, called a top plate, provided at one end in the central axis direction of the cylindrical portion 101, and a lid portion 102B, called a bottom plate, provided at the other end. The cylindrical portion 101 and the lid portion 102 may be collectively referred to as a main body.
[0012] The lid portion 102 is fixed to both ends of the cylindrical portion 101 by seaming. However, the method of fixing the lid portion 102 is not limited to seaming, and may be performed by using means such as welding, crimping, or brazing. Furthermore, the metal container 100 may be in a form in which the lid portions 102A and 102B are fixed to both ends of the central axis direction of the cylindrical portion 101 to close the cylindrical portion 101, or in a form in which only one of them is fixed.
[0013] The lid 102A has two openings 103 and 104. The openings 103 and 104 are formed, for example, by attaching a cap to a nozzle, and are used as holes for injecting or discharging liquid from one side and for venting air from the other side. The nozzle and cap that form the openings 103 and 104 are formed so as not to protrude beyond a chime 107 that is formed at the end of the cylindrical portion 101 of the metal container 100 and protrudes in the direction of the central axis.
[0014] The tube portion 101 has a generally cylindrical shape and includes a ring zone 105 (bead) protruding toward the middle in the central axis direction. The ring zone 105 is formed around the entire circumference of the cylindrical tube portion 101. The ring zone 105 is provided at multiple locations in the central axis direction. Note that the metal container 100 may not be provided with the ring zone 105.
[0015] Between the zone 105 and the chimes 107 is a cylindrical portion 106 having a generally smooth cylindrical surface.
[0016] 2 is an enlarged view of the cross-sectional structure of the print portion 10 of the metallic container 100 according to embodiment 1. The cylindrical portion 101 of the metallic container 100 includes a metallic base material 20 and a paint layer 21. The base material 20 is made of steel and may have a chemical conversion coating on its surface.
[0017] The coating layer 21 is composed of paints for producing the standard drum colors DM-1 to DM-14, or paints for producing other colors specified by the user, as shown in Fig. 7. The paints constituting the coating layer 21 each contain a pigment required for the corresponding color, and the pigments are compounds such as titanium dioxide, carbon black, yellow iron oxide, ferric oxide, chlorinated phthalocyanine green, copper phthalocyanine (pigment blue 15), iron oxyhydroxide, and polybrominated chlorinated copper phthalocyanine.
[0018] As shown in Fig. 1, a printed portion 10 is provided on a cylindrical portion 101 of a metal container 100. In the first embodiment, the printed portion 10 is formed by discoloring a coating layer 21 by laser marking. In Fig. 1, the printed portion 10 is provided on a drum portion 106, in a portion above a chime 107 on the main plate side.
[0019] As shown in Fig. 2, the printed portion 10 has a discolored portion 22 formed by laser marking, which is a portion including the surface 23 of the coating layer 21 that has been discolored. The discolored portion 22 is formed in a range of 0.3 µm to 10 µm from the surface 23, and is formed so as not to reach the base material 20. In Fig. 2, the surface 23 forms the outer surface of the metal container 100. The discolored portion 22 is also called a discolored layer, and the non-discolored portion of the coating layer 21 on the base material 20 side of the discolored portion 22 is sometimes called a non-discolored layer.
[0020] FIG. 3 is a schematic diagram of the laser light 30 irradiated to the metal container 100 according to the first embodiment. The laser light 30 is composed of a light beam in the wavelength region of visible light or ultraviolet light. Lasers are classified into classes 1 to 4, and the laser light 30 according to the first embodiment is a high-power laser of class 4. The focus of the laser light 30 can be moved relative to the surface 23 of the coating layer 21, as shown in FIGS. 3(a) to 3(c). FIG. 3(a) shows a state in which the focus is focused on the surface 23 of the coating layer 21, FIG. 3(b) shows a state in which the focus is located on the back side of the surface 23 (i.e., the base material 20 side), and FIG. 3(c) shows a state in which the focus is located on the front side of the surface 23. When the focus is located on the back side or the front side of the surface 23 as in FIGS. 3(b) and 3(c), the range on which the laser light 30 hits is wider than when the focus is focused on the surface 23 as in FIG. 3(a). 3 represents the amount of variation in the focal position relative to the state in which the laser light 30 is focused on the surface 23. In other words, as the dimension D increases, the area of the surface 23 that is hit by the laser light 30 becomes wider.
[0021] When the laser light 30 is focused on the surface 23 as shown in Fig. 3(a), the amount of energy given per unit area of the surface 23 is large, but the irradiation area is narrow. Therefore, it is easy to discolor a part of the coating layer 21, but the area of the discolored part 22 may be small and visibility may be low. Therefore, in the metal container 100 according to the first embodiment, the position of the focus of the laser light 30, the output of the laser light 30, and the scanning speed of the laser light 30 are changed according to the ease with which the paint constituting the coating layer 21 discolors, to adjust the visibility of the printed part 10 as a collection of discolored parts 22.
[0022] 4 is a schematic diagram of a portion of an apparatus 90 for manufacturing a metal container 100 according to embodiment 1. The apparatus 90 for manufacturing a metal container 100 includes at least a transport device 40 for moving the metal container 100, a head 31 for irradiating the metal container 100 with a laser beam 30, and a positioning jig 32 for determining the position of the metal container 100 when performing laser marking.
[0023] The conveying device 40 is, for example, a belt conveyor, and moves a plurality of metal containers 100 to a predetermined position where each process is performed. The conveying device 40 is sent to the laser marking process. The conveying device 40 moves the metal container 100 in front of the head 31 that performs laser marking. The moved metal container 100 abuts against the positioning jig 32 and is positioned so that the distance from the head 31 is a predetermined value. The position of the metal container 100 in the feed direction x may be determined by controlling the conveying device 40 or by using the jig 33 that abuts against the metal container 100 from the feed direction x side. The positioning jigs 32 and 33 may be configured so that the distance in the y direction from the head 31 and the position in the x direction are determined with high accuracy. For example, the metal container 100 may be pressed against the positioning jig 32 from the opposite side to the positioning jig 32 to abut against the positioning jig 32.
[0024] The head 31 irradiates the laser light 30 and is disposed to the side of the transport device 40. At least one head 31 is disposed to the side of the transport device 40, and the laser light 30 is irradiated from the head 31 to perform laser marking on the target metal container 100. The manufacturing apparatus 90 according to the first embodiment particularly illustrates a case in which the laser marking step is performed using two heads 31, but is not limited to this.
[0025] In FIG. 4, two heads 31 are arranged side by side in the z direction, and each of them irradiates a single metal container 100 placed on the conveying device 40 with a laser beam 30. The laser beam 30 irradiated from one head can be irradiated to an irradiation range 35 of, for example, 25 cm square. The irradiation ranges 35 of the two adjacent heads partially overlap each other. This configuration can shorten the time required to attach a predetermined identification mark to the printing section 10 of the metal container 100. Even if the area of the printing section 10 is large, the irradiation ranges 35 of the two heads 31 can cover the entire area of the printing section 10, and there is no need to divide the laser marking process into two. In addition, since multiple heads 31 are used to simultaneously print on the printing section 10, it is possible to suppress the characters or symbols printed by the two heads 31 from being misaligned with each other. If two heads 31 are arranged separately for each of the two laser marking processes, the metal container 100 needs to be accurately positioned relative to the heads 31 for each of the two laser marking processes. Therefore, there is a risk that the discolored parts 22 of the printed part 10 formed for each of the two laser marking processes will be misaligned. On the other hand, as described above, since printing is performed simultaneously with multiple laser beams 30 using multiple heads 31, the positional deviation of the markings printed with each laser beam 30 can be minimized.
[0026] Furthermore, when the metal container 100 is a drum, the printing unit 10 needs to display a large amount of information such as JIS, UN, and other marks, numbers, codes, etc. Conventionally, therefore, a method has been used in which a label incorporating identification information is separately attached after printing on the drum with a stamp or the like. On the other hand, according to the head 31 of the first embodiment, the identification mark is printed by the laser light 30, so that detailed characters or symbols can be printed with high accuracy. Furthermore, the manufacturing apparatus 90 shown in FIG. 4 automatically performs the laser marking process, so that the occurrence of problems such as attaching an incorrect label to the metal container 100 can be suppressed.
[0027] The manufacturing apparatus 90 in the first embodiment may be provided with a color identification sensor 36. In the manufacturing apparatus 90, the color identification sensor 36 is disposed at a position corresponding to the metal container 100 before entering the laser marking process, for example. That is, in Fig. 4, the color of the surface of the tube portion 101 of the metal container 100 at position A is detected by the color identification sensor 36. The color identification sensor 36 may be disposed inside the head 31 shown in Fig. 4, and may be disposed at any position as long as the color identification sensor 36 can detect the surface of the metal container 100 that is painted in the same manner as the portion irradiated with the laser light 30.
[0028] The color identification sensor 36, for example, irradiates the surface of the metal container 100 to be irradiated with laser light, detects the reflected light from the surface with a light receiving element, and identifies the color of the surface. The type of the paint layer 21 of the metal container 100 is identified by registering the color of the paint layer 21 of the metal container 100 as a sample in advance, and detecting whether the color of the metal container 100 flowing through the manufacturing device 90 matches any of the registered colors. The control device 50 has a database that associates the registered colors with the irradiation conditions of the laser light 30, and instructs the head 31 on the irradiation conditions corresponding to the color of the paint layer 21.
[0029] The color of the coating layer 21 may be determined by an imaging device 34 provided in the head 31. Also, a color identification sensor 36 may be provided in the head 31.
[0030] The manufacturing apparatus 90 includes a control device 50 for controlling each part of the manufacturing apparatus 90. The control device 50 controls, for example, the irradiation conditions of the laser light 30 of the head 31, the operation of the conveying device 40, and the image capture by the imaging device, and determines the type of the coating layer 21. The control device 50 is communicably connected to each part of the manufacturing apparatus 90, and acquires information of each part and transmits information to each part. The control unit 51 includes, for example, a central processing unit (CPU), a read only memory (ROM), and a random access memory (RAM). The CPU is also called a central processing unit, a central arithmetic unit, a processor, a microprocessor, a microcomputer, or a digital signal processor (DSP). In the control unit 51, the CPU reads out the programs and data stored in the ROM, and uses the RAM as a work area to control the control device 50.
[0031] The storage unit 52 is, for example, a non-volatile semiconductor memory such as a flash memory, an EPROM (Erasable Programmable ROM), or an EEPROM (Electrically Erasable Programmable ROM), and serves as a so-called secondary storage device. In the first embodiment, the storage unit 52 stores information acquired by each unit of the manufacturing apparatus 90. Furthermore, the storage unit 52 stores programs, data, and the like for communication between the control device 50 and each unit constituting the manufacturing apparatus 90.
[0032] FIG. 5 is a diagram showing an example of a functional configuration related to the control of the laser marking process of the manufacturing apparatus 90 for the metal container 100 according to the first embodiment. In the laser marking process of the manufacturing apparatus 90 for the metal container 100, laser marking is performed on the metal container 100 flowing through the manufacturing apparatus 90 by the hardware configuration shown in FIG. 4. The control device 50 communicates with the head 31, the color identification sensor 36, and the conveying device 40 wirelessly or by wire, and controls the laser marking. The control device 50 may have functions other than those shown in FIG. 5, and may communicate with other control devices provided in the manufacturing apparatus 90 and perform the laser marking process in conjunction with the functions realized by the other control devices. In addition, some of the functional blocks provided in the control unit 51 may be provided in a control device provided in other hardware.
[0033] As shown in FIG. 5, the control unit 51 includes a color identification sensor control unit 51a, a color identification unit 51b, an irradiation condition setting unit 51c, a print control unit 51d, and a transport device control unit 51e. The color identification sensor control unit 51a operates the color identification sensor 36 based on information obtained from the transport device control unit 51e regarding the position of the metal container 100 to be laser marked on the transport device 40. The color identification sensor 36 is, for example, a reflective photoelectric sensor, and obtains color information of the surface of the metal container 100 by reflected light and transmits it to the color identification unit 51b. The color identification unit 51b reads out information of the color information data 52a of the specimen stored in the memory unit 52, compares it with the color information obtained by the color identification sensor 36, and transmits it to the irradiation condition setting unit 51c. The irradiation condition setting unit 51c reads out irradiation conditions from the irradiation condition data 52b of the memory unit 52 according to the result of the comparison of the color information, and transmits it to the print control unit 51d. If there is a change in the print design, the print control unit 51d reads out the print design from the print design data 52c and transmits it to the head 31 together with the irradiation conditions.
[0034] The printing control unit 51d commands the head 31 to perform laser marking based on the position information of the metal container 100 to be laser marked, obtained from the transport device control unit 51e. In FIG. 5, the transport device control unit 51e obtains information on the operation of the transport device 40 from the transport device 40, but for example, a sensor may be used to detect the position of the metal container 100 and use it as information on the operation of the transport device 40. The transport device control unit 51e sends at least information on the position of the metal container 100 to be laser marked to the printing control unit 51d. In addition, the transport device control unit 51e sends information on the position of the metal container 100 to be color-identified to the color identification sensor control unit 51a. The transport device control unit 51e operates the transport device 40 upon receiving from the printing control unit 51d that the head 31 has completed laser marking.
[0035] FIG. 6 is an example of a flow chart of the control of the laser marking process of the manufacturing apparatus 90 for the metal container 100 according to the first embodiment. When the metal container 100 to be laser marked on the conveying device 40 reaches a predetermined position, i.e., position A in FIG. 4, the color identification sensor 36 acquires color information of the surface (step S1). The color identification unit 51b compares the color information of the surface of the target metal container 100 with the color information data of the specimen, and determines which of the color information data of the specimen the color of the surface of the target metal container 100 matches. Based on the result of the determination, the irradiation condition setting unit 51c reads out the irradiation conditions from the irradiation condition data 52b (step S2). If the irradiation conditions match the irradiation conditions of the metal container 100 that was laser marked before the target metal container 100 (Yes in step S3), the irradiation condition setting unit 51c does not output the irradiation conditions to the print control unit 51d (step S4). In addition, if the irradiation conditions do not match the irradiation conditions of the metal container 100 that was laser marked immediately before the target metal container 100 (No in step S3), the irradiation condition setting unit 51c outputs new irradiation conditions to the printing control unit 51d (step S5).
[0036] Next, if there is no instruction to change the print design (Yes in step S6), the print control unit 51d does not acquire a print design and maintains the print design that has already been set (step S7). Alternatively, if there is an instruction to change the print design (No in step S6), the print control unit 51d acquires a new print design from the print design data 52c (step S8).
[0037] Next, the printing control unit 51d receives from the transport device control unit 51e a notification that the metal container 100 to be laser marked has reached the appropriate position, and instructs the head 31 to execute printing. At this time, the printing control unit 51d appropriately rewrites the instruction content according to the irradiation conditions and print design set in the processes from step S3 to step S8, and instructs the head 31 (step S9). Note that the print design may be changed, for example, manually from an input device (not shown), or may be programmed in advance in the control device 50 according to the manufacturing plan.
[0038] In the first embodiment, as shown in FIG. 4, the color identification sensor 36 detects the color of the surface of the cylindrical part 101 of the metal container 100 located at a position (position A in FIG. 4) before the position where the laser marking is performed (position B in FIG. 4). In other words, the process from step S1 to step S8 shown in FIG. 6 is completed before the metal container 100 to be laser marked is placed at position B in FIG. 4. With this configuration, the manufacturing device 90 performs color identification of the metal container 100 to be laser marked in advance, and completes the setting of the irradiation conditions when the metal container 100 reaches the position where the laser light 30 is irradiated, thereby shortening the takt time of the entire laser marking process. In addition, it becomes possible to print by laser marking without increasing the overall takt time of the metal container 100.
[0039] The color identification sensor 36 is not limited to targeting the metal container 100 at position A in Fig. 4, and may be, for example, at position B where laser marking is performed. However, when color identification is performed at position B, the time that the metal container 100 remains at position B increases by the time required to perform the processes from step S3 to step S8 shown in Fig. 6.
[0040] 7 shows examples of the paint colors, paints, and ingredients of the metal container 100 according to the first embodiment, and the coloring of the printed portion 10 by each paint color. The paint colors shown are DM-1 to DM-14, which are standard paint colors for drums, and two other colors designated by the user. The color of the discolored portion 22 caused by irradiation with the laser light 30 varies depending on the paint color.
[0041] The color development in the discolored portion 22 is mainly due to (1) foaming, (2) condensation, (3) carbonization, and (4) chemical change. (1) Foaming: When the coating layer 21 is irradiated with the laser light 30, gas bubbles are generated in the substrate due to the thermal effect, causing a whitish rise. In particular, in dark-colored paints, the color changes to a lighter color than the coating color, and visibility is good. (2) Condensation: When the coating layer 21 is irradiated with the laser light 30, the molecular density of the coating layer 21 increases due to the thermal effect, condensing and changing to a dark color. (3) Carbonization: When the coating layer 21 is irradiated with the laser light 30, the irradiated portion of the coating layer 21 is carbonized and discolored black. (4) Chemical change: Discoloration occurs due to the following phenomenon. Since the coating layer 21 contains a pigment substance containing metal ions, irradiation with the laser light 30 causes a change in the valence of the metal ions, a change in the crystal structure, a change in the amount of hydration in the crystal, and the like. As a result, the state of the components contained in the coating layer 21 changes, causing color development. The chemical changes also include photochemical changes in metal compounds contained in the coating layer 21 caused by the light energy of the laser light 30, the mechanism of which will be described later.
[0042] The "Printing Discoloration" column in FIG. 7 indicates whether each coating color changes to black (a darker version of each coating color) or white (a lighter version of each coating color). Whether the darker or lighter color is more easily visible varies depending on each coating color. For example, DM-1 is a white paint, and the coating layer 21 changes to a darker color (black) when exposed to the laser light 30, making the discolored portion 22 easily visible. On the other hand, DM-2 is a black paint, and the coating layer 21 changes to a lighter color (white) when exposed to the laser light 30.
[0043] In addition, the right-hand column of the table in FIG. 7 shows the main compounds contained in the coating layer 21 and their amounts, along with the range of the content ratio.
[0044] Of the standard drum paint colors DM-1 to DM-14, the paint colors other than DM-2 and DM-12, and the paint color designated by user B contain titanium dioxide as an ingredient. Titanium dioxide is chemically changed to titanium pentoxide when irradiated with laser light 30. Titanium dioxide is primarily white, and changes to a dark color such as blackish gray or reddish brown when chemically changed to titanium pentoxide. Therefore, paint colors that contain titanium dioxide as an ingredient tend to have discolored portions 22 change to a relatively black or dark color.
[0045] The coating colors DM-2, DM-3, and DM-9 contain carbon black as an ingredient, which makes it easier for the coating layer 21 to change to white by foaming.
[0046] Of the paint colors, DM-8, DM-9, DM-12, DM-13, and user-specified B paint colors contain yellow iron oxide as a component. Also, DM-5, DM-13, and user-specified A paint colors contain ferric oxide as a component. The yellow iron oxide and ferric oxide change to ferrous oxide or triiron tetroxide when irradiated with laser light 30. Ferrous oxide and triiron tetroxide are black in color and tend to change discolored portion 22 of paint layer 21 to black or a darker color.
[0047] In each coating color shown in FIG. 7, the discolored portion 22 is formed mainly by the change of the above-mentioned components. The discolored portion 22 is formed in the portion irradiated with the laser light 30, and the degree of coloring varies depending on the intensity of the laser light 30, the focal position of the laser light 30, and the scanning speed of the laser light 30. For example, if the amount of energy of the laser light 30 irradiated per unit area is large, the above-mentioned discoloration is more pronounced. Even if the intensity of the laser light 30 is the same, if the focal position of the laser light 30 is not focused, the amount of energy irradiated per unit area decreases, so that discoloration is suppressed. In addition, if the scanning speed is increased, the amount of energy irradiated per unit area decreases, so that discoloration is suppressed. In the metal container 100 according to the first embodiment, the visibility of the printed portion 10 in each coating color can be ensured, and the time required for the laser marking process is adjusted so as not to increase.
[0048] FIG. 8 shows an example of the appearance of the printed portion 10 of the metal container 100. FIG. 8(a) shows an example of the discolored portion 22 when laser marking is applied to the coating color DM-1 shown in FIG. 7, and FIG. 8(b) shows an example of the discolored portion when laser marking is applied to the coating color DM-2 shown in FIG. 7. FIG. 8(c) shows an example of the discolored portion when laser marking is applied to the coating color DM-5 shown in FIG. 7. The tables of discolored samples in FIG. 8(a), (b) and (c) were created by varying the output, scanning speed and focal position of the laser light 30. The sample of the coating color DM-1 is white and a relatively bright color, and is discolored to a dark color by irradiation with the laser light 30, and the discolored portion 22 is formed. The sample of the coating color DM-2 is black, and is discolored to a light color by irradiation with the laser light 30, and the discolored portion 22 is formed.
[0049] In the example of the first embodiment, samples were created using MD-U1020C manufactured by Keyence Corporation. The laser was a YVO4 laser with a wavelength of 355 nm and an output of 2.5 W (at 40 kHz). The printable range was 330 mm x 330 mm in the vertical and horizontal directions and 42 mm in the depth direction. That is, the surface of the cylinder part 101 of the metal container 100 is a cylindrical surface with a depth in the irradiation direction of the laser light 30, but printing by the laser light 30 is possible within a range of 42 mm in the depth direction. The samples were formed by forming the coating layer 21 of each coating color shown in FIG. 7 on a steel plate arranged in the printable range. In addition, the samples No. 27 to No. 30 by the IR laser in FIG. 10 were created using MD-X1020 manufactured by Keyence Corporation. The laser was a YVO4 laser with a wavelength of 1064 nm and an output of 13 W. The printable area is 330mm x 330mm in the vertical and horizontal directions, and 42mm in the depth direction.
[0050] In the table printed on the discolored sample in Fig. 8, the discolored areas 22 shown in each of the columns labeled "A" to "O" in the left-right direction are those irradiated with the laser beam 30 while varying the spot diameter from -21 mm to +21 mm. The central column "H" is the result of irradiation with the minimum spot diameter, that is, with the spot focused on the surface 23.
[0051] In the tables printed on the discoloration samples in the upper rows (a-1) and (b) of Figures 8(a) and (b), the symbols shown in lines "1" to "5" indicate cases in which the scanning speed of the laser light 30 was changed from 2000 mm / min to 6000 mm / min, and the sample in line "5" has a faster scanning speed.
[0052] In the table printed on the discoloration samples in the lower rows (a-2) and (b-2) of Figures 8(a) and (b), the symbols shown in lines "1" to "5" indicate cases in which the output of the laser light 30 was changed from 60% to 100%, and the sample in line "5" has a higher output.
[0053] First, in all discolored samples, the discolored portion 22 of the sample in the "H" row arranged in the left-right direction is less discolored. This is because the spot diameter of the laser light 30 is smaller, the discolored range is smaller, and the discolored area as a whole is smaller. The head 31 irradiates the laser light 30 as a pulse, and when the focus is on the surface 23, the area of the surface 23 irradiated with the laser light 30 per point of the pulse is small, and the discolored portion 22 is difficult to visually recognize. On the other hand, the spot diameter becomes larger toward the "A" row or "O" row of the discolored sample, so the area of the surface 23 irradiated with the laser light 30 per point of the pulse is large, and the discolored portion 22 is easily visually recognized. However, in the relationship between the output of the laser light 30 and the spot diameter, if the energy received per unit area of the surface 23 is lower, the discoloration becomes lighter and difficult to visually recognize. For example, in the tables of discolored samples in the lower rows (a-2) and (b-2), the discolored portion 22 is difficult to visually recognize in and around "1A," "1O."
[0054] As can be seen from the upper rows (a-1) and (b-1) of Figures 8(a) and (b), as the scanning speed increases, the energy received per unit area of the surface 23 decreases and the color becomes lighter.
[0055] As can be seen from the lower rows (a-2) and (b-2) of Figures 8(a) and (b), as the output of the laser light 30 decreases, the energy received by the surface 23 per unit area decreases, and the color becomes lighter.
[0056] Also, as shown in FIG. 8(c), in the example of the discolored portion 22 when laser marking is applied to the coating color DM-5, the tendency of the discolored portion 22 shown in each row of the symbols "A" to "O" in the left-right direction is the same as in the above DM-1 and DM-2, with the "H" row having the lightest color and the color becoming darker toward the "A" row or the "O" row. However, in the case of DM-5, since coloring due to foaming and coloring due to chemical reaction occur simultaneously, whether the coloring due to foaming (white) or the coloring due to chemical reaction (black) predominates depends on the conditions of the scanning speed and intensity of the laser light 30. As for the tendency of coloring, when the amount of energy of the laser light 30 received per unit area of the surface 23 is large, white becomes predominant, and when the amount of energy is relatively low, black becomes predominant. When the output of the laser light 30 is 100%, white becomes predominant in almost the entire area from the "A" row to the "O" row with the spot diameter changed. In addition, DM-15 also produces color due to foaming (white) and color due to chemical changes (black), but in this case the black color is predominant throughout.
[0057] Fig. 9 shows examples in which laser marking was performed on each coating color, and the evaluation results. Fig. 10 shows examples and comparative examples in which printing such as laser marking was performed on each coating color, and the evaluation results. By the manufacturing method of the metal container 100 having the above-mentioned laser marking step, the coating layer 21 was irradiated with laser light 30 for each coating color, and the depth of the discolored part 22 and the thickness of the non-discolored part of the coating layer 21 (the distance from the discolored part 22 to the base material 20) were measured, and the visibility, rust resistance, and rubbing resistance were evaluated. The visibility, rust resistance, and rubbing resistance were evaluated on a scale of "1" to "5," with a rank of "3" or higher being the pass standard.
[0058] The visibility evaluation criteria were based on the ease of visual recognition from a distance of 1m. When visually recognized from a distance of 1m, rank "1" was not visible, rank "2" was difficult to distinguish 10mm characters, rank "3" was distinguishable 10mm square characters, rank "4" was clearly distinguishable 10mm square characters, and rank "5" was clearly distinguishable 5mm square characters.
[0059] The evaluation criteria for rust resistance were to conduct a salt spray test on a sample for the specified time listed below, and then perform tape peeling to observe the difference in peeling between the printed and non-printed areas: Rank "1" is when peeling of the printed area is noticeable after 120 hours of salt spray testing, rank "2" is when peeling of the printed area is noticeable after 168 hours of salt spray testing, rank "3" is when there is no difference between the printed and non-printed areas after 168 hours of salt spray testing, rank "4" is when there is no difference between the printed and non-printed areas after 240 hours of salt spray testing, and rank "5" is when there is no difference between the printed and non-printed areas after 336 hours of salt spray testing.
[0060] Rubbing resistance was evaluated by rubbing the printed surface with a 1kg load in a rubbing test, and the condition of the print was evaluated after a certain number of strokes. The surface of the friction element is made of felt. Rank "1" is when more than half of the print is lost within 10 strokes, rank "2" is when more than half of the print is lost within 50 strokes, rank "3" is when some of the print is lost after 50 strokes but the print is still recognizable, rank "4" is when some of the print is lost after 100 strokes but the print is still recognizable, and rank "5" is when no part of the print is lost after 100 strokes.
[0061] 9 and 10 show the output power [W] of the laser light, the scanning speed [mm / sec], the distance variation amount [mm], and the number of overlapping prints [times]. Each of the evaluation results No. 1 to No. 31 shown in Fig. 9 and 10 is a collection of the results of evaluating multiple samples, and the irradiation conditions and evaluation results are shown with a range.
[0062] In the embodiment shown in Fig. 9, in the case of color development due to foaming or photochemical reaction of the coating layer 21, the visibility is visible even when the discoloration of the discolored part 22 is at the very surface of 0.3 µm to 2.5 µm. In addition, in the case of color development due to foaming or photochemical reaction, there is a tendency for the visibility to be higher if the discolored part 22 is at least 2.5 µm and not more than 10 µm. However, in the case of color development due to foaming, as can be seen from samples Nos. 3, 4, 12, and 13, a certain degree of depth of the discolored part 22 is required, and therefore if the depth of the discolored part 22 is shallow, the visibility tends to be inferior to that due to chemical reaction.
[0063] In the examples shown in Fig. 9, the rust resistance met the standard when the thickness of the non-discolored portion was 2.5 to 5 µm, and the rust resistance was even higher when it was 5 µm or more. However, in the case of discoloration due to a photochemical reaction, there was a tendency for the rust resistance to be high even at a thickness of 2.5 to 5 µm (comparison of samples Nos. 1 to 9 and Nos. 10 to 18). This is because the examples were given points for less damage to the coating layer 21.
[0064] 9, when discoloration occurs due to a photochemical reaction, the rubbing resistance tends to be highly evaluated regardless of the depth of the discoloration. However, when discoloration occurs due to carbonization, the discolored area 22 bleeds due to friction, so although the pass criteria are met, the evaluation is not high.
[0065] In the samples shown in No. 19 to No. 22 in FIG. 10, although the laser light 30 in the UV wavelength region was used, the thickness of the portion (non-discolored layer) other than the discolored portion 22 of the coating layer 21 was thin, and some of them did not meet the pass standard in terms of rust resistance (see samples No. 19 to No. 22). Although the samples No. 19 to No. 22 are inferior to the embodiment shown in FIG. 9 in terms of visibility, rust resistance, and rubbing resistance, they are advantageous in terms of rubbing resistance to the stamp printing shown in No. 31. In addition, since the samples No. 19 to No. 22 are laser marking and do not use ink, etc., compared to printing using ink, such as stamp printing, there is no smearing due to insufficient supply of ink, etc. in the printing process, and they are superior to the sample shown in No. 31 in terms of clear printing.
[0066] In addition, in the samples shown in No. 23 to No. 26 in FIG. 10, although the laser light 30 in the UV wavelength region was used, the thickness of the discolored portion 22 was thin (0.1 μm to 0.3 μm), and the visibility and rubbing resistance tended to be lower than those of the embodiment shown in FIG. 9. Furthermore, as shown in samples No. 23 to No. 26, the samples with coloring due to foaming had lower rubbing resistance than those with coloring due to chemical changes. Although the samples No. 23 to No. 26 are also inferior to the embodiment shown in FIG. 9 in terms of visibility, rust resistance, and rubbing resistance, they are advantageous in terms of rubbing resistance in the case of discoloration due to chemical changes, compared to the stamp printing shown in No. 31. In addition, the samples No. 23 to No. 26 are also laser marked like the samples No. 19 to No. 22, and are superior to the sample shown in No. 31 in that they are clear printed without smudges during the printing process.
[0067] The samples shown in No. 27 to No. 30 in Fig. 10 were printed using an IR (infrared) laser, and the printing was performed by carbonizing or foaming the paint resin due to heat generation. Therefore, in these samples, it was difficult to control the depth dimension of the discolored part 22 within 5 μm from the surface 23, and the depth of the discolored part 22 was 5 μm or more, and the thickness of the paint layer 21 other than the discolored part 22 was easily thin, resulting in low rust resistance and rubbing resistance.
[0068] The sample No. 31 in Fig. 10 is a stamp print. This meets the standards for visibility and rust resistance because it is formed by placing ink on the surface of the coating layer 21. However, it did not meet the standards for rubbing resistance because it depends on the strength of the ink.
[0069] The printed portion 10 of the metal container 100 according to the first embodiment can ensure visibility, rust resistance, and rubbing resistance by performing laser marking so that the depth of the discolored portion 22 is 0.3 μm to 10 μm from the surface. Furthermore, the laser marking may be performed so that the depth of the discolored portion 22 is 0.3 μm to 2.5 μm from the surface, thereby ensuring visibility, rust resistance, and rubbing resistance.
[0070] Moreover, it is preferable that the printed portion 10 of the metal container 100 according to the first embodiment has a thickness of at least 2.5 μm in the coating layer 21 other than the discolored portion 22 (non-discolored layer). This allows the printed portion 10 to maintain good rust resistance and rubbing properties.
[0071] The printed portion 10 of the metal container 100 according to the first embodiment is formed by discoloration due to chemical reaction or foaming using laser light 30 in the visible or UV wavelength region, so it is possible to control the depth of the discolored portion 22 from the surface, and visibility can be ensured while appropriately ensuring the depth of the discolored portion 22. Furthermore, the printed portion 10 of the metal container 100 according to the first embodiment is more prone to discoloration due to chemical reaction than discoloration due to carbonization, and is also highly rubbing-resistant.
[0072] The printed part 10 of the metal container 100 according to the first embodiment is formed by discoloration mainly due to chemical reaction or foaming using the laser light 30 in the visible or UV wavelength region, and the depth of the discolored part 22 is not too deep, and the thickness of the non-discolored layer is sufficiently ensured to ensure rust resistance and rubbing resistance. Therefore, the metal container 100 does not need to have a thick coating layer 21 to ensure the durability of the printed part 10. In the case of laser marking using an IR laser, it is necessary to form the print by foaming or carbonization to ensure the necessary visibility, so it is difficult to control the depth of the discolored part 22 to a range of 0.3 μm to 10 μm, and as can be seen from the samples No. 27 to No. 30 of the comparative example, the discolored part 22 becomes deep and the non-discolored layer becomes thin. Therefore, the printed part using the IR laser is likely to have a thinner non-discolored layer than the printed part 10 of the metal container 100 according to the first embodiment, and is inferior in terms of rust resistance and rubbing properties.
[0073] FIG. 11 shows an example of the results of composition analysis by X-ray diffraction of the discolored portion of the printed portion 10 of the metal container 100 according to the first embodiment. FIG. 11(a) shows the results of analysis by X-ray diffraction in which X-rays are incident on the coating layer 21 before discoloration, and FIG. 11(b) shows the results of analysis by X-ray diffraction in which X-rays are incident on the discolored portion 22 of the coating layer 21 after discoloration. FIG. 11 shows the results of composition analysis of the discolored portion 22 before and after irradiation with the laser beam 30 of the coating color DM-5 as an example. As shown in FIG. 7, DM-5 contains 10 to 15% ferric oxide as a component of the coating layer 21. The coating layer 21 of DM-5 mainly discolors black when irradiated with the laser beam 30, but when the intensity of the laser beam 30 is strong, foaming of the coating layer 21 becomes dominant and the color changes to white. The diagrams shown at the top of Figures 11(a) and (b) are X-ray diffraction patterns of the measurement results obtained from the sample, and the columns shown at the bottom of Figures 11(a) and (b) show the crystal phases identified from the measurement results. Column P shows the position and intensity of the diffraction line of ferric oxide (Fe2O3), and column Q shows the position and intensity of the diffraction line of ferrous oxide (FeO). The horizontal axis of Figures 11(a) and (b) shows the diffraction angle 2θ (°) and displays the range of 5° to 70°. The vertical axis of Figures 11(a) and (b) shows the intensity (CPS) of the diffracted X-rays and displays the range of 0 to 2000 CPS.
[0074] Comparing (a) and (b) of Figure 11, ferrous oxide (FeO) that was not present before irradiation with the laser beam 30 appears after the irradiation {see column Q indicated by the arrow in Figure 11(b)}. Also, the peak of ferric oxide (Fe2O3) attenuates after irradiation {see columns P in Figures 11(a) and (b)}. In other words, the following reduction reaction occurs in the coating layer 21 of DM-5 due to the irradiation with the laser beam 30. Fe2O3+ e- → 2FeO + 1 / 2O 2- ... (Formula 1) The ferric oxide is reduced to ferrous oxide by irradiation with the laser beam 30. Therefore, the discolored portion 22 exhibits a black color.
[0075] FIG. 12 shows an example of the results of composition analysis by X-ray diffraction of the discolored portion of the printed portion 10 of the metal container 100 according to the first embodiment. FIG. 12(a) shows the results of analysis by X-ray diffraction in which X-rays are incident on the coating layer 21 before discoloration, and FIG. 12(b) shows the results of analysis by X-ray diffraction in which X-rays are incident on the discolored portion 22 of the coating layer 21 after discoloration. FIG. 12 shows the results of composition analysis of the discolored portion 22 before and after irradiation with the laser beam 30 of the coating color DM-12. As shown in FIG. 7, DM-12 contains 5 to 10% yellow iron oxide as a component of the coating layer 21. The coating layer 21 of DM-12 mainly discolors black when irradiated with the laser beam 30, but if the intensity of the laser beam 30 is strong, foaming of the coating layer 21 becomes dominant and the color may change to white. The diagrams shown at the top of Figures 12(a) and (b) are X-ray diffraction patterns obtained from the samples, and the columns shown at the bottom of Figures 12(a) and (b) show the crystal phases identified from the measurement results. Column P shows the position and intensity of the diffraction line of ferric oxide (Fe2O3), column Q shows the position and intensity of the diffraction line of ferrous oxide (FeO), and column R shows the position and intensity of the diffraction line of yellow iron oxide (Fe2O3·H2O). The horizontal axis of Figures 12(a) and (b) shows the diffraction angle 2θ (°), ranging from 5° to 70°. The vertical axis of Figures 12(a) and (b) shows the intensity (CPS) of the diffracted X-rays, ranging from 0 to 2000 CPS.
[0076] Comparing (a) and (b) of FIG. 12, ferrous oxide (FeO), which was not present before the irradiation with the laser beam 30, appears after the irradiation {see column Q of FIG. 12(b)}. Also, after the irradiation, Fe 3+ The peak of O(OH) is attenuated (see column R in Figures 12(a) and 12(b)). In other words, the following reduction reaction occurs in the coating layer 21 of DM-12 due to the irradiation of the laser beam 30. Fe2O3·H2O+e - → 2FeO+1 / 2O 2- +H2O ... (Formula 2) Yellow iron oxide (Fe2O3·H2O) is reduced to ferrous oxide by irradiation with laser light 30. Therefore, discolored portion 22 exhibits a black color.
[0077] Fig. 13 is a schematic diagram illustrating the reduction reaction of Fe2O3 by laser irradiation of the printed portion 10 of the metal container 100 according to the first embodiment. Looking at the analysis results shown in Figs. 11 and 12, each of the ferric oxide and yellow iron oxide contained in the coating layer 21 is reduced by irradiation with the laser light 30. This is because the light energy hν of the laser light 30 is larger than the band gap Eg of the substance (here, each of the ferric oxide and yellow iron oxide), so that electrons in the valence band are excited to the conduction band and become free electrons, causing a reduction reaction. Here, h is the Planck constant, and ν is the frequency of the laser light 30.
[0078] Fig. 14 is an example of a laser beam irradiated to the metal container 100 according to the embodiment 1. The laser beam 30 irradiated in the example shown in Fig. 9 is a YVO4 laser beam in the UV wavelength region (355 nm), and the light energy hν is 3.49 eV.
[0079] FIG. 15 shows the band gap of the substance contained in the coating layer 21 of the metal container 100 according to the first embodiment. In general, in semiconductors and insulators, the energy level from the outermost shell of the valence band to the bottom of the conduction band is large, and in order for electrons to transition from the valence band to the conduction band, it is necessary to absorb energy (light or heat) equal to or greater than the band gap Eg. For example, in the case of the coating layer 21 of the coating color DM-5, the analysis result of which is shown in FIG. 11, the band gap of the contained ferric oxide is 2.0 to 2.2 eV. Therefore, with the laser light 30 of the manufacturing apparatus 90 according to the first embodiment, the light energy hν exceeds the band gap of ferric oxide, and a reduction reaction can be caused in the coating layer 21. Note that the laser light 30 of the manufacturing apparatus 90 according to the first embodiment can cause a reduction reaction in the coating layer 21 even when the output is suppressed, and can be adjusted so that blackening by photochemical reaction is more prevalent than whitening by foaming.
[0080] Also, a YAG laser or YVO4 laser with a wavelength of 532 nm, and an argon laser with wavelengths of 488 nm, 514.4 nm, and 315 nm shown in Fig. 14 can cause a reduction reaction in ferric oxide in the same manner as described above. In other words, it is also possible to use a laser beam 30 with a wavelength in the visible light region, so long as the light energy hν of the laser beam 30 exceeds the band gap of the discoloring substance contained in the coating layer 21. In other words, the embodiment shown in Fig. 9 above can achieve color development by a photochemical reaction even if a laser beam 30 with a visible light wavelength region is used instead of a laser beam 30 with a UV wavelength region.
[0081] On the other hand, in the case of the laser light 30 having a wavelength of 1064 nm or 10600 nm shown in Fig. 14, the light energy hν is not enough to exceed the band gap of the material shown in Fig. 15, for example, so discoloration due to the reduction reaction shown in (Equation 1) and (Equation 2) above does not occur. In this case, discoloration occurs by carbonizing or foaming the resin that constitutes the coating layer 21 due to the thermal energy of the laser light 30.
[0082] In addition, if a 355 nm YAG laser or YVO4 laser with high light energy hν is used, it can also promote a chemical reaction of titanium dioxide (TiO2), which is contained in the paint colors DM-1 to DM-14 shown in Figure 7 except for DM-2 and DM-12, as well as the user-specified paint color B.
[0083] As described above, according to the metal container 100, the manufacturing apparatus 90 for the metal container 100, and the printing method for the metal container 100 of the first embodiment, the discolored portion 22 can be provided in the coating layer 21 by laser marking, which can prevent the printing from fading during transportation and use of, for example, a drum can. For example, when the printed portion 10 is formed by stamping, silk screen printing, or other means, ink for identification is placed on the surface of the coating layer 21, and the ink is easily removed by rubbing, etc., and the durability of the printed portion 10 is low. On the other hand, the printed portion 10 by laser marking of the first embodiment has excellent visibility, rust resistance, and rubbing resistance, as shown in FIG. 9.
[0084] Furthermore, according to the metal container 100, the manufacturing apparatus 90 for the metal container 100, and the printing method for the metal container 100 of the first embodiment, the discolored portion 22 is provided in an area of 5 μm or less from the surface 23 of the coating layer 21, so that the metal that is the base material 20 of the metal container 100 is not damaged. Furthermore, the laser marking process does not expose the base material 20, and the thickness of the undiscolored coating layer 21 from the discolored portion 22 to the surface of the base material 20 can be sufficiently ensured. This makes it possible to suppress damage such as rusting and corrosion from the printed portion 10 even if the metal container 100 is used for a long period of time.
[0085] Moreover, according to the metal container 100, the manufacturing device 90 for the metal container 100, and the printing method for the metal container 100 of the first embodiment, the laser light 30 in the visible light or UV wavelength region is used, and the light energy hν causes at least one substance contained in the coating layer 21 to undergo a chemical reaction and discoloration, so that damage to not only the base material 20 but also the coating layer 21 itself is suppressed. The coating layer 21 contains a resin that constitutes the paint, and the coating layer 21 of each coating color shown in FIG. 7 may contain an aminoalkyd resin as an example. Moreover, the coating layer 21 is preferably 30 μm or less, and more preferably 20 μm or less in consideration of the surface strength, weight, and cost of the coating layer 21.
[0086] In addition, the laser marking process directly discolors the paint of the coating layer 21, and therefore does not require consumables such as ink or cleaning fluid, and therefore has the advantage of not incurring costs for consumables and the management of consumables. In addition, by arranging a plurality of heads 31 for laser marking and processing the printed portion 10 in one process, even if the printed portion 10 has a large area and a large amount of information to be printed, a highly accurate printed portion 10 can be obtained without affecting the takt time of the metal container 100. Furthermore, the laser marking process uses a YAG laser, a YVO4 laser, or an argon laser including the wavelength range shown in FIG. 14, and the metal container 100 has a discolored portion 22 caused by a photochemical reaction using the light energy hν of the laser light 30. Therefore, the printed portion 10 discolors only a part of the coating layer 21 to provide an identification mark, and therefore does not impair the performance of the metal container 100. Note that the discolored portion 22 of the metal container 100 is not limited to discoloration caused by only photochemical reactions, and may also include discoloration caused by other chemical reactions.
[0087] In the metal container 100 according to the first embodiment, the printed portion 10 is provided on the side surface of the cylindrical portion 101, but the printed portion 10 may be provided on the lid portion 102.
[0088] Although the present invention has been described above based on the embodiments, the present invention is not limited to the configurations of the above-mentioned embodiments. In particular, the combination of components is not limited to the combinations in the embodiments, and the components described in each embodiment can be modified as appropriate. For example, it is to be noted that the gist (technical scope) of the present invention also includes various modifications, applications, and uses that a person skilled in the art may make as necessary. [Explanation of symbols]
[0089] 10 Printing section, 20 Base material, 21 Paint layer, 22 Discolored section, 23 Surface, 30 Laser light, 31 Head, 32 Positioning jig, 33 Jig, 34 Imaging device, 35 Irradiation range, 36 Color discrimination sensor, 40 Conveying device, 50 Control device, 51 Control section, 51a Color discrimination sensor control section, 51b Color discrimination section, 51c Irradiation condition setting section, 51d Printing control section, 51e Conveying device control section, 52 Memory section, 52a Color information data of specimen, 52b Irradiation condition data, 52c Printing design data, 90 Manufacturing device, 100 Metal container, 101 Tube section, 102 Lid section, 102A Lid section, 102B Lid section, 103 Opening, 104 Opening, 105 Ring, 106 Section, 107 Chime.
Claims
1. A head is provided for emitting laser light in the visible or UV wavelength range for marking on a metal container, The head is than the band gap of at least one pigment contained in the coating layer, An apparatus for manufacturing a metal container, which irradiates the laser light having a large light energy hν, The metal container comprises: The device includes a main body made of metal and having a cylindrical portion and a cover portion attached to close both ends of the cylindrical portion, The body includes: The coating layer constituting the outer surface of the main body is formed, a discolored portion formed by discoloring a part including a surface of the coating layer by the laser light having a visible light or UV wavelength; The discolored portion is An apparatus for manufacturing metal containers, the coating layer being formed in an area of 0.3 μm or more and 10 μm or less from the surface.
2. The head is A plurality of heads arranged side by side, Among the multiple heads, two adjacent heads are The metal container manufacturing apparatus according to claim 1 , wherein the laser beam irradiatable areas are arranged so as to overlap each other.
3. A control device for controlling the head; A color identification sensor for identifying the color of the surface of the coating layer, The control device includes: The type of the coating layer is identified by the color identification sensor; 3. The apparatus for manufacturing a metal container according to claim 1, wherein the laser light is irradiated at a focal position according to the type of the coating layer.
4. The control device includes: The type of the coating layer is identified by the color identification sensor; The metal container manufacturing apparatus according to claim 3 , wherein the laser light is irradiated with an output corresponding to the type of the coating layer.
5. The control device includes: The type of the coating layer is identified by the color identification sensor; The metal container manufacturing apparatus according to claim 3 , wherein the laser light is irradiated at a scanning speed according to the type of the coating layer.
6. The metal container manufacturing apparatus according to claim 3 , further comprising a jig against which the metal container abuts, for ensuring a distance between the head and the main body.
Citation Information
Patent Citations
Laser beam marking member
JP1990041785A
Transition metal oxide photochromic material and photochromic method and device using the same
JP2001303033A
Remote write and erase device
JP2004306574A
Tabular transfer original plate for security card, method for manufacturing tabular transfer original plate for security card, and method for manufacturing security card
JP2014168927A
Drum type discriminating system and method, and drum
JP2003285811A