Dynamically crosslinkable polymer compositions, articles, and methods thereof

Dynamically crosslinkable polymer compositions using thermoplastic polymers with ionic or metal-ligand interactions facilitate the reprocessing of crosslinked polymers, addressing environmental waste and cost issues by maintaining mechanical properties.

JP2024534883AInactive Publication Date: 2024-09-26BRASKEM SA
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2024513801
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-09-01
Filing Date
2022-09-01
Publication Date
2024-09-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Crosslinked polymers, such as ethylene vinyl acetate (EVA) foams, are difficult to reprocess and recycle due to their persistent network structures, leading to environmental waste and increased manufacturing costs.

Method used

Development of dynamically crosslinkable polymer compositions using thermoplastic polymers with monomers like C2-C12 olefins and vinyl esters, crosslinked through ionic bonding or metal-ligand interactions, which allow reprocessing at elevated temperatures without being sensitive to molecular oxygen.

Benefits of technology

Enables the reprocessing of crosslinked polymers, maintaining at least 40% of the initial storage modulus after multiple cycles, reducing waste and lowering recycling costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024534883000001
    Figure 2024534883000001
Patent Text Reader

Abstract

The polymer composition is vinyl ester, C2-C 12 The thermoplastic polymer may include at least one monomer selected from the group consisting of olefins, and combinations thereof; and a dynamic crosslinking group; and a crosslinking agent that dynamically crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions.
Need to check novelty before this filing date? Find Prior Art

Description

[Background technology]

[0001] Ethylene vinyl acetate (EVA) is widely used to produce foams that are lightweight and have very high toughness, resilience, and compression set. EVA foams find application in demanding applications such as running shoe insoles, as well as automotive and architectural applications such as interior padding, carpet underlay, and gaskets. The polymer structure required for EVA foam and other compact elastomer applications that require high heat resistance is a three-dimensional network created by cross-linking adjacent polymer molecules.

[0002] Covalently bonded polymer networks offer a balance of performance, properties, and durability. However, the same characteristics that make persistent networks excellent candidates in the selection of materials for high performance foams also present difficult environmental challenges. Once formed, these network structures cannot melt, flow, or dissolve, making them amenable to traditional reprocessing or recycling methods.

[0003] The molding process for manufacturing footwear insoles generates debris. The debris generated during processing of permanent networks cannot be fully reintroduced into the manufacturing process as secondary raw material because they are difficult to process. Only a small amount of waste debris from crosslinked polymers is ground and reintroduced as filler. Similarly, end-of-life parts manufactured from permanently crosslinked polymers have limited recycling options, such as energy-intensive grinding operations that produce low-value materials. As a result, a significant proportion of debris and used parts accumulate as environmental waste.

[0004] In addition to the significant environmental impact, the inability of covalently bonded, crosslinked EVA foam to be reprocessed by melting represents a significant cost to manufacturers, resulting in significant waste, limiting the utilization of primary materials and incurring waste handling costs. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] U.S. Patent Application Serial No. 17 / 063,488 [Non-patent literature]

[0006] [Non-Patent Document 1] GUO et al., 2019 - https: / / pubs.acs.org / doi / abs / 10.1021 / acs.macromol.9b02281 Summary of the Invention [Problem to be solved by the invention]

[0007] There is a need for technology that allows for the reprocessing of crosslinked polymers, particularly crosslinked EVA foam. [Means for solving the problem]

[0008] This Summary is provided to introduce a selection of concepts that are further described below in the Detailed Description. This Summary is not intended to identify key or essential features of the claimed subject matter, nor is it intended to be used as an aid in limiting the scope of the claimed subject matter.

[0009] In one aspect, embodiments disclosed herein relate to a polymeric composition comprising at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof, and a thermoplastic polymer comprising a dynamic crosslinking group. The polymeric composition further comprises a crosslinking agent that dynamically crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions.

[0010] In another aspect, embodiments disclosed herein relate to a polymeric composition comprising at least one monomer selected from vinyl esters, C2 to C12 olefins, and combinations thereof, and a thermoplastic polymer comprising a dynamic crosslinking group; and a crosslinking agent that crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions, wherein the crosslinking is relatively insensitive to the presence of molecular oxygen.

[0011] In another aspect, embodiments disclosed herein relate to a method for making a polymer composition comprising processing a crosslinking system with a thermoplastic polymer to form a polymer composition comprising at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof, and a thermoplastic polymer comprising dynamic crosslinking groups, the polymer composition further comprising a crosslinking agent that dynamically crosslinks the thermoplastic polymer by ionic bonds or metal-ligand interactions, the processing being at a first temperature that is less than a second temperature sufficient to form crosslinks in the polymer composition.

[0012] In another aspect, embodiments disclosed herein relate to a method for making a polymer composition, comprising processing a crosslinking system with a thermoplastic polymer to form a polymer composition comprising: a thermoplastic polymer comprising at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof; a crosslinking agent that crosslinks the thermoplastic polymer by ionic bonds or metal-ligand interactions; and the crosslinking is relatively insensitive to the presence of molecular oxygen. The processing is at a first temperature that is lower than a second temperature sufficient to form crosslinks in the polymer composition.

[0013] In another aspect, embodiments disclosed herein relate to a method of making a polymer composition comprising processing the polymer composition above its melting or softening temperature and crosslinking the polymer composition in the presence of molecular oxygen. The polymer composition comprises at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof, and a thermoplastic polymer comprising a dynamic crosslinking group. The polymer composition further comprises a crosslinking agent that dynamically crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions.

[0014] In another aspect, embodiments disclosed herein relate to a method of making a polymer composition comprising processing the polymer composition above its melting or softening temperature and crosslinking the polymer composition in the presence of molecular oxygen, the polymer composition comprising: a thermoplastic polymer comprising at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof; a crosslinking agent that crosslinks the thermoplastic polymer by ionic bonds or metal-ligand interactions; and the crosslinking is relatively insensitive to the presence of molecular oxygen.

[0015] In yet another aspect, embodiments disclosed herein relate to a method of reprocessing a polymer composition comprising reprocessing the polymer composition above the melting or softening temperature of the thermoplastic polymer, wherein after the reprocessing step, the polymer composition maintains at least 40% of its initial storage modulus plateau above its melting temperature as compared to the polymer composition prior to the reprocessing step, as measured by dynamic mechanical analysis. The polymer composition comprises at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof, and a thermoplastic polymer comprising a dynamic crosslinking group; and a crosslinking agent that dynamically crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions.

[0016] In yet another aspect, embodiments disclosed herein relate to a method of reprocessing a polymer composition comprising reprocessing the polymer composition above the melting or softening temperature of a thermoplastic polymer, wherein after repeating the processing step at least two additional times, the polymer composition maintains at least 40% of its initial storage modulus plateau above its melting temperature as compared to the polymer composition prior to the reprocessing step, as measured by dynamic mechanical analysis. The polymer composition comprises a thermoplastic polymer comprising at least one monomer selected from vinyl esters, C2-C12 olefins, and combinations thereof, and a crosslinking agent that crosslinks the thermoplastic polymer by ionic bonds or metal-ligand interactions, wherein the crosslinking is relatively insensitive to the presence of molecular oxygen.

[0017] In yet another aspect, embodiments disclosed herein relate to an article comprising a polymeric composition comprising at least one monomer selected from vinyl esters, C2 to C12 olefins, and combinations thereof, and a thermoplastic polymer comprising a dynamic crosslinking group; and a crosslinking agent that dynamically crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions.

[0018] In yet another aspect, embodiments disclosed herein relate to an article comprising a polymeric composition comprising a thermoplastic polymer comprising at least one monomer selected from vinyl esters, C2 to C12 olefins, and combinations thereof, and a crosslinking agent that crosslinks the thermoplastic polymer through ionic bonds or metal-ligand interactions, wherein the crosslinking is relatively insensitive to the presence of molecular oxygen.

[0019] Other aspects and advantages of the claimed subject matter will become apparent from the following description and the appended claims. [Brief description of the drawings]

[0020] [Figure 1] 1 is a graph showing a comparison of DSC cooling curves for a thermoplastic polymer control, EVA, and EVA crosslinked with 1.5 and 3% Zn acrylate. [Diagram 2] 1 is a graph showing a comparison of DSC heating curves (second melt) of a thermoplastic polymer control, EVA, and EVA crosslinked with 1.5 and 3% Zn acrylate. [Diagram 3] 1 is a graph showing the results of a shear rheology test. [Figure 4] 1 is a graph showing DMA storage modulus versus temperature. [Diagram 5] 1 is a graph showing DMA loss modulus versus temperature. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] The embodiments disclosed herein relate to polymer compositions, methods of forming and reprocessing such polymer compositions, and articles formed from such polymer compositions. The polymer composition may be a thermoplastic polymer comprising at least one monomer selected from the group consisting of dynamically crosslinked vinyl esters, C2-C12 olefins, and combinations thereof. According to embodiments of the present disclosure, the dynamic crosslinking reaction is relatively insensitive to the presence of molecular oxygen. As used herein, the term "relatively insensitive" means that the polymer composition has a tackiness number greater than 5.

[0022] Dynamically crosslinked systems are a type of chemically crosslinked polymers in which an external stimuli (temperature, stress, pH, etc.) can trigger bond exchange reactions, allowing the topology of the network to change while keeping the number of bonds and crosslinks constant. The dynamic ionic or metal-ligand bonds present can undergo associative exchange reactions, such that the topology of the network can change and the material can flow under stress relief. Dynamically crosslinked systems exhibit the characteristics of crosslinked materials at room temperature (high chemical resistance, exceptional mechanical properties), but can be processed or reprocessed as thermoplastic materials at elevated temperatures.

[0023] According to one or more embodiments, the polymer composition can be prepared by mixing a thermoplastic polymer with a crosslinking system. The crosslinking system can include a crosslinking agent and a catalyst. The thermoplastic polymer can include dynamic crosslinking groups and / or dynamic crosslinking groups can be grafted thereto. The crosslinkable polymer composition can be prepared via a method that includes processing the crosslinking system with a thermoplastic polymer. Crosslinking of the polymer composition can include processing that is carried out above the melting or softening temperature of the composition to cause crosslinking of the polymer composition. Furthermore, because the crosslinked polymer composition is dynamically crosslinked, the previously crosslinked polymer composition can be reprocessed at high temperatures in a subsequent process.

[0024] Thermoplastic Polymers In one or more embodiments, the thermoplastic polymer comprises at least one monomer selected from C2-C12 olefins, vinyl esters, and combinations thereof. The olefins can comprise one or more of ethylene, 1-propene, 1-butene, 1-pentene, 1-hexene, 1-heptene, 1-octene, 1-nonene, 1-decene, 1-undecene, 1-dodecene, and combinations thereof. Thus, for example, it is contemplated that the thermoplastic polymer can comprise polymers such as ethylene homopolymers, copolymers of ethylene and one or more C3-C12 alpha-olefins, propylene homopolymers, polyolefins including copolymers of propylene and one or more comonomers selected from ethylene, C4-C12 alpha-olefins, and combinations thereof, ethylene vinyl acetate, poly(vinyl acetate), and combinations thereof. In copolymers of olefins and vinyl esters, it is contemplated that the vinyl ester may be present as a comonomer in an amount ranging from a lower limit of 1, 5, 10, 15, 18, or 20 wt % to any upper limit of 25, 40, 60, or 80 wt % of the total weight of the copolymer. In one or more particular embodiments, vinyl acetate may be used as a monomer or comonomer. In one or more even more particular embodiments, the thermoplastic polymer may be a bio-based polymer, particularly ethylene vinyl acetate and polyethylene, for example, the ethylene may be derived from bio-based ethanol.

[0025] It is also contemplated that the thermoplastic polymer may include a branched vinyl ester comonomer (combined with ethylene alone to form a copolymer, or with ethylene and vinyl acetate to form a terpolymer). Such copolymers and terpolymers are described in U.S. Patent Application No. 17 / 063,488, the entirety of which is incorporated herein by reference. For example, such branched vinyl ester monomers may have the general structure (I):

[0026] [ka]

[0027] (In the formula, R 4 and R 5 have a combined carbon number of 6 or 7. However, it is also contemplated that other branched vinyl esters described in U.S. Patent Application Serial No. 17 / 063,488 can be used.

[0028] In one or more embodiments, the thermoplastic polymer forms at least 1 wt%, at least 5 wt%, 10 wt%, 15 wt%, at least 20 wt%, at least 25 wt%, at least 50 wt%, at least 70 wt%, or at least 80 wt%, or at least 90 wt%, or at least 99 wt% of the polymer composition. The amount of thermoplastic polymer can depend, for example, on the presence of other components, such as, but not limited to, crosslinkers, fillers, additives, oils, and / or plasticizers.

[0029] When referring to the thermoplastic polymer forming the polymer composition described herein, it is intended that the polymer is dynamically crosslinked through the addition of a dynamic crosslinking group and a crosslinking system. The dynamic crosslinking group, e.g., vinyl ester of EVA, can be incorporated into the thermoplastic polymer during polymerization, or the dynamic crosslinking group can be added to the base polymer after it is polymerized. The dynamic crosslinking group can be added to the base polymer through a grafting reaction, for example, during the reactive processing step that forms the thermoplastic polymer. The grafting reaction can include forming at least one covalent bond between the base polymer and a molecule that includes a dynamic crosslinking group. The grafting can include, for example, melt grafting, solution grafting, or solid state grafting.

[0030] Dynamic Crosslinking Group In one or more embodiments, the dynamic crosslinking groups can be derived from esters, carboxylic acids, such as acrylic acid, or derivatives thereof, such as carboxylates, and combinations thereof.

[0031] Also as mentioned above, the moiety or dynamic crosslinking group may be present in the thermoplastic polymer from polymerization (such as in the case of esters in thermoplastics containing vinyl ester monomers), or such moiety may be reacted with the base polymer via post-polymerization reactive processing to form the thermoplastic polymer. Such reactive processing may include, for example, melt grafting, solution grafting, or solid state grafting. It is also contemplated that the dynamic crosslinking group may be the same or different chemical species as the monomers that form the thermoplastic polymer. For example, if the thermoplastic polymer is polyvinyl acetate, vinyl acetate is both the monomer and the dynamic crosslinking group.

[0032] In one or more embodiments, the dynamic crosslinking group may include vinyl esters such as vinyl acetate, vinyl propionate, vinyl 2-ethylhexanoate, vinyl decanoate, vinyl neodecanoate, vinyl neononanoate, vinyl laurate, vinyl benzoate, vinyl pivalate, vinyl butyrate, vinyl trifluoroacetate, vinyl cinnamate, vinyl 4-tert-butylbenzoate, vinyl stearate, allyl cinnamate, vinyl methacrylate, and the like, and combinations thereof.

[0033] In one or more embodiments, the dynamic crosslinking group may include unsaturated organic acids such as itaconic acid, maleic acid, acrylic acid, crotonic acid, methacrylic acid, fumaric acid, 1-vinyl-1H-pyrrole-2-carboxylic acid, 1,2-benzenedicarboxylic acid, and the like, and combinations thereof.

[0034] In one or more embodiments, the dynamic crosslinking group can include a moiety capable of reacting with a dynamic crosslinking system. In one or more embodiments, the dynamic crosslinking group is present in the thermoplastic polymer in an amount up to 100 wt%, 90 wt%, 70 wt%, 50 wt%, 30 wt%, 10 wt%, 5 wt%, 4 wt%, 3 wt%, 2 wt%, 1 wt%, 0.05 wt%, or 0.01 wt% of the thermoplastic polymer.

[0035] Crosslinking Agent In one or more embodiments, the crosslinking agent may form an ionic bond or a metal ligand bond. The crosslinking agent may be selected from o-nucleophiles, n-nucleophiles, metal oxides, metal hydroxides, acid / alkali catalysts such as NaOH or KOH, organometallic salts selected from the group consisting of acetylacetonates, diacrylates, carbonates, acetates, and combinations thereof, where the metal is selected from the group consisting of zinc, molybdenum, copper, magnesium, sodium, potassium, calcium, nickel, tin, lithium, titanium, zirconium, aluminum, lead, iron, vanadium, and combinations thereof.

[0036] In one or more embodiments, the crosslinker forms any of the following lower limits: 0.01 wt%, 0.1 wt%, 0.5 wt%, at least 1 wt%, at least 2 wt%, or 3 wt% and any of the following upper limits: 4 wt%, 5 wt%, 6 wt%, 8 wt%, 10 wt%, 12 wt%, 15 wt%, 20 wt%, or 25 wt% of the polymer composition, any lower limit can be used in combination with any upper limit.

[0037] Optional Additives In addition to the crosslinked polymer, catalyst, and optional non-crosslinked polymer, the polymer composition of the present disclosure may also include one or more optional additives, such as, but not limited to, fillers, blowing agents, foaming promoters, elastomers, plasticizers, processing aids, release agents, lubricants, dyes, pigments, antioxidants, light stabilizers, flame retardants, antistatic agents, antiblock additives, or other additives to modify the balance of stiffness and elasticity in the polymer composition, such as fibers, fillers, flakes, nanoparticles, nanofibers, nanowhiskers, nanosheets, and other reinforcing elements. In some embodiments, one or more such additives may be added during the initial mixing or melt processing of the crosslinked polymer and catalyst, while in one or more embodiments, one or more such additives may be incorporated in a subsequent process step.

[0038] The polymeric composition according to the present disclosure may include one or more foaming accelerators (also known as kickers) that enhance or trigger the action of the foaming agent due to the associated low activation temperature. For example, a foaming agent accelerator may be used when the selected foaming agent reacts or decomposes at temperatures above 170° C., e.g., 220° C. or higher, and the surrounding polymer may decompose when heated to the activation temperature. The foaming accelerator may include any suitable foaming accelerator capable of activating the selected foaming agent. In one or more embodiments, suitable foaming accelerators may include cadmium salts, cadmium-zinc salts, lead salts, lead-zinc salts, barium salts, barium-zinc (Ba-Zn) salts, zinc oxide, titanium dioxide, triethanolamine, diphenylamine, sulfonated aromatic acids, and salts thereof, and the like. The polymeric composition according to certain embodiments of the present disclosure may include zinc oxide as one or more foaming accelerators.

[0039] The polymeric composition according to the present disclosure may include one or more blowing agents to produce an expanded polymeric composition and a foam. The blowing agent may include a solid, liquid, or gas blowing agent. In embodiments utilizing a solid blowing agent, the blowing agent may be combined with the polymeric composition as a powder or granules.

[0040] Blowing agents according to the present disclosure may include chemical blowing agents that decompose at polymer processing temperatures and release a blowing gas, e.g., N2, CO, CO2, etc. Examples of chemical blowing agents may include hydrazines such as toluenesulfonylhydrazine, hydrazides such as oxydibenzenesulfonylhydrazide, diphenyloxide-4,4'-disulfonic acid hydrazide, nitrates, azo compounds such as azodicarbonamide, cyanovaleric acid, azobis(isobutyronitrile), and organic blowing agents including N-nitroso compounds and other nitrogen-based materials, as well as other compounds known in the art.

[0041] Inorganic chemical blowing agents can include carbonates such as sodium hydrogen carbonate (sodium bicarbonate), sodium carbonate, potassium bicarbonate, potassium carbonate, ammonium carbonate, and the like, which may be used alone or in combination with weak organic acids such as citric acid, lactic acid, or acetic acid.

[0042] The polymeric compositions according to the present disclosure may include one or more plasticizers to adjust the physical properties and processability of the composition. In some embodiments, the plasticizer according to the present disclosure is selected from the group consisting of bis(2-ethylhexyl)phthalate (DEHP), di-isononyl phthalate (DINP), bis(n-butyl)phthalate (DNBP), butyl benzyl phthalate (BZP), di-isodecyl phthalate (DIDP), di-n-octyl phthalate (DOP or DNOP), di-o-octyl phthalate (DIOP), diethyl phthalate (DEP), di-isobutyl phthalate (DIBP), di-n-hexyl phthalate, tri-methyl trimellitate (TMTM), tris(2-ethylhexyl) trimellitate (TEHTM-MG), tri-(n-octyl, n-decyl) trimellitate, tri-(heptyl, nonyl) trimellitate, n-octyl trimellitate, bis(2-ethylhexyl) adipate, and the like. ethylhexyl) (DEHA), dimethyl adipate (DMD), mono-methyl adipate (MMAD), dioctyl adipate (DOA), dibutyl sebacate (DBS), polyesters of adipic acid such as VIERNOL, dibutyl maleate (DBM), di-isobutyl maleate (DIBM), benzoates, epoxidized soybean oil and derivatives, n-ethyltoluenesulfonamide, n-(2-hydroxypropyl)benzenesulfonamide, n-(n-butyl)benzenesulfonamide, tricresyl phosphate (TCP), tributyl phosphate (TBP), glycols / polyesters, triethylene glycol dihexanoate, 3gh), tetraethylene glycol di-heptanoate, polybutenes, acetylated monoglycerides;The additives may include one or more of alkyl citrates, triethyl citrate (TEC), acetyl triethyl citrate, tributyl citrate, acetyl tributyl citrate, trioctyl citrate, acetyl trioctyl citrate, trihexyl citrate, acetyl trihexyl citrate, butyryl trihexyl citrate, o-butyryl trihexyl citrate, trimethyl citrate, alkyl sulfonic acid phenyl esters, 2-cyclohexanedicarboxylic acid di-isononyl ester, nitroglycerin, butanetriol trinitrate, dinitrotoluene, trimethylolethane trinitrate, diethylene glycol dinitrate, triethylene glycol dinitrate, bis(2,2-dinitropropyl) formal, bis(2,2-dinitropropyl) acetal, 2,2,2-trinitroethyl 2-nitroxyethyl ether, mineral oil, vegetable oil or bio-based oil, among other plasticizers, and polymeric plasticizers. In certain embodiments, one of the one or more plasticizers can be a mineral oil;

[0043] The polymeric composition according to the present disclosure may include one or more inorganic fillers and nanofillers, such as talc, glass fiber, marble dust, cement dust, clay, carbon black, feldspar, silica or glass, fumed silica, silicates, calcium silicate, silicate powder, glass microspheres, mica, metal oxide particles and nanoparticles, such as magnesium oxide, antimony oxide, zinc oxide, inorganic salt particles and nanoparticles, such as barium sulfate, wollastonite, alumina, aluminum silicate, titanium-based oxides, calcium carbonate, graphene, carbon nanotubes and other carbon-based nanostructures, boron nitride nanotubes, cellulosic nanostructures, and other nanoparticles, nanofibers, nanowhiskers, nanosheets, polyhedral oligomeric silsesquioxanes (POSS), recycled EVA, and other recycled rubber. As defined herein, recycled EVA may be derived from regrind material that has been subjected to at least one processing method, such as molding or extrusion, followed by grinding or chopping of sprues, runners, flash, rejected parts, and the like. In accordance with embodiments of the present disclosure, such recycled materials are combined with a catalyst to form the polymer compositions described herein having a dynamically crosslinked network, although it is also envisioned that additional recycled EVA or other polymers can be added as fillers in a subsequent compounding step.

[0044] Crosslinked Polymer Composition In one or more embodiments, upon crosslinking, the composition exhibits a plateau elastic storage modulus within the temperature range of 20°C to 150°C.

[0045] In one or more embodiments, upon crosslinking, the composition has an elastic storage modulus that is time-dependent at temperatures above 120° C., such that it drops by at least 50% relative to its initial value (G0, plateau modulus) within 10,000 seconds at temperatures below 230° C. The normalized relaxation modulus value can be obtained via an exponential decay fit to the elastic storage modulus data. The plateau modulus corresponds to the fit at t=0 seconds, also referred to as G0.

[0046] processing In one or more embodiments, a crosslinkable polymer composition, which may include a thermoplastic polymer and a crosslinking system including a crosslinking agent and a catalyst, is subjected to a melt-processing operation to form a crosslinkable polymer composition (i.e., not yet dynamically crosslinked). This polymer composition can then be dynamically crosslinked as part of a multi-step process. In a first step, the polymer composition is prepared by melt mixing a thermoplastic polymer and a crosslinking agent at a temperature that is not sufficient to form dynamic crosslinks in the polymer composition. In a second step, the polymer composition formed in the first step is crosslinked, optionally in the presence of molecular oxygen, in a process using, for example, a hot air tunnel, an oven, an autoclave, or other suitable crosslinking equipment. The step of crosslinking the polymer composition is carried out at a temperature high enough to form a dynamically crosslinked polymer composition. The step of crosslinking can be carried out in the same equipment used to form the polymer composition, or it can be carried out in a separate equipment. Dynamic crosslinking is advantageously carried out without the use of peroxides. Thus, the chemistry for crosslinking is relatively insensitive to molecular oxygen. The crosslinking reaction to form the dynamic crosslinks can be carried out in an oxygen-containing environment.

[0047] In one or more embodiments, the crosslinkable polymer composition, which may include a thermoplastic polymer and a crosslinking agent, can be subjected to a melt-processing operation to form a dynamically crosslinked polymer composition in a one-step or multi-step process. Specifically, the thermoplastic polymer and the crosslinking agent can be mixed at an elevated temperature, i.e., above the softening or melting temperature of the composition. For example, the mixture of the thermoplastic polymer and the crosslinking agent can be subjected to a processing temperature higher than the processing temperature of the uncrosslinked thermoplastic polymer to form the polymer composition. That is, the mixture can be subjected to a temperature higher than either the melting or softening point of the uncrosslinked polymer. The temperature should be selected according to the requirements of the selected processing operation, as long as it does not exceed the decomposition temperature of the polymer. The softening point of the amorphous uncrosslinked polymer is determined by the Vicat method according to ASTM D-1525, and the melting point of the semi-crystalline uncrosslinked polymer is measured according to DSC.

[0048] In one or more embodiments, the polymer compositions according to the present disclosure can be prepared using continuous or discontinuous extrusion, or in continuous or batch mixing. The process can use a single screw extruder, twin screw extruder, or multiple screw extruder, internal mixer, hot air tunnel, oven, hydraulic press, injection molding machine, further manufacturing machine, or autoclave, any of which can be used at temperatures ranging from 60 to 270°C in some embodiments, and from 140 to 230°C in some embodiments. In some embodiments, the raw materials (thermoplastic polymer, and crosslinking system) are added simultaneously or sequentially to the extruder or other processing method.

[0049] A method of preparing a polymer composition according to the present disclosure may include the general steps of combining a thermoplastic polymer and a crosslinking agent in an extruder or mixer; melt extruding the composition; and forming pellets, filament powder, bulk compound, or sheets of the polymer composition.

[0050] The polymer composition prepared by this method may be in the form of granules that can be applied to different molding processes, including processes selected from extrusion, calendaring, injection molding, foaming, compression molding, steam chest molding, supercritical molding, additive manufacturing, etc., to produce articles.

[0051] Considering dynamic crosslinking, embodiments of the present disclosure also relate to reprocessing of the crosslinked polymer composition. In one or more embodiments, due to the inherent properties of the chemistry used, the crosslinked polymer formulation can be reprocessed or regenerated using similar processing applied to the virgin polymer in the original crosslinking process. Pieces or used parts can be reground or otherwise processed as required to provide material in the desired operation with acceptable reduction in processability or properties in a manner that is still useful as a secondary raw material. The intention is that the reprocessing parameters are generally similar to those used in the original manufacturing process. Advantageously, the polymer composition can be reprocessed and the properties of the polymer composition can be substantially maintained compared to those immediately before the reprocessing step. Specifically, in one or more embodiments, after the reprocessing step, the polymer composition maintains at least 40% of its initial storage modulus plateau above its melting temperature as measured by dynamic mechanical analysis compared to the polymer composition before the reprocessing step.

[0052] It is also contemplated that the reworking step may be performed repeatedly (through multiple cycles). In one or more embodiments, after the reworking step is repeated (e.g., after three or even five cycles of reworking), the polymer composition maintains at least 40% of its initial storage modulus plateau above its melt temperature as measured by dynamic mechanical analysis compared to the polymer composition prior to the reworking step.

[0053] Goods In one or more embodiments, an article can be formed from the dynamically crosslinked polymer composition. The article formed can be foamed or unfoamed.

[0054] In one or more embodiments, the article is selected from the group consisting of shoe soles, insoles, midsoles, unisoles, or other shoe accessories; gaskets, hoses, cables, wires, sealing systems, conveyor belts, foxing tapes, NVH materials, sound insulation, roofing materials, and industrial flooring. In embodiments of multi-layer articles, it is contemplated that at least one of the layers comprises the polymer composition of the present disclosure.

[0055] Oxygen insensitivity during crosslinking To evaluate the tack of the crosslinked polymer compositions after curing (crosslinking) in an oven (not vacuum or inert atmosphere), the following procedure was used.

[0056] A sheet of the polymer composition is prepared via calendaring and / or compression molding, then cut with a razor blade, scissors, or other cutting device to dimensions of 0.7-3 mm thick, 2.5 cm wide, and 4 cm long (although dimensions are not critical parameters since it is mostly a surface phenomenon). It is then placed on a surface such as a metal tray or hung over the top of an oven using a metal wire and placed in a preheated oven for 15 minutes with a hot air oven setting of 205°C for curing.

[0057] After 15 minutes of curing, the sheet is removed and immediately placed on an insulating surface (e.g., cured rubber) and then immediately covered with Kleenex® Facial Tissue, firm hand pressure is applied to the entire rubber surface, and a flat 1.8 kg weight is placed on the specimen for 5 minutes. After cooling to room temperature, the tissue paper is carefully removed.

[0058] Upon visual evaluation, the polymer surface should be free of tissue paper fibers. If the majority of the tissue paper or its fibers adhere to the polymer, this indicates insufficient surface crosslinking or excessive surface tackiness of the formulation.

[0059] The metric for this test is defined as the tack number, which ranges from 10 to 0, calculated as the percentage of the polymer surface not covered by paper fibers divided by 10. A non-tacky surface (no paper fibers) is rated 10, while a poor material surface completely covered by tissue paper fibers is rated 0.

[0060] According to embodiments of the present disclosure, the crosslinked polymer composition that is relatively insensitive to the presence of molecular oxygen has a tack number greater than 5. In more specific embodiments, the crosslinked polymer composition may have a tack number of at least 6, 7, 8, or 9. EXAMPLES

[0061] Example 1 Melting / mixing EVA with dynamic crosslinking agents Elastomeric networks were made by extrusion of ethylene-vinyl acetate copolymer (EVA) and zinc carboxylate salts at temperatures above the melting temperature of EVA. Conventional EVA (Braskem commercial grade HM728, VAc content 28 wt%, melt index (190°C / 2.16 kg=6 g / 10 min) was melted / mixed with the zinc-centered dicarboxylate salts in a Werner-Pfleiderer 18 mm twin-screw extruder. In a series of comparative examples, EVA was extruded with dicumyl peroxide (DCP) using the same extrusion conditions. Dicumyl peroxide is a conventional crosslinking agent that is widely used to crosslink EVA in commercial practice.

[0062] The extrusion conditions are detailed in Table 1. For each formulation, the EVA pellets were coated with a small amount (0.4 wt%) of mineral oil to facilitate mixing and then dry-blended with DCP or zinc diacrylate. The EVA and DCP or EVA and zinc diacrylate mixtures were introduced into the extruder hopper and the extrusion conditions were selected to avoid crosslinking with the dicumyl peroxide. The formulations were extruded through a die, cooled in a water bath, and pelletized.

[0063] Two additional samples (Example 7 and Example 8) were prepared by melting / mixing EVA HM728 and zinc acetylacetonate (Zn(acac)2) in an Xplore MC15 microcompounder with all temperature zones set at 120°C. The EVA pellets were fed into the mixing chamber using a feed hopper and mixed for approximately 1 minute using a screw speed of 150 rpm until the force remained constant indicating they were completely melted. The zinc acetylacetonate was then fed into the mixing chamber. Mixing with recirculation was continued for another minute. The mixture was then extruded through a die and cooled in air.

[0064] [Table 1]

[0065] Differential scanning calorimetry To explain the formation of dynamic crosslinked networks, the thermal response of the extruded EVA blends was measured by differential scanning calorimetry (DSC, Q200 instrument manufactured by TA Instruments).

[0066] In the first heating step, the sample was heated to 160°C with a heating rate of 10°C / min. The temperature was kept constant at 160°C. Then, the sample was cooled to -20°C with a rate of 10°C / min and equilibrated at -20°C for 1 min. In the second heating step, the sample was heated to 160°C with a heating rate of 10°C / min, kept at 160°C for 1 min, and then cooled to 30°C with a rate of 10°C / min. The cooling curve obtained after the first heating step is reported in Figure 1. The heating curve obtained after the second heating step is reported in Figure 2.

[0067] For each formulation, the crystallization peak temperature observed after the first heating step, Tc, and the melting temperature observed after the second heating step, Tm, are reported in Table 2.

[0068] The comparative examples in Table 2 show that conventional crosslinking of EVA with dicumyl peroxide (DCP) results in a decrease in both the melting and crystallization temperatures. The magnitude of these shifts to lower Tm and Tc values ​​increases as the amount of DCP increases. In the compositions of the present invention, the crystallization temperature, Tc, values ​​are decreased compared to uncrosslinked EVA. These shifts to lower Tc suggest that a dynamic crosslinked network was formed as a result of extruding EVA with a zinc salt.

[0069] [Table 2]

[0070] Shear Rheology Small angle oscillatory shear (SAOS) measurements were performed using an Anton Parr torque rheometer operating from room temperature to 150°C. Samples were prepared by molding extruded EVA pellets in a Carver press to give disks of 25 mm diameter. The viscoelastic response was measured by first equilibrating the samples at 25°C and then increasing the temperature to 150°C at a heating rate of 2°C / min. A normal force of 10 N was applied.

[0071] The results are reported in Figure 3. The elastic storage modulus (G') of the control sample shows a first plateau over the 25°C to 60°C temperature range, then drops sharply at 75°C and continues to drop as temperature increases. The sample crosslinked with dicumyl peroxide (DCP) shows a G' plateau in the 25°C to 60°C range that is significantly lower than that of the control. This is consistent with the formation of an elastic network that prevents the polyethylene component of the EVA from crystallizing. This inhibition of crystallization is also observed by DSC. At temperatures above 75°C, the DCP cured sample shows a broad G' plateau, indicating the formation of a rubbery network. Over a temperature range of approximately 75°C to 150°C, the DCP cured sample has a tan delta value of less than 1, another indication that a crosslinked elastomeric network has formed.

[0072] Like the DCP cured samples, the inventive compositions containing Zn-diacrylate also exhibit lower plateau modulus values ​​than the control over the temperature range of 25° C. to 60° C., suggesting that crystallization is suppressed. These samples also exhibit tan delta values ​​of less than 1 at temperatures above 75° C. Both the lower plateau modulus and the tan delta of less than 1 indicate the formation of a crosslinked network in the inventive compositions.

[0073] Example 2 Rework (multiple melting and cooling cycles) To demonstrate that the compositions of the present invention can be reprocessed by heating and melting, the extruded pellets were pressed multiple times in a Carver press using the conditions listed in Table 3. The pellet samples were pressed between steel plates using a 0.6 mm thick brass die to control the thickness of the samples. After the first pressing pass, the film was cooled, cut into strips, and pressed again to form a second film. The second film was cut into strips and pressed to form a third film. After each pressing, a sample of the film was collected for dynamic mechanical analysis.

[0074] Two formulations were tested for rework performance: Comparative Example 4, which contained 2 wt% DCP, and Inventive Example 6, which contained 3 wt% zinc diacrylate. The comparative sample, which contained dicumyl peroxide, was pressed only once (first press) because it did not flow upon heating during the subsequent pressing steps. The inventive sample provided a smooth, uniform film after each press, demonstrating that the composition flowed and assumed the shape of the mold.

[0075] [Table 3]

[0076] The viscoelastic response of the pressed films was measured by dynamic mechanical analysis (DMA) temperature sweep using a rheometer manufactured by TA Instruments equipped with a tensile fixture. The sample dimensions were 0.6 mm thick, 7 mm wide, and 22-26 mm long. The strain amplitude was 15 microns, the frequency was 1 Hz, and the heating rate was 3°C per minute.

[0077] The values ​​of elastic modulus and storage modulus as a function of temperature are reported in Figures 4 and 5. Like the peroxide cured formulations, the compositions of the present invention exhibit a plateau storage modulus over a temperature range of about 20° C. to about 80° C. After three processing steps, the plateau modulus of the compositions of the present invention retains at least half of its initial value, which is taken as the value of E' after the first press.

[0078] Although only a few exemplary embodiments have been described in detail above, those skilled in the art will readily appreciate that many modifications are possible in the exemplary embodiments without substantially departing from the present invention. Accordingly, all such modifications are intended to fall within the scope of the present disclosure as defined in the following claims. In the claims, means-plus-function clauses are intended to cover the structures described herein as performing the recited function, and structural equivalents as well as equivalent structures. Thus, while nails and screws may not be structural equivalents in that nails use cylindrical surfaces to fasten wooden parts together, whereas screws use helical surfaces, in the context of fastening wooden parts, nails and screws may be equivalent structures. It is the express intent of the applicants not to apply 35 U.S.C. 112(f) to any limitations in any of the claims herein, except where the claims expressly use the words "means for" with the relevant function.

Claims

1. Vinyl ester, C 2 ~C 12 at least one monomer selected from the group consisting of olefins, and combinations thereof; and A thermoplastic polymer comprising dynamic crosslinking groups; and A polymeric composition comprising a crosslinking agent that dynamically crosslinks a thermoplastic polymer through ionic bonds or metal-ligand interactions.

2. 10. The polymer composition of claim 1, wherein the dynamic crosslinking group is selected from the group consisting of esters, carboxylic acids, derivatives of carboxylic acids, and combinations thereof.

3. 3. The polymer composition of claim 1 or 2, wherein at least one monomer comprises a dynamic crosslinking group.

4. Vinyl ester, C 2 ~C 12 a thermoplastic polymer comprising at least one monomer selected from the group consisting of olefins, and combinations thereof; and 1. A polymer composition comprising a crosslinking agent that crosslinks a thermoplastic polymer by ionic bonds or metal-ligand interactions, A polymeric composition in which crosslinking is relatively insensitive to the presence of molecular oxygen.

5. 5. The polymer composition of claim 4, wherein the thermoplastic polymer comprises at least one moiety selected from the group consisting of esters, carboxylic acids, derivatives of carboxylic acids, and combinations thereof.

6. 6. The polymer composition of any one of claims 4 to 5, wherein the crosslinking agent is an o-nucleophile; an n-nucleophile; a metal oxide, a metal hydroxide such as NaOH or KOH; an organometallic salt selected from the group consisting of acetylacetonates, diacrylates, carbonates, acetates, and combinations thereof, wherein the metal is selected from the group consisting of zinc, molybdenum, copper, magnesium, sodium, potassium, calcium, nickel, tin, lithium, titanium, zirconium, aluminum, lead, iron, vanadium, and combinations thereof.

7. 7. The polymer composition according to claim 1, wherein the thermoplastic polymer is dynamically crosslinked by a crosslinking system.

8. 8. The polymer composition of claim 7, wherein the dynamic crosslinks are formed via ionic or metal ligand bonds.

9. 9. The polymer composition of claim 7 or 8, which exhibits a plateau elastic storage modulus within the temperature range of 20 to 150°C.

10. The elastic storage modulus returns to its initial value (G 0 10. The polymer composition according to claim 7, wherein the modulus is time-dependent at temperatures above 120°C such that the modulus (p / m) decreases by at least 50% relative to the plateau modulus (p / m).

11. A method for producing a polymer composition, comprising processing a crosslinking system with a thermoplastic polymer to form the polymer composition according to any one of claims 1 to 6, The method, wherein the processing step is at a first temperature less than a second temperature sufficient to form crosslinks in the polymer composition.

12. The method of claim 11 , wherein the processing step comprises melt mixing.

13. 13. The method of claim 11 or 12, further comprising the step of reacting the base polymer with at least one moiety selected from the group consisting of esters, carboxylic acids, derivatives of carboxylic acids, and combinations thereof via post-polymerization reactive processing to form a thermoplastic polymer prior to the processing step.

14. The method of claim 13, wherein the reactive processing comprises melt grafting, solution grafting, or solid state grafting.

15. 15. The method of any one of claims 12 to 14, further comprising crosslinking the polymer composition by processing the polymer composition at a second temperature above the melting or softening temperature.

16. The method of claim 15, wherein the crosslinking occurs in the presence of molecular oxygen.

17. 17. The method of claim 15 or 16, wherein the thermoplastic polymer is first formed by reactive processing, then melt mixed with a crosslinking system, and subsequently crosslinked.

18. A method for producing a polymer composition comprising the steps of processing a polymer composition according to any one of claims 1 to 6 above its melting or softening temperature in an internal mixer or extruder; and A method comprising the step of crosslinking a polymer composition in the presence of oxygen.

19. 19. The method of any one of claims 15 to 18, wherein the crosslinking step is in an internal mixer, an extruder, a hot air tunnel, an oven, a hydraulic press, an injection moulding machine, a further manufacturing machine, or an autoclave.

20. 20. The method of any one of claims 15 to 19, further comprising the step of reprocessing the crosslinked polymer composition.

21. 11. A method for reprocessing a polymer composition comprising the step of reprocessing a polymer composition according to any one of claims 7 to 10 above the melting or softening temperature of the thermoplastic polymer, wherein after the reprocessing step, the polymer composition maintains at least 40% of its initial storage modulus plateau above its melting temperature as compared to the polymer composition prior to the reprocessing step, as measured by dynamic mechanical analysis.

22. 22. The method of claim 21, further comprising repeating the processing step at least four additional times, wherein after repeating the reprocessing step, the polymer composition maintains at least 40% of its initial storage modulus plateau above its melt temperature as compared to the polymer composition prior to the reprocessing step, as measured by dynamic mechanical analysis.

23. A part comprising the polymer composition according to any one of claims 7 to 10.

24. 24. The article of claim 23, which is non-foamed.

25. 24. The article of claim 23 which is foamed.

Citation Information

Patent Citations

  • Polyethylene copolymers and products and methods thereof

    US11326002B2