Zeolite coated on battery electrodes

A zeolitic material coated on electrodes addresses thermal and mechanical stability issues in lithium-ion secondary batteries, ensuring efficient ion transport and safety by preventing dendrite penetration, thus maintaining battery performance.

JP2024538683AInactive Publication Date: 2024-10-23PACIFIC IND DEVELOPMENT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024520639
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-04
Filing Date
2022-09-28
Publication Date
2024-10-23
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional lithium-ion secondary battery separators made of polymeric materials face issues with thermal stability, ion transport impedance, and safety concerns such as dendrite formation and ignition during thermal runaway, while inorganic separators lack mechanical stability and are complex to manufacture.

Method used

Using a zeolitic material as a separator directly coated on the electrodes, which provides thermal stability, large pore surface area for electrolyte purification, and electrical insulation, while allowing reversible ion flow, with a moisture content below 7% and controlled porosity to prevent dendrite penetration.

Benefits of technology

The zeolitic material enhances thermal stability, improves ion transport, and prevents dendrite formation, maintaining battery performance and safety, comparable to conventional separators despite higher initial moisture content.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024538683000001_ABST
    Figure 2024538683000001_ABST
Patent Text Reader

Abstract

A cell for use in an electrochemical cell, comprising a positive electrode, a negative electrode, an electrolyte, and a separator in the form of a zeolitic material comprising one or more natural or synthetic zeolites directly attached to at least one of the positive and negative electrodes. The positive electrode is configured to reversibly extract non-reactive metal ions from the positive electrode and insert them into the positive electrode. The negative electrode is configured to reversibly accept and release non-reactive metal ions. The electrolyte is located between the negative electrode and the positive electrode and in contact with the negative electrode and the positive electrode. The electrolyte thereby supports a reversible flow of non-reactive metal ions between the positive electrode and the negative electrode. The separator is configured to electrically insulate the positive electrode from the negative electrode while being permeable to the reversible flow of non-reactive metal ions through the separator.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of the filing date under 35 U.S.C. § 119(e) of U.S. Provisional Patent Application No. 63 / 251,745, filed October 4, 2021, the entire contents of which are incorporated herein by reference.

[0002] The present invention relates generally to components used in the manufacture of electrochemical cells. More specifically, the present disclosure describes a separator in the form of a zeolitic material that is used in one or more of the electrodes present in the battery. [Background technology]

[0003] The statements in this section are merely intended to provide background information related to the present disclosure and may not constitute prior art.

[0004] The main difference between lithium ion batteries and lithium ion secondary batteries is that lithium ion batteries refer to batteries that contain primary cells, while lithium ion secondary batteries refer to batteries that contain secondary cells. The term "primary battery" refers to a battery cell that cannot be easily or safely recharged, while the term "secondary battery" refers to a battery cell that can be recharged. As used herein, "battery cell" or "cell" refers to the basic electrochemical device of a battery, including electrodes, separators, and electrolyte. In contrast, a "battery" refers to a collection of cells, e.g., one or more cells, including a housing, electrical connections, and possibly control and protection electronics.

[0005] Lithium-ion (i.e. primary) batteries are not rechargeable and therefore currently have a shelf life of about three years, after which they become useless. Even with this limited lifespan, lithium batteries can offer more in terms of capacity than lithium-ion secondary batteries. Lithium batteries use lithium metal as the battery anode, which differs from lithium-ion batteries, which can use many other materials for the anode.

[0006] One important advantage of lithium-ion secondary batteries is that they can be charged many times before they become useless. The reason why lithium-ion secondary batteries can be used for multiple charge-discharge cycles is due to the reversibility of the oxidation-reduction reaction that takes place. Because of their high energy density, lithium-ion secondary batteries are widely used as energy sources for many portable electronic devices (e.g., mobile phones, notebook PCs, etc.), power tools, electric vehicles, and energy storage for grids.

[0007] As shown in FIG. 1, a conventional electrochemical cell 1, such as a secondary lithium-ion battery, generally comprises a positive electrode 10, which includes an active material (cathode) 5 and a current collector 7, a non-aqueous electrolyte 30, which includes lithium ions 35, a separator 25, and a negative electrode 20, which includes an active material (anode) 15 and a current collector 17. All of these components are sealed in a case, enclosure, pouch, bag, cylindrical shell, or the like (commonly referred to as the battery's "enclosure"). The separator 25 electrically insulates the cathode 5 from the anode 15 while allowing ions 35 to flow between them. The flow of ions may be conducted by the separator (i.e., via a solid-state reaction mechanism) or may be conducted by the presence of a liquid electrolyte 30 that permeates the multiple pores of the separator 25 (e.g., a membrane).

[0008] In lithium-ion or lithium metal batteries, separators are generally constructed of polymer-based materials, such as polyethylene (PE), polypropylene (PP), polytetrafluoroethylene (PTFE), and nonwoven fabrics made of polymeric fibers, due to their high mechanical strength and electrochemical stability. However, these polymeric materials also have various problems. For example, polymer-based separators are not easily wetted by non-aqueous electrolytes, which increases the impedance of ion transport and reduces high-rate performance. In addition, these polymer-based separators generally lack thermal stability. More specifically, these polymeric materials tend to shrink and even melt at relatively high temperatures (e.g., below 165°C). Due to the organic nature of the polymeric materials, these separators may also ignite and burn during a thermal runaway event. Furthermore, the softness of the polyolefin membrane allows dendrites, such as lithium dendrites, to grow and penetrate, raising safety concerns.

[0009] By replacing the polymeric material with a purely inorganic material (e.g., ceramic oxide or glass), the softening and melting problems that can occur when exposed to high temperatures are avoided, thereby improving the thermal stability of the separator. However, separators formed from such purely inorganic materials tend to have poor mechanical stability (e.g., brittleness). Furthermore, the manufacturing process for these separators is more complicated and expensive due to the difficulties associated with making flexible, free-standing thin films of inorganic materials.

[0010] Pure inorganic materials can be applied directly to the surface of the polymer-based separator, simplifying the manufacturing process. These pure inorganic materials include α-Al 2 O 3 or ZrO 2 or TiO 2 or SiO 2These include solid ceramic oxide particles that provide limited electrical insulation to the electrodes while allowing ions to diffuse through the interparticle spaces that exist, however, these solid ceramic oxide particles have limited surface area and functionality to act as functional particles that can improve cell performance.

[0011] Zeolite particles and lithium ion-exchanged zeolite particles can be used to remove moisture, dissolved transition metal ions, and impurities from the electrolyte to improve cell performance. However, applying these high surface area particles to the surface of an electrode is problematic because many of these zeolite materials tend to retain large amounts of moisture even after drying. High water content in the zeolite particles can be released into the cell electrolyte, where the moisture irreversibly transforms into H2O during the first charge step. 2 This reduction irreversibly consumes electrons, resulting in a decrease in the first coulombic efficiency and therefore a decrease in the energy density of the cell. Summary of the Invention

[0012] The present disclosure generally relates to a cell for use in an electrochemical cell that addresses and overcomes problems and inefficiencies of the prior art. In general, the electrochemical cell includes a positive electrode, a negative electrode, an electrolyte located between the negative electrode and the positive electrode and in contact with the negative electrode and the positive electrode, and a separator in the form of a zeolitic material including one or more natural or synthetic zeolites that is directly attached to at least one of the positive and negative electrodes. The positive electrode is configured such that non-reactive metal ions are reversibly extracted from the positive electrode and inserted into the positive electrode. The negative electrode is configured to reversibly accept and release non-reactive metal ions. The electrolyte thereby supports a reversible flow of non-reactive metal ions between the positive and negative electrodes. The separator is configured to electrically insulate the positive electrode from the negative electrode while being permeable to the reversible flow of non-reactive metal ions through the separator.

[0013] According to one embodiment of the present disclosure, the zeolite-based material attached to at least one of the positive electrode and the negative electrode has a thickness in the range of 1 micrometer (μm) to 200 μm. In a preferred case, the zeolite-based material further comprises a binder, and the ratio of the zeolite to the binder is in the range of 99.5% / 0.5% to 10% / 90% by mass ratio. The binder may comprise an organic complex, an inorganic oxide, or an inorganic hydroxide. The organic complex may be PVDF, cmc, SBR, PTFE, PAA (polyacrylic acid), PVA, PEI, or PAI, and the inorganic oxide or inorganic hydroxide may include aluminum, magnesium, zirconium, or cerium as its element. The zeolite may have an aluminum-silicon ratio (SAR) in the range of 0.5 to 500.

[0014] The positive electrode has an active material as a cathode and a current collector in contact with the cathode. The active material is LMNO, LiMn 2 O 4 , LiFePO 4 , LiNi a Co b Mn c Al d O 2 (a+b+c+d=1), and LiFe 0.2 Mn 0.8 PO 4 The negative electrode includes one or more of the following: an active material as an anode and a current collector in contact with the anode. The active material is graphite, hard carbon, soft carbon, silicon, Li 4 Ti 5 O 12 , Nb 2 O 5 , and derivatives thereof. The negative electrode is an "anode-free" electrode and has only a current collector. The zeolitic material has a water content of 35% or less, alternatively a water content of 7% or less. The zeolitic material has a porosity of 55% or less, alternatively a porosity of 30%-36%. The non-reactive metal ions in the electrolyte are lithium, sodium, potassium, magnesium, calcium, aluminum, or mixtures thereof.

[0015] In another aspect of the present disclosure, the zeolite-based material further comprises one or more secondary materials, the ratio of zeolite to secondary materials being in the range of 99.9% / 0.1% to 50.1% / 49.9% by weight, and optionally the one or more secondary materials include a flame retardant material.

[0016] The zeolite may have an average particle size in the range of 50 nanometers (nm) to 30 micrometers (μm), or an average pore size in the range of 0.1 nm to 20 nm, or both. If desired, the zeolite may comprise one or more ion-exchanged zeolites. The ion-exchanged zeolite may be a lithium-exchanged zeolite. In other words, the lithium-exchanged zeolite may have a lithium mass content in the range of 0.1 wt. % to 20 wt. %, based on the total weight of the lithium-exchanged zeolite.

[0017] In another aspect of the present disclosure, there is provided a lithium ion secondary battery comprising one or more of the cells as previously described and further defined herein, and one or more housings, wherein an interior wall from one of the one or more housings encapsulates at least one or more of the cells.

[0018] Further areas of applicability will become apparent from the description provided herein. It is to be understood that the description and specific examples are intended for purposes of illustration only and are not intended to limit the scope of the present disclosure.

[0019] In order that the disclosure may be fully understood, various aspects of the present disclosure, illustrated by way of example, are described below with reference to the accompanying drawings, in which the components are not necessarily drawn to scale, emphasis instead being placed upon illustrating the principles of the present invention. [Brief description of the drawings]

[0020] [Figure 1] FIG. 1 is a schematic diagram of a conventional electrochemical cell. [Diagram 2]FIG. 2 is a graph plotted using thermogravimetric analysis (TGA) to compare the percent moisture content of zeolites before and after drying as a function of temperature. [Figure 3A] FIG. 3A is a schematic diagram of an electrochemical cell formed in accordance with the teachings of the present disclosure in which a zeolite-based material deposited directly on the negative electrode serves as a separator. [Figure 3B] FIG. 3B is a schematic diagram of the electrochemical cell of FIG. 3A, shown as a lithium ion secondary battery formed in accordance with the teachings of the present disclosure. [Figure 3C] FIG. 3C is a schematic diagram of another lithium ion secondary battery formed in accordance with the teachings of the present disclosure in which a zeolite-based material deposited directly on the positive electrode serves as a separator. [Figure 3D] FIG. 3D is a schematic diagram of another lithium ion secondary battery formed in accordance with the teachings of the present disclosure in which zeolite-based materials deposited directly on both the negative and positive electrodes function as separators. [Figure 4] FIG. 4 is a schematic diagram of a lithium ion secondary battery formed in accordance with the teachings of the present disclosure in which four secondary batteries of FIG. 3B are stacked in parallel to form a larger multi-cell battery. [Diagram 5] FIG. 5 is a schematic diagram of another lithium ion secondary battery in which four secondary batteries, including the secondary batteries of FIGS. 3A, 3B, 3C, and 3D, are stacked in series to form a larger mixed cell battery. [Figure 6] FIG. 6 is a comparative graph of the charge-discharge curves of LiMn2O4 / Li4Ti5O12 full cells with either PE separator or zeolite coated electrodes. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] The drawings described herein are for illustrative purposes only and are not intended to limit the scope of the present disclosure in any way. It should be understood that corresponding reference characters indicate like or corresponding parts and features throughout the description and drawings.

[0022] The following description is merely exemplary in nature and is not intended to limit the present disclosure or its application or uses in any manner. For example, the zeolitic materials prepared and used according to the teachings described herein are described throughout the present disclosure as separators applied to or in direct contact with one or more electrodes in secondary lithium ion batteries in order to more fully illustrate each structural element and their uses. The incorporation and use of such zeolitic materials in direct contact with or on the surface of an electrode is available for other applications, including, but not limited to, as at least an electrode and separator combination in other electrochemical cells, all-solid-state batteries, and primary batteries, and is considered to be within the scope of the present disclosure.

[0023] For purposes of this disclosure, the terms "about" and "substantially" are used herein in reference to measurable values ​​and ranges, which account for expected variations (e.g., limitations and variability of measurement) known to those of ordinary skill in the art.

[0024] For purposes of this disclosure, when referring to "at least one" and "one or more" of an element, these terms may be used interchangeably and may have the same meaning. These terms referring to the inclusion of a singular element or multiple elements may also be indicated by the suffix "(plural)" at the end of the element. For example, "at least one metal," "one or more metals," and "metals (plural)" may be used interchangeably and are intended to have the same meaning.

[0025] The present disclosure generally provides a zeolite-based material that is directly deposited or coated onto the surface of one or more electrodes that function as a separator layer in an electrochemical cell, such as a lithium-ion secondary battery. The use of the zeolite-based material provides the advantage of improving or enhancing the thermal stability of the separator. The zeolite-based material also provides a large pore surface area and volume for in-situ purification of electrolyte and for incorporating other functions, including but not limited to providing a support for encapsulating or depositing catalysts and flame retardants.

[0026] Conventional ceramic oxides (e.g., α-Al 2 O 3 , ZrO 2 , TiO 2 , or SiO 2 ), the zeolite-based materials of the present disclosure can perform a variety of additional functions based on the pore size, Si / Al ratio, and chemical composition of the zeolite. Zeolite-based materials can be used as supports for other active materials because of the adjustable pore structure and zeolite pore functions, including reversible ion exchange sites. For example, lithium-exchanged zeolites also provide the function of capturing dissolved transition metal ions present in the battery, thereby extending the battery's life. Zeolites have a very large surface area compared to conventional ceramic oxides, and therefore can absorb a very large amount of water and impurities from the organic electrolyte, which is necessary to extend the cycle life of the battery.

[0027] The zeolite in the zeolite-based material of the present disclosure is TO 4Zeolites are crystalline or paracrystalline aluminosilicates consisting of repeating tetrahedral units, where T is silicon (Si) or aluminum (Al) in the most common examples. These repeating units are linked together to form a crystalline framework or structure that contains cavities or channels of molecular dimensions within the crystal structure. Thus, these aluminosilicate zeolites have at least oxygen (O), aluminum (Al) and silicon (Si) as atoms incorporated into the framework structure. Zeolites are composed of silica (SiO 2 ) and alumina (Al 2 O 3 ) crystal framework, so the SiO 2 and Al 2 O 3 The signal strength can be characterized by the signal strength ratio (SAR).

[0028] Zeolites may exhibit any of the framework topographies known in the art, including, but not limited to, chabazite (framework designation = "CHA"), chiavenite (CHI), faujasite (FAU), Linde type A (LTA), and laumontite (LAU). The framework designation represents a code designated by the International Zeolite Association (IZA) that defines the framework structure of the zeolite. Thus, for example, chabazite refers to a zeolite in which the predominant crystalline phase of the zeolite is "CHA".

[0029] The crystalline phase or framework structure of a zeolite can be characterized by X-ray diffraction (XRD) data. However, XRD measurements can be affected by various factors, including the growth direction of the zeolite, the ratio of constituent elements, the presence or absence of adsorbed substances or defects, and the deviation of the intensity ratio or the deviation of the position of each peak in the XRD spectrum. Thus, as described in the definition provided by the International Zeolite Society, the deviation of 10% or less, or 5% or less, or 1% or less in the measured values ​​of each parameter of the framework structure of each zeolite is within the expected tolerance.

[0030] In one embodiment of the present disclosure, the zeolite may include natural zeolites, synthetic zeolites, or mixtures thereof. Alternatively, the zeolite is a synthetic zeolite, since such zeolites exhibit greater uniformity in terms of aluminum-silicon ratio (SAR), crystal size, and crystal morphology, and have fewer and lower concentrations of impurities (e.g., alkaline earth metals). The zeolite may be selected to be one or more zeolites having a silicon (Si)-aluminum (Al) ratio (SAR) in the range of about 0.5 to 500, or the silicon (Si)-aluminum (Al) ratio (SAR) may be in the range of about 1 to about 250, or in the range of about 1 to about 100, or in the range of about 2 to 50.

[0031] The zeolites in the zeolitic materials of the present disclosure may include a plurality of particles having or exhibiting morphologies that are plate-like, cubic, spherical, or combinations thereof. Alternatively, the morphology is predominantly spherical in nature. These particles have an average particle size (D) ranging from about 50 nanometers (nm) to about 30 micrometers (μm). 50) may be shown. Alternatively, the average particle size may be in the range of about 100 nanometers (nm) to about 25 micrometers (μm), alternatively in the range of 500 nanometers (nm) to about 20 micrometers (μm), alternatively in the range of 1 micrometer (μm) to about 5 micrometers (μm). A scanning electron microscope (SEM) or other optical and digital image processing methods known in the art may be used to determine the shape or morphology or both of the inorganic additive. The average particle size and particle size distribution may be measured using any conventional technique, such as sieving, microscopy, Coulter counting, dynamic light scattering, or particle image analysis, to name a few. Alternatively, a laser particle analyzer is used to determine the average particle size and the corresponding particle size distribution.

[0032] In addition, zeolite in zeolite-based materials has a diameter of about 1 m 2 / g~about 7500m 2 / g. Alternatively, the surface area may be in the range of about 3 m 2 / g~about 5000m 2 / g range or about 5m 2 / g ~ approx. 2500m 2 / g range or about 10m 2 / g~about 1000m 2 / g range or about 25m 2 / g~about 750m 2 The average pore size of the zeolite in the zeolitic material may range from 0.1 nm to 20 nm. Alternatively, the average pore size is between about 0.5 nm to about 15 nm, with a pore volume ranging from about 0.05 cc / g to about 3.0 cc / g, or from 0.1 cc / g to about 2.0 cc / g. Measurement of the surface area and pore volume of the zeolite in the zeolitic material may be performed using any known technique, including, but not limited to, microscopy, small angle X-ray scattering, mercury intrusion porosimetry, and Brunauer-Emmett-Teller (BET) analysis. Alternatively, the surface area and pore volume are determined using Brunauer-Emmett-Teller (BET) analysis.

[0033] The zeolitic material may have a sodium (Na) concentration of about 0.01% to about 2.0% by weight based on the total weight of the zeolitic material. Alternatively, the Na concentration may range from about 0.1% to about 1.0% by weight. The zeolitic material may include one or more ion-exchanged zeolites. These ion-exchanged zeolites may include, but are not limited to, lithium ion-exchanged zeolites. The lithium ion concentration is about 0.05% to about 25% by weight, alternatively about 0.1% to about 20% by weight, alternatively about 0.2% to about 15% by weight based on the total weight of the zeolites present in the zeolitic material, such as lithium ion-exchanged zeolites. If desired, the zeolites in the zeolitic material may further include one or more doping elements selected from Li, Na, Al, Mn, Sm, Y, Cr, Eu, Er, Ga, Zr, and Ti.

[0034] Referring to FIG. 2, the zeolitic material may initially have a moisture content of about 23 wt. % before or without drying as shown in 37. The moisture content may be reduced to about 7.5 wt. % after drying as shown in 39 at 80° C. in vacuum for at least several hours (e.g., 2-7 hours). Alternatively, the drying time may be 7 hours or more. The drying time of the dried zeolitic material 39 shown in FIG. 2 is 7 hours. This moisture content is considered very high for a conventional battery, since typical moisture contents from cell components (cathode, anode, separator) are on the scale of hundreds of ppm. However, the high moisture content shown in FIG. 2 shows LiMn with zeolite coated electrodes. 2 O 4 / Li 4 Ti 5 O 12The full cells show similar first cycle coulombic efficiency (93%) as the corresponding cells with commercial PE separators. The thickness of the zeolite coating is approximately 30-40 μm with 90 wt% zeolite and 10 wt% binder. Thus, full cells with zeolite coatings as separators on the electrodes can be fabricated in accordance with the present disclosure to perform similarly to conventional full cells, despite the large amount of water in the zeolite.

[0035] The zeolitic material may have a moisture content of more than 23% by weight without drying. However, generally, the lower the moisture content, the better. The zeolitic material may have a moisture content of 35% by weight or less. Alternatively, the moisture content is 23% by weight or less, alternatively, the moisture content is 11% by weight or less, or alternatively, the moisture content is 7% by weight or less.

[0036] A free-standing zeolite membrane with a relatively small thickness is very difficult to manufacture due to the brittleness of inorganic membranes. Comparatively, it is more practical to attach or coat a zeolite layer onto an existing electrode. In the manufacture, the cathode or anode can be formed as part of the electrode using a roll-to-roll coating process, including a bi-layer coating or multi-layer coating process. In other words, the electrode is formed by applying at least one layer of coating of an active material that can function as the cathode or anode. A similar bi-layer coating or multi-layer coating process can be used to coat the zeolite-based material onto an existing electrode (e.g., cathode or anode) layer.

[0037] The zeolite-based material may be applied directly to or on the surface of the electrode layer. However, it is more difficult to ensure that the applied zeolite layer functions as a separator, since the separator must electrically insulate the cathode and anode not only during the manufacturing process of the battery, but also during the life of the battery. In comparison, most commercially available porous PP / PE separators generally have a porosity in the range of 37% to 55%, whereas the porosity of the zeolite-based material or coating tends to be high without calendaring. For example, the porosity of a typical zeolite-based material or coating can be as high as about 73% for an as-coated zeolite membrane with 7 wt.% binder and 93 wt.% zeolite. Due to the high level of porosity, a typical zeolite-based material or coating may not be able to sufficiently electrically insulate the anode from the cathode during cycling. However, the porosity of the zeolitic materials of the present disclosure can be controlled so that the resulting coating or layer exhibits a porosity of about 37%-55%, or even 55% or less, which is at least comparable to commercially available PP / PE separators. If desired, the porosity of the zeolitic materials of the present disclosure can be even lower, for example, in the range of about 30%-36%. The porosity of the zeolitic materials can be controlled by adjusting the coating formulation. For example, particles having a bimodal or trimodal particle size distribution can be used in the coating formulation. The interior space between the larger particles may be filled with smaller particles to reduce the porosity of the coating. The porosity may be reduced by increasing the polymer binder / zeolite mass ratio. With increasing polymer content, the porosity of the coating decreases. This is because the polymer molecules fill the empty interior spaces that escape between the zeolite particles. In extreme cases, a pure polymer membrane coating may have almost no porosity.

[0038] Since the zeolitic material or coating is applied to a relatively hard substrate (such as an electrode), the adjustment of the porosity can be achieved by mechanically compressing the zeolitic coating to reduce the porosity. This process is called calendaring in the battery industry. This calendaring step for the zeolitic coating may be performed at temperatures from room temperature to about 140° C. on uncalendared electrode coating layers or on partially calendered electrode coating layers or on fully calendered electrode coating layers. The evaluation of the coating porosity can be done by measuring the mass loading per area of ​​the coating and its thickness. Using the true density of the zeolitic material, the coating thickness at 0% porosity can be calculated with the known formula of mass loading per area / density. The coating porosity is then calculated using the formula (1-coating thickness at 0% porosity / measured thickness)*100%.

[0039] Compared with commercially available PP / PE separators, the tortuosity of the zeolitic material or coating of the present disclosure is expected to be smaller. This means that lithium dendrites are more likely to form and penetrate the zeolite layer since they encounter less resistance. Therefore, the coating thickness of the zeolitic material needs to be thicker than that of a PP / PE separator with a similar porosity. Generally, a zeolitic material with a thickness of 1 micrometer (μm) to 200 μm is used. Alternatively, the thickness of the zeolitic material ranges from 20 μm to 80 μm with a porosity of 30% to 55%. Alternatively, the thickness of the zeolitic material or coating ranges from 40 μm to 60 μm.

[0040] In one example, if the battery does not have a pre-deposited anode (i.e., anode-free) or does not have a lithium metal anode, the thickness range of the zeolitic material or coating is 20-100 μm and the porosity is 30-55%. Alternatively, to allow for the extra mechanical strength required to block lithium dendrites during cycling, the thickness ranges from 40 μm to 100 μm and the porosity is 30-55%. In another example, graphite, Li 4 Ti 5 O 12 , Nb 2 O 5 Alternatively, for cells having a silicon anode, the zeolitic material may have a thickness of 1-100 μm, alternatively about 10-80 μm, with a porosity in the range of 30-55%.

[0041] The zeolite-based material or coating is applied only to the positive cathode. Alternatively, the zeolite coating is applied only to the negative anode. Alternatively, the zeolite coating is applied to both the positive and negative cathodes and anodes. Since the function of the zeolite-based material is to electrically insulate the cathode electrode from the anode electrode, it can effectively serve this purpose as long as it is coated between the active layers of the cathode and anode, respectively. However, since the cathode and anode have different electrode thicknesses and different binder compositions, it may be desirable to coat the zeolite coating on one or both of the electrodes. For example, in high energy EV cells, the capacity loading per area of ​​the anode and cathode is very high (e.g., 4.4 mAh / cm2). 2 These high capacity loadings per area can result in very thick cathode electrodes (e.g., greater than 170 μm). Such thick electrodes are prone to cracking unless further coatings are applied. Furthermore, if a zeolite material or coating is applied to such a thick electrode, the coating can crack or the electrode or part of it can peel off.

[0042] In another example, NMP is used as a solvent for the application of the cathode to the positive electrode. If the slurry used to form the zeolitic material contains NMP as a solvent, the wet zeolite coating will partially dissolve the existing cathode active layer and damage the positive electrode. In this case, it is necessary to select a slurry composition that does not contain NMP to directly coat the zeolitic material on the cathode. However, the slurry for forming the zeolitic material that contains NMP as a solvent can be used to apply such a zeolitic material to the anode. This is because graphite electrodes are generally prepared using aqueous slurries. The cmc and SRR binders incorporated in the graphite anode are not soluble in NMP.

[0043] The active materials of the positive electrode 10 and the negative electrode 20 may be any of the materials known to serve this function in lithium ion secondary batteries. The active materials used in the positive electrode 10 may include, but are not limited to, lithium transition metal oxides or transition metal phosphates. Some examples of active materials that may be used in the positive electrode 10 include LiCoO 2 , LiMn 2 O 4 , LiFePO 4 , N.C.M., N.C.A., NCMA, LiNi a Co b Mn c Al d O 2 (a+b+c+d=1), LiFe 0.2 Mn 0.8 PO 4 The active materials used in the negative electrode 15 include, but are not limited to, silicon and lithium metal, or their derivatives or combinations thereof, as well as graphite, hard carbon, soft carbon, Nb 2 O 5 , Li 4 Ti 5 O 12 Alternatively, the active material used in the negative electrode is silicon or lithium metal, which has an order of magnitude higher specific capacity. Alternatively, the anode active material is lithium, or there is no anode active material when the battery is manufactured.

[0044] The current collectors 7, 17 of both the positive electrode 10 and the negative electrode 20 may be made of any metal known in the art for use in lithium battery electrodes, such as aluminum for the cathode and copper for the anode. The cathode 5 of the positive electrode 10 and the anode 15 of the negative electrode 20 are generally composed of two different active materials.

[0045] If desired, the zeolite-based material or coating may further include a binder to bind the zeolite particles together and aid in adhesion to the electrode. The binder may be selected from any of the known conventional binders commonly used in lithium-ion batteries, including organic complexes, inorganic oxides, or inorganic hydroxides. Some examples of suitable organic complexes include, but are not limited to, PVDF, cmc, SBR, PTFE, PAA (polyacrylic acid), PVA, PEI, and PAI. The mass ratio of zeolite to binder should be in the range of 99.5% / 0.5% to 50% / 50%. Alternatively, it may be in the range of 90% / 10% to 60% / 40%. The zeolite-based material or coating is generally more flexible with a higher binder content. The binder may be an inorganic oxide or hydroxide containing one or more elements selected from, but not limited to, Al, Zr, Mg, Ti, and Ce. Zeolitic materials with high binder content are preferred for use in anodes that are susceptible to lithium dendrite formation during cycling.

[0046] The electrolyte 30 is used to support the oxidation / reduction process between the anode 15 and the cathode 5 and to provide a medium for the flow of non-reactive metal ions between the anode 15 and the cathode 5. The electrolyte 30 may be a solution of a non-reactive metal salt in an organic solvent, whereby the non-reactive metal salt dissolves to form the non-reactive metal ions. The non-reactive metals that form ions in the electrolyte may be lithium, sodium, potassium, magnesium, calcium, aluminum, or mixtures thereof. Alternatively, the non-reactive metal salt is a lithium salt. Some specific examples of lithium salts include lithium hexafluorophosphate (LiPF 6 Examples of suitable electrolytes include, but are not limited to, lithium bis(oxalato)borate (LiBOB), lithium bis(trifluoromethanesulfonyl)imide (LiTFSi). These lithium salts may form solutions with organic solvents, some of which include ethylene carbonate (EC), ethyl methyl carbonate (EMC), diethyl carbonate (DEC), dimethyl carbonate (DMC), propylene carbonate (PC), vinylene carbonate (VC), and fluoroethylene carbonate (FEC). A specific example of an electrolyte is 1 mole of LiPF in a mixture of ethylene carbonate and diethyl carbonate. 6 Solution (EC / DEC = 50 / 50 volume%).

[0047] Referring now to FIG. 3A, an electrochemical cell 1A is shown according to one embodiment of the present disclosure. The electrochemical cell 1A includes a positive electrode 10, a negative electrode 20, an electrolyte 30, and a separator 40 in the form of a zeolitic material, which includes one or more natural or synthetic zeolites, attached directly to the negative electrode 20. The positive electrode 10 is configured to reversibly extract and insert non-reactive metal ions therefrom, while the negative electrode 20 is configured to reversibly accept and release non-reactive metal ions. Each electrode 10, 20 typically includes a current collector 7 or 17 and an active material that functions as a cathode 5 or anode 15, respectively. As shown in FIG. 3A, the zeolitic material separator 40 is attached directly to the anode 15. However, it should be understood that negative electrode 20 may be an "anode-free" electrode having only a current collector 17, whereby a zeolitic separator 40 may be attached directly to the current collector 17 without going beyond the scope of this disclosure.

[0048] 3A , electrolyte 30 is located between and in contact with positive electrode 10 and negative electrode 20 such that electrolyte 30 supports the reversible flow of non-reactive metal ions 35 between negative electrode 20 and positive electrode 10. Separator 40 is configured to electrically insulate positive electrode 10 from negative electrode 20 while being permeable to the reversible flow of non-reactive metal ions 35 through separator 40.

[0049] Referring now to FIG. 3B, in accordance with another embodiment of the present disclosure, the electrochemical cell 1B of FIG. 3B is shown as a secondary battery 1B for use in a lithium ion secondary battery. In this particular application, the ions 35A that reversibly flow between the anode 15 and the cathode 5 are lithium ions (Li + ).

[0050] Similar to Fig. 3B, Figs. 3C and 3D both show electrochemical cells as secondary batteries 1C, 1D for use in lithium-ion secondary batteries. According to one embodiment of the present disclosure, a separator 40 formed from a zeolitic material may be attached directly to the positive electrode 10 or to a portion of said electrode, i.e., the cathode 5, as shown in Fig. 3C. Similarly, a separator 40 made from a zeolitic material may be applied to both the negative electrode 20 (e.g., anode 15) and the positive electrode 10 (e.g., cathode 5), as shown in Fig. 3D.

[0051] According to yet another aspect of the present disclosure, one or more secondary batteries may be combined to form an electrochemical cell, such as a lithium-ion secondary battery. An example of such a battery is shown in FIG. 4. In this battery, four secondary batteries 1B are stacked or combined to form a larger single secondary battery and encapsulated in a housing 55 to form a lithium-ion secondary battery 50A. The lithium-ion secondary battery 50A includes a housing 60 having an inner wall that surrounds or encapsulates the secondary battery 1B of FIG. 3B to provide both physical and environmental protection. Although the battery 50A shown in FIG. 4 incorporates four secondary batteries 1B of FIG. 3B, one skilled in the art will understand that such a battery 50A may include other numbers of secondary batteries 1B. Additionally, the secondary battery 1B of FIG. 3B in the battery 50A may be replaced with the secondary battery 1C of FIG. 3C or the secondary battery 1D of FIG. 3D.

[0052] FIG. 5 illustrates another example of a battery 50B in which four secondary batteries are stacked or arranged in series to form a larger capacity battery 50B, each housed individually. In this battery 50B, the four secondary batteries may include one or more of the batteries 1B, 1C, 1D shown in FIGS. 3B-3D. Alternatively, the secondary battery may include one or more of a conventional battery 1. Alternatively, the secondary battery may include a mixture of batteries 1B, 1C, 1D formed in accordance with the teachings of the present disclosure. As shown in FIG. 5, the battery 50B is shown to include, by way of example and not limitation, a conventional battery 1 and three different batteries 1B, 1C, 1D formed in accordance with the teachings of the present disclosure.

[0053] 4 and 5 show how secondary batteries 1B-1D can be incorporated into lithium-ion secondary batteries 50A, 50B, but those skilled in the art will appreciate that the same principles can be used to enclose or encase one or more electrochemical cells 1A in a housing 55 for use in other applications. In these electrochemical cells 1A, a zeolite-based separator 40 may be applied directly to one or more electrodes 10, 20, such as in the form of a coating applied to the surface of the cathode 5, the surface of the anode 15, or a combination thereof.

[0054] The housing 55 may be constructed of any material known in the art to be used for such applications and may be in any shape required or desired for a particular application. For example, lithium ion batteries are generally housed in three different primary forms or shapes: cylindrical, prismatic, or soft pouch. The housing 55 for cylindrical batteries may be made of aluminum, steel, etc. Prismatic batteries generally have a rectangular housing 55 rather than a cylindrical shape. The soft pouch housing 55 may be made in a variety of shapes and sizes. These soft housings may consist of an aluminum foil pouch coated with plastic on the inside, outside, or both. The soft housing 55 may be a polymeric type case. The polymeric composition used for the housing 55 may be any known polymeric material conventionally used for lithium ion secondary batteries. One specific example among many is the use of a laminate pouch having a polyolefin layer on the inside and a polyamide layer on the outside. The soft housing 55 should be designed to mechanically protect the secondary cells within the batteries 50A, 50B.

[0055] Due to the large internal surface area, zeolites can also be used as supports for secondary materials. The ratio of zeolites to secondary materials ranges from 99.9% / 0.1% to 50.1% / 49.9% by weight. The secondary materials may include, but are not limited to, catalysts or flame retardants or both.

[0056] According to one aspect of the present disclosure, a flame retardant can be loaded into the pores, which allows the zeolite-based material to function as a flame retardant. In this example, the flame retardant must be insoluble in the organic electrolyte, which is an organic carbonate in the lithium-ion battery. The flame retardant material can be selected from the group consisting of inorganic materials, polymeric materials, organic-inorganic hybrid materials, and organic materials. Conventional flame retardant materials include magnesium hydroxide, aluminum hydroxide, phosphates, and bromates, which can be utilized as needed. Various materials with a high content of crystal water can be selected. This is because the water released at high temperatures reduces the temperature of the battery and acts as a flame retardant.

[0057] According to another aspect of the present disclosure, the zeolite may be impregnated or functionalized with a catalyst. The catalyst may be configured to catalyze the polymerization reaction of unsaturated carbonates (such as ethylene carbonate, propylene carbonate, or trimethylene carbonate) at elevated temperatures. The catalyst may be CeO 2 and sodium stannate trihydrate.

[0058] The specific examples presented in this disclosure are intended to illustrate various embodiments of the present invention and should not be construed as limiting the scope of the disclosure. The embodiments described herein have been described so as to enable a clear and concise specification to be written, but it is intended and will be understood that the embodiments may be combined or separated in various ways without departing from the invention. For example, it will be understood that all preferred features described herein are applicable to all aspects of the invention described herein.

[0059] Example 1 Zeolite coating LiMn 2 O 4 / Zeolite Coating Li 4 Ti 5 O 12 Full cell and LiMn 2 O 4 / PE / Li 4 Ti5 O 12 Preparation of the reference cell

[0060] LiMn 2 O 4 , Li 4 Ti 5 O 12 Commercially available electrode materials include C65, PVDF (Gelon, China), and CNT (C-nano, China). The cathode electrode is made of 92 wt% LiMn 2 O 4 The cathode was fabricated with 2 wt% C65, 2 wt% CNT, and 4 wt% polyvinylidene fluoride (PVDF). The area-specific capacity loading of the cathode was approximately 0.8 mAh / cm. 2 The anode electrode was 92% by weight Li 4 Ti 5 O 12 , 3 wt.% C65, and 5 wt.% PVDF, with a capacity loading per area of ​​approximately 0.8 mAh / cm 2 For the reference cell, a commercially available ceramic oxide-coated polyethylene (PE) separator with a thickness of 16 μm was used. For the zeolite-coated cells, a layer of zeolite-based material with a pressed thickness of about 15–20 μm was deposited on both the cathode and anode electrodes. Full cells were fabricated by laminating a zeolite-coated cathode and a zeolite-coated anode without a commercial separator. The electrolyte was 1.0 M LiPF 6 in ethylene carbonate and diethyl carbonate (EC / DEC ratio 1 / 3), 1 wt% fluoroethylene carbonate (FEC), and 1 wt% vinylene carbonate (VC) (Gelon, China).

[0061] Referring now to Figure 6, as an electrochemical test, both cells were charged and discharged at room temperature. At this time, the voltage range was 1.5 V to 2.7 V, the charge and discharge rate was C / 10, and the upper limit current was limited (tapered) to C / 20 at 2.7 V. As shown in Figure 6, the charge and discharge curves for the first cycle of the full cell including the zeolite-coated electrode showed similar performance to the full cell with a conventional PE separator.

[0062] Although the embodiments have been described herein in a manner that enables a clear and concise specification to be written, it is intended and will be understood that the embodiments may be combined or separated in various ways without departing from the invention, and for example, it will be understood that all preferred features described herein are applicable to all aspects of the invention described herein.

[0063] Those skilled in the art will appreciate in light of this disclosure that many changes can be made in the specific embodiments disclosed herein without departing from or exceeding the spirit or scope of the disclosure and still obtain like or similar results. Those skilled in the art will further appreciate that any properties reported herein represent properties that are typically measured and that can be obtained in a number of different ways. The method described herein represents one such method, and the use of other methods does not depart from the scope of the disclosure.

[0064] The foregoing description of various forms of the present invention has been presented for purposes of illustration and description. The foregoing description is not intended to be exhaustive or to limit the present invention to the precise forms disclosed. Numerous modifications or variations are possible in light of the above teachings. The forms discussed have been chosen and described in order to best explain the principles of the present invention and its practical application. This will enable those skilled in the art to best utilize the present invention with various modifications in various forms suited to the particular uses contemplated. All such modifications and variations are within the scope of the present invention, as determined by the appended claims, when interpreted in accordance with the extent to which they are fairly, legally, and equitably entitled.

Claims

1. 1. A cell for use in an electrochemical cell, comprising: The electrochemical cell comprises: A positive electrode, The non-reactive metal ions are reversibly extracted from and inserted into the positive electrode. A positive electrode and A negative electrode, configured to reversibly accept and release the non-reactive metal ions; A negative electrode; an electrolyte located between and in contact with the negative electrode and the positive electrode, supporting a reversible flow of the non-reactive metal ions between the positive electrode and the negative electrode; An electrolyte; a separator in the form of a zeolitic material comprising one or more natural or synthetic zeolites, directly attached to at least one of the positive electrode and the negative electrode, the separator is configured to electrically insulate the positive electrode from the negative electrode while being permeable to reversible flow of the non-reactive metal ions through the separator; Separator and A cell comprising:

2. 2. The cell of claim 1 , The zeolite-based material deposited on at least one of the positive electrode and the negative electrode has a thickness in the range of 1 micrometer (μm) to 200 μm. cell.

3. 3. A cell according to claim 1 or 2, The positive electrode has an active material as a cathode and a current collector in contact with the cathode, The active material is LMNO, LiMn 2 O 4 , LiFePO 4 , LiNi a Co b Mn c A d O 2 (a+b+c+d=1), and LiFe 0.2 Mn 0.8 P.O. 4 Including one or more of the following: cell.

4. A cell according to any one of claims 1 to 3, The negative electrode has an active material as an anode and a current collector in contact with the anode, The active material is graphite, hard carbon, soft carbon, silicon, Li 4 Ti 5 O 12 , Nb 2 O 5 and one or more of these derivatives. cell.

5. The cell according to any one of claims 1 to 3, The negative electrode is an "anode-free" electrode and has only a current collector. cell.

6. A cell according to any one of claims 1 to 5, The zeolitic material has a moisture content of 35% or less. cell.

7. 7. The cell of claim 6, The zeolitic material has a moisture content of 7% or less. cell.

8. A cell according to any one of claims 1 to 7, The zeolite-based material has a porosity of 55% or less. cell.

9. 9. The cell of claim 8, The porosity of the zeolitic material is in the range of 30% to 36%. cell.

10. A cell according to any one of claims 1 to 9, The zeolitic material further comprises a binder; The ratio of the zeolite to the binder is in the range of 99.5% / 0.5% to 10% / 90% by weight. cell.

11. 11. The cell of claim 10, The binder comprises an organic complex, an inorganic oxide, or an inorganic hydroxide. cell.

12. 12. The cell of claim 11, the organic complex is PVDF, cmc, SBR, PTFE, PAA (polyacrylic acid), PVA, PEI, or PAI; The inorganic oxide or the inorganic hydroxide contains aluminum, magnesium, zirconium, or cerium as an element. cell.

13. A cell according to any one of claims 1 to 12, The zeolitic material further comprises one or more secondary materials; The ratio of the zeolite to the secondary material ranges from 99.9% / 0.1% to 50.1% / 49.9% by weight. cell.

14. 14. The cell of claim 13, the one or more secondary materials include a flame retardant material; cell.

15. A cell according to any one of claims 1 to 14, The zeolite has an average particle size ranging from 50 nanometers (nm) to 30 micrometers (μm); cell.

16. A cell according to any one of claims 1 to 15, The zeolite comprises one or more ion-exchanged zeolites. cell.

17. 17. The cell of claim 16, The ion-exchanged zeolite is a lithium-exchanged zeolite. cell.

18. 20. The cell of claim 17, The lithium-exchanged zeolite has a lithium mass content ranging from 0.1% to 20% by weight, based on the total weight of the lithium-exchanged zeolite. cell.

19. A cell according to any one of claims 1 to 18, The zeolite has an average pore size in the range of 0.1 nm to 20 nm. cell.

20. A cell according to any one of claims 1 to 19, The zeolite has an aluminum-silicon ratio (SAR) in the range of 0.5 to 500. cell.

21. A cell according to any one of claims 1 to 20, the non-reactive metal ion in the electrolyte is lithium, sodium, potassium, magnesium, calcium, aluminum, or a mixture thereof; cell.

22. A lithium ion secondary battery, One or more cells according to any one of claims 1 to 21; One or more housings, an interior wall from one of said one or more housings encapsulating at least one of said cells; One or more housings; Equipped with Lithium-ion secondary battery.