Backplate Film

The back plate film with a retardation base layer and adhesive layer addresses image distortion issues in under-display cameras, enabling clear image capture.

JP2024538959AInactive Publication Date: 2024-10-28LG CHEM LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024520614
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-25
Filing Date
2022-11-25
Publication Date
2024-10-28
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional back plate films for under-display cameras in mobile phones suffer from image distortion due to high phase difference in PET films and yellowish color issues with PI films, limiting effective color correction.

Method used

A back plate film comprising a retardation base layer with specific in-plane and thickness direction retardation values, combined with an adhesive layer, to minimize image distortion and enhance color accuracy.

Benefits of technology

The film allows the front camera of a mobile phone to capture subjects without image distortion, ensuring clear and accurate image reproduction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024538959000001_ABST
    Figure 2024538959000001_ABST
Patent Text Reader

Abstract

The present application relates to a backplate film. The present application provides a backplate film for an under-display camera, which enables a front camera of a mobile phone to capture an object without image distortion. The backplate film of the present application may be usefully used for, for example, an OLED panel.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to a backplate film.

[0002] This application claims the benefit of priority based on Korean Patent Application No. 10-2021-0164149 filed on November 25, 2021, and all contents disclosed in the documents of that Korean patent application are incorporated herein by reference. [Background technology]

[0003] In the case of a front camera of a mobile phone, it is manufactured by punching out a front camera area in an OLED (organic light emitting diode) panel and assembling a camera module (Patent Literature 1: Korean Patent Publication No. 10-2020-0098741).

[0004] In order to realize a display on the front camera, the front camera area does not need to be punched out in the OLED panel, but rather the internal camera (under-display camera) needs to be designed to capture the subject through the OLED panel or polarizer.

[0005] Backplate films applied to conventional OLED panels use PET (Polyethylene Terephthalate) film or PI (Polyimide) film as the base film. However, in the case of conventional PET film, the object is distorted due to high phase difference, and in the case of PI film, the color is yellowish, so there is a limit to color correction. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Korean Patent Publication No. 10-2020-0098741 Summary of the Invention [Problem to be solved by the invention]

[0007] The present application provides a backplate film for an under-display camera that enables the front camera of a mobile phone to capture an object without image distortion. [Means for solving the problem]

[0008] The present application relates to a backplate film. Fig. 1 exemplarily illustrates the backplate film of the present application. The backplate film may include a retardation substrate layer 10a and a first adhesive layer 10b formed on one side of the retardation substrate layer 10a.

[0009] In this specification, a backplate film that does not include the protective film 20 and release film 30 described below, but includes the retardation substrate layer 10a and the first adhesive layer 10b, may be referred to as a first backplate film, and a backplate film that includes all of the protective film 20 and release film 30 described below, the retardation substrate layer 10a, and the first adhesive layer 10b may be referred to as a second backplate film.

[0010] The absolute value of the in-plane retardation (R0) value of the retardation substrate layer may be 6,000 nm or more. The absolute value of the thickness direction retardation (Rth) value of the retardation substrate layer may be 6,000 nm or more. In this specification, the in-plane retardation (R0) value may be calculated by the following formula 1. In addition, in this specification, the thickness direction retardation (Rth) value may be calculated by the following formula 2. When the retardation value of the retardation substrate layer is within the above range, a backplate film for an under-display camera that allows the front camera of a mobile phone to capture an object without image distortion can be provided.

[0011] The upper limit of the absolute value of the in-plane retardation (R0) value of the retardation base layer may be, for example, 10,000 nm or less.The upper limit of the absolute value of the thickness direction retardation (Rth) value of the retardation base layer may be, for example, 10,000 nm or less.

[0012] The absolute value of the in-plane retardation (R0) value of the retardation substrate layer may be, for example, 6,000 nm or more, 6,500 nm or more, 7,000 nm or more, 7,100 nm or more, 7,200 nm or more, 7,300 nm or more, or 7,400 nm or more, and may be 10,000 nm or less, 9,500 nm or less, 9,000 nm or less, 8,500 nm or less, 8,000 nm or less, or 7,500 nm or less. In one example, the in-plane retardation (R0) value of the retardation substrate layer may be a positive number.

[0013] The absolute value of the thickness direction retardation (Rth) value of the retardation substrate layer may be, for example, 6,000 nm or more, 6,500 nm or more, 7,000 nm or more, 7,500 nm or more, 8,000 nm or more, or 8,100 nm or more, and may be 10,000 nm or less, 9,500 nm or less, 9,000 nm or less, 8,500 nm or less, or 8,300 nm or less. In one example, the thickness direction retardation (Rth) value of the retardation substrate layer may be a negative number.

[0014] [Formula 1] R0 = (nx-ny) × d

[0015] [Formula 2] Rth = [(nx + ny) / 2-nz] × d In formulas 1 and 2, nx, ny, and nz are the refractive indices of the retardation substrate layer in the x-axis, y-axis, and z-axis directions for light with a wavelength of 550 nm, respectively, and d is the thickness (nm) of the retardation substrate layer. The x-axis means an axis parallel to the slow axis direction of the retardation substrate layer, the y-axis means an axis parallel to the fast axis direction of the retardation substrate layer, and the z-axis means an axis parallel to the thickness direction of the retardation substrate layer.

[0016] In the physical properties mentioned in this specification, if the measurement temperature affects the results, the physical properties are measured at room temperature unless otherwise specified. The term room temperature refers to a natural temperature that is not heated or cooled, and is usually a temperature within a range of about 10°C to 30°C, or about 23°C or about 25°C. Furthermore, unless otherwise specified in this specification, the unit of temperature is °C. In the physical properties mentioned in this specification, if the measurement pressure affects the results, the physical properties are measured at normal pressure unless otherwise specified. The term normal pressure refers to a natural pressure that is not pressurized or reduced, and normal pressure is usually about 1 atmosphere.

[0017] The thickness of the retardation substrate layer may be appropriately selected within a range that does not impair the object of the present application. For example, the thickness of the retardation substrate layer may be within a range of 20 μm to 200 μm. Specifically, the thickness of the retardation substrate layer may be 20 μm or more, 40 μm or more, 60 μm or more, or 80 μm or more, and may be 200 μm or less, 180 μm or less, 160 μm or less, 140 μm or less, 120 μm or less, or 100 μm or less. If the thickness of the retardation substrate layer is too thin, problems with processability such as breakage and bending may occur, and if the thickness of the retardation substrate layer is too thick, it is difficult to apply the OLED curvature design in the process of the customer company, and there is a problem that durability is reduced due to repulsion force, so it may be advantageous for the thickness of the retardation substrate layer to be within the above range.

[0018] The retardation substrate layer may have antistatic properties. In one example, the back plate film may include an antistatic layer formed on one side of the retardation substrate layer. In this case, the antistatic layer may be formed on the opposite side of the retardation substrate layer to the side where the first adhesive layer is located. The surface resistance of the antistatic layer may be, for example, 10 4 Ω / square~10 11 The surface resistance of the antistatic layer may be in the range of 10 4 Ω / square or more, 10 5 Ω / square or more, 10 6 Ω / square or more, 10 7Ω / square or more or 10 9 It may be Ω / square or more, and 10 11 Ω / square or less or 10 10 It may be less than or equal to Ω / square.

[0019] The surface of the retardation substrate layer on which the first adhesive layer is attached may be subjected to a corona treatment. This can increase the adhesive strength between the retardation substrate layer and the acrylic adhesive layer when the first adhesive layer is, for example, an acrylic adhesive. In one example, the retardation substrate layer may be subjected to a corona treatment under conditions of 5A (amperes) to 25A (amperes) based on a line speed of 20m / min.

[0020] The first adhesive layer may be formed on one side of the retardation substrate layer. In the present specification, the adhesive layer may be, for example, a layer of an adhesive composition. In the present specification, the term "adhesive composition layer" may mean a layer formed by coating or curing an adhesive composition. The term "curing of an adhesive composition" may mean realizing a crosslinked structure in the adhesive composition through a physical or chemical action or reaction of components contained in the adhesive composition. Curing may be induced, for example, by maintaining at room temperature, applying moisture, applying heat, irradiating with active energy rays, or by simultaneously carrying out two or more of the above steps, and the adhesive composition in which curing is induced depending on each case may be called, for example, a room temperature curing adhesive composition, a moisture curing adhesive composition, a heat curing adhesive composition, an active energy ray curing adhesive composition, or a hybrid curing adhesive composition.

[0021] The first adhesive layer may include an adhesive resin and a curing agent. In one example, the adhesive resin may be an acrylic resin. In this specification, the acrylic resin may mean a resin in which acrylic monomers are 70 wt% or more, 75 wt% or more, 80 wt% or more, or 85 wt% or more of monomers constituting the resin.

[0022] The acrylic resin may be an acrylic polymer including polymerized units derived from a (meth)acrylic acid ester monomer. In the present specification, the term "monomer" refers to any type of compound capable of forming a polymer through a polymerization reaction, and a polymer including polymerized units derived from a certain monomer may refer to a polymer formed by polymerizing the certain monomer.

[0023] As the (meth)acrylic acid ester compound, for example, an alkyl (meth)acrylate may be used. As the alkyl (meth)acrylate, for example, an alkyl group having 1 to 20 carbon atoms, 1 to 14 carbon atoms, 1 to 12 carbon atoms, 1 to 8 carbon atoms, or 1 to 4 carbon atoms may be used in consideration of the adjustment of cohesive strength, glass transition temperature, and adhesiveness. In the above, the alkyl group may be, for example, linear, branched, or cyclic. Examples of such monomers include methyl (meth)acrylate, ethyl (meth)acrylate, n-propyl (meth)acrylate, isopropyl (meth)acrylate, n-butyl (meth)acrylate, sec-butyl (meth)acrylate, 2-methylheptyl (meth)acrylate, pentyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, 2-ethylbutyl (meth)acrylate, n-octyl (meth)acrylate, isobornyl (meth)acrylate, isooctyl (meth)acrylate, isononyl (meth)acrylate, or lauryl (meth)acrylate, and one or more of the above may be appropriately selected and used. Although not particularly limited, as the methacrylic acid ester compound, an alkyl (meth)acrylate having an alkyl group with 1 to 4 carbon atoms and an alkyl (meth)acrylate having an alkyl group with 5 to 8 carbon atoms may be mixed and used.

[0024] The acrylic polymer may further include a polymerization unit derived from a copolymerizable monomer having a crosslinkable functional group (hereinafter, sometimes simply referred to as a crosslinkable monomer). In this specification, the copolymerizable monomer having a crosslinkable functional group may mean a compound that has a site capable of copolymerizing with other monomers contained in the polymer, such as the (meth)acrylic acid ester monomer, and further has a crosslinkable functional group to impart a crosslinkable functional group to the polymer. Examples of the crosslinkable functional group include a hydroxyl group, a carboxyl group, an isocyanate group, a glycidyl group, an amine group, an alkoxysilyl group, or a vinyl group, and generally, a hydroxyl group or a carboxyl group may be used.

[0025] The crosslinkable monomer may be a copolymerizable monomer having a hydroxyl group. The copolymerizable monomer having a hydroxyl group may be, but is not limited to, a hydroxyalkyl (meth)acrylate such as 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 6-hydroxyhexyl (meth)acrylate, or 8-hydroxyoctyl (meth)acrylate, or a hydroxyalkylene glycol (meth)acrylate such as 2-hydroxyethylene glycol (meth)acrylate or 2-hydroxypropylene glycol (meth)acrylate. Among the above monomers, a hydroxyalkyl acrylate or a hydroxyalkylene glycol acrylate may be used in consideration of reactivity with other monomers forming blocks and ease of adjustment of the glass transition temperature.

[0026] The crosslinking monomer may be included in an amount of, for example, 1 to 30 parts by weight or 1 to 20 parts by weight per 100 parts by weight of the adhesive resin. Within such a range, the adhesive can realize an appropriate crosslinked structure.

[0027] The adhesive resin may further contain other optional comonomers, for example, for adjusting appropriate physical properties, etc., as necessary. Examples of the comonomers include alkylene oxide group-containing monomers such as NVP (N-vinylpyrrolidone), alkoxy alkylene glycol (meth) acrylates, alkoxy dialkylene glycol (meth) acrylates, alkoxy trialkylene glycol (meth) acrylates, alkoxy tetraalkylene glycol (meth) acrylates, alkoxy polyethylene glycol (meth) acrylates, phenoxy alkylene glycol (meth) acrylates, phenoxy dialkylene glycol (meth) acrylates, phenoxy trialkylene glycol (meth) acrylates, phenoxy tetraalkylene glycol (meth) acrylates, or phenoxy polyalkylene glycol (meth) acrylates, styrene-based monomers such as styrene or methylstyrene, glycidyl group-containing monomers such as glycidyl (meth) acrylate, or vinyl carboxylates such as vinyl acetate, but are not limited thereto. One or more suitable types of such comonomers may be selected as necessary and contained in the polymer. For example, such comonomers may be contained in the polymer in a ratio of 20 parts by weight or less, or 0.1 to 15 parts by weight, based on the total weight of other compounds used as polymerized units in the polymer.

[0028] The weight average molecular weight of the adhesive resin may be, for example, within the range of 500,000 to 1,500,000. The weight average molecular weight means a value converted to standard polystyrene measured by GPC (Gel Permeation Chromatograph). The weight average molecular weight of the adhesive resin may be specifically 600,000 or more, 700,000 or more, or 800,000 or more, and may be 1,400,000 or less, 1,300,000 or less, 1,200,000 or less, 1,100,000 or less, or 1,000,000 or less.

[0029] The adhesive resin may have a viscosity measured at a solid content of 28% within a range of about 1000 cps to 2000 cps. Specifically, the viscosity may be 1100 cps or more, 1200 cps or more, 1300 cps or more, 1400 cps or more, 1500 cps or more, or 1600 cps or more, or 1900 cps or less, 1800 cps or less, or 1700 cps or less.

[0030] The curing agent (crosslinking agent) may be included in an amount of, for example, 0.1 to 0.3 parts by weight per 100 parts by weight of the solid content of the adhesive resin. The type of curing agent is not particularly limited, and may be selected in consideration of the type of crosslinkable functional group contained in the adhesive resin. As the curing agent, for example, a general crosslinking agent such as an isocyanate crosslinking agent, an epoxy crosslinking agent, an aziridine crosslinking agent, and a metal chelate crosslinking agent may be used. According to one embodiment of the present application, an isocyanate crosslinking agent may be used as the curing agent.

[0031] The thickness of the first pressure-sensitive adhesive layer may be appropriately selected within a range that does not impair the object of the present application. For example, the thickness of the first pressure-sensitive adhesive layer may be within a range of 20 μm to 200 μm.

[0032] The first adhesive layer may have an adhesive strength to glass of 1,000 gf / in or more at a peel speed of 0.3 mpm (mm / min). Specifically, the adhesive strength may be 1,500 gf / in or more or 2,000 gf / in or more. The upper limit of the adhesive strength may be, for example, 4,000 gf / in or less. When the adhesive strength of the first adhesive layer to glass is within the above range, it may be advantageous in terms of durability after bonding to an OLED panel.

[0033] The method of forming the first adhesive layer on the retardation substrate layer is not particularly limited. In one example, an adhesive composition for forming the first adhesive layer is applied onto a known release film (a separate structure from the release film 30 described later), and then dried, and the adhesive composition is laminated with the retardation substrate layer and wound into a roll. The drying may be performed at a drying temperature of 50°C to 140°C (the length of the drying oven is about 20m to 50m) and at a line speed of 5m / min to 25m / min. The release film may be peeled off and removed before attaching the release film 30 described later to the first adhesive layer.

[0034] FIG. 2 exemplarily illustrates the structure of the second back plate film further including a protective film 20 and a release film 30 in addition to the retardation substrate layer 10a and the first pressure-sensitive adhesive layer 10b.

[0035] As shown in Fig. 2, the backplate film may further include a protective film 20 present on the side of the retardation substrate layer 10a. The protective film may serve to protect the retardation substrate layer during transportation or processing of the backplate film. When the backplate film is applied to an organic light emitting display, the protective film may be removed.

[0036] The protective film 20 may include a first base film 20a and a second adhesive layer 20b formed on one side of the first base film 20a. In this case, the protective film may be attached to the retardation base layer via the second adhesive layer.

[0037] The thicknesses of the first base film and the second pressure-sensitive adhesive layer may be appropriately selected within a range that does not impair the object of the present application. In one example, the thickness of the first base film included in the protective film may be within a range of 20 μm to 200 μm. In one example, the thickness of the second pressure-sensitive adhesive layer included in the protective film may be within a range of 10 μm to 200 μm.

[0038] In one example, the first base film may be a PET (polyethylene terephthalate) film.In one example, the second adhesive layer may be an acrylic adhesive.

[0039] The first base film and the second adhesive layer may each independently have antistatic properties. In one example, the backplate film may include an antistatic layer formed on one side of the first base film. In this case, the antistatic layer may be formed on the opposite side of the first base film to the side on which the second adhesive layer is formed. In one example, the backplate film may further include an antistatic layer formed on one side of the second adhesive layer. In this case, the antistatic layer may be formed on the opposite side of the second adhesive layer to the side on which the first base film is formed. The surface resistance of the antistatic layer may be, for example, 10 4 Ω / square~10 11 The surface resistance of the antistatic layer may be in the range of 10 4 Ω / square or more, 10 5 Ω / square or more, 10 6 Ω / square or more, 10 7 Ω / square or more or 10 9 It may be Ω / square or more, and 10 11 Ω / square or less or 10 10 It may be less than or equal to Ω / square.

[0040] As shown in FIG. 2, the backplate film may further include a release film 30 present on the side of the first pressure-sensitive adhesive layer 10b.

[0041] The release film 30 may include a second base film 30b and a silicone layer 30a formed on one side of the second base film. The release film may serve to protect the first adhesive layer. When the backplate film is applied to an organic light-emitting display, the release film may be removed.

[0042] The release film 30 may be arranged such that the silicon layer 30a is closer to the first adhesive layer 10b than the second base film 30b. The retardation base layer 10a and the release film 30 may be attached via the first adhesive layer 10b.

[0043] In one example, the second substrate film may be a polyethylene terephthalate (PET) film.

[0044] The second base film may have antistatic properties. In one example, the backplate film may include an antistatic layer formed on one or both sides of the second base film. In one example, the release film may include a silicone layer, an antistatic layer, a second base film, and an antistatic layer in that order. The surface resistance of the antistatic layer may be, for example, 10 4 Ω / square~10 11 The surface resistance of the antistatic layer may be in the range of 10 4 Ω / square or more, 10 5 Ω / square or more, 10 6 Ω / square or more, 10 7 Ω / square or more or 10 9 It may be Ω / square or more, and 10 11 Ω / square or less or 10 10 It may be less than or equal to Ω / square.

[0045] The thickness of the second base film may be appropriately selected within a range that does not impair the object of the present application. In one example, the thickness of the second base film may be within a range of 20 μm to 200 μm.

[0046] The silicon layer may be formed by coating the silicon layer-forming composition on the second substrate film and then drying the composition. The thickness of the coating of the silicon layer-forming composition may be within a range of, for example, 10 nm to 2000 nm.

[0047] The peel strength and line resistance between the layers of the backplate film may be appropriately selected within a range that does not impair the object of the present application.

[0048] In one example, the peel force measured while peeling off the protective film 20 after it is attached to the retardation base layer 10a may be in the range of 1 gf / in to 9 gf / in. In one example, the peel force measured while peeling off the first adhesive layer 10b of the first back plate film 10 after it is attached to glass may be in the range of 1,100 gf / in to 3,000 gf / in. In one example, the peel force measured while peeling off the release film 30 after it is attached to the first adhesive layer 10b of the first back plate film 10 may be in the range of 1 gf / in to 7 gf / in.

[0049] In one example, the line resistance measured on the base film 20a side of the protective film 20 is 10 4 Ω~10 9 Ohms, 10 5 Ω~10 9 Ohms, 10 6 Ω~10 9 Ohms, or 10 7 Ω~10 9 In one example, the linear resistance measured on the retardation substrate layer 10a surface of the first back plate film 10 may be in the range of 10 4 Ω~10 9 Ohms, 10 5 Ω~10 9 Ohms, 10 6 Ω~10 9 Ohms, 10 7 Ω~10 9 Ohms or 10 8 Ω~10 9 In one example, the line resistance measured on the first pressure-sensitive adhesive layer 10b side of the first back plate film 10 may be in the range of 10 11 Ω~10 16 Ohms, 10 11 Ω~10 15 Ohms, 10 11 Ω~10 14 Ohms or 10 13 Ω~10 14In one example, the line resistance measured on the silicon layer 30a side of the release film 30 may be in the range of 10 4 Ω~10 9 Ohms, 10 5 Ω~10 9 Ohms or 10 6 Ω~10 8 In one example, the linear resistance measured on the surface of the second base film 30b of the release film 30 is in the range of 10 4 Ω~10 9 Ohms, 10 4 Ω~10 8 Ohms, 10 5 Ω~10 7 It may be in the Ω range.

[0050] The present application further relates to uses of said backplate film.

[0051] In one example, the present application relates to an organic light emitting display including the backplate film and an OLED (organic light emitting diode) panel. The contents related to the backplate may be similarly applied to the contents described above. The backplate film may be applied to the OLED panel in a state where the protective film and the release film are removed, for example, in a state where only the retardation substrate layer and the first adhesive layer are included.

[0052] The OLED panel may be a flexible OLED panel including a plastic (polymer) substrate. The backplate film may be attached to the polymer substrate of the OLED panel via the first adhesive layer. In a flexible OLED panel production line, a polymer substrate, for example, a PI substrate, is prepared on a carrier glass, and an OLED panel that has been subjected to processes such as organic deposition and in-capping may undergo a laser lift-off (LLO) process. Since the polymer substrate from which the carrier glass has been removed through LLO is thin, if it is left as is, a problem of rolling up may occur. The backplate film may fix the polymer substrate so that it does not roll up. After the backplate film is attached to the polymer substrate, a process of attaching a touch sensor, a polarizing plate, etc. may be performed.

[0053] In one example, the present application relates to a mobile phone including the backplate film. That is, the organic light emitting display may be a mobile phone. FIG. 3 exemplarily illustrates the mobile phone. The mobile phone may sequentially include a cover window 100, a polarizer 200, a touch sensor 300, an OLED panel 400, a backplate film 500, and a camera 600. The above-mentioned contents may be similarly applied to the backplate. The backplate film may be applied to a mobile phone in a state where the protective film and the release film are removed, for example, in a state where only the retardation substrate layer and the first adhesive layer are included. The first adhesive layer of the backplate film may be in contact with the OLED panel. That is, the backplate film may be attached to the OLED panel via the first adhesive layer.

[0054] In one example, the mobile phone may further include a metal layer formed on one side of the retardation substrate layer of the backplate film. The metal layer may be attached to the retardation substrate layer via an adhesive layer. The metal layer may perform a heat dissipation function to diffuse heat generated in the display.

[0055] The camera may be a front camera of an OLED panel. The OLED panel does not need to have a front camera area punched out. Therefore, a display may be implemented in the front camera area of ​​the mobile phone.

[0056] The cover window, the polarizing plate, the touch sensor, the OLED (organic light emitting diode) panel, and the camera may be appropriately selected from those known in the art within the scope of the present application. Effect of the Invention

[0057] The present application provides a backplate film for an under-display camera that enables the front camera of a mobile phone to capture an object without image distortion. [Brief description of the drawings]

[0058] [Figure 1] 1 illustrates an exemplary backplate film of the present application. [Diagram 2] 1 illustrates an exemplary backplate film of the present application. [Diagram 3] 1 illustrates an exemplary structure of a mobile phone of the present application. [Figure 4] Photographs taken to evaluate the occurrence of image distortion. [Diagram 5] Photographs taken to evaluate the occurrence of image distortion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0059] The present application will be described in detail below through examples according to the present application and comparative examples not according to the present application, but the scope of the present application is not limited to the following examples.

[0060] Measurement example 1. Adhesive strength measurement The adhesive strength of the adhesive layer was measured using a Texture analyzer (Stable Micro Systems) at an angle of 180° and a peeling speed of 300 mm / min. The adhesive layer formed on the release film was cut into a size of 1 inch x 6 inches (horizontal x vertical), and then attached to a glass substrate by rolling it back and forth once with a 2 kg rubber roller, and then the adhesive strength was measured.

[0061] Measurement example 2. Demolding force measurement The release force of the adhesive layer was measured using a Texture Analyzer (Stable Micro Systems) at an angle of 180° and a peeling speed of 300 mm / min. The adhesive layer formed on the release film was cut into a size of 1 inch x 6 inches (horizontal x vertical), attached to a double-sided tape, and then the measurement was performed.

[0062] Measurement example 3. Optical property measurement A sample measuring 3 cm x 3 cm was prepared, and the haze and transmittance of the base layer with the adhesive layer attached after peeling off the release film was measured using a Hazemeter (Nippon Denshoku COH400) under a D65 light source.

[0063] Measurement example 4. Phase difference measurement A sample with a size of 3 cm x 3 cm was prepared, and the release film was peeled off, and the in-plane retardation (R0) value and thickness direction retardation (Rth) value of the substrate layer for light with a wavelength of 550 nm were measured using an AXO-SCAN (AXO-METRICS) device.

[0064] Example 1. As a retardation substrate layer, an SRF (Super retardation film) substrate layer (TA-044, Toyobo Co., Ltd.) having a thickness of 80 μm was prepared. The haze of the SRF substrate layer was 0.89%, and the transmittance was 93.13%. The SRF substrate layer had an in-plane retardation (R0) of 7,418 nm and a thickness direction retardation (Rth) of −8,110 nm. One side of the SRF substrate was coated with an antistatic agent using a Mayer bar #3, and then dried in a Matisse oven at a temperature of 100° C. for 100 seconds to form an antistatic layer. The surface resistance of the antistatic layer was 10 9 The sheet resistance was measured using a resistance meter (MCP-HT800 manufactured by Nittoseiko Analytech Co., Ltd.).

[0065] A first mixture liquid with a solid content of 19% was prepared by mixing 100 parts by weight (solid content) of adhesive resin (SYS-3355, SAN-EI), 0.25 parts by weight of hardener (DR-7030HD, SAN-EI), 3 parts by weight of retarder (acetylacetone) and toluene solvent. A second mixture liquid with a solid content of 21% was prepared by mixing adhesive resin (SYS-3355, SAN-EI) and toluene. The adhesive resin (SYS-3355, SAN-EI) contains 75 parts by weight of 2-EHA (2-Ethylhexyl acrylate), 10 parts by weight of MMA (Methyl methacrylate), 5 parts by weight of NVP (N-vinylpyrrolidone) and 10 parts by weight of 2-HEA (2-Hydroxyethyl acrylate) as polymerization units. The curing agent (DR-7030HD, San-ei) contains 30 parts by weight of H12MDI (1-isocyanato-4-[(4-isocyanatocyclohexyl)methyl]cyclohexan) and 70 parts by weight of IPDI (5-isocyanato-1-(isocyanatomehtyl)-1,3,3-trimethylcyclohexane). The weight average molecular weight of the adhesive resin is 890,000, and the viscosity of 28% solid content at 25°C is 1650cp.

[0066] The first and second blended liquids were mixed to prepare a pressure-sensitive adhesive composition. The pressure-sensitive adhesive composition was applied to the release layer (Si layer) of a release film using a slit die and a nip die, and then dried at a speed of 15 m / min at temperatures of 60°C, 90°C, 110°C, 120°C, 120°C, and 120°C in an oven consisting of six sections (5 m per section), to prepare a first pressure-sensitive adhesive layer having a thickness of 15 μm. The dried first pressure-sensitive adhesive layer and the retardation substrate layer were laminated, and then wound into a roll to prepare a first backplate film. The first pressure-sensitive adhesive layer had an adhesive strength of 2039 gf / in measured in Measurement Example 1 and a release strength of 4.5 gf / in measured in Measurement Example 2.

[0067] An antistatic layer is formed by coating an antistatic agent on one side of a PET film (first base film) having a thickness of 75 μm using microgravure. The surface resistance of the antistatic layer is 10 9 The electrical conductivity was Ω / square. An acrylic adhesive (second adhesive layer) having a thickness of 15 μm was coated on the opposite side of the PET film, and then oven-coated. The release layer (Si layer) of a release film was attached to the acrylic adhesive surface, rolled up, and aged for 2 days to produce a protective film 20.

[0068] An RF02ASW product manufactured by SKC HTM was prepared as the release film 30. The release film includes a PET film (second base film) and a silicone layer formed on one side of the PET film.

[0069] The retardation substrate layer and the release film were attached via the first adhesive layer formed on the retardation substrate layer. At this time, the silicone layer of the release film was attached so as to contact the first adhesive layer. The protective film was attached to the retardation substrate layer via the second adhesive layer of the protective film to produce a backplate film having the structure of FIG. 2.

[0070] The physical properties of the back plate film are shown in Table 1 below. With regard to the peel force, PF is a value measured while peeling off the protective film 20 that has been attached to the retardation substrate layer 10a, Adhesion is a value measured while peeling off the first adhesive layer 10b of the first back plate film 10 that has been attached to glass, and LF is a value measured while peeling off the release film 30 that has been attached to the first adhesive layer 10b of the first back plate film 10. The peel force was measured using a texture analyzer (Stable Micro Systems) at an angle of 180° and a peel speed of 0.3 mpm. In the line resistance, the PF side is a value measured on the substrate film 20a side of the protective film 20, the Film side is a value measured on the retardation substrate layer 10a side of the first back plate film 10, the PSA side is a value measured on the first adhesive layer 10b side of the first back plate film 10, the LF(Si) side is a value measured on the silicon layer 30a side of the release film 30, and the LF side is a value measured on the second substrate film 30b side of the release film 30. The line resistance was measured using a resistance meter (MCP-HT800 by Nittoseiko Analytech Co., Ltd.).

[0071] [Table 1]

[0072] Comparative Example 1 A back plate film was produced in the same manner as in Example 1, except that the retardation substrate layer and the first pressure-sensitive adhesive layer were changed as follows.

[0073] A PET substrate (T914J75, Mitsubishi) having a thickness of 50 μm was prepared as a retardation substrate layer. The haze of the PET substrate was 1.5% and the transmittance was 90.3%. The PET substrate had an in-plane retardation (R0) of 2,509 nm and a thickness direction retardation (Rth) of −3,297 nm. One side of the PET substrate was coated with an antistatic agent using a Mayer bar #3, and then dried in a Matisse oven at a temperature of 100° C. for 100 seconds to form an antistatic layer. The surface resistance of the antistatic layer was 10 9 It was Ω / square.

[0074] Except for changing the thickness of the first pressure-sensitive adhesive layer to 10 μm, a first pressure-sensitive adhesive layer was formed in the same manner as in Example 1. The first pressure-sensitive adhesive layer had an adhesive strength of 1909 gf / in measured in Measurement Example 1 and a release strength of 1.2 gf / in measured in Measurement Example 2.

[0075] Evaluation example 1. Image distortion evaluation The protective film and the release film were peeled off from the back plate films of Example 1 and Comparative Example 1. A sample in which a back plate film including a retardation substrate layer and a first adhesive layer was attached to a polarizer was placed in front of a camera, and an image was taken to evaluate whether the front camera could capture an object without image distortion. The polarizer was a PVA (polyvinyl alcohol) polarizer dyed with iodine as an absorption-type linear polarizer. Figures 4 and 5 show the photographs taken, respectively. When the back plate film of Example 1 was applied (A), the front camera was able to capture an object without image distortion, but when the back plate film of Comparative Example 1 (B) was applied, distortion of the object was found. [Explanation of symbols]

[0076] 10: First back plate film 10a: Retardation base material layer 10b: First adhesive layer 20: Protective film 20a: First base film 20b: second adhesive layer 30: Release film 30a: Silicon layer 30b: second base film 100: Cover window 200: Polarizing plate 300: Touch sensor 400:OLED panel 500: Backplate film 600: Camera

Claims

1. A retardation substrate layer; A first pressure-sensitive adhesive layer formed on one surface of the retardation substrate layer, The absolute value of the in-plane retardation (R0) value of the retardation base layer calculated by the following formula 1 is 6,000 nm or more, and the absolute value of the thickness direction retardation (Rth) value calculated by the following formula 2 is 6,000 nm or more, [Formula 1] R0=(nx-ny)×d [Formula 2] Rth=[(nx+ny) / 2-nz]×d In Formula 1 and Formula 2, nx, ny, and nz are the refractive indices of the retardation substrate layer in the x-axis direction, the y-axis direction, and the z-axis direction for light with a wavelength of 550 nm, respectively; d is the thickness (nm) of the retardation substrate layer of the backplate film.

2. The backplate film according to claim 1 , wherein the absolute value of the in-plane retardation (R0) value of the retardation substrate layer is 10,000 nm or less.

3. The backplate film according to claim 1 , wherein the absolute value of the thickness direction retardation (Rth) value of the retardation substrate layer is 10,000 nm or less.

4. The backplate film according to claim 1 , wherein the thickness of the retardation substrate layer is within a range of 20 μm to 200 μm.

5. An antistatic layer is formed on the surface of the retardation substrate layer on which the first pressure-sensitive adhesive layer is not formed, The surface resistance of the antistatic layer is 10 4 Ω / square to 10 11 The backplate film of claim 1 , wherein the resistance is in the range of Ω / square.

6. The backplate film of claim 1 , wherein the first adhesive layer comprises an acrylic resin and a curing agent, and has a thickness in the range of 20 μm to 200 μm.

7. The backplate film of claim 1 , wherein the first adhesive layer has an adhesive strength to glass at a peel speed of 0.3 mpm in the range of 1000 gf / in to 4000 gf / in.

8. The backplate film according to claim 1 , further comprising a protective film present on the side of the retardation substrate layer.

9. The protective film includes a first base film and a second pressure-sensitive adhesive layer formed on one surface of the first base film, The thickness of the first base film is in the range of 20 μm to 200 μm; The backplate film of claim 8 , wherein the thickness of the second adhesive layer is in the range of 10 μm to 200 μm.

10. The backplate film of claim 9 , wherein the first base film is a PET film.

11. The present invention further includes an antistatic layer formed on at least one surface of the first base film and the second pressure-sensitive adhesive layer, The surface resistance of the antistatic layer is 10 4 Ω / square to 10 11 The backplate film of claim 9 , wherein the resistance is in the range of Ω / square.

12. The backplate film according to claim 8 , further comprising a release film present on the first adhesive layer side.

13. The backplate film of claim 12 , wherein the release film comprises a second base film and a silicone layer formed on one side of the second base film.

14. The backplate film of claim 13 , wherein the second base film is a PET film.

15. An antistatic layer is formed on one or both sides of a second substrate film, The surface resistance of the antistatic layer is 10 4 Ω / square to 10 11 The backplate film of claim 13 , wherein the resistance is in the range of Ω / square.

16. An organic light-emitting display, comprising the backplate film of claim 1 and an OLED panel.

17. 17. The organic light-emitting display of claim 16, wherein the first adhesive layer of the backplate film contacts the OLED panel.

18. A mobile phone, comprising in sequence a cover window, a polarizer, a touch sensor, an OLED panel, the backplate film of claim 1, and a camera.

19. 20. The mobile phone of claim 18, wherein the OLED panel does not have a front camera area punched out.

Citation Information

Patent Citations

  • Display panel and display device

    CN113593414A

  • Layered optical product, optical display device, and method for manufacturing optical display device

    JP2009157363A

  • Antistatic pressure-sensitive adhesive sheet and optical film

    JP2014189787A

  • Laminated polyethylene terephthalate film

    JP2017064969A

  • Optical laminate and image display device including the same

    JP2020086429A