Phase change memory cell having pillar bottom electrode with improved thermal insulation - Patents.com

By employing metal pillars and internal spacers with smaller dimensions than lithographic limits, the PCM devices experience reduced programming currents and heat loss, improving their efficiency.

JP2024539551AActive Publication Date: 2024-10-29INTERNATIONAL BUSINESS MACHINE CORPORATION
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024518439
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-19
Filing Date
2022-10-04
Publication Date
2024-10-29
Estimated Expiration
2042-10-04

AI Technical Summary

Technical Problem

PCM devices face high programming currents and significant heat loss during the reset step due to the large contact area between the heater element and the phase change element, with most heat being conducted away through the thermally conductive bottom electrode.

Method used

The integration of metal pillars with smaller lateral dimensions than lithographic limits and internal spacers surrounding them, along with a stack of alternating conductor layers, reduces the contact area and heat loss in PCM devices.

Benefits of technology

This configuration decreases the programming current required for phase changes and minimizes heat loss, enhancing the efficiency of PCM devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024539551000001_ABST
    Figure 2024539551000001_ABST
Patent Text Reader

Abstract

A phase change memory cell having a pillar bottom electrode with improved thermal insulation. A phase change memory device includes a bottom electrode; a stack of alternating conductive layers in direct contact with a top surface of the bottom electrode; a metal pillar in direct contact with a top surface of the stack; a phase change material element in direct contact with a top surface of the metal pillar; and a top electrode on the phase change material element, wherein a lateral dimension of the metal pillar is smaller than a lateral dimension of the stack.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE This disclosure relates generally to Phase Change Memory (PCM) cells. [Background technology]

[0002] PCM is a new non-volatile (NV) random access memory (RAM) that offers several advantages over existing non-volatile memories (NVM). It has potential for both traditional memory applications and neuromorphic computing.

[0003] One of the major considerations for PCM devices is their programming current, which can be very large during the power-hungry reset step. Reducing the contact area of ​​the heater element and the phase change element can help reduce the set / reset current.

[0004] Furthermore, most of the heat is generated at the interface of the patterned contact and the phase change layer due to current confinement. Most of the heat generated in the cell ends up heating the nearby dielectric and metal electrodes. Thermal energy is usually lost through the bottom electrode because it is the most thermally conductive path from the interface.

[0005] Therefore, novel bottom electrode integration approaches are needed to reduce the programming current as well as the heat losses in PCM devices. Summary of the Invention

[0006] According to one aspect of the invention, there is provided a phase change memory device comprising a bottom electrode; a stack of alternating conductive layers in direct contact with a top surface of the bottom electrode; a metal pillar in direct contact with a top surface of the stack; a phase change material element in direct contact with a top surface of the metal pillar; and a top electrode on the phase change material element, wherein a lateral dimension of the metal pillar is smaller than a lateral dimension of the stack.

[0007] According to another aspect of the present invention, there is provided a method for manufacturing a crossbar-type phase change memory cell, comprising the steps of: providing a bottom electrode disposed on a lower layer; forming a multilayer stack including a plurality of alternating conductive layers; depositing a top metal layer formed of a material different from that of the multilayer stack on the multilayer stack; forming a hard mask pillar on the top metal layer; etching the top metal layer to form a metal pillar; forming an inner spacer surrounding the metal pillar; patterning the multilayer stack using the hard mask pillar; forming a dielectric layer having a height equal to a top surface of the metal pillar; removing the hard mask pillar; and forming a phase change material element on the metal pillar.

[0008] As used herein, "facilitating" an action includes performing an action, making an action easier, assisting in the performance of an action, or having an action performed. Thus, by way of example and not limitation, instructions executing on one processor may facilitate an action performed by instructions executing on a remote processor by transmitting appropriate data or commands that cause or assist in the performance of the action. For the avoidance of doubt, an action is performed by some entity or combination of entities even if an actor facilitates an action by other than performing the action.

[0009] One or more embodiments of the present invention or elements thereof may be implemented in the form of a computer program product including a computer-readable storage medium with computer usable program code for performing the illustrated method steps. Furthermore, one or more embodiments of the present invention or elements thereof may be implemented in the form of a system (or apparatus) including a memory and at least one processor coupled to the memory and operable to perform the illustrated method steps. Furthermore, in another aspect, one or more embodiments of the present invention or elements thereof may be implemented in the form of a means for performing one or more of the method steps described herein; the means may include (i) a hardware module, (ii) a software module stored in a computer-readable storage medium (or multiple such media) and implemented in a hardware processor, or (iii) a combination of (i) and (ii); any of (i)-(iii) may implement certain techniques described herein.

[0010] The techniques of the present invention are capable of providing significant beneficial technical advantages. Some embodiments may not have these potential advantages, and these potential advantages are not necessarily required for all embodiments. For example, one or more embodiments may include Metal pillars with small widths that reduce the programming current required to effect a phase change; lateral dimensions of the metal pillars smaller than the lithographic capabilities configured to achieve low programming currents; an internal spacer surrounding the metal pillar that reduces lateral heat loss of the metal nanopillar; and A stack of alternating conductor layers underneath the metal pillars to reduce downward heat loss may be provided.

[0011] These and other features and advantages of the present invention will become apparent from the following detailed description of illustrative embodiments, which is to be read in connection with the accompanying drawings. [Brief description of the drawings]

[0012] Preferred embodiments of the invention are described in more detail below with reference to the accompanying drawings.

[0013] [Figure 1] 1 is a method of forming a PCM cell according to one or more embodiments of the present invention.

[0014] [Diagram 2] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Diagram 3] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 4] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Diagram 5] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 6] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 7] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 8] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 9] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 10] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 11] 1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention. [Figure 12]1A-1D are cross-sectional views of a PCM at different steps in a manufacturing process in accordance with one or more embodiments of the present invention.

[0015] [Figure 13] 1A-1D are cross-sectional views of a PCM at different steps of a directional etching process in accordance with one or more embodiments of the present invention. [Figure 14] 1A-1D are cross-sectional views of a PCM at different steps of a directional etching process in accordance with one or more embodiments of the present invention.

[0016] [Figure 15] FIG. 2 is a diagram of a PCM cell stack in accordance with one or more embodiments of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] According to embodiments of the present invention, methods and structures are provided for forming a phase change memory PCM cell having a metal pillar / heater on a multi-layer metal electrode (i.e., pillar bottom electrode). According to some embodiments, the width dimension of the metal pillar is smaller than the current lithographic limit. According to some aspects, the metal pillar having a width dimension smaller than the lithographic limit is a metal nanopillar. According to some embodiments, a self-aligned internal spacer surrounds the metal nanopillar / heater, and the self-aligned internal spacer is a thermal and electrical insulator.

[0018] The present application will now be described in more detail by reference to the following discussion and drawings accompanying this application. It should be noted that the drawings in this application are provided for illustrative purposes only, and therefore the drawings are not to scale. It should also be noted that like and corresponding elements are referred to by like reference numerals.

[0019] In the following description, numerous specific details are set forth, such as particular structures, components, materials, dimensions, processing steps, and techniques, to provide an understanding of various embodiments of the present application. However, those skilled in the art will understand that various embodiments of the present application can be practiced without these specific details. In other instances, well-known structures or processing steps have not been described in detail to avoid obscuring the present application.

[0020] The fabrication of semiconductor devices involves various steps of device patterning processes. For example, the fabrication of semiconductor chips may begin with multiple device patterns, e.g., generated by CAD (Computer Aided Design), followed by replicating these device patterns in a substrate. The replication process may involve the use of various exposure techniques and various subtractive (etching) and / or additive (deposition) material processing procedures. For example, in a photolithography process, a layer of photoresist material may first be applied on top of a substrate and then selectively exposed according to a predetermined device pattern or patterns. Portions of the photoresist exposed to light or other ionizing radiation (e.g., ultraviolet light, electron beam, x-rays, etc.) may undergo some changes in solubility in certain solutions. The photoresist may then be developed in a developer, which may remove unirradiated (in the case of a negative resist) or irradiated (in the case of a positive resist) portions of the resist layer to create a photoresist pattern or photomask. The photoresist pattern or photomask may then be copied or transferred to the substrate beneath the photoresist pattern.

[0021] Numerous techniques are used by those skilled in the art to remove material at various stages in the fabrication of semiconductor structures. As used herein, these processes are collectively referred to as "etching." For example, etching includes wet etching, dry etching, chemical oxide removal (COR) etching, and reactive ion etching (RIE) techniques, all of which are known techniques for removing selected materials when forming semiconductor structures. Standard Clean 1 (SC1) contains a strong base, typically ammonium hydroxide, and hydrogen peroxide. SC2 contains a strong acid, such as hydrochloric acid and hydrogen peroxide. The techniques and applications of etching are well understood by those skilled in the art, and therefore a more detailed description of such processes is not presented herein.

[0022] While the overall fabrication method and structures formed thereby are novel, certain individual processing steps required to carry out the method may utilize conventional semiconductor fabrication techniques and conventional semiconductor fabrication tools, which techniques and tools will already be familiar to those of skill in the relevant art given the teachings herein. It is emphasized that while several individual processing steps are described herein, these steps are merely exemplary, and that those of skill in the art may be familiar with several equally suitable alternatives that may be applicable.

[0023] It should be understood that the various layers and / or regions illustrated in the accompanying figures are not necessarily drawn to scale. Additionally, one or more semiconductor layers of a type commonly used in such integrated circuit devices may not be explicitly shown in a given figure for ease of illustration. This is not intended to imply that the not explicitly shown semiconductor layers are omitted in the actual integrated circuit device.

[0024] Referring to FIG. 12, according to some aspects, in a crossbar-type phase change material (PCM) array with top and bottom electrodes, each PCM cell 1200 has a mushroom-shaped PCM element 1201 connected to a top electrode 1202 and a metal nanopillar 1203 with small (e.g., smaller than the lithographic limit) dimensions. According to some embodiments, the metal nanopillar 1203 is a heater. The small contact area of ​​the metal nanopillar with the mushroom-shaped PCM element reduces the total amount of heat required for phase change, which in turn reduces the current required for each set or reset operation. According to some aspects, an internal spacer 1204 surrounding the metal nanopillar can act as a thermal insulation layer to prevent heat from migrating away from the contact area towards the surrounding material.

[0025] FIG. 1 illustrates a method 100 for fabricating a crossbar-type PCM array having top and bottom electrodes in accordance with one or more embodiments of the present invention.

[0026] According to some embodiments of the present invention, and with reference to Figure 1, a method 100 for forming a phase change memory (PCM) cell having a bottom electrode (pillar type) on a multi-layer metal electrode comprises providing an underlayer in step 101, and forming an interlevel dielectric (ILD) disposed on the underlayer, and a bottom electrode disposed in the ILD and on the underlayer in step 102. It should be understood that the underlayer may comprise a semiconductor substrate, which itself may include other devices, such as transistors, isolation structures, contacts, etc.

[0027] According to some embodiments, the electrodes (e.g., top and bottom electrodes) of the PCM cell may be formed from TiN, TaN, tungsten (W), aluminum (Al), Ti, Ta, titanium silicon nitride (TiSiN), titanium aluminum nitride (TiAlN), tungsten nitride (WN), and other suitable metals.

[0028] According to some embodiments, a multi-layer stack is formed in step 103. The multi-layer stack can include a titanium nitride (TiN) / tantalum nitride (TaN) multi-layer stack. According to some embodiments, the first TiN layer can have a greater thickness than any of the other multi-layers.

[0029] According to some embodiments, a top metal layer is deposited in step 104, the top metal layer being different from the TiN or TaN layer. Optionally, the bottom TiN layer can have the same thickness as the subsequent TiN layer.

[0030] According to an example embodiment, hardmask pillars may be formed on the top metal layer in step 105. According to some embodiments, the top metal layer may be selectively etched using the hardmask pillars as a mask.

[0031] According to some embodiments, an isotropic (lateral) etch of the top metal layer is performed in step 106 to remove the edges of the top metal layer and form metal nanopillars below the hard mask pillars. According to some embodiments, the isotropic etch process can be selective to TaN and TiN, so that the multi-layer stack is not damaged.

[0032] According to exemplary embodiments, the dimensions of the metal nanopillars can exceed (i.e., be smaller than) those that can be formed by lithography, thereby reducing the contact area with the phase change material on top and reducing the total amount of heat required for the phase change, which in turn can reduce the current required for each set or reset operation.

[0033] According to some embodiments, in step 107, a dielectric liner is deposited and etched back using the hardmask pillars as a mask to form inner spacers.

[0034] According to some embodiments, in step 108, a directional reactive ion etch (RIE) of the multi-layer stack is performed, stopping on the bottom electrode.

[0035] According to some embodiments, in step 109, a dielectric layer (eg, oxide) is deposited and a chemical mechanical polish (CMP) is performed, stopping on top of the metal nanopillars.

[0036] According to some embodiments, in step 110, a phase change material, such as Ge2Se2Te5 (GST), is deposited.

[0037] According to some embodiments, in step 111, a TiN hard mask is formed and used to pattern the phase change material.

[0038] According to some embodiments, in step 112, an encapsulation layer such as SiN is deposited, a second dielectric layer is deposited, and CMP is performed.

[0039] According to some embodiments, vias are formed in the encapsulation layer and the second dielectric layer to expose the hard mask and metallized to form the top electrode and top electrode contact in step 113. The width dimension of the metal pillars can be smaller than the lithographic capabilities / limitations, resulting in a reduced contact area with the top phase change material, which reduces the programming current.

[0040] 2-12 are cross-sectional views of the PCM of FIG. 1 at different steps in the manufacturing process according to one or more embodiments of the present invention.

[0041] According to some embodiments of the present invention, and with reference to FIG. 2, an underlayer 201 is provided. The underlayer 201 may include a semiconductor substrate, which itself may include other devices, such as transistors, isolation structures, contacts, etc. According to some embodiments, an ILD 202 is deposited on the underlayer 201, and a bottom electrode 203 is disposed on the underlayer 201 and within the ILD 202. For example, the ILD 202 may be patterned to form an opening therein to expose the underlayer 201, and a metal material may be deposited by metallization. Excess portions of the metal material may be removed by CMP to form the bottom electrode 203.

[0042] According to some embodiments, the bottom electrode 203 may be formed from TiN, TaN, W, Al, Ti, Ta, TiSiN, TiAlN, WN, and other suitable metals.

[0043] According to some embodiments, and with reference to FIG. 3, the multi-layer stack 300 can comprise alternating layers of TiN 301a, 301b, 301c, and TaN 302a, 302b, 302c. According to some embodiments, the bottom TiN layer 301a of the multi-layer stack 300 can have a thickness greater than the combined thickness of the remaining layers of TiN and TaN. According to some aspects, the bottom TiN layer 301a can have the same thickness as the other TiN layers in the multi-layer stack 300. It should be understood that any number of layers can be formed. According to some aspects, a top metal layer 303 is deposited, which is formed of a material different from the TiN or TaN layers.

[0044] According to some embodiments, and with reference to Figure 4, hardmask pillars 401 may be formed on the top metal layer 303. According to some embodiments, the top metal layer 303 may be etched selectively to the hardmask pillars 401.

[0045] According to some embodiments, and with reference to Figure 5, an isotropic (lateral) etch of the top metal layer is performed to remove the ends of the top metal layer and form metal nanopillars 1203 below the hard mask pillars 401. According to some embodiments, the isotropic etch process can be selective to TaN or TiN.

[0046] According to an exemplary embodiment, the dimensions of the metal nanopillars 1203 can be smaller than can be formed by lithography, resulting in a smaller contact area with the phase change material on top, reducing the total amount of heat required for the phase change, which in turn reduces the current required for each set or reset operation.

[0047] According to some embodiments, and with reference to Figure 6, a dielectric liner (not shown) is deposited and etched back using the hard mask pillars 401 as a mask to form inner spacers 1204 around the metal nanopillars 1203. The inner spacers 1204 may be formed from materials including, but not limited to, oxide materials such as silicon nitride (SixNy), silicon oxynitride (SiON), and / or silicon carbide nitride (SiCN), and / or silicon oxide (SiOx).

[0048] According to some embodiments, and with reference to FIG. 7, a directional RIE of the multi-layer stack is performed, stopping at the bottom electrode 203, to form a patterned multi-layer stack 701 including patterned layers of TiN, e.g., 702, and TaN, e.g., 703.

[0049] According to some embodiments, and with reference to FIG. 8, a dielectric layer 801 (eg, oxide) is deposited and a chemical mechanical polishing (CMP) is performed, stopping on top of the metal nanopillars 1203 .

[0050] According to some embodiments, and with reference to Figure 9, a PCM 901, such as Ge2Se2Te5 (GST), is deposited on the dielectric layer 801. The PCM 901 may be formed, for example, from a Ge-Sb-Te (germanium-antimony-tellurium or "GST", e.g., Ge2Sb2Te5) alloy. Other suitable materials for PCM901 include Si-Sb-Te (silicon-antimony-tellurium) alloys, Ga-Sb-Te (gallium-antimony-tellurium) alloys, Ge-Bi-Te (germanium-bismuth-tellurium) alloys, In-Te (indium-tellurium) alloys, As-Sb-Te (arsenic-antimony-tellurium) alloys, Ag-In-Sb-Te (silver-indium-antimony-tellurium) alloys, Ge-In-Sb-Te alloys, Ge-Sb alloys, Sb-Te alloys, Si-Sb alloys, and combinations thereof. In some embodiments, PCM901 can further include nitrogen, carbon, and / or oxygen. In some embodiments, the PCM 901 can be doped with a dielectric material including, but not limited to, aluminum oxide (Al2O3), silicon oxide (SiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), zirconium oxide (ZrO2), cerium oxide (CeO2), silicon nitride (SiN), silicon oxynitride (SiON), and the like.

[0051] According to some embodiments, and with reference to FIG. 10, an upper hard mask 1001, for example made from TiN, is formed and used to pattern the PCM 901 to form mushroom-shaped PCM elements 1201.

[0052] According to some embodiments, and with reference to FIG. 11, an encapsulation layer 1101, such as SiN, is deposited, a second dielectric layer 1102 is deposited, and CMP is performed to planarize the second dielectric layer.

[0053] According to some embodiments, and with reference to Figure 12, vias are formed in the encapsulation layer 1101 and the second dielectric layer 1102 to expose the top surface of the top hardmask 1001, and metallization is performed to form the top electrode 1202 and top electrode contact 1205. The dimensions of the metal nanopillars 1203 can be smaller than the lithographic limit, resulting in a small contact area with the mushroom-shaped PCM element 1201 and reduced programming current.

[0054] 12, according to some embodiments, a PCM cell 1200 includes a mushroom-shaped PCM element 1201 connected to a top electrode 1202 and a metal nanopillar 1203 having small (e.g., smaller than the lithographic limit) dimensions. The small contact area between the metal nanopillar and the mushroom-shaped PCM element 1201 reduces the total amount of heat required for a phase change, which in turn reduces the current required for each set or reset operation. According to some embodiments, an internal spacer 1204 surrounding the metal nanopillar can act as a thermal insulation layer to prevent heat from migrating away from the contact area towards the surrounding material.

[0055] 13-14 are cross-sectional views of a PCM cell at different steps of a directional etching process in accordance with one or more embodiments of the present invention.

[0056] According to some embodiments, and with reference to Figure 13, directional RIE of the multi-layer stack can be performed following the formation of the hard mask pillars 401 in step 105. The directional RIE of the multi-layer stack stops at the bottom electrode 203 and forms a patterned multi-layer stack 1301 including patterned layers of TiN, e.g. 702, and TaN, e.g. 703, and a patterned top metal layer 1302.

[0057] According to some embodiments, and with reference to FIG. 14, in step 106, an isotropic (lateral) etch of the patterned top metal layer 1302 is performed to remove the edges of the patterned top metal layer and form metal nanopillars below the hard mask pillars. According to some embodiments, the isotropic etching process can be selective to TaN, TiN, and the materials forming the metal nanopillars. Following the isotropic etch in step 106, a dielectric liner (not shown) is deposited and etched back to form an inner spacer (see, for example, inner spacer 1204 in FIG. 7) around the metal nanopillars 1203. The method can proceed to step 109 where a dielectric layer is deposited and a chemical mechanical polishing (CMP) is performed, which removes the hard mask pillars 401 and stops at the top of the metal nanopillars 1203.

[0058] 15 is a diagram of a PCM cell 1501 in accordance with one or more embodiments of the present invention. The first lateral dimension d0 of the metal nanopillars 1203 is smaller than the lateral dimension of conventional lithography capabilities. The lateral dimension d0 is associated with reduced programming current. The inner spacers 1204 surrounding the metal nanopillars 1203 can act as a thermal insulation layer to reduce or prevent lateral heat loss.

[0059] According to some embodiments, alternating conductive layers (e.g., patterned layers of TiN, e.g., 702, and TaN, e.g., 703) having a second lateral dimension d1 below the metal nanopillars 1203 further reduce downward heat loss.

[0060] According to some embodiments, metal nanopillars 1203 to reduce programming current, internal spacers 1204 to reduce lateral heat loss, and alternating conductor layers (e.g., patterned layers of TiN, e.g., 702, and TaN, e.g., 703) to reduce downward heat loss improve the overall efficiency of the PCM cell 1501.

[0061] General

[0062] According to an embodiment of the present invention, a phase change memory device includes a bottom electrode 203; a stack 701 of alternating conductive layers in direct contact with a top surface of the bottom electrode; a metal pillar 1203 in direct contact with a top surface of the stack; a phase change material element 1201 in direct contact with a top surface of the metal pillar; and a top electrode 1202 on the phase change material element, wherein a lateral dimension of the metal pillar is smaller than a lateral dimension of the stack.

[0063] According to some embodiments, a method 100 for manufacturing a crossbar-type phase change memory cell includes providing a bottom electrode disposed on a lower layer in step 101; forming a multilayer stack including a plurality of alternating conductive layers in step 103; depositing a top metal layer formed of a material different from that of the multilayer stack on the multilayer stack in step 104; forming a hard mask pillar on the top metal layer in step 105; etching the top metal layer to form the metal pillar in step 106; forming an inner spacer surrounding the metal pillar in step 107; patterning the multilayer stack using the hard mask pillar in step 108; forming a dielectric layer having a height equal to a top surface of the metal pillar in step 109; removing the hard mask pillar also in step 109; and forming a phase change material element on the metal pillar in step 111.

[0064] According to some embodiments, forming the phase change material element includes, in step 110, depositing a phase change material; in step 111, forming an upper hard mask on the phase change material; and, in step 111, patterning the phase change material using the upper hard mask to form the phase change material element.

[0065] According to some embodiments, the method includes depositing an encapsulation layer over the phase change material element, at step 112; depositing a second dielectric layer on the encapsulation layer, at step 112; forming vias in the encapsulation layer and the second dielectric layer to expose the top hard mask, at step 113; and performing metallization to form a top electrode and a top electrode contact contacting the top hard mask, at step 113.

[0066] According to some embodiments, forming the inner spacer in step 107 includes depositing a dielectric liner over the multi-layer stack; and etching back the dielectric liner to the width of the hardmask pillars.

[0067] According to some embodiments, patterning the multi-layer stack using hard mask pillars in step 108 is performed prior to etching the top metal layer to form metal pillars in step 106 and forming interior spacers in step 107.

[0068] The terms used herein are for the purpose of describing particular embodiments only and are not intended to be limiting of the invention. As used herein, the singular forms "a", "an" and "the" are intended to include the plural forms as well, unless the context clearly dictates otherwise. It will be further understood that the terms "comprise" and / or "comprising", as used herein, specify the presence of stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups thereof.

[0069] In the following claims, the corresponding structure, material, acts, and equivalents of any means-plus-function or step-plus-function elements are intended to include any structure, material, or act for performing a function in combination with other claimed elements as specifically claimed. The description of various embodiments of the present invention has been presented for illustrative purposes, but is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the scope of the described embodiments. The terms used in this specification are selected to best explain the principles of the embodiments, practical applications, or technical improvements beyond the art found in the market, or to enable other skilled in the art to understand the embodiments disclosed herein.

Claims

1. Lower electrode; a stack of alternating conductive layers in direct contact with a top surface of the bottom electrode; a metal pillar in direct contact with a top surface of the stack; a phase change material element in direct contact with a top surface of the metal pillar; and A top electrode on the phase change material element wherein a lateral dimension of the metal pillar is smaller than a lateral dimension of the stack.

2. an underlayer beneath the bottom electrode; and an interlayer dielectric on the underlayer and surrounding the bottom electrode; The phase change memory device of claim 1 further comprising:

3. a thermally and electrically insulating spacer on the stack surrounding the metal pillar beneath the phase change material element; The phase change memory device of claim 1 further comprising:

4. The phase change memory device of claim 3 , wherein the thermally and electrically insulating spacer has a width equal to a width of the stack.

5. a first dielectric layer surrounding the stack; an encapsulation layer formed over the phase change material element and the first dielectric layer; and A second dielectric layer formed on the encapsulation layer.

2. The phase change memory device of claim 1, further comprising: a top electrode formed on the second dielectric layer, the top electrode further comprising a top electrode contact electrically connecting the top electrode to the phase change material element.

6. The phase change memory device of claim 5 further comprising a top hard mask between the phase change material element and the top electrode contact.

7. The phase change memory device of claim 5 , wherein the top electrode contact extends through the encapsulation layer.

8. The phase change memory device of claim 1 further comprising an upper hard mask over said phase change material element having the same width as said phase change material element.

9. the stack of alternating conductor layers comprising: a bottom titanium nitride (TiN) layer; and Top tantalum nitride (TaN) layer The phase change memory device of claim 1 , comprising:

10. 10. The phase change memory device of claim 9, wherein a thickness of the bottom TiN layer is equal to a thickness of the top TaN layer.

11. 10. The phase change memory device of claim 9, wherein the bottom TiN layer has a thickness greater than a thickness of any other layer in the stack.

12. The phase change memory device of claim 9 , wherein the metal pillars are formed from a material other than TiN and TaN.

13. The phase change memory device of claim 1 , wherein the metal pillars are formed from a material different than a material of the stack of alternating conductive layers.

14. The phase change memory device of claim 1 , wherein the metal pillar is a heater.

15. The phase change memory device of claim 1 , wherein the metal pillar is a heater configured to heat the phase change material element.

16. 1. A method for fabricating a crossbar-type phase change memory cell, comprising: providing a bottom electrode disposed on the underlayer; forming a multi-layer stack including a plurality of alternating conductive layers; depositing a top metal layer formed of a material different from that of the multi-layer stack onto the multi-layer stack; forming a hard mask pillar on the top metal layer; etching the top metal layer to form metal pillars; forming an inner spacer surrounding the metal pillar; patterning the multi-layer stack using the hardmask pillars; forming a dielectric layer having a height equal to a top surface of the metal pillar; removing the hard mask pillars; and forming a phase change material element on the metal pillar; A method comprising:

17. The step of forming the phase change material element comprises: depositing a phase change material; forming an upper hard mask over the phase change material; and 17. The method of claim 16, comprising patterning a phase change material using the upper hardmask to form the phase change material elements.

18. depositing an encapsulation layer over the phase change material element; depositing a second dielectric layer over the encapsulation layer; forming a via in the encapsulation layer and the second dielectric layer to expose the upper hardmask; and performing metallization to form a top electrode and a top electrode contact contacting the top hardmask; 20. The method of claim 17, further comprising:

19. The step of forming the inner spacer comprises: depositing a dielectric liner over the multi-layer stack; and Etching back the dielectric liner to a width of the hard mask pillar.

20. The method of claim 16, further comprising:

20. 17. The method of claim 16, wherein the patterning of the multi-layer stack using the hard mask pillars is performed prior to etching the top metal layer to form the metal pillars and forming the interior spacers.

Citation Information

Patent Citations

  • Phase change memory and manufacturing method thereof

    CN113270545A

  • Memory cell having improved mechanical stability

    US20090251944A1

  • Cross-Point Memory Structures

    US20120235211A1

  • Integrated reactive material erasure element with phase change memory

    US20170092694A1