Battery cell, method for producing same, and direct water-cooled battery module including same
Patent Information
- Application Number
- JP2024527222
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-06-14
- Filing Date
- 2023-06-13
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2043-06-13
AI Technical Summary
【0029】 以上で詳察した通り、本発明の少なくとも一態様に係るバッテリーセル、この製造方法およびこれを含む直接水冷用バッテリーモジュールは次のような効果を有する。
Smart Images

Figure 2024539731000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a battery cell, a manufacturing method thereof, and a direct water-cooling battery module including the same, and more particularly to a battery cell that can improve the corrosion resistance of a battery cell by using a sacrificial metal that has a higher metal ionization tendency than a battery cell case, a manufacturing method thereof, and a direct water-cooling battery module including the same.
[0002] This application claims the benefit of priority based on Korean Patent Application No. 10-2022-0072013 dated June 14, 2022, and all contents disclosed in the documents of the Korean patent application are incorporated herein by reference. [Background technology]
[0003] Batteries used in environmentally friendly vehicles are required to have high output, so they generate a large amount of heat. In order to improve the performance and lifespan of the battery, it is very important to efficiently discharge the heat generated in the battery and prevent the battery from overheating.
[0004] Conventionally, as cooling systems for dissipating heat from a battery, a direct air cooling system, an indirect water cooling system, a direct water cooling system, and the like are known.
[0005] In the direct water cooling method, the battery cells are directly immersed in the coolant so that the heat of the battery cells is directly dissipated into the coolant.
[0006] FIG. 1 is a schematic configuration diagram of a conventional battery module 10. As shown in FIG.
[0007] 1, a direct water-cooling type battery module 10 includes a cell frame 11 and a plurality of battery cells 12. The plurality of battery cells 12 are spaced apart from each other in the cell frame 11. The cell frame 11 is provided to allow cooling water to flow therethrough.
[0008] Generally, the battery cell 12 has an exterior case that contains an internal electrode and is made of nickel-plated iron. Accordingly, if the battery cell 12 is directly immersed in coolant, it is vulnerable to corrosion due to the characteristics of the material of the exterior case. In addition, the exterior case has polarity and is also vulnerable to electrical insulation.
[0009] In a conventional direct water-cooling battery module 10, insulating oil or special cooling water M (for example, NOVEC (registered trademark) by 3M Company) is used to prevent corrosion of the battery cells 12.
[0010] However, insulating oil has the problem of being vulnerable to fire, and special coolants such as 3M's NOVEC (registered trademark) are excellent as coolants for battery cells because they are non-polar and corrosion-resistant, but they are expensive, which increases the unit manufacturing cost of battery modules.
[0011] In addition, when applying an anti-rust liquid to the exterior case of the battery cell 12 to prevent corrosion of the battery cell 12 as in the conventional method, a post-treatment process is required in which the exterior case of the battery cell 12 is surrounded by a non-woven fabric or the like to maintain the anti-rust liquid.
[0012] In addition, even if an anti-rust liquid is applied to the exterior case of the battery cell 12, the anti-rust agent flows off the exterior case of the battery cell due to surface tension, and the anti-rust agent is not evenly applied to the exterior case. Summary of the Invention [Problem to be solved by the invention]
[0013] The present invention aims to provide a battery cell that can improve the corrosion resistance of a battery cell by using a sacrificial metal that has a higher metal ionization tendency than a battery cell case, a manufacturing method thereof, and a direct water-cooling battery module including the same. [Means for solving the problem]
[0014] According to one aspect of the present invention, a method for manufacturing a battery cell includes the steps of: forming a scratch area in a unit plate material having a plating layer by scratching a portion of the plating layer; bonding a sacrificial metal sheet to one side of the unit plate material so as to cover the scratch area; and processing the unit plate material into a cylindrical shape so that the sacrificial metal sheet is exposed to the outside.
[0015] The scratch region may include a plurality of non-plated portions in which a portion of the plating layer of the unit plate is removed, and a plating portion in which the plating layer remains between two adjacent non-plated portions.
[0016] Also, a sacrificial metal sheet may be bonded to the unit plate by being pressed against the plating in the scratch area and the plating outside the scratch area.
[0017] The sacrificial metal sheet may be pressed against the unit plate material in a surface-to-surface contact state.
[0018] Also, the sacrificial metal sheet may be pressure-welded to the unit plate material by hot pressure welding.
[0019] Also, the sacrificial metal sheet may be pressure welded to the unit plate material by gas pressure welding.
[0020] Also, the sacrificial metal sheet may be pressure-welded to the unit plate material by cold welding.
[0021] Also, the scratch area may be provided by scratching the plating layer with a laser.
[0022] Also, the scratch area may be provided by etching the plating layer.
[0023] In addition, the sacrificial metal sheet may be made of a metal material having a higher metal ionization tendency than the unit plate materials.
[0024] Also, the sacrificial metal sheet may be made of at least one selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
[0025] Furthermore, a battery cell according to one embodiment of the present invention includes an electrode assembly, a case that accommodates the electrode assembly, a plating layer formed on an outer surface of the case, a scratch area formed by removing a portion of the plating layer, and a sacrificial metal sheet surrounding the scratch area and formed of a material having a greater metal ionization tendency than the plating layer, wherein the scratch area includes a plurality of non-plated portions formed by removing a portion of the plating layer and a plating portion in which the plating layer remains between two adjacent non-plated portions.
[0026] Additionally, a sacrificial metal sheet may be bonded to the exterior surface of the case by being pressed against the plating in the scratched area and the plating outside the scratched area.
[0027] Also, the plating layer may be a nickel plating layer, and the sacrificial metal sheet may be made of at least one selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
[0028] In addition, a battery module according to one aspect of the present invention includes the plurality of battery cells, a cell frame in which the plurality of battery cells are arranged at a distance from each other and in which coolant can flow between the plurality of battery cells, and a coolant supply unit for supplying coolant to an inside of the cell frame, the coolant supply unit being configured to supply uninsulated coolant. Effect of the Invention
[0029] As described above, the battery cell according to at least one embodiment of the present invention, the manufacturing method thereof, and the direct water-cooling battery module including the battery cell have the following advantages.
[0030] A case-type plate can be manufactured by pressing a sacrificial metal sheet onto a plate having a scratched region, and then the case-type plate can be processed into a cylindrical shape and an electrode assembly can be accommodated inside to manufacture a battery cell. As a result, the manufacturing process of the battery cell case can be simplified, and the product defect rate can be reduced through the simplification of the manufacturing process.
[0031] In addition, the scratch area on the plating layer on the case can facilitate the movement of electrons between the case and the sacrificial metal sheet, thereby improving the stability of the electrical connection between the sacrificial metal sheet and the case.
[0032] In addition, in manufacturing the battery cell case, the sacrificial metal sheet is surface-bonded to the plate material by a pressure welding method, and thus the bonding strength between the sacrificial metal sheet and the plate material can be improved.
[0033] In addition, a sacrificial metal sheet is provided on the outer surface of the battery cell case, so that corrosion of the battery cell can be prevented even if the battery cell is immersed in general cooling water for a long period of time. [Brief description of the drawings]
[0034] [Figure 1] FIG. 1 is a schematic configuration diagram of a conventional battery module. [Diagram 2] 1 is a schematic diagram illustrating a configuration of a direct water-cooling battery module according to an embodiment of the present invention; [Diagram 3] 1 is a schematic cross-sectional view of a battery cell according to an embodiment of the present invention; [Figure 4] 1 is a diagram illustrating a method for manufacturing a battery cell according to a first embodiment of the present invention. [Diagram 5] 1 is a diagram illustrating a method for manufacturing a battery cell according to a first embodiment of the present invention. [Figure 6] 1 is a diagram illustrating a method for manufacturing a battery cell according to a first embodiment of the present invention. [Figure 7] 11 is a diagram illustrating a process of manufacturing a case in a manufacturing method of a battery cell according to a second embodiment of the present invention. [Figure 8] 11 is a diagram illustrating a process of manufacturing a case in a manufacturing method of a battery cell according to a second embodiment of the present invention. [Figure 9] 11 is a diagram illustrating a process of manufacturing a case in a manufacturing method of a battery cell according to a second embodiment of the present invention. [Figure 10] 11 is a diagram illustrating a process of manufacturing a case in a manufacturing method of a battery cell according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0035] Hereinafter, a direct water-cooled battery cell (hereinafter also referred to as a "battery cell") according to one embodiment of the present invention, a manufacturing method thereof, and a direct water-cooled battery module (hereinafter also referred to as a "battery module") including the same will be described in detail with reference to the drawings.
[0036] In addition, regardless of the drawing symbols, identical or corresponding components will be given the same or similar reference numbers, and duplicate descriptions thereof will be omitted, and the size and shape of each component illustrated may be exaggerated or reduced for the convenience of explanation.
[0037] FIG. 2 is a schematic diagram of a direct water-cooling battery module according to an embodiment of the present invention, and FIG. 3 is a schematic cross-sectional view of a battery cell according to an embodiment of the present invention.
[0038] Referring to FIG. 2, a battery module 200 according to an embodiment of the present invention includes a plurality of battery cells 100, a cell frame 210 accommodating the plurality of battery cells 100, and a coolant supply unit 160.
[0039] Specifically, the battery module 200 includes a plurality of battery cells 100, a cell frame 210 in which the plurality of battery cells 100 are arranged at a distance from each other and in which coolant W can flow between the plurality of battery cells 100, and a coolant supply unit 160 for supplying the coolant W into the inside of the cell frame 210.
[0040] 2, the cell frame 210 has a predetermined space 211 therein, and is configured to allow the coolant W to flow within the space 211. The coolant W may be supplied to the space 211 inside the cell frame 210 and then discharged to the outside of the cell frame 210. To this end, the battery module 200 may include a coolant discharge unit for discharging the coolant W to the outside of the cell frame 210. The coolant supply unit 160 may include a coolant storage tank and a pump. The coolant supply unit 160 may be configured to supply the coolant W that is not insulated. The general coolant W may be coolant commonly used in vehicles.
[0041] Referring to FIG. 3, a battery cell 100 according to one embodiment of the present invention includes an electrode assembly 101, a case 110, a plating layer 111a, a scratch area S provided on the plating layer 111a, and a sacrificial metal sheet 113 surrounding the scratch area S.
[0042] In addition, the battery cell 100 may include a cell sheet including a polymer film and disposed to surround the sacrificial metal sheet 113.
[0043] The battery cell 100 includes an electrode assembly 101, a case 110 that accommodates the electrode assembly 101, a plating layer 111a formed on the outer surface of the case 110, a scratch area S formed by removing a portion of the plating layer 111a, and a sacrificial metal sheet 113 that is disposed to surround the scratch area S and is made of a material having a higher metal ionization tendency than the plating layer 111a.
[0044] 2, when the direct water-cooling battery cell 100 is immersed in cooling water W, the water H may be transferred to the sacrificial metal sheet 113. At this time, the metal ionization reaction of the sacrificial metal sheet 113 to the water H is greater than the metal ionization reaction of the case 110 to the water, so that the corrosion resistance of the case 110 can be improved.
[0045] Referring to FIG. 2, when the battery module 200 uses a general cooling water W to cool the battery cell 100, if moisture H penetrates through a corroded portion on the surface of the battery cell 100, a problem may occur in which the power source of the battery cell 100 is electrically connected to the general cooling water W, damaging the battery module 200.
[0046] Referring to FIG. 2, when the direct water-cooled battery cell 100 is immersed in cooling water W, the moisture H of the cooling water W undergoes an ionization reaction with the sacrificial metal sheet 113 due to the difference in metal ionization reaction between the case 110 and the sacrificial metal sheet 113. As a result, the metal ionization reaction of the case 110 is suppressed, thereby preventing corrosion of the case 110.
[0047] The electrode assembly 101 is housed in a case 110 and includes a positive electrode, a negative electrode, and a separator disposed between the positive and negative electrodes. The electrodes and the separator may be integrated to form the electrode assembly 101. For example, the electrode assembly 101 may be a jelly roll type electrode assembly in which sheet-type positive and negative electrodes are wound up with a separator interposed therebetween, a stack type electrode assembly in which a number of positive and negative electrodes are stacked in sequence with a separator interposed therebetween, or a stack / folding type electrode assembly in which unit cells in which a predetermined number of positive and negative electrodes are stacked with a separator interposed therebetween are positioned on a separator film and wound up in sequence.
[0048] In addition, the case 110 houses the electrode assembly 101 and serves to protect the battery cell 100 from external impact. The case 110 may be cylindrical, pouch-shaped, or rectangular, for example, the case 110 may be cylindrical. In particular, the electrode assembly 101 may be a wound jelly-roll type electrode assembly, the case 110 may be a cylindrical case, and the direct water-cooling battery cell 100 may be a cylindrical battery cell.
[0049] Also, the case 110 may be made of a metal material, and the case 110 may be made of at least one selected from the group consisting of steel and stainless steel.
[0050] In addition, the surface of the case 110 may be nickel (Ni) plated, that is, the plating layer 111a may include a nickel plating layer.
[0051] On the other hand, the nickel plating layer has excellent corrosion resistance, wear resistance, and excellent rust prevention and discoloration resistance, but due to the material properties, the nickel plating layer may be corroded when immersed in cooling water, and as the corrosion progresses, polarity is generated, resulting in a decrease in insulation properties.
[0052] Meanwhile, when the sacrificial metal sheet 113 is provided on the plating layer 111 a, the plating layer 111 a may become a factor that hinders the movement of electrons between the sacrificial metal sheet 113 and the case 110.
[0053] After forming the scratch area S on the plating layer 111a, the sacrificial metal sheet 113 is bonded to the scratch area S, so that the transfer of electrons between the sacrificial metal sheet 113 and the case 110 can be facilitated.
[0054] In addition, the scratch portion S may be formed by removing a portion of the plating layer 111a along the thickness direction of the plating layer 111a, and the scratch portion S may be formed on a portion of the plating layer 111a along the thickness direction of the plating layer 111a and on the outer surface of the case facing the portion.
[0055] The scratch area S also includes a plurality of non-plated portions (111c, see FIG. 6) in which a portion of the plating layer 111a has been removed, and a plating portion 111d in which the plating layer remains between two adjacent non-plated portions 111c.
[0056] Also, the scratch area S may be provided by scratching the plating layer 111a with a laser.
[0057] Also, the scratch area S may be provided by etching the plating layer 111a.
[0058] In addition, the sacrificial metal sheet 113 may be bonded to the outer surface of the case 110 by being pressed against the plating portion 111d in the scratch area S and the plating layer 111a outside the scratch area S.
[0059] In addition, the sacrificial metal sheet 113 may be pressed against the case 110 in a surface-to-surface contact state.
[0060] For example, the sacrificial metal sheet 113 may be pressure-welded to the case 110 by a hot pressure welding method. Alternatively, the sacrificial metal sheet 113 may be pressure-welded to the unit plate material by a gas pressure welding method. Alternatively, the sacrificial metal sheet 113 may be pressure-welded to the case 110 by a cold pressure welding method.
[0061] The sacrificial metal sheet 113 may be made of one or more selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
[0062] Referring to FIG. 2, the battery module 200 may include a waterproof layer 150 provided inside a cell frame 210 and provided to cover upper and lower ends of the case 110 of the battery cell 100, respectively.
[0063] The waterproof layer 150 serves to prevent moisture from penetrating into the case 110 and to fix the battery cell 100 to the cell frame 210 .
[0064] An upper waterproof layer may be provided at an upper end of the case 110, and a lower waterproof layer may be provided at a lower end of the case 110. In addition, the upper end side and the lower end side of the battery cell 100 may be fixed to the inner surface of the cell frame 210 via the waterproof layers 150, respectively.
[0065] Also, the waterproof layer 150 may include a waterproof adhesive or a potting resin, and the potting resin may be any one of a silicone-based resin, a urethane-based resin, and an epoxy-based resin.
[0066] The case 110 according to this embodiment can be manufactured according to either a first embodiment or a second embodiment described below.
[0067] 4 to 6 are views for explaining a method of manufacturing a battery cell according to a first embodiment of the present invention, in particular, a method of manufacturing a case of the battery cell.
[0068] A method for manufacturing a battery cell according to a first embodiment includes the steps of: forming a scratch area in a unit plate material having a plating layer by scratching a portion of the plating layer; bonding a sacrificial metal sheet to one side of the unit plate material so as to cover the scratch area; and processing the unit plate material into a cylindrical shape so that the sacrificial metal sheet is exposed to the outside.
[0069] The method for manufacturing the battery cell may further include embedding the electrode assembly in a unit plate material processed into a cylindrical shape.
[0070] First, referring to Fig. 4(a) and Fig. 6(a), a unit plate material P1 having a plating layer 111a is prepared. Here, the unit plate material P1 refers to a metal plate material having a size that can be manufactured into the case 110. The unit plate material P1 includes a metal plate material 111b and a plating layer 111a provided on the metal plate material 111b. The plating layer 111a is provided by nickel plating one surface of the metal plate material 111b.
[0071] Nickel plating is less likely to discolor, has excellent rust prevention, and is excellent in corrosion resistance and wear resistance. However, the plating layer 111a can be an element that hinders the movement of electrons between the sacrificial metal sheet 113 and the unit plate material P1.
[0072] To solve this problem, a portion of the plating layer 111a of the unit plate material P1 having the plating layer 111a is scratched. Accordingly, a scratch area S is provided on one side of the unit plate material P1. Referring to FIG. 6(b), the scratch area S is an area where the plating layer 111a is damaged on one side of the unit plate material P1.
[0073] Referring to FIG. 4(b), the scratch area S is provided so as to be surrounded by the edge area E of the unit plate material P1. The scratch area S may be formed by scratching the plating layer 111a of the unit plate material P with a laser. Alternatively, the scratch area S may be formed by etching the plating layer 111a of the plate material P. The etching method is a chemical etching method. The edge area E is an area where the plating layer 111a is not damaged.
[0074] 5, the scratch area S may be formed to have a predetermined scratch pattern line. For example, the scratch pattern line may be any one of a regular lattice pattern line (FIG. 5(a)), a diagonal lattice pattern line (FIG. 5(b)), a wavy pattern line (FIG. 5(c)), a "1"-shaped pattern line (FIG. 5(e)), or a "1"-shaped pattern line (FIG. 5(c)).
[0075] Due to this scratch pattern, the scratch area S may include a plurality of non-plated portions 111c in which a portion of the plating layer 111a has been removed, and a plating portion 111d in which the plating layer remains between two adjacent non-plated portions 111c.
[0076] The scratch area S is provided so as to be surrounded by an edge area E of the unit plate material. The edge area E is an area on one surface of the unit plate material where the plating layer 111a has not been removed.
[0077] 4(c) and 6(c), the sacrificial metal sheet 113 is laminated on one side of the unit plate material P1 so as to cover the scratch area S. The sacrificial metal sheet 113 is pressed against the plated portion 111d of the edge area E and the scratch area S, thereby being joined face-to-face to the unit plate material P1.
[0078] The sacrificial metal sheet 113 may be a metal sheet having an area larger than the scratch area S. Also, the sacrificial metal sheet 113 may be a metal sheet having a thickness smaller than the thickness of the unit plate material P1.
[0079] The sacrificial metal sheet 113 has a metal material having a higher metal ionization tendency than the unit plate material P1. For example, the sacrificial metal sheet 113 may be made of one or more selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
[0080] The sacrificial metal sheet 113 is joined to the unit plate material P1 by a pressure welding method, which may be any one of a hot pressure welding method, a cold pressure welding method, and a gas pressure welding method.
[0081] As an example, the hot pressure welding method is a method in which a welding member applies pressure and heat to the sacrificial metal sheet 113, so that the sacrificial metal sheet 113 is pressure-welded to the unit plate material P1.
[0082] As another example, the cold pressure welding method is a method in which a welding member presses the sacrificial metal sheet 113 at room temperature, and the sacrificial metal sheet 113 is pressed to the unit plate material P1 while being deformed by firing.
[0083] As yet another example, the gas pressure welding method is a method in which the welding parts are heated with a gas flame to a temperature above the recrystallization temperature, and pressure is applied from the axial direction to weld them.
[0084] In the scratch area S and edge area E, the sacrificial metal sheet 113 is pressed against the unit plate material P1 at the portions in contact with the plating layer, and the bonding points of the unit plate material P1 are uniformly distributed over the entire area of the sacrificial metal sheet, thereby improving the bonding strength of the sacrificial metal sheet 113 to the unit plate material P1.
[0085] A case plate (110a in FIG. 3) can be manufactured by bonding a sacrificial metal sheet 113 to one surface of the unit plate P1. Referring to FIG. 4(d), the case plate 110a is processed into a cylindrical shape so that the sacrificial metal sheet 113 is exposed to the outside. Accordingly, a case 110 of the battery cell 100 having the sacrificial metal sheet 113 provided on its outer surface is manufactured. As an example, the sacrificial metal sheet 113 may be provided on the outer surface of the case 110 in the form of a band along the periphery of the case 110.
[0086] In this embodiment, the sacrificial metal sheet 113 is bonded to the unit plate material P1 face-to-face by pressure bonding, thereby improving the bonding strength between the sacrificial metal sheet 113 and the unit plate material P1.
[0087] According to an embodiment of the present invention, the problem of the plating layer 111a causing the electron movement can be eliminated through the scratch area S. In addition, the electron movement between the sacrificial metal sheet 113 and the unit plate material P1 can be facilitated, and therefore the sacrificial metal sheet 113 can be electrically and stably connected to the unit plate material P1.
[0088] Figures 7 to 10 are diagrams for explaining a method of manufacturing a battery cell according to a second embodiment of the present invention, and in particular, diagrams for explaining a method of manufacturing a battery cell case. Figure 8 is a cross-sectional view taken along line aa in Figure 7, Figure 9 is a cross-sectional view taken along line bb in Figure 7, and Figure 10 is a cross-sectional view taken along line cc in Figure 7.
[0089] The battery cell manufacturing method according to the second embodiment includes a first step in which a plating layer 111a of a plate material P is scratched to provide a plurality of scratch areas S in each unit area A1 to A4 of a plate material P having a plurality of unit areas on the same plane; a second step in which a sacrificial metal sheet 113 is stacked and bonded to one side of the plate material P so as to cover the scratch areas S; a third step in which the plate material P is cut into the unit areas A1 to A4 to manufacture a plurality of case plate materials 110a; and a fourth step in which the case plate material 110a is processed into a cylindrical shape so that the sacrificial metal sheet 113 is exposed to the outside.
[0090] 7(a), a plate material P that can be divided into a plurality of unit areas on the same plane is prepared. The plate material P has a plating layer 111a provided on one surface.
[0091] Each unit area has a size that can be manufactured into the case 110. In this embodiment, for convenience of explanation, the multiple unit areas are divided and designated as a first unit area A1 to a fourth unit area A4.
[0092] In this embodiment, for convenience of explanation, the plate material P is divided into four unit areas, but this is merely an example, and the number of unit areas can be changed depending on the size of the plate material P.
[0093] 7(b) and 8, a plurality of scratch areas S are provided on one surface of a plate material P. The scratch areas S are areas provided by scratching the plating layer 111a of the plate material P. The plating layer 111a may be scratched by a laser method or a chemical method, as in the first embodiment described above.
[0094] In the second embodiment, a scratch area S is provided for each of the unit areas A1 to A4. The scratch areas S of the unit areas A1 to A4 are divided and designated as a first scratch area S1 to a fourth scratch area S4.
[0095] Here, the first scratch region S1 is a region in the first unit region A1 where the plating layer 111a is damaged, and the second scratch region S2 is a region in the second unit region A2 where the plating layer 111a is damaged.
[0096] The third scratch region S3 is a region in the third unit region A3 where the plating layer 111a is damaged, and the fourth scratch region S4 is a region in the fourth unit region A4 where the plating layer 111a is damaged.
[0097] The first scratch area S1 to the fourth scratch area S4 are provided on the same plane of the plate material P and are spaced apart from one another.
[0098] 7(c) and 7(d), the sacrificial metal sheet 113 is pressed against each of the unit areas A1 to A4, and the sacrificial metal sheet 113 is bonded to one surface of the plate material P. As shown in FIG.
[0099] 9 and 10, a sacrificial metal sheet 113 is laminated onto one side of the plate material P so as to cover the scratch area S.
[0100] As described above, the sacrificial metal sheet 113 has a metal material having a higher metal ionization tendency than the plate material P. For example, the sacrificial metal sheet 113 may be made of one or more selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
[0101] The sacrificial metal sheet 113 is joined to the plate material P by a pressure welding method. The pressure welding method may be any one of a hot pressure welding method, a cold pressure welding method, and a gas pressure welding method.
[0102] As one example, the hot pressure welding method is a method in which a welding member applies pressure and heat to the sacrificial metal sheet 113, and the sacrificial metal sheet 113 is pressure-welded to the plate material P. As another example, the cold pressure welding method is a method in which a welding member applies pressure to the sacrificial metal sheet 113 at room temperature, and the sacrificial metal sheet 113 is pressed against the plate material P while being deformed by firing. As yet another example, the gas pressure welding method is a method in which a welding member is heated by a gas flame to a temperature above the recrystallization temperature, and pressure is applied from the axial direction to pressure-weld.
[0103] After the sacrificial metal sheet 113 is bonded to one side of the plate P through the above-mentioned process, the plate P is cut into unit areas along cutting lines (indicated by symbol L in FIG. 7). In this embodiment, the plate P cut into unit areas A1 to A4 is referred to as a case plate 110a.
[0104] 7(f), the case plate material 110a is processed into a cylindrical shape so that the sacrificial metal sheet 113 is exposed to the outside, thereby manufacturing the case 110 having the sacrificial metal sheet 113 on its outer surface.
[0105] The above-described embodiment of the present invention has been disclosed for illustrative purposes, and a person skilled in the art having ordinary knowledge of the present invention may make various modifications, changes, and additions within the spirit and scope of the present invention, and such modifications, changes, and additions are to be considered as falling within the scope of the following claims. [Industrial Applicability]
[0106] According to an embodiment of the battery cell, a manufacturing method thereof, and a direct water-cooling battery module including the battery cell, the corrosion resistance of the battery cell can be improved by using a sacrificial metal that has a higher metal ionization tendency than the battery cell case. [Explanation of symbols]
[0107] 100 Battery Cells 101 Electrode assembly 110 cases 111a plating layer 111c Non-plated part 111d Plating Department 113 Sacrificial Metal Sheet S Scratch area
Claims
1. forming a scratch area on a unit plate having a plating layer by scratching a portion of the plating layer; bonding a sacrificial metal sheet to one side of the unit plate so as to cover the scratched area; and processing the unit plate material into a cylindrical shape so that the sacrificial metal sheet is exposed to the outside.
2. 2 . The method of claim 1 , wherein the scratch area includes a plurality of non-plated portions in which a portion of the plating layer is removed from the unit plate material, and a plating area in which the plating layer remains between two adjacent non-plated portions.
3. 3 . The method of claim 2 , wherein the sacrificial metal sheet is joined to the unit plate material by being pressed against the plating in the scratch area and the plating outside the scratch area. 4 .
4. The method of manufacturing a battery cell according to claim 3 , wherein the sacrificial metal sheet is pressed against the unit plate material in a surface-to-surface contact state.
5. The method of manufacturing a battery cell according to claim 4 , wherein the sacrificial metal sheet is pressed onto the unit plate material by a hot welding method.
6. The method of manufacturing a battery cell according to claim 4 , wherein the sacrificial metal sheet is pressure-welded to the unit plate material by a gas pressure welding method.
7. The method of manufacturing a battery cell according to claim 4 , wherein the sacrificial metal sheet is pressed onto the unit plate material by a cold welding method.
8. The method of manufacturing a battery cell according to claim 1 , wherein the scratch area is provided by scratching the plating layer with a laser.
9. The method of manufacturing a battery cell according to claim 1 , wherein the scratch area is provided by etching the plating layer.
10. The method of manufacturing a battery cell according to claim 1 , wherein the sacrificial metal sheet is made of a metal material having a higher metal ionization tendency than the unit plate materials.
11. 10. The method of claim 1, wherein the sacrificial metal sheet is made of at least one selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
12. An electrode assembly; a case for housing the electrode assembly; a plating layer formed on an outer surface of the case; a scratch area formed by removing a portion of the plating layer; A sacrificial metal sheet is provided to surround the scratch area and is made of a material having a higher metal ionization tendency than the plating layer; Including, The scratch area includes a plurality of non-plated portions from which a portion of the plating layer has been removed, and a plating area in which the plating layer remains between two adjacent non-plated portions.
13. 13 . The battery cell of claim 12 , wherein the sacrificial metal sheet is coupled to the outer surface of the case by being pressed against the plating in the scratch area and the plating outside the scratch area.
14. the plating layer is a nickel plating layer, 13. The battery cell of claim 12, wherein the sacrificial metal sheet is formed of one or more selected from the group consisting of aluminum, magnesium, zinc, an aluminum alloy, a magnesium alloy, and a zinc alloy.
15. A plurality of the battery cells according to claim 12; a cell frame in which a plurality of battery cells are arranged at a distance from each other and in which a cooling water is allowed to flow between the plurality of battery cells; a cooling water supply unit for supplying cooling water to the inside of the cell frame; Including, The cooling water supply unit is configured to supply non-insulated cooling water to the battery module.
Citation Information
Patent Citations
Plated steel plate for battery can, battery and alkaline dry battery
JP2007323896A
Material for contact part or battery component, and battery using it
JP2007335120A
Storage element
JP2014103026A
Steel plate for battery electrode terminal, and battery including the same
JP2016039034A