Cylindrical battery, battery pack including same, and automobile
The tab-less cylindrical battery design addresses high resistance and heat generation issues by distributing current flow and stabilizing the electrode assembly, enhancing thermal stability and energy density in large batteries.
Patent Information
- Application Number
- JP2024523963
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-22
- Filing Date
- 2022-10-21
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2042-10-21
AI Technical Summary
Conventional cylindrical batteries face issues with high resistance, heat generation, and space inefficiency due to concentrated current flow at electrode tabs, leading to thermal runaway and reduced energy density, especially in large form factors used in electric vehicles.
A tab-less cylindrical battery design with a current collector plate structure that distributes current flow evenly, minimizing resistance and heat generation by locating uncoated areas at the ends and using a support system to stabilize the electrode assembly within the battery housing.
The design significantly reduces electrical resistance, improves thermal stability, enhances energy density, and simplifies the manufacturing process while maintaining structural integrity and safety, particularly in large cylindrical batteries.
Smart Images

Figure 2024540991000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a cylindrical battery and a current collector plate applied thereto, and to a battery pack and an automobile including such a cylindrical battery.
[0002] More specifically, one embodiment of the present invention relates to a cylindrical battery having a structure in which force is not concentrated at welded portions between parts even if external impact or vibration is applied during use of the battery, a current collector plate applied thereto, and a battery pack and automobile including the same.
[0003] Also, one embodiment of the present invention relates to a positive electrode for an electrochemical device having improved electrochemical properties and an electrode assembly including the positive electrode.
[0004] This application claims priority to Korean Patent Application No. 10-2021-0142184, filed on October 22, 2021, the entire contents of which are incorporated herein by reference in their entirety in the specification and drawings. [Background technology]
[0005] Secondary batteries, which have high applicability to each product group and electrical properties such as high energy density, are commonly used not only in portable devices but also in electric vehicles (EVs) and hybrid electric vehicles (HEVs) that are driven by electrical sources.
[0006] Such secondary batteries not only have the primary advantage of dramatically reducing the use of fossil fuels, but are also environmentally friendly as they do not produce any by-products from energy use, and are attracting attention as a new energy source for improving energy efficiency.
[0007] Currently, secondary batteries such as lithium ion batteries, lithium polymer batteries, nickel cadmium batteries, nickel metal hydride batteries, and nickel zinc batteries are widely used. The operating voltage of such a unit secondary battery cell is about 2.5V to 4.5V. Therefore, when a higher output voltage is required, a battery pack is constructed by connecting a plurality of batteries in series. In addition, a battery pack may be constructed by connecting a plurality of batteries in parallel according to the charge / discharge capacity required for the battery pack. Therefore, the number of batteries included in the battery pack and the electrical connection form may be variously set according to the required output voltage and / or charge / discharge capacity.
[0008] Meanwhile, known types of secondary battery cells include cylindrical, prismatic and pouch-type batteries. In the case of cylindrical batteries, a separator, which is an insulator, is interposed between the positive and negative electrodes, and the separator is rolled up to form a jelly-roll-type electrode assembly, which is then inserted into a battery housing together with an electrolyte to form a battery. Strip-shaped electrode tabs are connected to the uncoated portions of the positive and negative electrodes, and the electrode tabs electrically connect the electrode assembly to electrode terminals exposed to the outside. For reference, the positive terminal is a cap plate of a sealed body that seals the opening of the battery housing, and the negative terminal is the battery housing.
[0009] However, in conventional cylindrical batteries having such a structure, current is concentrated at the strip-shaped electrode tabs connected to the positive electrode uncoated portion and / or the negative electrode uncoated portion, resulting in problems such as high resistance, excessive heat generation, and poor current collection efficiency.
[0010] Resistance and heat generation are not major issues with small cylindrical batteries with form factors such as 18650 and 21700. However, when the form factor of a cylindrical battery is increased to be used in an electric vehicle, a large amount of heat is generated around the electrode tabs during the fast charging process, which can cause the cylindrical battery to catch fire.
[0011] To solve these problems, a cylindrical battery (so-called tab-less cylindrical battery) has been proposed in which positive and negative uncoated areas are designed to be located at the top and bottom of a jelly-roll type electrode assembly, respectively, and current collectors are welded to these uncoated areas to improve current collection efficiency.
[0012] The conventional cylindrical battery will be described in more detail with reference to FIGS. 1 to 4. FIG.
[0013] Figures 1 to 3 are diagrams showing the manufacturing process of a tabless cylindrical battery. Figure 1 shows the structure of the electrode, Figure 2 shows the electrode winding process, and Figure 3 shows the process of welding a current collector plate to the folded surface of the uncoated part. Figure 4 is a cross-sectional view of the tabless cylindrical battery cut in the longitudinal direction (Y axis).
[0014] 1 to 4, the positive electrode 500 has a structure including a positive electrode active material part 520 and a positive electrode uncoated part 530 provided on one long side along the winding direction on a positive electrode sheet 500S. Also, the negative electrode 400 has a structure including a negative electrode active material part 420 and a negative electrode uncoated part 430 provided on one long side along the winding direction on a negative electrode sheet 400S. The electrode assembly 300 is manufactured by stacking the positive electrode 500 and the negative electrode 400 together with two separators 600 in order as shown in FIG. 2, and then winding them in one direction (X-axis direction). At this time, the uncoated part 530 of the positive electrode 500 and the uncoated part 430 of the negative electrode 400 are arranged in opposite directions to each other.
[0015] After the winding process, the uncoated portion 530 of the positive electrode 500 and the uncoated portion 430 of the negative electrode 400 are folded toward the core. Then, the uncoated portions 530 and 430 are welded to the current collectors P and 30, respectively.
[0016] No separate electrode tabs are attached to the positive electrode uncoated portion 530 and the negative electrode uncoated portion 430, and the current collector plate P, 30 is connected to an external electrode terminal, and a current path is formed with a large cross-sectional area along the winding axis direction of the electrode assembly 300 (see arrow), which has the advantage of reducing the resistance of the battery. This is because resistance is inversely proportional to the cross-sectional area of the path through which the current flows.
[0017] However, as the form factor of cylindrical batteries increases and the charging current during fast charging becomes larger, the heat generation problem reoccurs in table-less cylindrical batteries.
[0018] Specifically, the conventional tabless cylindrical battery 1 includes a battery housing 20 and a sealing body A, as shown in Fig. 4. The sealing body A includes a cap plate 40, a sealing gasket G1, and a connection plate C1. The sealing gasket G1 is fixed by a crimping portion 22 while covering the periphery of the cap plate 40. In addition, the electrode assembly 300 is fixed in the battery housing 20 by a beading portion 21 to prevent vertical movement.
[0019] Typically, the positive terminal is the cap plate 40 of the sealed body A, and the negative terminal is the battery housing 20. Thus, the second current collecting plate P coupled to the uncoated portion 530 of the positive electrode 500 is electrically connected to the connection plate C1 attached to the cap plate 40 through a strip-shaped lead L. Also, the first current collecting plate 30 coupled to the uncoated portion 430 of the negative electrode 400 is electrically connected to the bottom of the battery housing 20. The insulator S covers the second current collecting plate P to prevent the battery housing 20 and the uncoated portion 530 of the positive electrode 500, which have opposite polarities, from coming into contact with each other and causing a short circuit.
[0020] When the second current collecting plate P is connected to the connecting plate C1, a strip-shaped lead L is used. The lead L is either separately attached to the second current collecting plate P or is manufactured integrally with the second current collecting plate P. However, since the lead L is a thin strip, its cross-sectional area is small and a large amount of heat is generated when a fast charging current flows. In addition, the excessive heat generated in the lead L is transferred to the electrode assembly 300 and causes the separator 600 to shrink, which can cause an internal short circuit, which is a main cause of thermal runaway.
[0021] The leads L also occupy a considerable amount of installation space within the battery housing 20. Therefore, a cylindrical battery 1 including the leads L has low space efficiency and is limited in increasing energy density.
[0022] Furthermore, in order to connect conventional table-less cylindrical batteries 1 in series and / or parallel, bus bar components must be connected to the cap plate 40 of the sealed body A and the bottom surface of the battery housing 20, resulting in reduced space efficiency. A battery pack mounted on an electric vehicle includes hundreds of cylindrical batteries 1. Therefore, inefficiency in electrical wiring causes considerable inconvenience during the assembly process of the electric vehicle and during maintenance of the battery pack. Therefore, there is a need to develop a cylindrical battery having a structure in which positive and negative terminals are applied in the same direction in order to simplify the electrical connection structure of multiple cylindrical batteries.
[0023] In a cylindrical battery having the above-mentioned structure, a relatively large empty space may be formed between the negative collector plate and the cap plate, and also between the bottom surface of the battery housing opposite the cap plate and the positive collector plate.
[0024] Such empty spaces may cause the jelly-roll-type electrode assembly to swing inside the battery housing, particularly in the vertical direction, i.e., in the height direction of the cylindrical battery. If the electrode assembly moves up and down in this manner, the connection between the current collector plate and the electrode tab may be damaged, and further, the connection between the current collector plate and the battery housing, and the connection between the current collector plate and the battery terminal may also be damaged.
[0025] Therefore, it is necessary to minimize the space required for the electrode assembly to move. Also, if additional parts are applied to reduce the space required for the electrode assembly to move, the process becomes more complicated and the manufacturing cost increases. Therefore, it is necessary to solve these problems by utilizing the parts that are already applied.
[0026] Meanwhile, conventional cylindrical batteries generally have a structure in which tabs connecting an electrode assembly to an external terminal are welded to the foil of the electrode assembly. However, cylindrical batteries having such a structure have a limited current path, and an excessive increase in the self-resistance of the electrode assembly is unavoidable.
[0027] In response to this, attempts have been made to reduce resistance by increasing the number of tabs connecting the electrode assembly and the external terminal, but there is a limit to how much the resistance can be reduced to a desired level and how much of a current path can be secured simply by increasing the number of tabs.
[0028] Therefore, in order to reduce the self-resistance of the electrode assembly, it is necessary to develop a new electrode assembly structure and a current collector plate structure suitable for such an electrode assembly structure. In particular, the need for such an electrode assembly and current collector plate having a new structure is even greater in the application to devices that require high-output / high-capacity battery packs, such as electric vehicles.
[0029] There is also a need to develop a cylindrical battery having a structure that maintains an improved bond between the current collector and the battery housing, and a current collector structure that is applicable to such a cylindrical battery.
[0030] Meanwhile, when an electrode is manufactured using a conventional positive electrode active material containing secondary particles, particle cracking may occur, and internal cracks that occur during charging and discharging may increase gas generation, which may lead to problems with battery stability.
[0031] To solve this problem, positive electrode active materials in the form of single particles or pseudo-single particles, in which the primary particles are relatively large, have been developed. However, when the positive electrode active materials in the form of single particles or pseudo-single particles are applied to a high-loading electrode and rolled, the electrode cracks before the porosity of the electrode reaches a target level, and the resistance characteristics and charge / discharge efficiency of the lithium secondary battery are poor. Summary of the Invention [Problem to be solved by the invention]
[0032] The present invention has been made in consideration of the above-mentioned problems, and has an object to provide a current collector having a structure suitable for an electrode assembly having a low resistance structure, and a cylindrical battery including the same.
[0033] Another object of the present invention is to provide a current collector having a structure capable of improving the bonding strength at a bonding portion between the current collector and a battery housing, and a cylindrical battery including the same.
[0034] It is yet another object of the present invention to prevent damage to electrical connections caused by movement of the jelly roll within the battery housing.
[0035] Another object of the present invention is to prevent movement of an electrode assembly by utilizing components that are already applied in manufacturing a cylindrical battery, thereby preventing the complication of manufacturing processes and increase in manufacturing costs that would occur due to the application of additional components.
[0036] It is yet another object of the present invention to provide a current collector having a structure capable of improving the energy density of a cylindrical battery, and a cylindrical battery including the same.
[0037] Another object of the present invention is to provide a current collector plate having a structure that can improve the convenience of a welding process for electrically connecting a battery housing and a current collector plate in manufacturing a cylindrical battery, thereby improving productivity, and a cylindrical battery including the same.
[0038] It is yet another object of the present invention to provide a cylindrical battery including an electrode assembly of an improved structure, a battery pack including the same, and an automobile including the battery pack.
[0039] Another object of the present invention is to provide an electrode and an electrode assembly including the same, which can achieve excellent thermal stability by using single particles or pseudo single particles as a positive electrode active material, and have high electrical conductivity and excellent rolling characteristics.
[0040] Another object of the present invention is to provide an electrode assembly having improved energy density by applying a silicon-based negative electrode active material to the negative electrode.
[0041] It is yet another object of the present invention to provide an electrode assembly in which the section of a positive electrode active material portion is increased without the risk of lithium precipitation.
[0042] Another object of the present invention is to provide a cylindrical battery that can exhibit excellent thermal stability even when the volume of the battery increases due to an increase in the form factor.
[0043] The technical problems to be solved by the present invention are not limited to the problems mentioned above, and other problems will be clearly understood by those skilled in the art from the following description of the invention. [Means for solving the problem]
[0044] In order to achieve the above object, a cylindrical battery according to one aspect of the present invention includes an electrode assembly having a first electrode tab and a second electrode tab, a battery housing that receives the electrode assembly through an opening formed on one side thereof, a support portion disposed on one side of the electrode assembly, at least one tab coupling portion extending from the support portion and coupled to the first electrode tab, and at least one housing coupling portion extending from an end of the tab coupling portion and coupled to an inner side of the battery housing, and includes a first current collecting plate located within the battery housing, a cap plate covering the opening, a battery terminal penetrating the battery housing from the opposite side of the opening and electrically connected to the second electrode tab, and a sealing spacer configured to prevent movement of the electrode assembly and strengthen the sealing force of the battery housing.
[0045] The battery housing may include a beading portion formed on a periphery adjacent the opening and pressed inward.
[0046] The housing mating portion may be mated onto the beading portion.
[0047] The housing coupling portion may include a contact portion coupled onto the beading portion, and a coupling portion connecting between the tab coupling portion and the contact portion.
[0048] The cylindrical battery may include a sealing gasket disposed between the battery housing and the cap plate.
[0049] The contact portion may be interposed and fixed between a beading portion of the battery housing and the sealing gasket.
[0050] In the cylindrical battery, a weld may be formed between the beading portion of the battery housing and the contact portion of the current collector plate.
[0051] In the cylindrical battery, a boundary area between the tab joint portion and the housing joint portion may be located inside an innermost portion of the beading portion.
[0052] The cylindrical battery may include a plurality of the tab coupling portions and a plurality of the housing coupling portions.
[0053] The connecting portion may include at least one bent portion where an extending direction is changed.
[0054] The contact portion may have an arc shape extending along a beading portion of the battery housing.
[0055] The connecting portion may have an arc shape extending along the contact portion.
[0056] The sealing spacer may include a motion prevention portion interposed between the first collecting plate and the cap plate, a sealing portion interposed between the battery housing and the cap plate, and a connecting portion connecting the motion prevention portion and the sealing portion.
[0057] The motion prevention portion may have a height corresponding to a distance between the first current collecting plate and the cap plate.
[0058] The motion prevention portion may be located at a center portion on one surface of the electrode assembly.
[0059] The motion prevention portion may include a spacer hole formed at a position corresponding to a winding center hole of the electrode assembly.
[0060] The sealing portion may have a shape extending along an inner circumferential surface of the battery housing.
[0061] The linkage may include a number of extension legs extending radially from the motion prevention portion.
[0062] The extension legs may be configured not to contact the first current collector plate.
[0063] The extension legs may be configured to not contact the cap plate.
[0064] The connection portion may be positioned so as not to overlap with the housing coupling portion along a height direction of the cylindrical battery.
[0065] The cylindrical battery may further include a second current collecting plate coupled to the second electrode tab, and an insulator interposed between a closing portion formed at an upper end of the battery housing and the second current collecting plate.
[0066] The insulator may have a height corresponding to the distance between the second current collector and the closure.
[0067] The active material layer of the second electrode includes a positive electrode active material including a single particle, a pseudo-single particle, or a combination thereof, and the positive electrode active material has a minimum particle size D min is 1.0 μm or more, and the particle size D when the volume cumulative amount is 50% in the volume cumulative distribution of the positive electrode active material 50 is 5.0 μm or less, and the maximum particle size D appearing in the volume cumulative distribution of the positive electrode active material is max can be 12 μm to 17 μm.
[0068] The positive active material may have a unimodal particle size distribution in which a single peak appears in a volume cumulative particle size distribution graph, and a particle size distribution (PSD) represented by the following Equation 1 may be 3 or less.
[0069] [Formula 1] Particle size distribution (PSD)=(D max -D min ) / D 50 The single particles, quasi-single particles, or a combination thereof may be included in an amount of 95 wt % to 100 wt % based on the total weight of the positive electrode active material included in the active material layer of the second electrode.
[0070] The positive electrode active material may include a lithium nickel-based oxide containing 80 mol % or more of Ni based on the total moles of transition metals.
[0071] The active material layer of the second electrode may have a porosity of 15% to 23%, and the active material layer of the second electrode may contain flake graphite at a weight ratio of 0.05 wt % to 5 wt %.
[0072] The active material layer of the second electrode may further include carbon nanotubes (CNTs).
[0073] The first electrode active material layer may include a silicon-based negative electrode active material and a carbon-based negative electrode active material, and the silicon-based negative electrode active material and the carbon-based negative electrode active material may be included in a weight ratio of 1:99 to 20:80.
[0074] A battery pack according to another aspect of the present invention includes the cylindrical battery according to the above-mentioned aspect of the present invention.
[0075] A vehicle according to yet another aspect of the present invention includes a battery pack according to the above-mentioned aspect of the present invention. Effect of the Invention
[0076] According to one aspect of the present invention, the resistance in the electrical connection between the electrode assembly and the battery housing can be significantly reduced.
[0077] Furthermore, according to one aspect of the present invention, the bonding strength of the bonding portion between the current collector plate and the battery housing can be improved.
[0078] Furthermore, according to one embodiment of the present invention, the energy density of a cylindrical battery can be improved.
[0079] In addition, according to one aspect of the present invention, in manufacturing a cylindrical battery, the convenience of a welding process for electrically connecting a battery housing and a current collector plate can be improved, thereby improving productivity.
[0080] Additionally, according to one aspect of the present invention, movement of the jelly roll within the battery housing is minimized, thereby preventing damage to electrical connections.
[0081] In addition, according to one aspect of the present invention, instead of applying additional parts to prevent the jelly roll from moving, the parts that are already applied can be utilized, thereby preventing the manufacturing process from becoming complicated and the manufacturing costs from increasing.
[0082] According to another aspect of the present invention, min By incorporating a positive electrode active material powder having a particle size of 1.0 μm or more in the positive electrode, the thermal stability of the battery can be further improved. According to the research of the present inventors, it has been confirmed that even if single particles and / or pseudo-single particles are used as the positive electrode active material, the effect of suppressing particle breakage after rolling and improving thermal stability differs depending on the particle size of the positive electrode active material powder. In particular, when particles having a particle size of less than 1.0 μm are contained in the positive electrode active material powder, the linear pressure increases in the rolling process, which increases particle cracking and reduces thermal stability, making it impossible to ensure sufficient thermal stability when applied to a large cylindrical battery. Therefore, in the present invention, min By using positive electrode active material powder with particle size controlled to 1.0 μm or more, the thermal stability improvement effect can be maximized.
[0083] According to another aspect of the present invention, 50 , D max By incorporating positive electrode active material powder with an appropriately controlled particle size distribution (PSD) into the positive electrode, the increase in resistance due to the application of single particles can be minimized, resulting in excellent capacity and output characteristics.
[0084] Moreover, according to one embodiment of the present invention, the conductivity of the electrode can be improved by including a single-particle positive electrode active material coated with a conductive coating layer or including the novel CNT as a conductive material.
[0085] According to one aspect of the present invention, the positive electrode active material layer includes flake graphite, and when the positive electrode active material layer is rolled, the flake graphite provides a sliding effect to the positive electrode active material, thereby improving the rolling characteristics of the electrode and reducing the electrode porosity to a target level, thereby improving the stability, initial resistance characteristics, and charge / discharge efficiency of the cylindrical battery.
[0086] Furthermore, according to one embodiment of the present invention, a higher energy density can be achieved by including a silicon-based negative electrode active material with a large capacity in the negative electrode.
[0087] Furthermore, according to one aspect of the present invention, since the positive electrode includes a reduced loading portion having a small amount of positive electrode active material loaded therein, the section of the positive electrode active material portion can be increased without worrying about lithium precipitation.
[0088] In addition, according to one embodiment of the present invention, the internal heat generation of the battery can be effectively reduced compared to conventional batteries equipped with strip-shaped electrode tabs, thereby improving the thermal stability of the battery.
[0089] The effects of the present invention are not limited to the effects described above, and other effects not mentioned will be clearly understood by those skilled in the art from the following description of the invention.
[0090] The following drawings attached to this specification illustrate preferred embodiments of the present invention and, together with the detailed description of the invention, serve to further understand the technical ideas of the present invention. Therefore, the present invention should not be interpreted as being limited to only the matters described in the drawings. [Brief description of the drawings]
[0091] [Figure 1]FIG. 1 is a plan view showing the structure of an electrode used in a conventional tabless cylindrical battery cell. [Diagram 2] 1A to 1C are diagrams showing a winding process of an electrode assembly included in a conventional tabless cylindrical battery cell. [Diagram 3] 3 is a diagram showing a process of welding a current collector plate to a bent surface of an uncoated portion in the electrode assembly of FIG. 2. [Figure 4] FIG. 1 is a cross-sectional view of a conventional tabless cylindrical battery cell cut in the longitudinal direction (Y axis). [Diagram 5] 1 is a vertical cross-sectional view showing a portion of a cylindrical battery according to an embodiment of the present invention. [Figure 6] 11 is a longitudinal sectional view showing a portion of a cylindrical battery according to another embodiment of the present invention. [Figure 7] 11 is a longitudinal sectional view showing a portion of a cylindrical battery according to still another embodiment of the present invention. [Figure 8] 8 is a diagram illustrating a first current collecting plate included in the cylindrical battery of FIG. 7. FIG. [Figure 9] FIG. 4 is a view illustrating a first current collecting plate according to another embodiment of the present invention. [Figure 10] FIG. 11 is a view illustrating a first current collecting plate according to still another embodiment of the present invention. [Figure 11] 1 is a perspective view showing the appearance of a cylindrical battery according to an embodiment of the present invention; [Figure 12] 1 is a cross-sectional view showing an internal structure of a cylindrical battery according to an embodiment of the present invention. [Figure 13] 4 is a partial cross-sectional view showing an area where a sealing spacer is applied according to an embodiment of the present invention; [Figure 14] 1 is a view illustrating a sealing spacer according to an embodiment of the present invention; [Figure 15] FIG. 2 is a plan view showing the bottom surface of a cylindrical battery according to an embodiment of the present invention. [Figure 16] 2 is a partial cross-sectional view showing an area where an insulator is applied according to an embodiment of the present invention; [Figure 17]4 is a partial cross-sectional view showing a coupling structure between a current collecting plate and an electrode tab according to an embodiment of the present invention; [Figure 18] 1 is a schematic diagram showing a battery pack according to an embodiment of the present invention; [Figure 19] 1 is a conceptual diagram showing a vehicle according to an embodiment of the present invention; [Figure 20] 1 is a scanning electron microscope (SEM) photograph of a novel CNT according to one embodiment of the present invention. [Figure 21] This is a scanning electron microscope (SEM) photograph of a commonly used conventional carbon nanotube (conventional CNT). [Figure 22] 1 is a table comparing the physical properties of conventional CNTs and the physical properties of new CNTs. [Diagram 23] 1 is a graph showing sheet resistance depending on the ratio of a conductive material when single-particle active material particles are used as a positive electrode active material. [Figure 24] 1 is a graph showing high-temperature life characteristics according to the ratio of a conductive material when single-particle active material particles are used as a positive electrode active material. [Diagram 25] 1 is a graph showing high-temperature life characteristics according to the ratio of a conductive material when single-particle active material particles are used as a positive electrode active material. [Figure 26] 1 is a graph showing high-temperature life characteristics according to the ratio of a conductive material when single-particle active material particles are used as a positive electrode active material. [Figure 27] 13 is a table comparing the solid content and viscosity of the positive electrode slurry, the resistance value in the MP coating layer, and the resistance value in the MP interface layer when carbon nanotubes (new CNTs) having a BET specific surface area of 300 m2 / g to 500 m2 / g are used, and when carbon nanotubes (conventional CNTs) having a BET specific surface area of 200 m2 / g or more and less than 300 m2 / g are used. [Figure 28a] 2 is a SEM photograph of the positive electrode active material used in Example 2-1 of the present invention. [Figure 28b] 2 is a SEM photograph of the positive electrode active material used in Example 2-2 of the present invention. [Figure 28c]1 is a SEM photograph of the positive electrode active material used in Comparative Example 2-2 of the present invention. [Figure 29a] 1 is a graph showing the results of a hot box test for a 4680 cell manufactured according to Example 1 of the present invention. [Figure 29b] 1 is a graph showing the results of a hot box test for a 4680 cell manufactured according to Comparative Example 1 of the present invention. [Figure 29c] 1 is a graph showing the results of a hot box test for 4680 cells manufactured according to Sample 1 of Example 2-1 of the present invention and Comparative Example 2-1. [Figure 29d] 1 is a graph showing the results of a hot box test for 4680 cells manufactured according to Samples 2 and 3 of Example 2-1 of the present invention, Samples 1 and 2 of Example 2-2, and Comparative Example 2-2. [Figure 30a] 2 is a cross-sectional SEM photograph of the positive electrode produced in Example 2-1 of the present invention. [Figure 30b] 1 is a cross-sectional SEM photograph of a positive electrode produced in Comparative Example 2-1. [Figure 31a] 13 is a graph showing the results of measuring the resistance characteristics according to SOC while charging coin-type half cells including the positive electrodes according to Example 3-3 of the present invention, Comparative Example 3-1, and Comparative Example 3-2 up to 4.2 V. [Figure 31b] 1 is a graph showing the measurement results of capacity retention and resistance increase rate obtained through a charge-discharge cycle experiment on 4680 cells according to Example 3-1, Example 3-3, and Comparative Example 3-1 of the present invention. [Diagram 32] 1 illustrates an electrode assembly according to an embodiment of the present invention. [Diagram 33] 33 is a cross-sectional view taken along line AA' in FIG. 32. [Diagram 34] 1A to 1C are diagrams illustrating a process for manufacturing a negative electrode according to an embodiment of the present invention. [Diagram 35] 1A to 1C are diagrams illustrating a process for manufacturing a negative electrode according to an embodiment of the present invention. [Diagram 36] FIG. 2 is a perspective view showing a negative electrode according to one embodiment of the present invention. [Figure 37] 1A to 1C are diagrams illustrating a process for producing a positive electrode according to one embodiment of the present invention. [Figure 38] 1A to 1C are diagrams illustrating a process for producing a positive electrode according to one embodiment of the present invention. [Figure 39] FIG. 2 is a perspective view showing a positive electrode according to one embodiment of the present invention. [Diagram 40] 13 is a diagram showing an electrode assembly according to a comparative example of the present invention; [Diagram 41] 41 is a cross-sectional view taken along line BB' in FIG. 40. [Diagram 42] FIG. 2 is a diagram showing a process for producing a negative electrode according to a comparative embodiment of the present invention. [Diagram 43] FIG. 2 is a diagram showing a process for producing a positive electrode according to a comparative embodiment of the present invention. [Diagram 44] 1 is a graph showing changes in energy density depending on the content of a silicon-based negative electrode active material and whether or not the silicon-based negative electrode active material is doped in a battery using a mixture of a silicon-based negative electrode active material and a carbon-based negative electrode active material as a negative electrode active material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0092] Hereinafter, a preferred embodiment of the present invention will be described in detail with reference to the attached drawings. Prior to this, the terms and words used in this specification and claims are not to be construed as being limited to their ordinary and dictionary meanings, but are to be construed as being in accordance with the meaning and concept of the technical idea of the present invention, in accordance with the principle that the inventor himself can appropriately define the concept of the term in order to best describe the invention. Therefore, it should be understood that the embodiment described in this specification and the configuration shown in the drawings are merely the most preferred embodiment of the present invention, and do not represent the entire technical idea of the present invention, and therefore there may be various equivalents and modifications that can be substituted therefor at the time of this application.
[0093] In addition, in order to facilitate understanding of the invention, the accompanying drawings may not be drawn to scale, and the dimensions of some components may be exaggerated. Also, the same reference numerals may be used to refer to the same components in different embodiments.
[0094] The size and thickness of each component shown in the drawings are arbitrarily shown for convenience of explanation, and the present invention is not necessarily limited by the drawings. In the drawings, the thicknesses are exaggerated to clearly show many layers and regions. In the drawings, the thicknesses of some layers and regions are exaggerated for convenience of explanation.
[0095] Furthermore, when a part such as a layer, film, region, or plate is described as being "on" or "above" another part, this includes not only the case where it is "directly on" the other part, but also the case where there is another part in between. Conversely, when a part is described as being "directly on" another part, it means that there is no other part in between. Furthermore, being "on" or "above" a reference part means being located above or below the reference part, and does not necessarily mean being located "on" or "above" the direction opposite to gravity.
[0096] Furthermore, throughout the specification, when a part "comprises" another component, it does not mean excluding the other component, but means that the other component may be further included, unless otherwise specified.
[0097] Furthermore, throughout the specification, a "plan view" means a view of the subject part viewed from above, and a "cross-sectional view" means a view of a vertical cross-section of the subject part viewed from the side.
[0098] 5, a cylindrical battery 1 according to an embodiment of the present invention includes an electrode assembly 300, a battery housing 20, a first current collector 30, a cap plate 40, and a battery terminal 60. The cylindrical battery 1 may further include a sealing gasket G1 and / or an insulating gasket G2 and / or a second current collector P and / or an insulator S.
[0099] The electrode assembly 300 includes a first electrode tab 11 and a second electrode tab 12. The electrode assembly 300 includes a first electrode having a first polarity, a second electrode having a second polarity, and a separator interposed between the first electrode and the second electrode. The first electrode is a negative electrode or a positive electrode, and the second electrode is an electrode having an opposite polarity to the first electrode. More specifically, the electrode assembly 300 may be manufactured by winding up a stack formed by sequentially stacking a first electrode, a separator, a second electrode, and a separator at least once. That is, the electrode assembly 300 applied to the embodiment of the present invention may be a jelly roll type electrode assembly. The jelly roll type electrode assembly 300 may include a winding center hole H1 formed at a substantially central portion thereof and extending along a height direction (a direction parallel to the height direction of the cylindrical battery 1 shown in FIG. 5). Meanwhile, a separator may be further provided on an outer circumferential surface of the electrode assembly 300 for insulation from the battery housing 20.
[0100] The first electrode includes a first electrode collector and a first electrode active material layer applied on one or both sides of the first electrode collector. An uncoated portion where the first electrode active material is not applied is present at one end of the first electrode collector in the width direction (parallel to the height direction of the cylindrical battery 1 shown in FIG. 5). The uncoated portion of the first electrode extends from one end to the other end along the length of the first electrode when the first electrode is in an unfolded state. The uncoated portion of the first electrode functions as the first electrode tab 11 as described above. The first electrode tab 11 is provided at the upper part of the electrode assembly 300 housed in the battery housing 20 in the height direction (parallel to the height direction of the cylindrical battery 1 shown in FIG. 5). The first electrode tab 11 may be, for example, a negative electrode tab.
[0101] The second electrode includes a second electrode collector and a second electrode active material layer applied on one or both sides of the second electrode collector. The second electrode collector has an uncoated portion at the other end in the width direction (parallel to the height direction of the cylindrical battery 1 shown in FIG. 5) where the second electrode active material is not applied. The uncoated portion of the second electrode extends from one end to the other end along the length of the second electrode when the second electrode is in an unfolded state. The uncoated portion of the second electrode functions as the second electrode tab 12 as described above. The second electrode tab 12 is provided at the lower part in the height direction of the electrode assembly 300 accommodated in the battery housing 20. The second electrode tab 12 may be, for example, a positive electrode tab.
[0102] That is, the first electrode tab 11 and the second electrode tab 12 extend in opposite directions along the height direction of the cylindrical battery 1 and protrude.
[0103] However, the present invention is not limited to this form of the electrode assembly 300.
[0104] The battery housing 20 is a substantially cylindrical container having an opening on one side thereof, and is made of a conductive metal material. The side of the battery housing 20 and a bottom surface (the bottom surface in reference to FIG. 5) located opposite the opening may be integrally formed. That is, the battery housing 20 may have a shape in which an upper end in a height direction thereof is open and a lower end thereof is closed. The bottom surface of the battery housing 20 may have a substantially flat shape. The battery housing 20 accommodates the electrode assembly 300 through an opening formed on one side in a height direction thereof. The battery housing 20 may also accommodate an electrolyte through the opening. However, the present invention is not limited to the shape of the battery housing 20.
[0105] The battery housing 20 is electrically connected to the electrode assembly 300. The battery housing 20 is connected to the first electrode tab 11 of the electrode assembly 300. Therefore, the battery housing 20 has the same polarity as the first electrode tab 11 electrically.
[0106] The battery housing 20 may include a beading portion 21 formed on a periphery adjacent to the opening and pressed inward. The battery housing 20 may have the beading portion 21 formed on an upper end portion. The battery housing 20 may further include a crimping portion 22 formed above the beading portion 21. The beading portion 21 has a shape in which the periphery of the battery housing 20 is pressed to a predetermined depth. The beading portion 21 is formed on the upper portion of the electrode assembly 300. The inner diameter of the battery housing 20 in the region where the beading portion 21 is formed is smaller than the diameter of the electrode assembly 300.
[0107] The beading portion 21 provides a support surface on which the cap plate 40 is placed. The beading portion 21 may also provide a support surface on which at least a portion of the periphery of the first current collecting plate 30 described below is placed and coupled. That is, at least a portion of the periphery of the first current collecting plate 30 according to the embodiment of the present invention and / or the periphery of the cap plate 40 according to the embodiment of the present invention may be placed on the upper surface of the beading portion 21. As shown in Figs. 6 and 7, the upper surface of the beading portion 21 may have a shape in which at least a portion of the upper surface of the beading portion 21 extends along a direction approximately parallel to the lower surface of the battery housing 20, i.e., along a direction approximately perpendicular to the side wall of the battery housing 20, so as to stably support at least a portion of the periphery of the first current collecting plate 30 and / or the periphery of the cap plate 40.
[0108] The crimping portion 22 is formed on the upper part of the beading portion 21. The crimping portion 22 is extended and bent to enclose the periphery of the cap plate 40 disposed on the upper part of the beading portion 21. Due to the shape of the crimping portion 22, the cap plate 40 is fixed on the beading portion 21. Of course, the crimping portion 22 may be omitted and the cap plate 40 may be fixed while covering the opening of the battery housing 20 through another fixing structure.
[0109] Hereinafter, the first current collecting plate 30 according to an embodiment of the present invention will be described in detail with reference to FIGS.
[0110] 7, a first current collecting plate 30 according to an embodiment of the present invention is accommodated inside a battery housing 20, electrically connected to an electrode assembly 300, and also electrically connected to the battery housing 20. That is, the first current collecting plate 30 electrically connects between the electrode assembly 300 and the battery housing 20.
[0111] The first current collecting plate 30 includes a support portion 31 disposed on one side of the electrode assembly 300, at least one tab connecting portion 32 extending from the support portion 31 and connected to the first electrode tab 11, and at least one housing connecting portion 33 extending from an end of the tab connecting portion 32 and connected to an inner surface of the battery housing 20, and is positioned within the battery housing.
[0112] The support portion 31 and the at least one tab coupling portion 32 are disposed on the upper portion of the electrode assembly 300, and may be located below the beading portion 21 if the beading portion 21 is formed on the battery housing 20.
[0113] The support part 31 may have a first current collecting plate hole H2 formed at a position corresponding to a winding center hole H1 formed at approximately the center of the electrode assembly 300. The winding center hole H1 and the first current collecting plate hole H2, which are in communication with each other, may function as a passage for inserting a welding rod or irradiating a laser for welding a battery terminal 60 and a second current collecting plate P, which will be described later, or for welding the battery terminal 60 and a lead tab (not shown).
[0114] The support part 31 may be in the form of a substantially circular plate. For example, referring to Fig. 8, the support part 31 may be in the form of a ring-shaped plate having a first current collecting plate hole H2 at its center.
[0115] The at least one tab coupling portion 32 may extend radially from the support portion 31 toward a side wall of the battery housing 20. For example, a plurality of tab coupling portions 32 may be provided. For example, referring to FIG. 8, the plurality of tab coupling portions 32 may be positioned spaced apart from each other along the circumference of the support portion 31. As such, the cylindrical battery 1 according to the embodiment of the present invention includes a plurality of tab coupling portions 32, so that the coupling area with the first electrode tab 11 can be increased. As a result, the coupling force between the first electrode tab 11 and the tab coupling portions 32 is secured, and electrical resistance is reduced.
[0116] A longitudinal end of the tab coupling portion 32 may be located inside an innermost portion of a beading portion 21 formed on the battery housing 20. More specifically, a boundary region between the tab coupling portion 32 and the housing coupling portion 33 may be located inside the innermost portion of the beading portion 21 formed on the battery housing 20 toward the winding center hole H1. This structure can prevent damage to the coupling portions between the components that may be caused by excessively bending the first current collecting plate 30 to position the end of the housing coupling portion 33 on the beading portion 21.
[0117] Meanwhile, in order to secure a bonding force and reduce electrical resistance by increasing the bonding area between the first current collector plate 30 and the electrode assembly 300, not only the tab coupling portion 32 but also the support portion 31 may be coupled to the first electrode tab 11. The end of the first electrode tab 11 may be formed in a shape bent parallel to the tab coupling portion 32. When the end of the first electrode tab 11 is shaped and coupled to the tab coupling portion 32 in a state parallel to the tab coupling portion 32, the bonding area is increased to improve the bonding force and reduce the electrical resistance, and the overall height of the electrode assembly 300 is minimized to improve the energy density.
[0118] The housing coupling part 33 may extend from an end of the tab coupling part 32 and be coupled to an inner surface of the battery housing 20. For example, the housing coupling part 33 may extend from an end of the tab coupling part 32 toward a side wall of the battery housing 20. For example, a plurality of the housing coupling parts 33 may be provided. For example, referring to FIG. 8, the plurality of housing coupling parts 33 may be positioned spaced apart from each other around the support part 31. Referring to FIG. 5, the housing coupling part 33 may be coupled to a beading part 21 of the inner surface of the battery housing 20. As shown in FIGS. 6 and 7, the upper surface of the beading part 21 extends in a direction substantially parallel to the lower surface of the battery housing 20, i.e., in a direction substantially perpendicular to the side wall of the battery housing 20, and the housing coupling part 33 also extends in the same direction, so that the housing coupling part 33 can stably contact the beading part 21. In addition, since the housing coupling portion 33 is in stable contact with the beading portion 21, the welding between the two parts is performed smoothly, thereby improving the coupling strength between the two parts and minimizing the increase in resistance at the coupling portion. In addition, since the first current collecting plate 30 is coupled onto the beading portion 21 of the battery housing 20 instead of onto the inner surface of the cylindrical portion of the battery housing 20, the distance between the first current collecting plate 30 and the beading portion 21 is reduced. Therefore, the dead space inside the battery housing 20 is minimized, and the energy density of the cylindrical battery 1 can be improved.
[0119] 7 and 8, the housing coupling portion 33 includes a contact portion 33a coupled to an inner surface of the battery housing 20, and a coupling portion 33b connecting the tab coupling portion 32 and the contact portion 33a.
[0120] The contact portion 33a is coupled to an inner surface of the battery housing 20. In the case where the beading portion 21 is formed on the battery housing 20, the contact portion 33a may be coupled to the beading portion 21 as described above. In this case, for stable contact and coupling, as described above, the beading portion 21 and the contact portion 33a may all extend in a direction substantially parallel to the lower surface of the battery housing 20, i.e., in a direction substantially perpendicular to the side wall of the battery housing 20.
[0121] 7, the connecting portion 33b may have at least one bent portion B where the extending direction is changed between the support portion 31 and the contact portion 33a. That is, the connecting portion 33b may have, for example, a spring-like structure or a bellows-like structure that can contract and expand within a certain range. This structure of the connecting portion 33b allows the contact portion 33a to be tightly attached onto the beading portion 21 during the process of housing the electrode assembly 300, to which the first current collecting plate 30 is coupled, into the battery housing 20, even if the height of the electrode assembly 300 varies within a certain range.
[0122] Although one bent portion B is provided in the drawing, the present invention is not limited to such an illustration, and it goes without saying that a plurality of bent portions B may be provided.
[0123] For example, it is preferable that the vertical distance (D) between the contact portion 33a and the support portion 31 in a state where no external force is applied to the first current collecting plate 30 and no deformation is the same as the vertical distance between the upper surface of the beading portion 21 and the support portion 31 when the electrode assembly 300 to which the first current collecting plate 30 is coupled is placed in the battery housing 20, or is formed to be smaller within the extensible range of the connecting portion 33b. If the connecting portion 33b is configured to satisfy this condition, the contact portion 33a is naturally brought into close contact with the beading portion 21 when the electrode assembly 300 to which the first current collecting plate 30 is coupled is placed in the battery housing 20.
[0124] Furthermore, the structure of the connecting part 33b, which can be contracted and expanded in this manner, can mitigate the impact caused by the movement of the electrode assembly 300 within a certain range even if vibrations and / or impacts occur during use of the cylindrical battery 1 (see Figure 5) and the electrode assembly 300 moves up and down.
[0125] Meanwhile, when the connecting portion 33b has only one bent portion B, the bent portion B may protrude in a direction toward the winding center of the electrode assembly 300, unlike the illustrated embodiment. The bending direction of the connecting portion 33b is to prevent the bonding portion between the first current collecting plate 30 and the electrode assembly 300 and / or the bonding portion between the first current collecting plate 30 and the battery housing 20 from being damaged during a sizing process. The sizing process is a compression process for reducing the height of the beading portion 21 area of the battery housing 20 in the manufacture of the cylindrical battery 1, thereby reducing the overall height of the cylindrical battery 1. As a result of checking the degree of damage to the welded portion after the sizing process by changing the formation of the bent portion B and the protruding direction of the bent portion B, it was confirmed that almost no damage occurred in the cylindrical battery 1 having a structure in which the connecting portion 33b is bent so that the bent portion B protrudes toward the center of the cylindrical battery 1.
[0126] 9, a first current collecting plate 30 according to another embodiment of the present invention is shown. The first current collecting plate 30 according to the other embodiment of the present invention differs from the first current collecting plate 30 of FIG. 8 described above only in the shape of the contact portion 33a, and otherwise the structure of the first current collecting plate 30 described above can be substantially similarly applied.
[0127] 9, the contact portion 33a may have a shape in which at least a portion thereof extends along the inner circumferential surface of the battery housing 20. For example, the contact portion 33a may have an arc shape extending along the beading portion 21. Also, although not shown, in order to maximize the contact area, the first current collecting plate 30 may be configured such that the sum of the extension lengths of the contact portions 33a of the respective housing coupling portions 33 is substantially equal to the inner circumferential surface of the battery housing 20. As a result, the coupling area is maximized, thereby improving the coupling force and reducing the electrical resistance.
[0128] 10, a first current collecting plate 30 according to yet another embodiment of the present invention is shown. The first current collecting plate 30 according to the still another embodiment of the present invention is different from the first current collecting plate 30 of FIG 9 only in the shape of the connecting portion 33b, and otherwise the structure of the first current collecting plate 30 described above can be substantially similarly applied.
[0129] 10, the connecting portion 33b may have a shape in which at least a portion extends along an inner peripheral surface of the battery housing 20. For example, the contact portion 33a may have an arc shape extending along the beading portion 21 of the battery housing, and the connecting portion 33b may have an arc shape extending along the contact portion 33a. With this structure, the area of the first current collecting plate 30 is further increased compared to the first current collecting plate 30 shown in FIG 9, thereby maximizing the effect of reducing electrical resistance.
[0130] Meanwhile, referring to Fig. 10, the first current collecting plate 30 may not have the bent portion B, unlike the first current collecting plate 30 shown in Fig. 8 or 9. When the bent portion B is not provided, it is possible to reduce raw materials required for manufacturing the first current collecting plate 30. As a result, it is possible to reduce the manufacturing cost of the first current collecting plate 30.
[0131] Referring to FIG. 5, the cap plate 40 covers the opening formed on one side of the battery housing 20. When the battery housing 20 according to the embodiment of the present invention includes a beading portion 21, the cap plate 40 may be placed on the beading portion 21 formed on the battery housing 20. When the battery housing 20 according to the embodiment of the present invention includes a crimping portion 22, the cap plate 40 may be fixed by the crimping portion 22. In this case, a sealing gasket G1 may be interposed between the battery housing 20 and the cap plate 40 to improve the fixing force and the sealing performance of the battery housing 20. However, in the embodiment of the present invention, the cap plate 40 is not a part that functions as a current path. Therefore, as long as the battery housing 20 and the cap plate 40 are firmly fixed to each other through welding or fixing by applying other parts, and the sealing performance of the opening of the battery housing 20 can be ensured, the application of the sealing gasket G1 is not essential.
[0132] The cap plate 40 may be made of, for example, a metal material to ensure rigidity. In the cylindrical battery 1 according to an embodiment of the present invention, the cap plate 40 has no polarity even when made of a conductive metal material. Having no polarity means that the cap plate 40 is electrically insulated from the battery housing 20 and a battery terminal 60, which will be described later. Thus, the cap plate 40 does not function as a positive or negative terminal. Thus, the cap plate 40 does not need to be electrically connected to the electrode assembly 300 and the battery housing 20, and the material thereof does not necessarily need to be a conductive metal.
[0133] Meanwhile, in the case where the sealing gasket G1 is applied, the sealing gasket G1 may be substantially ring-shaped to enclose the cap plate 40. The sealing gasket G1 may cover the upper surface, the lower surface, and the side surface of the cap plate 40 at the same time. The radial length of the portion of the sealing gasket G1 covering the lower surface of the cap plate 40 may be shorter than or equal to the radial length of the portion of the sealing gasket G1 covering the upper surface of the cap plate 40. If the radial length of the portion of the sealing gasket G1 covering the lower surface of the cap plate 40 is too long, the sealing gasket G1 may press the first current collecting plate 30 during the process of compressing the battery housing 20 vertically, which may damage the first current collecting plate 30 or the battery housing 20. Therefore, it is necessary to maintain the radial length of the portion of the sealing gasket G1 covering the lower surface of the cap plate 40 small at a certain level. For example, as shown in Fig. 5, the radial length of the portion of the sealing gasket G1 covering the lower surface of the cap plate 40 may be smaller than the radial length of the portion of the sealing gasket G1 covering the upper surface of the cap plate 40. Alternatively, as shown in Figs. 6 and 7, the radial length of the portion of the sealing gasket G1 covering the lower surface of the cap plate 40 may be the same as the radial length of the portion of the sealing gasket G1 covering the upper surface of the cap plate 40.
[0134] Meanwhile, the contact portion 33a may be fixed by being interposed between the beading portion 21 and the sealing gasket G1. That is, the contact portion 33a may be fixed by the crimping force of the crimping portion 22 in a state where the contact portion 33a is interposed between the beading portion 21 and the sealing gasket G1.
[0135] Alternatively, a welded portion may be formed between the beading portion 21 and the contact portion 33a. For example, the contact portion 33a may not be reliably fixed by the crimping force alone. Alternatively, if the sealing gasket G1 is shrunk by heat or the crimping portion 22 is deformed by an external impact, the bonding force between the current collector plate and the battery housing 20 may be reduced. Therefore, the first current collector plate 30 may be fixed to the battery housing 20 by welding while the contact portion 33a is placed on the beading portion 21. Then, a cap plate covered with the sealing gasket G1 is placed on the contact portion 33a, and the crimping portion 22 is formed, thereby completing the cylindrical battery 1. At this time, the welding method may be, for example, laser welding, resistance welding, ultrasonic welding, or the like, but is not limited thereto.
[0136] Meanwhile, the cap plate 40 may have a venting portion 41 formed to prevent an increase in internal pressure due to gas generated inside the battery housing 20. The venting portion 41 is formed in a part of the cap plate 40 and corresponds to a region structurally weaker than the surrounding region so as to be easily broken when pressure is applied. The venting portion 41 may be a region having a smaller thickness than the surrounding region. Therefore, if an abnormality occurs in the cylindrical battery 1 and the internal pressure of the battery housing 20 increases above a certain level, the venting portion 41 breaks to discharge the gas generated inside the battery housing 20. The venting portion 41 may be formed by, for example, notching one or both sides of the cap plate 40 to partially reduce the thickness of the battery housing 20.
[0137] The battery terminal 60 is electrically connected to the second electrode tab 12. The battery terminal 60 may be electrically connected to the second electrode tab 12 of the electrode assembly 300 by penetrating the battery housing 20 from the opposite side of the opening of the battery housing 20. The battery terminal 60 may penetrate approximately the center of the lower surface of the battery housing 20. A portion of the battery terminal 60 may be exposed to the outside of the battery housing 20, and the remaining portion may be located inside the battery housing 20. The battery terminal 60 may be electrically connected to the electrode assembly 300 by, for example, being coupled to a second current collecting plate P coupled to the second electrode tab 12 described below, or by being coupled to a lead tab (not shown) coupled to the second electrode tab 12. Therefore, the battery terminal 60 has the same polarity as the second electrode of the electrode assembly 300 and may function as a second electrode terminal T2. When the second electrode tab 12 is a positive electrode tab, the battery terminal 60 functions as a positive electrode terminal.
[0138] Considering the polarity and function of the battery terminal 60, the battery terminal 60 must maintain an insulated state from the battery housing 20 having the opposite polarity. For this reason, an insulating gasket G2 may be applied between the battery terminal 60 and the battery housing 20. Alternatively, insulation may be achieved by coating a part of the surface of the battery terminal 60 with an insulating material. Alternatively, the battery terminal 60 may be disposed at a distance from the battery housing 20 so that they cannot come into contact with each other, and the battery terminal 60 may be structurally and firmly fixed. Alternatively, a combination of two or more of the above-mentioned methods may be applied.
[0139] That is, the cylindrical battery 1 according to one embodiment of the present invention has a structure in which a pair of electrode terminals (battery terminal 60, first electrode terminal T1) are located in the same direction. Therefore, when a plurality of cylindrical batteries 1 are electrically connected, an electrical connection part such as a bus bar can be disposed only on one side of the cylindrical battery 1. This can simplify the battery pack structure and improve the energy density. In addition, the cylindrical battery 1 has a structure in which one surface of the battery housing 20 having a substantially flat shape can be used as the first electrode terminal T1, so that a sufficient joining area can be secured when joining an electrical connection part such as a bus bar to the first electrode terminal T1. As a result, the cylindrical battery 1 can secure sufficient joining strength between the electrical connection part and the first electrode terminal T1, and the resistance at the joining portion can be reduced to a preferable level.
[0140] Meanwhile, when the insulating gasket G2 is applied for electrical insulation and riveting is applied for fixing the battery terminal 60, the insulating gasket G2 may be deformed together with the battery terminal 60 when the battery terminal 60 is riveted, and may be bent toward the inner surface of the upper end closure of the battery housing 20. When the insulating gasket G2 is made of a resin material, the insulating gasket G2 may be bonded to the battery housing 20 and the battery terminal 60 by thermal fusion. In this case, the airtightness at the bonding interface between the insulating gasket G2 and the battery terminal 60 and at the bonding interface between the insulating gasket G2 and the battery housing 20 is enhanced.
[0141] In one embodiment of the present invention, the entire surface of the battery housing 20 can function as the first electrode terminal T1. For example, when the first electrode tab 11 is a negative electrode tab, the first electrode terminal T1 can be a negative electrode terminal. The cylindrical battery 1 according to the embodiment of the present invention has a structure in which the battery terminal 60 exposed on the lower surface located opposite the open portion of the battery housing 20 is used as the second electrode terminal T2, and the other area of the lower surface of the battery housing 20 excluding the area occupied by the battery terminal 60 is used as the first electrode terminal T1. Therefore, when a plurality of cylindrical batteries 1 are electrically connected, the cylindrical battery 1 according to the embodiment of the present invention can connect all the positive and negative electrodes in one direction, simplifying the electrical connection structure. In addition, the cylindrical battery 1 according to the embodiment of the present invention has a structure in which most of the lower surface located opposite the open portion of the battery housing 20 can be used as an electrode terminal, and therefore has an advantage in that a sufficient area can be secured for welding parts for electrical connection.
[0142] Preferably, the cylindrical battery may be, for example, a cylindrical battery having a form factor ratio (defined as the diameter divided by the height of a cylindrical battery, i.e., the ratio of height (H) to diameter (Φ)) greater than about 0.4.
[0143] Here, the form factor refers to a value indicating the diameter and height of a cylindrical battery. A cylindrical battery according to an embodiment of the present invention may be, for example, a 46110 battery, a 48750 battery, a 48110 battery, a 48800 battery, or a 46800 battery. In the value indicating the form factor, the first two digits indicate the diameter of the battery, the next two digits indicate the height of the battery, and the last digit 0 indicates that the cross section of the battery is circular.
[0144] A battery according to one embodiment of the present invention may be a generally cylindrical battery having a diameter of about 46 mm, a height of about 110 mm, and a form factor ratio of about 0.418.
[0145] Another embodiment of the battery may be a generally cylindrical battery having a diameter of about 48 mm, a height of about 75 mm, and a form factor ratio of about 0.640.
[0146] In yet another embodiment, the battery may be a generally cylindrical battery having a diameter of about 48 mm, a height of about 110 mm, and a form factor ratio of about 0.418.
[0147] In yet another embodiment, the battery may be a generally cylindrical battery having a diameter of about 48 mm, a height of about 80 mm, and a form factor ratio of about 0.600.
[0148] In yet another embodiment, the battery may be a generally cylindrical battery having a diameter of about 46 mm, a height of about 80 mm, and a form factor ratio of about 0.575.
[0149] Conventionally, batteries with a form factor ratio of about 0.4 or less have been used. That is, conventionally, for example, 18650 batteries, 21700 batteries, etc. have been used. In the case of the 18650 battery, the diameter is about 18 mm, the height is about 65 mm, and the form factor ratio is about 0.277. In the case of the 21700 battery, the diameter is about 21 mm, the height is about 70 mm, and the form factor ratio is about 0.300.
[0150] Hereinafter, the cylindrical battery 1 described above will be described in more detail with reference to Figs. 11 to 19. In the following description, there may be other embodiments that can be selectively applied in the description of the same components as those described above. Also, in the following description, some descriptions may overlap with those described above.
[0151] 12, 13, 16 and 17, the electrode assembly 300 includes a first electrode tab 11 and a second electrode tab 12. The first electrode tab 11 is provided at a lower part in a height direction (Z-axis direction) of the electrode assembly 300 accommodated in the battery housing 20. The second electrode tab 12 is provided at an upper part in a height direction (Z-axis direction) of the electrode assembly 300 accommodated in the battery housing 20.
[0152] 11, 12, 13 and 16, the battery housing 20 can accommodate the electrode assembly 300 through an opening formed at its lower end. The battery housing 20 is a substantially cylindrical container having an opening formed at its lower end and a closed portion formed at its upper end.
[0153] 12 and 13, the battery housing 20 may include a beading portion 21 and a crimping portion 22 formed at a lower end thereof. The beading portion 21 may be located below the electrode assembly 300 accommodated inside the battery housing 20. The beading portion 21 may be formed by pressing around the outer circumferential surface of the battery housing 20. The beading portion 21 partially reduces the inner diameter of the battery housing 20, thereby preventing the electrode assembly 300, which has a size substantially corresponding to the width of the battery housing 20, from slipping out of an opening formed at the lower end of the battery housing 20, and may also function as a support on which a cap plate 40 is placed.
[0154] The crimping portion 22 is formed below the beading portion 21. The crimping portion 22 may be extended and bent to enclose the peripheral portion of the cap plate 40 with the peripheral portion of the sealing spacer 50 interposed therebetween.
[0155] 12, 13 and 15, the cap plate 40 may cover an opening formed in the battery housing 20. The cap plate 40 may form a lower surface of the cylindrical battery 1.
[0156] 13 and 15, it is preferable that the lower end of the cap plate 40 is located higher than the lower end of the battery housing 20. In this case, even if the lower end of the battery housing 20 contacts the ground or the bottom of a housing for configuring a module or pack, the cap plate 40 does not contact the ground or the bottom of the housing. Therefore, it is possible to prevent a phenomenon in which the pressure required to break the venting portion 41 varies from a designed value due to the weight of the cylindrical battery 1, and therefore it is possible to ensure smooth breaking of the venting portion 41.
[0157] On the other hand, when the venting portion 41 has a closed loop shape as shown in Figs. 13 and 15, the greater the distance from the center of the cap plate 40 to the venting portion 41, the greater the force acting on the venting portion 41 and the easier it is to break it when the same venting pressure is applied. Also, the greater the distance from the center of the cap plate 40 to the venting portion 41, the greater the ease of discharging the venting gas. From this perspective, it is advantageous for the venting portion 41 to be formed along the periphery of a substantially flat region protruding downward (downward with reference to Fig. 15) from the peripheral region of the cap plate 40.
[0158] 15 shows the venting portion 41 being continuously formed while drawing an approximately circular shape, but the present invention is not limited thereto. The venting portion 41 may be discontinuously formed while drawing an approximately circular shape on the cap plate 40, or may be formed in an approximately linear shape or other shapes.
[0159] 12, 13 and 14, the sealing spacer 50 is configured to prevent the movement of the electrode assembly 300 and to strengthen the sealing force of the battery housing 20. The sealing spacer 50 may include, for example, a movement prevention portion 51, a sealing portion 52, and a connecting portion 53. The movement prevention portion 51 is interposed between the first current collecting plate 30 and the cap plate 40. The movement prevention portion 51 may have a height corresponding to the distance between the first current collecting plate 30 and the cap plate 40. In this case, the movement prevention portion 51 can effectively prevent the electrode assembly 300 from moving within the battery housing 20 due to a clearance formed between the first current collecting plate 30 and the cap plate 40. Therefore, the movement prevention portion 51 can prevent damage from occurring to a coupling portion between the electrode assembly 300 and the first current collecting plate 30 and / or a coupling portion between the first current collecting plate 30 and the battery housing 20.
[0160] The motion prevention portion 51 may be located at a substantially central portion on the lower surface of the electrode assembly 300. The motion prevention portion 51 may include a spacer hole H3 formed at a position corresponding to the winding center hole H1 of the electrode assembly 300. The spacer hole H3 may function as a passage for inserting a welding rod or a passage for irradiating a laser, similar to the first current collecting plate hole H2 described above. The spacer hole H3 may also function as a passage for smooth electrolyte impregnation into the electrode assembly 300 when the electrolyte is injected, similar to the first current collecting plate hole H2 described above.
[0161] The sealing part 52 is interposed between the battery housing 20 and the cap plate 40. The sealing part 52 may have a shape extending along the periphery of the inner circumferential surface of the battery housing 20. When the battery housing 20 includes the crimping part 22, the sealing part 52 may be folded along the folded shape of the crimping part 22 to enclose the peripheral region of the cap plate 40. As such, the sealing part 52 may function as a gasket for improving the fixing force of the cap plate 40 and the sealing force of the battery housing 20. As such, when the cylindrical battery 1 according to the embodiment of the present invention includes the sealing spacer 50, the sealing part 52 of the sealing spacer 50 may replace the sealing gasket G1 shown in FIGS. 5 to 7.
[0162] The connecting part 53 connects between the movement prevention part 51 and the sealing part 52. The connecting part 53 may include, for example, a plurality of extension legs 53a extending radially from the movement prevention part 51. When the connecting part 53 is configured in this manner, the electrolyte can be smoothly injected through the space between the adjacent extension legs 53a, and the internal gas can be smoothly discharged when venting occurs due to an increase in internal pressure.
[0163] As shown in Figs. 13 and 14, the extension legs 53a may be configured not to contact the cap plate 40 and / or other parts of the housing coupling part 33 of the first current collector plate 30 except for the part inserted into the crimping part 22. For example, the connection part 53 may be positioned so as not to overlap the housing coupling part 33 along the height direction (Z-axis direction) of the cylindrical battery 1. In particular, when the extension legs 53a extend radially from the movement prevention part 51 and the housing coupling parts 33 extend radially from the support part 31, the extension legs 53a and the housing coupling parts 33 may be alternately positioned so as not to overlap each other in the vertical direction. In this case, even if a compressive force is applied to the battery housing 20 in the vertical direction to cause deformation of the parts, the possibility of interference between the extension legs 53a and the housing coupling part 33 is significantly reduced, and therefore the possibility of problems such as damage to the coupling parts between the parts can be significantly reduced.
[0164] In this case, even if the sealing spacer 50 is deformed due to a sizing process that compresses the cylindrical battery 1 along the height direction (Z-axis direction) or other reasons, interference between the connection part 53 of the sealing spacer 50 and the housing coupling part 33 of the first current collecting plate 30 can be minimized. In particular, when the extension leg 53a is configured not to come into contact with the cap plate 40, the possibility of the extension leg 53a being deformed can be reduced even if deformation occurs in the battery housing 20 due to the sizing process or external impact.
[0165] Meanwhile, each component constituting the sealing spacer 50 may be integrally formed. For example, the sealing spacer 50 may be manufactured by injection molding, in which the movement prevention part 51, the sealing part 52, and the connecting part 53 are integrated. That is, the cylindrical battery 1 according to the embodiment of the present invention can obtain the effect of strengthening the sealing force for the opening of the battery housing 20 and preventing the movement of the electrode assembly 300 through one part by modifying and manufacturing a gasket part used for sealing the opening of the battery housing 20. Therefore, according to one embodiment of the present invention, it is possible to prevent the complication of the manufacturing process and the increase in manufacturing costs caused by the application of additional parts.
[0166] 12, 16 and 17, the second current collecting plate P is coupled to the upper part of the electrode assembly 300. The second current collecting plate P is made of a metal material having electrical conductivity and is coupled to the second electrode tab 12. The coupling between the second electrode tab 12 and the second current collecting plate P may be performed by, for example, laser welding. Referring to FIG. 13, the second current collecting plate P may be coupled to a coupling surface formed by bending an end of the second electrode tab 12 in a direction parallel to the second current collecting plate P. The bending direction of the second electrode tab 12 may be, for example, a direction toward the winding center of the electrode assembly 300. When the second electrode tab 12 has such a bent shape, the space occupied by the second electrode tab 12 is reduced, thereby improving the energy density. In addition, the increase in the coupling area between the second electrode tab 12 and the second current collecting plate P may provide the effects of improving the coupling force and reducing the resistance. Meanwhile, the above-mentioned connection structure and connection method between the second electrode tab 12 and the second current collecting plate P can be similarly applied to the connection between the first electrode tab 11 and the first current collecting plate 30.
[0167] 12 and 16, the insulator S is interposed between a closing portion formed at the upper end of the battery housing 20 and the upper end of the electrode assembly 300, or between the closing portion and the second current collector plate P. The insulator S may be made of, for example, a resin material having insulating properties. The insulator S prevents contact between the electrode assembly 300 and the battery housing 20 and / or between the electrode assembly 300 and the second current collector plate P. To this end, the insulator S may be interposed between the second electrode tab 12 and the battery housing 20 and / or between the second current collector plate P and the battery housing 20. When the insulator S is applied, the battery terminal 60 may penetrate the insulator S for electrical connection with the second electrode tab 12.
[0168] The insulator S may also be interposed between an upper end of the outer circumferential surface of the electrode assembly 300 and the inner surface of the battery housing 20. In this case, it is possible to prevent the second electrode tab 12 of the electrode assembly 300 from coming into contact with the inner surface of the side wall of the battery housing 20, thereby preventing a short circuit from occurring.
[0169] The insulator S may have a height corresponding to the distance between a closing portion formed at the upper end of the battery housing 20 and the electrode assembly 300 or the distance between the closing portion and the second current collecting plate P. In this case, the electrode assembly 300 can be prevented from moving inside the battery housing 20, and thus the risk of damage to the coupling portions for electrical connection between the components can be significantly reduced. When the insulator S is applied together with the above-mentioned sealing spacer 50, the effect of preventing the electrode assembly 300 from moving can be maximized.
[0170] The insulator S may have an opening formed at a position corresponding to the winding center hole H1 of the electrode assembly 300. The battery terminal 60 may directly contact the second current collector P through the opening.
[0171] 18, a battery pack 3 according to an embodiment of the present invention includes the cylindrical battery 1 according to an embodiment of the present invention as described above. For convenience of illustration, components such as bus bars for electrical connections, a cooling unit, and power terminals are not shown.
[0172] 19, an automobile 5 according to an embodiment of the present invention may be, for example, an electric automobile, a hybrid automobile, or a plug-in hybrid automobile, and includes a battery pack 3 according to an embodiment of the present invention. The automobile 5 includes a four-wheeled automobile and a two-wheeled automobile. The automobile 5 operates by receiving a supply of power from the battery pack 3 according to an embodiment of the present invention.
[0173] Hereinafter, an embodiment of a positive electrode active material used in a cylindrical battery according to an embodiment of the present invention will be described.
[0174] In the embodiment, the term "primary particle" refers to a particle unit that does not have grain boundaries when observed at a magnification of 5,000 to 20,000 times using a scanning electron microscope (SEM) or an electron backscatter diffraction (EBSD) pattern analyzer. The term "average particle size of primary particles" refers to the arithmetic average value calculated after measuring the particle sizes of primary particles observed in an SEM or EBSD image.
[0175] The term "secondary particle" refers to a particle formed by agglomeration of a plurality of primary particles. In the present invention, a secondary particle formed by agglomeration of 10 or less primary particles is referred to as a pseudo-single particle in order to distinguish it from conventional secondary particles formed by agglomeration of tens to hundreds of primary particles.
[0176] In the present invention, the "specific surface area" is measured by the BET method, and specifically, can be calculated from the amount of nitrogen gas adsorbed at liquid nitrogen temperature (77K) using a Belsorp-mini II manufactured by Bel Japan.
[0177] In the present invention, "D min ", "D50 " and "D max " is the particle size value of the volume cumulative distribution of the positive electrode active material measured using a laser diffraction method. Specifically, D min is the minimum particle size in the cumulative volume distribution, and D 50 is the particle size when the cumulative volume is 50%, and D max is the maximum particle size in the volume cumulative distribution. When the positive electrode active material is a single particle, D 50 means the average particle size of the primary particles. In addition, when the positive electrode active material is a pseudo-single particle, D 50 means the average particle size of particles formed by agglomeration of primary particles.
[0178] The particle size value of the volume cumulative distribution can be measured, for example, by dispersing the positive electrode active material in a dispersion medium, introducing the dispersed material into a commercially available laser diffraction particle size measuring device (e.g., MT3000 manufactured by Microtrac), irradiating the dispersed material with ultrasonic waves of about 28 kHz at an output of 60 W, and then obtaining a volume cumulative particle size distribution graph.
[0179] In the present invention, "consist essentially of A" means that the composition includes the component A and any unmentioned components that do not substantially affect the basic and novel characteristics of the present invention. The basic and novel characteristics of the present invention include at least one of minimizing particle cracking during battery manufacturing, minimizing gas generation due to such particle cracking, and minimizing the occurrence of internal cracks. A person of ordinary skill in the art can recognize the material effects of such characteristics.
[0180] The present inventors have conducted extensive research to develop a positive electrode for an electrochemical device that achieves high capacity while being highly safe, and an electrochemical device including the same, and as a result, have confirmed that the safety of large cylindrical batteries can be dramatically improved when a single-particle positive electrode active material consisting of one primary particle or a pseudo-single-particle positive electrode active material that is an aggregate of 10 or less primary particles is used alone as the positive electrode active material.
[0181] According to one embodiment, the positive electrode includes a positive electrode current collector and a positive electrode active material layer formed on at least one side of the positive electrode current collector. The positive electrode active material layer may include a positive electrode active material and may optionally include a conductive material and / or a binder.
[0182] The positive electrode may have a structure in which a positive electrode active material layer is formed on at least one surface or both surfaces of a long sheet-shaped positive electrode current collector, and the positive electrode active material layer may include a positive electrode active material and a binder.
[0183] Specifically, the positive electrode may be manufactured by coating one or both sides of a long sheet-shaped positive electrode current collector with a positive electrode slurry prepared by dispersing a positive electrode active material, a conductive material, and a binder in a solvent such as dimethyl sulfoxide (DMSO), isopropyl alcohol, N-methylpyrrolidone (NMP), acetone, water, etc., and then removing the solvent of the positive electrode slurry through a drying process, followed by rolling. Meanwhile, a positive electrode including a non-coated portion (uncoated portion) may be manufactured by not coating a portion of the positive electrode current collector, for example, one end of the positive electrode current collector, with the positive electrode slurry when coating the positive electrode slurry.
[0184] In another embodiment, the positive electrode active material includes single-particle active material particles. In one embodiment, the single-particle active material particles may be included in an amount of 90 wt% or more, 95 wt% or more, 98 wt% or more, or 99 wt% or more, based on 100 wt% of the positive electrode active material. In a specific embodiment, the positive electrode active material may be composed only of the single-particle active material particles.
[0185] In this specification, the single particle active material particles refer to single particles, pseudo-single particles, or both. The single particles are particles consisting of one primary particle, and the pseudo-single particles are aggregates of 10 or less primary particles.
[0186] Conventionally, as the positive electrode active material of a lithium battery, spherical secondary particles formed by agglomeration of tens to hundreds of primary particles are generally used. However, in the case of a positive electrode active material in the form of secondary particles formed by agglomeration of many primary particles, there is a problem that the primary particles are easily broken during the rolling process in the manufacture of the positive electrode, and cracks are generated inside the particles during charging and discharging. When the particle breakage or cracks occur in the positive electrode active material, the contact area with the electrolyte increases, and gas generation due to a side reaction with the electrolyte increases. If gas generation increases inside a cylindrical battery, the internal pressure of the battery increases, and there is a risk of the battery exploding. In particular, when the volume of a cylindrical battery is increased, the amount of active material inside the battery increases due to the increase in volume, and the amount of gas generation also increases significantly, so the risk of the battery catching fire and / or exploding becomes even greater.
[0187] On the other hand, single particle active material particles consisting of one primary particle or pseudo single particle form consisting of an aggregation of 10 or less primary particles have higher particle strength than conventional positive electrode active material in the form of secondary particles consisting of aggregation of tens to hundreds of primary particles, and therefore hardly crack during rolling. Also, in the case of single particle active material particles, the number of primary particles constituting the particle is small, so there is little change due to the volume expansion and contraction of the primary particles during charging and discharging, and therefore the occurrence of cracks inside the particles is significantly reduced.
[0188] Therefore, when using single particle type active material particles as in one embodiment of the present invention, the amount of gas generation due to particle breakage and internal cracks can be significantly reduced, thereby achieving excellent safety when applied to large cylindrical batteries.
[0189] On the other hand, the monoparticles and / or pseudo monoparticles are preferably contained in an amount of 95 wt% to 100 wt%, preferably 98 wt% to 100 wt%, more preferably 99 wt% to 100 wt%, and even more preferably 100 wt%, based on the weight of the entire positive electrode active material contained in the positive electrode.
[0190] When the content of the single particles and / or quasi-single particles is within the above range, sufficient safety can be obtained when applied to large batteries. When the secondary particle type positive electrode active material is contained in an amount exceeding 5 wt% of the total positive electrode active material, fine powder generated from the secondary particles during the manufacture and charging / discharging of the electrode increases side reactions with the electrolyte, reducing the effect of suppressing gas generation, and thus reducing the effect of improving stability when applied to large batteries.
[0191] Meanwhile, the positive electrode active material including the single particle and / or the pseudo-single particle according to one embodiment of the present invention is D min may be 1.0 μm or more, 1.1 μm or more, 1.15 μm or more, 1.2 μm or more, 1.25 μm or more, 1.3 μm or more, or 1.5 μm or more. min If the thickness is less than 1.0 μm, the line pressure increases during the rolling process of the positive electrode, which makes it easy for particle cracks to occur, and the thermal stability decreases, making it impossible to ensure sufficient thermal stability when applied to a large cylindrical battery.
[0192] On the other hand, considering the resistance and output characteristics, the D min may be 3 μm or less, 2.5 μm or less, or 2 μm or less. min If is too large, the diffusion distance of lithium ions within the particles increases, which may result in a decrease in resistance and output characteristics.
[0193] For example, D of the positive electrode active material min can be 1.0 μm to 3 μm, 1.0 μm to 2.5 μm, or 1.3 μm to 2.0 μm.
[0194] On the other hand, the positive electrode active material is D 50 The thickness may be 5 μm or less, 4 μm or less, or 3 μm or less, for example, from 0.5 μm to 5 μm, preferably from 1 μm to 5 μm, and more preferably from 2 μm to 5 μm.
[0195] A positive electrode active material in the form of a single particle and / or a pseudo single particle has a problem that the mobility of lithium is lower than that of a positive electrode active material in the form of a secondary particle because there are fewer interfaces between the primary particles that serve as diffusion paths for lithium ions inside the particle, and therefore the resistance increases. This increase in resistance becomes more severe as the particle size increases, and the increased resistance has a negative effect on the capacity and output characteristics. Therefore, the D of the positive electrode active material 50 By adjusting the particle size to 5 μm or less, the diffusion distance of lithium ions inside the particles of the positive electrode active material can be minimized, thereby suppressing an increase in resistance.
[0196] The positive electrode active material is D max The D of the positive electrode active material may be 12 μm to 17 μm, preferably 12 μm to 16 μm, and more preferably 12 μm to 15 μm. max If satisfies the above range, the resistance characteristic and the capacity characteristic are further excellent. max If the D of the positive electrode active material is too large, the lithium migration path inside the aggregated particles becomes longer and the lithium mobility decreases, which may increase the resistance. max If is too small, excessive crushing has occurred, and excessive crushing has caused D min The grain size may be as small as less than 1 μm, which may induce grain cracking during rolling and reduce thermal stability.
[0197] Meanwhile, the positive electrode active material may have a particle size distribution (PSD) represented by the following mathematical formula 1 of 3 or less, preferably 2 to 3, and more preferably 2.3 to 3.
[0198] [Formula 1] Particle size distribution (PSD)=(D max -D min ) / D 50 When the positive electrode active material has the above particle size distribution, the electrode density of the positive electrode can be appropriately maintained, and particle cracking and an increase in resistance can be effectively suppressed.
[0199] On the other hand, the positive electrode active material may have an average particle size of 5 μm or less, 4 μm or less, 3 μm or less, or 2 μm or less, for example, 0.5 μm to 5 μm, preferably 1 μm to 5 μm, and more preferably 2 μm to 5 μm. When the average particle size of the primary particles satisfies the above range, it is possible to form a positive electrode active material in the form of a single particle and / or a pseudo single particle having excellent electrochemical properties. If the average particle size of the primary particles is too small, the number of agglomerates of the primary particles forming the positive electrode active material increases, and the effect of suppressing the occurrence of particle cracking during rolling may decrease. In addition, if the average particle size of the primary particles is too large, the lithium diffusion path inside the primary particles may become long, increasing the resistance and decreasing the output characteristics.
[0200] In one embodiment of the present invention, the positive electrode active material preferably has a unimodal particle size distribution. In the past, bimodal positive electrode active materials, which are a mixture of a large particle size positive electrode active material having a large average particle size and a small particle size positive electrode active material having a small average particle size, have been widely used to improve the electrode density of the positive electrode active material layer. However, in the case of a positive electrode active material having a single particle or pseudo single particle form, as the particle size increases, the lithium migration path becomes longer and the resistance increases significantly, so that when large particle size particles are mixed, there is a risk of a problem of a decrease in capacity and output characteristics. Therefore, in the present invention, a positive electrode active material having a unimodal distribution is used to minimize the increase in resistance.
[0201] Meanwhile, the positive electrode active material may include a lithium nickel-based oxide, specifically, a lithium nickel-based oxide containing 80 mol% or more of Ni based on the total mole number of transition metals. Preferably, the lithium nickel-based oxide may contain 80 mol% or more and less than 100 mol%, 82 mol% or more and less than 100 mol%, or 83 mol% or more and less than 100 mol% of Ni. When a lithium nickel-based oxide having a high Ni content is used as described above, a high capacity can be achieved.
[0202] More specifically, the positive electrode active material may include a lithium nickel-based oxide represented by the following Chemical Formula 1:
[0203] [Chemical formula 1] Li a Ni b Co c M 1 d M 2 e O2 In Chemical Formula 1, the M 1 can be Mn, Al or a combination thereof, preferably Mn, or Mn and Al.
[0204] Said M 2 is at least one selected from the group consisting of Zr, W, Y, Ba, Ca, Ti, Mg, Ta and Nb, preferably at least one selected from the group consisting of Zr, Y, Mg and Ti, more preferably Zr, Y or a combination thereof. 2 Although the elements are not essential, when contained in an appropriate amount, they can play a role in promoting particle growth during firing or improving the stability of the crystal structure.
[0205] The a represents the lithium molar ratio in the lithium nickel-based oxide, and may be 0.8≦a≦1.2, 0.85≦a≦1.15, or 0.9≦a≦1.2. When the lithium molar ratio satisfies the above range, the crystal structure of the lithium nickel-based oxide can be stably formed.
[0206] The b represents a molar ratio of nickel in all metals excluding lithium in the lithium nickel-based oxide, and may be 0.8≦b<1, 0.82≦b<1, 0.83≦b<1, 0.85≦b<1, 0.88≦b<1, or 0.90≦b<1. When the nickel molar ratio satisfies the above range, a high energy density is exhibited and a high capacity can be achieved.
[0207] Said c represents the molar ratio of cobalt in the total metal excluding lithium in the lithium nickel-based oxide, and can be 0 < c < 0.2, 0 < c < 0.18, 0.01 ≤ c ≤ 0.17, 0.01 ≤ c ≤ 0.15, 0.01 ≤ c ≤ 0.12, or 0.01 ≤ c ≤ 0.10. When the molar ratio of cobalt satisfies the above range, good resistance characteristics and output characteristics can be realized.
[0208] Said d represents the molar ratio of element M in the total metal excluding lithium in the lithium nickel-based oxide 1 and can be 0 < d < 0.2, 0 < d < 0.18, 0.01 ≤ d ≤ 0.17, 0.01 ≤ d ≤ 0.15, 0.01 ≤ d ≤ 0.12, or 0.01 ≤ d ≤ 0.10. When the molar ratio of element M 1 satisfies the above range, the structure stability of the positive electrode active material is excellent.
[0209] Said e represents the molar ratio of element M in the total metal excluding lithium in the lithium nickel-based oxide 2 and can be 0 ≤ e ≤ 0.1 or 0 ≤ e ≤ 0.05.
[0210] On the other hand, the positive electrode active material according to an embodiment of the present invention may further include, if necessary, a coating layer containing one or more coating elements selected from the group consisting of Al, Ti, W, B, F, P, Mg, Ni, Co, Fe, Cr, V, Cu, Ca, Zn, Zr, Nb, Mo, Sr, Sb, Bi, Si, and S on the surface of the lithium nickel-based oxide particles. Preferably, the coating element can be Al, B, Co, or a combination thereof.
[0211] When a coating layer exists on the surface of the lithium nickel-based oxide particles, the contact between the electrolyte and the lithium nickel-based oxide is suppressed by the coating layer, and thus the effect of reducing the elution of transition metals or gas generation due to side reactions with the electrolyte can be obtained.
[0212] The positive electrode active material may be contained in an amount of 80 wt % to 99 wt %, preferably 85 wt % to 99 wt %, and more preferably 90 wt % to 99 wt %, based on the total weight of the positive electrode active material layer.
[0213] Meanwhile, various positive electrode current collectors used in the art may be used as the positive electrode current collector. For example, stainless steel, aluminum, nickel, titanium, calcined carbon, aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. may be used as the positive electrode current collector. The positive electrode current collector may have a thickness of typically 3 μm to 500 μm, and fine irregularities may be formed on the surface of the positive electrode current collector to enhance the adhesive strength of the positive electrode active material. The positive electrode current collector may be used in various forms, such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.
[0214] Meanwhile, in one embodiment of the present invention, the single particle active material particles may have a core-shell structure in which the surface of the particle is covered with a conductive coating layer. The conductive coating layer may cover at least a part or the entire particle. The conductive coating layer may include a conductive nano-material.
[0215] The single particle active material particles have a problem of lowering electrical conductivity due to a higher resistance and a smaller contact area with the conductive material compared to conventional positive active materials in the form of secondary particles. If an excessive amount of conductive material is added to improve electrical conductivity, aggregation occurs in the positive electrode slurry, increasing the viscosity, and thus causing a problem of lowering the coating property. Therefore, in order to achieve smooth coating property, it is necessary to reduce the solid content to lower the viscosity of the positive electrode slurry, but if the solid content in the positive electrode slurry is reduced, the content of the active material is reduced, causing a problem of lowering the capacity characteristics. In order to solve this problem, the present invention coats the surface of the single particle active material particles with a conductive nanomaterial, thereby making it possible to achieve excellent electrical conductivity without adding a separate conductive material to the positive electrode slurry.
[0216] In an embodiment of the present invention, when a positive electrode active material in which a conductive nano material is coated on the surface of the single particle type active material particle is used, the positive electrode active material layer does not need to use a conductive material in a portion other than the conductive coating layer. Since there is no need to use an additional conductive material that induces agglomeration of the positive electrode slurry, the viscosity of the positive electrode slurry is reduced and the solid content is increased, thereby improving the processability of the electrode coating and the electrode adhesion.
[0217] In one embodiment of the present invention, the conductive nano-material may be a material having a nano-sized size so as to be smoothly coated on particles and having conductivity, and the type of the conductive nano-material is not particularly limited. For example, the conductive nano-material may be a carbon nanotube, a carbon nanoparticle, etc.
[0218] The conductive nano-materials may have various shapes, for example, spherical, scale-like, or fibrous.
[0219] Meanwhile, the conductive coating layer may be formed by mixing the single particle active material particles as the core part with the conductive nano material, followed by heat treatment. In this case, the mixing may be performed as a solid phase mixing or a liquid phase mixing.
[0220] In one embodiment of the present invention, the positive electrode active material layer includes flake graphite. When the positive electrode active material layer includes flake graphite in the case of using the single particle-based active material as the positive electrode active material, the flake graphite provides a slipping effect to the positive electrode active material when the positive electrode active material layer is rolled, thereby improving the rolling characteristics of the electrode and reducing the porosity of the electrode to a target level. As a result, the stability, initial resistance characteristics, and charge / discharge efficiency of a battery using the positive electrode according to one embodiment of the present invention can be improved.
[0221] In one embodiment of the present invention, the flake graphite may be included in an amount of 0.1 wt % to 5 wt %, and preferably 0.1 wt % to 3 wt %, relative to 100 wt % of the positive electrode active material layer.
[0222] When the content of flake graphite satisfies the above range, the rolling characteristics of the positive electrode are improved, and excellent electrode density can be achieved. If the content of flake graphite is low, the effect of improving the rolling characteristics is low, and if the content is excessive, it may induce an increase in slurry viscosity and a decrease in phase stability, and may decrease electrode uniformity and increase resistance due to binding with the conductive material.
[0223] On the other hand, the flake graphite used in the present invention may have an average particle size of 1 μm to 20 μm, preferably 2 μm to 10 μm, and more preferably 3 μm to 5 μm, but is not limited thereto. If the flake graphite is too small, it is difficult to achieve the desired porosity, and there is a risk that the current density will be lowered and the capacity will decrease. In this case, the average particle size of the flake graphite can be measured by a laser diffraction method (ISO 13320).
[0224] The flake graphite may have an aspect ratio of 0.1 to 500, preferably 1 to 100, and more preferably 1 to 30. When the aspect ratio of the flake graphite satisfies the above range, it has the effect of improving the electrical conductivity and reducing the electrode resistance.
[0225] The flake graphite has a density of 2.0 g / cm 3 ~2.5g / cm 3 , preferably 2.1 g / cm 3 ~2.4g / cm 3 , more preferably 2.2 g / cm 3 ~2.3g / cm 3 It could be.
[0226] Meanwhile, in one embodiment of the present invention, the porosity of the positive electrode active material layer may be 15% to 23%, preferably 17% to 23%, and more preferably 18% to 23%. When the porosity of the positive electrode active material layer satisfies the above range, the electrode density increases, excellent capacity can be realized, and resistance decreases. If the porosity is too low, the electrolyte impregnation property decreases, and lithium precipitation due to non-impregnation of the electrolyte may occur, and if the porosity is too high, the contact between the electrodes is poor, resistance increases, energy density decreases, and the effect of improving capacity is low.
[0227] The porosity value of the positive electrode active material layer can be achieved by i) the positive electrode active material including single-particle active material particles, and ii) adding flake graphite to the positive electrode active material.
[0228] When realizing a high loading electrode having a relatively high loading amount of the positive electrode active material layer, by using a positive electrode active material in the form of a single particle or pseudo-single particle as in one embodiment of the present invention, particle cracking of the active material during rolling is significantly reduced compared to conventional positive electrode active materials in the form of secondary particles, and damage to the positive electrode current collector (Aluminum foil) is reduced, making it possible to roll at a relatively high linear pressure, and the porosity of the positive electrode active material layer is reduced to the above-mentioned numerical range, thereby increasing the energy density.
[0229] In addition, when flake graphite is included in the positive electrode active material layer as in one embodiment of the present invention, the flake graphite provides a slipping effect during rolling and can fill the voids in the positive electrode active material layer, so that the porosity of the positive electrode active material layer can be reduced to the above-mentioned numerical range.
[0230] The positive electrode has a loading of 570 mg / 25 cm 2 More than 600mg / 25cm 2 ~800g / 25m 2 , more preferably 600 mg / 25 cm 2 ~750mg / 25cm 2 Specifically, in the case of the lithium secondary battery according to an embodiment of the present invention, the rolling characteristics of the electrode are improved by using a positive electrode active material and flake graphite in the form of single particle and / or pseudo single particle, so that the loading amount of the positive electrode can be secured at a relatively high level, thereby achieving high capacity characteristics.
[0231] In one embodiment of the present invention, the positive electrode active material layer may further include a conductive material. The conductive material is used to impart conductivity to the electrode, and may be used without any particular limitation as long as it does not cause a chemical change inside the battery and has electrical conductivity. Specific examples include graphite such as natural graphite and artificial graphite; carbon-based materials such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, thermal black, carbon fiber, and carbon nanotubes; metal powder or metal fiber such as copper, nickel, aluminum, and silver; conductive whiskers such as zinc oxide and potassium titanate; conductive metal oxides such as titanium oxide; or conductive polymers such as polyphenylene derivatives, and the like. One of these may be used alone or a mixture of two or more of them may be used. The conductive material may be usually contained in an amount of 1 wt% to 30 wt%, preferably 1 wt% to 20 wt%, and more preferably 1 wt% to 10 wt% based on the total weight of the positive electrode active material layer.
[0232] In a specific embodiment according to an embodiment of the present invention, the conductive material may include carbon nanotubes.
[0233] In one embodiment of the present invention, the positive electrode active material may include, as a conductive material, multi-walled carbon nanotubes having a high specific surface area and a small wall number. The multi-walled carbon nanotubes may be included in an amount of 50 wt% or more, 70 wt% or more, 90 wt% or more, or 99 wt% or more, based on 100 wt% of the conductive material. In a specific embodiment of the present invention, the conductive material may be composed only of the multi-walled carbon nanotubes.
[0234] In one embodiment of the present invention, the multi-walled carbon nanotubes are 300 mm or longer. 2 / g~500m 2 / g. To distinguish this from the conventional technology, we call it the "new CNT."
[0235] Conventionally, the carbon nanotubes commonly used (conventional CNTs) have a BET specific surface area of 300 m 2The scanning electron microscope images and physical properties of the novel CNT used in the present invention (FIG. 20) and the conventional CNT (FIG. 21) are compared (FIG. 22) as follows.
[0236] As can be seen from the SEM image, the novel CNT applied in one embodiment of the present invention is of the bundled type and has a multi-wall structure, but has a higher BET, number of walls and a smaller diameter than conventional CNTs.
[0237] When using a positive electrode active material in the form of secondary particles, sufficient electrical conductivity can be achieved even if conventional CNTs are used at about 0.4 wt% to 0.6 wt%. However, in the case of a positive electrode active material in the form of single particle or pseudo single particle, the resistance is higher than that of a positive electrode active material in the form of conventional secondary particles, and the contact area with the conductive material is smaller, resulting in lower electrical conductivity. 2 To achieve sufficient electrical conductivity using conventional CNTs with less than 100 wt. / g, the content of the conductive material must be 0.9 wt.% or more.
[0238] 23 to 26 are graphs showing the sheet resistance and high-temperature life characteristics depending on the ratio of the conductive material when single particles or pseudo-single particles are used as the positive electrode active material.
[0239] From the graph, it can be seen that when single particles or pseudo-single particles are used as the positive electrode active material, the amount of conductive material used needs to be increased compared to when a conventional positive electrode active material in the form of secondary particles is used.
[0240] However, if the carbon nanotube content is increased to 0.9 wt% or more, aggregation occurs in the positive electrode slurry, increasing the viscosity and thus deteriorating the coating properties. Therefore, in order to achieve smooth coating properties, the solid content in the positive electrode slurry must be reduced to lower the viscosity of the positive electrode slurry, but if the solid content in the positive electrode slurry is reduced, the active material content is reduced, resulting in a problem of deteriorating capacity characteristics.
[0241] As a result of extensive research into solving such problems, the inventors have discovered that, in addition to the positive electrode active material, which is a single-particle active material particle, a conductive material having a BET specific surface area of 300 m 2 / g~500m 2 / g, it was confirmed that sufficient electrical conductivity can be secured even with a relatively small amount of carbon nanotubes, and therefore the slurry viscosity can be maintained low even if the solid content of the positive electrode slurry is formed high at about 70 wt% to 80 wt%.
[0242] Specifically, the carbon nanotubes used in the present invention have a BET specific surface area of 300 m 2 / g~500m 2 / g, preferably 300m 2 / g~450m 2 When the BET specific surface area satisfies the above range, sufficient electrical conductivity can be ensured even with a small amount of carbon nanotubes.
[0243] The carbon nanotube may be a multi-walled carbon nanotube having a wall number of 2-8, preferably 2-6, and more preferably 3-6.
[0244] The carbon nanotubes may have a diameter of 1 nm to 8 nm, preferably 3 nm to 8 nm, and more preferably 3 nm to 6 nm.
[0245] The carbon nanotubes may be contained in an amount of 0.7 wt% or less, preferably 0.3 wt% to 0.7 wt%, and more preferably 0.4 wt% to 0.6 wt% based on the total weight of the positive electrode active material layer. When the carbon nanotube content satisfies the above range, sufficient electrical conductivity can be achieved and the solid content in the positive electrode slurry can be maintained high, so that the positive electrode active material content in the positive electrode active material layer can be increased, thereby achieving excellent capacity characteristics.
[0246] The table shown in Figure 27 shows the BET specific surface area of 300 m 2 / g~500m2 / g carbon nanotubes (new CNTs) and a BET specific surface area of 200 m 2 / g or more 300m 2 The table compares the solid content, viscosity, resistance in the MP coating layer, and resistance in the MP interface layer of the positive electrode slurry when carbon nanotubes (conventional CNTs) with less than 1000 / g are used. The table shows that when the new CNTs are used, the viscosity is lower and electrical conductivity is superior, even when the solid content of the positive electrode slurry is high, compared to conventional CNTs.
[0247] The binder plays a role in improving the adhesion between the positive electrode active material particles and the adhesive strength between the positive electrode active material and the positive electrode current collector, and specific examples thereof include polyvinylidene fluoride (PVDF), vinylidene fluoride-hexafluoropropylene copolymer (PVDF-co-HFP), polyvinyl alcohol, polyacrylonitrile, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, polytetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene monomer (EPDM) rubber, sulfonated EPDM, styrene butadiene rubber (SBR), fluororubber, or various copolymers thereof, and one or more of these may be used alone or in combination. The binder may be contained in an amount of 1 wt% to 30 wt%, preferably 1 wt% to 20 wt%, more preferably 1 wt% to 10 wt%, based on the total weight of the positive electrode active material layer.
[0248] Another embodiment of the present invention relates to an electrode assembly including the positive electrode, and a battery including the same. The electrode assembly includes a negative electrode and a positive electrode, and the positive electrode has the structural characteristics as described above.
[0249] The electrode assembly can be laminated, for example, with a separator interposed between the negative electrode and the positive electrode to form a laminated or laminated / folded structure, or can be wound to form a jelly roll type structure. When forming a jelly roll type structure, a separator can be further disposed on the outside to prevent contact between the negative electrode and the positive electrode.
[0250] The negative electrode includes a negative electrode current collector and a negative electrode active material layer formed on at least one surface of the negative electrode current collector. The negative electrode can have a structure in which a negative electrode active material layer is formed on one or both surfaces of a long sheet-like negative electrode current collector, and the negative electrode active material layer can include a negative electrode active material, a conductive material, and a binder.
[0251] Specifically, the negative electrode can be manufactured by applying a negative electrode slurry prepared by dispersing a negative electrode active material, a conductive material, and a binder in a solvent such as dimethyl sulfoxide (DMSO), isopropyl alcohol, N-methylpyrrolidone (NMP), acetone, water, etc. on one or both surfaces of a long sheet-like negative electrode current collector, removing the solvent of the negative electrode slurry through a drying process, and then rolling. When applying the negative electrode slurry, a negative electrode without a coating can be manufactured by not applying the negative electrode slurry to a partial region of the negative electrode current collector, for example, one end of the negative electrode current collector.
[0252] As the negative electrode active material, a compound capable of reversible intercalation and deintercalation of lithium can be used. Specific examples include carbonaceous materials such as artificial graphite, natural graphite, graphitized carbon fiber, and amorphous carbon; silicon-based materials such as Si, Si-Me alloy (where Me is one or more selected from the group consisting of Al, Sn, Mg, Cu, Fe, Pb, Zn, Mn, Cr, Ti, and Ni), SiO y (where 0 < y < 2), Si-C composites, etc.; lithium metal thin films; metal materials capable of alloying with lithium such as Sn, Al, etc.; and any one or a mixture of two or more of these can be used.
[0253] In one embodiment of the present invention, the negative electrode may contain a silicon-based negative electrode active material. The silicon-based negative electrode active material may be Si, Si-Me alloy (where Me is one or more selected from the group consisting of Al, Sn, Mg, Cu, Fe, Pb, Zn, Mn, Cr, Ti, and Ni), SiO y (where 0 < y < 2), a Si-C composite, or a combination thereof, preferably SiO y (where 0 < y < 2). Since the silicon-based negative electrode active material has a high theoretical capacity, when the silicon-based negative electrode active material is included, the capacity characteristics can be improved.
[0254] The silicon-based negative electrode active material may be doped with M b metal. At this time, the M b metal may be a Group 1 metal element or a Group 2 metal element, specifically, Li, Mg, etc. Specifically, the silicon-based negative electrode active material may be Si doped with M b metal, SiO y (where 0 < y < 2), a Si-C composite, etc. In the case of a metal-doped silicon-based negative electrode active material, although the active material capacity decreases somewhat due to the doping element, it has high efficiency, so a high energy density can be realized.
[0255] Figure 44 is a graph showing the change in energy density according to the content of the silicon-based negative electrode active material and the presence or absence of doping of the silicon-based negative electrode active material in a battery using a mixture of the silicon-based negative electrode active material and the carbon-based negative electrode active material as the negative electrode active material.
[0256] In Figure 44, low-efficiency SiO is undoped SiO, and ultra-high-efficiency SiO means Mg / Li-doped SiO. From Figure 44, it can be confirmed that the energy density improves as the content of the silicon-based negative electrode active material in the total negative electrode active material increases. Also, it can be confirmed that the improvement effect of the energy density is more excellent as the ratio of the doped silicon-based negative electrode active material in the silicon-based negative electrode active material increases.
[0257] The silicon-based negative active material may further include a carbon coating layer on the surface of the particles. In this case, the amount of the carbon coating may be 20 wt% or less, preferably 1 to 20 wt%, based on the total weight of the silicon-based negative active material. The carbon coating layer may be formed by a method such as dry coating, wet coating, chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), etc.
[0258] In one embodiment of the present invention, the silicon-based negative electrode active material may have a capacity of 1,000 to 4,000 mAh / g and an initial efficiency of about 60 to 95%.
[0259] In another embodiment of the present invention, the silicon-based negative electrode active material D 50 can be 3 μm to 8 μm, and D min ~D max can be in the range of 0.5 μm to 30 μm.
[0260] The negative electrode may further include a carbon-based negative electrode active material as a negative electrode active material, if necessary. The carbon-based negative electrode active material may be, for example, artificial graphite, natural graphite, graphitized carbon fiber, amorphous carbon, soft carbon, hard carbon, etc., but is not limited thereto.
[0261] When a mixture of a silicon-based negative electrode active material and a carbon-based negative electrode active material is used as the negative electrode active material, the mixing ratio of the silicon-based negative electrode active material to the carbon-based negative electrode active material may be 1:99 to 20:80, preferably 1:99 to 15:85, and more preferably 1:99 to 10:90, by weight.
[0262] The negative electrode active material may be contained in an amount of 80 wt % to 99 wt %, preferably 85 wt % to 99 wt %, and more preferably 90 wt % to 99 wt %, based on the total weight of the negative electrode active material layer.
[0263] If necessary, the negative electrode active material may further include at least one selected from lithium metal and metal materials capable of being alloyed with lithium, such as Sn and Al.
[0264] The negative electrode current collector may be a negative electrode current collector generally used in the art, for example, copper, stainless steel, aluminum, nickel, titanium, calcined carbon, copper or stainless steel surface treated with carbon, nickel, titanium, silver, aluminum-cadmium alloy, etc. The negative electrode current collector may have a thickness of typically 3 μm to 500 μm, and like the positive electrode current collector, the surface of the current collector may be formed with fine irregularities to enhance the binding force of the negative electrode active material. For example, the negative electrode current collector may be used in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.
[0265] The conductive material is used to impart conductivity to the negative electrode, and can be used without any particular limitation as long as it does not cause a chemical change inside the battery and has electrical conductivity. Specific examples of the conductive material include graphite such as natural graphite and artificial graphite; carbon-based materials such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, thermal black, carbon fiber, and carbon nanotubes; metal powder or metal fiber such as copper, nickel, aluminum, and silver; conductive whiskers such as zinc oxide and potassium titanate; conductive metal oxides such as titanium oxide; and conductive polymers such as polyphenylene derivatives, and one of these may be used alone or a mixture of two or more of them may be used. The conductive material may usually be contained in an amount of 1 wt% to 30 wt%, preferably 1 wt% to 20 wt%, and more preferably 1 wt% to 10 wt% based on the total weight of the negative electrode active material layer.
[0266] The binder plays a role in improving the adhesion between the negative electrode active material particles and the adhesive strength between the negative electrode active material and the negative electrode current collector. Specific examples of the binder include polyvinylidene fluoride (PVDF), vinylidene fluoride-hexafluoropropylene copolymer (PVDF-co-HFP), polyvinyl alcohol, polyacrylonitrile, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, polytetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene monomer (EPDM) rubber, sulfonated EPDM, styrene butadiene rubber (SBR), fluororubber, or various copolymers thereof, and one or more of these may be used alone or in combination. The binder may be included in an amount of 1 wt% to 30 wt%, preferably 1 wt% to 20 wt%, more preferably 1 wt% to 10 wt%, based on the total weight of the negative electrode active material layer.
[0267] The electrode assembly further includes a separator disposed between the negative electrode and the positive electrode, and the separator separates the negative electrode and the positive electrode and provides a path for lithium ions to move. Any separator generally used as a separator in lithium batteries may be used without any particular limitation.
[0268] The separator may be a porous polymer film, for example, a porous polymer film made of a polyolefin polymer such as an ethylene homopolymer, a propylene homopolymer, an ethylene / butene copolymer, an ethylene / hexene copolymer, or an ethylene / methacrylate copolymer, or a laminate structure of two or more layers thereof. Also, a conventional porous nonwoven fabric, for example, a nonwoven fabric made of a high melting point glass fiber, a polyethylene terephthalate fiber, or the like, may be used. Also, a coated separator containing a ceramic component or a polymeric material may be used to ensure heat resistance or mechanical strength.
[0269] Another embodiment of the present invention relates to a battery including the electrode assembly. The battery includes an electrode assembly and an electrolyte housed together in a battery case. The battery case may be a pouch type or a metal can type, or any other type commonly used in the art, and may be appropriately selected without any particular limitation.
[0270] The electrolyte used in the present invention may be any of various electrolytes that can be used in lithium batteries, such as organic liquid electrolytes, inorganic liquid electrolytes, solid polymer electrolytes, gel-type polymer electrolytes, solid inorganic electrolytes, and molten inorganic electrolytes, and is not particularly limited in type.
[0271] Specifically, the electrolyte may include an organic solvent and a lithium salt.
[0272] The organic solvent may be any suitable one that can act as a medium through which ions involved in the electrochemical reaction of the battery can move. Specifically, examples of the organic solvent that can be used include ester-based solvents such as methyl acetate, ethyl acetate, γ-butyrolactone, and ε-caprolactone; ether-based solvents such as dibutyl ether and tetrahydrofuran; ketone-based solvents such as cyclohexanone; aromatic hydrocarbon-based solvents such as benzene, benzene, and fluorobenzene; carbonate-based solvents such as dimethyl carbonate (DMC), diethyl carbonate (DEC), methyl ethyl carbonate (MEC), ethyl methyl carbonate (EMC), ethylene carbonate (EC), and propylene carbonate (PC); alcohol-based solvents such as ethyl alcohol and isopropyl alcohol; nitriles such as R-CN (R is a C2 to C20 linear, branched, or cyclic hydrocarbon group that may contain a double bond aromatic ring or an ether bond); amides such as dimethylformamide; dioxolanes such as 1,3-dioxolane; or sulfolanes. Among these, carbonate-based solvents are preferred, and mixtures of cyclic carbonates (e.g., ethylene carbonate or propylene carbonate) having high ionic conductivity and high dielectric constant that can improve the charge / discharge performance of the battery, and low-viscosity linear carbonate-based compounds (e.g., ethyl methyl carbonate, dimethyl carbonate, diethyl carbonate, etc.) are more preferred.
[0273] The lithium salt may be used without any particular limitation as long as it is a compound capable of providing lithium ions used in a lithium battery. Specifically, the lithium salt may be LiPF6, LiClO4, LiAsF6, LiBF4, LiSbF6, LiAlO4, LiAlCl4, LiCF3SO3, LiC4F9SO3, LiN(C2F5SO3)2, LiN(C2F5SO2)2, LiN(CF3SO2)2, LiCl, LiI, or LiB(C2O4)2. The concentration of the lithium salt may be within a range of 0.1 to 5.0M, preferably 0.1 to 3.0M. If the concentration of the lithium salt is within the above range, the electrolyte has appropriate conductivity and viscosity, and therefore exhibits excellent electrolyte performance, and lithium ions can be effectively moved.
[0274] In addition to the electrolyte components described above, the electrolyte may further contain additives for the purpose of improving battery life characteristics, suppressing the decrease in battery capacity, and improving the discharge capacity of the battery. For example, the additives may be haloalkylene carbonate compounds such as difluoroethylene carbonate, pyridine, triethyl phosphite, triethanolamine, cyclic ethers, ethylenediamine, n-glyme, hexamethylphosphoric triamide, nitrobenzene derivatives, sulfur, quinoneimine dyes, N-substituted oxazolidinones, N,N-substituted imidazolidines, ethylene glycol dialkyl ethers, ammonium salts, pyrrole, 2-methoxyethanol, or aluminum trichloride, which may be used alone or in combination, but are not limited thereto. The additives may be contained in an amount of 0.1 wt% to 10 wt%, preferably 0.1 wt% to 5 wt%, based on the total weight of the electrolyte.
[0275] In yet another embodiment of the present invention, the positive electrode may include a loading reduction portion having a lower loading amount of positive active material than an adjacent region. When the positive electrode has such a structure, the section of the positive active material portion can be increased without worrying about lithium deposition, thereby improving the energy density of the electrode assembly.
[0276] In recent years, developments are being made in the direction of increasing the size of batteries to achieve high energy density and reduce costs. As energy increases according to the size of the battery, the resistance per battery must decrease. To decrease the resistance, a method of using the electrode collector as an electrode tab, rather than attaching an electrode tab to the electrode, can be used. At this time, due to the characteristics of the electrode manufacturing process in which electrode slurry is applied to the electrode collector, a portion where the loading amount decreases occurs at the boundary between the negative electrode active material portion where the negative electrode slurry is applied and the negative electrode current collector. Considering the N / P ratio, there is a risk of metallic lithium being deposited at the positive electrode active material portion facing the portion where the loading amount decreases. Here, the N / P ratio is a value obtained by dividing the capacity of the negative electrode calculated based on the capacity per area and mass of the negative electrode by the capacity of the positive electrode calculated based on the capacity per area and mass of the positive electrode, and generally has a value of 1 or more. In other words, the capacity of the negative electrode is made larger. For reference, if the N / P ratio is not 1, metallic lithium is likely to precipitate during charging and discharging, which causes a rapid deterioration in battery safety during high-rate charging and discharging. In other words, the N / P ratio has a significant impact on the safety and capacity of the battery. Due to the risk of metallic lithium precipitation, the positive electrode active material part cannot be positioned in the positive electrode part facing the part of the negative electrode where the loading amount is reduced. This makes it difficult to increase the energy density of the battery. Therefore, the present invention improves the energy density by increasing the section of the positive electrode active material part.
[0277] FIG. 32 is a view showing an electrode assembly according to an embodiment of the present invention, and FIG. 33 is a cross-sectional view taken along line AA' in FIG.
[0278] 32 and 33, an electrode assembly 300 according to an embodiment of the present invention includes a negative electrode 400, a positive electrode 500, and a separator 600. The separator 600 is located between the negative electrode 400 and the positive electrode 500. The negative electrode 400, the positive electrode 500, and the separator 600 are wound together to form a jelly roll structure 300S. Here, the jelly roll structure 300S refers to a structure formed by winding the negative electrode 400, the positive electrode 500, and the separator 600. In addition, when the jelly roll structure 300S is formed, it is preferable that a separator 600 is further disposed on the outside to prevent the negative electrode 400 and the positive electrode 500 from contacting each other.
[0279] The negative electrode 400 includes a negative electrode current collector 410 and a negative electrode active material part 420 formed by coating a negative electrode active material on the negative electrode current collector 410. In particular, as shown in the figure, the negative electrode active material may be coated on both sides of the negative electrode current collector 410 to form the negative electrode active material part 420. In addition, the negative electrode uncoated part 430, where the negative electrode active material is not coated, extends in a first direction d1 in the negative electrode current collector 410. The negative electrode uncoated part 430 extends along one end of the negative electrode 400 to be wound. In addition, the negative electrode uncoated part 430 extends in the first direction d1 longer than the separator 600. As a result, the negative electrode uncoated part 430 may be exposed at one end of the jelly roll structure 300S in the first direction.
[0280] The positive electrode 500 includes a positive electrode current collector 510 and a positive electrode active material part 520 formed by applying a positive electrode active material on the positive electrode current collector 510. In particular, as shown in the figure, the positive electrode active material may be applied to both sides of the positive electrode current collector 510 to form the positive electrode active material part 520. In addition, a positive electrode uncoated part 530 where the positive electrode active material is not applied extends in the second direction d2 in the positive electrode current collector 510. The positive electrode uncoated part 530 extends along one end of the positive electrode 500 to be wound. In addition, the positive electrode uncoated part 530 extends in the second direction d2 longer than the separator 600. As a result, the positive electrode uncoated part 530 may be exposed at one end of the jelly roll structure 300S in the second direction.
[0281] Here, the first direction d1 and the second direction d2 are opposite directions, and may be parallel to the height direction of the jelly roll structure 300S.
[0282] The electrode assembly 300 according to the present embodiment does not have a separate electrode tab attached, but rather uses the negative electrode uncoated portion 430 of the negative electrode collector 410 and the positive electrode uncoated portion 530 of the positive electrode collector 510 as electrode tabs in order to reduce resistance.
[0283] Although not shown, the negative electrode uncoated portion 430 and / or the positive electrode uncoated portion 530 may have substantially the same structure as the uncoated portions of the electrodes described above.
[0284] In one embodiment, the positive electrode active material unit 520 includes a loading reduction portion 500D having a smaller loading amount of positive electrode active material than an adjacent region, and the loading reduction portion 500D is located at one end of the positive electrode 500 in a first direction d1. More specifically, the loading reduction portion 500D may have a gradually decreasing loading amount of the positive electrode active material in the first direction d1.
[0285] Here, the loading amount refers to the amount of active material applied per unit area. In a portion with a large loading amount, a large amount of anode active material or cathode active material may be applied per unit area, resulting in a relatively thick anode active material portion or cathode active material portion. In a portion with a small loading amount, a small amount of anode active material or cathode active material may be applied per unit area, resulting in a relatively thin anode active material portion or cathode active material portion.
[0286] The active material portion is formed by applying a slurry containing an active material. During this process, a boundary portion where the loading amount is gradually reduced between the non-coated portion and the active material portion may be formed.
[0287] Specifically, the negative electrode active material unit 420 may include a negative electrode boundary portion 420B that forms a boundary between the negative electrode active material unit 420 and the negative electrode uncoated portion 430. The negative electrode boundary portion 420B may have a gradually decreasing loading amount toward the negative electrode uncoated portion 430.
[0288] Similarly, the positive electrode active material unit 520 may include a positive electrode boundary portion 520B that forms a boundary between the positive electrode active material unit 520 and the positive electrode uncoated portion 530. The positive electrode boundary portion 520B may have a gradually decreasing loading amount toward the positive electrode uncoated portion 530.
[0289] The negative electrode boundary portion 420B and the positive electrode boundary portion 520B, where the loading amount is gradually reduced, are naturally generated during the process of applying the slurry containing the active material to the negative electrode current collector 410 and the positive electrode current collector 510.
[0290] At this time, with respect to the direction perpendicular to the second direction d2, the amount of the positive electrode active material becomes smaller than the amount of the negative electrode active material in the region corresponding to the positive electrode boundary 520B. This results in an N / P ratio greater than 1, so that problems such as the precipitation of metallic lithium do not occur.
[0291] However, there is a problem in the region corresponding to the negative electrode boundary 420B. With respect to the direction perpendicular to the first direction d1, the amount of the negative electrode active material is less than the amount of the positive electrode active material in the region corresponding to the negative electrode boundary 420B. This causes the N / P ratio to be less than 1, which may cause a problem of metallic lithium precipitation.
[0292] Therefore, in the present embodiment, a loading reduction portion 500D is provided in the positive electrode 500, and the negative electrode active material portion 420 is located at a portion corresponding to the loading reduction portion 500D in a direction perpendicular to the first direction d1. More specifically, the negative electrode boundary portion 420B may be located at a portion corresponding to the loading reduction portion 500D in a direction perpendicular to the first direction d1.
[0293] By providing a loading reduction portion 500D in which the loading amount of the positive electrode active material is less than that of the adjacent region at a position corresponding to the negative electrode boundary portion 420B in which the loading amount is gradually reduced, the section in which the positive electrode active material is applied can be increased without worrying about lithium deposition. In particular, the loading reduction portion 500D may have a shape in which the loading amount of the positive electrode active material gradually decreases in the first direction d1, corresponding to the shape of the negative electrode boundary portion 420B in which the loading amount is gradually reduced toward the negative electrode uncoated portion 430. Therefore, the N / P ratio of the negative electrode 400 and the positive electrode 500 in the region in which the negative electrode boundary portion 420B is formed can be maintained high, and lithium deposition can be prevented.
[0294] Hereinafter, a method for manufacturing an electrode assembly according to an embodiment of the present invention will be described in detail with reference to FIGS.
[0295] 34 and 35 are views showing a process of manufacturing a negative electrode according to an embodiment of the present invention. Specifically, FIG. 34 is a top view of a negative electrode sheet, and FIG. 35 is a front view of the negative electrode sheet of FIG.
[0296] 34 and 35, a method for manufacturing an electrode assembly according to an embodiment of the present invention includes a step of manufacturing a negative electrode sheet 400S such that a negative electrode active material portion 420, on which a negative electrode active material is applied, and a negative electrode uncoated portion 430, on which a negative electrode active material is not applied, are alternately disposed on a negative electrode current collector 410.
[0297] Specifically, the negative electrode active material may be applied to extend in the third direction d3 to form the negative electrode active material parts 420. In addition, the application regions may be spaced apart along a fourth direction d4 perpendicular to the third direction d3, so that the negative electrode active material parts 420 may be positioned apart from each other along the fourth direction d4. That is, the application process may be performed such that the negative electrode uncoated parts 430 are positioned between the negative electrode active material parts 420.
[0298] Here, the third direction d3 and the fourth direction d4 are directions for explanation based on the negative electrode sheet 400S, and are directions unrelated to the first direction d1 and the second direction d2 in the above-mentioned jelly roll structure 300S.
[0299] Thereafter, the negative electrode uncoated portion 430 and the negative electrode active material portion 420 may be slit to manufacture the negative electrode 400. Figure 36 is a perspective view showing a negative electrode according to an embodiment of the present invention.
[0300] 34 to 36, as shown by dotted lines in FIGS. 34 and 35, the negative electrode uncoated portion 430 and the negative electrode active material portion 420 may each be slit in a direction parallel to the third direction d3. As a result, a plurality of negative electrodes 400 as shown in FIG. 36 may be manufactured from the negative electrode sheet 400S. That is, the negative electrode 400 in FIG. 36 corresponds to one of a plurality of negative electrodes manufactured by slitting the negative electrode sheet 400S in FIGS. 34 and 35. By slitting the negative electrode uncoated portion 430 and the negative electrode active material portion 420 in the negative electrode sheet 400S, a negative electrode 400 having the negative electrode uncoated portion 430 extending to one side may be manufactured.
[0301] When forming the negative electrode active material part 420, a slurry containing the negative electrode active material is applied onto the negative electrode current collector 410. During this slurry application process, a negative electrode boundary part 420B may be formed at the boundary between the negative electrode active material part 420 and the negative electrode uncoated part 430, where the loading amount gradually decreases toward the direction in which the negative electrode uncoated part 430 is located.
[0302] 37 and 38 are diagrams illustrating a process for manufacturing a positive electrode according to one embodiment of the present invention. Specifically, Fig. 37 is a top view of a positive electrode sheet, and Fig. 38 is a front view of the positive electrode sheet of Fig. 37.
[0303] 37 and 38, a method for manufacturing an electrode assembly according to an embodiment of the present invention includes a step of manufacturing a positive electrode sheet 500S such that positive electrode active material parts 520 coated with a positive electrode active material and positive electrode uncoated parts 530 not coated with a positive electrode active material are alternately arranged on a positive electrode current collector 510.
[0304] Specifically, the positive electrode active material may be applied to extend in a third direction d3 to form the positive electrode active material parts 520. In addition, the application interval may be adjusted along a fourth direction d4 perpendicular to the third direction d3 to space the positive electrode active material parts 520 apart from each other. That is, the application process may be performed such that the positive electrode uncoated parts 530 are located between the positive electrode active material parts 520.
[0305] Here, the third direction d3 and the fourth direction d4 are directions for explanation based on the positive electrode sheet 500S, and are directions unrelated to the first direction d1 and the second direction d2 in the above-mentioned jelly roll structure 300S.
[0306] Thereafter, the positive electrode uncoated portion 530 and the positive electrode active material portion 520 may be slit to manufacture the positive electrode 500. Figure 39 is a perspective view showing a positive electrode 500 according to an embodiment of the present invention.
[0307] 37 to 39, as shown by dotted lines in FIGS. 37 and 38, the positive electrode uncoated portion 530 and the positive electrode active material portion 520 may each be slit in a direction parallel to the third direction d3. As a result, a plurality of positive electrodes 500 as shown in FIG. 39 may be manufactured from the positive electrode sheet 500S. That is, the positive electrode 500 in FIG. 39 corresponds to one of a plurality of positive electrodes manufactured by slitting the positive electrode sheet 500S in FIGS. 37 and 38. By slitting the positive electrode uncoated portion 530 and the positive electrode active material portion 520 in the positive electrode sheet 500S, a positive electrode 500 having the positive electrode uncoated portion 530 extending to one side may be manufactured.
[0308] When forming the positive electrode active material part 520, a slurry containing a positive electrode active material is applied onto the positive electrode current collector 510. During this slurry application process, a positive electrode boundary part 520B may be formed at the boundary between the positive electrode active material part 520 and the positive electrode uncoated part 530, where the loading amount gradually decreases toward the position of the positive electrode uncoated part 530.
[0309] 32, 36 and 39, the manufactured negative electrode 400 and positive electrode 500 may be subsequently wound together with a separator 600 to form a jelly roll structure 300S. In this case, in the jelly roll structure 300S, the negative electrode uncoated portion 430 may extend longer than the separator 600 in a first direction d1, and the positive electrode uncoated portion 530 may extend longer than the separator 600 in a second direction d2 opposite to the first direction d1.
[0310] 37 to 39, in a method for manufacturing an electrode assembly according to an embodiment of the present invention, a positive electrode sheet 500S includes a reduced-loading region 500DA in which the loading amount of the positive electrode active material is less than that of an adjacent region. There is no particular limit to the method for forming the reduced-loading region 500DA, and as one example, the reduced-loading region 500DA may be formed by adjusting the degree of application of a slurry.
[0311] In the step of manufacturing the positive electrode 500, a loading reduction region 500DA is slit from the positive electrode active material part 520. The slit loading reduction region 500DA forms a loading reduction part 500D having a smaller loading amount of positive electrode active material than an adjacent region in the jelly roll structure 300S shown in FIGS.
[0312] Specifically, a loading reduction region 500DA having a smaller loading amount of the positive electrode active material than an adjacent region is formed in a positive electrode active material unit 520 formed in a positive electrode sheet 500S. As shown in Fig. 38, the loading reduction region 500DA may be formed in the center of the positive electrode active material unit 520. Meanwhile, the loading reduction region 500DA may be configured such that the loading amount of the positive electrode active material gradually decreases toward a central portion 500C of the loading reduction region 500DA, and in the step of manufacturing the positive electrode 500, the loading reduction portion 500D according to this embodiment may be formed by slitting the central portion 500C of the loading reduction region 500DA.
[0313] That is, a loading reduction region 500DA is formed by applying a slurry containing a positive electrode active material, and a central portion 500C of the loading reduction region 500DA is slit, thereby manufacturing a plurality of positive electrodes 500 each having a loading reduction portion 500D formed therein.
[0314] Referring to FIG. 39, a loading reducing portion 500D may be provided at one end of the manufactured positive electrode 500, and a positive electrode uncoated portion 530 may be provided at the other end of the positive electrode 500 opposite to the one end.
[0315] 32 and 33, when such a positive electrode 500 is wound to form a jelly roll structure 300S, the loading reduction portion 500D may be located at one end of the positive electrode 500 in a first direction d1, and the positive electrode uncoated portion 530 may be located at one end of the positive electrode 500 in a second direction d2.
[0316] In addition, by slitting the central portion 500C of the loading reduction region 500DA, the loading amount of the positive electrode active material may be gradually reduced in the loading reduction portion 500D in the first direction d1.
[0317] In addition, in the jelly roll structure 300S, the negative electrode active material part 420 may be located at a portion corresponding to the loading reduction part 500D in a direction perpendicular to the first direction d1. More specifically, in the jelly roll structure 300S, the negative electrode boundary part 420B may be located at a portion corresponding to the loading reduction part 500D in a direction perpendicular to the first direction d1.
[0318] The corresponding positional relationship between the loading reduction portion 500D and the negative electrode boundary portion 420B is the same as that described above, and therefore will not be described here.
[0319] Hereinafter, an electrode assembly according to a comparative example of the present invention will be described with reference to FIGS. 40 to 43, and advantages of the electrode assembly according to the embodiment of the present invention compared to the comparative example will be described.
[0320] FIG. 40 shows an electrode assembly according to a comparative embodiment of the present invention, and FIG. 41 is a cross-sectional view taken along line BB' of FIG.
[0321] 40 and 41, an electrode assembly 600 according to a comparative embodiment of the present invention includes a negative electrode 700, a positive electrode 800, and a separator 900, and the negative electrode 700, the positive electrode 800, and the separator 900 are wound to form a jelly roll structure 600S.
[0322] The negative electrode 700 may include a negative electrode current collector 710, a negative electrode active material part 720, and a negative electrode uncoated part 730. The negative electrode uncoated part 730 may extend in a first direction d1, and the negative electrode active material part 720 may include a negative electrode boundary part 720B that forms a boundary between the negative electrode active material part 720 and the negative electrode uncoated part 730 and in which the loading amount gradually decreases.
[0323] FIG. 42 is a diagram showing a process for producing a negative electrode 700 according to a comparative embodiment of the present invention.
[0324] Referring to FIG. 42, after a negative electrode sheet 700S is manufactured such that the negative electrode active material parts 720 and the negative electrode uncoated parts 730 are alternately positioned along a fourth direction d4, the negative electrode uncoated parts 730 and the negative electrode active material parts 720 may be slit to manufacture a plurality of negative electrodes 700.
[0325] 40 and 41, a positive electrode 800 may include a positive electrode current collector 810, a positive electrode active material part 820, and a positive electrode uncoated part 830. The positive electrode uncoated part 830 may extend in a second direction d2 opposite to the first direction d1, and the positive electrode active material part 820 may include a positive electrode boundary part 820B that forms a boundary between the positive electrode active material part 820 and the positive electrode uncoated part 830 and in which the loading amount gradually decreases.
[0326] FIG. 43 is a diagram showing a process for producing a positive electrode 800 according to a comparative embodiment of the present invention.
[0327] Referring to FIG. 43, a positive electrode sheet 800S is manufactured so that the positive electrode active material parts 820 and the positive electrode uncoated parts 830 are alternately positioned along the fourth direction d4, and then the positive electrode uncoated parts 830 and the positive electrode active material parts 820 are slit to manufacture a plurality of positive electrodes 800.
[0328] Then, the manufactured anode 700 and cathode 800 may be wound together with the separator 900 to manufacture the electrode assembly 600 according to the comparative embodiment of the present invention.
[0329] That is, the electrode assembly 600 according to the comparative example of the present invention may have a similar structure to the electrode assembly 300 according to the embodiment of the present invention, except for the loading reduction portion 500D (see FIG. 33).
[0330] 40 and 41, in the case of the electrode assembly 600 according to the comparative example, the positive electrode active material part 820 cannot be positioned in a portion corresponding to the negative electrode boundary part 720B with respect to a direction perpendicular to the first direction d1. If the positive electrode active material part 820 extends to a portion corresponding to the negative electrode boundary part 720B, the corresponding portion has a low N / P ratio, and it is highly likely that metallic lithium will be precipitated. Therefore, in order to prevent lithium precipitation, the length of the positive electrode active material part 820 must be limited. That is, the positive electrode active material part 820 can be formed only in the B1 region as shown in the figure, and the positive electrode active material part 820 cannot be formed in the B2 region, resulting in the length of the positive electrode active material part 820 being reduced by the negative electrode boundary part 720B.
[0331] Meanwhile, referring to FIG. 32 and FIG. 33, in the case of the electrode assembly 300 according to the embodiment of the present invention, the positive electrode active material part 520, particularly the loading reduction part 500D, may be located at a portion corresponding to the negative electrode boundary part 420B with respect to a direction perpendicular to the first direction d1. Since the loading reduction part 500D, which has a smaller loading amount of the positive electrode active material than the adjacent region, is provided at a position corresponding to the negative electrode boundary part 420B, the N / P ratio in the corresponding portion can be maintained high and lithium precipitation can be prevented. As a result, the positive electrode active material part 520 can be formed over the A1 region, and the A2 region where the positive electrode active material part 520 cannot be formed can be reduced. For example, the width of the positive electrode 500 in the height direction relative to the width of the negative electrode 400 in the height direction can be increased to 98% or more.
[0332] Comparing area A1 of Figures 32 and 33 with area B1 of Figures 40 and 41, the electrode assembly 300 according to this embodiment can increase the length of the positive electrode active material portion by the loading reduction portion 500D, thereby achieving a higher energy density in a limited space than the electrode assembly 600 according to the comparative example.
[0333] Yet another embodiment of the present invention relates to a cylindrical battery including a jelly-roll type electrode assembly having a structure in which a positive electrode, a negative electrode, and a separator interposed between the positive electrode and the negative electrode are wound in one direction, a cylindrical battery housing in which the electrode assembly is housed, and a battery cap as a sealing body disposed on the top of the battery housing to seal the battery housing. Here, the positive electrode is an embodiment of the present invention, and the positive electrode active material has an average particle diameter D 50 The cylindrical battery may further include an electrolyte, and the above description of the electrolyte may be referred to.
[0334] The electrode assembly may have a stacked type, a stacked / folded type, or a jelly roll type structure as described above. In a specific embodiment of the present invention, the electrode assembly may have a positive electrode having a loading reduction portion as described above.
[0335] Conventional cylindrical batteries have problems with current being concentrated on the strip-shaped electrode tabs, resulting in high resistance, large amounts of heat being generated, and poor current collection efficiency.
[0336] In recent years, with the development of electric vehicle-related technologies, the demand for high-capacity batteries has increased, and the development of large-volume cylindrical batteries is required. Conventionally used small cylindrical batteries, i.e., cylindrical batteries with 1865 or 2170 form factors, have a small capacity, so resistance and heat generation do not seriously affect battery performance. However, if the specifications of conventional small cylindrical batteries are directly applied to large cylindrical batteries, serious problems may occur in battery safety.
[0337] As the battery becomes larger, the amount of heat and gas generated inside the battery also increases, and the temperature and pressure inside the battery increase due to the heat and gas, which may cause the battery to ignite or explode. To prevent this, the heat and gas inside the battery must be properly discharged to the outside, and to do so, the cross-sectional area of the battery, which serves as a path for discharging heat to the outside of the battery, must increase with an increase in volume. However, since the increase in cross-sectional area is usually not as large as the increase in volume, the larger the battery, the greater the amount of heat generated inside the battery, which increases the risk of explosion and reduces output, etc. In addition, when fast charging at a high voltage, a large amount of heat is generated around the electrode tab in a short time, which may cause the battery to ignite. Therefore, the present invention proposes a cylindrical battery that has a large volume to achieve high capacity and is highly safe.
[0338] In addition, since a high loading electrode using the positive electrode active material in the form of single particle or quasi-single particle is applied to a cylindrical battery, the initial resistance characteristics and charge / discharge efficiency of the cylindrical battery can be improved.
[0339] The cylindrical battery according to an embodiment of the present invention significantly reduces the amount of gas generation compared to conventional batteries by applying a positive electrode active material in the form of a single particle or pseudo-single particle, thereby achieving excellent safety even in large cylindrical batteries with a form factor ratio of 0.4 or more.
[0340] The cylindrical battery according to an embodiment of the present invention is preferably a battery having a tabless structure that does not include electrode tabs, but is not limited thereto.
[0341] The tabless-structured battery may have, for example, a structure in which a positive electrode and a negative electrode each include an uncoated portion where no active material layer is formed, a positive electrode uncoated portion and a negative electrode uncoated portion are located at an upper end and a lower end of an electrode assembly, respectively, a current collecting plate is bonded to the positive electrode uncoated portion and the negative electrode uncoated portion, and the current collecting plate is connected to an electrode terminal.
[0342] When a cylindrical battery is formed in a tabless structure as described above, current concentration is reduced compared to conventional batteries having electrode tabs, so that heat generation inside the battery can be effectively reduced, thereby improving the thermal stability of the battery.
[0343] The present invention will now be described in more detail with reference to specific examples.
[0344] <Example 1> Average particle size D 50 The positive electrode active material Li[Ni 0.9 Co 0.06 Mn 0.03 Al 0.01 A positive electrode slurry was prepared by mixing 1,2-dichloroethane (1,2,3-trifluoroethylene (1,2,3,4-tetra ...
[0345] Anode active material (graphite:SiO = 95:5 (weight ratio) mixture), conductive material (Super C), styrene-butadiene rubber (SBR) and carboxymethyl cellulose (CMC) were mixed in water in a weight ratio of 96:2:1.5:0.5 to prepare anode slurry. The anode slurry was applied to one side of a copper current collector sheet, dried at 150°C and rolled to prepare anode.
[0346] The prepared positive and negative electrodes were laminated in the order of separator / positive electrode / separator / negative electrode with a separator interposed between them, and then wound up to prepare a jelly roll type electrode assembly. The prepared electrode assembly was inserted into a cylindrical battery can, and an electrolyte was injected to prepare a 4680 cell.
[0347] <Comparative Example 1> As a positive electrode active material, large particle size average particle size D 50 is 9 μm, and the small particle average particle size D 50 The Li[Ni 0.9Co 0.05 Mn 0.04 Al 0.01 A 4680 cell was manufactured in the same manner as in Example 1, except that ]O2 was used.
[0348] <Experimental Example 1> A hot box test was carried out on the 4680 cells manufactured according to Example 1 and Comparative Example 1.
[0349] Specifically, the 4680 cells manufactured according to Example 1 and Comparative Example 1 were placed in a hot box chamber at room temperature, and heated to 130°C at a heating rate of 5°C / min, and then maintained at that temperature for 30 minutes to measure the temperature change of the battery over time. For accurate evaluation, the hot box evaluation was performed twice for the cell of Example 1. The measurement results are shown in Figures 29a and 29b.
[0350] FIG. 29a is a graph showing the results of a hot box test for the 4680 cell prepared according to Example 1, and FIG. 29b is a graph showing the results of a hot box test for the 4680 cell prepared according to Comparative Example 1.
[0351] 29a and 29b show that in the case of the lithium secondary battery of Example 1 using the positive electrode active material in the form of single particles, the battery voltage and temperature were maintained stable until 65 minutes had elapsed, whereas in the case of the lithium secondary battery of Comparative Example 1, the battery temperature rose rapidly after 35 minutes had elapsed.
[0352] <Example 2-1> Unimodal particle size distribution min = 1.78 μm, D 50 = 4.23 μm, D max = 13.1 μm, and the positive electrode active material is a mixture of single particles and pseudo-single particles (composition: Li[Ni 0.9 Co 0.06 Mn 0.03 Al 0.01 ]O2) was prepared. FIG 28a shows an SEM image of the positive electrode active material used in Example 2-1.
[0353] The positive electrode active material, carbon nanotubes, and PVDF binder were mixed in a weight ratio of 97.8:0.6:1.6 in N-methylpyrrolidone to prepare a positive electrode slurry, which was then applied to one side of an aluminum current collector sheet, dried at 120° C., and rolled to prepare a positive electrode.
[0354] Anode active material (graphite:SiO = 95:5 (weight ratio) mixture), conductive material (Super C), styrene-butadiene rubber (SBR) and carboxymethyl cellulose (CMC) were mixed in water in a weight ratio of 96:2:1.5:0.5 to prepare anode slurry. The anode slurry was applied to one side of a copper current collector sheet, dried at 150°C and rolled to prepare anode.
[0355] The prepared positive and negative electrodes were laminated in the order of separator / positive electrode / separator / negative electrode with a separator interposed between them, and then wound up to prepare a jelly roll type electrode assembly. The prepared electrode assembly was inserted into a battery can, and an electrolyte was injected to prepare a 4680 cell.
[0356] <Example 2-2> As a positive electrode active material, it has a unimodal particle size distribution. min = 1.38 μm, D 50 = 4.69 μm, D max = 18.5 μm, and the positive electrode active material is a mixture of single particles and pseudo-single particles (composition: Li[Ni 0.9 Co 0.06 Mn 0.03 Al 0.01 ]O2) was used. A 4680 cell was manufactured in the same manner as in Example 2-1. Fig. 28b shows an SEM image of the positive electrode active material used in Example 2-2.
[0357] <Comparative Example 2-1> Large particle size average particle size D 50 is 9 μm, and the small particle average particle size D 50 The positive electrode active material (composition: Li[Ni 0.9Co 0.05 Mn 0.04 Al 0.01 ]O2) was used, a 4680 cell was produced in the same manner as in Example 2-1.
[0358] <Comparative Example 2-2> Unimodal particle size distribution min = 0.892 μm, D 50 = 3.02 μm, D max = 11 μm, and the positive electrode active material is a mixture of single particles and pseudo-single particles (composition: Li[Ni 0.9 Co 0.06 Mn 0.03 Al 0.01 ]O2) was used, a 4680 cell was produced in the same manner as in Example 2-1.
[0359] FIG. 28c shows an SEM image of the positive electrode active material used in Comparative Example 2-2.
[0360] <Experimental Example 2-1> A hot box test was carried out on the 4680 cells manufactured in Examples 2-1 and 2-2 and Comparative Examples 2-1 and 2-2.
[0361] Specifically, the 4680 cells manufactured according to Example 2-1 and Comparative Example 2-1 were placed in a hot box chamber at room temperature, and the temperature was raised to 130°C at a rate of 5°C / min, and the temperature was maintained for 30 minutes, after which the temperature change of the battery was measured. If no thermal runaway or ignition occurred during the test, it was indicated as "pass," and if thermal runaway and / or ignition occurred, it was indicated as "fail." In addition, for the accuracy of the test, the cells of Examples 2-1 and 2-2 were tested more than twice.
[0362] The measurement results are shown in Table 1 below and in Figures 29c and 29d. Figure 29c is a graph showing the results of a hot box test for the 4680 cells prepared according to Sample 1 of Example 2-1 and Comparative Example 2-1, and Figure 29d is a graph showing the results of a hot box test for the 4680 cells prepared according to Samples 2 and 3 of Example 2-1, Samples 1 and 2 of Example 2-2, and Comparative Example 2-2.
[0363] [Table 1]
[0364] Referring to Table 1, Figs. 29c and 29d, D min In the case of the 4680 cell of Example 2-1, in which a positive electrode active material having a single particle / quasi-single particle form with a particle size of 1.0 μm or more was used, the battery voltage and temperature were stably maintained until 65 minutes had elapsed, while in the case of Comparative Examples 2-1 and D, in which secondary particles were used as the positive electrode active material, min It can be seen that the 4680 cell of Comparative Example 2-2, which uses a positive electrode active material in the form of a single particle / quasi-single particle having a particle size of less than 1.0 μm, experienced a rapid rise in battery temperature.
[0365] <Experimental Example 2-2> In order to check the degree of cracking of the positive electrode active material particles after rolling for the positive electrodes manufactured in Example 2-1 and Comparative Example 2-1, the positive electrodes were cut using an ion milling device and the cross sections were photographed using an SEM. Figure 30a shows an SEM cross-sectional image of the positive electrode manufactured in Example 2-1, and Figure 30b shows an SEM cross-sectional image of the positive electrode manufactured in Comparative Example 2-1.
[0366] 30a and 30b, the positive electrode of Example 2-1 had almost no particle cracks in the positive electrode active material even after rolling, whereas the positive electrode of Comparative Example 2-2, which used secondary particles, had many particle cracks in the positive electrode active material after rolling.
[0367] <Example 3-1> Unimodal particle size distribution min = 1.78 μm, D 50 = 4.23 μm, D max= 13.1 μm, and the positive electrode active material powder (composition: Li[Ni 0.9 Co 0.06 Mn 0.03 Al 0.01 ]O2), flake graphite (SFG6L), conductive material (multi-walled carbon nanotubes), and PVDF binder were mixed in N-methylpyrrolidone in a weight ratio of 96.3:1.5:0.4:1.8 to prepare a positive electrode slurry. The positive electrode slurry was applied to one side of an aluminum current collector sheet, dried, and rolled at a linear pressure of 3.0 ton / cm to prepare a positive electrode. The porosity of the positive electrode active material layer of the prepared positive electrode was measured. The porosity was 17.5%.
[0368] <Example 3-2> A positive electrode was produced in the same manner as in Example 3-1, except that the positive electrode active material, the flake graphite, the conductive material, and the binder were mixed in a weight ratio of 97.2:0.6:0.4:1.8, and the porosity of the positive electrode active material layer was measured. The porosity was 19%.
[0369] <Example 3-3> A positive electrode was manufactured in the same manner as in Example 3-1, except that the positive electrode active material, the flake graphite, the conductive material, and the binder were mixed in a weight ratio of 97.4:0.4:0.4:1.8, and the porosity of the positive electrode active material layer was measured. The porosity was 20%.
[0370] <Example 3-4> A positive electrode was produced in the same manner as in Example 3-1, except that the positive electrode active material, the flake graphite, the conductive material, and the binder were mixed in a weight ratio of 97.6:0.2:0.4:1.8, and the porosity of the positive electrode active material layer was measured. The porosity was 21%.
[0371] <Comparative Example 3-1> A positive electrode was manufactured in the same manner as in Example 3-1, except that flake graphite was not added, and the positive electrode active material, the conductive material, and the binder were mixed in N-methylpyrrolidone in a weight ratio of 97.8:0.4:1.8 to prepare a positive electrode slurry, and the porosity of the positive electrode active material layer was measured. The porosity was 24%.
[0372] <Comparative Example 3-2> A positive electrode was manufactured in the same manner as in Example 3-1, except that flake graphite was not added, and the positive electrode active material, the conductive material, and the binder were mixed in N-methylpyrrolidone in a weight ratio of 97.8:0.4:1.8 to prepare a positive electrode slurry, and the positive electrode slurry was rolled at a linear pressure of 2.0 ton / cm. The porosity of the positive electrode active material layer was measured. The porosity was 30%.
[0373] <Experimental Example 3-1. Measurement of charge / discharge capacity and charge / discharge efficiency> Coin-type half cells including the positive electrodes according to Examples 3-1 to 3-4 and Comparative Examples 3-1 and 3-2 were manufactured, and charged to 4.25 V at a current of 0.2 C, and then discharged to 2.5 V at a current of 0.2 C to measure the charge capacity (mAh / g) and discharge capacity (mAh / g) of each coin-type half cell. The measurement results are shown in Table 2 below.
[0374] [Table 2]
[0375] It can be seen from Table 2 that Examples 3-1 to 3-4, which used positive electrodes containing added flake graphite, exhibit lower porosity and superior capacity characteristics compared to Comparative Examples 3-1 and 3-2.
[0376] <Experimental Example 3-2. Confirmation of resistance characteristics> The resistance characteristics according to the SOC were measured while charging the coin-type half-cells including the positive electrodes according to Example 3-3, Comparative Example 3-1, and Comparative Example 3-2 up to 4.2 V. The experimental results are shown in FIG.
[0377] 31a, it can be seen that the resistance value of Example 3-3, in which flake graphite was added to the positive electrode active material layer, was lower than that of Comparative Examples 3-1 and 3-2, which did not contain flake graphite, based on an SOC of 10%. This shows that adding flake graphite to the positive electrode active material layer has the effect of improving the resistance characteristics at a low SOC.
[0378] <Experimental Example 3-3. Measurement of high-temperature life characteristics and resistance increase rate> The positive and negative electrodes according to Examples 3-1, 3-3, and Comparative Example 3-1 were laminated in the order of separator / positive electrode / separator / negative electrode with a separator interposed between them, and then wound up to prepare a jelly roll type electrode assembly. The prepared electrode assembly was inserted into a cylindrical battery can, and an electrolyte was injected to prepare a 4680 cell.
[0379] In this case, the negative electrode was prepared by mixing a negative electrode active material (graphite:SiO = 95:5 (weight ratio) mixture), a conductive material (Super C), styrene-butadiene rubber (SBR), and carboxymethyl cellulose (CMC) in a weight ratio of 96:2:1.5:0.5 in water to prepare a negative electrode slurry, which was then applied to one side of a copper current collector sheet, dried at 150°C, and rolled.
[0380] The 4680 cell thus manufactured was subjected to 50 charge-discharge cycles, where one cycle is charging to 4.2 V at 0.5 C at 40° C. and discharging to 2.5 V at 0.5 C, and then the capacity retention rate and the increase rate of resistance (DCIR) were measured. The measurement results are shown in Figure 31b.
[0381] Referring to FIG. 31b, it can be seen that in the case of the secondary batteries of Examples 3-1 and 3-3, the change in capacity retention rate according to the number of cycles is smaller than that in the secondary battery of Comparative Example 3-1, and the change in the resistance increase rate according to the number of cycles is also smaller.
[0382] As described above, the present invention has been described using limited embodiments and drawings. However, the present invention is not limited thereto, and it goes without saying that various modifications and variations can be made by a person having ordinary knowledge in the technical field to which the present invention belongs within the technical spirit of the present invention and the equivalent scope of the claims. [Explanation of symbols]
[0383] 1 Cylindrical battery 11 First electrode tab 12 2nd electrode tab 20 Battery Housing 21 Beading Section 22 Crimping section 30 First current collector 31 Support part 32 Tab joint 33 Housing joint 33a Contact part 33b Connection part 40 Cap Plate 41 Venting section 50 Sealing Spacer 51 Anti-movement part 52 Sealing part 53 Connecting part 53a extension leg 60 Battery terminal 300 electrode assembly 400 negative electrode 410 Negative electrode current collector 420 Negative electrode active material section 430 Negative electrode uncoated area 430 Plain section 500 positive electrode 510 Positive electrode current collector 520 Cathode active material section 530 Positive electrode uncoated area 600 Separation membrane 700 negative electrode 710 Negative electrode current collector 720 Negative electrode active material section 730 Negative electrode uncoated area 800 positive electrode 810 Positive electrode current collector 820 Cathode active material section 830 Positive electrode uncoated area 900 Separation membrane
Claims
1. an electrode assembly including a first electrode tab and a second electrode tab; a battery housing that receives the electrode assembly through an opening formed on one side thereof; a first current collecting plate located within the battery housing, the first current collecting plate including: a support portion disposed on one surface of the electrode assembly; at least one tab connecting portion extending from the support portion and connected to the first electrode tab; and at least one housing connecting portion extending from an end of the tab connecting portion and connected to an inner surface of the battery housing; A cap plate for covering the opening; a battery terminal electrically connected to the second electrode tab; a sealing spacer configured to prevent movement of the electrode assembly and to enhance a sealing force of the battery housing.
2. the battery housing includes a beading portion formed on a periphery adjacent to the opening and pressed inward, The cylindrical battery according to claim 1 , wherein the housing joint portion is joined onto the beading portion.
3. the battery housing includes a beading portion formed on a periphery adjacent to the opening and pressed inward, The housing joint portion is a contact portion coupled onto the beading portion; 2. The cylindrical battery according to claim 1, further comprising a connecting portion connecting between the tab connecting portion and the contact portion.
4. The cylindrical battery according to claim 3 , further comprising a sealing gasket provided between the battery housing and the cap plate.
5. The cylindrical battery according to claim 4 , wherein the contact portion is interposed and fixed between the beading portion and the sealing gasket.
6. The cylindrical battery according to claim 3 , wherein a weld is formed between the beading portion and the contact portion of the first current collector plate.
7. the battery housing includes a beading portion formed on a periphery adjacent to the opening and pressed inward, The cylindrical battery according to claim 1 , wherein a boundary area between the tab joint portion and the housing joint portion is located inside an innermost portion of the beading portion.
8. The cylindrical battery according to claim 1 , wherein the cylindrical battery comprises a plurality of the tab joints and a plurality of the housing joints.
9. The cylindrical battery according to claim 3 , wherein the connecting portion has at least one bent portion at which an extending direction is changed.
10. The cylindrical battery according to claim 3 , wherein the contact portion has an arc shape extending along the beading portion.
11. The cylindrical battery according to claim 10 , wherein the connecting portion has an arc shape extending along the contact portion.
12. The sealing spacer is a movement prevention portion interposed between the first current collecting plate and the cap plate; a sealing portion interposed between the battery housing and the cap plate; The cylindrical battery according to any one of claims 1 to 11, further comprising a connecting portion connecting the movement prevention portion and the sealing portion.
13. The cylindrical battery according to claim 12 , wherein the anti-movement portion has a height corresponding to a distance between the first current collector plate and the cap plate.
14. The cylindrical battery according to claim 12 , wherein the motion prevention portion is located at a center on one surface of the electrode assembly.
15. The cylindrical battery according to claim 12 , wherein the motion prevention portion comprises a spacer hole formed at a position corresponding to a winding center hole of the electrode assembly.
16. The cylindrical battery according to claim 12 , wherein the sealing portion extends around an inner circumferential surface of the battery housing.
17. The cylindrical battery of claim 12 , wherein the coupling portion includes a plurality of extension legs extending radially from the motion prevention portion.
18. 18. The cylindrical battery of claim 17, wherein the plurality of extension legs are configured not to contact the first current collector plate.
19. 20. The cylindrical battery of claim 17, wherein the plurality of extension legs are configured not to contact the cap plate.
20. The cylindrical battery according to claim 12 , wherein the connecting portion is positioned so as not to overlap the housing coupling portion along a height direction of the cylindrical battery.
21. The cylindrical battery comprises: a second current collecting plate coupled to the second electrode tab; The cylindrical battery according to claim 1 , further comprising: an insulator interposed between a closing portion formed at an upper end of the battery housing and the second current collector plate.
22. 22. The cylindrical battery of claim 21, wherein the insulator has a height corresponding to the distance between the second current collector and the closure.
23. the active material layer of the second electrode comprises a positive electrode active material comprising single particles, quasi-single particles, or a combination thereof; The minimum particle size D appearing in the cumulative volume distribution of the positive electrode active material min is 1.0 μm or more, The particle size D when the volume cumulative amount is 50% in the volume cumulative distribution of the positive electrode active material 50 is 5.0 μm or less, The maximum particle size D appearing in the volume cumulative distribution of the positive electrode active material max The cylindrical battery according to any one of claims 1 to 11, wherein the thickness is 12 µm to 17 µm.
24. The positive electrode active material has a unimodal particle size distribution in which a single peak appears in a volume cumulative particle size distribution graph, and is represented by the following Equation 1: [Formula 1] Particle size distribution (PSD) = (D max -D min ) / D 50 24. The cylindrical battery of claim 23, wherein the particle size distribution (PSD) is 3 or less.
25. 24. The cylindrical battery of claim 23, wherein the single particle, pseudo-single particle, or a combination thereof is included in an amount of 95 wt % to 100 wt % based on the total weight of the positive electrode active material included in the active material layer of the second electrode.
26. The cylindrical battery according to claim 23 , wherein the positive electrode active material comprises a lithium nickel-based oxide containing 80 mol % or more of Ni based on the total mole number of transition metals.
27. the porosity of the active material layer of the second electrode is 15% to 23%, 24. The cylindrical battery according to claim 23, wherein the active material layer of the second electrode contains flake graphite at a weight ratio of 0.05 wt % to 5 wt %.
28. 24. The cylindrical battery of claim 23, wherein the second electrode active material layer further comprises carbon nanotubes (CNTs).
29. the active material layer of the first electrode includes a silicon-based negative electrode active material and a carbon-based negative electrode active material; 24. The cylindrical battery of claim 23, wherein the silicon-based negative electrode active material and the carbon-based negative electrode active material are contained in a weight ratio of 1:99 to 20:
80.
30. A battery pack comprising the cylindrical battery according to any one of claims 1 to 11.
31. 31. A motor vehicle comprising the battery pack of claim 30.
Citation Information
Patent Citations
Method for controlling out-of-kettle particle size of small-particle-size tricobalt tetraoxide
CN112429782A
Non-aqueous electrolytic secondary battery
JP2001093579A
Sealed battery
JP2005149909A
Battery
JP2008243811A
Sealed-type secondary battery
JP2009289683A