Organotin Precursor Compounds
Organotin compounds with alkoxide and/or amide functionality are used as precursors to form high-purity EUV patternable films on microelectronic devices, addressing the need for improved deposition methods in EUV lithography.
Patent Information
- Application Number
- JP2024530486
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-24
- Filing Date
- 2022-11-22
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-11-22
AI Technical Summary
There is a need for improved precursor composition and counter reactant pairings for the deposition of high-purity metal oxide films in extreme ultraviolet (EUV) lithography techniques used in microelectronic device manufacturing, particularly for forming EUV patternable films.
The use of certain organotin compounds with alkoxide and/or amide functionality as precursors, combined with suitable counter reactants, to form tin-containing films on microelectronic device substrates, which are then patterned using EUV light, allowing for precise manipulation and patterning.
These organotin compounds enable the deposition of high-purity EUV patternable films on microelectronic devices, facilitating precise patterning and film formation with desired thickness and purity.
Smart Images

Figure 2024541464000001 
Figure 2024541464000002 
Figure 2024541464000003
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This invention claims priority to U.S. Provisional Patent Application No. 63 / 282,893, filed November 24, 2021, which is incorporated herein by reference.
[0002] This invention is in the field of organotin chemistry, and in particular, relates to certain organotin precursor compounds. [Background technology]
[0003] Certain organometallic compounds have been shown to be useful as precursors in the deposition of high purity metal oxide films in applications such as extreme ultraviolet (EUV) lithography techniques used in the manufacture of microelectronic devices. In this method, certain organometallic precursors are utilized along with a counter reactant to form a polymerized organometallic film. A pattern is then formed on the surface, exposing the EUV patternable film including exposure of the film using a patterned beam of EUV light, followed by exposing the resulting microelectronic device surface to a post-exposure bake in ambient air. This treatment with patterned EUV light leaves some exposed and some unexposed portions of the surface, thus allowing further manipulation and patterning due to the distinct physical and chemical differences of the two regions. See, for example, U.S. Patent Publication No. 2021 / 0013034.
[0004] Thus, there is a need for further development of precursor composition and counter reactant pairings that can be used in this dry (photo)resist process. Summary of the Invention
[0005] In summary, the present invention provides certain organotin compounds that are believed to be useful for the deposition of tin-containing films on the surface of a microelectronic device substrate. Certain novel precursor compounds are also provided. In general, the precursor compounds of the present invention are organotin compounds that have two or three tin centers, for example, with alkoxide and / or amide functional groups. The precursors are believed to be particularly useful in EUV patterning operations. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0006] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless the content clearly dictates otherwise. As used in this specification and the appended claims, the term "or" is generally used in its sense including "and / or" unless the content clearly dictates otherwise.
[0007] The term "about" generally refers to a range of numbers that are considered equivalent to the recited value (e.g., having the same function or result). In many cases, the term "about" may include numbers that are rounded to the nearest significant figure.
[0008] Numeric ranges expressed using endpoints include all numbers subsumed within that range (eg, 1 to 5 includes 1, 1.5, 2, 2.75, 3, 3.80, 4, and 5).
[0009] In one aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000001.tif27170 (in the formula, R 1 is a group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-, R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 are H, -N(R)2, -OR, and -R 1 (selected from In one embodiment, a method is provided comprising: introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from the group consisting of:
[0010] The compounds of formula (I) are believed to be useful as precursors in the deposition of tin-containing films on substrates of microelectronic devices. As used herein, the term "tin-containing" films includes elemental tin, tin oxide, tin carbide, and tin nitride, and different percentages of each in a given film. If elemental tin films are desired, reducing agents such as hydrogen may be utilized as co-reactants. If tin nitride films are desired, co-reactants such as ammonia and nitrogen may be utilized.
[0011] In another aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000002.tif27170 (in the formula, R 1 is a divalent group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 are H, -N(R)2, -OR, and -R 1 (selected from A precursor composition comprising at least one compound selected from at least one counter reactant selected from compounds capable of reacting with -OR and -N(R); into a reaction zone under deposition conditions.
[0012] In this regard, compounds of formula (I) are believed to be useful in EUV patterning operations when utilizing counter reactants as described above.
[0013] In another aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000003.tif11170 (in the formula, R 1 is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 are H, -N(R)2, -OR, and -R 1 and m is an integer from 0 to 2. In one embodiment, a method is provided comprising: introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from the group consisting of:
[0014] Similar to the compounds of formula (I), the compounds of formula (II) are believed to be useful as precursors in the deposition of tin-containing films on substrates of microelectronic devices. Thus, the compounds of formula (II) can be utilized with a variety of co-reactants to deposit the desired tin-containing films as elemental tin, tin oxide, and tin nitride. Furthermore, when utilized with counter-reactants as described below, the precursors and methods can be used to prepare EUV patternable films.
[0015] Thus, in another aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000004.tif11170 (in the formula, R 1 is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 are H, -N(R)2, -OR, and -R 1 and m is an integer from 0 to 2. A precursor composition comprising at least one compound selected from at least one counter reactant selected from compounds capable of reacting with -OR and -N(R); into a reaction zone under deposition conditions.
[0016] R 2 Compounds of formula (II) in which the group is an amide group can be prepared according to Scheme I below: TIFF2024541464000005.tif17170 Scheme I. (In the formula, R 1 and R 2 is as above, and M is an alkali metal or an alkaline earth metal. Exemplary metals (M) include alkaline earth and alkali metal salts, including but not limited to lithium, sodium, potassium, magnesium, calcium, and zinc.
[0017] Furthermore, the compound of formula (II) can be prepared according to the following scheme II: TIFF2024541464000006.tif39170 Scheme II. (wherein "TMS" is trimethylsilyl) It can be prepared according to
[0018] See, for example, "Stille Cross-Coupling of Activated Alkyltin Reagents under "Ligandless" Conditions", A. Herve, et al., J. Org. Chem. 2005, 70, 5, 1953-1956. In Scheme II, R 1 and R 2 is as above, and M is a transition metal. Exemplary metals (M) include alkaline earth metal salts and alkali metal salts, including but not limited to lithium, sodium, potassium, magnesium, calcium, and zinc, and X is a halogen atom.
[0019] Compounds of formula (I) can be prepared according to the following Scheme III: TIFF2024541464000007.tif27170 Scheme III (In the formula, R, R 1 , and R 2 is as above, and M is a transition metal. Exemplary metals (M) include alkaline earth and alkali metal salts, including but not limited to lithium, sodium, potassium, magnesium, calcium, and zinc.
[0020] For example, (i) “Some Applications of the Methylene Di-Grignard Reagent for the Synthesis of Main Group IV Organometallic Compounds”, JW, Bruin, et al., Journal of Organometallic Chemistry, Volume 288, Issue 1,11 June 1985, pages 13-25; (ii) “A General Route to Alkylene-, Arylene-, or Benzylene-Bridged Ditin Hexachlorides and Hexaalkynides”, B. Jousseaume, et al., Organometallics 2002, 21, 22, 4590-4594; and (iii) “Macrocycles Containing Tin.Syntheses of Symmetrical Macrocycles Containing Two or Four Diphenylstanna Units”, Y. Azuma et al. al., Organometallics 1984, 3, 1, 9-14.
[0021] In a further aspect, the present invention provides certain compounds of formula (I) and (II) that are believed to be useful as precursors herein. In one aspect, the present invention provides compounds of formula: TIFF2024541464000008.tif27170 (in the formula, R 1 is a group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-, R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 is selected from groups of formula -N(R)2 and -OR A precursor composition is provided that includes a compound of the formula:
[0022] In this embodiment, similar to the compounds of formula (I) and (II) herein, each R is independently selected from hydrogen and C1-C5 alkyl; thus, a group of formula -N(R)2 includes a secondary amine of formula -NHR.
[0023] In a further aspect, the present invention provides a compound of formula: TIFF2024541464000009.tif9170 (in the formula, R 1 is a group selected from -CH2-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-, R is selected from H and C1-C5 alkyl; R 2 is a group of formula -N(R)2, and X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2. A precursor composition is provided that includes a compound of the formula:
[0024] In this embodiment, each R is independently selected from hydrogen and C1-C5 alkyl; thus, a group of formula -N(R)2 includes a secondary amine of formula -NHR.
[0025] As noted above, these organotin precursor compounds are believed to be useful in a variety of vapor deposition methods where deposition of tin-containing films on the surfaces of microelectronic devices is desired.
[0026] Also, as mentioned above, the precursors of the present invention are believed to be particularly useful in patterning microelectronic device substrates using extreme ultraviolet (EUV) technology. In this regard, see U.S. Patent Publication No. 2021 / 0013034, which is incorporated herein by reference. It is contemplated that the precursor compositions of the present invention are mixed in the form of a vapor stream with a counter reactant in a manner that forms an organometallic material in oligomeric or polymeric form on the microelectronic device surface. In this manner, the film so formed becomes an EUV patternable film when rendered reactive with EUV light.
[0027] Suitable counter reactant(s) are compounds capable of displacing the alkoxide or amide groups of the compounds of formulas (I) and (II) above, and include materials such as water, peroxides, e.g., hydrogen peroxide, di- or polyhydroxy alcohols, hydrogen sulfide, hydrogen disulfide, trifluoroacetaldehyde monohydrate, fluorinated di- or polyhydroxy alcohols, and fluorinated glycols.
[0028] The thin film thus formed is SnO x where x is from about 1.5 to about 2. Moreover, these EUV patternable thin films generally vary in thickness from about 0.5 to about 100 nm.
[0029] In certain embodiments, the pulse time of the precursor compounds (i.e., duration of precursor exposure to the substrate) ranges from about 1 to 30 seconds. If a purge step is used, the duration is about 1 to 20 seconds or 1 to 30 seconds. In other embodiments, the pulse time of the co-reactant ranges from 5 to 60 seconds.
[0030] In one embodiment, deposition conditions include a temperature in the reaction zone of about 0° C. to about 250° C., or about 22° C. to about 150° C., and a reduced pressure of about 10 mTorr to about 10 Torr.
[0031] The precursor composition comprising the precursor compounds described herein, when used with the counter reactant materials mentioned above, can be used to form (a) tin-containing films and (b) high purity EUV patternable films. Any suitable deposition technique can be utilized, such as chemical vapor deposition (CVD), digital (pulsed) CVD, atomic layer deposition (ALD), or flowable chemical vapor deposition (FCVD). In the case of pulse deposition, a series of alternating pulses of the precursor composition and counter reactant(s) with or without intermediate (e.g., inert gas) purge steps can be utilized to increase the film thickness to a desired endpoint.
[0032] The compounds described herein may be reacted with the reaction counter reactant(s) in a reaction zone and the surface of the desired microelectronic device substrate in any suitable manner, for example, in a single wafer CVD or ALD, or in a furnace containing multiple wafers.
[0033] Alternatively, the method of the present invention can be carried out as an ALD or ALD-like method. As used herein, the term "ALD or ALD-like" refers to a method in which (i) each reactant, including a precursor composition comprising a compound selected from formula (I) and (II), counter reactant(s) are sequentially introduced into a reactor, such as a single-wafer ALD reactor, a semi-batch ALD reactor, or a batch furnace ALD reactor, or (ii) each reactant is exposed to the substrate or microelectronic device surface by moving or rotating the substrate to different sections of the reactor, each section being separated by an inert gas curtain, i.e., a space ALD reactor or a roll-to-roll ALD reactor. In certain embodiments, the thickness of the ALD film can be from about 0.5 nm to about 40 nm, and the deposition temperature ranges from about 30° C. to about 500° C.
[0034] The deposition methods disclosed herein may include one or more purge gases. The purge gases used to purge unconsumed reactants and / or reaction by-products are inert gases that do not react with either the precursor composition or the counter reactant(s). Exemplary purge gases include, but are not limited to, argon, nitrogen, helium, neon, and mixtures thereof. In certain embodiments, a purge gas such as Ar is supplied to the reactor at a flow rate ranging from about 10 to about 2000 sccm for about 0.1 to 1000 seconds, thereby purging unreacted materials and any by-products that may remain within the reactor. Such purge gases may also be utilized as an inert carrier gas for either or both of the precursor composition and the counter reactant(s).
[0035] The respective steps of supplying the precursor composition and the counter reactant(s) may be performed by varying the order for supplying them and / or by varying the stoichiometry of the resulting EUV patternable film.
[0036] Energy is applied to the precursor composition and co-reactant(s) in the reaction zone to induce a reaction and form an EUV patternable film on the microelectronic device surface. Such energy can be provided by, but is not limited to, thermal, pulsed thermal, plasma, pulsed plasma, helicon plasma, high density plasma, inductively coupled plasma, x-ray, electron beam, photon, remote plasma methods, and combinations thereof. In certain embodiments, a secondary RF frequency source can be used to modify the plasma characteristics at the substrate surface. In embodiments where deposition involves plasma, the plasma generation method can include a direct plasma generation method where the plasma is generated directly in the reactor, or a remote plasma generation method where the plasma is generated "remote" to the reaction zone and substrate and fed into the reactor.
[0037] As used herein, the term "microelectronic device" corresponds to a semiconductor substrate, including 3D NAND structures, flat panel displays, and microelectromechanical systems (MEMS), fabricated for use in microelectronic integrated circuits or computer chip applications. It is understood that the term "microelectronic device" is not meant to be limiting in any way and includes any substrate that contains N-type metal oxide semiconductor (nMOS) and / or P-type metal oxide semiconductor (pMOS) transistors and that will ultimately become a microelectronic device or microelectronic assembly. Such microelectronic devices include at least one substrate that may be selected from, for example, tin, SiO2, Si3N4, OSG, FSG, tin carbide, hydrogenated tin carbide, tin nitride, hydrogenated tin nitride, tin carbonitride, hydrogenated tin carbonitride, boron nitride, anti-reflective coatings, photoresists, germanium, germanium-containing, boron-containing, Ga / As, flexible substrates, porous inorganic materials, metals such as copper and aluminum, and diffusion barrier layers such as, but not limited to, TiN, Ti(C)N, TaN, Ta(C)N, Ta, W, or WN.
[0038] In the situation where the compounds of formula (I) and / or (II) are used with co-reactants or counter-reactants, particularly in EUV patterning, they may be provided in the form of a kit. The container of the kit must be suitable for storing and transporting said compositions, and advantageously includes a means for conveying the components in one or more containers into the reaction zone where the deposition of the tin-containing film or EUV-patternable film is formed on the microelectronic device substrate. Furthermore, the container(s) and the system may include a distribution port for dispensing the composition(s) to a process tool. For example, gas pressure may be applied to the head space of a conventional pressurized container, or a pump may be used to enable fluid communication for the introduction of such components into the reaction zone of a vapor deposition apparatus. Furthermore, the system may include a distribution port for dispensing the components to a process tool.
[0039] Thus, in a further aspect, the present invention provides a kit comprising, in one or more containers, one or more compounds of formula (I) and / or (II) as described herein and one or more compounds (i.e., counter reactants) selected from water, peroxide, a di- or polyhydroxy alcohol, hydrogen sulfide, hydrogen disulfide, trifluoroacetaldehyde monohydrate, a fluorinated di- or polyhydroxy alcohol, and a fluorinated glycol. EXAMPLES
[0040] Synthesis of 1,3-bis(bis(trimethylsilylamido)iodotin(IV)]propane Bis(bis(trimethylsilylamide))tin(II) (5 g, 11.3 mmol) was placed in a 40 mL scintillation vial equipped with a magnetic stir bar and dissolved in hexanes (15 mL) to form a dark orange / red solution. In a separate vial, 1,3-diiodopropane was dissolved in hexanes (10 mL) and added dropwise to the Sn(II)-containing solution with stirring over a period of 1 min. During the addition, the reaction exhibited a slight exotherm and presented as a pale orange solution, which was stirred at room temperature for 1 h. At this point, the reaction was concentrated by removing 15 mL of solvent under reduced pressure and the resulting orange solution was stored at -35 °C overnight. The next morning, the reaction presented as a frozen yellow solid. After warming to room temperature, yellow crystals suitable for solid-state X-ray crystallography were collected for analysis. The remaining reaction contents were dried under reduced pressure to give the target molecule as a free-flowing yellow powder (4.67 g, 70.4%). 1 H-NMR(C6D6,400 MHz);s,36H,0.41 ppm; 119 Sn-NMR(C6D6,150 MHz);-153.35 ppm.
[0041] Aspects In a first aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000010.tif27170 (in the formula, R 1is a group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-, R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 are H, -N(R)2, -OR, and -R 1 (selected from In one embodiment, a method is provided comprising: introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from the group consisting of:
[0042] In a second aspect, the present invention provides a method for the preparation of a compound comprising the steps of: 1 is a group of formula -N(R).
[0043] In a third aspect, the present invention provides a method for the preparation of a compound comprising the steps of: 2 is a group of formula -N(R)2.
[0044] In a fourth aspect, the present invention provides a method according to any one of the first to fourth aspects, wherein the vapor deposition conditions are atomic layer deposition conditions.
[0045] In a fifth aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000011.tif27170 (in the formula, R 1 is a divalent group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 are H, -N(R)2, -OR, and -R 1 (selected from A precursor composition comprising at least one compound selected from at least one counter reactant selected from compounds capable of reacting with -OR and -N(R); into a reaction zone under deposition conditions.
[0046] In a sixth aspect, the present invention provides a method for producing an EUV patternable film on a surface of a microelectronic device substrate, comprising: Formula (I): TIFF2024541464000012.tif27170 (in the formula, R 1 is a divalent group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 are H, -N(R)2, -OR, and -R 1 (selected from mixing a vapor flow of a precursor composition comprising at least one compound selected from the group consisting of: depositing a metal-organic material onto a surface of a substrate to form an EUV patternable film; The present invention provides a method comprising:
[0047] In a seventh aspect, the present invention provides a compound comprising: 1 is a group of formula -N(R)-.
[0048] In an eighth aspect, the present invention provides a compound comprising: 2 is a group of formula -N(R)2.
[0049] In a ninth aspect, the present invention provides the method of any one of the fifth to eighth aspects, wherein the vapor deposition conditions are atomic layer deposition conditions.
[0050] In a tenth aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000013.tif11170 (in the formula, R 1 is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 are H, -N(R)2, -OR, and -R 1 and m is an integer from 0 to 2. In one embodiment, a method is provided comprising: introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from the group consisting of:
[0051] In an eleventh aspect, the present invention provides a compound comprising R 1 is a group of formula -N(R)-.
[0052] In a twelfth aspect, the present invention provides a compound comprising: 2 is a group of formula -N(R)2.
[0053] In a thirteenth aspect, the present invention provides the method of any one of the tenth to twelfth aspects, wherein the vapor deposition conditions are atomic layer deposition conditions.
[0054] In a fourteenth aspect, the present invention provides a method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, the method comprising the steps of: TIFF2024541464000014.tif11170 (in the formula, R 1is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 are H, -N(R)2, -OR, and -R 1 and m is an integer from 0 to 2. A precursor composition comprising at least one compound selected from at least one counter reactant selected from compounds capable of reacting with -OR and -N(R); into a reaction zone under deposition conditions.
[0055] In a fifteenth aspect, the present invention provides a method for producing an EUV patternable film on a surface of a microelectronic device substrate, comprising: Formula (II): TIFF2024541464000015.tif11170 (in the formula, R 1 is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 are H, -N(R)2, -OR, and -R 1 and m is an integer from 0 to 2. mixing a vapor flow of a precursor composition comprising at least one compound selected from the group consisting of: depositing a metal-organic material onto a surface of a substrate to form an EUV patternable film; The present invention provides a method comprising:
[0056] In a sixteenth aspect, the present invention provides a method for the preparation of a compound comprising the steps of: 1 is a group of formula -N(R)-.
[0057] In a seventeenth aspect, the present invention provides a method for the preparation of a compound comprising the steps of: 2 is a group of formula -N(R)2.
[0058] In an eighteenth aspect, the present invention provides the method of any one of the fourteenth to seventeenth aspects, wherein the vapor deposition conditions are atomic layer deposition conditions.
[0059] In a nineteenth aspect, the present invention provides a compound of formula (I): TIFF2024541464000016.tif27170 (in the formula, R 1 is a group selected from -C(R)-, -CR(X)-, -O-, and -N(R)-, R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; and R 2 is selected from groups of formula -N(R)2 and -OR A precursor composition is provided that includes a compound of the formula:
[0060] In a twentieth aspect, the present invention provides a compound of formula (II): TIFF2024541464000017.tif11170 (in the formula, R 1 is a divalent radical selected from -CH-, -C=C-, -C≡C-, -O-, -N(R)-, -ORRO-, and -CH(X)-; R is selected from H and C1-C5 alkyl; X is selected from F, Cl, Br, I, -OCH3, -OCH2CH3, -OCH2CH2CH3, and -OCH(CH3)2; n is an integer from 0 to 5; R 2 is a group of formula -N(R)2, and m is an integer from 0 to 2. A precursor composition is provided comprising:
[0061] In a twenty-first aspect, the present invention provides a kit comprising, in one or more containers, one or more compounds of formula (I) and / or (II) as claimed in the nineteenth and twentieth aspects, and one or more compounds selected from water, peroxide, a dihydroxy or polyhydroxy alcohol, hydrogen sulfide, hydrogen disulfide, trifluoroacetaldehyde monohydrate, a fluorinated dihydroxy or polyhydroxy alcohol, and a fluorinated glycol.
[0062] Having thus described several exemplary embodiments of the present disclosure, those skilled in the art will readily appreciate that still other embodiments may be made and used within the scope of the appended claims. Many advantages of the present disclosure covered by this document have been set forth in the foregoing description. However, it will be understood that the present disclosure is in many respects merely illustrative. The scope of the present disclosure is, of course, to be defined in the language in which the appended claims are expressed.
Claims
1. 1. A method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, comprising: (In the formula, R 1 is -C(R) 2 is a group selected from -, -CR(X)-, -O-, and -N(R)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 and R 2 is H, -N(R) 2 , -OR, and -R 1 (selected from introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from:
2. R 1 The method of claim 1 , wherein is a group of the formula -N(R)-.
3. R 2 is represented by the formula -N(R 2 The method of claim 1 , wherein the group is
4. The method of claim 1 , wherein the deposition conditions are atomic layer deposition conditions.
5. 1. A method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, comprising: (In the formula, R 1 is -C(R) 2 a divalent group selected from -, -CR(X)-, -O-, and -N(R)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 and R 2 is H, -N(R) 2 , and -OR, and -R 1 (selected from A precursor composition comprising at least one compound selected from -OR and -N(R) 2 at least one counter reactant selected from compounds capable of reacting with into a reaction zone under deposition conditions.
6. R 1 The method of claim 5 , wherein is a group of the formula -N(R)-.
7. R 2 is represented by the formula -N(R 2 The method according to claim 5 , wherein the group is
8. The method of claim 5 , wherein the deposition conditions are atomic layer deposition conditions.
9. 1. A method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, comprising: (In the formula, R 1 is -CH 2 a divalent group selected from -, -C═C-, -C≡C-, -O-, -N(R)-, -O-R-R-O-, and -CH(X)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 is selected from n is an integer from 0 to 5; R 2 is H, -N(R) 2 , -OR, and -R 1 and m is an integer from 0 to 2. introducing into a reaction zone under deposition conditions a precursor composition comprising at least one compound selected from:
10. R 1 The method of claim 9, wherein is a group of formula -N(R)-.
11. R 2 is represented by the formula -N(R 2 The method of claim 9, wherein the group is
12. The method of claim 9 , wherein the deposition conditions are atomic layer deposition conditions.
13. 1. A method for depositing a tin-containing film on a surface of a microelectronic device in a reaction zone, comprising: (In the formula, R 1 is -CH 2 a divalent group selected from -, -C═C-, -C≡C-, -O-, -N(R)-, -O-R-R-O-, and -CH(X)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 is selected from n is an integer from 0 to 5; R 2 is H, -N(R) 2 , and -OR, and -R 1 and m is an integer from 0 to 2. A precursor composition comprising at least one compound selected from -OR and -N(R) 2 at least one counter reactant selected from compounds capable of reacting with into a reaction zone under deposition conditions.
14. R 1 The method of claim 13, wherein is a group of formula -N(R)-.
15. R 2 is represented by the formula -N(R 2 The method of claim 13, wherein the group is
16. The method of claim 13 , wherein the deposition conditions are atomic layer deposition conditions.
17. Formula (I): (In the formula, R 1 is -C(R) 2 is a group selected from -, -CR(X)-, -O-, and -N(R)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 and R 2 is represented by the formula -N(R 2 and -OR groups. A precursor composition comprising the compound of formula (I).
18. Formula (II): (In the formula, R 1 is -CH 2 a divalent group selected from -, -C═C-, -C≡C-, -O-, -N(R)-, -O-R-R-O-, and -CH(X)-; R is H and C 1 -C 5 alkyl, X is F, Cl, Br, I, -OCH 3 , -OCH 2 CH 3 , -OCH 2 CH 2 CH 3 , and -OCH(CH 3 ) 2 is selected from n is an integer from 0 to 5; R 2 is represented by the formula -N(R 2 and m is an integer from 0 to 2. A precursor composition comprising:
19. 20. A kit comprising, in one or more containers, one or more compounds of formula (I) and / or (II) according to claim 17 and one or more compounds selected from water, peroxide, di- or polyhydroxy alcohols, hydrogen sulfide, hydrogen disulfide, trifluoroacetaldehyde monohydrate, fluorinated di- or polyhydroxy alcohols, and fluorinated glycols.
Citation Information
Patent Citations
Method for producing polyfunctional (METH)acrylate
JP2008231003A
Method for forming an EUV patternable hard mask
JP2021523403A