Pixel unit for semiconductor device and manufacturing method thereof, microdisplay, individual device

The vertical stacking of pixel units with a common cathode and metal surrounding frame in Micro LED displays addresses the efficiency losses in horizontal arrangements, enhancing light emitting area and pixel density while simplifying the connection process.

JP2024542399AActive Publication Date: 2024-11-15NUOSHI TECH (SUZHOU) CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024526806
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-04-29
Filing Date
2022-10-28
Publication Date
2024-11-15
Estimated Expiration
2042-10-28

AI Technical Summary

Technical Problem

Conventional Micro LED display technologies face challenges with horizontal pixel unit arrangements that limit the light emitting area and reduce external quantum efficiency due to the small size of the light emitters, especially when the diameter of the source region is below 10 μm, leading to severe efficiency losses.

Method used

A vertical stacking of pixel units with a common cathode connected to each element layer, utilizing a metal surrounding frame as a common cathode body to reduce the cathode area ratio and increase the light emitting area, while also providing pixel isolation and optical crosstalk prevention.

Benefits of technology

The vertical stacking method enhances the light emitting area ratio, reduces the size effect impact, allows for increased number of stacked layers, and improves pixel density without increasing horizontal space, while simplifying the electrical connection process and enabling redundant circuits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024542399000001_ABST
    Figure 2024542399000001_ABST
Patent Text Reader

Abstract

This application discloses a pixel unit for semiconductor devices and a manufacturing method thereof, a microdisplay, and a discrete device. The pixel unit includes a target driving circuit, a display unit, and a common cathode. A driving circuit is provided on the back plate, and the driving circuit is provided with at least one anode. The display unit includes a first device layer and a second device layer provided on the back plate, which are stacked vertically from bottom to top. The first device layer and the second device layer are respectively connected to corresponding anodes of the back plate. The common cathode is respectively connected to each device layer of the display unit. The common cathode is connected to an external cathode. The pixel unit according to this application realizes multi-color display by stacking at least two device layers vertically on the back plate, and compared with a pixel structure stacked horizontally to realize full color, the pixel unit according to this application occupies a smaller horizontal space and has a smaller pixel density loss, and each layer stacked vertically in the display unit adopts a common cathode to increase the area ratio of the light-emitting area.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to the technical field of semiconductor devices, in particular to pixel units and manufacturing methods for semiconductor devices, microdisplays, and discrete devices. [Background technology]

[0002] Micro LED display technology refers to a display technology in which micron-order self-emitting LEDs are assembled into a driving panel as light-emitting pixel units to form a high-density LED array. Micro LED chips have characteristics such as small size, high integration, and self-emitting, and therefore have greater advantages in terms of brightness, resolution, contrast, energy consumption, service life, response speed, and thermal stability compared to LCD and OLED in terms of display. The applications of Micro LED have expanded from flat panel displays to many fields such as AR / VR / MR, spatial displays, flexible transparent displays, wearable / embedded photoelectric elements, optical communication / optical interconnection, medical detection, and smart car lights. For this reason, industry engineers are constantly optimizing Micro LED display technology.

[0003] When Micro LED display technology is applied to the above fields, there is usually a demand for full-color display. Published Chinese patent CN201880019435 discloses a method for manufacturing a semiconductor device by stacking layers of Micro LEDs. As shown in FIG. 1, the semiconductor structure is a cross-sectional view of several pixels of an integrated multi-color LED display panel. As can be seen from FIG. 1, the Micro LEDs 140RGB are included in different layers 155R, 155G, and 155B stacked on top of a back plate and pixel driver. In one embodiment, the bottom layer 155R includes red Micro LEDs 140R, the middle layer 155G includes green Micro LEDs 140G, and the top layer 155B includes blue Micro LEDs 140B. Thus, the patent is essentially a horizontally arranged RGB tri-color scheme.

[0004] Those skilled in the art should be aware that for pixel units arranged horizontally, the proportion of the emitter in the source region in the pixel area greatly limits the size of the emitter, affecting the light-emitting area, and at the same time, the micro-LED device has a size effect in that the external quantum efficiency (EQE) drops sharply as the size decreases, and the drop is particularly severe when the diameter of the source region drops to 10 μm or less. Also, when the size of the source region decreases, the smaller the size of the source region, the lower the EQE for the same current density, and the EQE attenuation is more serious when the size of the source region is 20 μm or less.

[0005] Therefore, the stacking method of pixel horizontal array arrangement or essentially horizontal array arrangement adopted in the prior art is not very ideal in terms of light emitting area and external quantum efficiency.

[0006] Therefore, there is a need to find a pixel unit that can realize a multi-color display and effectively increase the size ratio of the source-containing area. Summary of the Invention

[0007] An object of the present application is to provide a pixel unit for a semiconductor device, a manufacturing method thereof, a microdisplay, and an individual device, which are capable of realizing a multi-color display with a large ratio of the area of ​​a source-containing region.

[0008] In order to achieve the above object of the present application, according to a first aspect of the present application, a back plate and a display unit provided on the back plate, the display unit including a first element layer and a second element layer vertically stacked in sequence, the second element layer being provided on a surface of one side of the first element layer spaced apart from the back plate, the first element layer and the second element layer being respectively connected to the back plate; A pixel unit for a semiconductor device is provided, the pixel unit including: a common cathode respectively connected to each element layer of the display unit.

[0009] In a preferred embodiment, the common cathode includes a common cathode body and a first connection part and a second connection part respectively connected to the common cathode body; the first connection portion is connected to the first element layer; The second connection portion is connected to the second element layer.

[0010] In a preferred embodiment, the back plate is provided with a driving circuit including at least two anodes; Any one of the anodes is connected to a corresponding device layer; At least two of the anodes are both located in a projection range of the display unit on the back plate; The common cathode is connected to an external cathode.

[0011] In a preferred embodiment, the first element layer includes a first bonding layer, a first compound light-emitting layer, and an insulating coating layer, which are provided in this order; the first compound light-emitting layer is provided on one surface of the first bonding layer spaced from the back plate, The insulating coating layer covers the first bonding layer and the first compound light-emitting layer.

[0012] In a preferred embodiment, the first bonding layer is made of a conductive material, A first insulating layer is provided between the back plate and the first bonding layer, At least one first through hole is formed in the first insulating layer, The first bonding layer is connected to the corresponding first anode through the first through hole.

[0013] In a preferred embodiment, the common cathode is provided inside the display unit, or The common cathode body is a metal surrounding frame provided in a circumferential direction of the display unit, and the first connection portion and the second connection portion are provided inside the display unit.

[0014] In a preferred embodiment, the first bonding layer is made of an insulating material, the first element layer further includes a first P-type ohmic contact layer provided between the first bonding layer and the first compound light-emitting layer; the first P-type ohmic contact layer includes a first P-type ohmic contact layer extension portion that extends toward the common cathode but does not contact the common cathode; The first device layer further includes a first electrical connection structure having one end connected to a corresponding first anode and a free end passing through the first bonding layer and connected to the first P-type ohmic contact layer extension.

[0015] In a preferred embodiment, the common cathode body is a metal surrounding frame provided in the circumferential direction of the display unit.

[0016] In a preferred embodiment, the first connection portion is connected to the first compound light-emitting layer.

[0017] In a preferred embodiment, the first element layer further includes a first cathode ohmic contact layer provided on one surface of the first compound light emitting layer spaced from the first bonding layer, The first connection portion is connected to the first cathode ohmic contact layer.

[0018] In a preferred embodiment, the second element layer includes the second bonding layer, the second compound light-emitting layer, and an insulating coating layer, the second compound light emitting layer is provided on one surface of the second bonding layer spaced apart from the first element layer, The insulating coating layer covers the first bonding layer and the first compound light-emitting layer.

[0019] In a preferred embodiment, the second bonding layer is made of a transparent conductive material or a transparent semiconductor material, The second device layer further includes a second electrical connection structure having one end connected to a second anode of the backplate and another end passing through the first device layer and connected to the second bonding layer.

[0020] In a preferred embodiment, the second electrical connection structure includes a first metal pillar having one end connected to a corresponding second anode and another end passing through the first element layer and connected to the second bonding layer; or The second electrical connection structure includes a first connection layer that passes through the first insulating layer and is connected to a corresponding second anode, and a first metal pillar that is connected to the first connection layer and is also connected to the second bonding layer.

[0021] In a preferred embodiment, the second bonding layer is made of a transparent insulating material, the second element layer includes a second P-type ohmic contact layer provided between the second bonding layer and the second compound light-emitting layer; the second P-type ohmic contact layer includes a second P-type ohmic contact layer extension portion that extends toward the common cathode but does not contact the common cathode; The second device layer further includes a third electrical connection structure having one end connected to a corresponding third anode and a free end passing through the first device layer and connected to the second P-type ohmic contact layer extension.

[0022] In a preferred embodiment, the compound light emitting material used in the first compound light emitting layer and the compound light emitting material used in the second compound light emitting layer are the same; The first and second device layers are connected to the same anode so as to be arranged in series or in parallel.

[0023] In a preferred embodiment, the display unit further includes a third element layer provided on one side of the second element layer spaced apart from the first element layer, the third device layer is connected to a third anode of the backplate; the common cathode further includes a third connection portion connected to the common cathode body; The third connection portion is connected to the third element layer.

[0024] In a preferred embodiment, the thickness of the common cathode decreases from one end adjacent the backplate to the other end.

[0025] In a preferred embodiment, the display further comprises an optical enhancement structure laminated to one side of the display unit spaced from the back plate.

[0026] In a preferred embodiment, the back plate is provided with N anode pads and one cathode pad; a portion of the anode pad and a portion of the cathode pad are each disposed within the back plate, and N≧1; Any one of the anode pads is connected to a corresponding device layer; The cathode pads are respectively connected to each element layer via the common cathode.

[0027] In a preferred embodiment, the display unit is provided separately from the back plate, and the at least two pads are provided separately from the back plate; It further includes a self-supporting structure covering the element body and a portion of the backplate.

[0028] In a preferred embodiment, the self-supporting structure includes a covering part and a fixing part which are connected in series, the covering part covers the display unit, and the fixing part is provided on the back plate; or The self-supporting structure includes a covering portion, a second connection portion and a fixing portion which are connected in sequence, the covering portion covers the display unit, the fixing portion is provided on the back plate, and the second connection portion is provided separately from the back plate.

[0029] According to a second aspect, the method includes the steps of: providing a back plate having a driving circuit provided thereon and at least one anode provided thereon; A first compound semiconductor prepared in advance is bonded to the back plate, and a first element layer and at least one surface corresponding to the first element layer are bonded to the back plate. First connection part A second compound semiconductor is bonded to a surface of one side of the first element layer spaced from the back plate, and a second element layer and a surface of at least one side of the second element layer in the circumferential direction are bonded to the second compound semiconductor. Second connection part and connecting the second device layer to the corresponding anode of the backplate and the Second connection part and a common cathode is formed. Second connection part and the above First connection part and fabricating a display unit and a corresponding common cathode to connect with each other.

[0030] In a preferred embodiment, the step of bonding the first compound semiconductor to the back plate using a conductive material and bonding a first compound semiconductor prepared in advance to the back plate includes: Coating an insulating material on the entire surface of the back plate on which the at least two anodes are provided, and forming at least two first through holes corresponding to the at least two anodes; coating an electrically conductive material over the entire surface of the backplate after coating the insulating layer to form a backplate coated with a bonding material; coating an electrically conductive material over the entire surface of the first compound semiconductor to form a first compound semiconductor coated with a bonding material; bonding the back plate coated with a bonding material to the first compound semiconductor; removing the first compound semiconductor substrate.

[0031] In a preferred embodiment, a first element layer and a second element layer are provided on at least one surface of the first element layer in a circumferential direction. First connection part The steps to build patterning the first compound semiconductor by exposing and etching the first compound semiconductor to form a first device layer corresponding to the pattern of the back plate, and pre-remaining at least one first through hole corresponding to the remaining anode; providing a first cathode ohmic contact layer on a surface of the first device layer spaced from the first bonding layer; constructing at least one metal pillar for a subsequent device layer other than the first device layer in at least one of the first through holes by semiconductor patterning coating; Passivating the first compound semiconductor by coating the entire surface of the first compound semiconductor; patterning and etching the first compound semiconductor after being blanket passivated with silicon oxide by a semiconductor patterning and etching process, so as to form electrical through holes corresponding to the remaining anode and the first cathode ohmic contact layer; Remaining anode electrical connections and First connection part and filling the formed electrical vias such that

[0032] In a preferred embodiment, the step of bonding a first compound semiconductor to the back plate using an insulating material to form a first bonding layer includes: Coating the entire surface of the back plate with an insulating material; forming a first P-type ohmic contact layer on a surface of a first compound semiconductor, and coating an insulating material on the entire surface of the first P-type ohmic contact layer; bonding the back plate and the first compound semiconductor; removing the first compound semiconductor substrate.

[0033] In a preferred embodiment, a first element layer and a second element layer are provided on at least one surface of the first element layer in a circumferential direction. First connection part The steps to build constructing a first element layer corresponding to the back plate pattern by patterning etching to expose a corresponding first P-type ohmic contact layer extension; forming at least one second through hole corresponding to at least one of the anodes in the first P-type ohmic contact layer extension by patterning etching; Passivating the first compound semiconductor by coating the entire surface of the first compound semiconductor; patterning and etching the first compound semiconductor after being passivated with silicon oxide over its entire surface by a semiconductor patterning and etching process, so as to form electrical through holes corresponding to each anode and electrical through holes corresponding to the first cathode ohmic contact layer; A first electrical connection structure corresponding to the first compound light-emitting layer, a second electrical connection structure corresponding to the second compound light-emitting layer, and a First connection part and filling the formed electrical via such that

[0034] In a preferred embodiment, the second element layer and the second element layer are provided on at least one surface in a circumferential direction. Second connection part After the completion of the above, the steps of manufacturing the display unit and the common cathode include: A third compound semiconductor prepared in advance is bonded to a surface of one side of the second element layer spaced apart from the first element layer, and is provided on a third element layer and at least one surface of the third element layer in a circumferential direction. Third connection part

[0023] Further comprising:

[0035] According to a third aspect, the method includes the steps of constructing at least two pads, including N anode pads and one cathode pad, N≧1, partially disposed inside a pre-prepared back plate; and sequentially stacking a first element layer and a second element layer on one side of a back plate on which at least two of the pads are provided, the first element layer and the second element layer being connected to corresponding anode pads along a direction away from the back plate so as to form a display unit, and both being connected to the cathode pads via a common cathode formed thereon.

[0036] In a preferred embodiment, before providing at least two pads on a pre-prepared backing plate, Etching at least two cavities corresponding to the at least two pads in a pre-prepared back plate; The method further includes coating the backplate, having at least two cavities formed therein, with a sacrificial layer.

[0037] In a preferred embodiment, after the step of sequentially stacking a first element layer and a second element layer on one side of a back plate on which at least two of the pads are provided in a direction away from the back plate to form a display unit, coating a surface of the display unit with a dielectric material extending over a portion of a surface of the backplate such that a self-supporting structure is formed; and etching a sacrificial layer on a surface of one side of the backplate that is not coated with the dielectric material such that at least two of the pads are separated from the backplate; The etch rate ratio between the sacrificial layer and the backplate is greater than 10:1, and the etch rate ratio between the sacrificial layer and the self-supporting structure is greater than 10:1.

[0038] According to a fourth aspect, a microdisplay backplate including at least two driving circuits, an input interface and an output interface; A display area provided on the microdisplay back plate, the display area including a display unit included in at least two of the pixel units for semiconductor elements according to any one of the first aspects or a display unit included in a pixel unit manufactured by the manufacturing method according to any one of the second aspects; a surrounding common cathode electrically connected to the common cathode of each of the display units, respectively.

[0039] According to a fifth aspect, a discrete element backplate including at least two anode pads and at least one cathode pad; An element body provided on the individual element back plate, the element body including a display unit included in a pixel unit for semiconductor element according to at least two of the first aspects or a display unit included in a pixel unit manufactured by the manufacturing method according to the third aspect; 16. A discrete element comprising:

[0040] Compared with the prior art, the present application has the following beneficial effects:

[0041] According to the present application, a pixel unit for semiconductor devices and a manufacturing method thereof, a microdisplay, and a discrete device are provided. The pixel unit includes a back plate. A display unit is provided on the back plate. The display unit includes a first element layer and a second element layer that are stacked vertically from bottom to top. The second element layer is provided on one side of the first element layer, which is spaced apart from the back plate. The first element layer and the second element layer are respectively connected to the back plate. A common cathode is respectively connected to each element layer of the display unit. The pixel unit according to the present application realizes multi-color display by stacking at least two element layers vertically on the back plate, and compared with a pixel structure that is stacked horizontally to realize full color, the pixel unit according to the present application occupies a smaller horizontal space and has a smaller loss of pixel density. Furthermore, by adopting a common cathode for each layer that is stacked vertically in the display unit according to the present application, the proportion of the area of ​​the cathode in the display unit can be reduced, the proportion of the area of ​​the light-emitting area can be increased, and the influence of the size effect can be reduced, while at the same time, the number of stacked element layers in the vertical direction can be increased or a redundant circuit can be formed.

[0042] In addition, the common cathode body is a metal surrounding frame arranged in the circumferential direction of the display unit. The present application not only realizes the common cathode of each element layer inside the pixel by providing a metal surrounding frame, but also realizes the connection between all pixels and the common cathode, i.e., the common cathode of all pixels, and at the same time, the metal surrounding frame can be pixel isolation to prevent optical crosstalk between pixels, and has the function of a sidewall reflector.

[0043] Furthermore, the thickness of the common cathode decreases from one end adjacent the backplate to the other end to form an inverted bowl-shaped peripheral cathode as a constrained sidewall reflector structure.

[0044] Furthermore, the pixel individual element of the present application is connected to an external circuit based on at least two pads, and when sealing the individual element to a target backplate and making an electrical connection, metal welding such as eutectic welding can be avoided so as to avoid affecting the performance of the individual element itself and to simplify the process.

[0045] Furthermore, the display unit of the present application is provided separately from the back plate, and the at least two pads are provided separately from the back plate. The pixel unit further includes a self-supporting structure. The self-supporting structure covers the display unit and a part of the back plate. The pixel unit provides the self-supporting structure, which realizes the structural stability when the display unit and the back plate are provided separately and the convenience of access in later use. More importantly, in this structure, the back plate can be used repeatedly, which reduces the cost.

[0046] Furthermore, the self-supporting structure includes a covering part, a second connecting part, and a fixing part, which are connected in sequence. The covering part covers the display unit. The fixing part is provided on the back plate. The second connecting part is provided separately from the back plate. According to the self-supporting structure in this structure, in addition to ensuring the fixing function of the element layer by the self-supporting structure, the convenience of operation is improved when the covering part and the fixing part are broken by an external force during movement. More importantly, the breaking position is located in the second connecting part, not in the covering part or the fixing part, so that damage to the back plate or the element layer is avoided.

[0047] Furthermore, the manufacturing method of a pixel unit for a semiconductor device according to the present application adopts a method of first constructing a metal pillar, then passivating, and then etching the passivation layer to construct an electrical through hole, and then filling the electrical through hole so that an electrical connection is formed, in the process of stacking and constructing the element layer. This method reduces the difficulty of the electrical connection process in the stacking method compared to the conventional method of etching a metal layer to construct an electrical connection, and improves the feasibility of the electrical connection structure, especially for metals (such as copper) that are difficult to dry etch. [Brief description of the drawings]

[0048] [Figure 1] FIG. 1 is a schematic diagram showing a structure of a semiconductor element according to the background art. [Diagram 2] FIG. 2 is a top view of the pixel unit according to the first embodiment. [Diagram 3] 3 is a cross-sectional view taken along line xx in FIG. 2. [Figure 4] 3 is a cross-sectional view taken along the line yy in FIG. 2. [Diagram 5] FIG. 2 is a schematic diagram showing an exemplary circuit structure of the back plate of Example 1. [Figure 6] FIG. 2 is a schematic diagram showing a circuit structure of one of the element layers. [Figure 7] FIG. 1 is a schematic diagram showing a circuit structure in which at least two device layers of the same compound light emitting layer material are provided in parallel. [Figure 8] FIG. 1 is a schematic diagram showing a circuit structure in which at least two device layers of the same compound light emitting layer material are arranged in series. [Figure 9] FIG. 2 is a schematic diagram showing the structure of a pixel unit having an optical reinforcement structure according to the first embodiment; [Figure 10] The bonding material of Example 1 is coated on the back plate. [Figure 11] FIG. 2 is a top view of the first element layer of Example 1 after construction. [Figure 12] 12 is a cross-sectional view taken along line xx in FIG. 11 . [Figure 13] 12 is a cross-sectional view taken along the line yy in FIG. 11 . [Figure 14] FIG. 2 is a top view after the electrical connection circuit of Example 1 is constructed. [Figure 15] 15 is a cross-sectional view taken along the line xx in FIG. 14. [Figure 16] 15 is a cross-sectional view taken along the line yy in FIG. 14. [Figure 17] 2 is a cross-sectional view of the xx cross section after electrical connection of the first element layer in Example 1 is completed. [Figure 18] 1 is a cross-sectional view of the yy cross section after electrical connection of the first element layer in Example 1 is completed. [Figure 19]1 shows visible light transmittance data when silicon is used as the bonding material in Example 1. [Figure 20] FIG. 11 is a cross-sectional view of the xx section of Example 2. [Figure 21] FIG. 11 is a cross-sectional view of the yy cross section of Example 2. [Figure 22] FIG. 11 is a cross-sectional view of a bowl-shaped common cathode of a pixel unit according to a second embodiment; [Figure 23] FIG. 11 is a top view of a pixel unit according to a third embodiment. [Figure 24] This is a cross-sectional view taken along line y3-y3. [Diagram 25] FIG. 11 is a cross-sectional view of Example 3 when lamination of the first layer is completed. [Figure 26] FIG. 11 is a cross-sectional view of Example 3 when lamination of the second layer is completed. [Figure 27] FIG. 11 is a schematic diagram showing a three-dimensional structure of a microdisplay according to a fourth embodiment. [Figure 28] FIG. 13 is a top view of a pixel level discrete element according to a fifth embodiment. [Figure 29] 29 is a cross-sectional view of the pixel level discrete element (comprising two element layers) of FIG. 28 along the AA direction. [Diagram 30] 29 is a cross-sectional view of the pixel level discrete element (comprising three element layers) of FIG. 28 along the AA direction. [Diagram 31] FIG. 29 is a cross-sectional view of the pixel level discrete element (comprising three element layers) of FIG. 28 in the BB direction. [Diagram 32] FIG. 11 is a top view of the backing plate and at least one pad of Example 5. [Diagram 33] 33 is a cross-sectional view of FIG. 32 in the BB direction (solid pad). [Diagram 34] 33 is a cross-sectional view of the hollow pad taken along the line BB in FIG. 32. [Diagram 35] FIG. 11 is a cross-sectional view of a pixel level discrete element (comprising two element layers) of Example 6 taken along the AA direction. [Diagram 36] FIG. 13 is a cross-sectional view of a pixel level discrete element (comprising two element layers) of Example 6 in the BB direction. [Figure 37]FIG. 13 is a cross-sectional view in the BB direction of a pixel level discrete element (comprising three element layers) of Example 6. [Figure 38] FIG. 13 is a cross-sectional view in the BB direction of a pixel level discrete element (comprising three element layers) of Example 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0049] In order to make the objectives, technical means and advantages of the present application clearer, the following will clearly and completely describe the technical means in the embodiments of the present application with reference to the drawings in the embodiments of the present application. Obviously, the described embodiments are only a part of the embodiments of the present application, but not all of the embodiments. Based on the embodiments of the present application, all other embodiments that a person skilled in the art can obtain without creative efforts are all within the scope of protection of the present application.

[0050] In the description of this application, the orientation or positional relationship indicated by terms such as "upper", "lower", "inner", and "outer" is based on the orientation or positional relationship shown in the drawings, and is for convenience and simplification of the description, and does not indicate or imply that the referred device or element must have a specific orientation or be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first" and "second" are used for descriptive purposes only, and are not to be understood as indicating or implying relative importance or implying the number of the indicated technical features. Thus, a feature defined as "first" or "second" may include one or more of the feature, either explicitly or implicitly. In the description of this application, unless otherwise specified, "plurality" means two or more.

[0051] In the description of this application, unless otherwise expressly specified or limited, the terms "attached", "connected to each other", and "connection" should be understood in a broad sense. For example, they may be fixed connections, detachable connections, or integral connections. They may be mechanical connections or electrical connections. They may be direct connections, indirect connections via intermediate media, or internal communication between two elements. For those skilled in the art, the specific meanings of the above terms in this application may be understood on a case-by-case basis.

[0052] As described in the Background section, conventional Micro-LED semiconductor devices generally adopt a horizontal stacking method to realize full color, but the horizontal stacking causes problems such as a large horizontal space occupied and a small light-emitting area ratio, which seriously affects the development of miniaturization of devices. For this reason, according to the present embodiment, a pixel unit for a semiconductor device, a manufacturing method thereof, and a micro display are provided that can effectively solve the above problems. Example 1

[0053] 2 to 4, according to the present embodiment, a pixel unit 100 for a semiconductor device is provided, which includes a back plate 10, a display unit 20 and a common cathode 30. The pixel unit 100 is used in semiconductor devices such as microdisplays and invisible light detectors.

[0054] Note: Figures 3 and 4 are two cross-sectional views of Figure 2 (top view) that are perpendicular to each other. All subsequent structural drawings are top views or corresponding cross-sectional views of the current structure. The xx cross section is a cross section in the horizontal direction of the top view, and the yy cross section is a cross section in the vertical direction of the top view.

[0055] Here, the back plate 10 is provided with a driving circuit. The driving circuit is provided with at least one anode. Exemplarily, a circuit diagram of the driving circuit is shown in FIG. 5. Note that the circuit diagrams of this embodiment are simple schematic diagrams, and all are active driving. The internal circuit of the pixel unit may include an active, passive or semi-passive control circuit. Exemplarily, FIG. 6 below is a circuit diagram of any one of the element layers. The display unit 20 is provided on the back plate 10 and includes a first element layer 21 and a second element layer 22 that are vertically stacked from bottom to top. The first element layer 21 and the second element layer 22 are respectively connected to the corresponding anodes of the back plate 10. Therefore, the pixel unit 100 of this embodiment is a vertical stack pixel (hereinafter referred to as VSP). The common cathode 30 is provided in the display unit 20 and is respectively connected to each element layer of the display unit 20. The common cathode 30 is connected to an external cathode. The common cathode 30 of this embodiment is preferably one of a columnar structure or a plate structure.

[0056] Of course, the number of vertically stacked device layers in this embodiment includes but is not limited to two layers, and may be three layers, four layers, or more, and the materials of the compound light-emitting layers used in all device layers may be the same or different. When the compound light-emitting layers used in each device layer are different, a multi-color display such as a full-color display can be realized. When the same compound light-emitting layer is used in two or more device layers, the light irradiation intensity can be enhanced or a redundant structure can be formed. Of course, the two methods can coexist in the same display unit 20, and this embodiment is not limited thereto.

[0057] For convenience of description, in this embodiment, the display unit 20 includes a first element layer 21, a second element layer 22 and a third element layer 23, and the first element layer 21 emits red light (R), the second element layer 22 emits green light (G), and the third element layer 23 emits blue light (B), that is, R, G, B full-color pixels are realized. For example, the first element layer 21 uses red InGaN compound epitaxy, the second element layer 22 uses green InGaN compound epitaxy, and the third element layer 23 uses blue InGaN compound epitaxy.

[0058] Specifically, the back plate 10 is one of a thin film transistor (TFT), a low temperature polysilicon (LTPS), a CMOS integrated circuit, and a high electron mobility transistor (HEMT). For convenience of explanation, the present embodiment takes the CMOS integrated circuit as an example for further detailed explanation, but is not limited thereto. Furthermore, the at least two anodes (anode through-holes) included in the back plate 10 are uniformly arranged, and the at least two anodes are all located in the projection range of the display unit 20 on the back plate 10. The at least two anodes are uniformly arranged. In the embodiment of three element layers, possible arrangement manners include distribution on a same line or distribution in a character shape. The preset number of anodes may be disposed at the edge, apex, center, or center of the back plate 10. In this embodiment, the number of anode through-holes provided in the back plate 10 is not limited, and the increase in the number of anode through-holes can realize the formation of more VSP stacks or redundant circuits. It should be noted that a cathode (cathode through-hole) may be provided in the back plate 10 so as to realize a connection between the common cathode 30 and a drive circuit.

[0059] In addition, the back plate 10 includes at least one top metal covering the at least one anode. Of course, the back plate 10 may not include a top metal, and this embodiment is not limited thereto.

[0060] The back plate 10 also includes an in-situ reflector disposed on its upper surface, which covers or exposes the at least one anode. The in-situ reflector may be a metal, aluminum, gold, silver, etc., or may be a Bragg reflector layer in which two or more thin films with different refractive indexes are stacked, such as a stack of silicon oxide and titanium oxide, silicon oxide and alumina, or silicon oxide and silicon nitride, or may be an ODR total reflector in which a metal and a dielectric are stacked, such as at least one combination of silver and silicon oxide, aluminum and alumina, gold and silicon oxide, etc. For example, a stack of metal aluminum 250 nm and silicon oxide 150 nm (target wavelength 620 nm, 1 / 4 is 150 nm) has excellent reflectance in a part of the visible light wavelength range.

[0061] The in situ reflector may be a polygonal structure such as a circle, triangle, square, pentagon, hexagon, octagon, or a compound polygon that avoids normally open contacts. The polygon may be inscribed in the pixel boundary or may be reduced from the boundary by a certain length.

[0062] 2 to 4, the common cathode 30 of this embodiment includes a common cathode body 31, and a first connection portion 32, a second connection portion 33, and a third connection portion 34, each of which is connected to the common cathode body 31. The first connection portion 32 is connected to the first element layer 21, the second connection portion 33 is connected to the second element layer 22, and the third connection portion 33 is connected to the third element layer 23.

[0063] Specifically, the first element layer 21 includes a first bonding layer 211, a first compound light-emitting layer 212, and an insulating coating layer 24, which are provided in this order from bottom to top. The first compound light-emitting layer 212 is provided on one surface of the first bonding layer 211 spaced apart from the back plate 10, and the insulating coating layer 24 covers the first bonding layer 211 and the first compound light-emitting layer 212.

[0064] Preferably, the insulating coating layer 24 may be an inorganic dielectric material such as silicon oxide, silicon nitride, alumina, or an organic dielectric material such as SU8, polyimide, etc., but is not limited thereto in this embodiment.

[0065] A conductive material or an insulating material is used for the first bonding layer 211. In this embodiment, the first bonding layer 211 is made of a conductive material. A first insulating layer 214 is provided between the back plate 10 and the first bonding layer 211. At least one first through hole is formed in the first insulating layer 214. The first bonding layer 211 is connected to the corresponding first anode 13 through the first through hole so as to avoid a situation in which a short circuit occurs at the bottom of the pixel stack. The conductive material used for the first bonding layer 211 may be a compound material such as ITO, ZnO, GaP, GaAs, GaN, etc., a metal material such as Au, Al, Cu, or a semiconductor material such as Si, an organic dielectric material such as SUB, BCB, etc. In addition, since the first bonding layer 211 does not have a requirement of light transparency, either a transparent or opaque conductive material may be used, and is not limited here. The first bonding layer 211 used may be a SiO2 film, and the thickness of the SiO2 film is 100±5 nm.

[0066] On this basis, the first compound light emitting layer 212 is bonded to the back plate 10 via the first compound semiconductor and obtained by removing the substrate.

[0067] In this embodiment, the first compound semiconductor forms a P-type ohmic contact on the P contact surface. The P-type ohmic contact material may be a transparent conductive material such as ITO, or may be a laminate or alloy of metal materials such as Au, Zn, and Be. It is preferable that the P contact surface is coated with ITO by deposition, sputtering, etc., and the thickness of the ITO film is 500 nm, and the ohmic contact is formed by annealing at a high temperature of 500°C in an N2 environment. Of course, the thickness of the P contact coating contact layer on the compound surface and the conditions for forming the contact can be adjusted and changed as necessary.

[0068] Exemplarily, when the substrate is N-GaAs and the red light is AlGaInP based, the structure is shown in Table 1 below.

[0069] [Table 1]

[0070] In the case of InGaN, the structure diagram can be shown in Table 2 or Table 3 below, and these two can be simultaneously used as wavelength compound structures such as blue light and green light.

[0071] [Table 2]

[0072] [Table 3]

[0073] Furthermore, the first connection unit 32 is connected to the first compound light-emitting layer 212. In a preferred embodiment, the first element layer 21 further includes a first cathode ohmic contact layer 215. The first cathode ohmic contact layer 215 is provided on one surface of the first compound light-emitting layer 212 spaced apart from the first bonding layer 211. The first connection unit 32 is connected to the first cathode ohmic contact layer 215 and is electrically connected to the first compound light-emitting layer 212 via the first cathode ohmic contact layer 215. Furthermore, the first connection unit 32 in this embodiment is provided vertically.

[0074] As shown in FIG. 4, the common cathode 30 of this embodiment is disposed vertically upward from the surface of the first compound light-emitting layer 212, and the subsequent second connection portion 33 and third connection portion 34 are both disposed horizontally.

[0075] 3 and 4, the second element layer 22 includes a second bonding layer 221, a second compound light-emitting layer 222, and an insulating coating layer 24. The second compound light-emitting layer 222 is provided on one surface of the second bonding layer 221 spaced apart from the first element layer 21. The insulating coating layer 24 covers the second bonding layer 221 and the second compound light-emitting layer 222.

[0076] The second bonding layer 221 may be made of a conductive material or an insulating material, but a transparent material is used for the second bonding layer 221 in order to transmit the red light of the first element layer 21. Illustratively, the second bonding layer 221 in this embodiment is made of a transparent conductive material or a transparent semiconductor material.

[0077] On this basis, the second element layer 22 further includes a second electrical connection structure 25 for realizing electrical connection with the corresponding second anode 14 of the back plate 10. The second electrical connection structure 25 has one end connected to the corresponding second anode 14 exposed on the back plate 10, and the other end connected to the second bonding layer 221 through the first element layer 22.

[0078] Furthermore, the second electrical connection structure 25 may be realized in various ways. In one implementation, the second electrical connection structure 25 includes a first metal pillar 251. One end of the first metal pillar 251 is connected to the corresponding second anode 14, and the other end is connected to the second bonding layer 221 through the first element layer 21. In another implementation, the second electrical connection structure 25 includes a first connection layer 252 and a first metal pillar 251 connected to the first connection layer 252. The first connection layer 252 is connected to the corresponding second anode 14 through the first insulating layer 214. The first metal pillar 251 is connected to the second bonding layer 221. Here, the first connection layer 252 may be formed by a bonding material that covers the second anode 14 that is left when the element is constructed by etching, or may be pre-fabricated and formed by a semiconductor patterning coating process manufacturing after the element is constructed by etching so that a through-hole of the exposed second anode 14 is formed.

[0079] As mentioned above, when the compound luminescent material used in the first compound luminescent layer 212 and the second compound luminescent layer 222 is the same, the first device layer 21 and the second device layer 22 are connected to the same anode to be arranged in series or parallel. It can be seen that in a compound VSP stack of N (N≧2) layers, when the compound luminescent material used in at least two device layers is the same, these two device layers can realize performance enhancement and pixel yield guarantee as redundancy as a vertical redundant structure, and at least two such device layers adopt common anode and common cathode electrical connection within a pixel.

[0080] For example, in a pixel unit of a full-color microdisplay, a driving circuit in which two element layers of the same compound light-emitting layer are connected in parallel is shown in FIG. 7, and a driving circuit in which two element layers of the same compound light-emitting layer are connected in series is shown in FIG. 8.

[0081] In this embodiment, the second electrical connection structure 25 and the first element layer 21 are not in contact with each other, so there is a certain degree of overlap and misalignment between the first element layer 21 and the second element layer 22 projected onto the back plate 10. The misalignment is used for positioning the second electrical connection structure 25 and the common cathode 30 in the vertical direction.

[0082] In a preferred embodiment, the second element layer 22 further includes a second cathode ohmic contact layer. The second cathode ohmic contact layer is provided on one surface of the second compound light-emitting layer 222 spaced apart from the second bonding layer 221. The second connection 33 is connected to the second cathode ohmic contact layer. More preferably, the second connection 33 is provided horizontally.

[0083] As with the first element layer 21, assuming that the second compound light-emitting layer 222 is set, the insulating coating layer 24 of the second element layer 22 and the insulating coating layer 24 of the first element layer 21 are made of the same material, and a detailed explanation of this is omitted in this embodiment.

[0084] Similar to the first element layer 21 and the second element layer 22, the third element layer 23 is laminated on one side of the second element layer 22 spaced apart from the first element layer 21. The third element layer 23 is connected to a third anode of the back plate 10. The common cathode 30 further includes a third connection portion 34 connected to the common cathode body 31. The third connection portion 34 is connected to the third element layer 23.

[0085] Specifically, the third element layer 23 similarly includes a third bonding layer 231, a third compound light-emitting layer 232, an insulating coating layer 24, a fourth electrical connection structure 26, and a third cathode ohmic contact layer. The third bonding layer 231 is made of a transparent conductive material (such as ITO). The fourth electrical connection structure 26 has one end connected to the third bonding layer 231, and the other end connected to the third anode 15 of the back plate 10 through the first element layer 21 and the second element layer 22. The third connection portion 34 included in the common cathode 30 is preferably connected to the common cathode body 31 via the third cathode ohmic contact layer 233. This realizes the common cathode 30 of the first element layer 21, the second element layer 22, and the third element layer 23.

[0086] In this embodiment, the fourth electrical connection structure 26 is not in contact with the first element layer 21 and the second element layer 22, and therefore there are some overlaps and offsets between the third element layer 23 and the second element layer 22 and the first element layer 21 projected onto the back plate 10. The offsets are used for the vertical arrangement of the third cathode ohmic contact layer 233, the fourth electrical connection structure 26, and the common cathode 30, and the area ratio of the offsets is small.

[0087] Therefore, the common cathode 30 of this embodiment is provided within the display unit 20. In order to realize the common cathode 30 between adjacent pixel units 100, a conductive film is provided on the top layer of the display unit 20. By sharing the external cathode by connecting the conductive film between adjacent pixel units 100, the proportion of the area of ​​the cathode in the display unit 20 is reduced, and the proportion of the area of ​​the light-emitting region is improved.

[0088] The pixel unit 100 preferably further includes an optical reinforcement structure 40 laminated on one surface of the pixel unit 100 away from the back plate 10. Specifically, as shown in Fig. 9, after a plurality of element layers are laminated by the VSP, the optical reinforcement structure 40 such as a polarizing mirror, a lens, etc. is subsequently laminated by the VSP. The lens may be an organic material such as SU8, polyimide, etc., or an inorganic material such as silicon oxide, alumina, etc.

[0089] Therefore, the pixel unit of the present embodiment realizes multi-color display by sequentially stacking at least two layers of device layers on a back plate, and the horizontal space occupied by the pixel unit of the present application is smaller and the loss of pixel density is smaller than the pixel structure that is horizontally stacked to realize full color. Furthermore, by adopting a common cathode for each layer vertically stacked in the display unit of the present application, the proportion of the cathode area in the display unit can be reduced, the proportion of the light-emitting area area can be increased, and the influence of size effect can be reduced, while at the same time, the number of stacked device layers in the vertical direction can be increased or a redundant circuit can be formed.

[0090] Corresponding to the pixel unit for semiconductor device of this embodiment, according to this embodiment, there is further provided a method for manufacturing a pixel unit for semiconductor device, which includes the following steps.

[0091] In step S1, a back plate 10 is provided, which includes a driving circuit and at least one anode. Corresponding to the pixel unit 100 described above, the back plate 10 in this embodiment is a CMOS back plate.

[0092] In S2, a first compound semiconductor prepared in advance is bonded to the back plate 10, and the first element layer 21 and a layer corresponding to the first element layer 21 are bonded to the back plate 10. First connection portion 32 A second compound semiconductor that has been prepared in advance is bonded to the surface of one side of the first element layer 21 that is spaced apart from the back plate 10, and the second element layer 22 and the corresponding Second connection portion 33 and attaching the second device layer 22 to the corresponding anodes and Second connection portion 33and a common cathode is formed which is connected to the external cathode. Second connection portion 33 and first connection portion 32 The display unit 20 and the corresponding common cathode 30 are manufactured to connect the above.

[0093] In this embodiment, a conductive material such as ITO is used to bond the first compound semiconductor to the back plate 10 so as to form a first bonding layer. The compound semiconductor is usually a wafer or a region of appropriate size cut from a wafer. Taking a wafer as an example, the compound wafer is a compound formed by two or more elements with a specific atomic ratio, and has semiconductor properties such as a specific band gap and band structure. Crystalline inorganic compounds (such as III-V and II-VI compound semiconductors), organic compounds (such as organic semiconductors), and oxide semiconductors are included. The substrate material may be GaAs, GaN, Si, SIC, Sapphire, etc. Next, a layer electrically contacting the surface of the compound is manufactured and formed, and can be arbitrarily combined in the subsequent compound stacking by VSP.

[0094] Based on this, step S2 specifically includes:

[0095] In S21, an insulating material (such as SiO2) is coated on the entire surface of the back plate 10 on which the at least two anodes are provided, and at least two first through holes corresponding to the at least two anodes are formed.

[0096] In S22, the entire surface of the back plate 10 after coating the insulating layer is coated to form the back plate 10 coated with the bonding material, and the entire surface ITO coating is 360±10 nm. Of course, before step S22, in a preferred embodiment, the surface of the back plate 10 may be provided with an in-situ reflector or a top metal corresponding to the anode through-hole. In an exemplary embodiment, as shown in FIG. 10, the photoelectric properties of ITO are optimized by high-temperature ITO annealing or heating during the coating process, and then the uneven surface of ITO is planarized by CMP process, and the surface roughness is required to be in the range of 0.1-5 nm.

[0097] In S23, a conductive material is coated on the entire surface of the first compound semiconductor so that a first compound semiconductor coated with a bonding material is formed. Specifically, Ni (5 nm) Au (10 nm) is laminated on the entire P surface of the first compound semiconductor, an ohmic contact is formed by high-temperature annealing so that a P contact layer is formed, and an ITO coating is performed on the surface of the P contact layer by deposition, sputtering, etc., and the ITO film thickness is set to 500 ± 10 nm. Then, an ohmic contact is formed by annealing at a high temperature of 500 ° C. in an N2 environment so that the photoelectric properties of ITO are optimized, and then the uneven surface of ITO is flattened by a chemical mechanical polishing (CMP) process, and the surface roughness is required to be in the range of 0.1 to 5 nm. Of course, the thickness of the P contact coating contact layer on the compound surface and the conditions for forming the contact can be adjusted and changed as necessary, and this is not limited in this embodiment.

[0098] In S24, the back plate 10 coated with the bonding material is bonded to the first compound semiconductor.

[0099] In S25, as shown in FIGS. 11 to 13, the substrate of the first compound semiconductor is removed so that the bonding between the first compound semiconductor and the back plate 10 is completed.

[0100] Specifically, in this embodiment, the ITO surface is treated by cleaning or surface activation. In one embodiment, the surface is activated by ammonia immersion after treatment with Ar plasma, and then the back plate 10 and the first compound semiconductor are bonded, and the compound substrate is removed after bonding, and the compound N contact is exposed by etching. The bonding may be a non-aligned bond or an aligned bond. If the target compound is a partial region cut from a wafer, it can be bonded by a fan-out sealing type. For example, if the compound semiconductor of the first layer is an AlGaInP quaternary compound, the substrate is removed by a mixture of ammonia and hydrogen peroxide after bonding, and the N contact layer is exposed by hydrochloric acid etching.

[0101] The first element layer 21 and the first element layer 21 are provided on at least one surface in the circumferential direction. First connection portion 32 After the completion of the construction, specifically, the process includes the following: In S26, the first compound semiconductor is patterned and exposed and etched to construct a first device layer 21 corresponding to the pattern of the back plate 10, and at least one first through hole corresponding to the remaining anode is left in advance. The first device layer 21 includes a first bonding layer 211 and a first compound light emitting layer 212.

[0102] In S27, a first cathode ohmic contact layer 215 is provided on one surface of the first element layer 21 that is spaced from the first bonding layer. Specifically, the first cathode ohmic contact layer 215 may be a laminate of metals such as Au, Ge, Ni, or an alloy material.

[0103] In addition, when stacking the compound VSP, the order of steps S26 and S27 is not limited, and the first element layer 21 may be formed first, or the first cathode ohmic contact layer 215 may be formed first.

[0104] Specifically, as shown in Fig. 11, the lower semicircular filling area is the first cathode ohmic contact layer 215, and the subsequent two-layer stacked anode (second anode 14, third anode 15) is exposed by a patterning etching process, and the exposure of the anode can be directly exposed to the back plate 10 or the conductive bonding material. For convenience of explanation, this embodiment takes the exposure of the anode to the back plate 10 as an example for further explanation.

[0105] In S28, at least one metal pillar 251 for a subsequent device layer other than the first device layer 21 is constructed in the at least one first through-hole by semiconductor patterning coating.

[0106] In S29, the first compound light-emitting layer 212 is coated and passivated on the entire surface. The insulating material used for coating and passivation can be inorganic dielectric material such as silicon oxide, silicon nitride, alumina, etc., or organic dielectric material such as SU8, polyimide, etc. For example, the passivation is completed by spin-coating silicon such as SU8.

[0107] In S210, the first compound light-emitting layer 212, which has been passivated with silicon oxide over its entire surface by a semiconductor patterning etching process, is patterned and etched so as to form electrical through-holes corresponding to the remaining anodes and the first cathode ohmic contact layer 215. The remaining anodes are to be the anodes (second anode 14, third anode 15) of the subsequent laminated layers. Details are shown in Figures 14 to 16.

[0108] In S211, the remaining anode electrical connections and First connection portion 32 The formed electrical via hole is filled so that First connection portion 32 As shown in FIG. 17 and FIG. 18, the part is included.

[0109] Step S211 specifically includes filling the entire surface with a film layer of metal Al, Ti, W, Au, Ni or Cu, either alone, alloy or laminated, by metal deposition, sputtering, electroplating, chemical plating or the like, and then exposing the silicon oxide covered with the metal by CMP so as to complete filling of the electrical through holes of the first cathode ohmic contact layer 215 and electrical connection of subsequent element layers (i.e., the second electrical connection structure 25 and the fourth electrical connection structure 26, etc.).

[0110] In addition, the above steps S28 to S211 are performed by constructing an electrical connection structure with reference to the damascene process in the field of integrated circuits. Compared to the conventional method of constructing electrical connections by etching metal layers, the process of constructing electrical connections in the lamination method is less difficult, and the feasibility of the electrical connection structure is improved, especially for metals (such as copper) that are difficult to dry etch.

[0111] After the construction of the first element layer 21 is completed in step S211, the second element layer 22 and the third element layer 23 are subsequently constructed in a similar manner, as shown in FIGS.

[0112] Specifically, the first layer of lamination can select opaque materials such as Au, Cu, etc., but from the lamination of N (N≧2) layers, the bonding thin film used needs to be matched with the compound of the N-1 layer, to ensure that the wavelength of light emitted by the compound semiconductor of the N-1 layer can be transmitted, and at the same time, the light of the compound of the N-1 layer can be screened to select and transmit light of a specific wavelength band. In addition, the bonding material of the Nth layer may have optical enhancement functions such as polarization, reflection, etc. in the N or N+1 layers. The bonding layer of the Nth layer must be transparent, and may be conductive, such as compound materials such as ITO, ZnO, GaP, GaAs, GaN, etc., or may be non-conductive, including a single layer or laminated pair of dielectric materials such as SiO2, Ti2O3, Si3N4, Al2O3, AlN, etc., or organic materials such as SU8, BCB, etc., or materials that can transmit light when the thickness is extremely thin and have a certain transmittance when the thickness is within 20 nm, such as Ag, Si, etc. In one embodiment, 20 nm of Si is used, and some of the visible light transmittance data is shown in FIG. 19.

[0113] Specifically, the second compound light emitting layer is a green light InGaN material, and the cathode ohmic contact material can be one or more of Cr, Al, Ti, Ni, etc. The third compound light emitting layer is an InGaN blue light epitaxy, and as shown in Figures 2 to 4, the cross-sectional views after device fabrication and electrical connection correspond to the X-axis and Y-axis of the top view, respectively.

[0114] More preferably, the bonding thin film of the Nth layer (N≧2) includes a laminate of silicon oxide and titanium oxide capable of screening the light of the N-1th layer. For example, when the N-1th layer is red light with a light output range of 600-650 nm, the transmitted light can be controlled to a wavelength of 620-630 nm by screening the light by the bonding thin film of the Nth layer. Or, the bonding thin film of the Nth layer (N≧2) includes a laminate of silicon oxide and alumina capable of reflecting the light of the Nth layer. When the Nth layer is green and ITO bonding is adopted, the reflectance of the 525 nm wavelength is less than 20%. Or, by introducing 150 nm of alumina and 180 nm of silicon oxide, the reflectance of the 525 nm wavelength can exceed 30%. Example 2

[0115] As shown in Figures 20 and 21, this embodiment provides another pixel unit 100 for semiconductor devices. The pixel unit 100 has a structure similar to that of the pixel unit 100 of the first embodiment, except that the common cathode body 31 of this embodiment is a metal surrounding frame arranged in the circumferential direction of the display unit 20. The material of the metal surrounding frame may be a metal such as aluminum.

[0116] In this difference, the first connection portion 32, the second connection portion 33 and the third connection portion 34 connecting each element layer (21, 22, 23) to the common cathode body 31 are located in any direction of the plane in which the upper surface of the current element layer is located, so the projections of the first connection portion 32, the second connection portion 33 and the third connection portion 34 on the back plate 10 may or may not overlap.

[0117] Preferably, each side of the metal surrounding frame is shared by two adjacent pixel units 100, thereby further reducing the area ratio of the common cathode 30 in the pixel unit and improving the area ratio of the light-emitting area.

[0118] Furthermore, the thickness of the common cathode 30 decreases from one end adjacent the backplate 10 to the other end.

[0119] Specifically, the metal surrounding frame grows with each layer as the compound semiconductors integrate and shrink, forming an inverted bowl-shaped peripheral cathode as a constrained sidewall reflector structure, as shown in FIG.

[0120] Therefore, the common cathode body 31 in this embodiment is a metal surrounding frame, which can not only realize the cathode interconnection of a single pixel, but also realize the common cathode 30 of the whole semiconductor device based on the pixel unit. Moreover, the metal surrounding frame can be a pixel isolation to prevent optical crosstalk between pixels, and has the function of a sidewall reflector.

[0121] The manufacturing method of the pixel unit of this embodiment is basically the same as that of the embodiment 1, except that when manufacturing the common cathode 30, metal etching and filling are required around the pixel when adopting the analogous damascene process, and finally a metal surrounding frame and corresponding connections of each layer are required. The relevant process steps are referred to the description in the embodiment 1 and are not specifically described here. Example 3

[0122] According to this embodiment, a further pixel unit for a semiconductor device is provided. As shown in Figures 23 and 24, its structure basically has a certain similarity to the pixel unit structure of the first embodiment, but differs in the following points:

[0123] (1) First bonding layer 211 is made of an insulating material, and second bonding layer 221 and third bonding layer 231 are each made of a transparent insulating material. Illustratively, first bonding layer 211, second bonding layer 221 and third bonding layer 231 are all SiO2-SiO2 bonding layers.

[0124] The first element layer 21 further includes a first P-type ohmic contact layer 216 disposed between the first bonding layer 211 and the first compound light-emitting layer. The first P-type ohmic contact layer 216 includes a first P-type ohmic contact layer extension 2161 that extends toward the common cathode 30 but does not contact the common cathode 30. The first element layer 21 further includes a first electrical connection structure 27. The first electrical connection structure 27 has one end connected to the corresponding first anode 13 and a free end passing through the first bonding layer 211 and connected to the first P-type ohmic contact layer extension 2161. The free end of the first electrical connection structure 27 preferably does not exceed the near one surface of the second element layer 22, and the free end of the first electrical connection structure 27 is preferably connected to the near one surface of the second element layer 22. This realizes self-support within the display unit 20, and improves the structural strength of the pixel unit 100 itself.

[0125] The second element layer 22 further includes a second P-type ohmic contact layer 224 provided between the second bonding layer 221 and the second compound light-emitting layer 22. The second P-type ohmic contact layer 224 includes a second P-type ohmic contact layer extension portion 2241 that extends toward the common cathode 30 but does not contact the common cathode 30.

[0126] The second element layer 22 further includes a third electrical connection structure 28. The third electrical connection structure 28 has one end connected to the corresponding second anode 14 and a free end passing through the first element layer 21 to be connected to the second P-type ohmic contact layer extension 2241.

[0127] The third element layer 23 further includes a fifth electrical connection structure 29 and a third P-type ohmic contact layer 234. One end of the fifth electrical connection structure 29 is connected to the corresponding third anode 15, and a free end passes through the first element layer 21 and the second element layer 22 and is connected to the third P-type ohmic contact layer extension 2341.

[0128] (2) The common cathode body 31 is a metal surrounding frame provided in the circumferential direction of the display unit 20 .

[0129] Therefore, in the pixel unit of this embodiment, since an insulating material is used for each bonding layer, each electrical connection structure needs to pass through the current and lower bonding layers to respectively connect to the corresponding anode of the back plate 10, and each layer is independently connected to the metal surrounding frame so as to realize the surrounding common cathode 30. Compared with the pixel unit of the embodiment 1 or embodiment 2, the pixel unit of this embodiment is also provided with the common cathode 30. Area with source In addition to increasing the area ratio, the compound light-emitting layers of all the element layers in this embodiment have the same area, and there is no overlapping projection on the back plate 10, no area loss or misalignment due to avoidance of the internal electrical connection structure, which further improves the horizontal space utilization rate and pixel density, and can effectively improve the light intensity of a single pixel when multiple layers emit light simultaneously.

[0130] The corresponding manufacturing method differs from that of Example 1 in the following respects.

[0131] (1) Since an insulating material is used to bond the first compound semiconductor to the back plate 10 so as to form the first bonding layer 211, the step of bonding the pre-prepared first compound semiconductor to the back plate 10 includes coating the entire surface of the back plate 10 with an insulating material (such as SiO2), fabricating a first P-type ohmic contact layer 216 on the surface of the first compound semiconductor, coating the entire surface of the first P-type ohmic contact layer 216 with an insulating material (such as SiO2), bonding the back plate 10 to the first compound semiconductor, and removing the substrate of the first compound semiconductor.

[0132] (2) Provided on the first element layer 21 and at least one surface of the first element layer 21 in the circumferential direction First connection portion 32 The steps of constructing include constructing a first element layer 21 corresponding to the back plate 10 pattern by patterning etching, exposing the corresponding first P-type ohmic contact layer extension 2161, constructing at least one second through hole corresponding to at least one anode in the first P-type ohmic contact layer extension 2161 by patterning etching, fully covering and passivating the first compound semiconductor, patterning and etching the first compound semiconductor after being fully passivated with silicon oxide by a semiconductor patterning etching process, so as to form electrical through holes corresponding to each anode and electrical through holes corresponding to the first cathode ohmic contact layer 215, and forming a first electrical connection structure 27 corresponding to the first compound light emitting layer 212, a second electrical connection structure corresponding to the second compound light emitting layer 222, and an electrical through hole corresponding to the first compound light emitting layer 212. First connection part 3 and filling the formed electrical vias such that a conductive layer 2 is formed. First connection portion 32 is part of the metal surrounding frame structure. Based on this, the second element layer 22 and the third element layer 23 are repeatedly constructed, the specific structures of which are shown in Figures 25 and 26. Example 4

[0133] According to the fourth embodiment, a micro display 200 is provided. As shown in FIG. 27, the micro display 200 includes: A microdisplay backplate 300 including at least two driving circuits and an input / output interface; A display area 400 provided on a microdisplay back plate 300, the display area 400 including at least two display units 20 arranged in an array according to the first to third embodiments and a corresponding common cathode 30; A peripheral common cathode 500 electrically connected to the common cathode 30 of each display unit 20 so that the entire microdisplay 200 is a common cathode; and an external IO interface 600 located at any position on the microdisplay back plate 300. The peripheral common cathode 500 is a metal surrounding frame structure provided around the periphery of the display area 400.

[0134] For the specific structure and corresponding technical effects of the microdisplay of this embodiment, please refer to the relevant descriptions in Examples 1 to 3, and no further detailed description will be provided in this embodiment. Example 5

[0135] As shown in Figs. 28-31, according to the present embodiment, a pixel level discrete element 100' is provided. The pixel level discrete element 100' includes a back plate 10', at least two pads, a display unit 20' and a common cathode 30'. Here, the at least two pads specifically include N anode pads and one cathode pad 41'. A part of the anode pad and a part of the cathode pad 41' are respectively provided in the back plate 10', where N≧1. The display unit 20' includes a first element layer 21' and a second element layer 22'. The first element layer 21' is provided on one side of the back plate 10' where the at least two pads are provided, and the first element layer 21' is connected to the corresponding anode pad. The second element layer 22' is provided on one surface of the first element layer 21' away from the back plate 10' and connected to the corresponding anode pad. For ease of explanation, the anode pad connected to the first device layer 21' is referred to as the first anode pad 42, and the anode pad connected to the first device layer 21 is referred to as the second anode pad 43. The common cathode 30' is connected to the first device layer 21', the second device layer 22' and the cathode pad 41, respectively.

[0136] Specifically, the material of the back plate 10' is one of the passive back plates such as silicon, PCB, sapphire, glass, etc., and may also adopt the SOI CMOS substrate to complete the single pixel circuit control switch. In this embodiment, silicon is taken as the back plate for further specific description.

[0137] In addition, since the pads are used to match the electrical connection interface preset in the downstream sealing product, the present embodiment does not limit the pad structure, and it is preferable that all pad structures are the same in order to simplify the structure and reduce the difficulty of the process. The pads may be solid or hollow, as shown in Figures 32 to 34.

[0138] Specifically, taking the cathode pad 41' as an example, as shown in Figs. 33 and 34, it includes a first connection part 411' and a needle piercing part 412' which are connected to each other. Here, the first connection part 411' is provided on the outside of the back plate 10' so as to be connected to the display unit 20', and the needle piercing part 412 is provided inside the back plate 10'. The needle piercing part 412' may be a vertebral structure, a step type structure, a cylindrical structure, a rectangular parallelepiped structure, etc. In addition, the pad may be made of one or more alloys or laminates of gold, titanium, tungsten, aluminum, and platinum.

[0139] At least two corresponding grooves are formed on the back plate 10' corresponding to the above-mentioned N anode pads and one cathode pad 41', and the groove structure formed on the back plate 10' is aligned with the corresponding pad structure.

[0140] 29 and 30, the first element layer 21' includes a first bonding layer 211', a first compound light-emitting layer 212', a first insulating covering layer 213' and a first electrical connection structure 214'. Here, the first bonding layer 211' is provided on the back plate 10'. The first compound light-emitting layer 212' is provided on one surface of the first bonding layer 211' spaced apart from the back plate 10'. The first insulating covering layer 213' covers the first bonding layer 211' and the first compound light-emitting layer 212'. The first electrical connection structure 214' is provided on a side of the first compound light-emitting layer 212'.

[0141] The material of the first bonding layer 211' may be an insulating material or a conductive material. The first bonding layer 211' in this embodiment is preferably made of a single layer or a laminated pair of dielectric materials such as SiO2, titanium oxide, Si3N4, Al2O3, AlN, or a transparent insulating material such as an organic material such as SU8, BCB, etc. The first element layer 21' further includes a first P-type ohmic contact layer 2121' disposed between the first bonding layer 211' and the first compound light emitting layer 212', and the area of ​​the first compound light emitting layer 212' is larger than that of the first P-type ohmic contact layer 2121'. The first electrical connection structure 214' is connected to the corresponding first anode pad 42' through the first P-type ohmic contact layer 2121' and the first bonding layer 211' in sequence. Here, the first P-type ohmic contact layer 2121' is formed by completing the ohmic contact by high-temperature annealing of Ni / Au alloy. The area of ​​the first P-type ohmic contact layer 2121' is preferably larger than the area of ​​the first compound light-emitting layer 212'.

[0142] Similar to the first element layer 21', the second element layer 22' includes a second bonding layer 221', a second compound light-emitting layer 222', a second insulating coating layer 223' and a second electrical connection structure 224'. Here, the second bonding layer 221' is provided on the first insulating coating layer 312'. The second compound light-emitting layer 222' is provided on one surface of the second bonding layer 221' spaced apart from the first element layer 21'. The second insulating coating layer 223' covers the second bonding layer 221' and the second compound light-emitting layer 222'. The second electrical connection structure 224' is provided on the side of the first compound light-emitting layer 212' and the second compound light-emitting layer 222'.

[0143] Similarly, the second bonding layer 221' is preferably made of silicon nitride, which is an insulating material. On this basis, the second element layer 22' further includes a second P-type ohmic contact layer 2221' provided between the second bonding layer 221' and the second compound light emitting layer 222', and the area of ​​the second compound light emitting layer 222' is larger than the area of ​​the second P-type ohmic contact layer 2121'. The second electrical connection structure 224' is connected to the corresponding second anode pad 43 by passing through the second P-type ohmic contact layer 2221', the second bonding layer 221', the first insulating cover layer 213', the first P-type ohmic contact layer 2121', and the first bonding layer 211' in sequence.

[0144] It should be noted that, if the first compound light emitting layer 212' and the second compound light emitting layer 222' are made of the same material, they are connected to the same anode pad, and the first anode pad 42' and the second anode pad 43' are actually the same pad. Furthermore, the first electrical connection structure 214' is connected to the second electrical connection structure 224' so as to simplify the structure. In this structure, the pixel individual element 100' can realize a redundant structure in the vertical direction by arranging the same element layer, thereby enhancing performance and ensuring pixel yield as redundancy. If the first compound light emitting layer 212' and the second compound light emitting layer 222' are made of different materials, the first anode pad 42' and the second anode pad 43' are two independent pads. Therefore, the number N of anode pads is the number N of element layers. In this structure, the pixel individual element 100' can realize full color display, so that the pixel size is compressed in the horizontal direction and the loss of pixel density is avoided. For convenience of explanation, the latter is taken as an example in this embodiment.

[0145] From the second device layer 22' and each subsequent device layer, a light screening and light enhancing structure can be introduced into the bonding layer, which needs to match the compound semiconductor of the previous layer, ensure that the wavelength of light emitted by the compound semiconductor of the previous layer can be transmitted, and at the same time, can screen the light of the compound of the previous layer and select and transmit the light of a certain wavelength band, and the bonding material of the current layer has an optical enhancing function such as polarization, reflection, etc. by itself or in the subsequent layer.

[0146] As shown in FIG. 30 and FIG. 31, the common cathode 30' is perforated in the first insulating cover layer 213' and the second insulating cover layer 223' so as to be connected to the cathode pad 41'. The common cathode 30' includes a first common cathode portion 31' and a second common cathode portion 32' connected to the first common cathode portion 31'. The first common cathode portion 31' is connected to the cathode pad 41'. The first common cathode portion 31' is provided on one side of the first compound light emitting layer 212' so as to be connected to the first compound light emitting layer 212', and the second common cathode portion 32' is provided on one side of the second compound light emitting layer 222' so as to be connected to the second compound light emitting layer 222'. Therefore, the electrical connection structure and the common cathode of this embodiment are both located on the side of the corresponding compound semiconductor layer, and can be avoided from causing a shielding of the light emitting surface.

[0147] Of course, in this embodiment, the number of element layers is not limited. As shown in FIG. 31 and FIG. 32, based on the first element layer 21' and the second element layer 22', a third element layer 23' and even a fourth element layer or more can be provided according to the needs of downstream products. Illustratively, when the display unit 20' further includes a third element layer 23', the third element layer 23' is provided on one side surface of the second element layer 22' separated from the second element layer 21'. The third element layer 23' is connected to a corresponding anode pad. The corresponding anode pad is the third anode pad 44.

[0148] In addition, for convenience of fixing and access, the pixel level discrete element 100 further includes a self-supporting structure 50'. The self-supporting structure 50' covers the display unit 20' and a part of the back plate 10', and forms a tether structure to fix and connect the display unit 20' to the back plate 10'. Specifically, the self-supporting structure 50' includes a covering part 51' and a fixing part 52' which are connected in sequence. The covering part 51' covers the display unit 20', and the fixing part 52 is provided on the back plate 10'. In addition, the display unit 20' is provided separately from the back plate 10', and the at least two pads are provided separately from the back plate 10'. The separate provision can be achieved by providing a sacrificial layer between the back plate and the at least two pads in advance during the manufacturing process, and removing the sacrificial layer by a method such as etching after the stacking of the elements is completed and the self-supporting structure 50' is formed. Therefore, the pixel level individual element 100' only needs to break the covering part 51' and the fixed part 52' by external force when moved, which makes it easy to access, and in this structure, the back plate can be used repeatedly, thereby reducing costs.

[0149] In addition, the portion of the self-supporting structure 50' that is provided on the back plate 10' is in complete contact with the back plate 10', and the edges may be flush with the corresponding edges of the back plate 10' (Figures 28-30), or may be in an overhanging or recessed state, and this is not limited to this embodiment.

[0150] Corresponding to the above-mentioned pixel level discrete element, according to the present embodiment, there is further provided a method for manufacturing a pixel level discrete element, which includes the following steps.

[0151] In S1, at least two pads are constructed, including N anode pads and one cathode pad, N≧1, partially disposed inside a pre-prepared back plate.

[0152] Before the above step S1, further including: In step S0, at least two cavities corresponding to at least two pads are etched on a pre-prepared back plate, and a sacrificial layer is coated on the back plate having the at least two cavities formed thereon. In this embodiment, a silicon plate is used as the back plate.

[0153] Specifically, the sacrificial layer is a silicon oxynitride film, which is formed on the surface of the back plate by coating, thermal oxidation, wet oxidation, or the like.

[0154] The pad in this embodiment uses a metal pad, which may be one or more alloys or laminate pairs of gold, titanium, tungsten, aluminum, platinum, etc. The manufacturing method includes thermal evaporation, sputtering, electroplating, chemical plating, etc., and the pad may be solid or hollow.

[0155] In S2, a first element layer and a second element layer are sequentially stacked on one side of a back plate on which at least two pads are provided, the first element layer and the second element layer being connected to corresponding anode pads along a direction away from the back plate, and both being connected to cathode pads via a common cathode formed thereon, so as to form a display unit.

[0156] Here, stacking and constructing the first element layer on one side of the back plate on which at least two pads are provided specifically includes the following.

[0157] In S21, an insulating material is coated on the entire surface of one side of a back plate on which at least two pads are provided, and an insulating material is coated on the entire surface of a first P-type ohmic contact layer prefabricated on a surface of a first compound semiconductor.

[0158] In S22, the first bonding layer is formed by bonding the back plate and the insulating material of the first compound semiconductor, so the bonding material used in this embodiment is an insulating material, specifically, silicon nitride or the like.

[0159] In S23, the substrate of the first compound semiconductor is removed and the epitaxy is thinned to expose the nitrogen contact layer of the first compound semiconductor, so that a first compound light emitting layer is formed.

[0160] Of course, before step S23, the method further includes preparing a first compound semiconductor in advance. Of course, in this embodiment, the type of the first compound semiconductor is not limited, but the type of the compound semiconductor needs to correspond to the back plate.

[0161] For example, when the back plate is N-GaAs and the red light is AlGaInP-based, the structure is shown in Table 1. When it is InGaN-based, the structure diagram can be shown in Table 2 or Table 3, and these two can be simultaneously combined to form a wavelength compound structure such as blue light and green light.

[0162] When the first compound semiconductor is a red light compound and the second compound light emitting layer is a green light compound, it is preferable to introduce a red light color filter between the second compound semiconductor layer and the second junction layer, which allows only red light in a specific wavelength range to pass through and prevents photoluminescence excitation of red light when the thick layer of short wavelength compound emits light.

[0163] In S24, the first compound light emitting layer is patterned and etched to the first P-type ohmic contact layer, i.e., the area of ​​the etched first compound light emitting layer is smaller than the area of ​​the first P-type ohmic contact layer, and the excess part of the first P-type ohmic contact layer is used for the subsequent construction of the electrical through hole.

[0164] In S25, the first compound light-emitting layer is completely coated and passivated to form a first coating passivation layer. The first coating passivation layer can be an inorganic dielectric material such as silicon oxide, silicon nitride, alumina, or an organic dielectric material such as SU8, polyimide, and the present embodiment is not limited thereto.

[0165] In S26, the first covering passivation layer is patterned and etched to form corresponding first electrical connection passages and first partial cathode electrical connection passages.

[0166] In S27, a first electrical connection structure having one end connected to a corresponding anode pad through the first P-type ohmic contact layer and a first cathode portion having one end connected to the first compound semiconductor and the other end connected to a cathode pad through the first P-type ohmic contact layer are formed by metal coating.

[0167] After the construction of the first layer of devices is completed, a second layer of devices is subsequently constructed in a similar manner, followed by a third layer of devices, and so on.

[0168] After completing the above step S2 to form the display unit, the manufacturing method preferably further includes coating a dielectric material on the surface of the display unit to extend to a part of the surface of the back plate, so as to form a self-supporting structure. The dielectric material is preferably silicon oxide, photoresist, etc.

[0169] Specifically, the sacrificial layer is first patterned and etched to remove a portion of the sacrificial layer located on one side of the back plate and expose a portion of the back plate, then a dielectric material is coated on the display unit and the exposed surface of the back plate to form a self-supporting structure, and finally, the sacrificial layer is etched on the surface of the back plate on one side where the dielectric material is not coated, so that at least two pads are separated from the back plate. The etching rate ratio between the sacrificial layer and the back plate is greater than 10:1, and the etching rate ratio between the sacrificial layer and the self-supporting structure is greater than 10:1.

[0170] After the coating of the dielectric material is completed, a sacrificial layer is provided between at least a part of the back plate and the display unit, and the inside of the pixel individual element is etched at the position, so that the entire surface of the sacrificial layer is etched to form a gap layer between at least two pads and the back plate to separate them. The thickness of the gap layer is determined by the thickness of the sacrificial layer. Specifically, the thickness of the sacrificial layer is 100 nm to 1000 nm, and preferably 300 to 500 nm.

[0171] As described above, in this embodiment, by providing at least two vertically stacked element layers on the back plate, compression of pixel size in the horizontal direction is achieved, loss of pixel density is avoided, the number of pixels arranged is reduced, and the number of chip movements during mass transfer is reduced, thereby improving accuracy and yield.

[0172] In addition, by adopting a common cathode for each element layer vertically stacked in the display unit of the present application, the proportion of the cathode area in the individual pixel element is reduced, the proportion of the light-emitting area area is increased, and the influence of size effects is reduced, while at the same time the number of element layers stacked in the vertical direction can be increased or redundant circuits can be formed.

[0173] In addition, the pixel individual element of the present application is connected to an external circuit based on at least two pads, and when sealing the individual element to a target backplate and making an electrical connection, metal welding such as eutectic welding can be avoided so as to avoid affecting the performance of the individual element itself and to simplify the process.

[0174] In addition, the pixel unit has a self-supporting structure, which provides structural stability when the display unit and the back plate are separately provided and provides convenience of access in later use.More importantly, in this structure, the back plate can be reused repeatedly, which reduces the cost.

[0175] Furthermore, since the electrical connection structure and the common cathode of this embodiment are both located to the sides of the corresponding compound semiconductor layers, it is possible to avoid blocking the light emitting surface. Example 6

[0176] 35-38, the present embodiment further provides a pixel-level discrete element 200 and a manufacturing method thereof. The pixel-level discrete element 200 is basically the same as the pixel-level discrete element 100 of the first embodiment in structure and manufacturing method, and only differs in the self-supporting structure 50.

[0177] Specifically, the self-supporting structure 50 of this embodiment includes a covering portion 51 that covers the display unit 20, a fixing portion 52 provided on the back plate 10, and a second connecting portion 53 that is provided separately from the back plate 10, one end of which is connected to the covering portion 51, and the other end of which is connected to the fixing portion 52. The second connecting portion 53 is preferably provided above the fixing portion 52 so as to form a step structure extending from top to bottom with the fixing portion 52. Compared with the first embodiment, the self-supporting structure 50 of this embodiment improves the convenience of operation when the covering portion 51 and the fixing portion 52 are broken by an external force during movement by adding the second connecting portion 53, in addition to ensuring the fixing function of the self-supporting structure 50 to the element layer 20. More importantly, the breaking position is located in the second connecting portion 53, not in the covering portion 51 or the fixing portion 52, and therefore the destruction of the back plate 10 or the element layer 20 is avoided.

[0178] 37 and 38, the fixing portion 52 and part of the second connecting portion 53 are not provided between the display unit 20 and the back panel 10, and the self-supporting structure 50 of this embodiment preferably further includes an extending structure that is connected at an angle to the covering portion 51. By providing the extending structure, it is possible to avoid a situation where the offset during etching is too large, resulting in exposing the sidewall of the display unit 30 that needs to be protected.

[0179] Furthermore, in this embodiment, when manufacturing the pixel level individual element 200, an improvement compared to embodiment 1 is the step of coating a dielectric material on the surface of the display unit and extending over part of the surface of the backplate so as to form a self-supporting structure.

[0180] Specifically, after the display unit is formed, the sacrificial layer is first patterned and etched to remove at least one side of the sacrificial layer outside a predetermined distance from the display unit and expose a portion of the back plate, then a dielectric material is coated on the surface of the display unit, the surface of the sacrificial layer and the surface of the back plate exposed on one side so that a self-supporting structure is formed, and finally, the sacrificial layer on one side where the dielectric material is not coated is etched so that at least two pads are separated from the back plate.

[0181] All the above-mentioned optional technical means may be arbitrarily combined to form optional embodiments of the present application, i.e., combining any multiple embodiments to obtain the requirements for different application scenarios is within the scope of protection of the present application and will not be described in detail herein.

[0182] It should be noted that the above is merely a preferred embodiment of the present application and is not used to limit the present application. Any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present application are all included in the scope of protection of the present application. [Explanation of symbols]

[0183] 100, pixel units 10, back plate 13, first anode 14, second anode 15, 3rd anode 20. Display unit 21, first element layer 211, first bonding layer 212, first compound light-emitting layer 214, first insulating layer 215, first cathode ohmic contact layer 216, first P-type ohmic contact layer 2161, first P-type ohmic contact layer extension 22, second element layer 221, second bonding layer 222, second compound light-emitting layer 223, second cathode ohmic contact layer 224, second P-type ohmic contact layer 2241, second P-type ohmic contact layer extension 23, third element layer 231, 3rd bonding layer 232, the third compound light-emitting layer 233, third cathode ohmic contact layer 234, third P-type ohmic contact layer 24. Insulating coating layer 25, second electrical connection structure 251, 1st metal pillar 252, first connection layer 26, the fourth electrical connection structure 27, first electrical connection structure 28. The third electrical connection structure 29. Fifth electrical connection structure 30, common cathode 31, common cathode body 32, first connection part 33, second connection part 34, third connection part 40 , optically enhanced structure 200, Microdisplay 300, Microdisplay back panel 400, display area 500, ambient common cathode 600, external IO interface 100', pixel level individual element 10', backboard 20', element body 21', first element layer 211', first bonding layer 212', a first compound light-emitting layer 2121', first P-type ohmic contact layer 213', first insulating coating layer 214', first electrical connection structure 22', second element layer 221', second bonding layer 222', a second compound light-emitting layer 2221', second P-type ohmic contact layer 223', second insulating coating layer 224', second electrical connection structure 23', third element layer 30', common cathode 31', first common cathode part 32', second common cathode part 33', third common cathode part 41', cathode pad 411', first connection part 412', needle piercing part 42', 1st anode pad 43', 2nd anode pad 44', 3rd anode pad 50', self-supporting structure 51', covering part 52', fixed part 53', second connection part

Claims

1. The back panel and a display unit provided on the back plate, the display unit including a first element layer and a second element layer stacked vertically in sequence, the second element layer being provided on a surface of one side of the first element layer spaced apart from the back plate, the first element layer and the second element layer being respectively connected to the back plate; a common cathode respectively connected to each element layer of the display unit; A pixel unit for a semiconductor device.

2. The common cathode includes a common cathode body and a first connection portion and a second connection portion respectively connected to the common cathode body; the first connection portion is connected to the first element layer; The second connection portion is connected to the second element layer. The pixel unit according to claim 1 .

3. The back plate is provided with a driving circuit including at least two anodes; Any one of the anodes is connected to a corresponding device layer; At least two of the anodes are both located in a projection range of the display unit on the back plate; The common cathode is connected to an external cathode. The pixel unit according to claim 2 .

4. the first element layer includes a first bonding layer, a first compound light-emitting layer, and an insulating coating layer, which are provided in this order; the first compound light-emitting layer is provided on one surface of the first bonding layer spaced from the back plate, the insulating coating layer covers the first bonding layer and the first compound light-emitting layer; The pixel unit according to claim 2 .

5. the first bonding layer is made of a conductive material; A first insulating layer is provided between the back plate and the first bonding layer, At least one first through hole is formed in the first insulating layer, The first bonding layer is connected to the corresponding first anode through the first through hole.

5. The pixel unit according to claim 4.

6. The common cathode is provided inside the display unit, or The common cathode body is a metal surrounding frame arranged in a circumferential direction of the display unit, and the first connection portion and the second connection portion are arranged inside the display unit.

6. The pixel unit according to claim 5.

7. the first bonding layer is made of an insulating material; the first element layer further includes a first P-type ohmic contact layer provided between the first bonding layer and the first compound light emitting layer; the first P-type ohmic contact layer includes a first P-type ohmic contact layer extension portion that extends toward the common cathode but does not contact the common cathode; the first element layer further includes a first electrical connection structure having one end connected to a corresponding first anode and a free end passing through the first bonding layer and connected to the first P-type ohmic contact layer extension; 5. The pixel unit according to claim 4.

8. The common cathode body is a metal surrounding frame arranged in the circumferential direction of the display unit; The pixel unit according to claim 7 .

9. the first connection portion is connected to the first compound light emitting layer; 6. The pixel unit according to claim 5.

10. The first element layer further includes a first cathode ohmic contact layer provided on one surface of the first compound light emitting layer spaced from the first bonding layer; The first connection portion is connected to the first cathode ohmic contact layer.

6. The pixel unit according to claim 5.

11. the second element layer includes the second bonding layer, the second compound light-emitting layer, and an insulating coating layer; the second compound light emitting layer is provided on one surface of the second bonding layer spaced apart from the first element layer, the insulating coating layer covers the first bonding layer and the first compound light-emitting layer; The pixel unit according to any one of claims 4 to 10.

12. The second bonding layer is made of a transparent conductive material or a transparent semiconductor material, the second element layer further includes a second electrical connection structure, one end of which is connected to a second anode of the back plate and the other end of which passes through the first element layer and is connected to the second bonding layer. The pixel unit according to claim 11 .

13. the second electrical connection structure includes a first metal pillar having one end connected to a corresponding second anode and another end passing through the first element layer and connected to the second bonding layer; or the second electrical connection structure includes a first connection layer that passes through the first insulating layer and is connected to a corresponding second anode, and a first metal pillar that is connected to the first connection layer and is connected to the second bonding layer; The pixel unit according to claim 12 .

14. the second bonding layer is made of a transparent insulating material; the second element layer includes a second P-type ohmic contact layer provided between the second bonding layer and the second compound light emitting layer; the second P-type ohmic contact layer includes a second P-type ohmic contact layer extension portion that extends toward the common cathode but does not contact the common cathode; the second element layer further includes a third electrical connection structure having one end connected to a corresponding third anode and a free end passing through the first element layer and connected to the second P-type ohmic contact layer extension. The pixel unit according to claim 11 .

15. the compound light emitting material used in the first compound light emitting layer and the compound light emitting material used in the second compound light emitting layer are the same; The first element layer and the second element layer are connected to the same anode so as to be provided in series or in parallel. The pixel unit according to claim 11 .

16. the display unit further includes a third element layer stacked on one side of the second element layer spaced apart from the first element layer, the third device layer is connected to a third anode of the backplate; The common cathode further includes a third connection portion connected to the common cathode body; the third connection portion is connected to the third element layer; The pixel unit according to any one of claims 2 to 15.

17. the thickness of the common cathode decreases from one end adjacent the back plate to the other end; 17. The pixel unit according to claim 16.

18. further comprising an optical reinforcement structure laminated to one side of the display unit spaced from the back panel; 17. The pixel unit according to claim 16.

19. The back plate is provided with N anode pads and one cathode pad; a portion of the anode pad and a portion of the cathode pad are each disposed within the back plate, N≧1; Any one of the anode pads is connected to a corresponding device layer; The cathode pads are respectively connected to each element layer via the common cathode. The pixel unit according to claim 1 .

20. The display unit is provided separately from the back plate, and the at least two pads are provided separately from the back plate; Further comprising a self-supporting structure covering the element body and a portion of the back plate.

20. The pixel unit according to claim 19.

21. The self-supporting structure includes a covering part and a fixing part which are connected in sequence, the covering part covers the display unit, and the fixing part is provided on the back plate; or The self-supporting structure includes a covering portion, a second connecting portion, and a fixing portion, which are connected in sequence, the covering portion covering the display unit, the fixing portion being provided on the back plate, and the second connecting portion being provided separately from the back plate.

21. The pixel unit according to claim 20.

22. providing a backplate provided with driving circuitry on which at least one anode is provided; bonding a first compound semiconductor prepared in advance to the back plate, constructing a first element layer and a first common cathode on at least one side surface corresponding to the first element layer; bonding a second compound semiconductor prepared in advance to one surface of the first element layer spaced from the back plate, constructing a second element layer and a second common cathode on at least one side surface in a circumferential direction of the second element layer; connecting the second element layer to a corresponding anode of the back plate and the second common cathode, respectively; and manufacturing a display unit and a corresponding common cathode to connect the second common cathode and the first common cathode to form a common cathode.

2. A method for manufacturing a pixel unit for a semiconductor element, comprising:

23. The step of bonding the first compound semiconductor to the back plate using a conductive material, the step of bonding a first compound semiconductor prepared in advance to the back plate, Coating an insulating material on the entire surface of the back plate on which the at least two anodes are provided, and forming at least two first through holes corresponding to the at least two anodes; coating an electrically conductive material over the entire surface of the backplate after coating the insulating layer to form a backplate coated with a bonding material; coating an electrically conductive material over the entire surface of the first compound semiconductor to form a first compound semiconductor coated with a bonding material; bonding the back plate coated with a bonding material to the first compound semiconductor; removing the first compound semiconductor substrate. The method of claim 22 .

24. The step of constructing a first element layer and a first common cathode provided on at least one circumferential surface of the first element layer includes: patterning the first compound semiconductor by exposing and etching the first compound semiconductor to form a first device layer corresponding to the pattern of the back plate, and pre-remaining at least one first through hole corresponding to the remaining anode; providing a first cathode ohmic contact layer on a surface of the first device layer spaced from the first bonding layer; constructing at least one metal pillar for a subsequent device layer other than the first device layer in at least one of the first through holes by semiconductor patterning coating; coating and passivating the first compound semiconductor; patterning and etching the first compound semiconductor after being blanket passivated with silicon oxide by a semiconductor patterning and etching process, so as to form electrical through holes corresponding to the remaining anode and the first cathode ohmic contact layer; and filling the formed electrical vias such that electrical connections for the remaining anodes and the first common cathode are formed. The method of claim 22 .

25. The step of bonding a first compound semiconductor to the back plate using an insulating material to bond the first compound semiconductor to the back plate so as to form a first bonding layer includes: Coating the entire surface of the back plate with an insulating material; forming a first P-type ohmic contact layer on a surface of a first compound semiconductor, and coating an insulating material on the entire surface of the first P-type ohmic contact layer; bonding the back plate and the first compound semiconductor; removing the first compound semiconductor substrate. The method of claim 22 .

26. The step of constructing a first element layer and a first common cathode provided on at least one circumferential surface of the first element layer includes: constructing a first device layer corresponding to the back plate pattern by patterning etching to expose a corresponding first P-type ohmic contact layer extension; constructing at least one second through hole corresponding to at least one of the anodes in the first P-type ohmic contact layer extension by patterning etching; coating and passivating the first compound semiconductor; patterning and etching the first compound semiconductor after being passivated with silicon oxide over its entire surface by a semiconductor patterning and etching process, so as to form electrical through holes corresponding to each anode and electrical through holes corresponding to the first cathode ohmic contact layer; filling the formed electrical through holes so as to form a first electrical connection structure corresponding to the first compound light emitting layer, a second electrical connection structure corresponding to the second compound light emitting layer, and a first common cathode corresponding to the first compound light emitting layer; The method of claim 25.

27. After the second element layer and the second common cathode provided on at least one surface of the second element layer in the circumferential direction are completed, the step of manufacturing a display unit and a common cathode includes: The method further includes bonding a third compound semiconductor prepared in advance to a surface of one side of the second element layer spaced apart from the first element layer, and constructing a third common cathode provided on a third element layer and at least one surface of the third element layer in a circumferential direction. The method according to any one of claims 22 to 26.

28. constructing at least two pads, including N anode pads and one cathode pad, N≧1, partially disposed inside a pre-prepared back plate; and sequentially laminating a first element layer and a second element layer, each of which is connected to a corresponding anode pad along a direction away from the back plate on one side of the back plate on which at least two of the pads are provided, so as to form a display unit, the first element layer and the second element layer being connected to the cathode pad via a common cathode formed thereon.

2. A method for manufacturing a pixel unit for a semiconductor element, comprising:

29. Before placing at least two pads on a pre-prepared backing board, Etching at least two cavities corresponding to the at least two pads in a pre-prepared back plate; and coating the backplate having at least two cavities formed therein with a sacrificial layer.

29. The method of claim 28.

30. After the step of sequentially stacking a first element layer and a second element layer along a direction away from the back plate on one side of the back plate on which at least two of the pads are provided so as to form a display unit, coating a surface of the display unit with a dielectric material extending over a portion of a surface of the backplate such that a self-supporting structure is formed; and etching a sacrificial layer on a surface of one side of the backplate that is not coated with the dielectric material such that at least two of the pads are separated from the backplate; an etch rate ratio between the sacrificial layer and the backplate is greater than 10:1, and an etch rate ratio between the sacrificial layer and the self-supporting structure is greater than 10:1; 30. The method of claim 29.

31. a microdisplay backplate including at least two driving circuits, an input interface and an output interface; A display area provided on the microdisplay back plate, the display area including at least two display units included in the pixel unit for semiconductor element according to any one of claims 1 to 19 or a display unit included in a pixel unit manufactured by the manufacturing method according to any one of claims 22 to 27; a surrounding common cathode electrically connected to the common cathode of each of the display units, A microdisplay characterized by:

32. an individual element backplate including at least two anode pads and at least one cathode pad; An element body provided on the individual element back plate, the element body including at least two display units included in the pixel unit for semiconductor element according to any one of claims 1 and 19 to 21, or a display unit included in the pixel unit manufactured by the manufacturing method according to any one of claims 28 to 30, 16. A discrete element comprising:

Citation Information

Patent Citations

  • Full-color active addressing Micro-LED chip structure and manufacturing method thereof

    CN112117356A

  • Light emitting diode structure and method for manufacturing the same

    CN113488576A

  • Semiconductor light-emitting device and image display device

    JP2011159672A

  • LED unit for display and display device having the same

    JP2021504752A

  • Micro-Emitter Array Based Full-Color Micro-Display

    US20090078955A1