Method for manufacturing a laminated core for an electrical machine - Patents.com

By diffusing austenite stabilizers and insulators into the metal sheet laminate of electrical machine cores, a targeted magnetic flux barrier is created, improving insulation and vibration resistance while maintaining high operational speeds.

JP2024543630AActive Publication Date: 2024-11-21ROBERT BOSCH GMBH
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024534284
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-08
Filing Date
2022-11-14
Publication Date
2024-11-21
Estimated Expiration
2042-11-14

AI Technical Summary

Technical Problem

Existing methods for manufacturing laminated cores of electrical machines do not effectively create a targeted, three-dimensional magnetic flux barrier, which is crucial for modifying material properties to make the rotor web magnetically non-conducting.

Method used

A method involving the use of aluminum support foil with aluminum oxide and austenite stabilizers like manganese, nickel, or cobalt, along with an electrical insulator, is applied to form a magnetic flux barrier by diffusing these substances into the metal sheet laminate during heat treatment, creating a non-magnetic austenite phase and an insulating layer.

Benefits of technology

This approach results in a laminated core with localized magnetic flux barriers and improved electrical insulation, enhancing vibration resistance and allowing higher operational speeds without significant additional manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543630000001_ABST
    Figure 2024543630000001_ABST
Patent Text Reader

Abstract

A method for manufacturing a laminated core (1) for an electric machine, comprising the steps of: a) providing a foil sheet (4) each comprising an aluminum support foil (6) and a natural or produced aluminum oxide layer (7) and each coated on at least one side (11, 12) on a flux barrier surface (8) with a first foil coating (10) of a first powder mixture, the first powder mixture comprising an austenite stabilizer, aluminum oxide and an adhesive binder; b) providing metal sheets (5) of a laminated core (1); c) stacking the metal sheets (5) and the foil sheets (4) alternately, the orientation of the foil sheets (4) relative to the metal sheets (5) being such that the magnetic flux barrier surface (8) of each foil sheet (4) is in direct contact with each metal sheet (5) at a specific magnetic flux barrier point (9) of each metal sheet (5); and d) heating the stack of metal sheets (5) and foil sheets (4), austenite stabilizer from the first foil coating (10) of the foil sheet (4) diffuses into the metal of the respective contacting metal sheet (5) at the respective flux barrier points (9) to form a flux barrier (15); and - with dissolution of the support foil (6), aluminium from the support foil (6) of the foil sheet (4) diffuses into the metal of the respective adjacent metal sheet (5).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a laminated core of an electrical machine. [Background technology]

[0002] From EP 3511429 A1, a laminated core and a method for producing a laminated core are known. Here, the metal plate layer is coated with a coating containing at least 20% aluminum and / or silicon mass fraction. Further, a heat treatment of the coated starting laminated core is carried out to produce a laminated core. In one embodiment, the produced laminated core can have a silicon content corresponding to a mass fraction of at least 6.5%. In another embodiment, a silicon content corresponding to a mass fraction of more than 4% and less than 6.5% can be achieved. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] European Patent Application Publication No. 3511429 Summary of the Invention [Means for solving the problem]

[0004] The method according to the invention with the features of the independent claims has the advantage that it allows for targeted local production of flux barriers in the metal laminations of the laminated core, which makes it possible to modify the material properties of the rotor webs to make them magnetically non-conductive and thus to produce the flux barriers. In particular, the lamination structure of the laminated core allows for the production of flux barriers with three-dimensional shapes.

[0005] According to the invention, this is achieved by the following method steps. In a first step 1a), a foil sheet is provided, each comprising an aluminum support foil and a natural or produced aluminum oxide layer, each coated on at least one side, on the flux barrier side, with a first foil coating of a first powder mixture, each comprising an austenite stabilizer or eutectic former, in particular manganese and / or nickel and / or cobalt, an electrical insulator, in particular aluminum oxide or silicon oxide (SiO2), and an adhesive binder, where the first foil coating is formed as a flux barrier after a subsequent heat treatment.

[0006] In a subsequent second step 1b), sheet metal sheets of a laminate core are provided, which are in particular not electrically insulating, ie have no paint coating. In a subsequent third step 1c), the metal sheets and the foil sheets are stacked alternately and the orientation of the foil sheets relative to the metal sheets, in particular with respect to the rotational position, is such that the magnetic flux barrier surface of each foil sheet is in direct contact with each respective metal sheet at a specific magnetic flux barrier point of each metal sheet.

[0007] In the subsequent fourth step 1d), the heating, in particular the heat treatment, of the stack of metal sheets and foil sheets takes place as follows: - the austenite stabilizer from the first foil coating of the foil lamination diffuses into the metal of the respective contacting metal lamination at the respective flux barrier point to form a flux barrier; - With the dissolution of the supporting foil, the aluminum from the supporting foil of the foil sheet diffuses into the metal of the respective adjacent sheet metal sheet, whereby the aluminum content between the surface and the core of the sheet metal sheet can be reduced.

[0008] In this way, a non-magnetic austenite phase is formed at the flux barrier points. Advantageous developments of the method presented in the independent claims are possible by the measures recited in the dependent claims.

[0009] It is advantageous if the first powder mixture further comprises an electrically insulating insulator material, in particular aluminum oxide or silicon oxide (SiO2), and / or an alloying material, in particular silicon, since in this way an insulating layer is then produced between the respective adjacent metal sheets in the region of the magnetic flux barrier surface of the respective foil sheet and / or further alloying of the respective adjacent metal sheets takes place in the region of the magnetic flux barrier surface.

[0010] It is also advantageous if in step 1a) each foil sheet is coated on the insulating side with at least one second foil coating of a second powder mixture, the second powder mixture comprising an electrically insulating insulator material, in particular aluminum oxide or silicon oxide (SiO2), and an adhesive binder. In this way, provision is made for the production of a complete insulating layer between adjacent, in particular non-insulated, metal sheet sheets.

[0011] It is highly advantageous if heating is performed in step 1d) such that insulating material, in particular from the first and / or second foil coating of the foil laminations and / or from the aluminium oxide layer, remains between the metal laminations after heating, forming insulating layers respectively between adjacent metal laminations, each insulating layer being formed in the region of the insulating surfaces and in particular in the region of the flux barrier surfaces or flux barriers. Such generation of insulating layers between adjacent metal laminations allows the use of the generated flux barrier in a laminated core.

[0012] Furthermore, an adhesive binder is provided for adhering the first or second powder mixture to the support foil of the respective foil sheet, which is advantageously in particular a paste and / or a polysaccharide, in particular xanthan and / or amylopectin. For example, in order to achieve a reliable bonding of the powder to the foil sheet, aluminum oxide powder or a powder mixture consisting of manganese powder and aluminum oxide powder can be mixed with water and xanthan. At least one side of the foil sheet can then be coated with this mixture, for example using a compressed air spray gun. Here, by means of a suitable stencil, a part of the respective metal sheet sheet can be appropriately covered, so that only the areas that will later act as flux barriers are coated when coating with the manganese-containing powder mixture. In the case of manganese-free powder mixtures, a stencil is preferably used that covers only the areas of the flux barrier. During subsequent drying, the water evaporates. The xanthan remaining in the mixture causes the powder to adhere well. The other side of the foil sheet can then be coated in the same way.

[0013] According to an exemplary embodiment, the shape and / or area of ​​the foil sheets correspond to the shape and / or area of ​​the metal sheet sheets. The foil sheets can be punched to the same shape as the metal sheet sheets before stacking on the laminated core. However, preferably, non-punched foil sheets and punched metal sheet sheets are stacked alternately to form the laminated core, and after stacking is completed, the excess aluminum foil is removed. Since the aluminum foil is very thin, less waste is required. In another possible form, the removal of the excess foil can be omitted, since it melts and drips off during the heat treatment.

[0014] It is furthermore advantageous if the first powder mixture comprises a further substance suitable for forming a eutectic with the austenite stabilizer, in particular with a melting point below 1300° C. Since nickel does not form a eutectic with iron, in order to form a eutectic with the austenite stabilizer, in particular tin is provided for forming a eutectic with nickel.

[0015] The eutectic formers are advantageously capable of promoting the formation of austenite from the liquid phase down to low temperatures without decomposition into two phases on further cooling, so that austenite is present even at room temperature. The eutectic formers are based on copper and / or zinc and / or carbon and / or nitrogen.

[0016] During heat treatment, the austenite stabilizer diffuses into the iron and austenite is produced rather than other transformations, in particular ferrite. In this case, high concentrations can be provided locally, with the austenite stabilizer diffusing to some extent from especially two faces of the respective metal sheet to the core. By means of additional substances for forming eutectics, advantageously a reduction in the melting point can be achieved, for example manganese, nickel or cobalt or a mixture of these austenite stabilizers. It is also conceivable that only the eutectic formers copper and / or zinc and / or carbon and / or nitrogen are used to bring about the formation of austenite. However, carbon has the disadvantage of being very diffusive, and nitrogen has the disadvantage of being very poorly diffusive.

[0017] Advantageously, a multi-step heat treatment in the presence of hydrogen can be envisaged. Advantageously, said heat treatment is preceded by a further heat treatment of the metal sheets between which the coated foil sheets are placed, in the range of about 150°C to about 500°C for about 1 hour to about 2 hours. In particular, this can be carried out at 400°C. In this first step, the xanthan is decomposed into water, carbon monoxide, carbon dioxide and methane and can thus be removed. In the next step, which involves a heat treatment in the range of 950°C to 1250°C, preferably 1000°C to 1100°C, in particular for 1 to 24 hours, the diffusion of the austenite stabilizer, in particular manganese and aluminium, into the metal sheets takes place. When the austenite stabilizer and aluminium have been completely diffused, an electrically insulating solid, for example aluminium oxide powder, remains between the metal sheets as an electrically insulating layer.

[0018] In one possible embodiment, an inexpensive production of laminated cores with an inherent magnetic flux barrier and a very good electrical insulation between the individual metal sheets is possible. Here, advantageously, the formation of a local inherent magnetic flux barrier in the metal sheets can be achieved by at least one austenitic stabilizer diffused in the metal sheets. Preferably, the local inherent magnetic flux barrier here extends over the thickness of each metal sheet. The inherent magnetic flux barrier is generated by the fact that each metal sheet locally loses its ferromagnetic properties and thus also loses its very high magnetic permeability or at least substantially reduces it. Furthermore, at the same time, electrical insulation between the metal sheets can be ensured.

[0019] Thus, the flux barrier is realized by omitting the electrical sheet, which, unlike conventional configurations in which slots are provided or the thickness is locally reduced by embossing, improves the mechanical stability of the metal sheet. In particular, this allows higher maximum speeds, in particular for the rotor, and improves the vibration resistance of the laminated core. Furthermore, advantageously, the morphology of the flux circuit can be improved, in particular allowing a more free morphology without requiring significant manufacturing costs.

[0020] Thus, the austenite stabilizer advantageously makes it possible to achieve paramagnetic austenite and thus avoid the formation of ferromagnetic and therefore highly permeable ferrite. In the regions where the austenite stabilizer is diffused, the paramagnetic austenite is stable up to room temperature.

[0021] The powdered austenite stabilizer can advantageously be part of a powder mixture with insulating solids (especially silicon dioxide) and possibly further substances as alloying materials (especially silicon). The coated aluminum foil is preferably cut into foil sheets of a size that can completely cover the individual metal sheet. When stacking metal sheets for the rotor or stator electrical sheets, preferably one piece of foil is placed for each metal sheet to be placed in the stack. The stack formed thereby advantageously consists of alternating stacks of metal sheets and foil sheets. During the subsequent heat treatment, the austenite stabilizer or silicon or aluminum of the aluminum foil is diffused depending on the presence in one area, and the electrically insulating powder remains as an electrically insulating layer between adjacent metal sheets.

[0022] In one possible form, the aluminum foil is coated with at least two different powder mixtures, both powder mixtures containing powders of inorganic electrical insulators. Here, at least one of the powder mixtures preferably contains at least one austenite stabilizer. The coated aluminum foil can then be stacked alternately with metal sheet laminations to form a laminated core. A heat treatment is then performed to diffuse the aluminum and austenite stabilizer into the metal sheet laminations. Here, the insulating powder remains as an electrical insulating layer between adjacent metal sheet laminations. The coating can be performed by methods such as spraying, brushing, printing, etc.

[0023] Substances suitable for the austenite stabilizer are preferably those which strongly promote the formation of austenite when cooling from temperatures above 1200 ° C. A further requirement may be that such an austenite stabilizer is stable to hydrogen atmospheres and diffuses into the iron of the sheet metal at least at 1200 ° C. Manganese, nickel and cobalt are particularly preferred, but also copper. Copper forms a eutectic up to low temperatures at which austenite can no longer be decomposed into other phases. Furthermore, it is advantageous to apply the austenite stabilizer together with further substances, especially with melting points below 1300 ° C, which do not participate in the formation of ferrite or austenite but form a eutectic with the austenite stabilizer. Such further substances may also be austenite stabilizers, but less effectively.

[0024] Suitable materials for the electrically insulating powder are electrically insulating solids which are stable and do not melt, preferably in a water atmosphere up to at least 1250°C. In a hydrogen atmosphere, a significant reduction in aluminum oxide occurs only at 1300°C, up to a mass fraction of 20%. At a heat treatment temperature of 1250°C, the aluminum oxide is reduced by up to 7%. Silicon oxide (SiO2) and mullite (Al (4+2x) S (2-2x) O (10-x) , where x = 0.17 to x = 0.59), are also stable and do not melt in strongly reducing aqueous atmospheres up to 1250 °C, and therefore are similarly suitable as electrically insulating solids.

[0025] For example, the aluminum foil may have a foil thickness of 5 μm and may be print coated on both sides with a mixture of manganese powder and aluminum oxide powder, or only aluminum oxide powder, depending on the desired flux barrier geometry in one form. The manganese powder may consist of manganese nanopowder with a particle size of between about 30-50 nm, and / or manganese powder with an average particle size of 1-5 μm. The aluminum oxide powder may have an average particle size of, for example, 3 μm, or alternatively 40 nm. However, depending on the application and availability, other particle sizes may be used for the manganese powder or manganese nanopowder, and the aluminum oxide powder. The same applies for other materials.

[0026] It is therefore possible to realize laminated cores at low cost and with advantageous properties, which in particular allows the economical realization of very powerful electric motors, which are used, for example, in electric cars, electric bicycles or hybrid drives.

[0027] Preferred exemplary embodiments of the present invention are described herein below in more detail with reference to the accompanying drawings, in which corresponding elements are marked with the same reference numerals, and in which: [Brief description of the drawings]

[0028] [Figure 1] FIG. 2 is a schematic diagram of a laminated core before heat treatment. [Figure 2A] FIG. 2 is a partial view of the laminated core according to FIG. 1 according to detail II in FIG. [Figure 2B] FIG. 2 is a partial view of the laminated core according to FIG. 1 after heat treatment according to detail II in FIG. [Diagram 3] 2C is a partial view of the laminated core corresponding to the viewing direction III in FIG. 2B. [Figure 4A] FIG. 1 is a phase diagram for explaining the present invention, in which a diagram for an austenite stabilizer is shown. [Figure 4B] FIG. 1 is a phase diagram for explaining the present invention, in which a diagram for eutectic formers is shown. [Figure 4C]FIG. 1 is a phase diagram for explaining the present invention, in which a diagram for ferrite forming materials is shown. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0029] FIG. 1 shows a schematic diagram of a laminated core 1 before heat treatment. FIG. 2A shows a partial view of the laminated core according to FIG. 1 according to detail II in FIG. FIG. 2B is a partial view of the laminated core according to FIG. 1 after heat treatment according to detail II in FIG.

[0030] The laminated core 1 includes a plurality of metal sheet laminations 5 based on an iron-based material stacked on top of each other. Here, FIG. 1 shows the state of the laminated core 1 before heat treatment. The laminated core 1 may be a rotor or stator laminated core of an electric machine. The laminated core 1 is formed into a cylindrical shape.

[0031] 2A and 2B show in schematic and partial views the laminated core 1 according to a possible form, before and after heat treatment. To manufacture the laminated core 1, the following method steps are carried out according to the invention:

[0032] In a first step 1a), a foil sheet 4 is provided, comprising an aluminium support foil 6, i.e. aluminium foil 6, and a natural or produced aluminium oxide layer 7, each coated on at least one side 11, 12, respectively, on a flux barrier surface 8 with a first foil coating 10 of a first powder mixture, the first powder mixture comprising an austenitic stabiliser, in particular manganese and / or nickel and / or cobalt, aluminium oxide and an adhesive binder.

[0033] In a second step 1b), a metal sheet 5 of the laminated core 1 is provided, which is in particular not electrically insulated. The metal sheet 5 is produced from an electrical sheet. The shape and / or area of ​​the foil sheet 4 may correspond to the shape and / or area of ​​the metal sheet 5.

[0034] In a third step 1c), the metal sheets 5 and the foil sheets 4 are stacked alternately, the foil sheets 4 being oriented relative to the metal sheets 5 such that the magnetic flux barrier surface 8 of each foil sheet 4 is in direct contact with each respective metal sheet 5 at a specific magnetic flux barrier point 9 of each metal sheet 5.

[0035] In a fourth step 1d), the laminate of metal sheets 5 and foil sheets 4 is heated, for example by heat treatment in an oven. According to the invention, the heating is carried out as follows: - the austenite stabilizer from the first foil coating 10 of the foil lamination 4 diffuses into the metal of the respective contacting metal lamination 5 at the respective flux barrier point 9 and forms a flux barrier 15 in the metal lamination 5, With the melting of the supporting foil 6, the aluminium from the supporting foil 6 of the foil lamella 4 diffuses to a certain depth into the metal of the respective adjacent metal sheet lamella 5.

[0036] The first powder mixture may further comprise an electrically insulating insulator material, in particular aluminum oxide or silicon oxide (SiO2), and / or an alloy material, in particular silicon. It can further be provided that in step 1a), the foil sheets 4 are each coated on the coated side 11, 12, respectively on the insulating side 16 on which the magnetic flux is retained, with at least one second foil coating 20 of a second powder mixture, the second powder mixture comprising an electrically insulating insulator material, in particular aluminum oxide or silicon oxide (SiO2), respectively, and an adhesive binder. Then, heating in step 1d) is performed, in which the insulator material, in particular from the first and / or second foil coating 20 of the foil sheet 4 and / or from the aluminum oxide layer 7, remains between the metal sheet sheets 5 after completion of the heating and forms an insulating layer 32, respectively, between adjacent metal sheet sheets 5, where the respective insulating layer 32 can be formed in the region of the insulating side 16, more particularly in the region of the magnetic flux barrier side 8 or the magnetic flux barrier 15.

[0037] The adhesive binder of the first and second powder mixtures is used to adhere the first or second powder mixture to the support foil 6 of the respective foil sheet 4 and may be, for example, a paste and / or a polysaccharide, in particular xanthan.

[0038] Several exemplary embodiments of the present invention are described below. Before the heat treatment, an aluminum-based foil sheet 4, which can be cut, for example, from an aluminum foil, is inserted between the metal sheet sheets 5 when they are stacked. The aluminum foil from which the foil sheet 4 is derived is provided or coated, for example, preferably on both sides, with a natural or produced aluminum oxide layer 7. Here, the aluminum oxide layer 7 is formed continuously. Furthermore, on both sides, at least one first coating 10 comprising an austenite stabilizer is provided, which coating 10 is only partially applied. In this exemplary embodiment, the foil sheet 4 has an upper side 11, 12, to which the first coating 10 comprising an austenite stabilizer is applied. Furthermore, in the areas where the first coating 10 is not applied, a second coating 20, which may comprise, for example, a silicon-based alloy material, is applied.

[0039] Between adjacent metal sheet laminates 5 of the laminated core 1 foil laminates 4 are arranged, each having at least one aluminium oxide layer 7. Furthermore, a first coating 10, which for example comprises manganese as an austenite stabiliser, is applied to the foil laminates 4. Where no manganese is applied on each foil piece 4 a second coating 20, which comprises silicon as alloying material, can be applied.

[0040] A respective first foil coating 10 is applied to the foil sheet 4 and each foil sheet 4 is positioned between two metal sheets 5 of the laminated core 1, thereby allowing austenite stabilizers and / or eutectic formers and / or formers of eutectics with austenite formers to be diffused into the material of each metal sheet 5 at the flux barrier points 9 of each metal sheet 5 by heat treatment.

[0041] After heat treatment, the metal sheet laminae 5 may have areas diffused with manganese, areas diffused with silicon and aluminum, and an aluminum oxide layer 32 remaining between the metal sheet laminae 5 . As shown in FIG. 2B, after the heat treatment, an insulating layer 32 remains between the metal sheets 5. Here, the insulating layer 32 is obtained from the electrically insulating solid remaining between the metal sheets 5. The aluminum of the support foil 6 of the foil sheet 4 diffuses into the metal sheets 5 together with the silicon, resulting in an average penetration depth in each metal sheet 5. The metal sheets 5 are thereby formed with ferroalloy or high-alloy ferroalloy material at least near the surface. The austenite stabilizer from the first coating 10 also diffuses into the metal sheets 5, whereby some diffusion from the further foil sheets 4 (not shown) also occurs on both sides. An appropriate concentration of the austenite stabilizer results in a magnetic flux barrier 15 in the metal sheets 5 and a magnetic flux barrier 14 in the adjacent metal sheets 5 across the entire thickness 33 of the metal sheet 5.

[0042] The austenite stabilizer of the first coating 10 is based on manganese and / or nickel and / or cobalt and / or copper. Here, it is also possible to use further substances which preferably form a eutectic to lower the melting point, but which at the same time promote austenite formation or have little effect on austenite formation. These substances, in particular the electrically insulating solid and the austenite stabilizer, are preferably formed in powder form and applied to the top side 11, 12 of the foil sheet 4 by means of an adhesive, in particular an adhesive binder and / or a polysaccharide, in particular xanthan or amylopectin. Here, it is not necessarily necessary to separate them into individual layers as shown in FIG. 1. This means, on the one hand, that the alloy material, in particular silicon, can also be mixed with the electrically insulating solid and then applied partially to the top side 11, 12 of the foil sheet 4 by means of an adhesive binder and / or a polysaccharide. On the other hand, the austenite stabilizer can be applied to the remaining part mixed with the electrically insulating solid. Here, other sequences are also possible.

[0043] FIG. 3 is a partial view of the laminated core corresponding to the viewing direction III in FIG. 2B. The austenite stabilizer is applied to the foil laminations 4 in such a way as to form flux barriers 15 at the flux barrier points 9 in the respective metal laminations 5. In this exemplary embodiment, the flux barriers 15 are arranged in or on the webs 16 of the metal laminations 5. The webs 16 are formed, for example, by recesses 22 in the respective metal laminations 5. The recesses 22 may be provided, for example, near the circumference 21 of the laminated core 1.

[0044] Thus, for example, specific local magnetic flux barriers 15 can be formed in the metal sheet 5. These magnetic flux barriers 15 allow substantial improvements in form and functionality. 4A, 4B, and 4C, the effect of a suitable alloying element X on the size of each austenite domain is shown in each phase diagram of FeX, where the concentration (wt%) of each alloying element X is plotted on the x-axis, respectively, and the temperature T is plotted on the y-axis, respectively.

[0045] 4A is a phase diagram for illustrating the present invention, showing a diagram of an austenite stabilizer. With manganese as an austenite stabilizer, the austenite phase (γ) becomes stable at lower temperatures as the concentration of manganese increases, as shown in the schematic phase diagram. In this diagram, room temperature is shown as the lower temperature limit.

[0046] 4A an exemplary behavior according to the invention is shown according to line Y, illustrating the effect of austenite stabilization during the course of heat treatment. Due to the diffusion of the austenite stabilizer into the respective metal sheet 5, the austenite of the heated metal sheet 5 is stabilized, so that on cooling of the metal sheet 5, the austenite is not transformed back into ferrite according to the phase diagram.

[0047] FIG. 4B shows a phase diagram for explaining the present invention, in which a diagram for eutectic forming materials is shown. As shown in the schematic phase diagram, with copper as a eutectic former, the austenite phase becomes stable at lower temperatures as the concentration of copper increases. However, this does not allow stability down to room temperature. At a certain copper concentration, a minimum temperature value occurs at which the austenite phase is still stable. This region, where austenite is stable even at low temperatures clearly below A3, allows the austenite to be nearly frozen on cooling and thus preserved on further cooling to room temperature. Then, as the concentration of copper increases further, the temperature at which the austenite phase is stable also increases. This makes it increasingly difficult and eventually impossible to nearly freeze the austenite on cooling. A further increase in the copper concentration leads to a concentration at which the formation of the austenite phase in iron is no longer possible.

[0048] FIG. 4C is a phase diagram for explaining the present invention, showing a diagram for ferrite forming materials. As shown in the schematic phase diagram, ferrite (α) is the stable phase at room temperature due to ferrite formers such as silicon and aluminum. This means that austenite is stable only when low concentrations of ferrite formers and high temperatures are simultaneously present. Therefore, austenite cannot freeze out on cooling, since it will transform to ferrite at higher temperatures.

[0049] The invention is not limited to the exemplary embodiments described above.

Claims

1. A method for manufacturing a laminated core (1) of an electric machine, in particular for creating a flux barrier within said laminated core (1), comprising the steps of: a) providing a foil sheet (4) each comprising an aluminum support foil (6) and a natural or produced aluminum oxide layer (7) and each coated on at least one side (11, 12) on a flux barrier surface (8) with a first foil coating (10) of a first powder mixture, said first powder mixture comprising an austenitic stabilizer, in particular manganese and / or nickel and / or cobalt, aluminum oxide and an adhesive binder; b) providing a metal sheet (5) of the laminated core (1), said metal sheet (5) being in particular not electrically insulating; c) stacking metal sheet laminations (5) and foil laminations (4) alternately, the foil laminations (4) being oriented relative to the metal sheet laminations (5) such that the magnetic flux barrier surface (8) of each foil lamination (4) is in direct contact with each metal sheet lamination (5) at a specific magnetic flux barrier point (9) of each metal sheet lamination (5); d) heating, in particular heat treating, the laminate of metal sheets (5) and foil sheets (4), - the austenite stabilizer from the first foil coating (10) of the foil laminate (4) diffuses into the metal of the respective contacting metal sheet laminate (5) at the respective flux barrier points (9) to form a flux barrier (15); - with the dissolution of the support foil (6), the aluminium from the support foil (6) of the foil laminations (4) diffuses into the metal of the respective adjacent metal laminations (5); method.

2. The first powder mixture further comprises an electrically insulating insulating material, in particular aluminum oxide or silicon oxide (SiO 2 2. The method according to claim 1, characterized in that the material contains a metal, a ferroelectric material, and / or an alloy material, in particular silicon.

3. In step 1a), the foil sheets (4) are each further coated on the coated side (11, 12), respectively on the further insulating side (16), with at least one second foil coating (20) of a second powder mixture, the second powder mixture being each an electrically insulating insulator material, in particular aluminum oxide or silicon oxide (SiO 2 3. The method of claim 1, further comprising the step of:

4. 4. The method according to claim 2 or 3, characterized in that the heating in step 1d) is performed such that the insulating material, in particular from the first and / or second foil coating (20) of the foil laminations (4) and / or from the aluminium oxide layer (7), remains between the metal sheet laminations (5) after the heating, forming insulating layers (32) between adjacent metal sheet laminations (5), respectively, the insulating layers (32) being formed in the region of the insulating surface (16) and in particular in the region of the flux barrier surface (8) or the flux barrier (15).

5. 5. The method according to any one of claims 1 to 4, characterized in that the adhesive binder is provided for adhering the first or second powder mixture to the support foil (6) of the respective foil sheet (4), and is in particular a paste and / or a polysaccharide, in particular xanthan and / or amylopectin.

6. 6. The method according to claim 1, wherein the shape and / or area of ​​the foil sheet (4) corresponds to the shape and / or area of ​​the metal sheet (5).

7. 7. The method according to any one of claims 1 to 6, characterized in that the first powder mixture comprises a further substance suitable for forming a eutectic with an austenite stabiliser, in particular tin, in particular with a melting point below 1300°C.

8. 8. The method according to claim 7, characterized in that the eutectic formers promote the formation of austenite from the liquid phase down to low temperatures, so that the austenite is also present at room temperature, and are in particular based on copper and / or zinc and / or carbon and / or nitrogen.

9. 9. The method according to any one of the preceding claims, characterized in that, prior to said heat treatment, a further heat treatment of the metal sheet laminates (5) between which the coated foil laminates (4) are arranged is carried out in a hydrogen-containing atmosphere at a temperature in the range of about 150°C to about 500°C for about 1 hour to about 2 hours in order to decompose the adhesive binder of the first and / or second foil coating (10, 20).

Citation Information

Patent Citations

  • Rotating electrical machine

    CN209659032U

  • Magnetic substance and its manufacture

    JP1996222422A

  • Method of forming non-magnetic region of steel material, and steel material having non-magnetic region formed thereon

    JP2008099360A

  • Methods of manufacturing coil and coil device

    JP2010199291A

  • Rotor core

    JP2015198475A