Surface treatment equipment

The surface treatment method optimizes laser irradiation parameters to remove hematite and magnetite layers on steel, enhancing surface preparation for painting and adhesion by ensuring 78.5% hematite removal, addressing environmental and efficiency issues in existing methods.

JP7551247B2Active Publication Date: 2024-09-17NIPPON STEEL TEXENG CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021035877
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-05
Publication Date
2024-09-17
Estimated Expiration
2041-03-05

AI Technical Summary

Technical Problem

Existing methods for removing surface oxidation scale from steel materials, such as shot blasting and conventional laser treatments, face issues with environmental impact, inefficiency, and inadequate quality evaluation, particularly in preparing surfaces for painting and adhesion.

Method used

A surface treatment method using a pulsed laser beam with variable irradiation distance and scanning mechanism to effectively remove hematite and magnetite layers on steel surfaces, optimizing laser density and spot diameter for efficient scale removal and improved adhesion.

Benefits of technology

The method enhances the quality of surface treatment by ensuring 78.5% or more area ratio of hematite removal, improving adhesion of coatings and adhesives on steel materials, while maintaining efficient processing times.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007551247000003
    Figure 0007551247000003
  • Figure 0007551247000002
    Figure 0007551247000002
  • Figure 0007551247000006
    Figure 0007551247000006
Patent Text Reader

Abstract

To improve a quality of substrate treatment of a steel material which is supplied to a treatment process such as coating, bonding and lining of attaching and bonding an object to an object by a coating material (coating material and lining material) and an adhesive.SOLUTION: A laser density step ST1 initially sets laser density of a pulse-irradiated laser beam per one pulse at laser density effective for removing hematite (Fe2O3) of a surface layer of an oxide film on the basis of a spot diameter dp of a pulse laser beam based on a laser irradiation distance and a moving distance dm of an irradiation position per one pulse. A Keren treatment step ST2 performs Keren treatment of emitting the pulse laser beam of the initially set laser density, and removing the hematite (Fe2O3) of the surface layer of the oxide film, and thereby removes a slag 3B having low adhesion from the steel plate surface after laser Keren, and only an oxide film (Fe3O4)3A having high adhesion is provided thereon.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a surface preparation method and a surface preparation treatment device for removing deposits from an object by laser irradiation, and in particular to a method for removing part of a two-layer oxide coating of hematite and magnetite that is attached to the surface of a steel material, which is the object of treatment. Substrate treatment equipment to be removed Regarding.

[0002] Here, the process of removing the oxide film adhering to the surface of the object is called scraping process. [Background technology]

[0003] Conventionally, when removing rust or paint from the surface of an object, paint removers or shot blasting have been used. However, this not only results in poor working conditions and efficiency, but also poses problems in recovering and disposing of the large amount of material removed. For this reason, a method of removing rust or removing paint using laser irradiation has been proposed.

[0004] For example, a method for producing metal nanocolloids has been proposed in which a target placed in a liquid is irradiated with pulsed laser processing by scanning the laser spot at a distance of at least a certain distance from the target (see, for example, Patent Document 1).

[0005] Patent Document 1 describes that the distance from the water surface to the target is kept constant, the water surface and the target surface are made parallel, and a pulsed laser is applied at a constant speed for laser processing.

[0006] In addition, as a laser processing apparatus and method capable of cutting brittle materials having high residual stress without causing cracks, a laser light irradiation mechanism has been proposed which pulses laser light to irradiate and scan the workpiece at a constant repetition frequency, and the irradiation mechanism is provided with a laser light irradiation mechanism which sets the repetition frequency to H, the beam diameter of the laser light to a, the number of scans of the laser light on the same processing line to n, and the moving distance L per irradiation of the pulsed laser light to n / 2×a, where the scanning speed S of the laser light is set to L / (1 / H), the start position of irradiation of the laser light for the first scan is set to L1, and the start position of irradiation of the laser light for the nth scan is set to L1+(L / n)×(n−1), and irradiation is performed by shifting the start position of irradiation for each scan (see, for example, Patent Document 2).

[0007] Furthermore, when manufacturing thin steel sheets, a heated slab is hot-rolled into a steel sheet, and as the steel sheet cools naturally, an oxide film (scale) forms on the surface of the steel sheet. In the pickling process, the steel sheet is passed through a pickling tank to remove the oxide film.

[0008] In order to efficiently and reliably remove the oxide film in the pickling process, it has been proposed to irradiate the oxide film containing magnetite with laser light before the pickling process to transform the magnetite into wustite of approximately the same thickness as the magnetite, and then irradiate the oxide film with terahertz waves and determine the thickness of the oxide film using the signal of the reflected wave of the irradiated terahertz waves (see, for example, Patent Document 3). [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2018-40033 A [Patent Document 2] JP 2011-177781 A [Patent Document 3] JP 2009-186333 A Summary of the Invention [Problem to be solved by the invention]

[0010] As mentioned above, when painting or welding steel materials, it is necessary to remove the scale (iron oxides formed during manufacturing) from the surface of the relevant area before carrying out the work. Usually, shot blasting is used, in which tiny iron balls are struck against the surface of the steel material, and the kinetic energy is used to remove the scale (or a handy grinder is used for small-scale work), but this method has environmental problems such as dust, noise, and vibration, as well as high costs for disposing of the shot balls used and the waste material after removal.

[0011] Therefore, surface preparation using a laser has been conventionally carried out as a method that can improve both the environment and costs.

[0012] In the coating removal treatment using laser irradiation, the coating film on the surface of the treatment object can be removed by laser ablation without using chemicals.

[0013] However, the technology disclosed in Patent Document 1 is a metal nanocolloid production method in which a pulsed laser is irradiated onto a target placed in a liquid, with the laser spot scanned and irradiated at a distance of at least a certain distance from the target, and the laser irradiation pitch for each pulse is set at a distance of at least 10 times the spot diameter, which is unique to the field of metal nanocolloid production.In normal cases, it is clear that unirradiated areas will occur if the distance between spot diameters is made too large, and there is a problem that these areas cannot be treated.

[0014] In addition, the technology disclosed in Patent Document 2 is a cutting method that suppresses the thermal effects of the laser, but by making the irradiation pitch per pulse 1.5 times the spot diameter, overlapping irradiation is avoided and the resulting unirradiated areas are filled in by the next and subsequent irradiations. This method requires multiple irradiations, which causes a problem of reduced work efficiency.

[0015] Due to its focusing characteristics, lasers enable processing with high energy density, but they must be used under optimal conditions in terms of equipment capacity (cost) and work efficiency. Naturally, in work with high laser density and high laser focusing rate (small spot diameter), the quality (scale removal performance in surface preparation work) is excellent, but the work time is longer and work efficiency is reduced. On the other hand, in work with low laser density and low laser focusing rate (large spot diameter), the quality is reduced but the irradiation time is shorter. Therefore, it is necessary to set optimal conditions in terms of the quality and work efficiency of the work.

[0016] As mentioned above, surface preparation work is carried out when painting or gluing components in order to improve the paint and adhesive performance. There are judgment standards such as ISO for evaluating the performance of the surface preparation work, but all of them are qualitative judgments made by the installer at the work site through visual inspection.

[0017] Surface preparation using a laser (hereinafter referred to as laser cleaning) was developed as a new surface preparation method, and the quality evaluation standards for the blasting method may not be able to evaluate it correctly. In response to this, JIS Z2358 has established a method for quantitatively judging the quality of laser surface preparation using a colorimeter. In contrast to the conventional qualitative evaluation standards for the blasting method, this method evaluates the performance of laser cleaning by measuring the color saturation of the surface after laser cleaning (visual inspection is also possible) and comparing it with an existing color sample. However, although this method measures color saturation, the measurement is strongly affected by external disturbances such as the degree of exposure to external light, and there is a problem that it cannot be evaluated correctly. In addition, the comparison with the color sample is done visually, and in this case, the evaluation is qualitative.

[0018] On the other hand, one of the important quality performance factors of coatings and adhesives is the adhesion to the components, and for existing materials, especially steel materials, the degree to which surface oxide scale has been removed is one of the important factors.

[0019] The technology disclosed in Patent Document 3 is to measure the oxide film thickness and optimize the steel sheet conveying speed in the pickling line based on the measurement results in order to improve the efficiency of the pickling process for removing surface scale from hot-rolled steel sheets. In measuring the oxide film thickness, the hematite on the outermost surface is removed by irradiating a laser beam onto an oxide film having a two-layer structure of hematite and magnetite from the surface, and the remaining magnetite is transformed into wustite, after which the thickness of the wustite is measured. Patent Document 3 describes the removal of hematite by laser irradiation, but the purpose is to measure the oxide film thickness, and not to improve pretreatment (surface treatment) such as painting or adhesion. In addition, there is no description regarding the feed speed of laser irradiation.

[0020] In view of the above-mentioned conventional circumstances, the object of the present invention is to provide a method for qualitatively removing surface oxide scale of steel materials. Possible surface treatment equipment The purpose of this invention is to provide

[0021] Another object of the present invention is to improve the quality of the surface preparation of steel materials to be supplied to processing processes such as painting, bonding, lining, etc., in which objects are attached or bonded to each other using coating materials (paints and lining materials) or adhesives.

[0022] Other objects of the present invention and specific advantages obtained by the present invention will become more apparent from the following description of the embodiments. [Means for solving the problem]

[0023] As a result of detailed observation of the surface condition after laser scraping, the inventors of the present invention discovered that the surface preparation performance can be improved by removing hematite (Fe2O3), which is one of the main components that make up the oxide scale on the surface of steel.

[0024] In the present invention, the hematite (Fe2O3) on the surface side, which is part of the two-layer oxide film of hematite (Fe2O3) and magnetite (Fe3O4) adhering to the surface of the steel material to be treated, is removed.

[0032] That is, The present invention is a surface treatment device for removing a part of an oxide film having a two-layer structure of hematite (Fe2O3) and magnetite (Fe3O4) adhering to the surface of a steel material, which is a processing object, by irradiating the surface with a pulse of laser light, the device comprising: irradiation distance variable setting means for variably setting a laser irradiation distance for irradiating a processing target area of ​​the steel material, which is the processing object, with a pulsed laser light; scanning means for moving an irradiation position of the pulsed laser light within a working area including the processing target area; a pulsed laser light irradiation device for irradiating the processing target area of ​​the steel material, which is the processing object, with a pulsed laser light; and a control device for controlling the operation of the pulsed laser light irradiation device, the control device controlling the operation of the pulsed laser light irradiation device to adjust the laser density per pulse of the pulsed laser light irradiated by the pulsed laser light irradiation device to a spot diameter d of the pulsed laser light based on the laser irradiation distance. p and the moving distance of the irradiation position per pulse d m The present invention is characterized in that the operation of the pulsed laser light irradiation device is controlled so that a laser density effective for removing hematite (Fe2O3) on the surface of the oxide film is initially set based on the above-mentioned, and the irradiation position of the pulsed laser light is moved by the scanning means within a working area including the area to be treated, and the pulsed laser light of the initially set laser density is irradiated to perform a scraping process for removing hematite (Fe2O3) on the surface of the oxide film. Here, the laser projection distance is the distance between the lens that focuses the laser light and the surface of the target object. Therefore, when the laser projection distance is equal to the focal length of the lens, the spot diameter is minimized.

[0033] In the surface treatment device of the present invention, the control device can control the operation of the pulsed laser light irradiation device so that the proportion of hematite (Fe2O3) removed by the scraping process is 78.5% or more in terms of area ratio on the surface of the oxide coating after the scraping process.

[0034] In the surface treatment device according to the present invention, the control device is configured to control the moving distance d of the irradiation position of the pulsed laser beam per pulse by the scanning means. m is the spot diameter d pThe operation of the pulsed laser light irradiation device can be controlled so as to move the pulsed laser light irradiation device at a moving speed within the range of ×(1 / 2 to 1).

[0035] Furthermore, in the surface treatment device according to the present invention, the control device defocuses the pulsed laser light irradiated onto the treatment target area of ​​the steel material, which is the treatment target, by the irradiation distance variable setting means, thereby setting a spot diameter d p may be set to an optimal value. Here, defocusing refers to making the laser irradiation distance longer or shorter than the focal distance of the lens, which makes the spot diameter of the laser light larger than the minimum spot diameter. Effect of the Invention

[0036] In the present invention, the laser density per pulse of the pulsed laser light is determined by the spot diameter d of the pulsed laser light based on the laser irradiation distance. p and the moving distance of the irradiation position per pulse d m Based on this, the laser density is initially set to an effective value for removing the hematite (Fe2O3) on the surface of the oxide film, and pulsed laser light of the initially set laser density is irradiated to remove the hematite (Fe2O3) on the surface of the oxide film. As a result, the hematite (Fe2O3), which has low adhesion, is removed from the steel sheet surface after laser scraping, and magnetite (Fe3O4), which has high adhesion, takes up the majority of the surface, improving the adhesion of the paint.

[0037] Therefore, according to the present invention, it is possible to improve the quality of the surface preparation of steel materials to be supplied to processing processes such as painting, bonding, lining, etc., in which objects are attached or bonded to each other using coating materials (paints and lining materials) or adhesives.

[0038] In addition, in the present invention, the ratio of hematite (Fe2O3) to be removed in the scraping process is set to 78.5% or more in terms of the area ratio on the surface of the oxide film after the scraping process, thereby qualitatively improving the removal of surface oxide scale of steel materials. Possible surface treatment equipment can be provided.

[0039] Furthermore, in the present invention, when performing the cleaning process, the moving distance d of the irradiation position of the pulsed laser light per pulse is m is the spot diameter d p By moving the material at a speed within the range of × (1 / 2 to 1), the qualitative effect of removing surface oxide scale of the steel material can be obtained. Possible surface treatment equipment can be provided. [Brief description of the drawings]

[0040] [Figure 1] 1 is a block diagram showing an example of the configuration of a substrate processing apparatus according to the present invention; [Diagram 2] FIG. 2 is a perspective view showing a schematic structure of a two-axis galvanometer mirror mechanism provided in the substrate processing apparatus. [Diagram 3] 4 is a schematic diagram showing a feeding state of an irradiation position of a pulsed laser beam in the above-mentioned surface treatment device. FIG. [Figure 4] FIG. 13 is a schematic diagram showing the movement trajectory of the laser spot by the above-mentioned two-axis galvanometer mirror mechanism, in which (A) is a schematic diagram showing the state of laser irradiation, and (B) is a schematic diagram showing the state of laser irradiation in which the second row and subsequent rows are irradiated at intermediate positions between the irradiation positions of the previous row when the laser is irradiated in a folded manner. [Diagram 5] 1A and 1B are diagrams showing schematic cross-sectional structures of objects to be processed by the above-mentioned base treatment device, in which (A) is a schematic cross-sectional view of the object to be processed before the base treatment, and (B) is a schematic cross-sectional view of the object to be processed after the base treatment. [Figure 6] 3A to 3C are process diagrams showing a surface treatment method carried out by the surface treatment device. [Figure 7] (A) shows the case where the moving speed is such that the moving distance dm1 per pulse is equal to the spot diameter dp, (B) shows the case where the moving distance dm2 per pulse is equal to (1 / √2) times the spot diameter dp, and (C) shows the case where the moving distance dm3 per pulse is equal to (1 / 2) times the spot diameter dp. [Figure 8]This figure shows the results of checking the adhesion strength by a tensile test (pull-off test) after coating a test piece with paint and drying and curing it in order to evaluate the performance of a laser scraper with different laser intensity (energy density). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0041] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. Common components will be described with common reference numerals in the drawings. Furthermore, the present invention is not limited to the following examples, and can be modified as desired without departing from the gist of the present invention.

[0042] The present invention relates to For example, as shown in the block diagram of FIG. 1, the process is carried out by a surface treatment device 100 that performs surface treatment work using a robot.

[0043] In this substrate processing device 100, the robots used for substrate processing work include manipulator robots composed of multi-joint links, three-axis robots composed of three axes (X, Y, Z), or transport devices using mobile trolleys, and this substrate processing device 100 employs a manipulator robot 40 consisting of a manipulator 20 (including a robot arm 21) and a robot control unit 30.

[0044] That is, this base treatment device 100 is a device in which a pulsed laser light irradiation device 10 is carried by a manipulator robot 40 and performs base treatment work to remove adhesions from the treatment object 1 by irradiating it with pulsed laser light, and is composed of a pulsed laser light irradiation device 10, a manipulator robot 40, and an overall control device 50, etc.

[0045] The pulsed laser light irradiation device 10 comprises a laser oscillator 11, an optical fiber 12 for transmitting laser light from the laser oscillator 11, and a laser head 13 for irradiating the laser light.

[0046] In this pulsed laser light irradiation device 10, the laser light irradiation conditions are controlled by an overall control device 50, a pulsed laser light Lp is generated by a laser oscillator 11, and is emitted from a laser head unit 13 to irradiate the treatment object 1.

[0047] As shown in FIG. 2, the laser head unit 13 of the pulsed laser light irradiation device 10 is provided with a two-axis galvanometer mirror mechanism 130 consisting of two motors 131X and 131Y and two mirrors 132X and 132Y.

[0048] This two-axis galvanometer mirror mechanism 130 is capable of scanning the pulsed laser light Lp supplied from the laser oscillator 11 via the optical fiber 12 by changing the laser reflection angle independently in the X-axis and Y-axis directions.

[0049] The two-axis galvanometer mirror mechanism 130 functions as a scanning means for moving the irradiation position of the pulsed laser light Lp within the processing target area of ​​the processing target 1.

[0050] That is, the mirror 132X is rotated around the Z axis by the motor 131X, thereby scanning the pulsed laser light Lp to be irradiated onto the processing object 1 in the X axis direction.

[0051] Furthermore, the mirror 132Y is rotated around the X-axis by the motor 131Y, thereby scanning the pulsed laser light Lp to be irradiated onto the processing object 1 in the Y-axis direction.

[0052] The two mirrors 132X and 132Y in the two-axis galvanometer mirror mechanism 130 can each be replaced with a polygon mirror.

[0053] That is, with the position of the laser head portion 13 of the pulsed laser light irradiation device 10 fixed, it is possible to irradiate within a predetermined range.

[0054] In addition, in scanning by a galvanometer mirror or a polygon mirror, the optical axis coincides with the normal direction at only one point, and the focal position of the pulsed laser light Lp is located on an arc, so this two-axis galvanometer mirror mechanism 130 irradiates the processing object 1 with the pulsed laser light Lp via a telecentric f-θ lens (or a telecentric optical system having optical characteristics equivalent to a telecentric f-θ lens) 133. That is, in laser irradiation by galvanometer mirror scanning, the focal length to the processing object 1 changes, so it is necessary to restrict the laser irradiation range so that the irradiation position of the pulsed laser light Lp is scanned within a range where the deterioration of the laser processing ability is small.

[0055] Moreover, the manipulator 20 of the manipulator robot 40 includes a multi-joint robot arm 21, and the laser head unit 13 of the pulsed laser light irradiation device 10 is attached to a tip portion 21A of the robot arm 21.

[0056] That is, the laser head 13 of the pulsed laser light irradiation device 10 attached to the tip 21A of the robot arm 21 is capable of irradiating pulsed laser light Lp in any direction at any position within the working range of the manipulator robot 40.

[0057] In addition, the manipulator robot 40 functions as an irradiation distance variable setting means for variably setting the laser irradiation distance at which the pulsed laser light Lp is irradiated from the laser head unit 13 onto the processing target area of ​​the processing target 1.

[0058] The overall control device 50 transmits predetermined robot operating conditions to the robot control unit 30 so that the laser head unit 13 of the pulsed laser light irradiation device 10 attached to the tip 21A of the robot arm 21 passes through a pre-set surface treatment work trajectory by the manipulator robot 40, and the robot control unit 30 controls the robot based on this and transmits the laser irradiation conditions of the pulsed laser light irradiation device 10 to the laser oscillator unit 11, and the laser oscillator unit 11 emits laser based on this and operates the galvanometer mirror mechanism 130, thereby automatically controlling a series of surface treatment work operations by this surface treatment device 100.

[0059] The manipulator robot 40 in this surface treatment device 100 is basically controlled by programming the movement trajectory in advance by teaching using the robot control unit 30.

[0060] In addition, the laser irradiation pattern determined by the overall control device 50 is instructed to the laser oscillator 11, and the laser oscillator 11 performs laser irradiation as specified by driving the galvanometer mirror mechanism 130 built into the laser head unit 13 based on the instruction from the overall control device 50.

[0061] The overall control device 50 receives a signal from the robot control unit 30 that the robot has arrived at a predetermined position where the laser is to be irradiated, and sends a command to start laser irradiation to the laser oscillation unit 11. The overall control device 50 also receives a signal from the laser oscillation unit 11 that laser irradiation is complete, and sends a command to the robot control unit 30 to start moving to the next irradiation position. Here, the robot movement completion signal and the laser irradiation completion signal may be exchanged directly between the robot control unit 30 and the laser oscillation unit 11 without going through the overall control device 50. In this case, it is possible to shorten the signal transmission time, but if it is desired to transmit additional information during that time, the method will be via the overall control device 50 as described above.

[0062] The overall control device 50 repeats the above control operations from the laser irradiation start position to the end position, thereby carrying out the surface preparation work for the entire processing target area of ​​the processing object 1.

[0063] That is, as shown in FIG. 3, the scanning range of the irradiation position of the pulsed laser light Lp by the two-axis galvanometer mirror mechanism 130, i.e., the size of the laser irradiation range, is a square basic area of, for example, 50 mm × 50 mm, and the entire processing target area of ​​the processing target object 1 is divided into (n-1) in the X direction and (m-1) in the Y direction, with the upper left end point set to (1, 1), the point 50 mm ahead in the X-axis direction set to (1, 2), and so on until the end point in the right direction is (1, n).

[0064] Next, let the point 50 mm downward in the Y direction be (2,n), then let the point 50 mm to the left in the X direction be (2,n-1), and so on, continuing to move left until the end point is (2,1).

[0065] The same operation is then carried out up to the final point (m, n) at the bottom right.

[0066] The method of moving the manipulator 40 is to start from the upper left point (1,1) based on the above points and move the manipulator 40 to the irradiation range AR indicated by the diagonal lines. 11 After the surface preparation work is performed by scanning the laser beam with the two-axis galvanometer mirror mechanism 130, the laser head unit 13 is moved to the next point (1, 2), and the irradiation range AR shown by dots is similarly increased. 12 The surface is scanned by a two-axis galvanometer mirror mechanism 130 to perform surface preparation work.

[0067] In addition, in the scanning by the two-axis galvanometer mirror mechanism 130, the irradiation locus RT S1 As shown in FIG. 4A, the galvanometer mirror 132X moves the light back and forth in the X-axis direction while the galvanometer mirror 132Y moves the light in the Y-axis direction, thereby turning the light around and irradiating it in a zigzag pattern. Alternatively, the light may be irradiated along the irradiation locus RT S2 As shown in FIG. 1, the X-axis direction feed and the Y-axis direction feed can be combined to irradiate in a spiral pattern.

[0068] Furthermore, the irradiation locus RT shown in FIG. S3 As shown in Fig. 4(A), the irradiation locus RT S1 In the case of irradiating in a folded manner as described above, the second and subsequent rows can be irradiated at intermediate positions between the irradiation positions of the previous row, and this can be continued up to the final bottom edge.

[0069] Here, in this surface treatment device 100, for example, a hot-rolled steel plate or the like is treated, and the steel material which is the treatment object 1 is a steel material which is supplied to a treatment process in which the objects are attached or bonded to each other by coating materials (paints and lining materials) or adhesives such as painting, bonding, lining, etc.

[0070] FIG. 5 is a schematic diagram showing the cross-sectional structure of a steel material, which is the processing object 1 to be subjected to surface treatment by this surface treatment device 100, where (A) is a schematic cross-sectional view of the steel material before surface treatment, and (B) is a schematic cross-sectional view of the steel material after surface treatment.

[0071] As shown in Fig. 5(A) on the steel material which is the processing object 1, in an unprocessed state, a two-layered oxide film 2 having a thickness of t1 and mainly composed of magnetite (Fe3O4) 2A and hematite (Fe2O3) 2B is attached to the surface of the Fe base material 1A. In the above-mentioned surface treatment device 100, the hematite (Fe2O3) 2B on the outermost surface of the processing object 1 is removed, and as shown in Fig. 5(B), a surface treatment is performed to form a single-layered structure of only an oxide film 2A having a thickness of t2 and mainly composed of highly adhesive magnetite (Fe3O4) on the surface of the Fe base material 1A.

[0072] In other words, the surface treatment method performed by this surface treatment device 100 is a surface treatment method for removing an oxide film 2 adhering to the surface of a steel material, which is a processing object 1, by irradiating it with a pulse of laser light, and includes a scraping process step for removing hematite (Fe2O3) in the surface layer of the oxide film 2, which has a two-layer structure of hematite (Fe2O3)2B and magnetite (Fe3O4)2A that constitutes the oxide film 2, by irradiating it with a pulse of laser light, as shown in Figure 6.

[0073] Specifically, the surface treatment method carried out by the surface treatment device 100 includes a laser density setting step ST1 and a scraping step ST2, as shown in a process diagram of FIG.

[0074] That is, in this surface treatment apparatus 100, the overall control device 50 controls the operation of the pulsed laser light irradiation device 10 in the laser density setting step ST1 and the scraping treatment step ST2 as follows.

[0075] First, in the laser density setting step ST1, the integrated control device 50 sets the laser density per pulse of the laser light to be irradiated from the pulsed laser light irradiating device 10 to the steel material, which is the processing object 1, in the scraping processing step ST2, to the spot diameter d of the pulsed laser light based on the laser irradiation distance. p and the moving distance of the irradiation position per pulse d m Based on this, the laser density is initially set to a value effective for removing the hematite (Fe2O3)2B on the surface of the oxide film 2.

[0076] In the laser density setting step ST1, the initial laser density is determined according to the required performance for the surface properties before and after the processing of the object, and the spot diameter d is set by defocusing the pulsed laser light to be irradiated in the cleaning processing step ST2. p can be set to an optimal value.

[0077] In the cleaning process ST2, the integrated control device 50 determines the spot diameter d of the pulsed laser light based on the laser irradiation distance in the laser density setting process ST1. p and the moving distance of the irradiation position per pulse d m The operation of the pulsed laser beam irradiation device 10 is controlled so as to irradiate a pulsed laser beam having a laser density initially set based on the above, and remove hematite (Fe2O3) 2B from the surface layer of the oxide coating 2.

[0078] Here, the integrated control device 50 controls the moving distance d of the irradiation position of the pulsed laser light per pulse in the cleaning process ST2. m is the spot diameter d p The moving speed may be within the range of ×(1 / 2 to 1).

[0079] By changing the intensity of the pulsed laser beam to remove the oxide scale, the state of the remaining scale after laser irradiation changes.

[0080] FIG. 7 is a diagram showing the irradiation state when the moving speed of the irradiation position of the pulsed laser light, i.e., the scanning speed of the laser spot LS, is changed in order to change the irradiation energy of the pulsed laser light in this surface treatment device 100. (A) shows the moving distance d m1 The spot diameter d p (B) shows the moving distance per pulse d m2 The spot diameter d p (C) shows the case where the moving speed is (1 / √2) times that of the moving distance d m3 The spot diameter d p The figure shows the case where the moving speed is 1 / 2 times faster than the normal speed.

[0081] Here, the laser spot diameter d p is the spot diameter of the laser light at the focal position obtained by the optical system of the pulsed laser light irradiation device 10 used, and in the following description, it is assumed that the shape is circular.

[0082] In addition, in FIG. 7, the movement speed in the X direction (horizontal direction) and the Y direction (vertical direction) are set to the same value, but this is not limited to this, and the X direction (horizontal direction) and the Y direction (vertical direction) may be set separately.

[0083] For example, as shown in FIG. 7A, the moving distance per pulse d m1 The spot diameter d pWhen the scraping process is performed by moving the workpiece at a speed of 1000 mm / min, scale remains in the unirradiated areas where the laser light is not irradiated, so the proportion of hematite (Fe2O3)2B removed in the scraping process ST2 is 78.5% in terms of area on the surface of the oxide coating after the scraping process.

[0084] FIG. 6B above shows a case where the hematite (Fe2O3)2B on the surface of the oxide film 2 has been completely removed, but depending on the application, it may not be necessary to remove 100% of the hematite (Fe2O3)2B.

[0085] As shown in FIG. 7B, the moving distance per pulse is d m2 The spot diameter d p By setting the moving speed to (1 / √2) times the normal speed, the laser spots LS can be overlapped to eliminate unirradiated areas, making it possible to achieve the most efficient state.

[0086] As shown in FIG. 7C, the moving distance per pulse is d m3 The spot diameter d p When the moving speed is set to 1 / 2, there are no unirradiated areas, but the overlap rate of the laser spot LS increases, and the energy input efficiency is inferior to that in the case of FIG. 7B.

[0087] According to these methods, (Fe2O3)2B can be removed from the laser irradiated area, and hematite (Fe2O3)2B remains in the area not irradiated with the laser light.

[0088] The removal rate of hematite (Fe2O3) in FIG. 7(A) is (area of ​​four circles) / (area of ​​square circumscribing four circles)=π / 4=0.785 (78.5%).

[0089] In (B) and (C) of Figure 7, the removal rate of hematite (Fe2O3) is 100% because the laser spots LS overlap.

[0090] Here, in order to evaluate the performance of the laser scraper with different laser intensities (energy densities), paint was applied to each test piece, which was then dried and cured, and the adhesion strength was confirmed by a tensile test (pull-off test). The results are shown in Figure 8.

[0091] In Figure 8, (o) shows the steel plate surface as is (black surface) without laser irradiation, (a) shows the case where the steel plate was irradiated with the laser irradiation method in Figure 7 (A) above, and (c) shows the case where the steel plate was irradiated with the laser irradiation method in Figure 7 (C) above. Two test pieces were prepared for each test, and the average value of the results was normalized with the untreated black surface being set as '1.0'.

[0092] These results show that laser scraping improves the adhesion of the coating and improves its performance as a surface treatment.

[0093] In addition, the laser intensity changes when the scanning speed of the laser light is changed, but the moving distance per pulse d m1 The spot diameter d p The lower limit is the moving speed of 1000 mm / s, and the spot diameter d p Distance traveled d is 1 / 2 of m3 It is necessary to set appropriate laser irradiation conditions (scanning speed) based on the required quality performance and processing efficiency of the surface treatment, with the upper limit being the movement of only one laser beam.

[0094] Under the above conditions, the spot diameter d p Distance traveled d is (1 / √2) times the distance traveled m2 The method of moving the laser beam by only one second is considered to be a desirable method in terms of performance and efficiency, since no part is left unirradiated by the laser beam and the overlap rate can be made small.

[0095] From these test results, it was found that the performance as a base treatment can be obtained by setting the proportion of hematite (Fe2O3)2B removed in the scraping treatment step ST2 to 78.5% or more in terms of area ratio on the surface of the oxide film after scraping treatment.

[0096] In this way, by carrying out the surface treatment method consisting of the laser density setting process ST1 and the scraping process ST2 using the surface treatment device 100 and removing a certain amount (78.5% or more) of the less adhesive hematite (Fe2O3)2B, the surface of the steel material (process object 1) after laser scraping will be dominated by highly adhesive magnetite (Fe3O4)2A, improving the adhesion of the paint.

[0097] When higher adhesion is required, the scraping work can be carried out using a laser irradiation method, which has a high removal rate of hematite (Fe2O3)2B.

[0098] In addition, in addition to using a robot, the laser irradiation can also be performed by a person holding the laser head by hand, but in order to ensure uniformity of the laser irradiation, it is preferable to use a mechanical device such as a robot. [Explanation of symbols]

[0099] 1 Processing object, 1A Base material (Fe), 2 Oxide coating, 2A Magnetite (Fe3O4), 2B Hematite (Fe2O3), 10 Laser irradiation device, 11 Laser oscillation section, 12 Optical fiber, 13 Laser head section, 20 Manipulator, 21 Robot arm, 21A Tip section, 30 Robot control section, 40 Manipulator robot, 50 Overall control device, 100 Substrate processing device, 130 Galvano mirror mechanism, 131X, 131Y Motor, 132X, 132Y Mirror, 133 Telecentric f-θ lens

Claims

1. The hematite (Fe) attached to the surface of the steel material to be treated by pulsed irradiation of laser light 2 O 3 ) and magnetite (Fe 3 O 4 ) a surface preparation treatment device for removing a part of a two-layer oxide film, a pulsed laser light irradiating device including an irradiation distance variable setting means for variably setting a laser irradiation distance for irradiating a processing target area of ​​the steel material, which is the processing target, with a pulsed laser light, and a scanning means for moving an irradiation position of the pulsed laser light within a working area including the processing target area, and for irradiating the processing target area of ​​the steel material, which is the processing target, with the pulsed laser light; a control device for controlling the operation of the pulsed laser light irradiation device; Equipped with The control device controls the laser density per pulse of the pulsed laser light irradiated by the pulsed laser light irradiating device to be equal to or smaller than the spot diameter d of the pulsed laser light based on the laser irradiation distance. p and the moving distance d of the irradiation position per pulse m Based on this, the hematite (Fe 2 O 3 The laser density is initially set to an effective value for removing hematite (Fe) from the surface layer of the oxide film, and the irradiation position of the pulsed laser light is moved by the scanning means within a working area including the area to be treated, and the pulsed laser light having the initially set laser density is irradiated to remove hematite (Fe) from the surface layer of the oxide film. 2 O 3 ) by controlling the operation of the pulsed laser light irradiation device so as to perform a cleaning process to remove the A surface treatment device comprising:

2. The control device is configured to detect hematite (Fe 2 O 3 2. The surface treatment apparatus according to claim 1, wherein the operation of the pulsed laser light irradiation apparatus is controlled so that the ratio of the surface area of ​​the oxide film after the scraping treatment is 78.5% or more.

3. The control device detects a moving distance d of the irradiation position of the pulsed laser light per pulse by the scanning means. m is the spot diameter d p 2. The surface treatment apparatus according to claim 1, wherein the operation of the pulsed laser light irradiation device is controlled so as to move the pulsed laser light irradiation device at a moving speed within a range of x (1 / 2 to 1).

4. The control device defocuses the pulsed laser light irradiated onto the processing target area of ​​the steel material, which is the processing target, by the irradiation distance variable setting means, thereby setting a spot diameter d p 4. The surface treatment apparatus according to claim 1, wherein the thickness of the surface is set to an optimum value.

Citation Information

Patent Citations

  • Production of hot rolled steel plate excellent in surface characteristic and acid pickling property by continuous hot rolling process

    JP1997235622A

  • Method for removing coating by laser and laser processor

    JP1998309516A

  • Method of controlling laser beam decoration on resin molding and device therfor

    JP2001334374A

  • Oxide film thickness measuring method and oxide film thickness measuring device

    JP2009186333A

  • Laser beam machining apparatus and laser beam machining method

    JP2011177781A