Element substrate, liquid ejection head, and method for manufacturing element substrate
The element substrate enhances temperature detection sensitivity by integrating a temperature sensing element via between a heat generating resistor and insulating layers, addressing the issue of high connection resistance in existing designs.
Patent Information
- Application Number
- JP2020104702
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-07-30
- Filing Date
- 2020-06-17
- Publication Date
- 2024-09-17
- Estimated Expiration
- 2040-06-17
AI Technical Summary
Existing temperature sensing elements in liquid ejection heads suffer from reduced sensitivity due to high connection resistance between wiring and vias, leading to inadequate detection of resistance value changes with temperature variations.
The element substrate is designed with a temperature sensing element via formed between a heat generating resistor element and a first insulating layer, and a second insulating layer that electrically insulates the temperature sensing element, reducing connection resistance and enhancing sensitivity.
This configuration improves the sensitivity of temperature detection by minimizing the influence of connection resistance and allowing precise detection of resistance value changes, thereby optimizing the discharge state of the liquid ejection process.
Smart Images

Figure 0007551348000005 
Figure 0007551348000004 
Figure 0007551348000006
Abstract
Description
[Technical field]
[0001] The present invention relates to an element substrate having a heat generating resistor element, a liquid ejection head for ejecting liquid, and a method for manufacturing the element substrate. [Background technology]
[0002] Liquid ejection heads used in liquid ejection printers include thermal ejection type and piezoelectric element type liquid ejection heads. Thermal ejection type liquid ejection heads use thermal energy generated by a heat generating resistor element to eject droplets of ink or the like toward recording paper to form images, etc. Thermal ejection type liquid ejection heads are suitable for high density recording because they can generate relatively large amounts of thermal energy even with a small area of heat generating resistor element. Liquid ejection heads have an element substrate equipped with a heat generating resistor element.
[0003] In recent years, liquid ejection heads have been provided with a temperature detection element (temperature sensor) on the element substrate to detect temperature. This temperature detection element is used to obtain temperature information and control the heating resistor element. Patent Document 1 describes a configuration in which a temperature detection element is provided that is configured by connecting two layers of wiring and vias that connect them in series. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2018-24126 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, in the configuration described in Patent Document 1, in a temperature detection element that detects a change in temperature by a change in the electrical resistance value of the constituent materials, the resistance is dominated by the connection resistance between the wiring and the via, so there is a risk that sufficient sensitivity cannot be obtained. For example, the ratio of the connection resistance to the resistance of the wiring and via materials is large, about 100 to 10,000 times, making it difficult to detect changes in the resistance value of the temperature detection element that accompany temperature changes. Factors that reduce the detection sensitivity include a large factor of resistance change other than the temperature resistance coefficient of the wiring and via materials, a large variation between each bit, and a large change over time.
[0006] SUMMARY OF THE PRESENT EMBODIMENTS In view of the above, an object of the present invention is to provide an element substrate capable of improving the sensitivity of temperature detection by a temperature detection element. [Means for solving the problem]
[0007] The element substrate of the present invention is characterized in having a laminated structure in which a heating resistance element and a first insulating layer in which a temperature detection element consisting of a via is formed, and a second insulating layer provided between the heating resistance element and the temperature detection element and electrically insulates the heating resistance element and the temperature detection element. Effect of the Invention
[0008] According to the present invention, it is possible to provide an element substrate capable of improving the sensitivity of temperature detection by a temperature detection element. [Brief description of the drawings]
[0009] [Figure 1] 3A and 3B are a plan view and a cross-sectional view each showing a schematic view of an element substrate. [Diagram 2] 5A to 5C are cross-sectional views each showing a schematic diagram of a method for manufacturing an element substrate. [Diagram 3] 3A and 3B are a plan view and a cross-sectional view each showing a schematic view of an element substrate. [Figure 4] 3A and 3B are a plan view and a cross-sectional view each showing a schematic view of an element substrate. [Diagram 5] 3A and 3B are a plan view and a cross-sectional view each showing a schematic view of an element substrate. [Figure 6] FIG. 2 is a plan view illustrating a liquid ejection head. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the following description and drawings, multiple drawings can be mutually referenced. In addition, common reference numerals are used for identical or similar components, and descriptions of components with common reference numerals will be omitted as appropriate.
[0011] First Embodiment The first embodiment will be described with reference to FIG. 1. FIG. 1(a) is a schematic plan view showing a part of an element substrate 10. FIG. 1(a) shows one of a plurality of heat generating resistor elements 112 provided on the element substrate 10, including the periphery thereof. Note that FIG. 1(a) shows some layers in perspective in order to show the positional relationship of each layer of the element substrate 10. Plan views of the element substrate 10 of the following embodiments are also shown in the same manner as FIG. 1(a). FIG. 1(b) is a schematic cross-sectional view of the element substrate 10 taken along line A-A' in FIG. 1(a). FIG. 1(c) is a schematic cross-sectional view of the element substrate 10 taken along line B-B' in FIG. 1(a). FIG. 6 is a schematic plan view showing a liquid ejection head 200 including the element substrate 10.
[0012] The liquid ejection head 200 has an element substrate 10 equipped with a heating resistor element 112, and an ejection port forming member 601 in which ejection ports 600 are formed to eject liquid using heat generated by the heating resistor element 112. The ejection port forming member 601 has a plurality of ejection port arrays 602 in which a plurality of ejection ports 600 are arranged. The element substrate 10 has heating resistor elements 112 and temperature detection elements 110 fabricated and arranged corresponding to each ejection port 600. Electrode terminals 115 for connecting to external wiring are provided on the periphery of the element substrate 10.
[0013] Next, the configuration of the element substrate 10 will be described. In this specification, the element substrate 10 has a layered structure in which a plurality of layers are stacked, and in a cross-sectional view such as Fig. 1(b), the layering direction in the element substrate 10 coincides with the up-down direction in the figure. For convenience, the element substrate 10 will be described with the substrate 100 side as the bottom and the liquid ejection side as the top, but this does not limit the up-down position of the element substrate 10.
[0014] The element substrate 10 includes a substrate 100 made of, for example, single crystal silicon, and an insulating layer 101 is disposed on the substrate 100. The insulating layer 101 is formed of, for example, an inorganic material such as silicon oxide, has electrical insulation properties, and electrically separates each wiring. The insulating layer 101 is configured by laminating a plurality of insulating layers 101a, 101b, and 101c, and in this specification, each layer may be individually shown or may be collectively shown as the insulating layer 101. For example, connection wirings 102, 104, and 106 and signal wirings 103, 105, and 107 are disposed on the substrate 100, forming a multilayer wiring configuration. This makes it possible to improve the degree of integration without increasing the chip area even with a complex circuit configuration. The signal wirings 103, 105, and 107 are formed of, for example, a metal material mainly composed of aluminum or copper. The connection wirings 102, 104, and 106 are formed of, for example, a metal material mainly composed of tungsten or copper.
[0015] The power supply wiring 108 is disposed in the insulating layer 101. The power supply wiring 108 is patterned and disposed as 108a, 108b, 108c, and 108d. The power supply wiring 108 is formed of a metal material containing aluminum or copper as a main component, for example.
[0016] A connection wiring 109 and a temperature detection element 110 are disposed on the power supply wiring 108. The connection wiring 109 and the temperature detection element 110 are electrically connected to the power supply wiring 108. The connection wiring 109 and the temperature detection element 110 may be made of the same material, or may be formed at the same time. The connection wiring 109 and the temperature detection element 110 are formed of a metal material mainly composed of, for example, tungsten, copper, or aluminum. As will be described later, the connection wiring 109 and the temperature detection element 110 are vias formed in the insulating layer 101b of the insulating layer 101. The first via, which is the connection wiring 109, and the second via, which is the temperature detection element, are formed at the same position in the stacking direction of the layers. A connection wiring 111 is disposed on the connection wiring 109. The connection wiring 111 is formed of a metal material mainly composed of, for example, aluminum or copper.
[0017] The discharge state of the liquid can be detected by detecting the temperature using the temperature detection element 110. More specifically, the temperature change after discharge differs depending on whether the liquid is being discharged normally or not, and this temperature change is detected using the temperature detection element 110. Depending on the detection result, the heating resistor element 112 and recovery means provided in the printer can be controlled.
[0018] The top surface of the insulating layer 101 is planarized. The planarization process is performed by, for example, CMP (Chemical Mechanical Polishing). The planarization process may be performed during or after each process of forming the connection wiring, the signal wiring, the power supply wiring, and the temperature detection element.
[0019] A heating resistor element 112 is disposed on the top surface of the insulating layer 101. The heating resistor element 112 is electrically connected to the power supply wirings 108a and 108b via connection wirings 111 and 109, and functions as a resistive element between the power supply wirings 108a and 108b. The heating resistor element 112 is formed of a resistive material such as tantalum silicon nitride or tungsten silicon nitride.
[0020] A protective layer 113 is disposed on the heating resistor element 112. The protective layer 113 is formed of an inorganic material containing, for example, silicon nitride, and has electrical insulation properties. An anti-cavitation layer 114 is disposed on the protective layer 113. The anti-cavitation layer 114 is formed of a single layer or multilayer of a high-melting point metal having excellent heat resistance, containing, for example, tantalum or iridium. The anti-cavitation layer 114 is formed to a thickness of, for example, 30 to 250 nm. The protective layer 113 is formed to a thickness of, for example, 50 to 200 nm, and insulates the heating resistor element 112 from the anti-cavitation layer 114.
[0021] The signal wirings 103, 105, and 107 are formed with a thickness of, for example, 100 to 400 nm. The power supply wiring 108, including the power supply wirings 108a and 108b that supply power for driving the heat generating resistor element 112, is formed with a thickness of, for example, 500 to 2000 nm. The thickness of the connection wiring is determined by the thickness of the wiring below it. That is, the thickness of each wiring determines the lower limit of the thickness of the insulating layer 101 provided on each wiring, and therefore the lower limit of the thickness of the connection wiring penetrating the insulating layer 101 is also determined by the thickness of the wiring below it. Therefore, the connection wirings 102, 104, and 106 provided on the signal wirings 103 and 105 are formed with a thickness of, for example, 100 to 400 nm. The connection wiring 109 and the temperature detection element 110 provided on the power supply wiring 108 are formed with a thickness of, for example, 500 to 2000 nm.
[0022] The temperature detection element 110 is electrically connected to the power supply wirings 108c and 108d, and functions as a temperature detection sensor between the power supply wirings 108c and 108d. As described above, the element substrate 10 is provided with a plurality of segments in which the temperature detection element 110 is provided under the heat generating resistor element 112 via the insulating layer 101 (101c).
[0023] Since the temperature detection element 110 detects the discharge state of the liquid due to the heat generated by the heating resistor element 112, it is preferable that the heating resistor element 112 and the temperature detection element 110 are provided so as to at least partially overlap each other when the element substrate 10 is viewed in a plan view (FIG. 1(a)). In addition, the sensitivity of the temperature detection sensor can be increased by increasing the resistance value of the temperature detection element 110 in the area overlapping with the heating resistor element 112. For this reason, it is preferable that the temperature detection element 110 is formed in a meandering shape in which it is folded back multiple times, and its resistance value is increased. In addition, as described later, this embodiment uses the temperature detection element 110 formed only of vias that are not connected to conductors such as other wiring, so there is no need to provide a margin for connection with the wiring, and the width of the temperature detection element can be narrowed and its resistance value can be increased.
[0024] Figures 2(a) to (g) are schematic cross-sectional views showing a method for manufacturing the element substrate 10 shown in Figure 1. Hereinafter, the method for manufacturing the element substrate 10 will be described in the order of steps with reference to Figures 2(a) to (g).
[0025] First, as shown in Fig. 2(a), connection wirings 102, 104, 106, signal wirings 103, 105, 107, insulating layer 101a, and power supply wirings 108 (108a to 108d) are formed on substrate 100 made of single crystal silicon. These wirings and layers can be formed by using general semiconductor manufacturing techniques such as CVD (Chemical Vapor Deposition), photolithography, etching, sputtering, plating, and CMP. Power supply wirings 108 are formed by forming a film of a metal material constituting power supply wirings 108 on the surface of insulating layer 101a, forming a resist pattern thereon by photolithography, and partially removing the resist pattern by etching.
[0026] Thereafter, as shown in FIG. 2(b), a silicon oxide film is formed by CVD, and the surface is planarized by CMP to form an insulating layer 101b (first insulating layer).
[0027] 2(c), the photoresist is patterned and the insulating layer 101b is etched to form a hole 201. This hole 201 is a through-hole that penetrates the insulating layer 101b so as to expose the surface of the power supply wiring 108 from the insulating layer 101b, or a recess formed in the surface of the insulating layer 101b. Figures 2(a) to (c) also show steps of preparing a substrate 100 including an insulating layer 101 in which at least one of a recess and a through-hole is formed.
[0028] 2(d), a tungsten film is formed by CVD so as to fill the holes 201, thereby forming a film 202. Alternatively, an aluminum film is formed by CVD so as to fill the holes 201, thereby forming a film 202. Alternatively, copper is plated so as to fill the holes 201, thereby forming a film 202. If necessary, a barrier metal or a seed layer may be formed by sputtering before filling the holes.
[0029] Thereafter, as shown in FIG. 2(e), the connection wiring 109 and the temperature detection element 110 are formed by planarizing the surface while removing excess tungsten, aluminum, or copper by CMP. In this manner, the temperature detection element 110 is formed only with wiring, i.e., vias, connecting the interlayer wiring, which is formed by forming holes or recesses in the insulating layer, filling the interior of the holes or recesses with a metal material, and planarizing the surface while removing excess metal material on the surface. The temperature detection element 110 thus formed has a flat surface on its surface and on the surface of the insulating layer 101b. The connection wiring 109 is also a via formed as described above, similar to the temperature detection element 110. Unless otherwise described in this specification, the connection wiring other than the connection wiring 109 can be formed in the same configuration using the same manufacturing method as the connection wiring 109.
[0030] 2(f), a silicon oxide film is formed by CVD to form an insulating layer 101c (second insulating layer) that covers the planarized surface of the insulating layer 101b and the temperature detection element 110. This insulating layer 101c has a function of electrically insulating the temperature detection element 110 from the heating resistor element 112 to be formed later. Because the surface is planarized in the state of FIG. 2(e), the surface of the insulating layer 101c may be planarized by CMP, although this is not essential.
[0031] Thereafter, as shown in FIG. 2(g), holes are made in the insulating layer 101c, a film of tungsten is formed by CVD so as to fill the holes, and the excess tungsten is removed by CMP while being planarized, thereby forming the connection wiring 111.
[0032] Thereafter, a film of tantalum silicon nitride is formed on the insulating layer 101c by sputtering, and is patterned to form the heat generating resistor element 112. Furthermore, a film of silicon nitride is formed by CVD to form the protective layer 113. Furthermore, a film of tantalum is formed by sputtering, and is patterned to form the cavitation-resistant layer 114. In this manner, the element substrate 10 shown in FIG. 1 is formed.
[0033] As described above, in this embodiment, the temperature detection element 110 is provided under the heating resistor element 112 via the insulating layer 101, and the temperature detection element 110 is formed by filling a metal material inside a recess or a through hole provided in the insulating layer 101 (insulating layer 101b) and flattening the surface. Therefore, after the temperature detection element 110 is formed, its surface (the surface on the heating resistor element side) is flat without any steps. This makes it possible to reduce the thickness T (FIG. 1(b)) of the insulating layer 101c between the heating resistor element 112 and the temperature detection element 110. The temperature detection element 110 can improve the detection sensitivity of the temperature of the heat application part used to detect the discharge state of the liquid by reducing the distance to the heat application part that directly transfers the heat generated by the heating resistor element 112 to the liquid. In this embodiment, the surface of the cavitation-resistant layer 114 that contacts the liquid (the surface opposite to the surface facing the heating resistor element 112) functions as the heat application part. Therefore, by reducing the thickness T of the insulating layer, the distance to the heat acting part is shortened, and it is possible to improve the sensitivity of the temperature detection element 110. Therefore, according to this embodiment, it is possible to provide an element substrate 10 that can improve the sensitivity of temperature detection by the temperature detection element 110.
[0034] Furthermore, the temperature detection element 110 configured with the vias does not have a connection portion with other wiring or conductors such as vias at least in the region overlapping with the heating resistor element 112. In other words, the temperature detection element 110 is configured as a single via at least in the region overlapping with the heating resistor element 112. This makes it easier to detect a change in the resistance value of the constituent material of the temperature detection element 110 accompanying a change in temperature without being affected by the connection resistance between the wiring and the via. In other words, it is possible to make the change in the resistance value of the temperature detection element 110 with respect to a change in temperature approximately equal. This makes it possible to provide an element substrate 10 capable of improving the sensitivity of temperature detection by the temperature detection element 110.
[0035] <Second embodiment> The second embodiment will be described with reference to Fig. 3. Fig. 3(a) is a schematic plan view showing a part of the element substrate 10. Fig. 3(b) is a schematic cross-sectional view of the element substrate 10 taken along line A-A' in Fig. 3(a). In the second embodiment, an example of a configuration in which the sensitivity is further increased by reducing the thickness of the temperature detection element will be described.
[0036] As in the first embodiment, a substrate 100, an insulating layer 101, connection wirings 102, 104, 106, and 111, signal wirings 103, 105, and 107, power supply wiring 108, a heat generating resistor element 112, a protective layer 113, and an anti-cavitation layer 114 are arranged.
[0037] A connection wiring 309 is disposed on the power supply wiring 108. The connection wiring 309 is electrically connected to the power supply wiring 108. The connection wiring 309 is formed of a metal material mainly composed of, for example, tungsten or copper. A temperature detection element 310 is disposed on the connection wiring 309. The temperature detection element 310 is electrically connected to the power supply wiring 108 through the connection wiring 309, which is a via different from the via constituting the temperature detection element 310. The temperature detection element 310 is formed of a metal material mainly composed of, for example, tungsten, copper, or aluminum. The connection wiring 309 and the temperature detection element 310 are formed in different processes. Note that the connection wiring 309 and the temperature detection element 310 may be formed using a partly common process as long as the process for defining at least each of the thicknesses is performed separately. Therefore, the thickness of the temperature detection element 310 can be set to be thin without depending on the thickness of the power supply wiring 108. Here, since a high current flows through the power supply wiring 108 (108a, 108b) that supplies power for driving the heat generating resistor element 112, the thickness of the power supply wiring 108 is, for example, 500 to 2000 nm in order to reduce the resistance and to keep the current density below a predetermined level. In order to reliably cover the power supply wiring 108, the insulating layer 101b covering the power supply wiring 108 is also required to have a sufficient thickness. The temperature detection element 110 of the first embodiment has a thickness equivalent to the thickness of the portion of the insulating layer 101b located on the power supply wiring 108. On the other hand, the temperature detection element 310 of the present embodiment can be made thinner than the thickness of the portion of the insulating layer 101b located on the power supply wiring 108. That is, the temperature detection element 310 of the present embodiment can be made thinner than the temperature detection element 110 of the first embodiment. The temperature detection element 310 can be formed using the manufacturing method described in the first embodiment.
[0038] As described above, according to the element substrate 10 of the second embodiment, the thickness of the temperature detection element 310 can be reduced and the resistance value thereof can be increased, thereby providing an element substrate 10 capable of further improving the sensitivity of temperature detection.
[0039] <Third embodiment> The third embodiment will be described with reference to Fig. 4. Fig. 4(a) is a schematic plan view showing a part of the element substrate 10. Fig. 4(b) is a schematic cross-sectional view of the element substrate 10 taken along line A-A' in Fig. 4(a). In the third embodiment, an example different from the second embodiment will be described, in which the thickness of the temperature detection element is reduced to increase the sensitivity.
[0040] As in the first embodiment, a substrate 100, an insulating layer 101, connection wires 102 and 104, a signal wire 103, a heat generating resistor element 112, a protective layer 113, and an anti-cavitation layer 114 are arranged.
[0041] A power supply wiring 408 is disposed on the connection wiring 104. On the power supply wiring 408, connection wirings 404, 406, and 411 and signal wirings 405 and 407 are disposed.
[0042] The temperature detection element 410 is disposed in the same layer as the connection wiring 406 between the signal wirings 405 and 407. The signal wirings 405 and 407 are formed to be thinner than the power supply wiring 408 that supplies power to the heating resistor element 112. For example, the signal wirings 405 and 407 are formed to a thickness of 100 to 400 nm, and the power supply wiring 408 is formed to a thickness of 500 to 2000 nm. The thickness of the connection wiring and the temperature detection element formed as a via is determined by the thickness of the wiring below. That is, since the connection wiring and the temperature detection element are vias formed in an insulating layer that covers the wiring below them, by reducing the thickness of the wiring below them, the thickness of the insulating layer that covers them can also be reduced, and the thickness of the via formed in this insulating layer can also be reduced. Therefore, by forming the temperature detection element 410 on the signal wiring 405 that is thinner than the power supply wiring 408, the thickness of the temperature detection element 410 can be reduced. In this embodiment, when the thickness of the signal wirings 405, 407 is 100 to 400 nm, the thickness of the temperature detection element 410 can be 100 to 400 nm. Since the thickness of the temperature detection element affects the detection sensitivity, a thinner thickness is preferable, but the thickness of the temperature detection element is preferably 100 to 2000 nm, and more preferably 100 to 400 nm.
[0043] In FIG. 4(b), the temperature detection element 410 performs signal processing by connecting the temperature detection element 410 to a signal wiring 405.
[0044] Fig. 4(c) is a schematic cross-sectional view of the element substrate taken along line A-A' in Fig. 4(a), and is of a different form from Fig. 4(b). In Fig. 4(c), signal processing is performed by connecting the temperature detection element 410 to a signal wiring 407 provided on the heating resistor element 112 side of the temperature detection element 410. The temperature detection element 410 in Figs. 4(b) and 4(c) can be formed by the manufacturing method described in the first embodiment.
[0045] In addition, in the third embodiment, the temperature detection element 410 is formed in the same process as the process of forming the connection wiring 406 for electrically connecting the heating resistance element 112 and the power supply wiring 408, so there is no need for a dedicated mask for forming the temperature detection element 410. Therefore, the number of processes can be reduced by one mask compared to the first embodiment, and the number of processes can be reduced by two masks compared to the second embodiment.
[0046] As described above, according to the element substrate 10 of this embodiment, the resistance value of the temperature detection element 410 can be increased by reducing the thickness thereof while reducing the load on the manufacturing process, and therefore an element substrate 10 can be provided that can further improve the sensitivity of temperature detection.
[0047] <Fourth embodiment> The fourth embodiment will be described with reference to Fig. 5. Fig. 5(a) is a schematic plan view showing a part of the element substrate 10. Fig. 5(b) is a schematic cross-sectional view of the element substrate taken along line A-A' in Fig. 5(a). In the fourth embodiment, an example of a configuration in which the number of wiring layers is minimized will be described.
[0048] As in the first embodiment, a substrate 100, an insulating layer 101, a protective layer 113, and an anti-cavitation layer 114 are arranged.
[0049] A temperature detection element 510 is disposed in the insulating layer 101. The temperature detection element 510 can be formed by the manufacturing method described in the first embodiment. A heating resistor element 512 is disposed on the insulating layer 101. Power supply wiring 508 (508a, 508b) is disposed on the heating resistor element 512. The heating resistor element 512 and the power supply wiring 508 can also be upside down. A connection wiring 511 is disposed on the temperature detection element 510. The temperature detection element 510 is electrically connected to the power supply wiring 508 (508c, 508d) via the connection wiring 511 and a connection wiring 513 formed in the same layer as the heating resistor element 512 using the same material in the same process.
[0050] As described above, according to the element substrate 10 of this embodiment, it is possible to provide an element substrate 10 that can improve the sensitivity of temperature detection by the temperature detection elements 510 while further reducing the load on the manufacturing process. [Explanation of symbols]
[0051] 10 Element substrate 101 Insulating layer 110 Temperature detection element 112 Heating resistor element
Claims
1. A heating resistor element; a first insulating layer having a temperature detection element formed of a via; a second insulating layer provided between the heating resistor element and the temperature detection element to electrically insulate the heating resistor element from the temperature detection element; 1. An element substrate having a laminated structure in which:
2. The element substrate according to claim 1 , wherein the heating resistor element and the temperature detection element at least partially overlap each other when the element substrate is viewed from above.
3. The element substrate according to claim 2 , wherein the temperature detection element has no connection portion with a conductor other than the via in an area overlapping the heat generation resistor element.
4. 4. The element substrate according to claim 1, wherein the via is configured by embedding a metal material inside at least one of a recess provided in the first insulating layer and a through hole penetrating the first insulating layer.
5. The element substrate according to claim 1 , wherein a surface of the temperature detection element facing the second insulating layer and a surface of the first insulating layer facing the second insulating layer are configured as flat surfaces.
6. The element substrate according to claim 1 , further comprising: a wiring electrically connected to the temperature detection element; and a via hole, separate from the temperature detection element, that connects the temperature detection element to the wiring.
7. The element substrate according to claim 1 , wherein the vias are made of a material mainly composed of any one of tungsten, aluminum, and copper.
8. 8. The element substrate according to claim 1, wherein the temperature detection element has a thickness of 100 to 2000 nm.
9. A liquid ejection head comprising the element substrate according to claim 1 , the liquid ejection head ejecting liquid by utilizing heat generated by the heating resistor element.
10. preparing a substrate including a first insulating layer having at least one of a recess and a through hole formed therein; a step of filling at least one of the recess and the through hole with a metal material, planarizing surfaces of the first insulating layer and the metal material, and forming a temperature detection element made of the metal material; forming a second insulating layer covering a surface of the first insulating layer and the temperature detection element; forming a heating resistor element so as to be electrically insulated from the temperature detection element via the second insulating layer; A method for manufacturing an element substrate having the above structure.
11. The method for manufacturing an element substrate according to claim 10 , wherein the heat generating resistor element and the temperature detecting element are formed so that, when the element substrate is viewed in a plan view, the heat generating resistor element and the temperature detecting element at least partially overlap each other.
12. 12. The method for manufacturing an element substrate according to claim 10, wherein in the step of forming the temperature detection element, a via made of the metal material and electrically connected to the heating resistor element is formed.
13. 13. The method for manufacturing an element substrate according to claim 10, wherein in the step of forming the temperature detection element, a material containing any one of tungsten, aluminum, and copper as a main component is used as the metal material.
14. 14. The method for manufacturing an element substrate according to claim 10, wherein in the step of forming the temperature detection element, the temperature detection element has a thickness of 100 to 2000 nm.
Citation Information
Patent Citations
Recording head and recording apparatus using the recording head
JP2008023987A
Element substrate, recording head, and recording apparatus
JP2018024126A
Element substrate, liquid discharge head, and recording device
JP2019001172A
Element substrate, recording head, recording device, and manufacturing method for element substrate
JP2019072999A
Element substrate, manufacturing method thereof, printhead, and printing apparatus
US10493774B2