A three-axis MEMS capacitive acceleration sensor and a manufacturing method thereof

By using a combination of comb-toothed dynamic electrode, fixed electrode, Z-type structure and low-resistance SOI silicon wafer in MEMS capacitive acceleration sensor, the problems of low sensor sensitivity and large temperature drift are solved, and high sensitivity, stability and Acceleration sensors with a large measurement range reduce costs and noise.

CN113176423BActive Publication Date: 2024-11-08THE 54TH RESEARCH INSTITUTE OF CHINA ELECTRONICS TECHNOLOGY GROUP CORPORATION
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202110578087.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-05-26
Publication Date
2024-11-08
Estimated Expiration
2041-05-26

AI Technical Summary

Technical Problem

The existing MEMS capacitive acceleration sensors have problems such as low sensitivity, low signal-to-noise ratio, high temperature drift and high material difficulty in terms of high temperature harsh environment capabilities. At the same time, the sensor perceives a small acceleration range, poor stability and low effective area utilization.

Method used

Three-axis MEMS capacitive acceleration sensor, including upper, middle and lower structures, the mass block is fixed through cantilever group, comb-toothed dynamic electrode and fixed electrode are set, the Z-type structure is used to increase the capacitance change, and low-resistance SOI silicon wafer is used. Bonding with silicon and silicon, increases integration and sensitivity, and improves reliability through limiting frames and anti-collision bumps.

Benefits of technology

It improves the sensitivity, reliability and integration of the sensor, reduces the temperature impact, expands the measurement range, enhances the capacitance variation, reduces costs and improves the stability of noise performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113176423B_ABST
    Figure CN113176423B_ABST
Patent Text Reader

Abstract

The present invention discloses a three-axis MEMS capacitive acceleration sensor and a manufacturing method thereof, belonging to the technical field of micro-electromechanical systems. It comprises an upper structure for detecting acceleration in the x direction, a middle structure for detecting acceleration in the z direction, and a lower structure for detecting acceleration in the y direction; the upper structure and the lower structure both constitute a comb-tooth type multiplication capacitance acceleration sensor, which is respectively composed of a moving electrode and a fixed electrode; the middle structure constitutes a sandwich-type differential capacitance acceleration sensor, which includes an upper plate, a lower plate, and a mass block. The present invention has the advantages of large capacitance facing area, large range, high sensitivity, high reliability, high integration, low cost, low noise, stable performance, etc.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of micro-electromechanical systems, and in particular to a three-axis MEMS capacitive acceleration sensor and a manufacturing method thereof. Background Art

[0002] MEMS (Micro-Electro-Mechanical System) accelerometer is an important inertial device that can convert the physical signal of external acceleration into an electrical signal that is easy to measure. It is widely used in aviation, aerospace, automobile and other fields. According to the detection principle, MEMS accelerometers can be divided into piezoresistive, piezoelectric and capacitive types.

[0003] A capacitive accelerometer is a sensor that converts the measured acceleration signal into a change in the capacitance of a capacitor. There are usually two ways to achieve this function: variable gap type and variable area type. The movable mass block of the sensor constitutes a movable electrode of the variable capacitor. When the mass block is displaced by acceleration, the gap or facing area of ​​the parallel plate capacitor composed of the movable electrode and the fixed electrode changes, causing the capacitance of the parallel plate capacitor to change. This change is detected by the peripheral circuit to calculate the magnitude of the acceleration.

[0004] In the patent with application number CN201811616953.5, the accelerometer is made of all-silicon carbide material and consists of a lower silicon carbide base layer, an intermediate connecting layer and an upper silicon carbide structural frame. The upper silicon carbide structural frame has five groups of centrally symmetrical array-type four-beam mass island structures inside. The piezoresistive strips on the beams are used for vibration sensing to obtain acceleration in three-axis directions.

[0005] This structure has improved its ability to withstand high temperature and harsh environments, but it also has the following problems: the deformation produced by the sensitive piezoresistive strip is limited, and the sensor sensitivity is low; the thermal mechanical noise generated by the mechanical structure and piezoresistance is large, and the sensor signal-to-noise ratio is low; the piezoresistive material is greatly affected by temperature, which leads to temperature drift of the sensor; the use of unconventional materials such as silicon carbide brings certain difficulties to the production of the sensor.

[0006] In the patent application number CN201921626254.9, a three-axis MEMS capacitive acceleration sensor is proposed. Among them, two orthogonally distributed comb-tooth micro-accelerometers are set on the plane detection layer to sense the acceleration in the horizontal direction, and a pendulum-type micro-accelerometer is set on the off-plane monitoring layer to sense the acceleration in the vertical direction. A base layer is set between the plane detection layer and the off-plane detection layer, and a substrate layer is set below the off-plane detection layer.

[0007] This structure can achieve high sensitivity, but it also has the following problems: the sensor has a small acceleration sensing range; the pendulum accelerometer has poor stability and reliability, and the sensor's horizontal acceleration sensing ability is reduced; the two orthogonal comb-tooth accelerometers in the plane have low utilization of the sensor's effective area. Summary of the invention

[0008] In view of this, the present invention provides a three-axis MEMS capacitive acceleration sensor and a manufacturing method thereof. The sensor has the advantages of large capacitance facing area, large measuring range, high sensitivity, high reliability, high integration, low cost, low noise, stable performance, etc.

[0009] In order to achieve the above object, the technical solution adopted by the present invention is:

[0010] A three-axis MEMS capacitive acceleration sensor, comprising an upper structure for detecting acceleration in the x direction, a middle structure for detecting acceleration in the z direction, and a lower structure for detecting acceleration in the y direction;

[0011] The middle-level structure comprises an upper plate, a fixed frame and a lower plate stacked in sequence; a mass block is arranged in the fixed frame, and the mass block is fixed at the center of the fixed frame through a cantilever group; a limit convex frame and an anti-collision convex point are arranged on the lower surface of the upper plate and the upper surface of the lower plate for constraining the movement of the mass block; there are gaps between the upper plate and the mass block and between the mass block and the lower plate;

[0012] The upper structure is located on the upper surface of the upper plate, and includes n x-direction moving electrodes and n+1 x-direction fixed electrodes arranged at intervals, wherein n≥1; the x-direction fixed electrode is fixedly connected to the upper plate, and the x-direction moving electrode is connected to the upper plate through a flexible structure; adjacent sides of the x-direction moving electrode and the x-direction fixed electrode are provided with comb teeth, and the comb teeth of the x-direction moving electrode and the x-direction fixed electrode are staggered and leave movable gaps with equal spacing;

[0013] The lower structure is located on the lower surface of the lower plate, and includes n y-direction moving electrodes and n+1 y-direction fixed electrodes arranged at intervals; the y-direction fixed electrode is fixedly connected to the lower plate, and the y-direction moving electrode is connected to the lower plate through a flexible structure; adjacent sides of the y-direction fixed electrode and the y-direction moving electrode are provided with comb teeth, and the comb teeth of the y-direction moving electrode and the y-direction fixed electrode are staggered and leave active gaps with equal spacing; the x-direction moving electrode and the y-direction moving electrode are perpendicular to each other.

[0014] Furthermore, the upper surface and the lower surface of the mass block are both square; the cantilever group includes an upper group of cantilevers and a lower group of cantilevers corresponding to the upper and lower surfaces of the square respectively, and each group of cantilevers includes four rotationally symmetrical cantilevers; the cantilever is a Z-shaped structure, and its two ends are respectively connected to the outer frame and the square edge end points.

[0015] Furthermore, the cantilevers that are located directly opposite to each other in the upper and lower positions are connected to the end points on the opposite sides of the corresponding square sides.

[0016] Furthermore, the upper surface of the upper plate and the lower surface of the lower plate are both covered with an insulating layer, and the upper surface of the upper plate and the lower surface of the lower plate are both provided with anchor points, and the x-direction moving electrodes and the y-direction moving electrodes are connected to the corresponding anchor points through a flexible structure.

[0017] Furthermore, the outer surfaces of the anti-collision protrusions and the limiting protrusion frame are covered with an insulating layer.

[0018] Furthermore, n=2.

[0019] A method for manufacturing a three-axis MEMS capacitive acceleration sensor, used to manufacture the above acceleration sensor, comprises the following manufacturing steps:

[0020] First, the production of the superstructure and upper plate,

[0021] Step 1, selecting a double-sided polished low-resistance SOI silicon wafer and performing a first oxidation on it;

[0022] Step 2: etching an x-direction fixed electrode, an x-direction moving electrode, a flexible structure and corresponding anchor points on the front side of the oxidized low-resistance SOI silicon wafer; etching a limiting convex frame on the back side of the oxidized low-resistance SOI silicon wafer;

[0023] Step 3, re-oxidizing the low-resistance SOI silicon wafer;

[0024] Step 4: For the front side of the low-resistance SOI silicon wafer, release the x-direction moving electrode; for the back side of the low-resistance SOI silicon wafer, retain the oxide layer on the anti-collision bump and the limit convex frame, and remove the oxide layer at other positions in the limit convex frame area; thereby obtaining the upper structure and the upper board;

[0025] Second, the production of mass block and fixed frame.

[0026] Step 1: Performing deep wet etching on the front side of two double-sided polished low-resistance silicon wafers to obtain two sets of low-resistance silicon wafers with under-arm cavities;

[0027] Step 2, making the cavities under the arms of the two groups of low-resistance silicon wafers face each other and performing silicon-silicon bonding;

[0028] Step 3, etching an upper group of cantilevers and a lower group of cantilevers on the upper and lower surfaces of the bonded low-resistance silicon wafer, thereby obtaining a mass block and a fixed frame;

[0029] Third, the production of the lower structure and the lower plate,

[0030] Step 1, selecting a double-sided polished low-resistance SOI silicon wafer and performing a first oxidation on it;

[0031] Step 2: Etching a y-direction fixed electrode, a y-direction moving electrode, a flexible structure and corresponding anchor points on the front side of the oxidized low-resistance SOI silicon wafer; etching a limiting convex frame on the back side of the oxidized low-resistance SOI silicon wafer;

[0032] Step 3, re-oxidizing the low-resistance SOI silicon wafer;

[0033] Step 4: For the front side of the low-resistance SOI silicon wafer, release the y-direction moving electrode; for the back side of the low-resistance SOI silicon wafer, retain the oxide layer on the anti-collision bump and the limit convex frame, and remove the oxide layer at other positions in the limit convex frame area; thereby obtaining the lower structure and the lower board;

[0034] After the above steps are completed, the obtained parts are connected by silicon-silicon bonding according to the corresponding relationship.

[0035] The beneficial effects of the above technical solution of the present invention are:

[0036] 1. The present invention adopts a three-axis capacitive acceleration sensor, which effectively improves the utilization rate of silicon wafers in the vertical direction, improves integration, reduces volume, and ensures the sensor range and sensitivity.

[0037] 2. The present invention adopts a three-axis capacitive acceleration sensor, which is less affected by temperature and has a large measurement range and stable performance.

[0038] 3. The present invention adopts a comb-tooth type multiplied capacitance acceleration sensor in the x and y directions, and utilizes a common fixed electrode to effectively increase the capacitance change of the sensor and improve the sensitivity of acceleration.

[0039] 4. The present invention adopts a Z-direction sandwich-type differential capacitive acceleration sensor, and utilizes a Z-shaped structure to effectively increase the movable range of the mass block, increase the capacitance change, and thus improve the sensitivity of acceleration.

[0040] 5. The various layers of the structure of the present invention adopt silicon-silicon bonding, which effectively ensures the bond and strength of the sensor and improves the reliability of the sensor.

[0041] 6. Each layer of the present invention adopts low-resistance silicon material, which is easy to lead and effectively reduces the production cost, while reducing the difficulty of producing each layer of electrodes.

[0042] 7. The present invention provides a limit convex frame and an anti-collision convex point to prevent the sensor from being damaged or failing during bonding, dicing and use. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 It is a schematic diagram of the overall structure of an embodiment of the present invention.

[0044] Figure 2 yes Figure 1 Schematic diagram of the middle part structure.

[0045] Figure 3 yes Figure 2 Schematic diagram of the structure of the middle mass block and cantilever.

[0046] Figure 4 yes Figure 1 Schematic diagram of the middle and upper structure.

[0047] Figure 5 yes Figure 1 Schematic diagram of the lower surface of the middle and upper level board.

[0048] Figure 6 yes Figure 1 Schematic diagram of the middle and lower structure.

[0049] Figure 7 yes Figure 1 Schematic diagram of the upper surface of the middle and lower boards.

[0050] In the figure: 31, upper structure, 32, middle structure, 33, lower structure, 41, 45, 48, x-direction fixed electrode, 42, x-direction flexible structure, 43, x-direction anchor point, 44, upper plate lead area, 46, insulating layer, 47, upper plate, 51, upper plate insulating layer, 52, limiting convex frame, 53, anti-collision convex point, 61, 63, cantilever, 62, z-direction lead area, 64, mass block, 65, fixed frame, 71, lower plate insulating layer, 72, limiting convex frame, 73, anti-collision convex point, 81, 85, 88, y-direction fixed electrode, 82, y-direction flexible structure, 83, y-direction anchor point, 84, lower plate lead area, 86, insulating area, 87, lower plate. DETAILED DESCRIPTION

[0051] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0052] like Figures 1 to 7 As shown, this embodiment includes an upper structure 31 composed of an x-direction fixed electrode, an x-direction movable electrode, an x-direction anchor point, an x-direction flexible structure and a lead area of ​​an upper plate, a middle structure 32 composed of an upper plate, a lower plate, a mass block and a cantilever, and a lower structure 33 composed of a y-direction fixed electrode, a y-direction movable electrode, a y-direction anchor point, a y-direction flexible structure and a lead area of ​​a lower plate.

[0053] The x-direction fixed electrode 41 , the x-direction movable electrode and the x-direction anchor point 43 are located on the top of the upper plate, and the x-direction movable electrode and the x-direction anchor point are connected via the x-direction flexible structure 42 .

[0054] An insulating layer is provided on the upper surface of the upper board, and an insulating layer is provided on the lower surface of the lower board; the limiting convex frame of the upper board is consistent with the square in the fixed frame, the anti-collision convex point of the upper board is facing the position of the mass block, and the lead area 44 of the upper board is located at the edge of the upper board.

[0055] The inner end of each cantilever 61 in the upper group of cantilevers is connected to the upper surface of the mass block 64, and the outer end of each cantilever in the upper group of cantilevers is connected to the upper surface of the fixed frame 65; the inner end of each cantilever in the lower group of cantilevers is connected to the lower surface of the mass block, and the outer end of each cantilever in the lower group of cantilevers is connected to the lower surface of the fixed frame; the upper group of cantilevers and the lower group of cantilevers are rotationally symmetrical about the center of the mass block, and a z-direction lead area 62 is provided at the edge of the fixed frame, and the z-direction lead area and the upper board lead area are on the same side but the projection positions do not overlap.

[0056] The y-direction fixed electrode 81, the y-direction movable electrode and the y-direction anchor point 83 are all located at the bottom of the lower plate, and the y-direction movable electrode is connected to the y-direction anchor point through a flexible structure; an insulating layer is provided on the lower surface of the lower plate, the anti-collision protrusion of the lower plate is located on the upper surface of the lower plate, the limiting convex frame of the lower plate is consistent with the square in the fixed frame, the anti-collision protrusion of the lower plate is opposite to the position of the mass block, the lead area of ​​the lower plate is located at the edge of the lower plate, the lead area 84 of the lower plate 87 is on the same side as the lead area of ​​the upper plate and the z-direction lead area, but the projection positions do not overlap.

[0057] The sensor uses an x-direction fixed electrode and an x-direction moving electrode to form a comb-tooth type multiplied capacitance acceleration sensor for sensing acceleration in the x direction; uses a y-direction fixed electrode and a y-direction moving electrode to form a comb-tooth type multiplied capacitance acceleration sensor for sensing acceleration in the y direction; and uses an upper plate, an upper group of cantilevers, a lower group of cantilevers and a mass block, and a lower plate to form a sandwich-type differential capacitance acceleration sensor for sensing acceleration in the z direction.

[0058] The sensor consists of an upper structure, a middle structure, and a lower structure, and performs the function of three-axis acceleration sensing. The insulating layer 46 on the upper surface of the upper board 47 provides a silicon oxide isolation layer for the sensor sensing the x and z directions, and the insulating layer 86 on the lower surface of the lower board provides a silicon oxide isolation layer for the sensor sensing the y and z directions.

[0059] The upper and lower structures of the sensor are made of SOI silicon wafers, and the middle structure is made of two low-resistance silicon wafers; the upper and middle structures are formed by silicon-silicon bonding of the insulating layer on the lower surface of the upper board and the fixed frame, and the lower and middle structures are formed by silicon-silicon bonding of the insulating layer on the upper surface of the lower board and the fixed frame.

[0060] The x-direction moving electrode and the y-direction moving electrode 82 of the sensor provide elasticity for sensing acceleration in the x or y direction through a flexible structure.

[0061] The sensor adopts dry etching to obtain the upper cantilever and the lower cantilever, which are respectively located on the upper and lower sides of the mass block and are both elastic movable beam structures, providing elasticity for the forced motion of the mass block.

[0062] The sensor adopts two oxidations and etchings to form the step spacing of the upper structure and the lower structure, that is, to form the limit convex frame of the upper plate and the limit convex frame of the lower plate, to provide a capacitance gap for the sandwich-type acceleration differential sensor for z-direction acceleration perception, to provide a warning for bonding, dicing, and use, to prevent dicing from damaging the sensor, to prevent the mass block from being attracted to the upper plate and the lower plate due to external force during bonding and use, resulting in failure of the sensor, and to form the upper plate anti-collision convex point and the lower plate anti-collision convex point at the same time. This setting can prevent the mass block from being attracted to the upper plate and the lower plate when moving up and down, resulting in failure of the sensor, and improve the reliability of the sandwich-type acceleration differential sensor for z-direction acceleration perception.

[0063] The x-direction fixed electrode, x-direction moving electrode, x-direction anchor point, upper plate, upper group of cantilevers, lower group of cantilever beams, mass block, fixed frame, y-direction fixed electrode, y-direction moving electrode, y-direction anchor point and lower plate of the sensor are all made of low-resistance silicon material; the insulating layer, upper plate insulating layer 51, upper plate anti-collision bumps 53, lower plate insulating layer 71, lower plate anti-collision bumps 73 and insulating layer 86 are all made of silicon oxide.

[0064] The working principle of the present invention is as follows:

[0065] The acceleration sensing in the x and y directions of the three-axis MEMS capacitive acceleration sensor is a comb-tooth type multiplied capacitance acceleration sensor, which is composed of a moving electrode and a fixed electrode. When subjected to acceleration in the x or y direction, the moving electrode moves along the x or y direction, and the capacitance value of the parallel plate capacitor composed of the fixed electrode changes. Since the comb-tooth type multiplied acceleration sensor uses a common fixed electrode, the capacitance change is twice that of a single comb-tooth type acceleration sensor, and the acceleration value in the x or y direction is obtained by using the multiplied capacitance value; and the acceleration sensing in the z direction is a sandwich-type differential capacitance acceleration sensor, which is composed of an upper plate, a lower plate and a mass layer. When subjected to acceleration in the z direction, the mass block moves along the Z direction, and the capacitance value of the parallel plate capacitor composed of the upper and lower plates changes, and the acceleration value in the z direction is obtained by using the differential capacitance.

[0066] The working principle of getting the acceleration value in the x or y direction is as follows:

[0067] Ideally, the moving electrode comb teeth are located in the middle of the fixed electrode comb teeth. In the absence of acceleration, the moving electrode does not move, and the expression of the comb tooth capacitance value is:

[0068]

[0069] Where C s0 is the initial capacitance value of a single comb-tooth capacitive accelerometer, ε is the relative dielectric constant, S s is the sum of the areas facing each comb tooth of a single comb-tooth capacitive accelerometer, d s0is the initial spacing between comb teeth.

[0070] When the three-axis MEMS capacitive accelerometer senses acceleration in the x or y direction, the movable electrode is forced to move to produce a displacement x s , so the capacitance difference of a single comb-tooth capacitive accelerometer is:

[0071]

[0072] Then the capacitance value obtained when the acceleration is sensed in the x or y direction is twice the capacitance difference of a single comb-tooth capacitive acceleration sensor, and the acceleration value can be calculated as:

[0073]

[0074] Where m s is the mass of the movable electrode, k s is the elastic stiffness of the system.

[0075] The working principle of obtaining the acceleration value in the z direction is as follows:

[0076] Ideally, the mass block is located in the middle of the upper and lower plates. In the absence of acceleration, the mass block does not move, and the expression of the upper and lower capacitance values ​​is:

[0077]

[0078] Where C1 and C2 are the capacitance values ​​of the upper and lower parts respectively, S is the facing area between the mass block and the upper and lower plates, and d0 is the initial distance between the mass block and the upper and lower plates.

[0079] When the three-axis MEMS capacitive accelerometer senses the acceleration in the Z direction, the mass block is forced to move and produces a displacement x, so the capacitance difference of the sandwich capacitive accelerometer is obtained as

[0080]

[0081] The acceleration value calculated by the capacitance value obtained when the acceleration is sensed in the z direction is:

[0082]

[0083] Where m is the mass of the mass block and k is the elastic stiffness of the system.

[0084] The preparation process of the superstructure and upper plate mainly includes the following steps:

[0085] Step 1: performing a first oxidation on a double-sided polished low-resistance SOI silicon wafer to form an oxide layer on the upper and lower surfaces of the SOI silicon wafer;

[0086] Step 2: using dry etching to remove the oxide layer on the upper surface of the SOI silicon wafer to form a front pattern, which is consistent with the shape of the edge where the x-direction fixed electrode, the x-direction moving electrode, the x-direction anchor point and the lead area of ​​the upper plate are located;

[0087] Step 3: Dry etching is used to remove the oxide layer on the lower surface of the SOI silicon wafer to form a reverse pattern, which is consistent with the shape of the upper plate limit convex frame;

[0088] Step 4: After the photolithography is completed, the SOI silicon wafer is oxidized for the second time. At this time, the thickness of the oxide layer at the reverse pattern is lower than the thickness of the oxide layer at the peripheral position;

[0089] Step 5: Use wet etching to remove the oxide layer and other excess oxide layers under the x-direction moving electrode on the front side of the SOI silicon wafer, and release the edge of the x-direction moving electrode on the front side and the lead area of ​​the upper board;

[0090] Step 6: Use wet etching to remove the oxide layer on the back side of the SOI silicon wafer to form a limiting convex frame of the upper plate and retain the anti-collision convex points of the upper plate;

[0091] Step seven, using dry etching to obtain the upper board lead area on the front side of the SOI silicon wafer.

[0092] The preparation process of the mass block and the fixed frame in the middle structure mainly includes the following steps:

[0093] Step 1: deep etching the double-sided polished low-resistance silicon wafer on the front side by wet etching, and obtaining the arm cavity under the upper cantilever group and the arm cavity under the lower cantilever group by self-stop etching process;

[0094] Step 2: Select two deep-etched low-resistance silicon wafers and perform silicon-silicon bonding on the front side to complete the cavity structure under the double-sided round-shaped arm in the middle layer structure;

[0095] Step 3, using dry etching to remove the excess portion of the silicon wafer to form an upper group of cantilevers and a z-direction lead area on the front side of the silicon wafer after bonding;

[0096] Step 4: using dry etching to remove the excess portion of the silicon wafer to form a lower group of cantilever beams on the reverse side of the silicon wafer after bonding;

[0097] The preparation process of the lower structure and the lower plate mainly includes the following steps:

[0098] Step 1: performing a first oxidation on a double-sided polished low-resistance SOI silicon wafer to form an oxide layer on the upper and lower surfaces of the SOI silicon wafer;

[0099] Step 2: using dry etching to remove the oxide layer on the upper surface of the SOI silicon wafer to form a front pattern, which is consistent with the shape of the edge where the y-direction fixed electrode, the y-direction moving electrode, the y-direction anchor point and the lead area of ​​the lower board are located;

[0100] Step 3: Dry etching is used to remove the oxide layer on the lower surface of the SOI silicon wafer to form a reverse pattern, which is consistent with the shape of the lower plate limit convex frame;

[0101] Step 4: After the photolithography is completed, the SOI silicon wafer is oxidized for the second time. At this time, the thickness of the oxide layer at the reverse pattern is lower than the thickness of the oxide layer at the peripheral position;

[0102] Step 5: Use wet etching to remove the oxide layer under the y-direction moving electrode on the front side of the SOI silicon wafer and other excess oxide layers, releasing the edge of the y-direction moving electrode on the front side and the lead area of ​​the lower board;

[0103] Step 6: Use wet etching to remove the oxide layer on the back side of the SOI silicon wafer to form a lower-level board limiting convex frame and retain the lower-level board anti-collision convex points;

[0104] Step seven, using dry etching to obtain the lower-level board lead area on the front side of the SOI silicon wafer.

[0105] After the upper structure 31, the middle structure 32, and the lower structure 33 are prepared respectively, they are aligned on the left side, and the upper structure 31, the middle structure 32, and the lower structure 33 are arranged from top to bottom in this order, and the three-layer structure of the three-axis MEMS capacitive acceleration sensor is bonded using a silicon-silicon bonding method.

[0106] The present invention can sense acceleration in the x, y and z directions and has the advantages of small size, large measuring range, high sensitivity, high reliability, high integration, low cost, low noise and stable performance. The number of fixed electrodes, movable electrodes and cantilever beams can be adjusted according to the requirements of the use environment to obtain different system elastic coefficients and system characteristic frequencies.

Claims

1. A three-axis MEMS capacitive acceleration sensor, It is characterized in that It includes an upper structure for detecting acceleration in the x direction, a middle structure for detecting acceleration in the z direction, and a lower structure for detecting acceleration in the y direction; The middle-level structure comprises an upper plate, a fixed frame and a lower plate stacked in sequence; a mass block is arranged in the fixed frame, and the mass block is fixed at the center of the fixed frame through a cantilever group; a limit convex frame and an anti-collision convex point are arranged on the lower surface of the upper plate and the upper surface of the lower plate for constraining the movement of the mass block; there are gaps between the upper plate and the mass block and between the mass block and the lower plate; The upper structure is located on the top of the upper plate, and includes n x-direction moving electrodes and n+1 x-direction fixed electrodes arranged at intervals, wherein n≥1; the x-direction fixed electrode is fixedly connected to the upper plate, and the x-direction moving electrode is connected to the upper plate through a flexible structure; adjacent sides of the x-direction moving electrode and the x-direction fixed electrode are provided with comb teeth, and the comb teeth of the x-direction moving electrode and the x-direction fixed electrode are staggered and leave movable gaps with equal spacing; The lower structure is located at the bottom of the lower plate, and includes n y-direction moving electrodes and n+1 y-direction fixed electrodes arranged at intervals; the y-direction fixed electrode is fixedly connected to the lower plate, and the y-direction moving electrode is connected to the lower plate through a flexible structure; the adjacent sides of the y-direction fixed electrode and the y-direction moving electrode are provided with comb teeth, and the comb teeth of the y-direction moving electrode and the y-direction fixed electrode are staggered and leave active gaps with equal spacing; the x-direction moving electrode and the y-direction moving electrode are perpendicular to each other; The upper and lower surfaces of the mass block are both square; the cantilever group includes an upper group of cantilevers and a lower group of cantilevers corresponding to the upper and lower surfaces of the square, respectively, and each group of cantilevers includes four rotationally symmetrical cantilevers; the cantilever is a Z-shaped structure, and its two ends are respectively connected to the outer frame and the end points of the square edge; The upper surface of the upper plate and the lower surface of the lower plate are both covered with an insulating layer, and the upper surface of the upper plate and the lower surface of the lower plate are both provided with anchor points, and the x-direction moving electrodes and the y-direction moving electrodes are connected to the corresponding anchor points through a flexible structure.

2. A three-axis MEMS capacitive acceleration sensor according to claim 1, It is characterized in that The cantilevers that are directly opposite to each other in the upper and lower positions are connected to the opposite end points of the corresponding square sides.

3. The three-axis MEMS capacitive acceleration sensor according to claim 1, It is characterized in that The outer surfaces of the anti-collision convex points and the limiting convex frame are both covered with an insulating layer.

4. The three-axis MEMS capacitive acceleration sensor according to claim 1, It is characterized in that Said n=2.

5. A method for manufacturing a three-axis MEMS capacitive acceleration sensor, It is characterized in that Used to manufacture the acceleration sensor as claimed in any one of claims 1 to 4, comprising the following manufacturing process: (I) The production of the superstructure and upper plate includes the following steps: (101) Selecting a double-sided polished low-resistance SOI silicon wafer and performing a first oxidation on it; (102) etching an x-direction fixed electrode, an x-direction movable electrode, a flexible structure and corresponding anchor points on the front side of the oxidized low-resistance SOI silicon wafer; etching a limiting convex frame on the back side of the oxidized low-resistance SOI silicon wafer; (103) Re-oxidizing the low-resistance SOI silicon wafer; (104) For the front side of the low-resistance SOI silicon wafer, the x-direction moving electrode is released; for the back side of the low-resistance SOI silicon wafer, the oxide layer on the anti-collision bump and the limiting convex frame is retained, and the oxide layer at other positions in the limiting convex frame area is removed; thereby, the upper structure and the upper board are obtained; (II) The production of the mass block and the fixed frame includes the following steps: (201) Two double-sided polished low-resistance silicon wafers are subjected to front-side wet deep etching to obtain two sets of low-resistance silicon wafers with under-arm cavities; (202) making the cavities under the arms of two sets of low-resistance silicon wafers face each other and performing silicon-silicon bonding; (203) etching an upper group of cantilevers and a lower group of cantilevers on the upper and lower surfaces of the bonded low-resistance silicon wafer, thereby obtaining a mass block and a fixed frame; (III) The production of the lower structure and the lower plate includes the following steps: (301) Selecting a double-sided polished low-resistance SOI silicon wafer and performing a first oxidation on it; (302) etching a y-direction fixed electrode, a y-direction moving electrode, a flexible structure and corresponding anchor points on the front side of the oxidized low-resistance SOI silicon wafer; etching a limiting convex frame on the back side of the oxidized low-resistance SOI silicon wafer; (303) re-oxidizing the low-resistance SOI silicon wafer; (304) For the front side of the low-resistance SOI silicon wafer, the y-direction moving electrode is released; for the back side of the low-resistance SOI silicon wafer, the oxide layer on the anti-collision bump and the limiting convex frame is retained, and the oxide layer at other positions in the limiting convex frame area is removed; thereby obtaining the lower structure and the lower board; (iv) Connecting the parts produced in the above steps by silicon-silicon bonding according to the corresponding relationship.

Citation Information

Cited By

  • Three-axis acceleration chip and manufacturing method

    CN120028574A

  • A three-axis acceleration chip and a manufacturing method thereof

    CN120028574B

  • Novel MEMS acceleration sensor switch and processing method thereof

    CN121186399A

  • A novel MEMS acceleration sensor switch

    CN225001249U