Sintered insert parts
The method addresses height variations in sintered parts by using a movable mold with a parting surface and tapered surfaces to integrate sintered bearings with exterior components effectively, preventing gaps and burrs, and ensuring secure attachment and appearance.
Patent Information
- Application Number
- JP2023112363
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-07-07
- Publication Date
- 2024-09-18
- Estimated Expiration
- 2040-01-31
AI Technical Summary
Existing insert molding processes for sintered parts, such as sintered bearings, face challenges in integrating them with exterior components due to variations in height, leading to gaps or burrs, as well as issues with rotation and axial movement prevention.
A method involving a molding die with a fixed and movable mold, where the movable mold moves along a parting surface to accommodate height variations, forming a parting line at a ridge line, and using tapered surfaces to prevent material coverage and burrs, while integrating the sintered and exterior parts through grooves or protrusions.
Ensures reliable integration of sintered and exterior parts without gaps or burrs, preventing rotation and axial movement, and maintaining a clean appearance by forming parting lines at ridge lines.
Smart Images

Figure 0007553660000009 
Figure 0007553660000010 
Figure 0007553660000004
Abstract
Description
[Technical field]
[0001] The present invention relates to an insert sintered part in which a sintered part, such as a sintered bearing, and an exterior part are integrated together. [Background technology]
[0002] Sintered bearings are made by impregnating the interior of the sintered body with lubricating oil in advance, and the oil seeps out to lubricate the friction surfaces through the pumping action caused by the rotation of the shaft and thermal expansion due to frictional heat. Since sintered bearings can be used for long periods of time without lubrication, they are widely used as bearings for rotating shafts in automobiles, home appliances, audio equipment, etc. In order to incorporate such sintered bearings into structures such as automobiles, they are integrated with exterior components such as housings by insert molding. In this case, radial and thrust loads act on the sintered bearing, so it is necessary to prevent both rotation relative to the exterior component and axial removal.
[0003] For example, Patent Document 1 discloses a sintered bearing (sintered part) with bottomed grooves formed on the outer circumferential surface at positions that do not coincide with each other in the axial direction, the bottomed grooves extending from both end faces to each end face and partway along the axial direction. It discloses that when a resin part (exterior part) is integrally molded on the outer circumferential surface of the sintered bearing by insert molding, the resin gets into the bottomed grooves, preventing rotation and axial falling off. Furthermore, Patent Document 2 discloses a sintered bearing (sintered part) in which an axially extending groove and a circumferentially extending enlarged diameter part are formed on the outer peripheral surface thereof, with the groove part interrupting the circumferential extension of the enlarged diameter part. When a resin part is integrally molded onto the outer peripheral part of this sintered bearing by insert molding, the resin gets into the groove part, preventing the sintered bearing from rotating relative to the resin part, and the enlarged diameter part is integrated so as to bite into the resin part, preventing the sintered bearing from coming loose in the axial direction. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2003-159720 A [Patent Document 2] JP 2003-193113 A Summary of the Invention [Problem to be solved by the invention]
[0005] When insert-molding a sintered part such as a sintered bearing into a resin part, a space (cavity) is formed on the outer periphery of the sintered part placed in a molding die, and molten resin (molten material) is injected into the cavity to fill it. At this time, in order to cover the outer periphery of the sintered part with the resin part, a cavity is formed around the outer periphery of the sintered part with both end faces abutted against the molding die. However, even if sintered parts are manufactured with the same dimensions, it is difficult to eliminate variations in height. For example, if the height of the sintered part is slightly lower than the preset dimension, a gap will be generated between one end face of the sintered part and the molding die, and the molten material that will become the exterior part will enter the gap and form a film on the end face of the sintered part. On the other hand, if the height of the sintered part is slightly higher than the preset dimension, the molding die will be pressed by the sintered part, causing a gap at the parting line of the molding die, and the molten material will protrude from the gap and become a burr.
[0006] The present invention has been made in consideration of the above circumstances, and has an object to appropriately integrate a sintered part and an exterior part such as a resin part by insert molding, even when there is variation in the height of the sintered part, such as a sintered bearing. [Means for solving the problem]
[0007] The method for producing an insert sintered part of the present invention includes a sintered part forming step of forming a sintered part having a first end portion and a second end portion by powder molding, and an insert molding step of forming an insert sintered part in which an exterior part is integrated with the outer periphery of the sintered part, The molding die used in the insert molding step has a fixed die and a movable die, and a parting surface between the fixed die and the movable die is formed along a moving direction of the movable die, The insert molding process includes a mold assembly process in which the sintered part is held between the fixed mold and the movable mold, the movable mold is moved along the parting surface, and the sintered part is pressed toward the fixed mold by the movable mold, thereby forming a cavity around the sintered part by covering with the molding die at a distance around the sintered part, except for the portion of the sintered part at a first end that abuts against the fixed mold and the portion of the sintered part at a second end that abuts against the movable mold, and a filling process in which the cavity is filled with molten material that will become the exterior part after the mold assembly process.
[0008] The insert sintered part of the present invention comprises a sintered part having a first end and a second end, and an exterior part integrally molded on the outer periphery of the sintered part, and a parting line is formed on a ridge line formed at the intersection between the outer periphery of the exterior part and an end face of the exterior part located on either the first end or the second end side.
[0009] According to the present invention, since the movable die moves along the parting surface of the molding die, even if the height of the sintered part varies, the movable die presses the sintered part toward the fixed die, so that the fixed die and the movable die can be reliably abutted against the sintered part. This prevents the abutment portion of the fixed die and the movable die from being covered in a film by the material of the exterior part, and prevents burrs from being generated. In addition, since the parting line is formed on the ridge line, not on the outer circumferential surface or end surface of the exterior part, the appearance of the insert sintered part can be improved. Furthermore, when a groove or a protrusion is formed on the outer circumferential surface of the sintered part, the sintered part and the exterior part are integrated in a state where they are prevented from rotating by the groove or protrusion of the sintered part.
[0010] As one embodiment of the manufacturing method for an insert sintered part, in the sintered part forming process, an outer inclined surface is formed on the outer peripheral surface of at least one of the first end and the second end, the diameter of which gradually decreases toward the end face of the one end, and at least one of the fixed mold and the movable mold is formed with a recess having a first tapered surface abutting the outer inclined surface, and in the mold assembling process, the first tapered surface is abutted against the outer inclined surface. In this case, the sintered part may be a sintered bearing having one through hole penetrating the first end and the second end.
[0011] In another embodiment of the manufacturing method of an insert sintered part, in the sintered part forming process, a through hole penetrating the first end and the second end is formed, and an inner inclined surface is formed in the through hole, the diameter of which gradually increases toward the end face of at least one of the first end and the second end, and at least one of the fixed mold and the movable mold is formed with a convex portion having a second tapered surface that abuts against the inner inclined surface, and in the mold assembling process, the second tapered surface is abutted against the inner inclined surface. In this case, the sintered part may consist of a sintered bearing.
[0012] In each of the above aspects, since the outer inclined surface provided on the outer peripheral surface of the sintered part is covered by the first tapered surface, or the inner inclined surface provided on the through hole of the sintered part is covered by the second tapered surface, it is possible to more reliably prevent at least one of the first end and the second end from being covered in a film-like manner with the material of the exterior part. Also, when the sintered part is made of a sintered bearing, it is possible to prevent the through hole (bearing hole) from being covered in a film-like manner with the material of the exterior part.
[0013] In one embodiment of the insert sintered part, at least one of the first end and the second end of the sintered part may protrude from the exterior part, and an outer circumferential surface of the one end of the sintered part may be provided with an outer inclined surface that gradually reduces in diameter toward the end face of the one end. In this case, the sintered part may be a sintered bearing having a through hole that penetrates the first end and the second end.
[0014] As another embodiment of the insert sintered part, the sintered part may have one through hole penetrating the first end and the second end, and the through hole may have an inner inclined surface that gradually expands in diameter toward an end face of at least one of the first end and the second end. In this case, the sintered part may be a sintered bearing.
[0015] In one embodiment of the insert sintered part, a groove or a protrusion may be formed on the outer periphery of the sintered part.
[0016] In another embodiment of the insert sintered part, a large diameter portion having an outer diameter larger than that of the one end portion is formed on the outer periphery of the sintered part, and the large diameter portion is formed with at least one of a groove or a protrusion along the axial direction on the outer periphery surface of the large diameter portion and a groove or a protrusion along the radial direction on the end face of the large diameter portion. Effect of the Invention
[0017] The present invention makes it possible to appropriately integrate a sintered part, such as a sintered bearing, with an exterior part, such as a resin part, by insert molding, even when there is variation in the height of the sintered part. [Brief description of the drawings]
[0018] [Figure 1] 1 is a vertical cross-sectional view showing an insert bearing according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a vertical cross-sectional view of a sintered bearing used in the insert bearing of FIG. 1. [Diagram 3]3 is an end view of the sintered bearing of FIG. 2, viewed from a first end side in the axial direction. [Figure 4] 4 is a flowchart showing a manufacturing process of the insert bearing of the first embodiment. [Diagram 5] FIG. 4 is a vertical cross-sectional view showing a state in which a molded body is being formed in a molding process. [Figure 6] 1 is a vertical cross-sectional view showing a state in which a sintered body is being straightened in a straightening process (left half) and a state in which the sintered body has been removed from the straightening die (right half). FIG. [Figure 7] FIG. 2 is a vertical cross-sectional view showing a state during a mold clamping step in an injection molding process. [Figure 8] FIG. 4 is a vertical sectional view of a sintered bearing according to a second embodiment of the present invention. [Figure 9] 9 is an end view of the sintered bearing of FIG. 8, as viewed from a first end side in the axial direction. [Figure 10] FIG. 9 is a vertical cross-sectional view showing the state of the sintered bearing in FIG. 8 during a mold clamping process. [Figure 11] FIG. 11 is a longitudinal sectional view of a sintered bearing used in an insert bearing according to a third embodiment of the present invention. [Figure 12] 12 is an end view of the sintered bearing of FIG. 11 as viewed from a first end side in the axial direction. [Figure 13] FIG. 11 is a vertical cross-sectional view showing a state during a mold clamping process of a sintered bearing used in an insert bearing according to a fourth embodiment of the present invention. [Figure 14] FIG. 11 is a vertical cross-sectional view showing a state during a mold clamping process of a sintered part used in an insert sintered part according to a modified example of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, embodiments of the present invention will be described. In each of the following embodiments, a resin part is integrated with a sintered bearing by injection molding. Therefore, in each embodiment, the exterior part of the present invention is a resin part, and the insert molding process is an injection molding process. In the following embodiments, a sintered bearing is exemplified as the sintered part, and an insert sintered bearing (insert bearing) is exemplified as the insert sintered part.
[0020] [First embodiment] First, an insert bearing according to a first embodiment will be described. In this embodiment, a large diameter portion is provided in a region of the outer periphery of a sintered bearing used in the insert bearing except for one end, and the large diameter portion has an outer diameter larger than that of the one end of the sintered bearing. As shown in FIG. 1, this insert bearing 1 has a cylindrical sintered bearing 10 formed from a sintered body of metal powder, and a resin part 20 (corresponding to the exterior part of the present invention) molded integrally with the outer periphery of the sintered bearing. 2 and 3, the sintered bearing 10 has a bearing hole 11 formed in the center in a penetrating state, and has a first end 121 located on the upper end side of the bearing hole 11 and a second end 122 located on the lower end side of the bearing hole 11. In other words, the bearing hole 11 consists of a single through hole that penetrates the first end 121 and the second end 122. The sintered bearing 10 also has a large diameter portion 13 whose axially intermediate portion has a larger outer diameter than the first end 121, and this large diameter portion 13 extends to the second end 122. In other words, the end face of the large diameter portion 13 on the second end 122 side and the end face of the second end 122 are located on the same plane and are continuous.
[0021] Moreover, the first end 121 of the sintered bearing 10 is formed in a tapered shape that gradually reduces in diameter from the large diameter portion 13 toward the first end 121. The gradient of this tapered surface (outer inclined surface 123) is formed to be, for example, 15° (taper angle 30°), and a part of it protrudes from the resin part 20. In addition, both ends of bearing hole 11 are formed in a tapered shape with the outer diameter gradually increasing toward the end face of first end portion 121 and the end face of second end portion 122. This tapered surface 111 of bearing hole 11 corresponds to the inner inclined surface of the present invention, and is formed during the molding process or straightening process described below, or by machining (cutting) after the straightening process, or the like.
[0022] In addition, multiple (four) grooves 14 are formed in the outer peripheral surface of large diameter portion 13 along the axial direction over the entire length of large diameter portion 13 to both end faces of large diameter portion 13, and both ends in an open state are formed into tapered surfaces. These four grooves 14 are formed at 90° intervals as shown in Fig. 3. The deepest parts of these grooves 14 are formed into a concave arc surface, and both sides are connected to the outer peripheral surface of large diameter portion 13 by convex arc surfaces. In this embodiment, an example in which only the groove 14 is formed has been shown, but for example, a convex ridge protruding in the radial direction may be formed in the large diameter portion 13 along the axial direction.
[0023] On the other hand, as shown in FIG. 1, the outer periphery of the sintered bearing 10 is embedded in the resin part 20 except for the tip of the first end 121 (the end continuing to the end face of the first end 121). That is, the resin part 20 exposes the tip of the first end 121 and embeds the base end (root part) of the first end 121 and the large diameter part 13 in the outer periphery of the sintered bearing 10. That is, in the resin part 20, the bearing holder 21 is fixed integrally to the outer periphery of the sintered bearing 10, and the bearing holder 21 is formed to have substantially the same height as the entire height of the sintered bearing 10, and embeds the entire large diameter part 13 from the midpoint in the axial direction of the first end 121 of the sintered bearing 10. Therefore, both end faces of the large diameter part 13 are covered by the bearing holder 21. The reference numeral 22 denotes a bracket that is connected to other parts.
[0024] A method for manufacturing the insert bearing 1 thus formed (a method for manufacturing a sintered insert part) will now be described. When manufacturing this insert bearing 1, as shown in the flowchart of Fig. 4, first there is a sintered bearing formation process (sintered part formation process) in which a sintered bearing 10 is formed by powder molding, and then there is an injection molding process (corresponding to the insert molding process of the present invention) in which the sintered bearing 10 formed in the sintered bearing formation process is placed in an injection molding die 60 (corresponding to the molding die of the present invention) and a resin part 20 is formed integrally with the outer periphery of the sintered bearing 10 by injection molding. Each process will be described in detail below.
[0025] <Sintered bearing forming process> The sintered bearing formation process includes a molding process for forming a green body 10' that will become the sintered bearing 10, a sintering process for sintering the green body 10' to form a sintered body (not shown), and a straightening process (sizing process) for straightening the sintered body.
[0026] (molding process) 5, a molding die 40 for forming the molded body 10' includes a die 42 having a circular through hole 41 formed therein, a core rod 43 disposed in the through hole 41, a first upper punch 44 and a second upper punch 46 provided from the outside, and a first lower punch 45 opposed to the first upper punch 44 and the second upper punch 46. These punches 44 to 46 are formed in the shape of a concentric cylinder with the core rod 43 at the center.
[0027] Then, powder is filled into the space formed by the die 42, core rod 43, and first lower punch 45, and compressed by upper and lower punches 44 to 46 to form a compact 10'. At this time, the tip of the first upper punch 44 is shaped to have an inclined surface as shown in Fig. 5, and the distance between the first lower punch 45 and the second upper punch 46 is made smaller than the distance between the first lower punch 45 and the first upper punch 44, thereby forming a compact 10' having a large diameter portion 13' on the outer periphery. Also, a bearing hole 11' is formed in a penetrating state by the core rod 43.
[0028] (Sintering process) The resulting molded body 10' is heated to sinter the powder, forming a sintered body.
[0029] (straightening process) The sintered body is subjected to sizing using a sizing die 80. In this sizing process, the outer shape is finished to the final dimensions, and a groove 14 is formed on the outer periphery of the large diameter portion 13. 6, the straightening die 80 used for this straightening has a first upper punch 84 and a first lower punch 85, and a second upper punch 86 and a second lower punch 87 arranged in an upper and lower pair from the outside between a die 82 in which a circular through hole 81 is formed, and a core rod 83 arranged in the through hole 81. In this case, a plurality of protrusions 88 penetrating along the axial direction are formed on the inner peripheral surface of the through hole 81 of the die 82 at intervals in the circumferential direction, and grooves 89 into which the protrusions 88 of the die 82 are slidably fitted are formed on the outer peripheral parts of the first upper punch 84 and the first lower punch 85 at intervals in the circumferential direction.
[0030] The sintered body is then straightened by being forced into between the die 82 and the core rod 83 while being axially pressed by the first punches 84, 85 and the second punches 86, 87. By placing the sintered body in this straightening die 80 and straightening it, grooves 14 are formed in the outer periphery of the large diameter portion 13 along the axial direction at intervals in the circumferential direction. Moreover, the tapered surface 111 of the bearing hole 11 is formed by machining (cutting) or the like after the straightening step.
[0031] Although the grooves 14 are formed in the straightening step of the sintered bearing forming process, the invention is not limited to this and the grooves 14 may be formed in the molding step. The tapered surface 111 of the bearing hole 11 may also be formed in the molding step or the straightening step. Furthermore, the outer inclined surface 123 may also be formed in any of the molding step, the straightening step, machining after the straightening step, etc.
[0032] <Injection molding process> The sintered bearing 10 formed as described above is integrally molded with the resin part 20 by an injection molding process. This injection molding process includes a mold clamping process (corresponding to the mold assembly process of the present invention) of placing the sintered bearing 10 in an injection molding die 60 with a cavity 61 formed on the outside, and an injection process (corresponding to the filling process of the present invention) of injecting molten resin (corresponding to the molten material of the present invention) that will become the resin part into the cavity 61.
[0033] (Mold clamping process) 7, the injection molding die 60 has a fixed die 62 and a movable die 63, and a parting surface 620 between the fixed die 62 and the movable die 63 is formed along the movement direction of the movable die 63. The sintered bearing 10 is held between the fixed die 62 and the movable die 63, and a cavity 61 into which molten resin is filled is formed on the outer periphery of the sintered bearing 10. The fixed die 62 is formed with a recess 64 having a first tapered surface 641 that comes into contact with the outer inclined surface 123 of the sintered bearing 10, and this first tapered surface 641 comes into contact with the outer inclined surface 123.
[0034] Specifically, the movable die 63 moves along the parting surface 620, and the movable die 63 presses the sintered bearing 10 toward the fixed die 62. Therefore, even if the height of the sintered bearing 10 varies, the first end 121 is held in a fitted state up to a midway position in the length direction in the recess 64 of the fixed die 62. As a result, the inner peripheral surface including the first tapered surface 641 of the recess 64 abuts against the outer inclined surface 123 of the first end 121 of the sintered bearing 10 over the entire circumference. In addition, the end face of the protruding portion 65 protruding from the inner surface of the movable die 63 abuts against the end face of the second end 122. The cavity 61 has a bearing retaining space 66 formed to surround the outer periphery of the sintered bearing 10, and a communicating portion 67 communicates with the bearing retaining space 66. The outer circumferential surface and end surface of the large diameter portion 13 of the sintered bearing 10 and the base end (root portion) of the first end 121 near the large diameter portion 13 are exposed in the bearing retaining space 66 of the cavity 61. A sprue 68, through which molten resin is supplied, is connected to the cavity 61 via a gate 69, and a plunger (not shown) for injecting molten resin is connected to the sprue 68.
[0035] (injection process) Then, molten resin is injected into the cavity 61 of the clamped injection mold 60. At this time, injection pressure acts in the cavity 61, but the tip of the first end 121 of the sintered bearing 10 is arranged in a fitted state in the recess 64 of the fixed mold 62, and the second end 122 is in contact with the protruding portion 65. Since the tip of the first end 121 is not exposed in the cavity 61, the injection pressure acts on the outer surface of the sintered bearing 10 except for the tip of the first end 121. Therefore, the molten resin does not leak out to the end face of the first end 121 of the sintered bearing 10. In addition, when the injection pressure increases and the molten resin leaks out from the parting surface 620, a parting line (not shown) is formed on the outer peripheral surface of the exterior part 20. 7, the parting surface 620 of the mold 60 is formed along the moving direction of the movable die 63, and is therefore formed on a ridge line formed at the intersection between the outer circumferential surface of the exterior part 20 and the end face of the exterior part located on the first end part 121 side. Therefore, the appearance of the resin part 20 is hardly affected.
[0036] Therefore, since the movable die 63 moves along the parting surface 620, even if the height of the sintered bearing 10 varies, the fixed die 62 and the movable die 63 can be brought into contact with the sintered bearing 10, so that the contact portion of the fixed die 62 and the movable die 63 is prevented from being covered in a film-like manner with the material of the exterior part 20 and from being burred. As shown in FIG. 1, the insert bearing 1 has a central portion including the large diameter part 13 except for the tip part at both ends 12 of the sintered bearing 10 surrounded by the resin part 20, and the sintered bearing 10 and the resin part 20 are prevented from rotating by the groove 14 and are integrated in a state where they are prevented from coming off in the axial direction by the large diameter part 13. Since no resin film is formed on both end faces of the sintered bearing as described in the prior art and the parting line is formed on the ridge line, the appearance is not impaired and interference with other parts is suppressed.
[0037] [Second embodiment] 8 and 9 are diagrams showing a sintered bearing 10A used in the insert bearing of the second embodiment, and Fig. 10 is a diagram showing a state during a mold clamping step in the manufacturing process of the insert bearing of the second embodiment. The sintered bearing 10A of this embodiment is a cylindrical sintered bearing 10A that does not have the large diameter portion 13 provided in the sintered bearing 10 of the first embodiment. In the second embodiment and the subsequent embodiments, elements common to the first embodiment are given the same reference numerals to simplify the explanation. 8 and 9, the sintered bearing 10A has a bearing hole 11 (through hole) formed in the center in a penetrating state, and has a first end 121A located on the upper end side of the bearing hole 11, and a second end 122A located on the lower end side of the bearing hole 11. Both ends of this bearing hole 11 are formed in a tapered shape with the outer diameter gradually increasing toward the end face of the first end 121A and the end face of the second end 122A. The tapered surface 111A of this bearing hole 11 corresponds to the inner inclined surface of the present invention, and is formed during the molding process or straightening process, or by machining (cutting) after the straightening process, or the like.
[0038] In addition, a plurality of (four) grooves 14A are formed along the axial direction on the outer peripheral surface of the sintered bearing 10A. Specifically, four grooves 14A shorter than half the height of the sintered bearing 10A are formed on the first end 121A side of the outer peripheral surface. The deepest parts of these grooves 14A are formed into a concave arc surface, and both sides of the concave arc surface are connected to the outer peripheral surface of the sintered bearing 10A. These four grooves 14A are formed at 90° intervals as shown in FIG. 9.
[0039] The method for manufacturing such an insert bearing is substantially the same as the method for manufacturing the sintered bearing 10 of the first embodiment, but there are some differences in the shapes of the injection molding die used in the die clamping step and the injection molding step. This will be explained in detail below.
[0040] As shown in Fig. 10, the injection mold 60A has a fixed mold 62A and a movable mold 63A, and the sintered bearing 10A is held between the fixed mold 62A and the movable mold 63A, and a cavity 61 is formed in which molten resin is filled on the outer periphery of the sintered bearing 10A. In the sintered bearing 10A, a convex portion 65A of the movable mold 63A fits into the second end portion 122 side of the bearing hole 11, so that a second tapered surface 651 of the convex portion 65A abuts against the tapered surface 111A of the bearing hole 11 over the entire circumference. In addition, an end face of a protruding portion 64A protruding from the inner surface of the fixed mold 62A abuts against an end face of the first end portion 121A. The cavity 61 has a bearing holding space 66 formed to surround the outer periphery of the sintered bearing 10, and a communication portion 67 communicates with the bearing holding space 66. The outer circumferential surface and part of the end surface of the sintered bearing 10A are exposed in the bearing retaining space 66 of the cavity 61. A sprue 68, through which molten resin is supplied, is connected to the cavity 61 via a gate 69, and a plunger (not shown) for injecting the molten resin is connected to the sprue 68.
[0041] Then, molten resin is injected into the cavity 61 of the clamped injection mold 60A. At this time, injection pressure acts in the cavity 61, but the convex portion 65A of the movable mold 63A fits into the bearing hole 11 on the second end 122A side of the sintered bearing 10A, the tip of the convex portion 65A is arranged in a fitted state, and the first end 121A abuts against the protruding portion 64A. In this way, the tapered surface 111A of the bearing hole 11 on the second end 122A side and the second tapered surface 651 of the convex portion 65A abut against each other, and this portion is not exposed in the cavity 61, so the injection pressure acts on the outer surface of the bearing hole 11 of the sintered bearing 10A except for the second end 122A side. For this reason, the molten resin does not leak out to the portion of the bearing hole 11 of the sintered bearing 10A on the second end 122A side. Furthermore, when the injection pressure increases and the molten resin leaks out from the parting surface 620, a parting line (not shown) is formed on the outer circumferential surface of the exterior part, but since the parting surface 620 of the mold 60A is formed along the moving direction of the movable die 63A as shown in Fig. 8, the parting line is formed on the ridge line formed at the intersection between the outer circumferential surface of the exterior part and the end face of the exterior part located on the first end portion 121A side. Therefore, the appearance of the resin part is hardly affected.
[0042] [Third embodiment] 11 and 12 show a sintered bearing 10B used in an insert bearing according to a third embodiment. 11 and 12, the sintered bearing 10B of this embodiment, like the second embodiment, has a bearing hole 11 (through hole) formed in the center in a penetrating state, and has a first end 121B located on the upper end side of the bearing hole 11 and a second end 122B located on the lower end side of the bearing hole 11. Tapered surfaces 111B are formed on both ends of this bearing hole 11 by machining (cutting) during the molding process or straightening process, or after the straightening process.
[0043] The grooves 14B formed in this sintered bearing 10B are formed in the end face of the first end portion 121B, as shown in Figures 11 and 12. Four of these grooves 14B are formed at 90° intervals and extend in the radial direction of the end face of the first end portion 121B. The deepest parts of these grooves 14B are formed as a flat surface and have an inclined surface that gradually increases in diameter from the deepest part toward the upper side. The sintered bearing 10B in this embodiment differs from the second embodiment only in the shape of the groove 14B, and therefore uses the same injection molding die 60A as in the second embodiment to form an insert bearing. Therefore, this embodiment can also achieve the same effects as the second embodiment.
[0044] [Fourth embodiment] FIG. 13 is a view showing a state during a mold clamping step in the manufacturing process of the insert bearing of the fourth embodiment. The sintered bearing 10C of this embodiment is a pivot bearing formed in a solid shape, unlike the above-mentioned embodiments. As shown in Fig. 13, this sintered bearing 10C has a first end 121C and a second end 122C, and has a large diameter part 13C whose outer diameter is larger than that of the first end 121C. The first end 121C is formed in a tapered shape with the outer diameter gradually decreasing from the large diameter part 13C toward the first end 121C. The gradient of this tapered surface (outer inclined surface 123C) is formed to be, for example, 15° (taper angle 30°).
[0045] This sintered bearing 10C is accommodated in an injection mold 60C to form an insert bearing. Specifically, the sintered bearing 10C is pressed toward the fixed mold 62C by the movable mold 63 as the movable mold 63 moves along the parting surface 620. Therefore, even if the height of the sintered bearing 10C varies, the first end 121C is held in a fitted state up to a midway position in the length direction in the recess 64C of the fixed mold 62C. As a result, the inner peripheral surface including the first tapered surface 641C of the recess 64C abuts against the outer inclined surface 123C of the first end 121C of the sintered bearing 10C over the entire circumference. In addition, the end surface of the protruding portion 65 protruding from the inner surface of the movable mold 63 abuts against the end surface of the second end 122C.
[0046] Then, molten resin is injected into the cavity 61 of the clamped injection mold 60C. At this time, injection pressure acts in the cavity 61, but the tip of the first end 121C of the sintered bearing 10C is arranged in a fitted state in the recess 64C of the fixed mold 62C, and the second end 122C abuts on the protruding portion 65. Since the tip of the first end 121C is not exposed in the cavity 61, the injection pressure acts on the outer surface of the sintered bearing 10C except for the tip of the first end 121C. In addition, the parting surface 620 of the mold 60C is formed along the moving direction of the movable mold 63 as shown in FIG. 13, and is therefore formed on the ridge line formed at the intersection between the outer circumferential surface of the exterior part and the end face of the exterior part located on the first end 121C side. For this reason, the appearance of the resin part is hardly affected. Therefore, even if the sintered bearing 10C does not have the bearing hole 11, the same effects as those of the above-described embodiments can be achieved.
[0047] Furthermore, the present invention is not limited to the configuration of the above-described embodiment, and various changes can be made to the details of the configuration without departing from the spirit of the present invention. For example, in the above first embodiment, the outer inclined surface 123 of the first end 121 is accommodated in the recess 64 of the fixed die 62, and the protruding portion 65 of the movable die 63 is abutted against the second end 122. However, this is not limited to the above, and as in the second embodiment, the second tapered surface 651 may be abutted against the tapered surface 111 of the bearing hole 11 on the second end 122 side. In this case, it is possible to reliably prevent the resin material from entering the bearing hole 11 from both the first end 121 and the second end 122.
[0048] In the above embodiments, examples have been shown in which grooves are formed on the end face and outer circumferential surface of the first end portion as well as on the large diameter portion, but instead of the grooves, protrusions may be formed along the axial direction. In addition, it is preferable to form a plurality of these grooves or protrusions at intervals in the circumferential direction, but it is also possible to form only one. Furthermore, in the embodiment, the exterior part is made of a resin part and is insert molded by injection molding, but the present invention can also be applied to an exterior part made of a metal part such as an aluminum alloy and insert molded by casting. In that case, the sintered bearing and the exterior part made of a metal part are integrated by placing the sintered part in a casting mold (molding die) and assembling it (assembling process), and filling the cavity around it with molten metal (molten material) that will become the metal part (filling process).
[0049] In the above embodiment, the sintered part is exemplified as a sintered bearing, and the insert sintered part is exemplified as an insert bearing, but the present invention is not limited to this. The sintered part may be a valve seat, a bush, etc. In other words, the present invention is not limited to sintered bearings, and can be applied to any sintered part, and can be applied to all products in which the sintered part is integrated with an exterior part. For example, the sintered part may be a rectangular plate-shaped sintered part 10D as shown in Fig. 14, in which case it is sufficient that a first end 121D of the sintered part 10D abuts against a protruding part 64D of a fixed die 62D and a second end 122D abuts against a protruding part 65 of a movable die 63. In other words, a sintered part that does not have an outer inclined surface or an inner inclined surface is also within the scope of the present invention. [Explanation of symbols]
[0050] 1. Insert bearings (sintered insert parts) 10, 10A, 10B, 10C Sintered bearings (sintered parts) 10D Sintered Parts 10´ Molded body 11 Bearing hole (through hole) 111 Tapered surface (inner inclined surface) 121,121A,121B,121C,121D 1st end 122,122A,122B,122C,122D 2nd end 123,123C Outside slope 13,13C Large diameter section 14,14A,14B Groove 20 Plastic parts (exterior parts) 21 Bearing holder 40 Molding tool 80 Correction mold 60, 60A, 60C Injection mold (mold) 61 Cavity 62,62A,62C,62D Fixed type 63,63A Movable type 64,64C Recess 641,641C First tapered surface 64A,64D, 65 Protrusion 65A Convex 651 Second tapered surface 66 Bearing retention space
Claims
1. A sintered part having a first end and a second end, and an exterior part integrally formed on an outer periphery of the sintered part, The sintered part is a sintered bearing, The exterior part is made of resin or metal, a parting line is formed on a ridge line formed at an intersection between an outer circumferential surface of the exterior part and an end surface of the exterior part located on the first end side, the resin or the metal protrudes in the axial direction of the sintered bearing at the parting line, The first end of the sintered part has an outer inclined surface that gradually reduces in diameter from the base end toward the end face of the first end, and the base end of the first end is embedded in the exterior part and the tip end protrudes and is exposed from the exterior part.
2. A sintered part having a first end and a second end, and an exterior part integrally molded on an outer periphery of the sintered part, The sintered part is a sintered bearing, The first end portion is exposed at an axial end. The exterior part is made of resin or metal, a parting line is formed on a ridge line formed at an intersection between an outer circumferential surface of the exterior part and an end surface of the exterior part located on the first end side, the resin or the metal protrudes in the axial direction of the sintered bearing at the parting line, The sintered part has a through hole penetrating the first end and the second end, and the through hole is provided with an inner inclined surface that gradually increases in diameter toward an end face of the second end, An insert sintered part, wherein the exterior part has an inclined surface formed thereon that is continuous with the inner inclined surface.
3. 2. The sintered insert part according to claim 1, wherein the sintered bearing is a pivot bearing formed in a solid shape.
4. The sintered insert part according to claim 1 , wherein the sintered part comprises the sintered bearing having one through hole penetrating the first end and the second end.
5. The insert sintered part according to any one of claims 1 to 4, characterized in that a groove or a protrusion is formed on an outer periphery of a portion of the sintered part where the exterior part is provided.
6. The insert sintered part according to claim 1, characterized in that a large diameter portion having an outer diameter larger than that of the first end portion is formed on the outer periphery of the sintered part, and the large diameter portion is formed with at least one of a groove or a protrusion along the axial direction on the outer periphery surface of the large diameter portion and a groove or a protrusion along the radial direction on the end surface of the large diameter portion.
Citation Information
Patent Citations
Insert metal fitting
JP1997193192A
Sintered product
JP2003159720A
Sintered product, method for forming sintered product, and forming die
JP2003193113A
Method for manufacturing thrust bearing for turbocharger, and thrust bearing for turbocharger
JP2015010249A