Multi-core optical fiber preform, method for manufacturing multi-core optical fiber preform, and method for manufacturing multi-core optical fiber

The multi-core optical fiber preform's design, featuring a core-less or single-core distal end, facilitates accurate coating thickness detection by reducing light scattering, thereby improving manufacturing precision and efficiency.

JP7553692B2Active Publication Date: 2024-09-18FUJIKURA LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023500949
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-02-22
Filing Date
2022-02-18
Publication Date
2024-09-18
Estimated Expiration
2042-02-18

AI Technical Summary

Technical Problem

In multi-core optical fibers, accurately confirming the uneven thickness of the coating is challenging due to light scattering from multiple cores, which complicates the detection process.

Method used

The multi-core optical fiber preform is designed with a distal end connecting portion that lacks or has only one core rod, allowing for the confirmation of coating unevenness with high accuracy by minimizing light scattering during the detection process.

Benefits of technology

This design enables precise confirmation of coating thickness deviations with reduced light scattering, enhancing manufacturing accuracy and efficiency of multi-core optical fibers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007553692000009
    Figure 0007553692000009
  • Figure 0007553692000010
    Figure 0007553692000010
  • Figure 0007553692000015
    Figure 0007553692000015
Patent Text Reader

Abstract

This multi-core optical fiber base material comprises: a rod-like main clad body in which at least one main inner hole is formed; a plurality of main core rods which are inserted the main inner hole; and a tip end contiguous part which is provided contiguously at one end of the main clad body. The tip end contiguous part is a glass rod which has no core rods or has a single core rod. The tip end contiguous part is, for example, a solid glass rod.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a multi-core optical fiber preform, a manufacturing method of a multi-core optical fiber preform, and a manufacturing method of a multi-core optical fiber. This application claims priority to Patent Application No. 2021-026466, filed in Japan on February 22, 2021, the contents of which are incorporated herein by reference. [Background technology]

[0002] The thickness of the coating of an optical fiber affects the microbending characteristics, temperature characteristics, and the like of the optical fiber. Therefore, when manufacturing an optical fiber, asymmetry in the coating thickness (hereinafter referred to as asymmetry in coating layers) may be checked. Asymmetry in coating layers can be checked by forward scattered light obtained by irradiating the side surface of the optical fiber with laser light (see, for example, Patent Document 1). The positions of light and dark in the forward scattered light are affected by the distribution of the coating thickness. Therefore, asymmetry in the coating can be checked based on the positions of light and dark in the forward scattered light. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Publication No. 9-126946 Summary of the Invention [Problem to be solved by the invention]

[0004] In recent years, with an increase in communication traffic, multi-core optical fibers have been attracting attention as optical fibers capable of increasing transmission capacity. However, in the case of a multi-core optical fiber, it may be difficult to accurately check the uneven thickness of the coating.

[0005] An object of the present invention is to provide a multi-core optical fiber preform, a manufacturing method of a multi-core optical fiber preform, and a manufacturing method of a multi-core optical fiber, which are capable of accurately checking uneven thickness of a coating. [Means for solving the problem]

[0006] A multi-core optical fiber preform according to a first aspect of the present invention comprises a rod-shaped main clad body having one or more main inner holes, a plurality of main core rods inserted into the main inner holes, and a tip connection portion connected to one end of the main clad body, wherein the tip connection portion is a glass rod having no core rod or one core rod.

[0007] The multi-core optical fiber preform includes a tip connection portion that has no core rod or has one core rod. The tip connection portion has a smaller number of cores than a glass material unit (a unit having a main cladding body and a main core rod). The tip connection portion can produce a coated wire with one or less cores, so that uneven thickness of the coating can be checked under conditions with little light scattering. Therefore, uneven thickness of the coating can be checked with high accuracy.

[0008] The plurality of main core rods may include a first core rod and a second core rod having a dimension shorter than an axial dimension of the main clad body, and the first core rod may be disposed at the center of the main clad body.

[0009] The tip connection portion may be a solid glass rod.

[0010] The tip connecting portion may include a constant diameter portion having a constant outer diameter, and a reduced diameter portion that protrudes from the tip of the constant diameter portion while reducing in diameter, and the axial length of the constant diameter portion may be greater than or equal to the axial length of the reduced diameter portion.

[0011] The tip connecting portion may include a constant diameter portion having a constant outer diameter and a reduced diameter portion that protrudes from the tip of the constant diameter portion while reducing in diameter, and the axial length of the constant diameter portion may be less than the axial length of the reduced diameter portion.

[0012] A manufacturing method of a multi-core optical fiber preform according to a second aspect of the present invention includes a preparation step of preparing a glass material unit in which a plurality of main core rods are inserted into one or a plurality of main inner holes formed in a rod-shaped main clad body, a glass rod connecting step of butt-jointing a glass rod having no core rod or one core rod to one end of the glass material unit, and a glass rod cutting step of separating the remaining part of the glass rod by fusing, while leaving a part of the glass rod as a tip connecting part connected to the glass material unit.

[0013] According to the above-mentioned manufacturing method, since the tip connecting portion does not have a core rod or has one core rod, the number of cores in the covered wire is small, so that uneven thickness of the covering can be checked under conditions with little light scattering. Therefore, uneven thickness of the covering can be checked accurately.

[0014] The main core rod includes a first core rod and a second core rod having a dimension shorter than the axial dimension of the main clad body, and in the preparation step, the glass material unit is prepared in the main inner hole, with the first core rod inserted at the center of the main clad body and the second core rod inserted around the first core rod so as to have a gap between an end face of the main clad body and the second core rod, and after the preparation step, the gap is heated and the main clad body is reduced in diameter to close the gap.

[0015] The tip connection portion may be a solid glass rod.

[0016] The tip connecting portion may be a single core unit including a rod-shaped tip clad body having a tip inner hole formed therein, and a tip core rod inserted into the tip inner hole.

[0017] In the glass rod cutting process, the tip connecting portion is formed to have a constant diameter portion having a constant outer diameter and a reduced diameter portion protruding from the tip of the constant diameter portion while reducing in diameter, and the axial length of the constant diameter portion may be equal to or greater than the axial length of the reduced diameter portion.

[0018] In the glass rod cutting process, the tip connecting portion may be formed to include a constant diameter portion having a constant outer diameter and a reduced diameter portion protruding from the tip of the constant diameter portion while reducing in diameter, and the axial length of the constant diameter portion may be less than the axial length of the reduced diameter portion.

[0019] In the manufacturing method of a multi-core optical fiber according to a third aspect of the present invention, a multi-core optical fiber is formed by drawing the multi-core optical fiber preform obtained by the manufacturing method of a multi-core optical fiber preform. Effect of the Invention

[0020] According to the present invention, it is possible to provide a multi-core optical fiber preform capable of accurately checking uneven thickness of a coating, a manufacturing method of a multi-core optical fiber preform, and a manufacturing method of a multi-core optical fiber. [Brief description of the drawings]

[0021] [Figure 1] 1 is a cross-sectional view taken along an axial direction of a multi-core optical fiber preform according to a first embodiment. [Diagram 2] 1A to 1C are process diagrams illustrating a method for manufacturing a multi-core optical fiber preform. [Diagram 3] FIG. 3 is a process diagram continuing from FIG. [Figure 4] FIG. 4 is a process diagram continuing from FIG. [Diagram 5] FIG. 5 is a process diagram continuing from FIG. [Figure 6] FIG. 6 is a process diagram continuing from FIG. [Figure 7] FIG. 7 is a process diagram continuing from FIG. [Figure 8] FIG. 8 is a process diagram continuing from FIG. [Figure 9] 2 is a cross-sectional view perpendicular to the axial direction of the multi-core optical fiber preform. FIG. [Figure 10] 1 is a configuration diagram showing an example of a manufacturing apparatus for a multi-core optical fiber. [Figure 11] 4 is a schematic diagram showing a configuration of a first thickness deviation detection section. FIG. [Figure 12] 6 is a cross-sectional view taken along the axial direction of a multi-core optical fiber preform according to a second embodiment. FIG. [Figure 13] 11 is a cross-sectional view taken along the axial direction of a multi-core optical fiber preform according to a third embodiment. FIG. [Figure 14] 14 is a process diagram illustrating a method for manufacturing the multi-core optical fiber preform of FIG. 13. [Figure 15] 14 is a process diagram illustrating a method for manufacturing the multi-core optical fiber preform of FIG. 13. [Figure 16] 1 is a photograph showing an example of forward scattered light when a single-core coated wire is irradiated with laser light. [Figure 17] 1 is a photograph showing an example of forward scattered light when a multi-core coated wire is irradiated with laser light. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0022] Hereinafter, a multi-core optical fiber preform, a manufacturing method of a multi-core optical fiber preform, and a manufacturing method of a multi-core optical fiber according to embodiments will be described with reference to the drawings.

[0023] (First embodiment) [Multi-core optical fiber preform] FIG. 1 is a cross-sectional view along the axial direction of a multi-core optical fiber preform 10 (hereinafter simply referred to as the optical fiber preform 10) according to a first embodiment. The optical fiber preform 10 includes a main cladding body 1 , a plurality of main core rods 2 , a tip connecting portion 3 , and a dummy tube 13 .

[0024] The main clad body 1 is formed in a cylindrical (rod-like) shape. The main clad body 1 is made of glass. The main clad body 1 is, for example, an integrally molded product made of quartz glass. A plurality of main inner holes 4 are formed in the main clad body 1. The main inner holes 4 are formed along the axial direction of the main clad body 1. The first end 1a is an end of the main clad body 1 on the side where the tip connecting portion 3 is provided. The second end 1b is an end face of the main clad body 1 opposite to the first end 1a. Possible shapes of the first end 1a and the second end 1b include, for example, an end face shape and a non-end face shape.

[0025] The main core rod 2 is formed in a cylindrical (rod-like) shape. The main core rod 2 includes a region having a higher refractive index than the main clad body 1. The main core rod 2 may be made of glass (e.g., quartz glass) partially doped with a refractive index increasing dopant (germanium, phosphorus, aluminum, titanium, etc.) or glass (e.g., quartz glass) partially doped with a refractive index decreasing dopant (boron, fluorine, etc.). The main core rod 2 is inserted into the main bore 4. The main clad body 1 and the multiple main core rods 2 constitute a "glass material unit U1."

[0026] The tip connecting portion 3 is made of glass (e.g., quartz glass). The tip connecting portion 3 is connected to the first end 1a (one end) of the main clad body 1 by welding. The tip connecting portion 3 is coaxial with the main clad body 1. The tip connecting portion 3 closes the openings of all of the main bores 4 of the main clad body 1. The outer diameter of the tip connecting portion 3 is preferably the same as the outer diameter of the main clad body 1. The tip connecting portion 3 is, for example, a solid glass rod. Since the tip connecting portion 3 is solid, it does not have a core rod (i.e., the number of core rods is zero). The refractive index of the tip connecting portion 3 may be approximately the same as the refractive index of the main clad body 1. As described later, the number of core rods held in the tip continuous portion may be one. That is, the tip continuous portion has one core rod, or the tip continuous portion does not have a core rod.

[0027] The tip connecting section 3 comprises a constant diameter section 5 and a reduced diameter section 6. The constant diameter section 5 is a section including an end section connected to the first end 1a of the main cladding body 1. The constant diameter section 5 is formed in a cylindrical (rod-like) shape. The outer diameter of the constant diameter section 5 is constant. The reduced diameter section 6 protrudes from the tip 5a of the constant diameter section 5 while decreasing in diameter. The reduced diameter section 6 is formed in a tapered shape (for example, a cone shape) that tapers toward the tip.

[0028] The axial length of constant diameter portion 5 is defined as A1. The axial length of reduced diameter portion 6 is defined as A2. Length A1 of constant diameter portion 5 may be equal to or greater than length A2 of reduced diameter portion 6. Length A1 of constant diameter portion 5 may be less than length A2 of reduced diameter portion 6. The dummy tube 13 is connected to the second end 1b of the glass material unit U1. The optical fiber preform 10 may be configured without the dummy tube 13.

[0029] [Manufacturing method of multi-core optical fiber preform] A method for producing the optical fiber preform 10 will be described with reference to Fig. 2 to Fig. 8. Note that in the drawings used in the following description, the scale may be changed so that members are of a recognizable size.

[0030] The manufacturing method of the optical fiber preform shown here includes (1) a hole drilling step, (2) a cleaning step, (3) a preparation step, (4) a dummy tube connecting step, (5) a sealing step, (6) a glass rod connecting step, and (7) a glass rod cutting step. Each step will be described below.

[0031] (1) Hole drilling process As shown in Fig. 2, a plurality of through holes 14 are formed in the main clad body 1 using a drill tool or the like. The through holes 14 are formed in the main clad body 1 along the axial direction. Both ends of the through holes 14 are opened to end faces in the axial direction of the main clad body 1. The through holes 14 are formed at a plurality of locations spaced apart in the axial direction so as to surround the central axis of the main clad body 1, for example.

[0032] (2) Cleaning process Since cutting fluid used when drilling the through hole 14 and metal powder from the drill tool may remain inside the through hole 14, the outer surface of the main clad body 1 and the inner surface of the through hole 14 are cleaned using a cleaning liquid such as pure water, alcohol (ethanol), or alkaline liquid.

[0033] In the cleaning process, the inner surface of the through hole 14 can also be treated by etching. For example, foreign matter (such as the metal powder) attached to microcracks on the inner surface of the through hole 14 can be removed by etching. The etching can be wet etching or dry etching. In the wet etching, an etching solution containing hydrofluoric acid, for example, BHF (buffered hydrofluoric acid) in which hydrofluoric acid and ammonium fluoride are mixed, can be used. In the dry etching, a fluoride gas such as SF6 (sulfur hexafluoride) gas or C2F6 (ethane hexafluoride) gas can be used as an etching gas. In the dry etching, for example, an etching gas is introduced into the through hole 14 while the main clad body 1 is heated to 1200°C or higher.

[0034] (3) Preparation process As shown in Fig. 3, a glass material unit U1 is prepared. A glass rod 2 serving as a core (hereinafter referred to as a main core rod) is inserted into each of a plurality of through holes 14 in the main clad body 1. In this way, a glass material unit U1 having a configuration in which the main core rod 2 is inserted into each of a plurality of through holes 14 in the main clad body 1 is obtained.

[0035] The main core rod 2 is preferably cleaned in advance with a cleaning liquid such as water, alcohol, an alkaline liquid, etc. The main core rod 2 may be etched to remove dirt on its surface. The preparation step is preferably carried out in a room with a high degree of cleanliness, which can prevent dust, dirt, etc., which cause transmission loss, from adhering to the main core rod 2.

[0036] A glass rod for core identification marker (not shown) may be inserted into one or more of the multiple through holes 14 in the main clad body 1 in place of the main core rod 2. The glass rod for core identification marker is, for example, a glass rod having a refractive index different from that of both the main clad body 1 and the main core rod 2.

[0037] The outer diameter of the main core rod 2 is, for example, 80 to 99% of the inner diameter of the through hole 14. In order to stably ensure the core position accuracy in the optical fiber, the outer diameter of the main core rod 2 is more preferably 90 to 99%, and further preferably 95 to 99%, of the inner diameter of the through hole 14.

[0038] (4) Dummy tube connection process As shown in Fig. 4, dummy tubes 12 and 13 are connected to both ends of the glass material unit U1 by welding or the like. The dummy tubes 12 and 13 are cylindrical tubes made of, for example, quartz glass. To fuse the dummy tubes 12 and 13 to the main clad body 1, the ends of the glass material unit U1 are heated by a flame 16 (for example, an oxyhydrogen flame) or the like.

[0039] The first dummy tube 12 is connected to the glass material unit U1 by abutting its axial end face on one axial end face of the glass material unit U1. The second dummy tube 13 is connected to the glass material unit U1 by abutting its end face on the other axial end face of the glass material unit U1. The dummy tubes 12 and 13 can be held by a chuck 20. In this embodiment, the dummy tube connecting step is performed after the preparation step, but the dummy tube connecting step may be performed before the preparation step.

[0040] (5) Sealing process As shown in Fig. 5, one end of the glass material unit U1 (hereinafter referred to as the first end, the end on the right in Fig. 5) is heated using a flame 16 (e.g., an oxyhydrogen flame) or the like to reduce its diameter, thereby blocking (i.e., sealing) the opening of the through-hole 14. As a result, the first dummy tube 12 on the first end side of the glass material unit U1 is separated from the glass material unit U1 by melting. The use of the dummy tube 12 makes it easy to melt the tube. The means for heating the glass material unit U1 is not limited to the flame 16, but an electric furnace or the like may also be used.

[0041] The first end of the glass material unit U1 in a state in which the opening of the through hole 14 is sealed is referred to as a first end sealing portion 17. In the first end sealing portion 17, the first end of the main clad body 1 is reduced in diameter together with the first end of the main core rod 2 to be solidified. The first end sealing portion 17 is formed, for example, in a tapered shape (for example, a conical shape).

[0042] A vacuum pump may be connected to the dummy tube 13 to reduce the pressure inside the through hole 14. This can reduce voids (air bubbles) in the glass material unit U1.

[0043] (6) Glass rod connection process As shown in Fig. 6, an end of a glass rod 15 is fused and integrated with a first end sealing portion 17 of a glass material unit U1. The glass rod 15 is made of, for example, quartz glass. The glass rod 15 has a solid structure. The glass rod 15 is formed in a cylindrical shape. The outer diameter of the glass rod 15 is preferably the same as the outer diameter of the main clad body 1.

[0044] The glass rod 15 is butted against an end face of a first end (one end) of the glass material unit U1, and is coaxially aligned with the glass material unit U1, fused and integrated. The glass rod 15 is connected to the first end of the glass material unit U1. The glass rod 15 closes the openings of all the through holes 14. As a result, the glass rod 15 is connected to the first end of the glass material unit U1 (see FIG. 7). The through holes 14 become the main inner hole 4 (see FIG. 7).

[0045] 7, if necessary, a soldering iron 18 can be applied to the outer peripheral surface of the connection portion between the glass rod 15 and the glass material unit U1 to reduce the step between the glass rod 15 and the glass material unit U1, thereby making it possible to prevent breakage of the optical fiber or glass wire during drawing.

[0046] (7) Glass rod cutting process As shown in FIG. 8, the glass rod 15 is heated at a longitudinal midpoint using a flame 16 (for example, an oxyhydrogen flame) or the like, and the glass rod 15 is cut by melting. A portion of the glass rod 15 in the longitudinal direction remains as the tip connected portion 3 connected to the glass material unit U1. In this way, the optical fiber preform 10 shown in Fig. 1 is obtained. The remaining portion of the glass rod 15 in the longitudinal direction is separated from the tip connected portion 3.

[0047] In this process, the second end of the glass material unit U1 (for example, the left end of the optical fiber preform 10 in FIG. 8) may be sealed with the interior of the glass material unit U1 depressurized by a depressurizing pump. This allows the manufacture of an optical fiber with fewer voids (air bubbles). If the second end of the glass material unit U1 is not sealed, the optical fiber preform 10 may be heated and melt-spun by the heating unit 101 in the thickness deviation checking process and this manufacturing process described below with the interior of the glass material unit U1 depressurized by a depressurizing pump.

[0048] Fig. 9 is a cross-sectional view showing an example of the optical fiber preform 10. Fig. 9 shows a cross section perpendicular to the axial direction of the optical fiber preform 10. The optical fiber preform 10 in this example has four main holes 4, which are arranged at equal intervals around the central axis of the main cladding body 1.

[0049] [Manufacturing method of multi-core optical fiber] A method for manufacturing a multi-core optical fiber using the optical fiber preform 10 will be described with reference to FIG. 10 is a configuration diagram showing a manufacturing apparatus 100 for a multi-core optical fiber (hereinafter, simply referred to as the manufacturing apparatus 100). FIG.

[0050] As shown in FIG. 10, manufacturing apparatus 100 includes a heating section 101, a cooling section 102, a first coating section 103, a first hardening section 104, a first thickness deviation detection section 105, a second coating section 106, a second hardening section 107, a second thickness deviation detection section 108, a pulley 109, a take-up section 110, and a winding section 111. The first curing section 104 includes one or more UV lamps 104a. The second curing section 107 includes one or more UV lamps 107a.

[0051] The manufacturing method of the multi-core optical fiber according to the embodiment includes (1) a thickness deviation checking step, and (2) a main manufacturing step.

[0052] (1) Thickness unevenness confirmation process The optical fiber preform 10 is heated by the heating section 101 and melt spun. That is, the tip portion of the optical fiber preform 10 (the tip portion of the tip connecting section 3) is heated to reduce the glass viscosity (soften), and the softened glass is drawn. Since the tip connecting section 3 is a solid glass rod (see FIG. 1), the drawn glass is a glass wire 21 that does not have a core. The glass wire 21 is cooled by the cooling section 102.

[0053] The first coating unit 103 forms a first coating by applying (coating) a coating material such as a urethane acrylate resin to the outer periphery of the glass wire 21. The glass wire 21 on which the first coating has been formed is called an intermediate body 22 (coated wire). The preform 22 is irradiated with UV light by the UV lamps 104a of the first curing section 104, thereby curing the first coating.

[0054] 11, the first thickness deviation detection unit 105 includes a light-emitting unit 112 and a light-receiving unit 113. The light-emitting unit 112 irradiates the intermediate body 22 with laser light L1 (test light). The light-receiving unit 113 receives forward scattered light L2. The first thickness deviation detection unit 105 can confirm deviation in thickness (thickness deviation) of the first coating based on the forward scattered light L2.

[0055] As shown in Fig. 10, since intermediate body 22 does not have a core, scattering of laser light due to multiple cores does not occur. Therefore, it is easy to confirm uneven thickness of the first coating based on the positions of light and dark in the forward scattered light. If uneven thickness of the first coating is confirmed, it is possible to suppress the uneven thickness by adjusting the coating conditions in first coating section 103.

[0056] The second coating unit 106 forms a second coating by applying (coating) a coating material such as a urethane acrylate resin to the outer periphery of the intermediate body 22. The intermediate body 22 on which the second coating has been formed is called a coated glass wire 23 (coated wire). The UV lamps 107a of the second curing section 107 irradiate the coated glass wire 23 with UV light to cure the second coating.

[0057] Second thickness deviation detection unit 108 includes a light-emitting unit (not shown) and a light-receiving unit (not shown). Second thickness deviation detection unit 108 may have a configuration similar to that of first thickness deviation detection unit 105 (see FIG. 11). The light-emitting unit irradiates laser light (test light) onto coated glass wire 23. The light-receiving unit receives forward scattered light. Second thickness deviation detection unit 108 can check the thickness deviation of the second coating based on the forward scattered light.

[0058] Since the coated glass wire 23 does not have a core, scattering of the laser light due to multiple cores does not occur. Therefore, uneven thickness of the second coating can be easily confirmed based on the positions of light and dark in the forward scattered light. If uneven thickness of the second coating is confirmed, it can be suppressed by adjusting the coating conditions in the second coating unit 106.

[0059] The pulley 109 changes the direction of the coated glass wire 23. The take-up unit 110 is, for example, a take-up capstan and determines the drawing speed. The winding unit 111 winds up the coated glass wire 23.

[0060] (2) Main manufacturing process When the tip connecting portion 3 is consumed by drawing, the drawing end is transferred to the glass material unit U1 (see FIG. 1). The bare optical fiber drawn from the glass material unit U1 has a first coating formed by the first coating portion 103, and the first coating is hardened by the first hardening portion 104, becoming an optical fiber bare wire intermediate body.

[0061] The optical fiber intermediate body has a second coating formed by the second coating section 106 and the second coating hardened by the second hardening section 107 to become an optical fiber. As shown in Fig. 1, the main clad body 1 of the glass material unit U1 becomes the clad of the optical fiber. The main core rod 2 becomes the core of the optical fiber. Since there are multiple main core rods 2, the optical fiber is a multi-core optical fiber.

[0062] [Effects of the optical fiber preform and the method for manufacturing a multi-core optical fiber according to the embodiment] The optical fiber preform 10 of this embodiment includes a tip continuous portion 3 in which no core rod is provided or in which one core rod is provided. The tip continuous portion 3 has a smaller number of cores than the glass material unit U1. The tip continuous portion 3 can produce an intermediate body 22 and a coated glass wire 23 in which the number of cores is one or less. Therefore, the thickness deviation detection units 105, 108 can check the thickness deviation of the coating under conditions with little light scattering. Therefore, the thickness deviation of the coating can be checked with high accuracy.

[0063] Since the tip connecting portion 3 of the optical fiber preform 10 is a solid glass rod, the intermediate body 22 and the coated glass wire 23 without a core can be produced in the thickness deviation checking step. Therefore, the thickness deviation detecting units 105 and 108 can check the thickness deviation of the coating under conditions with less light scattering.

[0064] According to the manufacturing method, in order to draw the optical fiber preform 10 having the tip continuous portion 3, the intermediate 22 and the coated glass wire 23 each having one or less cores can be manufactured prior to the main manufacturing process for manufacturing the multi-core optical fiber. Therefore, the uneven thickness detection units 105 and 108 can check the uneven thickness of the coating under conditions with little light scattering. Therefore, the uneven thickness of the coating can be checked with high accuracy.

[0065] In the above-described manufacturing method, since the tip connecting portion 3 is a solid glass rod, the intermediate body 22 and the covered glass wire 23 having no core can be produced in the thickness deviation checking step. Therefore, the thickness deviation detection units 105, 108 can check the thickness deviation of the coating under conditions with less light scattering.

[0066] The tip connecting portion 3 includes a constant diameter portion 5 having a constant outer diameter, and a reduced diameter portion 6 that protrudes from a tip 5a of the constant diameter portion 5 while reducing in diameter. When the length A1 of the constant diameter portion 5 is equal to or greater than the length A2 of the reduced diameter portion 6, the intermediate body 22 and the covered glass wire 23 are provided with a sufficient length for checking for uneven thickness. This allows for more accurate checking of uneven thickness of the coating.

[0067] The length A1 of the constant diameter portion 5 may be less than the length A2 of the reduced diameter portion 6. In this case, the time required for the step of checking for thickness deviation by irradiating the coated wire with laser light (thickness deviation checking step) can be shortened, and the manufacturing process can be started earlier, thereby improving the manufacturing efficiency of the multi-core optical fiber.

[0068] Second embodiment [Multi-core optical fiber preform] 12 is a cross-sectional view along the axial direction of the optical fiber preform 210 of the second embodiment. The same components as those in the optical fiber preform 10 of the first embodiment (see FIG. 1) are denoted by the same reference numerals and will not be described.

[0069] The optical fiber preform 210 includes a main cladding body 1, a plurality of main core rods 2, a tip connecting portion 203, and a dummy tube 13. The optical fiber preform 210 differs from the optical fiber preform 10 shown in FIG. 1 in that the tip connecting portion 203 is used instead of the tip connecting portion 3.

[0070] The tip connecting portion 203 is a single core unit equipped with a tip clad body 204 and one tip core rod 205 . The outer shape of the tip cladding body 204 is similar to the outer shape of the tip connecting portion 3 shown in Figure 1. The tip cladding body 204 is made of glass (e.g., quartz glass). One tip inner hole 206 is formed in the tip cladding body 204. The tip inner hole 206 is formed in the center of the tip cladding body 204 along the axial direction of the tip cladding body 204.

[0071] The tip core rod 205 is formed in a cylindrical shape (rod shape). The tip core rod 205 is made of glass (for example, quartz glass). The tip core rod 205 includes a region having a higher refractive index than the tip cladding body 204. The tip core rod 205 is inserted into the tip inner hole 206.

[0072] The tip connecting portion 203 is connected to the first end 1a (one end) of the main clad body 1 by welding. The tip connecting portion 203 is coaxial with the main clad body 1. The tip connecting portion 203 blocks all of the main inner holes 4 of the main clad body 1. The outer diameter of the tip connecting portion 203 is preferably the same as the outer diameter of the main clad body 1. The tip connecting portion 203 includes one core rod (tip core rod 205), and therefore the number of core rods held is one.

[0073] By drawing the optical fiber preform 210, a multi-core optical fiber can be manufactured in the same manner as the optical fiber preform 10 of the first embodiment (see FIG. 10).

[0074] Since the optical fiber preform 210 includes the tip continuous portion 203 that has one core rod, an intermediate body and a coated glass wire having one or less cores can be produced in the thickness deviation confirmation step. Therefore, the thickness deviation detection unit can check the thickness deviation of the coating under conditions with little light scattering. Therefore, the thickness deviation of the coating can be checked with high accuracy.

[0075] Third embodiment [Multi-core optical fiber preform] 13 is a cross-sectional view along the axial direction of an optical fiber preform 310 of the third embodiment. The same components as those in the optical fiber preform 10 of the first embodiment (see FIG. 1) are denoted by the same reference numerals and will not be described.

[0076] The optical fiber preform 310 includes a main cladding body 31, a plurality of main core rods 32, a tip connecting portion 301, and a dummy tube 13. The optical fiber preform 310 differs from the optical fiber preform 10 shown in FIG. 1 in the configuration of the glass material unit U2 and the position where the tip connecting portion 301 is provided.

[0077] The multiple main core rods 32 include a first core rod 32a and a second core rod 32b. The axial dimension M1 of the first core rod 32a is the same as the axial dimension MA of the main clad body 31. The axial dimension M2 of the second core rod 32b is shorter than the axial dimension MA of the main clad body 31. In addition, the axial dimension M2 of the second core rod 32b is shorter than the axial dimension M1 of the first core rod 32a. The first core rod 32a is disposed in the center of the main clad body 31. For example, the main core rod 2 shown in Fig. 9 corresponds to the second core rod 32b of this embodiment, and the first core rod 32a is configured to be surrounded by four second core rods 32b.

[0078] The tip connecting portion 301 includes a constant diameter portion 302 and a reduced diameter portion 303. The length relationship between the constant diameter portion 302 and the reduced diameter portion 303 is the same as in the first embodiment. The tip connecting portion 301 does not have a core rod.

[0079] The tip connecting portion 301 is connected to the first end 31a (end face) of the main clad body 31 by welding. The tip connecting portion 301 is coaxial with the main clad body 31. The tip connecting portion 301 closes the main inner bore 4 of the first core rod 32a. The outer diameter of the tip connecting portion 301 is slightly larger than the outer diameter of the first core rod 32a. The tip of the main cladding body 31 is tapered so that the diameter decreases toward the first end 31a.

[0080] In the embodiment, the axial dimension M1 of the first core rod 32a is the same as the axial dimension MA of the main clad body 31, but the dimension M1 of the first core rod 32a may be shorter than the dimension MA of the main clad body 31.

[0081] According to the multi-core optical fiber preform 310 of this embodiment, the outer diameter of the tip continuous portion 301 is smaller than those of the multi-core optical fiber preform 10 in Fig. 1 and the multi-core optical fiber preform 210 in Fig. 12, and therefore the heat capacity of the tip continuous portion 301 is smaller. As a result, the tip continuous portion 301 is more likely to melt. Therefore, when the multi-core optical fiber preform 310 in Fig. 13 is placed in a drawing device and the tip continuous portion 301 is heated, the time required for the step of dropping the tip continuous portion 301 of the multi-core optical fiber preform 310 (dropping step) can be shortened. Therefore, particularly when the length of the first core rod 32a is long in the axial direction, the time required from the dropping step to the main drawing step of paying out the fiber to be the product from the multi-core optical fiber preform 310 can be shortened.

[0082] [Manufacturing method of multi-core optical fiber preform] A method for manufacturing the optical fiber preform 310 will be described with reference to Fig. 14 and Fig. 15. In the drawings used in the following description, the scale may be changed so that the members are of a recognizable size. The description of the same steps as those in the first embodiment will be omitted.

[0083] In the drilling step, through holes 14 are formed at the center of main clad body 31 and at a plurality of locations spaced apart in the axial direction so as to surround the center of main clad body 31 . The cleaning process is the same as in the first embodiment.

[0084] In the preparation step, a glass material unit U2 is prepared as shown in Fig. 14. A glass rod 32a (hereinafter referred to as a first core rod) and a glass rod 32b (hereinafter referred to as a second core rod) serving as cores are inserted into each of a plurality of through holes 14 in the main clad body 31. Specifically, the first core rod 32a is inserted into the through hole (main inner hole) 14 formed in the center of the main clad body 31, and the second core rod 32b is inserted into the through hole 14 formed so as to surround the center of the main clad body 31. The axial dimension M1a of the first core rod 32a is the same as the axial dimension MA of the main clad body 31. In this embodiment, the axial dimension M1a of the first core rod 32a is the same as the axial dimension MA of the main clad body 31, but the dimension M1a of the first core rod 32a may be shorter than the dimension MA of the main clad body 31. The axial dimension M2a of the second core rod 32b is shorter than the axial dimension MA (the dimension of the through hole 14) of the main clad body 31. In addition, the axial dimension M2a of the second core rod 32b is shorter than the axial dimension M1a of the first core rod 32a. Therefore, a gap S is formed between the end face of the main clad body 31 and the second core rod 32b. In addition, no gap is formed on the second end 31b side of the through hole 14 through which the second core rod 32b is inserted. In this manner, a glass material unit U2 is obtained in which the first core rod 32a and the second core rod 32b are inserted into the plurality of through holes 14 of the main clad body 31, respectively.

[0085] Thereafter, the dummy tube connecting step is carried out in the same manner as in the first embodiment. Next, while still in a vacuum state, the following processing is carried out in the sealing process. 15, tip connecting portion 301 has an outer diameter slightly smaller than the outer diameter of main clad body 31. With this configuration, it becomes possible for the outer diameter of main clad body 31 and the outer diameter of tip connecting portion 301 to be substantially the same when gap S is crushed in the sealing process described below. Also, the outer diameter MS3 of the main clad body 31 in Fig. 15 on the tip connecting portion 301 side may be equal to the outer diameter MS1 of the main clad body 31 in Fig. 13 on the tip connecting portion 301 side. In this case, the gap S is eliminated in the state of Fig. 14, and the tip connecting portion 301 is provided. Alternatively, the outer diameter MS2 of the main cladding 31 in Fig. 14 may be the largest, followed by the outer diameter MS3 of the main cladding 31 in Fig. 15, and the outer diameter MS1 of the main cladding 31 in Fig. 13, which is the smallest (MS2>MS3>MS1). In this case, as shown in Fig. 14, the dummy tube 12 is melted while the gap S of the through hole 14 is provided. At this time, the gap S in the vicinity of the melted portion is slightly collapsed. Thereafter, in the sealing process or the glass dummy connection process, a vacuum is drawn to collapse the gap S, thereby forming the optical fiber preform 310 in Fig. 13. However, by timing the evacuation so that it occurs halfway through when the dummy tube 12 is melted after the gap S is created, it is possible to create a structure in which the gap is completely eliminated, as shown in Figure 13.

[0086] For example, if the outer diameter of main clad body 31 is φ80 mm, the inner diameter of through hole 14 is φ20 mm, and four gaps S are collapsed, the outer diameter of main clad body 31 after collapse is φ70(2×√((80 / 2)^2×π-4×(20 / 2)^2×π)) mm. In other words, if the outer diameter of main clad body 31 is φ1 and the inner diameter of through hole 14 is φ2, the outer diameter of main clad body 31 after collapse can be expressed as 2×√((φ1 / 2)^2-Σi(φ2 / 2)^2) (Σ is i=1 to N). That is, the outer diameter of the tip connecting portion 301 is adjusted so that it coincides with the outer diameter of the main cladding body 31 after the gap S is crushed. In this embodiment, the tip connecting portion 301 is welded to the tip of the main clad body 31. Alternatively, after a thin rod (tip connecting portion) is attached to the tip of the main clad body 31, the tip of the rod may be melted to form the tip connecting portion.

[0087] As shown in Fig. 15, in the sealing process, the gap S is evacuated to a vacuum. Next, the area of ​​the main clad 31 including the gap S is heated by a flame 16 or the like, and the main clad 31 is reduced in diameter to close the gap S. As a result, when the gap S is collapsed, the outer diameter of the main clad 31 and the outer diameter of the tip continuous portion 301 become substantially the same. In this manner, the optical fiber preform 310 shown in Fig. 13 is formed.

[0088] By drawing the optical fiber preform 310, a multi-core optical fiber can be manufactured in the same manner as the optical fiber preform 10 of the first embodiment (see FIG. 10).

[0089] The optical fiber preform 310 of this embodiment can also provide the same effects as those of the first embodiment. Even if the first core rod 32a is melted and cut in the sealing step shown in Fig. 15, and the first core rod 32a protruding from the second core rod 32b becomes the tip-connected portion, it is easy to check for uneven thickness because there is only one core at the tip of the glass material unit U2. In addition, since the tip of the glass material unit U2 has the same configuration as the single-core fiber, it is possible to easily check for uneven thickness in this region. In addition, since the dimension M2 of the second core rod 32b is shorter than the dimension MA of the through hole 14, the gap S is easily collapsed by melting while drawing a vacuum inside the hole of the main cladding body 31. That is, the outer diameter of the base material is smaller than in a region where rods are inserted in all the through holes 14. As a result, the time required for melting is reduced compared to a region where rods are inserted in all the through holes 14, making melting easier.

[0090] Figure 16 is a photograph showing an example of forward scattered light when a laser beam is irradiated onto a single-core coated wire, and Figure 17 is a photograph showing an example of forward scattered light when a laser beam is irradiated onto a multi-core coated wire. The intermediate body and the coated glass wire obtained by drawing the tip connecting portion 203 shown in Fig. 15 are single-core coated wires. Therefore, as shown in Fig. 16, the forward scattered light shows a clear pattern of bright and dark areas. This makes it easy to check for uneven thickness of the coating. In contrast, when the coated wire is multi-core, as shown in FIG. 17, the forward scattered light has multiple bright areas caused by the multiple cores, making it difficult to check for uneven thickness of the coating.

[0091] 15, tip connecting portion 203 is a single core unit including tip cladding body 204 and one tip core rod 205. Therefore, tip connecting portion 203 can be fabricated using waste optical fiber preform for single-core optical fibers. This facilitates the preparation of the optical fiber preform 210. Furthermore, the optical fiber preform 210 can be prepared at low cost.

[0092] Although the present invention has been described above based on the best mode, the present invention is not limited to the above-mentioned best mode, and various modifications are possible without departing from the gist of the present invention. The optical fiber preform of the embodiment may be formed by applying a stack-and-draw method. When applying the stack-and-draw method, for example, a plurality of main core rods and a plurality of spacer rods are inserted into one through hole (main inner hole) of a glass tube (main cladding body). In this way, a glass material unit including a glass tube, a main core rod, and a spacer rod is obtained. The optical fiber preform is composed of this glass material unit and a tip connecting portion.

[0093] The optical fiber preform of the embodiment may be formed by the rod-in-tube method. In this case, the number of through holes (main inner holes) in the main clad body is preferably more than one, but is not limited to more than one. In other words, the glass material unit may be formed by a main clad body having one through hole and a plurality of main core rods inserted into the through hole. [Explanation of symbols]

[0094] Reference Signs List 1: Main cladding body, 2: Main core rod, 3,203: Tip connecting portion, 4: Main inner hole, 10,210: Multi-core optical fiber preform, 22: Intermediate body (coated wire), 23: Coated glass wire (coated wire), 204: Tip cladding body, 205: Tip core rod, 206: Tip inner hole, A1: Length of fixed diameter portion, A2: Length of reduced diameter portion, L1: Laser light (test light), L2: Forward scattered light

Claims

1. a rod-shaped main cladding body having one or more main bores; a plurality of main core rods inserted into the main bore; a tip connecting portion connected to one end of the main clad body; Equipped with The tip connecting portion is a glass rod having one core rod. Multi-core optical fiber preform.

2. the plurality of main core rods include a first core rod and a second core rod having a dimension shorter than an axial dimension of the main clad body; The multi-core optical fiber preform according to claim 1 , wherein the first core rod is disposed at the center of the main cladding body.

3. 3. The multi-core optical fiber preform according to claim 1, wherein the tip continuous portion is a solid glass rod.

4. The tip connecting portion includes a constant diameter portion having a constant outer diameter, and a reduced diameter portion protruding from a tip of the constant diameter portion while reducing in diameter, 4. The multi-core optical fiber preform according to claim 1, wherein the constant diameter portion has an axial length equal to or greater than the axial length of the tapered portion.

5. The tip connecting portion includes a constant diameter portion having a constant outer diameter, and a reduced diameter portion protruding from a tip of the constant diameter portion while reducing in diameter, 4. The multi-core optical fiber preform according to claim 1, wherein an axial length of the constant diameter portion is less than an axial length of the tapered portion.

6. a preparation step of preparing a glass material unit in which a plurality of main core rods are inserted into one or a plurality of main inner holes formed in a rod-shaped main clad body; a glass rod connecting step of butt-connecting a glass rod having one core rod to one end of the glass material unit; a glass rod cutting step of leaving a part of the glass rod as a tip connected to the glass material unit and separating the remaining part of the glass rod by fusing; The present invention relates to a method for producing a multi-core optical fiber preform.

7. the plurality of main core rods include a first core rod and a second core rod having a dimension shorter than an axial dimension of the main clad body; In the preparation step, preparing the glass material unit in which the first core rod is inserted into the main inner hole at the center of the main clad body and the second core rod is inserted around the first core rod so that a gap is formed between an end face of the main clad body and the second core rod; The method for manufacturing a multi-core optical fiber preform according to claim 6 , further comprising the steps of: heating the gaps after the preparation step; and reducing a diameter of the main cladding body to close the gaps.

8. 8. The method for manufacturing a multi-core optical fiber preform according to claim 6, wherein the tip continuous portion is a solid glass rod.

9. 7. The method for manufacturing a multi-core optical fiber preform according to claim 6, wherein the tip continuous portion is a single core unit including a rod-shaped tip cladding body having one tip inner hole formed therein, and one tip core rod inserted into the tip inner hole.

10. In the glass rod cutting step, the tip connecting portion is formed to have a constant diameter portion having a constant outer diameter and a reduced diameter portion protruding from a tip of the constant diameter portion while reducing in diameter, 10. The method for manufacturing a multi-core optical fiber preform according to claim 6, wherein an axial length of the constant diameter portion is equal to or longer than an axial length of the tapered portion.

11. In the glass rod cutting step, the tip connecting portion is formed to have a constant diameter portion having a constant outer diameter and a reduced diameter portion protruding from a tip of the constant diameter portion while reducing in diameter, 10. The method for manufacturing a multi-core optical fiber preform according to claim 6, wherein an axial length of the constant diameter portion is less than an axial length of the reduced diameter portion.

12. A method for manufacturing a multi-core optical fiber, comprising drawing a multi-core optical fiber preform obtained by the method for manufacturing a multi-core optical fiber preform according to any one of claims 6 to 11 to manufacture a multi-core optical fiber.

Citation Information

Patent Citations

  • Measurement of eccentric thickness of coated optical fiber

    JP1997126946A

  • Optical fiber manufacturing method

    JP2012137615A

  • Method for manufacturing optical fiber

    JP2016175779A

  • Method for manufacturing optical fiber preform, optical fiber preform and method for manufacturing optical fiber

    JP2019031427A

  • Method for manufacturing multi-core optical fiber

    JP2019172480A