Circuit component and method for manufacturing the same
The circuit component design with non-through holes and specific ratios in the insulating resin layer addresses heat dissipation limitations in MIDs by enhancing thermal conductivity and adhesion, achieving efficient heat transfer and insulation.
Patent Information
- Application Number
- JP2020066410
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-04-02
- Publication Date
- 2024-09-19
- Estimated Expiration
- 2040-04-02
AI Technical Summary
Existing MIDs used in electronic devices face challenges in achieving high heat dissipation due to limitations in reducing the thickness of resin layers containing alumina or silica particles, which hinder effective heat conduction from circuit wiring to metal members.
A circuit component design featuring a metal member, an insulating resin layer with non-through holes filled with a plating film, and a specific ratio of hole depth to width (0.5 to 5) and spacing (0.3 to 3) enhances heat dissipation and adhesion, using thermosetting resins and thermally conductive fillers.
The design achieves both high heat dissipation and adhesion of circuit wiring, ensuring effective thermal conductivity and insulation while maintaining surface flatness and adhesion strength.
Smart Images

Figure 0007554057000007 
Figure 0007554057000013 
Figure 0007554057000010
Abstract
Description
[Technical field]
[0001] The present invention relates to a circuit component and a method for manufacturing a circuit component. [Background technology]
[0002] In recent years, MIDs (Molded Interconnected Devices) have been put to practical use in smartphones and other devices, and their application in the automotive field is expected to expand in the future. MIDs are devices in which circuits are formed with a metal film on the surface of a resin molded body, and can contribute to making products lighter, thinner, and with fewer parts.
[0003] MIDs mounted with light-emitting diodes (LEDs) have also been proposed. LEDs generate heat when current is passed through them, and so it is necessary to exhaust the heat from the back, making it important to improve the heat dissipation properties of the MID. Patent Document 1 proposes a composite part that integrates an MID with a metal heat dissipation material. In addition, in the MID of Patent Document 1, the circuit wiring is formed by a plating film. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 3443872 Summary of the Invention [Problem to be solved by the invention]
[0005] In recent years, electronic devices have become more powerful and smaller, and the MIDs used in these devices have also become denser and more functional, requiring higher heat dissipation. In an MID in which a resin layer is provided on a metal member, which is a heat dissipation material, thinning the resin layer is effective for improving heat conduction from the circuit wiring on the resin layer to the metal member. However, the resin layer often contains alumina or silica particles as a filler responsible for heat conduction, and there is a limit to improving heat dissipation by only thinning the resin layer. The present invention solves these problems and provides a circuit component (MID) with high heat dissipation. [Means for solving the problem]
[0006] According to a first aspect of the present invention, there is provided a circuit component comprising: a metal member; an insulating resin layer formed on the metal member; circuit wiring including a plating film formed on the insulating resin layer; and a mounted component mounted on the circuit wiring and electrically connected to the circuit wiring, wherein a plurality of non-through holes filled with the plating film are formed in a wiring region on a surface of the insulating resin layer where the circuit wiring is formed, and a ratio d / D of a depth d of the non-through holes to a width D of the non-through holes is 0.5 to 5.
[0007] The surface roughness (Ra) of the wiring region other than the non-through holes may be 1 / 5 or less of the depth d of the non-through holes. The ratio P / D of the distance P between the non-through holes to the width D of the non-through holes may be 0.3 to 3. The thickness of the circuit wiring may be greater than 1 / 2 the depth d of the non-through holes or greater than 1 / 2 the width D. The width D of the non-through holes may be 10 to 200 μm. The thickness of a portion of the insulating resin layer that is sandwiched between the circuit wiring and the metal member and in which the non-through holes are not formed may be 30 to 200 μm. The distance from the bottom of the non-through hole to the surface of the insulating resin layer facing the metal member may be 5 to 100 μm. The non-through holes may be formed in a scattered manner so that the density in the wiring region is averaged.
[0008] The insulating resin layer may include a thermosetting resin. The thermosetting resin may be an epoxy resin. The insulating resin layer may include an insulating thermally conductive filler. An inorganic oxide layer may be further provided between the metal member and the insulating resin layer. The mounting component may be disposed such that a surface on which a terminal is provided faces the circuit wiring, and the terminal and the circuit wiring may be electrically connected by solder.
[0009] According to a second aspect of the present invention, there is provided a method for manufacturing a circuit component according to the first aspect, comprising: preparing the metal member; forming the insulating resin layer on the metal member; irradiating the wiring region of the insulating resin layer with laser light to form the plurality of blind holes; forming the circuit wiring in the wiring region by electrolytic plating; and mounting the mounted components on the circuit wiring. Effect of the Invention
[0010] The circuit component of the present invention can achieve both high heat dissipation properties and high adhesion of the circuit wiring. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a schematic top view of a circuit component according to an embodiment. [Diagram 2] Fig. 2(a) is an enlarged view of region IIA shown in Fig. 1, and Fig. 2(b) is a schematic cross-sectional view taken along line IIB-IIB in Fig. 1. Note that mounted components are omitted in Fig. 2(a). [Diagram 3] 3(a) to (c) are schematic top views of a wiring region in which non-through holes having an elliptical opening shape are formed, and FIGS. 3(d) and (e) are schematic top views of a wiring region in which non-through holes having openings of various shapes are formed. [Figure 4] FIG. 4(a) is a schematic top view of a wiring region in which non-through holes are formed at a roughly averaged density, and FIG. 4(b) is a schematic top view of a wiring region in which non-through holes are formed at a non-uniform density. [Diagram 5]FIG. 5 is a flowchart illustrating a method for manufacturing a circuit component according to an embodiment. [Figure 6] FIG. 6 shows an example of a laser drawing pattern when non-through holes are formed by irradiation with laser light. [Figure 7] 7(a) to (e) are diagrams illustrating how a plating film is formed on a substrate in the embodiment. [Figure 8] 8(a) to (e) are diagrams illustrating the formation of a plating film on a base material having non-through holes with a small ratio d / D. [Figure 9] FIG. 9 is a schematic cross-sectional view of a portion of a circuit component according to a modified example. [Figure 10] FIG. 10(a) is a schematic top view of the circuit component produced in Example 13, and FIG. 10(b) is a schematic cross-sectional view taken along line XB-XB of FIG. 10(a). [Figure 11] FIG. 11 is a cross-sectional photograph of the circuit component produced in Example 14. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] [Circuit components] A circuit component 100 shown in Fig. 1 and Fig. 2(a) and (b) will be described. The circuit component 100 includes a base material 70 including a metal member 50 and an insulating resin layer 10, a circuit wiring 20 including a plating film formed on the insulating resin layer 10 of the base material 70, and a mounting component 30 mounted on the insulating resin layer 10 and electrically connected to the circuit wiring 20. The mounting component 30 is disposed and mounted on the circuit wiring 20. On the surface 10a of the insulating resin layer 10, a wiring region 10A in which the circuit wiring 20 is formed has a plurality of non-through holes 11 (recesses) filled with the plating film of the circuit wiring 20 formed therein.
[0013] The metal member 50 dissipates heat generated by the mounting components 30 mounted on the insulating resin layer 10. Therefore, it is preferable to use a metal with heat dissipation properties for the metal member 50, such as iron, copper, aluminum, titanium, magnesium, stainless steel (SUS), etc. Among them, it is preferable to use magnesium and aluminum from the viewpoints of weight reduction, heat dissipation, and cost. These metals may be used alone or in combination of two or more kinds. The thermal conductivity of the metal member 50 is, for example, 80 to 300 W / m·K.
[0014] The shape and size of the metal member 50 are not particularly limited, and can be designed arbitrarily according to the application of the circuit component 100. For example, the shape of the metal member 50 may be a plate-like body (metal plate), a heat dissipation fin, or a complex shape formed by die casting.
[0015] The insulating resin layer 10 has insulating properties to insulate the circuit wiring 20 from the metal member 50 to prevent short circuits. The degree of insulation of the insulating resin layer 10 depends on the application of the circuit component 100, but for example, the resistance between the circuit wiring 20 and the metal member 50 when a voltage of 16 V is applied is 1 MΩ or more. If the resistance between the circuit wiring 20 and the metal member 50 is less than 1 MΩ, a minute current may flow from the circuit wiring 20 to the metal member 50, causing the circuit wiring 20 to fail to function. In addition, the insulating resin layer 10 has a certain degree of thermal conductivity to enhance the heat dissipation of the circuit component 100. Thus, the insulating resin layer 10 is an insulating heat dissipation resin layer that has both insulating properties and a certain degree of thermal conductivity. The thermal conductivity of the insulating resin layer 10 is, for example, 1 to 5 W / m·K.
[0016] The insulating resin layer 10 contains a resin. When the mounting components 30 are mounted on the insulating resin layer 10 by soldering, the resin used for the insulating resin layer 10 is preferably a heat-resistant, high-melting-point resin that has solder reflow resistance. The melting point of the resin used for the insulating resin layer 10 is preferably 260° C. or higher, and more preferably 290° C. or higher. However, this does not apply when low-temperature solder is used to mount the mounting components 30.
[0017] The resin used for the insulating resin layer 10 may be, for example, a thermosetting resin, a thermoplastic resin, or an ultraviolet-curing resin. Among them, a thermosetting resin is preferred because it is easy to mold thinly, has high molding accuracy, and has high heat resistance and high density after curing. As the thermosetting resin, for example, a heat-resistant resin such as an epoxy resin, a silicone resin, or a polyimide resin may be used, and among them, an epoxy resin is preferred. As the photocurable resin, for example, a polyimide resin, an epoxy resin, or the like may be used. As the thermoplastic resin, for example, aromatic polyamides such as 6T nylon (6TPA), 9T nylon (9TPA), 10T nylon (10TPA), 12T nylon (12TPA), and MXD6 nylon (MXDPA) and alloy materials thereof, polyphenylene sulfide (PPS), liquid crystal polymer (LCP), polyether ether ketone (PEEK), polyetherimide (PEI), polyphenylsulfone (PPSU), or the like may be used. These thermosetting resins, ultraviolet curing resins and thermoplastic resins may be used alone or in combination of two or more kinds.
[0018] The insulating resin layer 10 may contain an insulating thermally conductive filler. The insulating thermally conductive filler can improve the thermal conductivity while maintaining the insulating properties of the insulating resin layer 10. The insulating thermally conductive filler is a filler having a thermal conductivity of 1 W / m·K or more, and conductive heat dissipation materials such as carbon are excluded. Examples of the insulating thermally conductive filler include ceramic powders such as aluminum oxide, silicon oxide, magnesium oxide, magnesium hydroxide, boron nitride, and aluminum nitride, which are inorganic powders with high thermal conductivity. In order to increase the contact rate between the fillers and improve the heat transferability, rod-shaped fillers such as wollastonite, and plate-shaped fillers such as talc and boron nitride may be mixed. These insulating thermally conductive fillers may be used alone or in combination of two or more types.
[0019] The maximum diameter (maximum particle size) of the insulating thermally conductive filler is preferably 30 μm to 100 μm when relatively inexpensive ceramic particles are used, for example, and when the thickness of the insulating resin layer 10 is reduced, the maximum diameter of the insulating thermally conductive filler is preferably 10 μm to 60 μm.
[0020] The insulating thermally conductive filler is contained in the insulating resin layer 10 in an amount of, for example, 10% by weight to 90% by weight, and preferably 30% by weight to 80% by weight. When the amount of the insulating thermally conductive filler is within the above range, the circuit component 100 can obtain sufficient heat dissipation properties.
[0021] The insulating resin layer 10 may further contain rod-shaped or needle-shaped fillers such as glass fibers and calcium titanate in order to control its strength. The insulating resin layer 10 may also contain various general-purpose additives that are added to resin molded bodies as necessary. Hereinafter, a material that includes all of the resin and insulating thermally conductive filler that constitute the insulating resin layer 10 may be referred to as a "resin material."
[0022] As shown in FIGS. 2(a) and 2(b), a plurality of non-through holes (recesses) 11 filled with the plating film of the circuit wiring 20 are formed in the wiring region 10A on the surface 10a of the insulating resin layer 10 where the circuit wiring 20 is formed. The ratio d / D of the depth d of the non-through hole 11 to the width D of the non-through hole 11 is 0.5 to 5. The ratio d / D may be preferably 0.8 to 3.0 μm, or 1.0 to 1.6 μm. The plating film of the circuit wiring 20 is filled in the non-through hole 11 having the ratio d / D within the above range, so that the adhesion of the circuit wiring 20 to the insulating resin layer 10 is improved. In addition, in the non-through hole 11 having the ratio d / D within the above range, the distance between the plating film of the circuit wiring 20 and the metal member 50 is short, so that the heat generated by the circuit wiring 20 and the mounting component 30 arranged thereon can be easily released to the metal member 50. As a result, the heat dissipation of the circuit component 100 is improved. In this manner, by providing the non-through holes (recesses) 11 with the ratio d / D within the above range, the heat dissipation property of the circuit component 100 and the adhesion of the circuit wiring 20 are improved. Furthermore, the circuit wiring 20 formed on the wiring region 10A in which the non-through holes 11 with the ratio d / D within the above range are formed can obtain a sufficiently flat (smooth) surface 20a.
[0023] On the other hand, if the ratio d / D is outside the above range, the heat dissipation properties of the circuit component 100 and the adhesion of the circuit wiring 20 cannot be achieved at the same time, as described below. In addition, sufficient flatness (smoothness) of the circuit wiring 20 cannot be obtained. If the ratio d / D is less than the lower limit of the above range, the depth d is small (shallow) relative to the width D, so that the adhesion of the circuit wiring 20 is not sufficient and the heat dissipation properties of the circuit component 100 may also be reduced. In addition, since the width D is large relative to the depth d, it is difficult to fill the non-through holes 11 with a plating film, and the flatness of the circuit wiring 20 may be reduced (see FIGS. 8(a) to (e) described later). On the other hand, if the ratio d / D exceeds the upper limit of the above range, it is necessary to increase (deepen) the depth d. However, if d is greater than the thickness of the insulating resin layer 10, the circuit wiring 20 comes into contact with the metal member 50, and the circuit wiring 20 and the metal member 50 cannot be insulated from each other. If the insulating resin layer 10 is made thicker in order to increase (deepen) the depth d, the circuit wiring 20 and the metal member 50 can be insulated from each other, but the heat transfer from the circuit wiring 20 to the metal member 50 is hindered, and the heat dissipation performance decreases.
[0024] In the present specification, the width D of the non-through hole 11 means the diameter of the opening 11a of the non-through hole 11 in the surface 10a (wiring region 10A) when the opening 11a is a perfect circle. The shape of the opening 11a of the non-through hole 11 is preferably a circle from the viewpoint of improving the smoothness and adhesion of the plating film constituting the circuit wiring 20, but is not particularly limited. For example, it may be an ellipse as shown in Figs. 3(a) to (c), or may be a shape as shown in Figs. 3(d) and (e). When the opening 11a is not a perfect circle, it means the diameter of a perfect circle having the same area as the opening 11a. In addition, the depth d of the non-through hole 11 means the depth of the deepest part (bottom 11b) of the non-through hole 11, that is, the distance (length) from the surface 10a to the bottom 11b of the non-through hole 11.
[0025] The width D of the non-through hole 11 is not particularly limited as long as the ratio d / D satisfies the above range, and may be, for example, 10 to 200 μm, 20 to 150 μm, or 30 to 50 μm. If the width D is less than the lower limit of the above range, there is a risk that sufficient adhesion of the circuit wiring 20 cannot be obtained. If the width D exceeds the upper limit of the above range, there is a risk that it becomes difficult to keep the ratio d / D within the above-mentioned appropriate range.
[0026] The depth d of the non-through hole 11 is not particularly limited as long as the ratio d / D satisfies the above range, and may be, for example, 20 to 200 μm, 30 to 150 μm, or 50 to 100 μm. If the depth d is less than the lower limit of the above range, there is a risk that sufficient adhesion of the circuit wiring 20 cannot be obtained. If the depth d exceeds the upper limit of the above range, there is a risk that sufficient insulation between the circuit wiring 20 and the metal member 50 cannot be obtained, or that the heat dissipation property is reduced because the insulating resin layer 10 is thickened to obtain insulation.
[0027] The ratio P / D of the distance P between the non-through holes 11 to the width D of the non-through holes 11 is preferably 0.3 to 3, 0.5 to 2.5, or 1.0 to 1.5. Here, the distance P between the non-through holes 11 is the shortest distance between one non-through hole 11 and another non-through hole 11 adjacent thereto on the surface 10a (wiring region 10A) of the insulating resin layer 10, and is the shortest distance from the edge of the opening 11a of one non-through hole 11 to the edge of the opening 11a of another non-through hole 11 adjacent thereto. If the ratio P / D is less than the lower limit of the above range, the distance P between the non-through holes 11 is too close, so that the flatness of the circuit wiring 20 formed thereon may be insufficient. If the ratio P / D exceeds the upper limit of the above range, the distance P between the non-through holes 11 becomes large, so that the number of the non-through holes 11 that can be arranged decreases, and the heat dissipation of the circuit component 100 and the adhesion of the circuit wiring 20 may be insufficient.
[0028] The distance P between the non-through holes 11 is not particularly limited as long as the ratio P / D satisfies the above range, and may be, for example, 20 to 300 μm, or 50 to 150 μm.
[0029] The depth d and width D of the non-through hole 11 and the distance P between the non-through holes 11 are obtained, for example, as the average value of a plurality of non-through holes 11 present in a predetermined range (measurement range). For example, as described below, they may be obtained by measuring the height of the wiring region 10A by an optical measurement method. First, the circuit wiring 20 is peeled off from the insulating resin layer 10 to expose the wiring region 10A. The surface roughness (Ra) of the entire predetermined range (measurement range) of the wiring region 10A is measured using an optical measurement device such as a laser microscope. A portion having a depth of at least twice the surface roughness (Ra) of the entire measurement range is determined as a non-through hole (recess) 11, and the width D of each non-through hole 11 and the distance P between the non-through holes 11 are measured to obtain an average value. It is preferable to measure 10 or more non-through holes 11 and obtain the average value, taking into account the variation in the depth d in order to eliminate noise in the optical measurement.
[0030] The depth d and width D of the non-through holes 11 and the distance P between the non-through holes 11 may be determined by a shape analysis method using X-ray CT to be described below. For example, when the metal member 50 is made of aluminum and the circuit wiring 20 is made of copper, a portion of the circuit component 100 including the circuit wiring 20 is cut out to a predetermined size and measured by X-ray CT. This provides an X-ray CT image of only the circuit wiring 20 including copper, which has lower X-ray transmittance than aluminum. This X-ray CT image is extracted as slice data for each plane in the depth direction, and the slice depth at which the circuit wiring 20 becomes invisible is set as the depth d of the non-through hole 11. The width D and distance P of the non-through hole 11 are measured from the shape of the image sliced at the surface 10a of the insulating resin layer 10. The average value is calculated from the depth d, width D and distance P of each non-through hole 11 thus obtained. In addition, the shape analysis method using X-ray CT is performed for a sample having an area of 3 to 15 mm from the viewpoints of ease of sampling and detection sensitivity. 2 It is preferable to cut out the wiring portion and measure it.
[0031] The depth d and width D of the non-through hole 11 may be obtained by observing a cross section of the circuit wiring 20 of the circuit component 100. As shown in FIG. 2(b), the cross section observation must be performed at a cross section where the depth d and width D of the non-through hole 11 can be measured, and may be performed, for example, as follows. First, the circuit component 100 is cut and the cross section of the non-through hole 11 is observed. Then, the cross section is polished and cut by 2 to 3 μm with sandpaper or the like, and the cross section is observed again. This is repeated to obtain a cross section photograph at the position where the depth of the non-through hole 11 is observed to be the deepest, and the depth of the non-through hole 11 obtained from the position is defined as the depth d. If the shape of the non-through hole is a cone as shown in FIG. 2(b), the width D can be obtained from the cross section photograph from which the depth d can be obtained. In consideration of the variation in the depth d and the width D, it is preferable to measure 10 or more non-through holes 11 by the same method and obtain the average thereof.
[0032] The structure of the non-through hole 11 is not particularly limited, and may be any shape. As shown in Figs. 2(a) and (b), the shape of the non-through hole 11 in this embodiment is a cone with its bottom surface located on the surface 10a (wiring region 10A). Therefore, the shape of the opening 11a of the non-through hole 11 is a perfect circle. However, the shape of the non-through hole 11 is not limited to this, and may be, for example, a polygonal pyramid such as a triangular pyramid or a quadrangular pyramid, or a cone with a complex bottom shape. In addition, the non-through hole 11 may be a cylinder, a polygonal prism, or a cylinder with a complex bottom shape, or may be a hemisphere. From the viewpoint of ease of forming the non-through hole 11 (ease of processing), it is preferable that the inside of the non-through hole 11 does not expand more than the opening 11a. That is, it is preferable that the area of the cross section parallel to the surface 10a inside the non-through hole 11 is equal to or less than the area of the opening 11a. Therefore, when the shape of the non-through hole 11 is a pyramid, a column, or a hemisphere, it is preferable that the bottom surface thereof is located on the surface 10a (wiring region 10A).
[0033] The non-through holes 11 are formed in the wiring region 10A. It is preferable that the non-through holes 11 are formed only in the wiring region 10A and not formed on the surface 10a other than the wiring region 10A. This shortens the time (processing time) for forming the non-through holes 11, and improves the manufacturing efficiency of the circuit component 100. It is preferable that the non-through holes 11 are formed in a scattered manner so that the density in the wiring region 10A is approximately equal. This makes it possible to uniformize the heat dissipation property of the circuit component 100 and the adhesion of the circuit wiring 20. For example, the density of the non-through holes 11 in the entire wiring region 10A shown in FIGS. 4(a) and (b) is the same. However, the non-through holes 11 shown in FIG. 4(a) are formed in a scattered manner so that the density in the wiring region 10A is approximately equal, while the non-through holes 11 shown in FIG. 4(b) are formed in a biased manner. In Fig. 4(b), the upper left portion has a high density of non-through holes 11, while the lower right portion has a low density of non-through holes 11. A plating film of the circuit wiring 20 grows uniformly on the wiring region 10A shown in Fig. 4(a). On the other hand, it is difficult for a plating film to grow on the lower right portion of the wiring region 10A shown in Fig. 4(b). Therefore, the plating film becomes non-uniform on the wiring region 10A shown in 4(b), and the smoothness of the plating film decreases.
[0034] In order to form the non-through holes 11 in a scattered manner so that the density in the wiring region 10A is approximately uniform, it is preferable to satisfy the following condition: In the wiring region 10A, it is preferable that the difference between the maximum and minimum values of the distance P (the shortest distance from the edge of the opening 11a of one non-through hole 11 to the edge of the opening 11a of another non-through hole 11 adjacent thereto) is less than 50% of the average value of the distance P in the wiring region 10A. Also, in the wiring region 10A, the density (number of non-through holes 11 / mm 2 ) and the density in the lowest density area (particles / mm 2 ) is the average density (number / mm 2 ) is preferably less than 50% of the total.
[0035] The thickness of the insulating resin layer 10 is not particularly limited, and can be arbitrarily designed according to the application of the circuit component 100. The thickness of the insulating resin layer 10 may be approximately constant or may vary depending on the location. Since the thinner the insulating resin layer 10, the more the heat dissipation of the circuit component 100 tends to improve, it is preferable that the thickness of the insulating resin layer 10 in the vicinity of the mounting components 30 that generate a large amount of heat is small. On the other hand, if the thickness of the insulating resin layer 10 is too small, the flow resistance of the resin increases during molding of the insulating resin layer 10, and molding defects (filling defects) may occur. In addition, it becomes difficult to form the non-through holes 11 with sufficient depth. From these viewpoints, the thickness B of the part of the insulating resin layer 11 that is sandwiched between the circuit wiring 20 and the metal member 50 and where the non-through holes 11 are not formed (the film thickness B of the insulating resin layer 11 under the circuit wiring 20) is preferably 30 to 200 μm, 50 to 150 μm. When the thickness B varies depending on the location, it is preferable that the smallest value (the thickness of the thinnest portion) is within the above range.
[0036] Furthermore, the thickness of the portion of the insulating resin layer 10 where the non-through holes 11 are formed, i.e., the distance (shortest distance) C from the bottom 11b of the non-through hole 11 to the surface 10b of the insulating resin layer 10 facing the metal member 50, is preferably 5 to 100 μm, 20 to 80 μm, or 30 to 60 μm. If the distance C is smaller than the lower limit of the above range, there is a risk that the circuit wiring 20 and the metal member 50 cannot be sufficiently insulated from each other. If the distance C is larger than the upper limit of the above range, there is a risk that the heat dissipation property of the circuit member 100 will decrease.
[0037] The surface roughness (Ra) of the wiring region 10A other than the non-through holes 11 is preferably 1 / 5 or less, or 1 / 10 or less, of the depth d of the non-through holes 11. In this embodiment, since the non-through holes 11 are provided to improve the adhesion of the circuit wiring 20, sufficient adhesion can be maintained even if the surface roughness (Ra) of the wiring region 10A is reduced. Since the surface roughness (Ra) of the wiring region 10A other than the non-through holes 11 can be reduced, the flatness of the circuit wiring 20 formed thereon is improved. On the other hand, from the viewpoint of facilitating selective formation of the plating film of the circuit wiring 20 only in the wiring region 10A, it is preferable that the surface roughness (Ra) of the wiring region 10A is larger than the surface roughness (Ra) of the surface 10a other than the wiring region 10A. The surface roughness (Ra) of the wiring region 10A may be, for example, 1 to 30 μm, 3 to 20 μm, or 5 to 10 μm.
[0038] The circuit wiring 20 is formed by a plating film in the wiring region 10A of the surface 10a of the insulating resin layer 10. The circuit wiring 20 is preferably composed of an electroless plating film 21 formed on the wiring region 10A and an electrolytic plating film 22 formed on the electroless plating film 21 (see FIG. 7(e)).
[0039] Examples of the electroless plating film 21 include electroless nickel phosphorus plating film, electroless copper plating film, and electroless nickel plating film, and among these, electroless nickel phosphorus plating film is preferred. Examples of the electrolytic plating film 22 include electrolytic nickel phosphorus plating film, electrolytic copper plating film, and electrolytic nickel plating film. In addition, a plating film of gold, silver, tin, or the like may be formed on the outermost surface of the circuit wiring 20 in order to improve the solder wettability of the plating film.
[0040] Since the plating film constituting the circuit wiring 20 fills the non-through holes 11, the circuit wiring 20 can be strongly adhered to the insulating resin layer 10. The thickness A of the circuit wiring 20 is preferably larger than the smaller of 1 / 2 the depth d and 1 / 2 the width D of the non-through holes 11. That is, the thickness A of the circuit wiring 20 is preferably larger than 1 / 2 the depth d or 1 / 2 the width D of the non-through holes 11. When the thickness A of the circuit wiring 20 is within the above range, the flatness of the plating film forming the circuit wiring 20 is further improved. However, when the size of the non-through holes 11 is relatively small, the non-through holes 11 can be filled with the plating film even if the thickness A of the circuit wiring 20 is thinner than the above range, and the flatness of the circuit wiring 20 can be ensured. If the size of the non-through hole 11 is relatively small, there is a concern that the heat dissipation performance may decrease. However, for example, by reducing the thickness B of the insulating resin layer 10 and bringing the bottom 11b of the non-through hole 11 closer to the metal member 50 (by reducing the distance C), the heat dissipation performance of the circuit component 100 can be sufficiently ensured.
[0041] The thickness A of the circuit wiring 20 means a thickness that does not include the portion filled in the non-through holes 11. In other words, the thickness A of the circuit wiring 20 is the distance from the surface 10a of the insulating resin layer 10 to the surface 20a of the circuit wiring 20 that faces the mounted component 30. The thickness A of the circuit wiring 20 may be, for example, 10 to 100 μm, or 20 to 80 μm.
[0042] As shown in FIG. 2(b), the mounting component 30 is disposed with a surface (bottom surface) 30b on which terminals are provided facing the circuit wiring 20, and the terminals and the circuit wiring 20 are electrically connected by solder. There is no particular limitation on the solder, and a general-purpose solder can be used. The mounting component 30 generates heat when electricity is applied, and becomes a heat source. Any mounting component can be used as the mounting component 30, and examples of such components include an LED (light-emitting diode), a power module, an IC (integrated circuit), and a thermal resistor.
[0043] In this embodiment, since the surface 20a of the circuit wiring 20 on which the mounting component 30 is mounted is flat, the adhesive strength of the mounting component 30 to the circuit wiring 20 is increased, and the thermal conductivity from the mounting component 30 to the circuit wiring 20 is improved. This further improves the heat dissipation performance of the circuit component 100.
[0044] [Manufacturing method of circuit components] A method for manufacturing the circuit component 100 will be described with reference to the flowchart shown in Fig. 5. First, a metal member 50 is prepared (step S1 in Fig. 5). The metal member 50 may be a commercially available metal plate (plate-shaped body), a heat dissipation fin, or the like, or may be formed into any shape by die casting.
[0045] The surface of the metal member 50 on which the insulating resin layer 10 is formed may be roughened to improve adhesion with the insulating resin layer 10 laminated thereon. The surface of the metal member 50 may be roughened by chemical etching or nanomolding technology (NMT) disclosed in JP-A-2009-6721, Japanese Patent No. 5681076, etc. Alternatively, laser roughening may be performed.
[0046] Next, the insulating resin layer 10 is formed on the metal member 50 (step S2 in FIG. 5). For example, the insulating resin layer 10 may be formed by insert molding (integral molding). Specifically, the metal member 50 is placed in a mold first, and a resin material is injected and filled into the empty part of the mold. As a result, the metal member 50 and the insulating resin layer 10 are integrally molded. As the insert molding, injection molding, transfer molding, etc. can be used. In this way, the insulating resin layer 10 and the metal member 50 may be an integrally molded body. Here, the integrally molded body means a body manufactured by a process (typically insert molding) in which the metal member 50 is joined to the insulating resin layer 10 during molding, rather than by bonding or joining (secondary bonding or mechanical joining) the metal member 50 and the insulating resin layer 10 that are separately prepared.
[0047] Next, a plurality of non-through holes 11 are formed in the wiring region 10A of the insulating resin layer 10 (step S3 in FIG. 5). The method of forming the non-through holes 11 is not particularly limited, but for example, the non-through holes 11 may be formed by cutting the surface 10a of the insulating resin layer 10 by irradiating with laser light (laser processing). Laser processing can efficiently form a plurality of non-through holes 11, and the size (width D, depth d) of the non-through holes 11 can be easily adjusted. At the same time as forming the non-through holes 11, the entire wiring region 10A may be irradiated with laser light to roughen the wiring region 10A. By roughening the wiring region 10A, it becomes easier to selectively form the circuit wiring 20 (plating film) in the wiring region 10A, and the adhesion of the circuit wiring 20 can be improved. However, in order to ensure the flatness of the circuit wiring 20 formed thereon, it is preferable that the surface roughness (Ra) of the wiring region 10A other than the non-through holes 11 is 1 / 5 or less, or 1 / 10 or less, of the depth d of the non-through holes 11. The type of laser light and the laser processing device used for laser processing of the non-through holes 11 are not particularly limited, and can be appropriately selected and used taking into consideration the type of the insulating resin layer 10 and the like.
[0048] When forming the non-through holes 11 by laser processing, it is preferable to perform laser drawing of a pattern composed of discontinuous lines, as shown in FIG. 6, for example. The laser drawing shown in FIG. 6 will be described. First, a discontinuous line L1 extending in a predetermined direction (Y direction shown in FIG. 6) is drawn. The discontinuous line L1 is a pattern in which line segments (laser drawn parts) of length N1 are arranged at intervals (spaces) of length N2. Next, as the discontinuous line L2, a pattern similar to the line L1 is laser drawn by translating the line L1 in a direction perpendicular to the predetermined direction (X direction shown in FIG. 6) by a length N3 and translating the line L1 in the Y direction by a length N4. At this time, N4=(N1+N2) / 2. The same operation is repeated to draw a plurality of discontinuous lines Ln extending in the Y direction at equal intervals (length N3) in the X direction. This forms a laser-drawn pattern in which line segments (laser-drawn portions) of length N1 are arranged at a pitch of length (N1+N2) in the X direction and at a pitch of length 2×N3 in the Y direction, as shown in FIG. 6. The laser light is only applied to the line segments of length N1, but since the laser light has a width called the spot diameter, the insulating resin layer 10 around the drawn pattern lines is also cut. When the line length N1 is short, the spread of the width due to the spot diameter and the cutting depth are almost the same, and the laser processing marks become conical non-through holes 11. If the diameter of the non-through holes 11 formed by cutting and spreading from the laser-irradiated portion of length N1 is D, the interval P is given by P=√[(N3) 2 +(N4) 2 ]-D. By changing the values of lengths N1 to N4, patterns of non-through holes 11 of various sizes can be created. Furthermore, by using such laser drawing, non-through holes 11 can be easily formed by scattering them in the wiring region 10A so that the density is approximately uniform. As a method for forming a plurality of non-through holes 11 by laser light, in addition to making the drawing pattern discontinuous, a method of irradiating the laser light in pulses may also be used.
[0049] Next, the circuit wiring 20 contained in the plating film is formed in the wiring region 10A of the insulating resin layer 10. The method of forming the circuit wiring 20 is not particularly limited, and a general-purpose method can be used. For example, a method of forming a plating film on the entire surface 10a, patterning the plating film with a photoresist, and removing the plating film in the portion other than the circuit wiring by etching, a method of irradiating a portion where the circuit wiring is to be formed with a laser beam to roughen the resin layer, and forming a plating film only in the laser beam irradiated portion, etc. are included. In particular, when a thermosetting resin such as an epoxy resin is used for the insulating resin layer 10, the adsorption of metal ions, which are a plating catalyst, can be promoted by roughening the wiring region 10A with a laser beam, and it becomes easier to form an electroless plating film only in the wiring region 10A.
[0050] A portion of the plating film constituting the circuit wiring 20 fills the non-through holes 11. As shown in Figures 7(a) to (e), the formation of the circuit wiring 20 may include forming an electroless plating film 21 on the wiring region 10A (see Figure 7(a)), and forming an electrolytic plating film 22 on the electroless plating film 21 (see Figures 7(b) to (e)).
[0051] There is no particular limitation on the method for forming the electroless plating film 21, and a general-purpose electroless plating method can be appropriately selected and used. By forming the conductive electroless plating film 21 on the insulating resin layer 10, electrolytic plating can be performed on the electroless plating film 21. In this way, the electroless plating film 21 is a base film for forming the electrolytic plating film 22.
[0052] The method for forming the electrolytic plating film 22 is not particularly limited, and a general-purpose electrolytic plating method can be appropriately selected and used, but an electrolytic plating method with high uniform electrodeposition is preferable. In electrolytic plating, a large current flows at the corners and protrusions of the plating film formation surface, and a small current flows at the center and recesses. Since the thickness of the electrolytic plating film tends to be proportional to the strength of the current, if the plating film formation surface has unevenness, the thickness of the electrolytic plating film will be uneven. An electrolytic plating method with high uniform electrodeposition can suppress such unevenness in the thickness of the electrolytic plating film. As a result, as shown in Figures 7(b) to (e), the electrolytic plating films 22a, 22b, and 22c are not formed thickly at the edges (corner parts) of the openings 11a of the non-through holes 11, but grow with a substantially uniform thickness from the inner walls and surfaces 10a of the non-through holes 11. This makes it easy to fill the non-through holes 11, and further improves the flatness of the surface of the electrolytic plating film 23c (surface 20a of the circuit wiring 20).
[0053] As described above, the ratio d / D of the depth d to the width D of the non-through hole 11 is 0.5 to 5. Since the ratio d / D of the non-through hole 11 is within the above range, the electrolytic plating film 22 can easily fill the non-through hole 11, and the flatness (smoothness) of the surface 20a of the circuit wiring 20 can be improved. On the other hand, if the ratio d / D is outside the above range, it is difficult to fill the non-through hole 11 with the plating film, and the flatness of the circuit wiring 20 cannot be improved. For example, FIGS. 8(a) to (e) show how a plating film is formed on a substrate having a non-through hole 111 with a ratio d / D smaller than 0.5, that is, a through hole 111 with a width D that is too wide compared to the height d. The electrolytic plating films 22a, 22b, and 22c growing from the inner wall of the non-through hole 111 cannot easily fill the non-through hole 111 because the width D of the non-through hole 111 is large compared to the film thickness. 8(e), the non-through hole 111 can be filled by forming a plating film with a thickness equivalent to the depth d, but a bulge of the plating film is formed at the edge of the opening 111a of the non-through hole 111, making it impossible to flatten the surface 20a of the circuit wiring 20. In order to flatten the surface 20a of the circuit wiring 20, it is necessary to form an even thicker electrolytic plating film 22, which is inefficient and increases the manufacturing cost.
[0054] After forming the circuit wiring 20 on the insulating resin layer 10, the mounted component 30 is mounted on the circuit wiring 20 (step S5 in FIG. 5). This results in the circuit component 100 of this embodiment. The method for mounting the mounted component 30 is not particularly limited, and a general-purpose method can be used. For example, the mounted component 30 may be soldered to the insulating resin layer 10 by a solder reflow method in which room temperature solder and the mounted component 30 are placed on the circuit wiring 20 and passed through a high-temperature reflow furnace, or a laser soldering method (spot mounting) in which laser light is irradiated to the interface between the insulating resin layer 10 and the mounted component 30 to perform soldering.
[0055] In the circuit component 100 of the present embodiment described above, by providing the non-through holes 11 with a ratio d / D within a specific range in the wiring region 10A, it is possible to achieve both high heat dissipation properties and high adhesion of the circuit wiring 20 to the insulating resin layer 10. Furthermore, since the surface 20a of the circuit wiring 20 on which the mounting components 30 are mounted is flat, the adhesion strength of the mounting components 30 to the circuit wiring 20 is improved, and the thermal conductivity from the mounting components 30 to the circuit wiring 20 is improved. This further improves the heat dissipation properties of the circuit component 100.
[0056] [Variations] In the circuit part 100 of the present embodiment described above, the insulating resin layer 10 is formed directly on the metal member 50, but the present embodiment is not limited to this. As shown in FIG. 9, a ceramic layer 60 may be formed between the metal member 50 and the insulating resin layer 10. In this modification, a circuit part 200 having the ceramic layer 60 shown in FIG. 9 will be described below. The configuration of the circuit part 200 is the same as that of the circuit component 100 shown in FIGS. 2(a) and (b) described above, except for having the ceramic layer 60. Therefore, in this modification, a description of the components other than the ceramic layer 60 will be omitted.
[0057] The ceramic layer 60 is formed on the metal member 50. The ceramic layer 60 is more difficult to cut by laser light than the insulating resin layer 10. This makes it possible to prevent the non-through holes 11 from reaching the metal member 50 when they are formed by irradiating laser light. The ceramic layer 60, together with the insulating resin layer 10, has insulating properties to insulate the circuit wiring 20 from the metal member 50 and prevent short circuits. The degree of this insulating properties depends on the application of the circuit component 100, but it is preferable that the ceramic layer 60 has a resistance of 5000 MΩ or more when a voltage of 500 V is applied, for example.
[0058] Moreover, the ceramic layer 60 preferably has high thermal conductivity in order to enhance the heat dissipation of the circuit component 100. Thus, the ceramic layer 60 is preferably an insulating heat-conducting layer (insulating heat dissipation layer) that has both insulating properties and high thermal conductivity. The thermal conductivity of the ceramic layer 60 is, for example, 5 to 150 W / m·K. Moreover, in order to efficiently dissipate heat generated by the mounted components 30 on the insulating resin layer 10 to the metal member 50, the thermal conductivity of the ceramic layer 60 is preferably lower than that of the metal member 50 and higher than that of the insulating resin layer 10.
[0059] Examples of ceramics contained in the ceramic layer include aluminum oxide (alumina), aluminum nitride, boron nitride, silicon nitride, beryllium oxide, silicon carbide, yttria, zirconia, titanium dioxide, silicon dioxide, clay minerals, etc. Among them, yttria and alumina are preferred because they are easy to form dense thin films at low cost. These ceramics may be used alone or in combination of two or more.
[0060] The thickness of the ceramic layer 60 may be, for example, 1 μm to 100 μm, 5 μm to 20 μm, or 5 μm to 10 μm.
[0061] Next, a method for manufacturing the circuit component 200 of this modified example will be described. First, the metal member 50 is prepared.
[0062] Next, the ceramic layer 60 is formed on the metal member 50. The method of forming the ceramic layer 60 is not particularly limited, and examples of the method include physical vapor deposition (PVD) such as vacuum deposition and ion plating, chemical vapor deposition (CVD) such as plasma CVD, aerosol deposition (AD), sputtering, thermal spraying, cold spray, and warm spray. When aluminum and its alloy are used for the metal member 50, an alumite layer (aluminum oxide (alumina) coating) may be formed as the ceramic layer 60 by anodization. The alumite layer may be formed only on a part of the metal member 50, or may be formed on the entire surface of the metal member 50. The ceramic layer 60 may be formed of a multilayer film using the above-described multiple film forming methods to increase the film strength.
[0063] Next, an insulating resin layer 10 is formed on the ceramic layer 60, a plurality of non-through holes 11 are formed in the wiring region 10A of the insulating resin layer 10, circuit wiring 20 contained in a plating film is formed in the wiring region 10A of the insulating resin layer 10, and mounting components 30 are mounted on the circuit wiring 20 to obtain a circuit component 200 of this modified example. The formation of the insulating resin layer 10, the formation of the plurality of non-through holes 11, the formation of the circuit wiring 20, and the mounting of the mounting components 30 can be performed in the same manner as in the manufacturing method of the circuit component 100 described above.
[0064] The circuit component 200 of this modification has the same effects as the above-described circuit component 100. Furthermore, since the circuit component 200 has the ceramic layer 60, the circuit wiring 20 and the metal member 50 can be insulated more reliably. EXAMPLES
[0065] The present invention will be described in detail below with reference to examples and comparative examples, but the present invention is not limited to the following examples and comparative examples.
[0066] [Example 1] In this example, a circuit component 100 was manufactured as shown in Fig. 1. As the mounted component 30, an LED (light emitting diode) was used.
[0067] (1) Preparation of metal parts As the metal member 50, an aluminum plate (A1050, aluminum content: 99% or more, 8 cm×12 cm) was prepared.
[0068] (2) Formation of insulating resin layer Next, an epoxy resin (thermosetting resin, thermal conductivity: 1 W / m·K) containing 75% by weight of alumina particles (aluminum oxide) with a maximum diameter of 35 μm was insert-molded (transfer-molded) onto the surface of the metal member 50 using a general-purpose molding machine to form an insulating resin layer 10. In this way, a base material 70 composed of an aluminum plate (metal member) 50 and an insulating resin layer 10 was obtained. The size of the insulating resin layer 10 was 40 mm × 40 mm × 200 μm thick. The insulating resin layer 10 was formed in the center of the metal member 50.
[0069] (3) Formation of non-through holes A laser beam was applied to the area (wiring area 10A) on the surface 10a of the insulating resin layer 10 where the circuit wiring 20 was to be formed, to process the wiring area 10A. A 3D laser marker (Keyence, YVO4 laser, MD-9920A, 13W) was used for the laser processing (laser drawing).
[0070] First, a laser beam was irradiated to roughen the area (wiring area 10A) of the surface 10a of the insulating resin layer 10 where the circuit wiring 20 was to be formed. Specifically, a pattern of parallel lines arranged at a pitch of 40 μm was laser-drawn in the wiring area 10A (laser drawing conditions: line speed 2000 mm / s, frequency 40 kHz, power 20%). As a result, the surface roughness (Ra) of the wiring area 10A became 13 μm.
[0071] Next, a plurality of non-through holes (recesses) 11 were formed in the wiring region 10A by laser processing. Specifically, a pattern consisting of discontinuous lines as shown in FIG. 6 was laser-drawn in the wiring region 10A (laser drawing conditions: linear speed 30 mm / s, frequency 50 kHz, power 80%) to form a plurality of non-through holes 11. The number of laser drawings (repeated number of laser drawings) was one. The sizes of the laser-drawn patterns were as follows: N1=35 μm, N2=365 μm, N3=200 μm, N4=200 μm. The shape of the formed non-through holes 11 was a cone with its bottom surface located on the surface 10a (wiring region 10A), as shown in FIGS. 2(a) and (b).
[0072] The width D, depth d, and distance P between the formed through holes 11 and the non-through holes 11 were measured using a laser microscope (Keyence laser microscope VK-9700, objective lens 20x). For the depth d, the depth distribution of one non-through hole 11 was calculated, and the range with the largest depth value, which is less than 1% of cumulative frequency, was ignored as optical noise, and the depth value with a cumulative frequency of 1% was calculated as the depth d of that one non-through hole. For the width D, the area of the opening 11a of one non-through hole 11 was calculated, and the diameter when the shape of the opening 11a was considered to be a perfect circle was calculated as the width D of one non-through hole 11. For each of all non-through holes 11 present in the measurement field of view, the width D and depth d were obtained by the same method, and the average value of these widths D and depths d was further obtained.
[0073] As for the distance P between the non-through holes 11, first, the distance between the center of gravity of the opening 11a of one non-through hole 11 and the center of gravity of the opening 11a of the adjacent non-through hole 11 was measured. For all non-through holes 11 present within the measurement field of view, the distance between the centers of gravity of the adjacent openings 11a was obtained by the same method, and further, the average value of the distances between these centers of gravity was obtained. Next, the value obtained by subtracting the average value of the width D obtained earlier from the average value of the distances between the centers of gravity was determined as the distance P between the non-through holes 11.
[0074] The width D (average value) of the non-through holes 11 calculated as described above was 155 μm, the depth d (average value) was 178 μm, and the distance P between the non-through holes 11 was 128 μm. Therefore, the ratio d / D was 1.15. The calculated values of the width D, depth d of the through holes 11, the distance P between the non-through holes 11, and the ratio d / D are shown in Table 4.
[0075] (4) Formation of circuit wiring (a) Addition of electroless plating catalyst The substrate 70 having the non-through holes 11 formed therein was immersed for 5 minutes in a commercially available aqueous solution of palladium chloride (PdCl2) (Activator, manufactured by Okuno Chemical Industries Co., Ltd.) adjusted to 30° C. Then, the substrate was taken out of the aqueous solution of palladium chloride and washed with water.
[0076] (b) Electroless plating and electrolytic plating Next, the substrate was immersed for 10 minutes in an electroless nickel phosphorus plating solution (Top Nicoron LPH-L, pH 6.5, manufactured by Okuno Chemical Industries) adjusted to 60° C. A nickel phosphorus film (electroless nickel phosphorus plating film) was grown to a thickness of about 1 μm on the wiring region 10A.
[0077] On the nickel phosphorus film, a 95 μm electrolytic copper plating film, a 4.0 μm electroless nickel phosphorus plating film, and a 0.1 μm electroless gold plating film were further laminated in this order to form a circuit wiring 20. For the electrolytic copper plating, an electrolytic plating method with high uniform electrodeposition was used. For the electrolytic copper plating solution, a mixture of solution A: Top Lucina 2000 manufactured by Okuno Pharmaceutical Co., Ltd. and solution B: Coppergleam HS-200 manufactured by Rohm & Haas Electronic Materials Co., Ltd. was used. As a result, a circuit wiring 20 composed of an electroless plating film and an electrolytic plating film was formed in the wiring area 10A irradiated with the laser light.
[0078] (5) Mounting of mounting parts As the mounting components 30, surface-mounted high-brightness LEDs (NS2W123BT, manufactured by Nichia Chemical, 3.0 mm x 2.0 mm x height 0.7 mm) were used. First, as shown in FIG. 1, five mounting components 30 were placed on the circuit wiring 20 via room temperature solder. The interval between each mounting component 30 was set to 0.5 mm. Next, the substrate on which the LEDs were placed was placed in a reflow furnace (solder reflow). The substrate was heated in the reflow furnace, and the maximum temperature of the substrate was 240°C to 260°C, and the time during which the substrate was heated to the maximum temperature was about 1 minute. The mounting components 30 were mounted on the resin part 10 by solder, and the circuit component 100 of this embodiment shown in FIG. 1 was obtained.
[0079] [Examples 2 to 12] In Examples 2 to 12, circuit components 100 were manufactured in the same manner as in Example 1, except that the thickness of insulating resin layer 10, the laser drawing conditions, the sizes (N1 to N4) of the laser-drawn patterns shown in Fig. 6, and the thickness of the circuit wiring (thickness of the plating film) were changed as shown in Tables 1, 2, and 4. In Examples 5 to 12, a UV laser (Keyence, 3D laser marker, MD-U1000C, output 2.5 W) was used instead of the YVO4 laser used in Example 1.
[0080] Moreover, the width D, depth d, and distance P between non-through holes 11 were calculated by the same method as in Example 1. The calculated values of the width D, depth d, and distance P between non-through holes 11, and ratio d / D of the through holes 11 are shown in Tables 4 and 5.
[0081] [Example 13] In this example, a circuit component 300 shown in Figures 10(a) and (b) was manufactured. As shown in Figure 10(b), the thickness of the resin layer 310 of the circuit component 300 is not constant. Other configurations are the same as those of the circuit component 100 shown in Figure 1.
[0082] In this embodiment, the thinnest thickness X1 of the resin layer 310 is 75 μm, and the thickest thickness X2 is 450 μm. Since the insulating resin 310 contains filler (alumina particles) with a maximum particle diameter of 35 μm, it is difficult to mold the entire insulating resin 310 to a thickness of 75 μm, but it is possible to mold it by partially setting the thickness to 75 μm. By providing a region with a thin thickness (region with thickness X1) in a portion, the heat dissipation of the circuit component 300 is further improved. In addition, it is preferable to provide the thin thickness region (region with thickness X1) in a portion where the mounting component (LED) 30, which is a heat source, is mounted.
[0083] In this example, circuit component 300 was manufactured in the same manner as in Example 1, except that the thickness of insulating resin layer 310, the laser drawing conditions, the sizes (N1 to N4) of the laser drawing patterns shown in Fig. 6, and the thickness of the circuit wiring (thickness of the plating film) were changed as shown in Tables 2 and 5. In this example, the UV laser used in Example 5 was used to form non-through holes 11.
[0084] Moreover, the width D, depth d, and distance P between non-through holes 11 were calculated by the same method as in Example 1. The calculated width D, depth d, and distance P between non-through holes 11, and the ratio d / D are shown in Table 5.
[0085] [Example 14] In this example, a circuit component was manufactured in which the thickness of the resin layer 310 is not constant like the circuit component 300 shown in Figures 10(a) and (b), and which has a ceramic layer 60 like the circuit component 200 shown in Figure 9. The circuit component manufactured in this example has the same configuration as the circuit component 100 shown in Figure 1, except that the thickness of the resin layer is not constant and that a ceramic layer is included. In this example, the thinnest film thickness X1 of the resin layer was set to 65 µm, and the thickest film thickness X2 was set to 450 µm.
[0086] First, the same metal member as that used in Example 1 was degreased and chemically etched, and then hard anodized (TOA Denka, TAF-TR). As a result, an anodized film (anodized aluminum) was formed on the entire surface of the metal member. The thickness of the anodized film was 50 μm.
[0087] The circuit components of this example were manufactured by using metal members on which an anodized film was formed, in the same manner as in Example 1, except that the thickness of the insulating resin layer, the laser drawing conditions, the sizes (N1 to N4) of the laser-drawn patterns shown in Fig. 6, and the thickness of the circuit wiring (thickness of the plating film) were changed as shown in Tables 2 and 5. In this example, the UV laser used in Example 5 was used to form the blind holes.
[0088] Moreover, the width D, depth d, and distance P between non-through holes 11 were calculated by the same method as in Example 1. The calculated width D, depth d, and distance P between non-through holes 11, and the ratio d / D are shown in Table 5.
[0089] Furthermore, a cross-section of the circuit component of this example was observed using a microscope (Keyence, VH-6000). As shown in Fig. 11, it was observed that non-through holes were regularly formed in the insulating resin layer.
[0090] [Comparative Example 1] In this comparative example, instead of the non-through holes 11, a lattice pattern constituted by grooves (recesses) was formed over the entire surface of the wiring region 10A of the base material .
[0091] (1) Preparation of substrate A substrate having an insulating resin layer formed on a metal member was produced in the same manner as in Example 1, except that the thickness of the insulating resin layer was set to 150 μm.
[0092] (2) Formation of a grid pattern A grid pattern was formed by laser processing in the area (wiring area) on the surface of the insulating resin layer where circuit wiring was to be formed, under the laser drawing conditions shown in Table 3. The grid pattern had a pitch of 200 μm. The depth of the grooves forming the grid pattern (maximum depth of the laser processed portion) was 130 μm.
[0093] (3) Formation of circuit wiring and mounting of mounted components Circuit wiring was formed on the substrate on which the grid pattern was formed, and components were mounted in the same manner as in Example 1. This resulted in a circuit component of this comparative example. The electrolytic plating was performed under the same conditions as in Example 2 (plating solution composition, current density, time), and the average thickness of the circuit wiring was adjusted to be the same as in Example 2. The average thickness of the circuit wiring is shown in parentheses in Table 5.
[0094] [Comparative Examples 2 to 4] In Comparative Examples 2 to 4, similarly to Comparative Example 1, a lattice pattern composed of grooves (recesses) was formed over the entire wiring area of the substrate instead of the non-through holes 11. In Comparative Examples 2 to 4, circuit components were manufactured in the same manner as in Comparative Example 1, except that the thickness of the insulating resin layer 10, the laser drawing conditions, and the average thickness of the circuit wiring were changed as shown in Tables 3 and 5. In Comparative Examples 3 and 4, a UV laser (Keyence, 3D laser marker, MD-U1000C, output 2.5 W) was used instead of the YVO4 laser used in Comparative Example 1, and a lattice pattern with a pitch of 80 μm was laser-drawn.
[0095] [Comparative Example 5] In this comparative example, similarly to Comparative Example 1, instead of the non-through holes 11, a lattice pattern composed of grooves (recesses) was formed on the entire wiring area of the substrate. However, in this comparative example, a circuit component was manufactured in which the thickness of the resin layer 310 was not constant like the circuit component 300 shown in Figs. 10(a) and (b), and the ceramic layer 60 was included like the circuit component 200 shown in Fig. 9. The circuit component manufactured in this comparative example is similar to the circuit component manufactured in Comparative Example 1 in terms of configuration, except that the thickness of the resin layer is not constant and that the ceramic layer is included. In this comparative example, the thinnest film thickness X1 of the resin layer was set to 65 μm, and the thickest film thickness X2 was set to 450 μm.
[0096] First, the same metal member as that used in Comparative Example 1 was degreased and chemically etched, and then hard anodized (TOA Denka, TAF-TR). As a result, an anodized film (anodized aluminum) was formed on the entire surface of the metal member. The thickness of the anodized film was 50 μm.
[0097] A circuit component of this comparative example was manufactured by the same method as in Comparative Example 1, using a metal member on which an anodized film was formed, and changing the thickness of the insulating resin layer, the laser drawing conditions, and the average thickness of the circuit wiring as shown in Tables 3 and 5. In this comparative example, the UV laser used in Comparative Example 3 was used instead of the YVO4 laser used in Comparative Example 1.
[0098] [Comparative Examples 6 and 7] In Comparative Examples 6 and 7, a plurality of through holes 11 were formed in a region (wiring region 10A) of the surface 10a of the insulating resin layer 10 where the circuit wiring 20 was to be formed. In Comparative Examples 6 and 7, the circuit component 100 was manufactured in the same manner as in Example 1, except that the thickness of the insulating resin layer 10, the laser drawing conditions, the sizes (N1 to N4) of the laser drawing patterns shown in FIG. 6, and the thickness of the circuit wiring (thickness of the plating film) were changed as shown in Tables 3 and 5. In Comparative Examples 6 and 7, the UV laser used in Comparative Example 3 was used instead of the YVO4 laser used in Example 1.
[0099] Moreover, the width D, depth d of the through hole 11, and distance P between the non-through holes 11 were calculated by the same method as in Example 1. The calculated values of the width D, depth d of the through hole 11, distance P between the non-through holes 11, and ratio d / D are shown in Table 5. However, the depth d of the non-through hole 11 in Comparative Example 7 was obtained by cross-sectional observation.
[0100] [Table 1]
[0101] [Table 2]
[0102] [Table 3]
[0103] [Circuit component evaluation] The circuit components produced in Examples 1 to 14 and Comparative Examples 1 to 7 described above were evaluated as follows. The evaluation results are shown in Tables 4 and 5. In addition, in Tables 4 and 5, the following values for the circuit components of Examples 1 to 14 and Comparative Examples 1 to 7 are also shown in addition to the evaluation results. The width D and depth d of the non-through hole 11, the ratio d / D, the distance P between the non-through holes 11, the ratio P / D, the surface roughness (Ra) of the wiring area 10A, the ratio d / 5, the thickness B of the resin layer under the circuit wiring, the distance C, the thickness A of the circuit wiring, and the smaller value of D / 2 or d / 2. In addition, for Comparative Examples 1 to 5, instead of the depth d of the non-through hole 11 and the thickness A of the circuit wiring, the depth of the grooves forming the lattice pattern and the average thickness of the circuit wiring are shown in parentheses in Table 5.
[0104] (1) Adhesion test of circuit wiring (plating film) Apart from the circuit components produced in the above-mentioned Examples 1 to 14 and Comparative Examples 1 to 7, samples for adhesion tests in each Example and Comparative Example were produced by the following method. First, a base material was prepared, which was made of a metal member and an insulating resin layer made of the same material as those used in Examples 1 to 14 and Comparative Examples 1 to 7. Laser drawing was performed on the insulating resin layer of the base material in the same manner as in each Example and Comparative Example. An electroless nickel phosphorus plating film was formed to a thickness of 1 μm on the base material on which laser drawing was performed, and further, electrolytic copper plating of 40 μm was formed thereon to prepare a sample for adhesion tests. The size of the plating film on the sample was 2 mm wide and 40 mm long. The adhesion strength of the plating film of the measurement sample was measured by a vertical tensile test, and the adhesion of the circuit wiring (plating film) was evaluated according to the following evaluation criteria.
[0105] <Adhesion evaluation criteria> A: The adhesion strength of the plating film on the measurement sample was 15 N / cm or more. B: The adhesion strength of the plating film of the measurement sample was 10 N / cm or more and less than 15 N / cm. C: The adhesion strength of the plating film of the measurement sample was 1 N / cm or more and less than 3 N / cm. E: The adhesion strength of the plating film of the measurement sample was less than 1 N / cm.
[0106] (2) Insulation test of insulating resin layer In the circuit components produced in Examples 1 to 14 and Comparative Examples 1 to 7, a voltage of 500 V was applied between the circuit wiring 20 and the metal member 50, and the resistance between the circuit wiring 20 and the metal member 50 was measured using a tester, and the insulation of the insulating resin layer was evaluated based on the following insulation evaluation criteria. In Example 14 and Comparative Example 5, a part of the anodized aluminum layer in a place where the insulating resin layer was not formed was cut with a metal file to expose the metal member, and the resistance between the circuit wiring 20 and the metal member 50 was measured.
[0107] <Insulation evaluation criteria> A: The resistance value between the circuit wiring 20 and the metal member 50 was 5000 MΩ or more. B: The resistance value between the circuit wiring 20 and the metal member 50 was 100 MΩ or more and less than 5000 MΩ. C: The resistance value between the circuit wiring 20 and the metal member 50 was 1 MΩ or less. E: It was confirmed that the circuit wiring 20 and the metal member 50 were short-circuited.
[0108] (3) Heat dissipation test for circuit components In the circuit components produced in Examples 1 to 14 and Comparative Examples 1 to 7, a thermocouple was attached to the end of the mounted component (LED) 30, and then a constant current (0.8 A) was passed through the LED 30 to light it up, and the temperature of the LED 30 was measured 30 minutes after lighting. The average temperature of all the LEDs 30 on the circuit component was calculated, and the heat dissipation of the circuit component was evaluated according to the following evaluation criteria. However, for circuit components in which a short circuit between the circuit wiring 20 and the metal member 50 was confirmed in the insulation test of the insulating resin layer (2) above (evaluation result: E), this test was not performed because the current flows through the metal member and an accurate value cannot be measured.
[0109] <Evaluation criteria for heat dissipation of circuit components> A: The LED surface temperature was below 90°C 30 minutes after it was turned on. B: The LED surface temperature exceeded 90°C and was below 100°C 30 minutes after it was turned on. C: The LED surface temperature 30 minutes after being turned on was above 100°C and below 120°C. E: The LED surface temperature exceeded 120°C 30 minutes after it was turned on.
[0110] (4) Evaluation of flatness of circuit wiring (plating film) In the circuit components produced in Examples 1 to 14 and Comparative Examples 1 to 7, the plated surface of the circuit wiring 20 was observed using a microscope, and the difference between the maximum height and the minimum depth was measured from the cross-sectional profile (height profile) in the width direction of the circuit wiring. This measurement was performed in three fields of view, and the average value was taken as the surface roughness of the circuit wiring, and the flatness was evaluated based on the following flatness evaluation criteria.
[0111] <Flatness evaluation criteria> A: The surface roughness of the circuit wiring was 5 μm or less. B: The surface roughness of the circuit wiring was more than 5 μm and less than 10 μm. C: The surface roughness of the circuit wiring was more than 10 μm and less than 20 μm. E: The surface roughness of the circuit wiring exceeded 20 μm.
[0112] [Table 4]
[0113] [Table 5]
[0114] As shown in Tables 4 and 5, the circuit components produced in Examples 1 to 14 all had good evaluation results, and were compatible with high heat dissipation and high adhesion of the circuit wiring. Furthermore, it was confirmed that the circuit wiring and the metal member were reliably insulated, and the surface of the circuit wiring was flat. In addition, in the circuit components of Examples 1 to 14, the surface roughness (Ra) of the wiring region 10A was 1 / 5 or less of the depth d of the non-through hole 11, the ratio P / D was 0.3 to 3, the thickness A of the circuit wiring (plating film) 20 was larger than 1 / 2 of the depth d of the non-through hole 11 or larger than 1 / 2 of the width D, the width D of the non-through hole was 10 to 200 μm, the thickness B of the resin layer was 30 to 200 μm, and the distance C was 5 to 100 μm.
[0115] On the other hand, the flatness evaluation results were poor (Evaluation result: E) for Comparative Examples 1 to 5 in which a grid pattern made up of grooves (recesses) was formed over the entire surface of the wiring region 10A instead of forming the non-through holes 11. This is presumably because the unevenness formed over the entire surface of the wiring region 10A due to the grid pattern deteriorated the flatness of the plating film formed thereon.
[0116] Furthermore, in Comparative Examples 1, 3 and 5, in addition to the evaluation result of flatness, the evaluation result of insulation was also poor (evaluation result: E), and therefore a heat dissipation test was not performed. The cause of this is presumed to be as follows. When forming a lattice-like groove shape by laser drawing, the intersection parts are irradiated with laser light twice, so the variation in the depth of the grooves becomes large. Under microscope observation, only grooves shallower than the thickness of the insulating resin layer were observed. However, in the actual lattice pattern, there are places where grooves deeper than the thickness of the insulating resin layer are formed, and it is believed that this is why the insulation properties have deteriorated.
[0117] In addition to the evaluation result of flatness, the evaluation result of heat dissipation was also poor in Comparative Examples 2 and 4 (Evaluation result: E). The causes of this are presumed to be as follows. First, it is presumed that the thickness of the solder between the plating film and the mounted components was increased due to the decrease in the smoothness of the plating film. Second, it is presumed that the insulation of Comparative Examples 2 and 4 was improved by reducing the depth of the groove compared to Comparative Examples 1 and 3, but the adhesion between the plating film and the insulating resin layer was decreased (Evaluation result: C). It is presumed that this caused an increase in the thermal resistance from the plating film to the insulating resin layer. Furthermore, it is presumed that the third cause was that the thickness (distance C) of the insulating resin layer between the plating film and the metal member was increased due to the shallowing of the groove, resulting in a decrease in heat transfer to the metal member.
[0118] Moreover, in Comparative Example 6, in which the ratio d / D of the non-through holes 11 was less than 0.5, the evaluation results of adhesion and heat dissipation were poor (evaluation result: E). In Comparative Example 6, it is presumed that the heat dissipation was deteriorated due to the deterioration of adhesion between the plating film and the insulating resin layer and the increase in the thickness (distance C) of the insulating resin layer between the plating film and the metal member, similar to the second and third causes of the deterioration of heat dissipation in Comparative Examples 2 and 4 described above.
[0119] In addition, in Comparative Example 7, in which the ratio d / D of the non-through holes 11 is 5 or more, the evaluation result of the insulation was poor (evaluation result: E), and therefore the heat dissipation test was not performed. The cause of this is presumed to be as follows. In Comparative Example 7, the number of laser drawing was increased (number of laser drawing: 10 times) in order to deepen the non-through holes 11. In the cross-sectional observation, the thickness (distance C) of the insulating resin layer between the bottom of the non-through holes 11 and the metal member was 93 μm, but it is presumed that the insulating resin layer between the non-through holes 11 and the metal member became brittle due to the large number of laser drawing. It is presumed that the plating solution penetrated into the brittle insulating resin layer, causing the plating film to grow, which caused a short circuit between the circuit wiring (plating film) and the metal member. [Industrial Applicability]
[0120] The circuit component of the present invention has high heat dissipation properties, making it suitable for use in components that incorporate LEDs and other mounted components, and is applicable to smartphones and automobile components. [Explanation of symbols]
[0121] 10 Insulating resin layer 11 Non-through hole (recess) 20 Circuit wiring 30 Mounting parts (LED) 50 Metallic parts 70 Base material 100 Circuit Components
Claims
1. A circuit component, A metal member; an insulating resin layer formed on the metal member; a circuit wiring including a plating film formed on the insulating resin layer; a mounting component mounted on the circuit wiring and electrically connected to the circuit wiring; a plurality of non-through holes filled with the plating film are formed in a wiring region in which the circuit wiring is formed on a surface of the insulating resin layer; a ratio d / D of a depth d of the non-through hole to a width D of the non-through hole is 0.5 to 5; a ratio P / D of a distance P between the non-through holes to a width D of the non-through holes is 0.3 to 3; The width D of the non-through hole is 20 μm or more, And the depth d of the non-through hole is 24 μm or more, The non-through holes are formed in a scattered manner so that their density in the wiring region is approximately uniform.
2. 2. The circuit component according to claim 1, wherein a surface roughness (Ra) of said wiring region other than said non-through holes is 1 / 5 or less of a depth d of said non-through holes.
3. 3. The circuit component according to claim 1, wherein the thickness of the circuit wiring is greater than half the depth d or greater than half the width D of the non-through hole.
4. 4. The circuit component according to claim 1, wherein the non-through holes have a width D of 20 to 200 μm.
5. The circuit component according to any one of claims 1 to 4, wherein a thickness of the insulating resin layer at a portion sandwiched between the circuit wiring and the metal member and where the non-through holes are not formed is 30 to 200 µm.
6. 6. The circuit component according to claim 1, wherein the distance from the bottom of the non-through hole to the surface of the insulating resin layer facing the metal member is 5 to 100 μm.
7. 7. The circuit component according to claim 1, wherein the insulating resin layer contains a thermosetting resin.
8. 8. The circuit component according to claim 7, wherein the thermosetting resin is an epoxy resin.
9. 9. The circuit component according to claim 1, wherein the insulating resin layer contains an insulating thermally conductive filler.
10. 10. The circuit component according to claim 1, further comprising an inorganic oxide layer between the metal member and the insulating resin layer.
11. The circuit component according to any one of claims 1 to 10, wherein the mounting component is arranged with a surface on which a terminal is provided facing the circuit wiring, and the terminal and the circuit wiring are electrically connected by solder.
12. A method for producing a circuit component according to any one of claims 1 to 11, comprising the steps of: providing the metal member; forming the insulating resin layer on the metal member; forming the plurality of non-through holes by irradiating the wiring region of the insulating resin layer with a laser light; forming the circuit wiring in the wiring region by electrolytic plating; and mounting the component on the circuit wiring.
Citation Information
Patent Citations
Adhesive having excellent anchor characteristic and printed circuit board formed by using this adhesive and its production
JP1995188935A
Method of etching resin and resin product having surface etched thereby
JP2006120840A
Manufacturing method for heat sink integrated circuit molded body
JP3443872B2
Light source module, fabrication method therefor, and lighting device including the same
US20170009974A1
Circuit component
WO2019172405A1