DEVICE AND METHOD FOR MANUFACTURING SAME - Patent application
The lateral wiring process for micro-LED displays addresses high assembly costs and low yield by using a substrate with laterally separated electrodes, reducing stress and enabling cost-effective, high-yield large screen manufacturing with repair options.
Patent Information
- Application Number
- JP2022581005
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-06-28
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2040-06-28
AI Technical Summary
The high assembly costs and low yield of micro-LED displays are due to traditional bonding methods like wire bonding and flip-chip bonding, which are costly and prone to breakage, especially for large screens, and the gang bonding method struggles with thickness variations and stress issues.
A lateral wiring process using a substrate with laterally separated electrodes and metal wiring connects micro-LEDs, allowing for a mature wiring method that reduces stress and facilitates large screen manufacturing, with optional repair capabilities.
This approach lowers manufacturing costs and improves yield by using a mature wiring process, enabling high-resolution displays with repair options and flexibility for large screen production.
Smart Images

Figure 0007554852000006 
Figure 0007554852000012 
Figure 0007554852000002
Abstract
Description
[Technical field]
[0001] The present disclosure relates to devices and methods for manufacturing the same, in particular to displays and methods for manufacturing the same that use micro LEDs. [Background technology]
[0002] Various applications such as mobile phones, automotive displays, AR, VR, monitors, TVs, and large-screen displays require high resolution, high brightness, wide viewing angles, and low power consumption, increasing the need for displays using micrometer-sized LEDs (micro LEDs). Summary of the Invention [Problem to be solved by the invention]
[0003] However, one of the challenges of displays using micro LEDs is the high assembly cost. Traditionally, LEDs are connected one by one using bonding processes such as wire bonding and flip chip bonding, which results in high manufacturing costs. Therefore, the more pixels there are, the higher the manufacturing cost. For example, for a 4K display, about 25,000,000 micro LEDs are used. Even if the yield rate of micro LEDs is 99.99%, about 2500 micro LEDs need to be repaired.
[0004] As a method for reducing the assembly cost, there is a gang bonding method as shown in FIG. 1. The gang bonding method allows multiple micro LEDs 3 to be bonded to a substrate 1 at once via solder 2 by applying pressure to the multiple micro LEDs 3 by a bonding head 4. However, since the thicknesses of the multiple micro LEDs 3 may vary, a thickness variation absorbing film 5 is required to counteract the thickness difference. Even if the thickness variation absorbing film 5 is used, the thickness variation of the multiple micro LEDs 3 cannot be completely counteracted. As a result, different stresses may be applied to the multiple micro LEDs 3. In particular, the red light-emitting micro LED 3 may be made of fragile GaAs, so it is easily destroyed by excessive stress. Therefore, the production of devices using the gang bonding method has a low yield.
[0005] Also, the larger the area of the device, the greater the variation in the stress applied to the device. Moreover, the gang bonding method has a small area that can be bonded accurately at one time due to the limited size of the bonding head 4. Therefore, it is difficult to manufacture a large screen display by the gang bonding method.
[0006] In addition, manufacturers need to verify that the micro LEDs in their devices are working properly during and after the manufacturing process, but it is difficult to repair the micro LEDs once they are installed in the device.
[0007] Therefore, there is a need for a display and manufacturing method that has low manufacturing costs and high yields. [Means for solving the problem]
[0008] The first aspect of the present disclosure is A substrate; a first electrode on the substrate; a light-emitting element electrically connected to the first electrode by a first metal wiring; a second electrode electrically connected to the light-emitting element; Equipped with the first electrode and the light emitting element are laterally spaced apart from one another; The light emitting element is connected to the first metal wiring on the side facing the substrate. It is a device.
[0009] In the above aspects of the present disclosure, the device may further comprise a first aspect including a light-emitting element, and the thickness of the first dielectric layer may be equal to or greater than the thickness of the light-emitting element.
[0010] In the above aspects of the present disclosure, the first electrode may include a pad on the substrate and a first contact metal electrically connected to the pad, and the first metal wiring may be electrically connected to the first contact metal.
[0011] In the above aspects of the present disclosure, the device may further comprise an adhesive layer on the substrate, and the thickness of the pad may be equal to or less than the thickness of the adhesive layer.
[0012] In the above embodiment of the present disclosure, the device may further comprise a second dielectric layer on the first electrode, and at least one of the first dielectric layer and the dielectric layer may be made of a photosensitive transparent resin.
[0013] In the above aspects of the present disclosure, the device may comprise a plurality of light emitting elements having different thicknesses.
[0014] In the above aspects of the present disclosure, the light emitting device may be a vertical micro LED.
[0015] In the above aspect of the present disclosure, the device comprises: a third electrode on the substrate; a repair light emitting element electrically coupled to the third electrode; A fourth electrode electrically connected to the repaired light-emitting element; and The repair light emitting element may cover at least a portion of the third electrode.
[0016] In the above embodiments of the present disclosure, the second electrode and the fourth electrode may be a common electrode.
[0017] In the above embodiment of the present disclosure, the second electrode and the fourth electrode may be transparent electrodes.
[0018] A second aspect of the present disclosure is a method of manufacturing a device, comprising: disposing a light emitting device on a carrier; forming a first dielectric layer on the carrier such that the light emitting device is exposed; forming metal wiring on the light emitting device and the first dielectric layer; forming an adhesive layer on a substrate having pads; Bonding the carrier and the substrate, comprising: The metal traces on the carrier face the pads and the adhesive layer on the substrate; a step in which the light emitting element and the pad are laterally spaced apart from each other; removing the carrier; Etching the first dielectric layer and the adhesion layer down to the pad to form an opening; depositing a contact metal in the opening such that the pad and the metal wiring are electrically connected to each other; forming a second dielectric layer on at least the first dielectric layer such that the light emitting element is exposed; forming an electrode on the light-emitting device; The method includes:
[0019] In the above aspects of the present disclosure, the light emitting device may be a vertical micro LED.
[0020] In the above aspects of the present disclosure, the thickness of the first dielectric layer may be equal to or greater than the thickness of the light emitting element.
[0021] In the above aspects of the present disclosure, the light emitting element may include a plurality of light emitting elements having different thicknesses.
[0022] In the above aspects of the present disclosure, the thickness of the pad may be less than or equal to the thickness of the adhesive layer.
[0023] In the above-described aspect of the present disclosure, the step of arranging the light-emitting element on the carrier may include a step of transferring the light-emitting element prepared on the spare substrate to a spare carrier, and a step of transferring the light-emitting element transferred to the spare carrier to the carrier.
[0024] In the above aspects of the present disclosure, the electrode may be a common electrode.
[0025] In the above aspects of the present disclosure, the electrode may be a transparent electrode.
[0026] In the above embodiment of the present disclosure, at least one of the first dielectric layer and the dielectric layer may be made of a photosensitive transparent resin.
[0027] In the above aspect of the disclosure, the method comprises: testing the operation of the light emitting device prior to the step of forming the second dielectric layer; When the light-emitting element does not work, cutting the metal wiring connected to the light-emitting element that does not work; placing a repair light emitting element on the contact metal connected to the cut metal wiring; may include:
[0028] In the above aspects of the present disclosure, testing the operation of the light-emitting element may include electrically connecting a test carrier having a conductive layer to the light-emitting element.
[0029] In the above aspects of the present disclosure, the step of disposing the repair light-emitting element on the contact metal may include a step of bonding using solder.
[0030] In the above aspects of the present disclosure, the step of forming a second dielectric layer on at least the first dielectric layer may include forming the second dielectric layer in the opening such that the repair light-emitting element is exposed, and the step of forming an electrode on the light-emitting element includes forming an electrode on the repair light-emitting element. Effect of the Invention
[0031] Because the present disclosure uses a wiring process that is a mature technology, it can provide a display and a manufacturing method with low manufacturing cost and high yield. [Brief description of the drawings]
[0032] [Figure 1] 1 shows a prior art gang bonding method. [Diagram 2] 1 shows a device according to the present disclosure. [Diagram 3] 13 shows a step of transferring the light emitting elements prepared on the preliminary substrate to a preliminary carrier. [Figure 4] 13 shows a step of transferring the light emitting element transferred to the preliminary carrier to a carrier. [Diagram 5] The steps of forming a first dielectric layer on the carrier so that the light emitting element is exposed, and forming metal wiring on the light emitting element and the first dielectric layer are shown. [Figure 6] 4 illustrates the step of bonding the carrier to the substrate. [Figure 7] 4 shows the step of removing the carrier. [Figure 8] 4 shows the step of forming an opening by etching the first dielectric layer and the adhesion layer until the pad is reached. [Figure 9] 13 shows a step of depositing contact metal in the opening so that the pad and the metal wiring are electrically connected. [Figure 10] 4 shows steps for testing the operation of a light-emitting element. [Figure 11]13 shows a step of cutting the metal wiring connected to the non-operating light-emitting element when the light-emitting element does not operate. [Figure 12] 13 shows a step of placing a repair light emitting element on the contact metal connected to the cut metal wiring. [Figure 13] A step of forming a second dielectric layer over at least the first dielectric layer such that the light emitting element is exposed is shown. [Figure 14] 4 shows a step of forming an electrode on a light-emitting element. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0033] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. Although the following detailed description describes a display using micro LEDs, the present disclosure is applicable to optical communication devices using edge-emitting lasers, VCSELs (vertical cavity surface-emitting lasers), ToF modules (image sensors), laser printers, etc.
[0034] FIG. 2 illustrates a device 100 according to the present disclosure.
[0035] The device 100 of the present disclosure may include a substrate 10, a first electrode 20 including a pad 22 on the substrate 10 and a contact metal 24 electrically connected to the pad 22, an adhesive layer 26, a first dielectric layer 36, a light-emitting element 30 having an upper electrode 34 on the opposite side of the substrate 10 and a lower electrode 32 on the side facing the substrate 10, a metal wiring 28 having one end electrically connected to the contact metal 24 and the other end electrically connected to the lower electrode 32 of the light-emitting element 30, a second dielectric layer 40, and a second electrode 42 electrically connected to the upper electrode 34 of the light-emitting element 30. The metal wiring 28 electrically connects the first electrode 20 and the light-emitting element 30. The metal wiring 28 extends laterally from the contact metal 24 toward the light-emitting element 30. Also, the first electrode 20 and the light-emitting element 30 are laterally separated from each other. Here, the term "laterally" refers to a direction parallel to the surface of the substrate 10. For example, multiple elements being laterally separated means that the elements do not overlap in a top view, and multiple elements being laterally separated does not limit the elements to being in the same plane.
[0036] The device 100 of the present disclosure is manufactured by a mature wiring method without using a bonding method that applies high pressure, which improves the yield of the manufactured devices and makes it easier to manufacture large-sized devices, compared with a process using bonding that is highly likely to damage the light-emitting element 30.
[0037] In addition, the device 100 of the present disclosure may further include a repair light-emitting element 50. The repair light-emitting element 50 may be electrically connected to the contact metal 24 via the lower electrode 52 and the solder 56, and electrically connected to the second electrode 42 via its upper electrode 54.
[0038] Additionally, the device 100 of the present disclosure may include a malfunctioning NG light-emitting element 60. The NG light-emitting element 60 may be electrically connected at its bottom electrode 62 to the cut metal wiring 58 and at its top electrode 64 to the second electrode 42. Because the metal wiring is cut, no voltage is applied to the NG light-emitting element 60 between the first electrode 20 and the second electrode 42.
[0039] A method of manufacturing the device 100 of the present disclosure is described.
[0040] 3 shows a step of transferring the light-emitting element 30 prepared on the preliminary substrate 12 to the preliminary carrier 14. The preliminary carrier 14 may have a first adhesive 13. The preliminary substrate 12 is brought close to the preliminary carrier 14, so that the light-emitting element 30 on the preliminary substrate 12 comes into contact with the first adhesive 13 on the preliminary carrier 14. Thereafter, the light-emitting element 30 is removed from the preliminary substrate 12 by, for example, laser lift-off (LLO) using a laser 15, and transferred onto the preliminary carrier 14.
[0041] The preliminary substrate 12 may be a substrate commonly used in the art, for example, a sapphire substrate or a gallium nitride substrate.
[0042] The light emitting element 30 may be multiple light emitting elements, for example, a red light emitting element, a green light emitting element, and a blue light emitting element. The multiple light emitting elements may have different thicknesses. Because the device 100 of the present disclosure may include light emitting elements having different thicknesses, a multicolor display can be provided.
[0043] The light emitting element 30 may be a light emitting diode (LED). The LED may be a micro LED. A micro LED refers to an LED having a footprint of less than about 50 μm×50 μm, preferably less than 20 μm×20 μm, more preferably less than about 10 μm×10 μm. The micro LED may be a vertical micro LED. A vertical micro LED refers to an LED having a top electrode 34 and a bottom electrode 32. A vertical micro LED with vertical electrodes may have a smaller footprint, so that higher pixels per inch (PPI) may be achieved.
[0044] At least one electrode of the vertical micro LED faces the substrate 10. Therefore, in the prior art, the electrode facing the substrate is electrically connected to a pad on the substrate by a bonding method using solder or the like. This bonding method makes it difficult to accurately connect the micro LED and the substrate at one time. In contrast, in the present disclosure, the metal wiring 28 using a wiring method can be electrically connected to the micro LED 30 and the pad 22.
[0045] The first adhesive 13 may be an adhesive commonly used in the art, for example, the first adhesive 13 may be a heat curable adhesive such as an epoxy, acrylic, or silicone based adhesive, or a UV curable adhesive.
[0046] The pads 22 may be any pad commonly used in the art, for example, the pads 22 may be titanium, nickel, chromium, gold, copper, or alloys thereof.
[0047] Laser 15 may be a laser commonly used in the art. For example, laser 15 may be a UV laser emitting a wavelength of 200 to 400 nm, a green-emitting laser, or a near-infrared laser emitting a wavelength of 800 to 1,000 nm.
[0048] 4 shows a step of transferring the light-emitting element 30 transferred to the preliminary carrier 14 to the carrier 18. The carrier 18 may have a second adhesive 17. The preliminary carrier 14 is brought close to the carrier 18 so that the light-emitting element 30 on the preliminary carrier 14 comes into contact with the second adhesive 17 on the carrier 18. Next, the light-emitting element 30 is removed from the preliminary carrier 14, for example, by utilizing the difference in adhesive strength between the first adhesive 13 on the preliminary carrier 14 and the second adhesive 17 on the carrier 18, and the light-emitting element 30 is transferred onto the carrier 18. In this case, the adhesive strength of the second adhesive 17 on the carrier 18 is greater than the adhesive strength of the first adhesive 13 on the preliminary carrier 14.
[0049] As shown in the top view at the bottom right of FIG. 4, a plurality of light emitting elements 30 can be precisely positioned at predetermined positions on the carrier 18 .
[0050] The carrier 18 may be any carrier commonly used in the art. For example, the carrier 18 may be a carrier made of quartz or glass. The spare carrier 14 and the carrier 18 may be made of the same material or different materials.
[0051] The second adhesive 17 may be an adhesive commonly used in the art. For example, the second adhesive 17 may be a heat-curable adhesive, such as an epoxy, acrylic, or silicone-based adhesive, or a UV-curable adhesive. The first adhesive 13 and the second adhesive 17 may be made of the same material or different materials.
[0052] In the following Figures 5 to 14, top views and cross-sectional views along lines A-A', B-B', and C-C' of the top view of an embodiment of the present disclosure are shown.
[0053] 5 shows the steps of forming a first dielectric layer 36 on the carrier 18 so that the light-emitting element 30 is exposed, and forming metal wiring 28 on the light-emitting element 30 and the first dielectric layer 36. As shown in the cross section A-A', the first dielectric layer 36 is formed on the carrier 18. The first dielectric layer 36 includes the light-emitting element 30. The first dielectric layer 36 has a via through which the electrode 32 of the light-emitting element 30 is exposed. Then, the metal wiring 28 is formed on the first dielectric layer 36 and in the via, and one end of the metal wiring 28 is electrically connected to the light-emitting element 30.
[0054] The metal traces 28 are formed by lithography, for example using photoresist. A metal layer is deposited on the first dielectric layer 36 and in the vias, and photoresist is patterned on the metal layer. The metal layer is then patterned according to the photoresist pattern by etching. The photoresist is then removed to form the metal traces 28.
[0055] The first dielectric layer 36 may include a photosensitive material or a non-photosensitive material such as a thermosetting material. Preferably, the first dielectric layer 36 may include a photosensitive material. More preferably, the first dielectric layer 36 may include a photosensitive resin. When the first dielectric layer 36 includes a photosensitive resin, it is easy to form vias by lithography. Also, the flexibility of the device can be increased, enabling the production of large-sized devices.
[0056] The metal traces 28 may be any conductive material, including metal, any conductive metal or conductive metal oxide, and preferably, one or more selected from the group consisting of copper, nickel, titanium, chromium, and indium tin oxide (ITO).
[0057] The thickness of the first dielectric layer 36 can be equal to or greater than the thickness of the light-emitting element 30. Because a portion of the light-emitting element 30 is covered by the first dielectric layer 36, the mechanical strength of the device is increased. Thus, the yield of the device can be improved, enabling the manufacture of large-sized devices.
[0058] Thereafter, a substrate 10 having pads 22 is provided, and an adhesive layer 26 is formed on the substrate 10 .
[0059] 6 shows a step of bonding the carrier 18 and the substrate 10. The metal wiring 28 on the carrier 18 can face the pads 22 and the adhesive layer 26 on the substrate 10. The metal wiring 28 can be precisely aligned with the pads 22. The carrier 18 is brought close to the substrate 10, and the carrier 18 and the substrate 10 are bonded by the adhesive layer 26, so that the light-emitting element 30 and the pads 22 are laterally spaced apart from each other. The pads 22 and the light-emitting element 30 are laterally spaced apart and electrically connected by the metal wiring 28.
[0060] The substrate 10 may be a substrate commonly used in the art, for example, a driving substrate in which TFTs are formed on a glass substrate.
[0061] The adhesive layer 26 may be a heat curable adhesive, such as an epoxy, acrylic, or silicone based adhesive, or a UV curable adhesive. In this way, the flexibility of the device can be increased, allowing the production of large sized devices.
[0062] The thickness of the pad 22 can be equal to or less than the thickness of the adhesive layer 26. In this way, during the step of bonding the carrier 18 and the substrate 10, the metal wiring 28 does not come into contact with the pad 22, so that no undesirable stress is generated. Therefore, the yield of the device can be improved, and it is possible to manufacture a large size device.
[0063] 7 shows a step of removing the carrier 18. The removal of the carrier 18 may be performed using techniques known in the art, such as laser lift-off (LLO) and mechanical removal. For example, a UV laser that transmits through the carrier 18 is irradiated onto the second adhesive 17, and the carrier 18 is peeled off from the second adhesive 17. Although not shown, after the carrier 18 is removed, the second adhesive 17 may be removed, and the upper electrode 34 of the light-emitting element 30 may be exposed.
[0064] 8 shows the step of forming an opening 38 by etching the first dielectric layer 36 and the adhesion layer 26 until the pad 22 is reached. The metal trace 28 may act as a mask for the etch. After etching, the pad 22 and the metal trace 28 may be exposed in the opening 38.
[0065] In this step, the pads 22 and the metal wiring 28 do not necessarily have to be electrically connected.
[0066] Etching may be performed using techniques well known in the art, for example, etching may be performed by reactive ion etching, such as oxygen plasma etching.
[0067] 9 shows a step of depositing contact metal 24 in opening 38 so that pad 22 and metal wiring 28 are electrically connected. Pad 22 and contact metal 24 may constitute first electrode 20. In this manner, pad 22 and light-emitting element 30 may be electrically connected via contact metal 24 and metal wiring 28. Deposition of contact metal 24 may be performed by sputtering, photoresist formation, etching of a metal layer, etc.
[0068] 10 to 12 show steps from testing the operation of the light emitting element 30 to disposing a repair light emitting element 50. These steps are optional. They may be performed before the step of forming the second dielectric layer 40.
[0069] 10 shows a step of testing the operation of the light-emitting element 30. This step may include electrically connecting a test carrier 68 having a conductive layer 66 to the light-emitting element 30. The test carrier may be made of glass. The conductive layer 66 may be a conductive sheet with a low elastic modulus. Since the conductive layer 66 has a low elastic modulus, the conductive layer 66 and the top electrode 34 of the light-emitting element 30 may be electrically connected by applying an appropriate pressure.
[0070] Thereafter, it is possible to test whether the light-emitting element 30 operates normally by applying a voltage between the pad 22 and the conductive layer 66 to generate electroluminescence (EL) of the light-emitting element 30. Instead of EL, it is possible to use photoluminescence (PL) to test the operation of the light-emitting element 30. When PL is used, it is possible to test whether the light-emitting element 30 operates normally by generating PL in the light-emitting layer of the light-emitting element 30 with excitation light such as ultraviolet light.
[0071] 11 shows a step of cutting the metal wiring 28 connected to the malfunctioning light-emitting element 60. When the light-emitting element 30 does not operate normally, for example, when it does not emit light or when the light-emitting intensity is less than a predetermined value, such a light-emitting element 30 is called an NG light-emitting element 60. The metal wiring 28 connected to the NG light-emitting element 60 is cut by, for example, a laser 70, and the NG light-emitting element 60 and the pad 22 lose the electrical connection therebetween.
[0072] Laser 70 may be any laser commonly used in the art, for example, laser 70 may be a UV laser emitting a wavelength of 200-400 nm, a green-emitting laser, a near-infrared laser emitting a wavelength of 800-1,000 nm, or a CO2 laser emitting a wavelength around 10 microns.
[0073] 12 shows a step of placing the repaired light-emitting element 50 on the contact metal 24 connected to the cut metal wiring 58. This step may include bonding the bottom electrode 52 of the repaired light-emitting element 50 to the contact metal 24 using solder 56. The repaired light-emitting element 50 may be electrically connected to the first electrode 20 on the substrate 10. The solder 56 may be formed on the bottom electrode 52 or on the contact metal 24 of the repaired light-emitting element 50. The repaired light-emitting element 50 may cover at least a portion of the first electrode 20, including the contact metal 24 and the pad 22.
[0074] 10 to 12, testing of the operation of the light-emitting element 30 and disposing of a repaired light-emitting element 50 are performed. In this manner, testing and repair of the light-emitting element 30 can be easily performed in the process of the present disclosure.
[0075] 13 illustrates forming a second dielectric layer 40 on at least the first dielectric layer 36 such that the light emitting element 30 is exposed. Optionally, this step may include forming a second dielectric layer 40 on at least the first dielectric layer 36 such that the repair element 50 is exposed.
[0076] The second dielectric layer 40 may have a via through which the top electrode 34 of the light-emitting element 30 is exposed. Optionally, the second dielectric layer 40 may have a via through which the top electrode 54 of the repair element 50 is exposed.
[0077] Also, the second dielectric layer 40 may be formed in the opening 38 on at least one of the substrate 10, the pad 22, the contact metal 24, the adhesion layer 26, and the metal wiring 28. The second dielectric layer 40 may be formed on the first electrode 20.
[0078] The second dielectric layer 40 may include a photosensitive material or a non-photosensitive material such as a thermosetting material. Preferably, the first dielectric layer 36 may include a photosensitive material. More preferably, the first dielectric layer 36 may include a photosensitive resin. When the second dielectric layer 40 includes a photosensitive resin, it is easy to form a via by dry etching. Also, the flexibility of the device can be increased, enabling the production of large-sized devices. The first dielectric layer 36 and the second dielectric layer 40 may be made of the same material or different materials.
[0079] 14 shows a step of forming a second electrode 42 on the light-emitting element 30. The second electrode 42 may be electrically connected to the top electrode 34 of the light-emitting element 30. The second electrode 42 may be formed on the second dielectric layer 40. The second electrode 42 may be a common electrode electrically connected to multiple light-emitting devices 30. The second electrode 42 may also be a transparent electrode.
[0080] Optionally, forming the second electrode 42 on the light-emitting element 30 may include forming the second electrode 42 on the repair light-emitting element 50. The second electrode 42 may be electrically connected to the top electrode 54 of the repair light-emitting element 50. The second electrode 42 may be a common electrode electrically connected to the repair light-emitting element 50 and the light-emitting element 30.
[0081] As described above, the device 100 of the present disclosure is manufactured. In the manufacturing process of the present disclosure, the metal wiring 28 is formed by a mature wiring method. A bonding method is used in the step of placing the repair light-emitting element 50 on the contact metal 24, but no bonding method is used in other steps.
[0082] Therefore, the present disclosure can provide a display using micro LEDs and a manufacturing method thereof that has high yield, is applicable to large screens, and allows repair of the micro LEDs if necessary. [Explanation of symbols]
[0083] 1 Board 2 Solder 3 LED 4 Bonding head 5. Thickness variation absorbing film 10 Substrate 12 Spare board 13 The First Adhesive 14 Spare Carrier 15 Laser 17 The Second Glue 18 Career 20 First electrode 22 Pad 24 Contact Metal 26 Adhesive layer 28 Metal wiring 30 Light emitting element, micro LED 32 Lower electrode 34 Upper electrode 36 First Dielectric Layer 38 Opening 40 Second dielectric layer 42 Second electrode 50 Repair light emitting element 52 Lower electrode 54 Upper electrode 56 Solder 58 Cut metal wiring 60 NG light emitting element 62 Lower electrode 64 Upper electrode 66 Conductive Layer 68 Test Carrier 70 Laser 100 devices
Claims
1. A substrate; a first electrode on the substrate; a normally operating light emitting element electrically connected to the first electrode by a first metal wiring; a second electrode electrically connected to the light emitting element; a third electrode provided in the first opening and connected to the first metal wiring; a fourth electrode provided in the first opening and constituting a common electrode together with the second electrode; a first' electrode on the substrate; a malfunctioning NG light-emitting element electrically connected to the first electrode by a first metal wiring; a second electrode electrically connected to the NG light emitting element; a third electrode provided in the second opening and connected to the first metal wiring; a repair light emitting element electrically coupled to the third electrode; a fourth electrode provided in the second opening, electrically connected to the repair light emitting element, and constituting a common electrode together with the second electrode; Equipped with the first electrode and the light emitting element are laterally spaced apart from one another; the light emitting element is connected to the first metal wiring on a side facing the substrate, the first electrode and the NG light emitting element are laterally spaced apart from each other; the NG light emitting element is connected to the first' metal wiring on the side facing the substrate, the first' metal wiring is cut between the first' electrode and the third' electrode; device.
2. A first dielectric layer including the light emitting element is further provided, The device of claim 1 , wherein a thickness of the first dielectric layer is equal to or greater than a thickness of the light emitting element.
3. 3. The device of claim 2, wherein the first electrode comprises a pad on the substrate and a first contact metal electrically connected to the pad, and the first metal wiring is electrically connected to the first contact metal.
4. The device of claim 3 , further comprising an adhesive layer on the substrate, the pad having a thickness equal to or less than a thickness of the adhesive layer.
5. 5. The device of claim 4, further comprising a second dielectric layer on the first electrode, at least one of the first dielectric layer and the dielectric layer being made of a photosensitive transparent resin.
6. The device according to claim 1 , comprising a plurality of the light-emitting elements having different thicknesses.
7. 7. The device of claim 1, wherein the light emitting element is a vertical micro LED.
8. The device of claim 1 , wherein the second electrode and the fourth electrode are transparent electrodes.
9. 1. A method of manufacturing a device, comprising: disposing a light emitting device on a carrier; forming a first dielectric layer on the carrier such that the light emitting device is exposed; forming metal wiring on the light emitting device and the first dielectric layer; forming an adhesive layer on a substrate having pads; Bonding the carrier and the substrate, the metal traces on the carrier face the pads and the adhesive layer on the substrate; the light emitting element and the pad are laterally spaced from one another; removing the carrier; Etching the first dielectric layer and the adhesion layer down to the pad to form an opening; depositing a contact metal in the opening such that the pad and the metal wiring are electrically connected to each other; testing the operation of the light emitting device; When the light emitting element does not operate normally, cutting the metal wiring connected to the light emitting element that does not operate normally; placing a repair light emitting element on the contact metal connected to the cut metal wiring; forming a second dielectric layer on at least the first dielectric layer such that the light emitting element is exposed; forming an electrode on the light-emitting element; A method comprising:
10. The method of claim 9 , wherein the light emitting element is a vertical micro LED.
11. 11. The method according to claim 9 or 10, wherein the thickness of the first dielectric layer is equal to or greater than the thickness of the light emitting element.
12. 12. The method of claim 9, wherein the light emitting element comprises a plurality of light emitting elements having different thicknesses.
13. 13. The method according to any one of claims 9 to 12, wherein the thickness of the pad is equal to or less than the thickness of the adhesive layer.
Citation Information
Patent Citations
Display device and method of manufacturing display device
JP2020088392A
Display apparatus
US20170336690A1
Display device using semiconductor light emitting device
US20180277589A1