Magnetoresistance element for two-dimensional magnetic sensors with reduced hysteresis response

The magnetoresistive element addresses hysteresis issues by employing a sensing layer with a defined magnetization ratio and structured sublayers to minimize stray fields, improving sensitivity and signal-to-noise ratio and extending sensor life.

JP7555484B2Active Publication Date: 2024-09-24ALLEGRO MICROSYSTEMS LLC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023515805
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-09-18
Filing Date
2021-09-14
Publication Date
2024-09-24
Estimated Expiration
2041-09-14

AI Technical Summary

Technical Problem

Conventional magnetoresistive elements exhibit hysteresis in response to angular variations of external magnetic fields due to stray magnetic fields induced by saturated sensing magnetization, which disrupts exchange coupling and affects sensitivity and signal-to-noise ratio.

Method used

The magnetoresistive element incorporates a sensing layer with a specific magnetization ratio defined by ΔM = M SFM1 / M SFM2, where M SFM1 and M SFM2 are the spontaneous magnetizations of the first and second sensing sublayers, respectively, and t FM1 and t FM2 are their thicknesses, with the second sublayer having increased magnetization away from the spacer layer to reduce net stray magnetic fields.

Benefits of technology

This configuration significantly reduces hysteresis, enhances sensitivity, improves signal-to-noise ratio, and increases sensor lifetime by minimizing stray magnetic fields, thereby optimizing the angular response.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555484000014
    Figure 0007555484000014
  • Figure 0007555484000008
    Figure 0007555484000008
  • Figure 0007555484000011
    Figure 0007555484000011
Patent Text Reader

Abstract

To improve the sensitivity, signal-to-noise ratio, and sensor life of a magnetic sensor. The present invention provides a magnetoresistive element (10) for a two-dimensional magnetic sensor, the magnetoresistive element (10) comprising a tunnel barrier layer (22) included between a reference layer (21) having a reference magnetization (210) and a sense layer (23) having a sense magnetization (230); the sensing layer (23) comprises a synthetic antiferromagnetic (SAF) structure comprising a ferromagnetic first sensing sublayer (231) in contact with the tunnel barrier layer (22) and separated from a ferromagnetic second sensing sublayer (232) by a first nonmagnetic spacer layer (233), whereby the first sensing sublayer (231) is antiferromagnetically coupled to the second sensing sublayer (232); The sensing layer (23) is configured such that the sensing magnetization ratio (ΔM) is defined by the following equation: TIFF2023545902000005.tif11170In the above formula, M SFM1 and M SFM2 are the spontaneous magnetizations of the first and second sensing sublayers (231, 232), respectively, and t FM1 and t FM2 are the thicknesses of the first and second sensing sublayers (231, 232), respectively, and the sensing magnetization ratio (ΔM) is between 0.1 and 0.25.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a magnetoresistive element adapted to sense an external magnetic field and having reduced hysteresis in its response to a changing angle of the external magnetic field.The present invention further relates to a two-dimensional (2D) magnetic sensor having a plurality of magnetoresistive elements. [Background technology]

[0002] 1 shows a conventional magnetoresistive element 10 comprising a reference layer 21 having a reference magnetization 210, a tunnel barrier layer 22, and a sense layer 23 having a sense magnetization 230. In FIG. 1, the reference layer 21 comprises a synthetic antiferromagnetic (SAF) structure comprising a first reference sublayer 211 separated from a second reference sublayer 212 by a first nonmagnetic spacer layer 213 such that the first reference sublayer 211 is antiferromagnetically coupled to the second reference sublayer 212.

[0003] The sensor application of the magnetoresistive element 10 requires that the reference magnetization 210 is fixed so that it cannot be oriented by the external magnetic field to be measured. To that end, the reference magnetization 210 is pinned by a pinning layer 24, such as an antiferromagnetic layer, by exchange coupling. In contrast, the sense magnetization 230 is free to be aligned by the external magnetic field to be sensed.

[0004] Furthermore, to obtain good sensitivity to the external magnetic field being measured, the sense magnetization 230 is saturated. However, the saturated sense magnetization 230 induces a local stray magnetic field that couples with the reference layer 21 in a closed flux configuration, indicated by numeral 55 in FIG. 1. The magnitude of the local stray magnetic field 55 can reach values ​​of up to 1000 Oe at the edges of the magnetoresistive element 10.

[0005] The pinning layer 24 typically contains a certain amount of thermally unstable grains that can switch when an external magnetic field is applied. A stray magnetic field 55 can locally disturb the exchange coupling of the pinning layer 24, resulting in hysteresis in the response of the magnetoresistance element 10 when the angle of the external magnetic field is changed. Figure 2 reports the simulated response of a 2D sensor with a magnetoresistance element 10 such as that of Figure 1 when the external magnetic field is rotated clockwise (positive angle) and counterclockwise (negative angle). Hysteresis is seen between clockwise and counterclockwise rotation.

[0006] Possible solutions aimed at minimizing such hysteresis include strengthening the exchange coupling between the pinning layer 24 and the reference layer 21. Alternatively, the reference layer 21 could contain a ferromagnetic material with a higher exchange stiffness, for example a Co-rich alloy. However, alloys with high exchange stiffness and compatible with tunnel magnetoresistance technology are very limited. Another possible solution would include reducing the thickness of the sense layer 23 to reduce the stray magnetic field 55. However, this is detrimental to the signal-to-noise ratio of the magnetoresistance element 10. Other solutions would include optimizing the growth of the pinning layer 24 and using a larger magnetoresistance element 10 so that the relative contribution of the edges of the magnetoresistance element 10 reduces the response signal. The latter two solutions are not satisfactory.

[0007] Patent Document 1 discloses a laminated structure in which a tunnel barrier layer is sandwiched between a magnetization fixed layer, each of which has a multi-layer structure, and a magnetization free layer, each of which has a multi-layer structure. The magnetization fixed layer, each of which has a multi-layer structure, the tunnel barrier layer, and the magnetization free layer, each of which has a multi-layer structure, are laminated in this order on a substrate.

[0008] US Pat. No. 5,999,333 discloses a read sensor with an unbalanced SAF free layer structure. The unbalanced SAF free layer structure includes a first magnetic layer having a first magnetic moment value and a second magnetic layer having a second magnetic moment value different from the first magnetic moment value. A separation layer is provided between the first magnetic layer and the second magnetic layer. The first magnetic layer and the second magnetic layer are antiferromagnetically coupled. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] US Patent Application Publication No. 2010 / 316890 [Patent Document 2] US Patent Application Publication No. 2017 / 140781 Summary of the Invention

[0010] The present disclosure relates to a magnetoresistive element comprising a tunnel barrier layer included between a reference layer having a reference magnetization and a sense layer having a sense magnetization. The sense layer comprises an SAF structure including a ferromagnetic first sense sublayer in contact with the tunnel barrier layer and separated from a ferromagnetic second sense sublayer by a first nonmagnetic spacer layer such that the first sense sublayer is antiferromagnetically coupled to the second sense sublayer. The sense layer is configured to have a sense magnetization ratio defined as:

[0011]

number

[0012] In the above formula, M SFM1 and M SFM2 are the spontaneous magnetizations of the first and second sensing sublayers, respectively, and t FM1 and t FM2 are the thicknesses of the first and second sense sublayers, respectively. The sense magnetization ratio is between 0.1 and 0.25. The second sense sublayer has a spontaneous magnetization that increases with increasing distance from the sense spacer layer.

[0013] The present disclosure further relates to a two-dimensional (2D) magnetic sensor comprising a plurality of the magnetoresistive elements disclosed herein.

[0014] The ratio of the magnetic moments results in a non-null magnetic moment in the sense layer, and the net stray field above the location of the pinned layer is significantly suppressed. Effect of the Invention

[0015] The magnetoresistive elements disclosed herein have reduced hysteresis response when measuring an angularly varying external magnetic field, have improved sensitivity, signal-to-noise ratio, and have better sensor lifetime.

[0016] The invention further relates to a 2D magnetic sensor having a plurality of magnetoresistive elements.

[0017] Exemplary embodiments of the invention are disclosed in the description and illustrated by the drawings. [Brief description of the drawings]

[0018] [Figure 1] FIG. 1 is a schematic diagram of a conventional magnetoresistance element. [Diagram 2] FIG. 2 reports the simulated response of a 2D sensor including the magnetoresistive element of FIG. [Diagram 3] FIG. 3 illustrates a schematic of a magnetoresistive element comprising a reference layer, a sense layer, and a tunnel barrier layer, according to one embodiment, where the sense layer comprises a sense SAF structure including a first sense sublayer separated from a second sense sublayer by a non-magnetic sense spacer layer. [Figure 4] FIG. 4 reports the ratio of the SAF stray field of the magnetoresistive element of the invention to the FM stray field of a conventional magnetoresistive element as a function of the ratio of the magnetic moment of the first sense sublayer to the magnetic moment of the second sense sublayer. [Diagram 5] FIG. 5 reports the ratio of the SAF stray field to the FM stray field as a function of the thickness of the second sense sublayer of the magnetoresistive element of the invention. [Figure 6] FIG. 6 shows the change in signal measured by a magnetoresistive element of the invention as a function of the angle of the external magnetic field. [Figure 7] FIG. 7 shows a magnetoresistive element according to another embodiment. [Figure 8] FIG. 8 shows details of the second sensing sublayer according to another embodiment. [Figure 9]FIG. 9 shows a magnetoresistive element according to yet another embodiment. [Figure 10] FIG. 10 shows a magnetoresistive element according to yet another embodiment. [Figure 11] FIG. 11 shows details of the sensing layer, according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] 3, a magnetoresistive element 10 is shown with a reference layer 21 having a reference magnetization direction 210 and a sense layer 23 having a sense magnetization direction 230. A tunnel barrier layer 22 is provided between the reference layer 21 and the sense layer 23. The reference layer 21 comprises a reference SAF structure with a first reference sublayer 211, a second reference sublayer 212 in contact with the tunnel barrier layer 22, and a non-magnetic reference spacer layer 213 between the first reference sublayer 211 and the second reference sublayer 212 such that the first reference sublayer 211 is antiferromagnetically coupled to the second reference sublayer 212. The sense layer 23 comprises a sense SAF structure with a first sense sublayer 231 in contact with the tunnel barrier layer 22 and separated from the second sense sublayer 232 by a non-magnetic first sense spacer layer 233 such that the first sense sublayer 231 is antiferromagnetically coupled to the second sense sublayer 232.

[0020] Preferably, the sense magnetization layer 230 is saturated.

[0021] In one embodiment, the magnetic moment of first sensing sublayer 231 is smaller than the magnetic moment of second sensing sublayer 232 . More specifically, the sense magnetization ratio ΔM, ie, the ratio of the magnetic moment of the first sensing sublayer 231 to the magnetic moment of the second sensing sublayer 232, can be defined by the following equation (1):

[0022]

number

[0023] In the above formula, M SFM1 corresponds to the spontaneous magnetization of the first sensing sublayer 231, and tFM1 corresponds to the thickness of the first sensing sublayer 231, and M SFM2 corresponds to the spontaneous magnetization of the second sensing sublayer 232, and t FM2 corresponds to the thickness of the second sensing sublayer 232.

[0024] In a preferred embodiment, the sensed magnetization ratio ΔM is between 0.1 and 0.25.

[0025] Figure 4 shows the SAF stray magnetic field H AFM and FM stray magnetic field H FM as a function of the sensed magnetization ratio ΔM, where the SAF stray field H AFM corresponds to the net stray magnetic field 55 generated by the sensing SAF structure 23, i.e., the stray magnetic fields arising from the different sensing sublayers 231, 232. The FM stray magnetic field H FM corresponds to the stray magnetic field generated by a sensing layer 23 comprising a single ferromagnetic layer or several ferromagnetically coupled ferromagnetic layers. The SAF stray magnetic field H AFM was calculated for a first sensing sublayer 231 having a thickness of 2 nm and a second sensing sublayer 232 having a thickness between 2 nm and 6 nm. The FM stray field H FM was calculated for ferromagnetic layers with thicknesses between 0 and 4 nm. Figure 4 shows that a sense magnetization ratio ΔM of 0.2 corresponds to a FM stray field H FM SAF stray magnetic field H AFM This shows that it results in a ratio of

[0026] Figure 5 shows the SAF stray magnetic field H AFM FM stray magnetic field H FM is reported as a function of the thickness of the second sensing sublayer 232. The first sensing sublayer 231 has a thickness of 2 nm. AFM and FM stray magnetic field H FM is zero and the sense magnetization ratio ΔM is zero, the sense layer 23 loses the ability to sense external magnetic fields. This corresponds to the second sense sublayer 232 having a thickness of 3 nm in the example of FIG.

[0027] A sense magnetization ratio ΔM between 0.1 and 0.25 provides good sensitivity of the magnetoresistive element 10 to an external magnetic field. Furthermore, the net stray magnetic field 55 on the reference layer 21 is reduced so that the response of the magnetoresistive element 10 to an angularly varying external magnetic field exhibits substantially no hysteresis. FIG. 6 shows the change in signal (e.g., resistance) measured by the magnetoresistive element 10 as a function of the angle of the measured external magnetic field. Here, the net stray magnetic field 55 generated by the sense layer 23 has a magnitude of 400 Oe. Little hysteresis is observed.

[0028] The magnetoresistive element 10 described herein provides lower magnetic noise and higher tunneling magnetoresistance (TMR) through the use of thick magnetic layers in the sense layer 23. The reduction in the net stray magnetic field 55 generated by the sense layer 23 and acting on the pinned reference layer 21 can further enhance high temperature stability, improve lifetime stability, and improve overall performance.

[0029] As shown in FIGS. 4 and 5 , by selecting the thicknesses of the first and second sensing sublayers 231, 232, by selecting the compositions of the first and second sensing sublayers 231, 232, and / or by other variables of the sensing layer 23, the ratio of the magnetic moments of the first and second sensing sublayers 231, 232 can be varied to optimize the net stray magnetic field 55.

[0030] In one aspect, the first and second sensing sublayers 231, 232 may contain a ferromagnetic material such as a ferromagnetic alloy based on any one of Fe, Co, and Ni (iron, cobalt, and nickel), for example, CoFe or NiFe (cobalt iron or nickel iron). At least one of the first and second sensing sublayers 231, 232 may further contain a nonmagnetic element such as B, Ta, Ru, or W (boron, tantalum, ruthenium, and tungsten), or a combination of these elements. More specifically, the first sensing sublayer 231 contains a nonmagnetic element to dilute the ferromagnetic material constituting the first sensing sublayer 231 and reduce its spontaneous magnetization 230.

[0031] In another aspect, the second sensing sublayer 232 has a greater thickness than the first sensing sublayer 231 .

[0032] In one aspect, the first sensing spacer layer 233 may include a non-magnetic material, such as, but not limited to, Ru, W, Mo, or Ir (ruthenium, tungsten, molybdenum, iridium), or a combination of these elements.

[0033] 7, another embodiment of the magnetoresistive element 10 is shown in which a first sense sublayer 231 is antiferromagnetically coupled to a second sense sublayer 232 that has a gradient of sense spontaneous magnetization 230. More specifically, the sense spontaneous magnetization 230 in the second sense sublayer 232 increases as the distance from the first sense spacer layer 233 increases.

[0034] The net spontaneous magnetization 230 of the second sensing sublayer 232 may be adjusted to compensate for the spontaneous magnetization 230 of the first sensing sublayer 231 to adjust the sense magnetization ratio ΔM, for example, between 0.1 and 0.25, where M SFM2 corresponds to the net spontaneous magnetization of the second sensing sublayer 232.

[0035] Since the magnitude of the stray magnetic field 55 decreases as the cube of the distance, the larger sense magnetization 230 in the portion of the second sensing sublayer 232 farthest from the reference layer 21 does not contribute significantly to the net stray magnetic field 55 at the level of the reference layer 21. On the other hand, the larger the sense magnetization 230, the larger the TMR of the magnetoresistive element 10 can be.

[0036] The second sensing sublayer 232 has a sense spontaneous magnetization 230 that is smaller, e.g., at least two times smaller, than the sense spontaneous magnetization 230 of the first sensing sublayer 231, and therefore generates a smaller net magnetic stray field 55 on the reference layer 21. At the level of the reference layer 21, the net magnetic stray field 55 generated by the second sensing sublayer 232 is smaller than the net magnetic stray field generated by the first sensing sublayer 231.

[0037] In one aspect, the second sensing sublayer 232 comprises a gradient of non-magnetic impurities. More specifically, the second sensing sublayer 232 includes a concentration of non-magnetic impurities that decreases as the distance from the first sensing spacer layer 233 increases. The increasing content of non-magnetic impurities dilutes the ferromagnetic material of the second sensing sublayer 232 toward the first sensing spacer layer 233.

[0038] 8 shows another view of the second sensing sublayer 232 in detail, where the second sensing sublayer 232 comprises a plurality of ferromagnetic sensing bilayers 232bl, each of which comprises a low spontaneous sensing layer 237 and a high spontaneous sensing layer 238. The high spontaneous sensing layer 238 has a higher sense spontaneous magnetization 230 than the sense spontaneous magnetization of the low spontaneous sensing layer 237. The thickness of the low spontaneous sensing layer 237 relative to the thickness of the high spontaneous sensing layer 238 decreases as the distance from the first sensing spacer layer 233 increases.

[0039] To achieve a ratio of the magnetic moment of the first sensing sublayer 231 to the magnetic moment of the second sensing sublayer 232 between 0.1 and 0.25 and to reduce the net stray magnetic field 55 applied to the reference layer 21, the thickness of the second sensing sublayer 232, the gradient of the sensing spontaneous magnetization 230, or the arrangement of the sensing double layer 232bl may be adjusted alone or in combination.

[0040] 7 and 8 allows for a low stray magnetic field 55 and the illustrated configuration has a sense magnetization ratio ΔM between 0.1 and 0.25 using only a single sense spacer layer 233. When the second sense sublayer 232 comprises multiple ferromagnetic sense bilayers 232bl, the term M (in the equations given above) SFM2 corresponds to the net spontaneous magnetization of the multiple ferromagnetic sensing bilayers 232bl, and t FM2 corresponds to the thickness of the second sensing sublayer 232 comprising a plurality of ferromagnetic sensing bilayers 232bl. 9 illustrates yet another embodiment of the magnetoresistive element 10, in which the second sensing sublayer 232 includes a proximal second sensing sublayer 232a and a distal second sensing sublayer 232b. The distal second sensing sublayer 232b has a sense spontaneous magnetization 230 that is at least two times greater (higher) than the sense spontaneous magnetization 230 of the proximal second sensing sublayer 232a. The proximal second sensing sublayer 232a is ferromagnetically coupled to the distal second sensing sublayer 232b.

[0041] Here, the sense magnetization ratio ΔM does not depend on the particular arrangement of the first and second sense layers 231, 232a, 232b, but rather on the net magnetic moments of these layers. More specifically, the term M in Eq. SFM2 t FM2 is M SFM2a t FM2a +M SFM2b t FM2b where M SFM2a and t FM2a correspond to the spontaneous magnetization and thickness, respectively, of the proximal second sensing sublayer 232a, and M SFM2b and t FM2b correspond to the spontaneous magnetization and thickness, respectively, of the distal second sensing sublayer 232b.

[0042] In one aspect, the lower sensed spontaneous magnetization 230 of the proximal second sensing sublayer 232a relative to the distal second sensing sublayer 232b is obtained by including non-magnetic impurities in the ferromagnetic proximal second sensing sublayer 232a to dilute the spontaneous magnetization of the ferromagnetic material. Alternatively or in combination, the relatively low sensed spontaneous magnetization 230 of the proximal second sensing sublayer 232a is obtained by the distal second sensing sublayer 232b having a thickness greater than the thickness of the proximal second sensing sublayer 232a.

[0043] The sense spontaneous magnetization 230 of the proximal second sensing sublayer 232a can be adjusted to compensate for the stray field generated by the first sensing sublayer 231 and reduce the net stray field 55 at the reference layer 21. Because the magnitude of the stray field 55 decreases with the cube of the distance, the contribution of the stray field generated by the thicker distal second sensing sublayer 232b is negligible in the net stray field 55 at the reference layer 21. The larger sense magnetization 230 of the distal second sensing sublayer 232b allows for an increase in the TMR of the magnetoresistive element 10.

[0044] FIG. 10 illustrates a variation of the magnetoresistive element 10 shown in FIG. 9, in which the second sensing sublayer 232 includes a proximal second sensing sublayer 232a separated from a distal second sensing sublayer 232b by a non-magnetic second sensing spacer layer 235. The second sensing spacer layer 235 may contain a non-magnetic material, such as, but not limited to, Ru, W, Mo, or Ir, or a combination of these elements. In this configuration, the distal second sensing sublayer 232b is antiferromagnetically coupled to the proximal second sensing sublayer 232a.

[0045] 9, the thickness of the proximal second sensing sublayer 232a may be adjusted to compensate for the stray field generated by the first sensing sublayer 231 and reduce the net stray field 55 in the reference layer 21. The stray field contribution generated by the thicker distal second sensing sublayer 232b is negligible in the net stray field 55 in the reference layer 21. The larger sense magnetization 230 of the distal second sensing sublayer 232b allows for an increase in the TMR of the magnetoresistive element 10.

[0046] In a variation not shown, the sequence "first sensing layer 231 / first sensing spacer layer 233 / second sensing layer 232" can be repeated multiple times to form a multi-layer structure. Such a multi-layer structure can have a lower spontaneous magnetization than the spontaneous magnetization of the distal second sensing layer 232b. The multi-layer structure can be strongly coupled to the distal second sensing layer 232b.

[0047] At least one of the thicknesses of the first sensing layer 231 and the second sensing layer 232 in the magnetoresistive element 10 having the configuration of Figures 9 and 10 and the thicknesses of the proximal and distal second sensing layers 232a, 232b can be adjusted to reduce the stray magnetic field 55.

[0048] FIG. 11 shows details of the sensing layer 23 according to an embodiment, further comprising an intermediate ferromagnetic sensing layer 236 on both sides (top and bottom in FIG. 11 ) of and in contact with the first sensing spacer layer 233. The intermediate ferromagnetic sensing layer 236 may be a nanolayer having a thickness of, for example, about 1 nm. The intermediate ferromagnetic sensing layer 236 may contain any one of Co or CoFe based alloys. The intermediate ferromagnetic sensing layer 236 preferably has a high spontaneous magnetization. For example, the intermediate ferromagnetic sensing layer 236 may contain a CoFe alloy containing 25 to 50 wt % Fe.

[0049] An improved sensing layer structure having two or more antiferromagnetically coupled sublayers. By proper selection of the sensing layer material and sensing layer thickness, the hysteresis in the sensor's angular response can be significantly reduced, improving the sensitivity, signal-to-noise ratio, and sensor lifetime.

[0050] In one embodiment, a two-dimensional magnetic sensor comprises a plurality of magnetoresistance elements 10 as disclosed herein. Embodiments of the present application from different points of view are listed below. (a) a magnetoresistive element (10) for a two-dimensional magnetic sensor, the magnetoresistive element (10) comprising a tunnel barrier layer (22) included between a reference layer (21) having a reference magnetization (210) and a sense layer (23) having a sense magnetization (230); the sensing layer (23) comprises a synthetic antiferromagnetic (SAF) structure comprising a ferromagnetic first sensing sublayer (231) in contact with the tunnel barrier layer (22) and separated from a ferromagnetic second sensing sublayer (232) by a first nonmagnetic spacer layer (233), whereby the first sensing sublayer (231) is antiferromagnetically coupled to the second sensing sublayer (232); The sensing layer (23) is configured such that a sensing magnetization ratio (ΔM) is defined by the following equation:

number

[0051] 10. Magnetoresistance element 21 Reference layer, reference SAF structure 210 Reference magnetization 211 1st standard sublayer 212 2nd standard sublayer 213 Reference Spacer Layer 22 Tunnel Barrier Layer 23 Detection layer, detection SAF structure 230 Detecting Magnetism 231 First Detection Sublayer 232 Second Detection Sublayer 232a Proximal second sensing sublayer 232b Distal second sensing sublayer 232bl Sensing Double Layer 233 First sensing spacer layer 234 3rd Detection Sublayer 235 Second sensing spacer layer 236 Intermediate Strong Magnetization Sensing Layer 237 Low spontaneous detection layer 238 Highly spontaneous detection layer 24 Pinning layer, antiferromagnetic layer 55 Local magnetic stray fields, net magnetic stray fields ΔM Detected magnetization ratio H AFM SAF stray magnetic field H FM FM stray magnetic field

Claims

1. 1. A magnetoresistive element for a two-dimensional magnetic sensor, the magnetoresistive element comprising a tunnel barrier layer included between a reference layer having a reference magnetization and a sense layer having a sense magnetization, the sense layer comprises a synthetic antiferromagnetic (SAF) structure comprising a ferromagnetic first sense sublayer in contact with the tunnel barrier layer and separated from a ferromagnetic second sense sublayer by a first nonmagnetic sense spacer layer, whereby the first sense sublayer is antiferromagnetically coupled to the second sense sublayer; The sensing layer is configured such that a sense magnetization ratio ΔM is defined by the following equation: [0010] In the above formula, M SFM1 and M. SFM2 are the spontaneous magnetizations of the first and second sensing sublayers, respectively, and t FM1 and t FM2 are the thicknesses of the first and second sensing sublayers, respectively, in the magnetoresistive element; The detected magnetization ratio ΔM is between 0.1 and 0.25, A magnetoresistive element, wherein the second sense sublayer has a spontaneous magnetization that increases with increasing distance from the first nonmagnetic sense spacer layer.

2. The magnetoresistive element of claim 1 , wherein the first sensing sublayer has a thickness between 1 nm and 3 nm and the second sensing sublayer has a thickness between 2 nm and 6 nm.

3. The magnetoresistive element of claim 2 , wherein the second sensing sublayer has a thickness greater than the first sensing sublayer.

4. The magnetoresistive element of claim 3 , wherein the first sensing sublayer comprises a non-magnetic element that reduces the spontaneous magnetization of the first sensing sublayer.

5. The magnetoresistive element of claim 1 , wherein the first non-magnetic sensing spacer layer comprises Ru, W, Mo, or Ir, or a combination of the foregoing elements.

6. The magnetoresistive element of claim 1 , wherein said second sensing sublayer comprises a ferromagnetic material containing non-magnetic impurities in a concentration that decreases with increasing distance from said first non-magnetic sensing spacer layer.

7. the second sensing sublayer comprises a plurality of ferromagnetic sensing bilayers, each sensing bilayer comprising a low spontaneous sensing layer and a high spontaneous sensing layer having a spontaneous magnetization higher than the spontaneous magnetization of the low spontaneous sensing layer; a thickness of the low spontaneous sensing layer relative to a thickness of the high spontaneous sensing layer decreases with increasing distance from the first nonmagnetic sensing spacer layer; The magnetoresistive element according to claim 1 .

8. the second sensing sublayer comprises a proximal second sensing sublayer proximal to the first non-magnetic sensing spacer layer and a distal second sensing sublayer distal to the first non-magnetic sensing spacer layer and ferromagnetically coupled to the proximal second sensing sublayer; The magnetoresistive element of claim 1 , wherein the distal second sensing sublayer has a spontaneous magnetization at least twice as large as the proximal second sensing sublayer.

9. The magnetoresistive element of claim 8 , wherein the proximal second sensing sublayer comprises a ferromagnetic material that contains non-magnetic impurities that reduce the spontaneous magnetization of the ferromagnetic material.

10. The second sensing sublayer comprises: a proximal second sensing sublayer proximal to the first non-magnetic sensing spacer layer; a distal second sensing sublayer distal to the first non-magnetic sensing spacer layer; the proximal second sensing sublayer is separated from the distal second sensing sublayer by a second non-magnetic sensing spacer layer; The magnetoresistive element of claim 1 , wherein the proximal second sensing sublayer is antiferromagnetically coupled to the distal second sensing sublayer.

11. The magnetoresistive element of claim 10 , wherein the spontaneous magnetization of the distal second sensing sublayer is higher than the spontaneous magnetization of the first sensing sublayer and the proximal second sensing sublayer.

12. The magnetoresistive element of claim 10, comprising a plurality of sensing SAF structures, the SAF structure comprising the first sensing sublayer, another SAF structure comprising the second sensing sublayer, and yet another SAF structure comprising the first non-magnetic sensing spacer layer.

13. The magnetoresistive element of claim 1 , wherein the sense layer further comprises intermediate ferromagnetic sense layers on either side of and in contact with the first nonmagnetic sense spacer layer.

14. A two-dimensional magnetic sensor comprising a plurality of the magnetoresistance elements according to claim 1.

Citation Information

Patent Citations

  • Magnetoresistive device and method of manufacturing the same

    JP2004172599A

  • Magnetic storage element

    JP2006332527A

  • Magnetic reluctance device and magnetic memory using it

    JP2006352062A

  • Magnetoresistive element

    JP2007096092A

  • Magnetoresistance effect element and magnetic random access memory using it

    JP2008109118A