Welded assembly steel
By shifting and non-overlapping the weld beads in welded steel materials, the fatigue life is enhanced, addressing stress concentration issues and improving the structural integrity of welded steel assemblies.
Patent Information
- Application Number
- JP2020098501
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-06-05
- Publication Date
- 2024-09-25
- Estimated Expiration
- 2040-06-05
AI Technical Summary
Welded steel materials, particularly those assembled in a cross section with intermittent fillet welding, experience reduced fatigue life due to stress concentration and tensile residual stress at the weld bead edges, leading to early crack initiation and overlapping crack initiation positions, which further reduces fatigue life.
The solution involves forming intermittent fillet welds at the corners of steel materials such that the longitudinal ends of the weld beads do not overlap when projected, and shifting the weld beads relative to each other in the length direction, using steel plates made of Fe-Mn-(Cr, Ni)-Si alloys or similar materials with enhanced fatigue resistance.
This approach improves the fatigue life of welded assemblies by preventing overlapping crack initiation sites, enhancing welding strength, and reducing stress concentration, thereby extending the material's lifespan without requiring costly post-treatments or expensive welding materials.
Smart Images

Figure 0007555733000001 
Figure 0007555733000002 
Figure 0007555733000003
Abstract
Description
[Technical field]
[0001] The present invention relates to welded fabricated steel products. [Background technology]
[0002] Patent Document 1 discloses a technique for a fillet welding method for vibration-damping steel plates. In this prior art, the end face of a normal steel plate is brought into contact with the surface of a vibration-damping steel plate having a structure in which a viscoelastic resin is sandwiched between two steel plates, and the corners of the vibration-damping steel plate and the normal steel plate are staggered fillet welded by arc welding.
[0003] Patent Document 2 discloses a technique relating to a welding method for a cruciform fillet welded joint. In this prior art, the final pass of welding is performed on the main material side to which the main stress is applied as a product.
[0004] Patent Document 3 discloses a technique relating to a welding method for welding low alloy steel materials for structures using a welding material. In this prior art, the weld metal produced by welding is caused to undergo martensitic transformation during the cooling process after welding, and is in a state of being expanded at room temperature compared to when the martensitic transformation started.
[0005] Patent Document 4 discloses a technique relating to a method for improving the fatigue strength of welded parts of metallic materials. In this prior art, a fiber-reinforced plastic layer is fixed to the entire surface of a metal fillet weld or to a portion of the surface near the weld toe and to a portion of the main plate of the metal, in which the elastic modulus of the fiber-reinforced plastic in the longitudinal direction of the joint and along the surface is 5% to 150% of that of the main plate, and (elastic modulus) x (thickness) is 1% to 50% of that of the main plate.
[0006] Patent Document 5 discloses a technology related to a fatigue reducing welded joint structure that improves the fatigue strength of fillet joints. In this prior art, a putty layer that covers the entire surface of the weld metal of the fillet weld and is fixed to the main plate and rib plate is laminated to form a concave cylindrical surface toward the weld, so that the putty layer shares and bears the stress applied to the fillet weld and relieves the stress concentration at the weld toe, thereby improving the fatigue strength of the joint structure. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Japanese Patent Application Publication No. 2-46979 [Patent Document 2] Japanese Patent Application Publication No. 10-85934 [Patent Document 3] Patent No. 3350726 [Patent Document 4] Japanese Patent Application Publication No. 8-243778 [Patent Document 5] JP 2007-75826 A Summary of the Invention [Problem to be solved by the invention]
[0008] In braces and other welded steel products, steel plates are assembled and welded into a cross section, and the steel plates are arranged in a cross shape and fillet welded at the four corners. The fillet welds may be applied along the entire length, or may be applied intermittently to reduce the amount of welding material and to suppress distortion of the components due to welding heat.
[0009] In general, stress concentration and tensile residual stress in welds reduce fatigue life. This is particularly noticeable at the ends of weld beads in intermittent fillet welds, and initial cracks in fatigue fracture often start at the ends of the weld beads.
[0010] In an intermittent fillet weld, multiple weld beads are generally arranged in the same position, so that the initial crack initiation positions of fatigue fracture in the weld beads overlap on the same cross section, resulting in a shortened fatigue life.
[0011] In view of the above, an object of the present invention is to improve the fatigue life of welded steel materials assembled by intermittent fillet welding. [Means for solving the problem]
[0012] The first aspect is a welded and assembled steel material in which an intermittent fillet weld is formed at each of the corners on both sides of one steel material formed from one steel material and another steel material, and the longitudinal end of one weld bead and the longitudinal end of the other weld bead have a portion that does not overlap when projected.
[0013] In the first embodiment of the welded assembled steel material, the longitudinal end of one weld bead and the longitudinal end of the other weld bead have portions that do not overlap when projected, thereby improving the fatigue life of the welded assembled steel material compared to when all ends overlap when projected.
[0014] A second aspect is a welded assembly steel material according to the first aspect, in which one of the weld beads and the other of the weld beads are offset from each other in the longitudinal direction and an end of one of the weld beads overlaps when projected at an intermediate portion between the ends of the other weld bead.
[0015] In the second embodiment of the welded steel product, one weld bead and the other weld bead are offset from each other in the longitudinal direction. Therefore, the longitudinal end of one weld bead and the longitudinal end of the other weld bead do not overlap when projected, improving the fatigue life of the welded steel product. Also, the end of one weld bead overlaps when projected at a middle portion between the ends of the other weld bead, improving the weld strength compared to when the end of one weld bead and the middle portion of the other weld bead do not overlap.
[0016] A third aspect is the welded and assembled steel material according to the first or second aspect, in which the steel material is a steel plate made of an Fe-Mn-(Cr,Ni)-Si based alloy containing at least either Cr or Ni, or an alloy further containing Al, and an end of one of the steel plates is abutted against both sides of the other steel plate to form a cross section.
[0017] In the third embodiment of the welded assembled steel material, the steel material is made of an Fe-Mn-(Cr, Ni)-Si based alloy containing either Cr or Ni, or an alloy which further contains Al and has excellent fatigue resistance properties, so that the effect of improving fatigue life is higher than when, for example, SN material, LY material or other steel material is used as the base material. Effect of the Invention
[0018] According to the present invention, the fatigue life of a welded assembly assembled with intermittent fillet welds can be improved. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1A shows a vibration-damping brace of an embodiment, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 1A-1A in FIG. 1B. FIG. 1B shows the vibration-damping brace as viewed from a direction perpendicular to the longitudinal direction. [Diagram 2] (A) shows a brace core material of an embodiment, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 2A-2A in (B), while (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Diagram 3] (A) shows the brace core material of the first modified example, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 3A-3A in (B), while (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 4] (A) shows the brace core material of the second modified example, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 4A-4A in (B), while (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Diagram 5](A) shows the brace core material of the third modified example, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 5A-5A in (B), while (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 6] (A) showing the brace core material of the fourth modified example is a cross-sectional view of a section perpendicular to the longitudinal direction along line 6A-6A in (B), and (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 7] (A) showing the brace core material of the fifth modified example is a cross-sectional view of a section perpendicular to the longitudinal direction along line 7A-7A in (B), and (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 8] (A) showing the brace core material of the sixth modified example is a cross-sectional view of a section perpendicular to the longitudinal direction along line 8A-8A in (B), and (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 9] (A) shows a brace core material of a reference example, and is a cross-sectional view of a section perpendicular to the longitudinal direction along line 9A-9A in (B), and (B) is a view of the brace core material from a direction perpendicular to the longitudinal direction. [Figure 10] 9, and (B) is a cross-sectional view showing an initial crack in a cross section perpendicular to the longitudinal direction passing through the end of the weld bead of the brace core material of the embodiment of FIG. 2. [Figure 11] 10 is an explanatory diagram for explaining a distance between a tip of an end of one weld bead and a tip of an end of another weld bead; FIG. [Figure 12] 10 is an explanatory diagram for explaining a distance between a tip of an end of one weld bead and a tip of an end of another weld bead; FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] <Embodiment> A welded and fabricated steel material according to one embodiment of the present invention will now be described.
[0021] [structure] First, the structure of the welded and assembled steel material will be described. Although each of the (A) figures is a cross-sectional view, the hatching indicating the cross section has been omitted in order to make the figure easier to see.
[0022] (Vibration-damping brace) The overall structure of the vibration-damping brace using welded steel materials will be described.
[0023] As shown in FIG. 1, the vibration-damping brace 10 is configured to include a brace core material 30 and a stiffening portion 20.
[0024] The brace core material 30, which is an example of a welded assembled steel material, is a cross-sectional member assembled and welded by butting an end 53 of a steel plate 52 and an end 55 of a steel plate 54 (see FIG. 1(A)) against one surface 50A and the other surface 50B (see FIG. 1(A)) of a steel plate 50, respectively, and applying fillet welding to four corners 70A, 70B, 70C, 70D (FIG. 1(A)). Note that the steel plates 50, 52, 54 in this embodiment are made of flat steel, which is a flat, band-shaped steel material.
[0025] As shown in FIG. 1(B), the axial end of the brace core material 30 is a bolt joint portion 40 in which a bolt hole 42 is formed for bolting to a gusset plate or the like. A recess 43 is formed in the central portion of the brace core material 30 in the axial direction. Both end portions of the brace core material 30 in the axial direction are widened portions 44, and the central portion in which the recess 43 is formed is a shape-deformed portion 46. The shape-deformed portion 46 in the central portion of this brace core material 30 is a plastically deformed portion, and the widened portions 44 at both end portions are elastically deformed portions.
[0026] As shown in FIG. 1, the stiffening portion 20 is provided on the outside of the brace core material 30 excluding the bolt joint portion 40, and has a function of preventing or suppressing buckling of the brace core material 30. In this embodiment, the stiffening portion 20 is composed of mortar and steel pipes provided around the brace core material 30, but is not limited to such a configuration. For example, the stiffening portion 20 may be composed of steel pipes only. Alternatively, the stiffening portion 20 may be composed of angle iron bolted to the brace core material 30, or may be composed of steel pipes and steel plates. In short, the stiffening portion 20 may have a configuration that has a function of preventing or suppressing buckling of the brace core material 30.
[0027] (Brace core material) As described above, the brace core material 30 shown in Figures 1 and 2 is a cross-sectional member assembled and welded by abutting ends 53, 55 (see Figures 1(A) and 2(A)) of steel plates 52 and 54 (see Figures 1(A) and 2(A)) against one surface 50A and the other surface 50B (see Figures 1(A) and 2(A)) of steel plate 50, respectively, and applying fillet welding to the four corners 70A, 70B, 70C, 70D (Figures 1(A) and 2(A)).
[0028] The steel plates 50, 52, and 54 of the present embodiment are made of an Fe-Mn-Si alloy having excellent fatigue resistance. More specifically, the steel plates 50, 52, and 54 are made of an Fe-Mn-(Cr, Ni)-Si alloy containing at least one of Cr and Ni, or an alloy further containing Al, as disclosed in JP 2014-129567 A (Patent No. 6182725).
[0029] Intermittent fillet welds are applied to the four corners 70A, 70B, 70C, and 70D (see Figs. 1(A) and 2(A)) except for both axial ends.
[0030] The weld beads 80A, 80B, 80C, and 80D of the intermittent fillet welds at the four corners 70A, 70B, 70C, and 70D (see FIGS. 1(A) and 2(A)) shown in FIGS. 1(B) and 2(B) are spaced apart in the axial direction.
[0031] Here, the four corners 70A, 70B, 70C, and 70D (see Figs. 1(A) and 2(A)) are referred to as a first corner 70A, a second corner 70B, a third corner 70C, and a fourth corner 70D. The weld bead at the first corner 70A is referred to as a first weld bead 80A, the weld bead at the second corner 70B is referred to as a second weld bead 80B, the weld bead at the third corner 70C is referred to as a third weld bead 80C, and the weld bead at the fourth corner 70D is referred to as a fourth weld bead 80D. When no distinction is required, they are referred to as corners 70 and weld beads 80. The left side of (B) in each figure in the longitudinal direction of weld bead 80 is referred to as one side, and the right side is referred to as the other side.
[0032] 2B, the four weld beads, ie, first weld bead 80A, second weld bead 80B, third weld bead 80C, and fourth weld bead 80D, are offset from one another in the length direction. The length direction of the weld beads 80 coincides with the axial direction of the brace core material 30.
[0033] When one end 82B in the longitudinal direction of the second weld bead 80B is projected onto an intermediate portion 83A between one end 82A and the other end 84A of the first weld bead 80A, they overlap, and when the other end 84A of the first weld bead 80A is projected onto an intermediate portion 83B between one end 82B and the other end 84B of the second weld bead 80B, they overlap.
[0034] Similarly, when one end 82C of the third weld bead 80C is projected onto the intermediate portion 83B of the second weld bead 80B, they overlap, and when the other end 84B of the second weld bead 80B is projected onto the intermediate portion 83C between one end 82C and the other end 84C of the third weld bead 80C, they overlap.
[0035] When one end 82D of the fourth weld bead 80D is projected onto the intermediate portion 83C of the third weld bead 80C, they overlap, and when the other end 84C of the third weld bead 80C is projected onto the intermediate portion 83D between one end 82D and the other end 84D of the fourth weld bead 80D, they overlap.
[0036] When one end 82A of first weld bead 80A projects onto middle portion 83D of fourth weld bead 80D, they overlap, and when the other end 84D of fourth weld bead 80D projects onto middle portion 83A of first weld bead 80A, they overlap.
[0037] In this manner, the four weld beads 80 are offset from one another in the longitudinal direction, and when projected, there are no portions where the ends 82, 84 overlap with each other.
[0038] Here, ends 82, 84 of weld bead 80 will be described.
[0039] As shown in Fig. 10, ends 82, 84 of a weld bead 80 are locations where stress concentration and tensile residual stress of the steel plates 50, 52, 54 occur significantly, and are locations where an initial crack S due to fatigue fracture occurs. Note that Fig. 10 will be described later. Also, although only the end 82 is shown in Fig. 10, the same applies to the end 84.
[0040] In addition, "overlapping when projected" and "not overlapping when projected" mean that the weld beads 80 on both sides of the steel plates 50, 52, 54 overlap or do not overlap when viewed from a direction perpendicular to the longitudinal direction (out-of-plane direction).
[0041] [Action and Effects] Next, the operation and effects of this embodiment will be described.
[0042] First, a brace core material 900 of a reference example will be described.
[0043] In the brace core material 900 of the reference example shown in Fig. 9, as shown in Fig. 9(B), the four first weld beads 80A, second weld bead 80B, third weld bead 80C, and fourth weld bead 80D are at the same position in the length direction, and overlap when the ends 82, 84 are projected. Note that in Fig. 9(B), the dashed lines of the third weld bead 80C and the fourth weld bead 80D are slightly shifted for ease of understanding, but in reality, the four first weld beads 80A, second weld bead 80B, third weld bead 80C, and fourth weld bead 80D are at the same position in the length direction.
[0044] As described above, the ends 82, 84 of the weld bead 80 are locations where stress concentration and tensile residual stress of the steel plates 50, 52, 54 occur significantly, and are locations where the initial crack S due to fatigue fracture shown in FIG. 10(A) occurs.
[0045] In the reference example, as described above, the ends 82, 84 of the four weld beads 80 overlap when projected. In other words, as shown in Fig. 10(A), the positions at which the initial cracks S occur overlap on the same cross section, making it easier for breakage to occur due to the progression of the initial cracks S and shortening the fatigue life. As described above, although only the end 82 is shown in Fig. 10(A), the same is true for the end 84.
[0046] In contrast, in the brace core material 30 of this embodiment shown in Fig. 2, the four weld beads 80 are offset from each other in the length direction, and when projected, there are no areas where the ends 82, 84 overlap with the ends 82, 84. Therefore, as shown in Fig. 10(B), the occurrence positions of the initial cracks S do not overlap on the same cross section, improving the fatigue life.
[0047] In addition, one end 82 and the other end 84 of one weld bead 80, which are arranged at intervals in the longitudinal direction, overlap at an intermediate portion 83 between one end 82 and the other end 84 of the other weld bead 80 when projected, thereby improving the weld strength.
[0048] In addition, the steel plates 50, 52, 54 constituting the brace core material 30 of this embodiment use an Fe-Mn-Si alloy having an excellent fatigue life as the base material. Therefore, by using the brace core material 30 as the vibration-damping brace 10, it is possible to achieve an excellent fatigue life.
[0049] Here, since the steel plates 50, 52, 54 that make up the brace core material 30 are made of an alloy having a long fatigue life as the base material, stress concentration and breakage due to tensile residual stress are unlikely to occur at the boundary between the widened portions 44 at both axial ends of the brace core material 30 and the deformed portion 46 in the central part where the recess 43 is formed.
[0050] Therefore, the fatigue life of the brace core material 30 is often determined not by fracture due to stress concentration and tensile residual stress at the boundary between the widened portion 44 and the shape-deformed portion 46, but by fracture due to the progression of an initial crack S that occurs at the ends 82, 84 of the weld bead 80.
[0051] Therefore, as in this embodiment, the steel plates 50, 52, 54 that make up the brace core material 30 are made of an alloy having a long fatigue life as a base material, and the weld beads 80 are shifted from each other in the longitudinal direction so that there are no overlapping portions between the ends 82, 84, making it possible to create a vibration-damping brace 10 that exhibits high vibration-damping performance and has a long fatigue life.
[0052] The ends 82, 84 of the weld bead 80 are locations where stress concentration and tensile residual stress of the steel plates 50, 52, 54 occur significantly, and where an initial crack S (see FIG. 10) due to fatigue fracture occurs.
[0053] Therefore, if ends 82, 84 of one weld bead 80 and ends 82, 84 of the other weld bead 80 are close to each other even if they do not overlap, the initial cracks S (see Figure 10) may connect, and there is a risk that the fatigue life will not be sufficiently improved.
[0054] Therefore, as shown in Figures 11 and 12, it is desirable to secure a sufficient distance L between tip 81 of end 82 of one weld bead 80 and tip 85 of end 84 of the other weld bead 80. Also, it is desirable that this distance L is at least twice the plate thickness of the steel plates constituting brace core material 30 (if the plate thicknesses of steel plates 50, 52, 54 are different, at least twice the smallest plate thickness). Note that Figure 12 shows the case of a structure represented by a first modified example shown in Figure 3 described later.
[0055] Here, methods for reducing stress concentration and tensile residual stress in a weld bead and improving fatigue life include a method of smoothing the weld bead by a mechanical method such as a grinder or by remelting using TIG welding, a method of removing tensile residual stress by a mechanical method such as peening or by post-weld heat treatment, a method of using a low transformation temperature welding material (e.g., Japanese Patent No. 3350726), a method of applying fiber-reinforced plastic or resin-based putty to the weld bead (e.g., Japanese Patent Publication Nos. H8-243778 and 2007-75826), etc. These methods may also be effective for stress concentration at the end of the weld bead in the longitudinal direction. However, these methods require post-processing after welding and the use of welding materials containing expensive elements, which increases production costs.
[0056] In contrast, in this embodiment, as described above, the fatigue life is improved by shifting the four weld beads 80 from one another in the longitudinal direction so that the ends 82, 84 do not overlap, that is, by preventing the occurrence positions of the initial cracks S from overlapping on the same cross section. Therefore, compared to post-treatment after welding or using welding materials containing expensive elements, the fatigue life can be improved at low cost.
[0057] [Variations] Next, a modified example of the brace core material of this embodiment will be described. Note that the description of only the structural parts different from the above embodiment will be omitted or simplified.
[0058] (First Modification) In the brace core material 31 of the first modified example shown in Figure 3, as shown in Figure 3 (B), the four first weld beads 80A, second weld beads 80B, third weld beads 80C and fourth weld beads 80D are each offset from each other in the longitudinal direction.
[0059] 3(B), one end 82B of second weld bead 80B is disposed on the other outer side in the longitudinal direction of the other end 84A of first weld bead 80A. Similarly, one end 82C of third weld bead 80C is disposed on the other outer side in the longitudinal direction of the other end 84B of second weld bead 80B, and one end 82D of fourth weld bead 80D is disposed on the other outer side in the longitudinal direction of the other end 84C of third weld bead 80C. One end 82A of first weld bead 80A is disposed on the other outer side in the longitudinal direction of the other end 84D of fourth weld bead 80D.
[0060] In this embodiment, ends 82, 84 of one weld bead 80 do not overlap with intermediate portion 83 between end 82 and end 84 of the other weld bead 80 when projected.
[0061] In this way, the four weld beads 80 are offset from one another in the longitudinal direction, and when projected, there are no overlapping portions between the ends 82, 84. Therefore, the occurrence positions of initial cracks S (see FIG. 10) do not overlap on the same cross section, improving the fatigue life.
[0062] (Second Modification) In the brace core material 32 of the second modified example shown in Fig. 4, as shown in Fig. 4(B), the first weld bead 80A and the third weld bead 80C are at the same position in the length direction, and the second weld bead 80B and the fourth weld bead 80D are at the same position in the length direction. The first weld bead 80A and the third weld bead 80C, and the second weld bead 80B and the fourth weld bead 80D are shifted from each other in the length direction.
[0063] As shown in FIG. 4(B), when projected onto intermediate portions 83A, 83C between one end 82A, 82C and the other end 84A, 84C of first weld bead 80A and third weld bead 80C, one end 82B, 82D of second weld bead 80B and fourth weld bead 80D overlap.
[0064] In addition, when projected onto intermediate portions 83B, 83D between one end 82B, 82D and the other end 84B, 84D of second weld bead 80B and fourth weld bead 80D, the other end 84A, 84C of first weld bead 80A and third weld bead 80C overlap.
[0065] In this way, ends 82A, 84A of first weld bead 80A and ends 82B, 84B of second weld bead 80B overlap when projected, and ends 82B, 84B of second weld bead 80B and ends 82D, 84D of fourth weld bead 80D overlap when projected.
[0066] However, ends 82A, 82C, 84A, and 84C of first weld bead 80A and third weld bead 80C do not overlap with ends 82B, 82D, 84B, and 84D of second weld bead 80B and fourth weld bead 80D when projected. Therefore, compared to the brace core material 900 of the reference example (see Figs. 9 and 10(A)), the number of overlapping areas on the same cross section where initial cracks S (see Fig. 10) occur is reduced, improving the fatigue life.
[0067] (Third Modification) In brace core material 33 of the third modified example shown in Fig. 5, as shown in Fig. 5(B), first weld bead 80A and second weld bead 80B are at the same position in the length direction, and third weld bead 80C and fourth weld bead 80D are at the same position in the length direction. Furthermore, first weld bead 80A and second weld bead 80B, and third weld bead 80C and fourth weld bead 80D are shifted from each other in the length direction.
[0068] As shown in FIG. 5(B), when projected onto intermediate portions 83A, 83B between one end 82A, 82B and the other end 84A, 84B of first weld bead 80A and second weld bead 80B, one end 82C, 82D of third weld bead 80C and fourth weld bead 80D overlap.
[0069] In addition, when projected onto intermediate portions 83C, 83D between one end 82C, 82D and the other end 84C, 84D of the third weld bead 80C and the fourth weld bead 80D, the other end 84A, 84B of the first weld bead 80A and the second weld bead 80B overlap.
[0070] In this way, ends 82A, 84A of first weld bead 80A and ends 82B, 84B of second weld bead 80B overlap when projected, and ends 82C, 84C of third weld bead 80C and ends 82D, 84D of fourth weld bead 80D overlap when projected.
[0071] However, ends 82A, 82B, 84A, and 84B of first weld bead 80A and second weld bead 80B do not overlap ends 82C, 82D, 84C, and 84D of third weld bead 80C and fourth weld bead 80D when projected. Therefore, compared to the brace core material 900 of the reference example (see Figs. 9 and 10(A)), the number of overlapping areas on the same cross section where initial cracks S (see Fig. 10) occur is reduced, improving the fatigue life.
[0072] (Fourth Modification) In the brace core material 34 of the fourth modified example shown in Fig. 6, as shown in Fig. 6(B), the first weld bead 80A and the second weld bead 80B are at the same position in the length direction, and the third weld bead 80C and the fourth weld bead 80D are at the same position in the length direction. Furthermore, the first weld bead 80A and the second weld bead 80B, and the third weld bead 80C and the fourth weld bead 80D are shifted from each other in the length direction.
[0073] As shown in FIG. 6(B), when projected, one ends 82C, 82D and the other ends 84C, 84D of the third weld bead 80C and the fourth weld bead 80D overlap with intermediate portions 83A, 83B between one ends 82A, 82B and the other ends 84A, 84B of the first weld bead 80A and the second weld bead 80B.
[0074] In addition, when projected, one end 82A, 82B and the other end 84A, 84B of the first weld bead 80A and the second weld bead 80B overlap with the intermediate portions 83C, 83D between one end 82C, 82D and the other end 84C, 84D of the third weld bead 80C and the fourth weld bead 80D.
[0075] In this way, ends 82A, 84A of first weld bead 80A and ends 82B, 84B of second weld bead 80B overlap when projected, and ends 82C, 84C of third weld bead 80C and ends 82D, 84D of fourth weld bead 80D overlap when projected.
[0076] However, ends 82A, 82B, 84A, and 84B of first weld bead 80A and second weld bead 80B do not overlap ends 82C, 82D, 84C, and 84D of third weld bead 80C and fourth weld bead 80D when projected. Therefore, compared to the brace core material 900 of the reference example (see Figs. 9 and 10(A)), the number of overlapping areas on the same cross section where initial cracks S (see Fig. 10) occur is reduced, improving the fatigue life.
[0077] Furthermore, compared to the third modified example, the weld beads 80 are dense and continuous, so the weld strength is high.
[0078] (Fifth Modification) 7, in the brace core material 35 of the fifth modified example, the first weld bead 80A and the second weld bead 80B are at the same position in the length direction, and the third weld bead 80C and the fourth weld bead 80D are at the same position in the length direction. The first weld bead 80A and the second weld bead 80B, and the third weld bead 80C and the fourth weld bead 80D are offset from each other in the length direction.
[0079] The second weld bead 80B has a shorter bead length than the first weld bead 80A, and one end 82A of the first weld bead 80A is positioned on one longitudinal outside of one end 82B of the second weld bead 80B, and the other end 84A of the first weld bead 80A is positioned on the other longitudinal outside of the other end 84B of the second weld bead 80B.
[0080] Similarly, the third weld bead 80C has a shorter bead length than the fourth weld bead 80D, and one end 82D of the fourth weld bead 80D is positioned on one longitudinal outside of one end 82C of the third weld bead 80C, and the other end 84D of the fourth weld bead 80D is positioned on the other longitudinal outside of the other end 84C of the third weld bead 80C.
[0081] In this way, first weld bead 80A and second weld bead 80B are at the same position in the length direction, and third weld bead 80C and fourth weld bead 80D are at the same position in the length direction, but because the bead lengths are different, when projected there is no overlap between ends 82, 84. Therefore, the occurrence positions of initial cracks S (see FIG. 10) do not overlap on the same cross section, improving the fatigue life.
[0082] (Sixth Modification) The brace core material 36 of the sixth modified example shown in Figure 8 is a T-shaped cross-sectional component assembled and welded by abutting an end 53 (see Figure 8(A)) of a steel plate 52 against one surface 50A of a steel plate 50 and applying intermittent fillet welding to two corners 70A, 70B.
[0083] The two first weld beads 80A and the second weld bead 80B are offset from each other in the length direction. When one end 82B of the second weld bead 80B projects onto an intermediate portion 83A between one end 82A and the other end 84A of the first weld bead 80A, they overlap, and when the other end 84A of the first weld bead 80A projects onto an intermediate portion 83B between one end 82B and the other end 84B of the second weld bead 80B, they overlap.
[0084] In this way, the two first weld beads 80A and the second weld beads 80B are offset from each other in the length direction, and when projected, there is no portion where the ends 82A, 84A overlap with the ends 82B, 84B. Therefore, the occurrence positions of the initial cracks S (see FIG. 10) do not overlap on the same cross section, improving the fatigue life.
[0085] <Other> The present invention is not limited to the above embodiment.
[0086] For example, in the above embodiment and modified example, the brace core material has a cross-shaped or T-shaped cross section, but is not limited thereto. For example, the brace core material may have an H-shaped cross section.
[0087] Furthermore, the present invention may be applied to steel materials other than steel plates. For example, the present invention may be applied to a welded and assembled steel material in which an end of a steel plate is butted against the outer surface (plate surface) of a steel pipe and welded.
[0088] In addition, for example, in the above embodiment and modified example, the welded assembled steel material is the brace core material that constitutes the vibration-damping brace, but is not limited to this. For example, the welded assembled steel material may be a brace that does not have a vibration-damping function, or may be a knee brace.
[0089] Also, for example, in the above embodiment and modified example, the welded assembly steel material and the brace core material as an example are made of an Fe-Mn-(Cr, Ni)-Si alloy containing at least one of Cr and Ni, or an alloy further containing Al, as disclosed in JP 2014-129567 A (Patent No. 6182725), but are not limited thereto. The welded assembly steel material may be made of an Fe-Mn-Si alloy other than the alloy disclosed in JP 2014-129567 A (Patent No. 6182725). Furthermore, the welded assembly steel material may be made of a steel material having better fatigue resistance than SN material, LY material, etc., other than the Fe-Mn-Si alloy, or may be made of a general steel material such as SN material or LY material.
[0090] In addition, a steel material with excellent fatigue resistance is, for example, a steel material that can withstand 2,000 or more repeated tensile and compressive deformation cycles at a strain amplitude of ±1% before fracture. Specifically, steel materials with excellent fatigue resistance are found not only in Fe-Mn-Si alloys and Fe-Mn-Si-Al alloys, but also in iron-based shape memory alloys and iron-based superelastic alloys.
[0091] Furthermore, it is sufficient that the welded and assembled steel material has one or more portions where the longitudinal ends of the weld beads do not overlap.
[0092] Furthermore, the present invention can be embodied in various forms without departing from the spirit and scope of the present invention. A plurality of embodiments and modifications can be implemented in appropriate combination. [Explanation of symbols]
[0093] 30 Brace core material 31 Brace core material 32 Brace core material 33 Brace core material 34 Brace core material 35 Brace core material 36 Brace core material 50 Steel plate (example of steel material) 52 Steel plate (example of steel material) 54 Steel plate (example of steel material) 70A First corner 70B Second corner 70C Third corner 70D Fourth corner 80A First Weld Bead 80B Second Weld Bead 80C 3rd weld bead 80D 4th weld bead 82A end 82B End 82C end 82D End 83A Middle section 83B Middle part 83C middle part 83D middle part 84A End 84B End 84C end 84D End
Claims
1. It is a welded assembly steel material in which three steel plates are assembled into a cross section and fillet welds are applied to the four corners. An intermittent fillet weld is formed at each of the four corners, The ends of the weld beads of the intermittent fillet welds formed at the four corners in the length direction do not overlap each other when projected. Welded assembled steel.
2. When projected, an end of one of the weld beads overlaps an intermediate portion between ends of another of the weld beads adjacent thereto in the longitudinal direction. The welded fabricated steel material of claim 1.
3. When projected, one of the weld beads on both sides of the steel plate is overlapped between the ends of the other weld bead, the other weld bead being shorter than the one weld bead. The welded fabricated steel material of claim 1.
4. The steel plate is made of an Fe-Mn-(Cr, Ni)-Si alloy containing at least one of Cr and Ni, or an alloy further containing Al. The welded and assembled steel material according to any one of claims 1 to 3.
5. A brace core material or a knee brace. The welded and assembled steel material according to any one of claims 1 to 4.
6. A welded assembly steel material in which three steel plates are assembled into a cross section and fillet welds are applied to the four corners, An intermittent fillet weld is formed at each of the four corners, When projected, the ends of the weld beads in the length direction do not overlap, and one of the weld beads on both sides of the steel plate is overlapped between the ends of the other weld bead, the other weld bead being shorter than the one weld bead. Welded assembled steel.
Citation Information
Patent Citations
Fillet welding method for vibration-damping steel plate
JP1990046979A
Working method for upper structure of ship
JP1994016175A
Weld zone fatigue strength improvement method
JP1996243778A
Welding method and welded structure
JP1998085934A
Welding equipment
JP2006255758A