Waveguide element

The waveguide element with a thin inorganic substrate and low dielectric constant cavity structure addresses propagation loss issues, ensuring low loss performance and miniaturization in high-frequency ranges by minimizing electric field leakage and resonance.

JP7556155B2Active Publication Date: 2024-09-25NGK CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023541423
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-08-12
Filing Date
2022-08-04
Publication Date
2024-09-25
Estimated Expiration
2042-08-04

AI Technical Summary

Technical Problem

Existing waveguide elements face challenges in achieving low propagation loss performance in the frequency range of millimeter waves to terahertz waves, particularly when mounted on a support substrate, due to issues like slab mode induction and substrate resonance.

Method used

The waveguide element incorporates a thin inorganic material substrate with a low dielectric constant portion, such as a cavity, supported by a substrate with a recess, and includes a coplanar electrode configuration to minimize electric field leakage and resonance, using materials like quartz glass for the inorganic substrate and silicon for the support substrate.

Benefits of technology

This configuration achieves excellent low propagation loss performance over a wide frequency range from 30 GHz to 20 THz, supporting miniaturization and reducing leakage and resonance effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007556155000005
    Figure 0007556155000005
  • Figure 0007556155000006
    Figure 0007556155000006
  • Figure 0007556155000007
    Figure 0007556155000007
Patent Text Reader

Abstract

Provided is a waveguide element that exhibits excellent low propagation loss performance over a wide frequency range in a region of a high frequency higher than 30 GHz even with a configuration in which an inorganic material substrate is mounted (supported) on a support substrate. A waveguide element according to an embodiment of the present invention comprises: a waveguide member that can guide electromagnetic waves having a frequency in a range of 30 GHz to 20 THz; a support substrate that supports the waveguide member; and a low dielectric part. This waveguide member is provided with an inorganic material substrate, and a coplanar-type electrode provided on the inorganic material substrate. The support substrate is provided below the inorganic material substrate. The low dielectric part has a dielectric constant lower than that of the inorganic material substrate and is provided below the inorganic material substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a waveguide element. [Background technology]

[0002] Waveguide elements are being developed as one type of element that guides millimeter waves to terahertz waves. Waveguide elements are expected to be applied and developed in a wide range of fields, such as optical waveguides, next-generation high-speed communications, sensors, laser processing, and solar power generation. As an example of such a waveguide element, a technology has been proposed that uses a grounded coplanar waveguide that is composed of a glass substrate with a thickness of 300 μm, a coplanar conductor provided on the glass substrate, and a ground electrode provided on the surface of the glass substrate opposite to the coplanar conductor (Patent Document 1). When using waveguide elements based on such technology in various industrial products, mounting the waveguide element on a supporting substrate such as an IC substrate or a printed circuit board is considered. However, when mounting the waveguide element on a supporting substrate, the range in which practical low propagation loss performance can be ensured is narrow in the frequency range from millimeter waves to terahertz waves (especially in the frequency range of 300 GHz or higher), making it difficult to achieve excellent low propagation loss performance over a wide frequency range. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Special Publication No. 2021-509767 Summary of the Invention [Problem to be solved by the invention]

[0004] The main object of the present invention is to provide a waveguide element that has a configuration in which an inorganic material substrate is mounted (supported) on a support substrate and yet can achieve excellent low propagation loss performance over a wide frequency range in the high frequency region of 30 GHz or more. [Means for solving the problem]

[0005] A waveguide element according to an embodiment of the present invention comprises a waveguide member capable of guiding electromagnetic waves with a frequency of 30 GHz or more and 20 THz or less, a support substrate supporting the waveguide member, and a low dielectric constant portion. The waveguide member comprises an inorganic material substrate and a coplanar electrode provided on an upper portion of the inorganic material substrate. The support substrate is provided on a lower portion of the inorganic material substrate. The low dielectric constant portion is provided on the lower portion of the inorganic material substrate and has a dielectric constant smaller than that of the inorganic material substrate. In one embodiment, the thickness t of the inorganic material substrate satisfies the following formula (1).

number

[0006] According to an embodiment of the present invention, a waveguide element having excellent low propagation loss performance over a wide frequency range in the high frequency region of 30 GHz or more can be realized, even though the inorganic material substrate is mounted (supported) on a support substrate. [Brief description of the drawings]

[0007] [Figure 1] 1 is a schematic perspective view of a waveguide element according to an embodiment of the present invention; [Diagram 2] 2 is a cross-sectional view of the waveguide element of FIG. 1 along line II-II'. [Diagram 3] FIG. 2 is a schematic perspective view of a waveguide element according to another embodiment of the present invention. [Figure 4] FIG. 13 is a schematic perspective view of a waveguide element according to yet another embodiment of the present invention. [Diagram 5] 5 is a cross-sectional view of the waveguide element of FIG. 4 along the line V-V′. [Figure 6] 3 is a schematic cross-sectional view illustrating a modified example of the waveguide element in FIG. 2. [Figure 7] FIG. 13 is a schematic perspective view of a waveguide element according to yet another embodiment of the present invention. [Figure 8] 8 is a cross-sectional view of the waveguide element of FIG. 7 along the line VIII-VIII'. [Figure 9] 9 is a cross-sectional view of the waveguide element of FIG. 7 taken along line IX-IX'. [Figure 10] 8 is a cross-sectional view of the waveguide element of FIG. 7 taken along the line XX'. [Figure 11] 8A to 8C are schematic cross-sectional views illustrating modified shapes of vias in the waveguide element of FIG. 7. [Figure 12] 12A to 12C are schematic cross-sectional views illustrating modified examples of the arrangement of vias in the waveguide element of FIG. [Figure 13] 8A to 8C are schematic cross-sectional views illustrating modified examples of the arrangement of vias in the waveguide element of FIG. 7. [Figure 14] 12A to 12C are schematic cross-sectional views illustrating a modified example of the via configuration in the waveguide element of FIG. [Figure 15] FIG. 13 is a schematic perspective view of a waveguide element according to yet another embodiment of the present invention. [Figure 16]16 is a cross-sectional view of the waveguide element of FIG. 15 along the line XVI-XVI'. [Figure 17] FIG. 16 is an exploded perspective view of the director element of FIG. [Figure 18] 17 is a schematic cross-sectional view illustrating a state in which the conductor pin in FIG. 16 is covered with an insulating material. [Figure 19] FIG. 13 is a schematic perspective view of a waveguide element according to yet another embodiment of the present invention. [Figure 20] 4 is a schematic cross-sectional view illustrating an example of an arrangement of joints in the waveguide element of FIG. 3. [Figure 21] 3 is a schematic cross-sectional view illustrating an example of an arrangement of joints in the waveguide element of FIG. 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, embodiments of the present invention will be described, but the present invention is not limited to these embodiments. A. Overall configuration of the waveguide element A-1. Overall configuration of the waveguide element 100 FIG. 1 is a schematic perspective view of a waveguide element according to one embodiment of the present invention; FIG. 2 is a cross-sectional view of the waveguide element of FIG. 1 taken along line II-II'. The waveguide element 100 of the illustrated example includes a waveguide member 10, a support substrate 20, and a low dielectric constant portion 50. The waveguide member 10 can guide electromagnetic waves having a frequency of 30 GHz or more and 20 THz or less, in other words, electromagnetic waves from millimeter waves to terahertz waves. Note that millimeter waves are typically electromagnetic waves having a frequency of about 30 GHz to 300 GHz, and terahertz waves are typically electromagnetic waves having a frequency of about 300 GHz to 20 THz. In particular, the waveguide member 10 can guide electromagnetic waves having a frequency of 30 GHz or more and 2 THz or less (particularly electromagnetic waves having a frequency of 30 GHz or more and 1 THz or less) while maintaining excellent low propagation loss. The waveguide member 10 constitutes a coplanar line, and includes an inorganic material substrate 1 and a coplanar electrode 2 provided on the inorganic material substrate 1. The support substrate 20 is provided below the inorganic material substrate 1 and supports the waveguide member 10. The low dielectric constant portion 50 is provided below the inorganic material substrate 1 and has a dielectric constant smaller than that of the inorganic material substrate 1. The low dielectric constant portion 50 is typically a low refractive index portion having a refractive index smaller than that of the inorganic material substrate 1. As will be described in detail later, in the waveguide member that constitutes the coplanar line, when a voltage is applied to the coplanar electrodes, an electric field is generated, and the above-mentioned high-frequency electromagnetic waves are coupled with the electric field and propagated. When such a waveguide member is supported by a supporting substrate and guides the above-mentioned high-frequency electromagnetic waves (particularly electromagnetic waves of 300 GHz or higher), a slab mode may be induced and / or substrate resonance may occur, resulting in a significant increase in propagation loss. In order to suppress the increase in propagation loss due to slab mode and substrate resonance, it is effective to have a structure in which the thickness of the inorganic material substrate on which the coplanar electrodes are provided is made sufficiently thin. However, in this case, a new problem arises in that the propagating electromagnetic waves leak into the supporting substrate located below the inorganic material substrate, resulting in increased propagation loss due to dielectric loss in the supporting substrate. On the other hand, by providing a low dielectric constant portion under the inorganic material substrate on which the coplanar electrodes are provided, it is possible to suppress the induction of slab modes and the occurrence of substrate resonance while suppressing leakage of the electric field to the support substrate over a wide frequency range in the high frequency region described above. Therefore, the director element can ensure excellent low propagation loss performance over a wide frequency range in the high frequency region described above. In addition, development of miniaturized waveguide elements is underway, and since circuit integration is expected in the future, it is expected that the waveguide member (line structure) will also be required to be accordingly miniaturized. In the above-mentioned waveguide element, the waveguide member (line structure) is supported by a support substrate, so that the inorganic material substrate of the waveguide member can be made thinner. As a result, it is possible to meet the demand for miniaturization while ensuring excellent low propagation loss performance over a wide frequency range in the above-mentioned high frequency region.

[0009] In one embodiment, the thickness of the inorganic material substrate 1 satisfies the following formula (1).

number

[0010] In one embodiment, the relative dielectric constant ε of the inorganic material substrate 1 at 300 GHz is typically 3.5 or more, and typically 12.0 or less, preferably 10.0 or less, and more preferably 5.0 or less. The dielectric tangent (dielectric loss) tan δ of the inorganic material substrate 1 at 300 GHz is typically 0.0030 or less, preferably 0.0020 or less, and more preferably 0.0015 or less. When the dielectric constant ε and the dielectric loss tangent (dielectric loss) tan δ of the inorganic material substrate are in the above range, excellent low propagation loss performance can be stably ensured over the wide frequency range of the high frequency range described above. The dielectric constant ε and the dielectric loss tangent (dielectric loss) tan δ can be measured by terahertz time domain spectroscopy. In addition, in this specification, when the measurement frequency is not mentioned for the dielectric constant and the dielectric loss tangent, the dielectric constant and the dielectric loss tangent at 300 GHz are meant.

[0011] The thickness of the inorganic material substrate 1 is specifically 1 μm or more, preferably 2 μm or more, more preferably 10 μm or more, and even more preferably 20 μm or more, and is, for example, 300 μm or less, preferably 200 μm or less, more preferably 100 μm or less, and even more preferably 70 μm or less. From the viewpoint of miniaturization by reducing the size of the electrodes, the thickness of the inorganic material substrate 1 is particularly preferably 60 μm or less. When the thickness of the inorganic material substrate 1 is within the above range, excellent low propagation loss performance can be more stably ensured over a wide frequency range in the above-mentioned high frequency region.

[0012] In one embodiment, the waveguide member 10 forms a grounded coplanar line, and includes a ground electrode 3. The ground electrode 3 is located between the inorganic material substrate 1 and the support substrate 20. If the waveguide member is provided with a ground electrode, the electric field generated when a voltage is applied to the coplanar electrodes can be stably prevented from leaking to the support substrate, and the occurrence of substrate resonance can also be suppressed. Although the illustrated waveguide 10 constitutes a grounded coplanar line, the waveguide of the present invention does not have to include a ground electrode, like the waveguide 11 shown in FIG.

[0013] In one embodiment, the coplanar electrode 2 includes a signal electrode 2a, a first ground electrode 2b, and a second ground electrode 2c. The signal electrode 2a has a linear shape extending in a predetermined direction (the waveguide direction of the waveguide member). The width w of the signal electrode 2a (the dimension in the direction perpendicular to the waveguide direction) is, for example, 2 μm or more, preferably 20 μm or more, for example, 200 μm or less, preferably 150 μm or less. The first ground electrode 2b is disposed at a distance from the signal electrode 2a in a direction intersecting (preferably perpendicular) the longitudinal direction of the signal electrode 2a. The second ground electrode 2c is located on the opposite side of the first ground electrode 2b with respect to the signal electrode 2a in a direction intersecting (preferably perpendicular) the longitudinal direction of the signal electrode 2a, and is disposed at a distance from the signal electrode 2a. As a result, a gap extending in the longitudinal direction of the signal electrode 2a is formed between the signal electrode 2a and the ground electrodes 2b and 2c. The width g of the gap (the dimension in the direction intersecting the longitudinal direction) is, for example, 2 μm or more, preferably 5 μm or more, and for example, 100 μm or less, preferably 80 μm or less.

[0014] 6, the ground electrodes 2b, 2c may be electrically connected to the ground electrode 3. When the ground electrodes 2b, 2c are electrically connected to the ground electrode 3, the ground can be strengthened and stray capacitance due to surrounding lines and elements can be suppressed. In the illustrated example, a plurality of via holes 9 are formed in the inorganic material substrate 1, and the ground electrode and the earth electrode are short-circuited by the vias 6 located in each via hole 9. The arrangement of the plurality of vias 6 (via holes) is not particularly limited. In the illustrated example, the plurality of vias 6 (via holes) are lined up in the longitudinal direction of the signal electrode 2a. The vias 6 are typically conductive films formed on the entire inner surface of the via holes. The vias 6 are made of a conductive material, typically a metal (described later) similar to that of the coplanar electrode 2. The via holes may be filled with a conductive material throughout the entire hole. When the vias are made of a metal film, the interior of the vias may be filled with a conductive material. The conductive material may be the same metal as the vias, or a different material such as a conductive paste.

[0015] The director element 100 may further include a second ground electrode 4. Hereinafter, the ground electrode 3 may be referred to as the first ground electrode 3. The ground electrode 3 may be referred to as the first metal layer, and the second ground electrode 4 may be referred to as the second metal layer. The second ground electrode 4 is located on the opposite side of the support substrate 20 to the first ground electrode 3. In the illustrated example, the second ground electrode 4 is formed on the surface of the support substrate 20 opposite to the first ground electrode 3, and is in direct contact with the support substrate 20. According to this configuration, the first ground electrode is disposed between the inorganic material substrate and the support substrate, and the second ground electrode is disposed on the opposite side of the support substrate to the first ground electrode, so that leakage of electromagnetic waves to the support substrate can be further suppressed.

[0016] The director element 100 may include a through-substrate via 22 that electrically connects the first ground electrode 3 and the second ground electrode 4. The director element 100 shown in Fig. 6 includes a via 6 that connects the first ground electrode 3 and the ground electrode of the coplanar electrode 2, and a through-substrate via 22 that connects the first ground electrode 3 and the second ground electrode 4. This further strengthens the ground and stray capacitance due to surrounding lines and elements can be stably suppressed.

[0017] As shown in FIG. 1 and FIG. 2, in one embodiment, the low dielectric constant portion 50 is a cavity. In other words, the cavity functions as the low dielectric constant portion 50 (low refractive index portion). More specifically, the support substrate 20 has a recess 21, and the cavity is defined by the lower surface of the inorganic material substrate 1 and the recess 21 of the support substrate 20. The recess 21 is typically recessed downward from the upper surface of the support substrate 20 and extends in the same direction as the signal electrode 2a. When the ground electrode 3 is provided on the inner surface of the recess 21, the cavity may be defined by the lower surface of the inorganic material substrate 1 and the ground electrode 3 provided on the inner surface of the recess 21. In one embodiment, the cavity (low dielectric constant portion) 50 is arranged so as to overlap at least a part of the signal electrode in the thickness direction of the inorganic material substrate 1. The low dielectric constant portion preferably has a dielectric constant of less than 3.5, and may be, for example, SiO2, magnesium fluoride, calcium fluoride, or a low dielectric constant polymer (for example, a Teflon (registered trademark)-based polymer with a relative dielectric constant of 2.3). When the low dielectric constant portion is hollow, the electromagnetic waves propagating through the waveguide can be more stably prevented from leaking out of the waveguide than when the low dielectric constant portion is made of other materials, and the propagation loss (dielectric loss) in the low dielectric constant portion can be more effectively suppressed.

[0018] In one embodiment, the lower limit of the cavity dimension d in the thickness direction of the inorganic material substrate 1 is equal to or larger than the width g of the void (gap), preferably equal to or larger than 2 g. The upper limit of the cavity dimension d in the thickness direction of the inorganic material substrate 1 is equal to or smaller than 20 g, preferably equal to or smaller than 5 g. If the dimensions of the cavity are equal to or greater than the lower limit, it is possible to further reduce the propagation loss when guiding the above-mentioned high-frequency electromagnetic waves.

[0019] In one embodiment, the lower limit of the cavity size in the width direction (direction perpendicular to the waveguiding direction) of the inorganic material substrate 1 is equal to or larger than the width w of the signal electrode, preferably equal to or larger than the width w of the signal electrode plus the width g of the void (gap) × 2. The upper limit of the cavity size in the width direction of the inorganic material substrate 1 is equal to or smaller than the width w of the signal electrode plus the width g of the void (gap) × 40, preferably equal to or smaller than the width w of the signal electrode plus the width g of the void (gap) × 20.

[0020] When the low dielectric constant portion is other than a cavity, the low dielectric constant portion made of the above-mentioned materials may be disposed in the recess 21 of the support substrate 20 . 4 and 5, the support substrate 20 may not have the recess 21, and a low dielectric constant portion 51 made of the above-mentioned material may be disposed between the inorganic material substrate 1 and the support substrate 20. In the illustrated example, the low dielectric constant portion 51 is formed in a layer shape and is sandwiched between the inorganic material substrate 1 and the ground electrode 3. The range of the dimension d of the low dielectric constant portion 51 in the thickness direction of the inorganic material substrate 1 is the same as the range of the dimension d of the cavity in the thickness direction of the inorganic material substrate 1 described above.

[0021] A-2. Overall configuration of the director element 101 7 is a schematic perspective view of a waveguide element according to another embodiment of the present invention; FIG. 8 is a cross-sectional view of the waveguide element of FIG. 7 taken along line VIII-VIII'; FIG. 9 is a cross-sectional view of the waveguide element of FIG. 7 taken along line IX-IX'; and FIG. 10 is a cross-sectional view of the waveguide element of FIG. 7 taken along line XX'.

[0022] The illustrated waveguide element 101 includes the inorganic material substrate 1, the coplanar electrode 2, the first ground electrode 3, the support substrate 20, and the second ground electrode 4, as well as a first via 5 and a second via 6. Although not shown, the waveguide element 101 may include a joint portion, which will be described later.

[0023] In one embodiment, the first via 5 electrically connects the ground electrode of the coplanar electrode 2 to the second ground electrode 4, and is also electrically connected to the first ground electrode 3. The director element 101 includes a plurality of the above-mentioned first vias 5. The second via 6 electrically connects the first ground electrode 3 to the ground electrode. The second via 6 is disposed between adjacent first vias 5 among the plurality of first vias 5. According to this configuration, the first via electrically connects the first ground electrode, the second ground electrode, and the ground electrode of the coplanar electrode. Therefore, the ground can be further strengthened, and the stray capacitance due to the surrounding lines and elements can be suppressed more stably. In addition, an excellent heat dissipation function can be added to the support substrate, and transmission in a high-order mode can be suppressed. In addition, the relative positional accuracy of the part of the first via located between the first ground electrode and the ground electrode and the part located between the first ground electrode and the second ground electrode can be easily ensured. Therefore, the occurrence of ripples can be suppressed compared to the case where the via connecting the first ground electrode and the ground electrode and the via connecting the first ground electrode and the second ground electrode are provided separately (see FIG. 6). Furthermore, the waveguide element 101 including the first via 5 can be manufactured more smoothly compared to the waveguide element 100 shown in FIG. Furthermore, since the second vias are disposed between the adjacent first vias, the pitch of the first and second vias in the inorganic material substrate can be made smaller than the pitch of the first vias in the support substrate, so that the strength of the inorganic material substrate can be sufficiently ensured even if the inorganic material substrate is thinned.

[0024] A-2-1. First via 7, in the waveguide element 101, the first vias 5 are provided on both sides of the signal electrode 2a in a direction intersecting (preferably perpendicular) to the longitudinal direction of the signal electrode 2a. In the following, the first vias electrically connecting the first ground electrode 2b and the second ground electrode 4 may be referred to as the first via 5a, and the first vias electrically connecting the second ground electrode 2c and the second ground electrode 4 may be referred to as the first via 5b, to be distinguished from each other. As shown in FIG. 8, the first via 5a is in contact with the first ground electrode 2b and the second ground electrode 4, and extends continuously between the first ground electrode 2b and the second ground electrode 4. The first via 5b is in contact with the second ground electrode 2c and the second ground electrode 4, and extends continuously between the second ground electrode 2c and the second ground electrode 4. Each of the first vias 5a and 5b penetrates the first ground electrode 3 and is in contact with the first ground electrode 3. Note that the director element may include only one of the first vias 5a and 5b.

[0025] The first via 5 is typically a conductive film. The first via 5 is made of a conductive material, typically a metal (described later) similar to that of the coplanar electrode 2. The shape of the first via 5 corresponds to the shape of the first via hole 8 in which it is arranged. That is, the waveguide element 101 has a plurality of first via holes 8 corresponding to a plurality of first vias 5. The first via hole 8 penetrates the inorganic material substrate 1, the first ground electrode 3, and the support substrate 20. The first via hole 8 typically has a circular shape when viewed from above the inorganic material substrate 1. When the first via hole has a circular shape, the inner diameter of the first via hole is, for example, 10 μm or more, preferably 20 μm or more, and, for example, 200 μm or less, preferably 100 μm or less, more preferably 80 μm or less.

[0026] 8, the first via hole 8 has a circular shape when viewed from above the inorganic material substrate 1, and penetrates the inorganic material substrate 1, the first ground electrode 3, and the support substrate 20 linearly in the thickness direction of the inorganic material substrate 1. When the first via hole is circular and linear, the first via 5 has a columnar or cylindrical shape extending in the thickness direction of the inorganic material substrate 1. In this case, the range of the outer diameter of the first via 5 is the same as the range of the inner diameter of the above-mentioned first via hole.

[0027] 11, the first via hole 8 may have a circular shape when viewed from above the inorganic material substrate 1, and may have a tapered shape with a smaller diameter toward the first ground electrode 3. Although not shown, the first via hole 8 may have a circular shape when viewed from above the inorganic material substrate 1, and may have a tapered shape with a larger diameter toward the ground electrode 3. When the first via hole has a tapered shape, it is possible to provide features such as facilitating the formation of a conductive film in the first via and facilitating the securing of strength of the support substrate. In addition, the first via may be formed such that a conductive material is embedded in the first via hole. When the first via hole is circular and tapered, the first via 5 preferably has an hourglass shape in which the diameter is small at the contact portion with the first ground electrode 3 and the diameter becomes larger as it moves away from the first ground electrode 3. In other words, the first via 5 preferably has a shape in which the apexes of two cones are connected to each other. In this case, the maximum outer diameter of the first via 5 falls within the above range. In one embodiment, the outer diameter of one end of the first via 5 that contacts the ground electrode is smaller than the outer diameter of the other end of the first via 5 that contacts the second ground electrode. In the first via 5, the taper angle on the coplanar electrode 2 side with respect to the first ground electrode is smaller than the taper angle on the second ground electrode side with respect to the first ground electrode. In the illustrated example, the ground electrode and the second ground electrode of the coplanar type electrode are each formed to block the first via hole, but the configuration of the ground electrode and the second ground electrode is not limited to this. Each of the ground electrode and the second ground electrode only needs to be electrically connected to the first via, and may be open without blocking the first via hole.

[0028] The pitch P1 of the multiple first vias 5a (the distance between the centers of adjacent first vias 5) is, for example, 40 μm or more, preferably 60 μm or more, and for example, 600 μm or less, preferably 400 μm or less, more preferably 200 μm or less.

[0029] 7 to 11, the multiple first vias 5 are arranged at intervals in the longitudinal direction of the signal electrode 2a. The direction in which the multiple first vias 5 are arranged is not limited to the longitudinal direction of the signal electrode 2a. As shown in FIG. 13, the multiple first vias 5 may be arranged at intervals in a direction intersecting (preferably perpendicular) the longitudinal direction of the signal electrode 2a. The waveguide element may have multiple rows of first vias 5 arranged in the longitudinal direction of the signal electrode 2a in a direction intersecting (preferably perpendicular) the longitudinal direction of the signal electrode 2a.

[0030] A-2-2. Second via As shown in FIG. 7, in the director element 101, the second vias 6 are provided on both sides of the signal electrode 2a in a direction intersecting (preferably perpendicular to) the longitudinal direction of the signal electrode 2a. In the following, the second vias electrically connecting the first ground electrode 2b and the first ground electrode 3 may be referred to as the second via 6a, and the second vias electrically connecting the second ground electrode 2c and the first ground electrode 3 may be referred to as the second via 6b, and may be distinguished from each other. The second via 6a is in contact with the first ground electrode 2b and the first ground electrode 3, but is not in contact with the second ground electrode 4. The second via 6b is in contact with the second ground electrode 2c and the first ground electrode 3, but is not in contact with the second ground electrode 4. The director element may include only one of the second vias 6a and 6b.

[0031] The second via 6 is typically a conductive film. The second via 6 is made of a conductive material, typically a metal (described later) similar to that of the first via 5. The shape of the second via 6 corresponds to the shape of the second via hole 9 in which it is disposed. In other words, the waveguide element 101 has a second via hole 9 corresponding to the second via 6.

[0032] 9, the second via hole 9 penetrates at least the inorganic material substrate 1 and does not penetrate the support substrate 20. The second via hole 9 typically has a circular shape when viewed from above the inorganic material substrate 1. When the second via hole has a circular shape, the range of the inner diameter of the second via hole is, for example, the same as the range of the inner diameter of the first via hole described above.

[0033] The second via hole 9 in the illustrated example penetrates the inorganic material substrate 1 linearly in the thickness direction of the inorganic material substrate 1, and does not penetrate the first ground electrode 3. When the second via hole 9 is circular and linear, the second via 6 has a columnar or cylindrical shape extending in the thickness direction of the inorganic material substrate 1. In this case, the range of the outer diameter of the second via 6 is the same as the range of the inner diameter of the above-mentioned second via hole.

[0034] As shown in FIG. 11, the second via hole 9 may have a conical shape that tapers away from the coplanar electrode 2. The second via hole 9 in the illustrated example penetrates the inorganic material substrate 1 and the first ground electrode 3, and its tip reaches the support substrate 20. When the second via hole 9 has a conical shape, the second via 6 preferably has a conical shape similar to that of the second via hole 9. In this case, the maximum outer diameter of the second via 6 is within the range of the inner diameter of the second via hole. In addition, the apex of the second via 6 (the end of the second via 6 opposite to the coplanar electrode 2) may reach the support substrate 20. In the illustrated example, the ground electrode is formed so as to cover the second via hole, but the configuration of the ground electrode is not limited to this. The ground electrode only needs to be electrically connected to the second via, and the second via hole may be open and not covered.

[0035] 10 to 13, the second via 6 is disposed between adjacent first vias 5 among a plurality of first vias 5 aligned in a predetermined direction. The second via 6 is typically located at the center of the space between the adjacent first vias 5. The illustrated waveguide element 101 has a plurality of second vias 6 (a plurality of second vias 6a and a plurality of second vias 6b). The second vias 6 shown in Figs. 7 to 12 are disposed between the first vias 5 adjacent to each other in the longitudinal direction of the signal electrode 2a. The second vias 6 shown in Fig. 13 are disposed between the first vias 5 adjacent to each other in a direction intersecting (preferably perpendicular to) the longitudinal direction of the signal electrode 2a. Also, the second vias 6 can be arranged at any appropriate position between the first vias 5 adjacent to each other. The second vias 6 may be arranged for every n first vias 5 in the direction in which the multiple first vias are arranged. n is, for example, 1 or more and 5 or less, and preferably 1 or 2. More preferably, the first vias 5 and the second vias 6 are arranged alternately. Also, the multiple second vias 6 may all be arranged between the first vias 5 adjacent to each other as shown in Figs. 10 and 11, or may include a second via 6 that is not arranged between the first vias 5 as long as at least one second via 6 is arranged between the first vias 5 adjacent to each other as shown in Fig. 12.

[0036] As shown in Figure 11, the pitch P2 between adjacent first vias 5 and second vias 6 (the distance between the centers of adjacent first vias 5 and second vias 6) is substantially 1 / 2 of the pitch P1 (the distance between the centers of adjacent first vias 5), and is, for example, 25 μm or more, preferably 60 μm or more, and for example, 600 μm or less, preferably 400 μm or less, and more preferably 200 μm or less. In this way, by arranging the second vias 6 between the adjacent first vias 5, the pitch P2 of the first vias 5 and the second vias 6 in the inorganic material substrate 1 can be made smaller than the pitch P1 of the first vias 5 in the support substrate 20. Therefore, even if the inorganic material substrate is thinned, the strength of the inorganic material substrate can be sufficiently ensured.

[0037] A-2-3. Modifications of the director element 101 14, the waveguide element 101 may include the first via 5 but may not include the second via 6. However, as shown in FIG. 14, if the first via hole 8 has a tapered shape that increases in diameter as it moves away from the first ground electrode 3 and the thickness of the support substrate 20 is greater than that of the inorganic material substrate 1, the outer diameter of the other end of the first via 5 that contacts the second ground electrode 4 may be larger than the outer diameter of the one end of the first via 5 that contacts the ground electrode. In this case, if the pitch P of the multiple first vias 5 is narrowed to the pitch P2 described above without providing the second vias 6, the other ends of the first vias 5 may interfere with each other. Therefore, it is preferable that the waveguide element 101 includes the first via 5 and the second via 6 and the second via 6 is disposed between the adjacent first vias 5, since this can suppress the interference between the first vias 5.

[0038] A-3. Overall configuration of director element 102 15 is a schematic perspective view of a waveguide element according to yet another embodiment of the present invention; FIG. 16 is a cross-sectional view taken along line XVI-XVI' of the waveguide element of FIG. 15; and FIG. 17 is an exploded perspective view of the waveguide element of FIG. The illustrated waveguide element 102 includes the inorganic material substrate 1, the coplanar electrode 2, the first ground electrode 3, the support substrate 20, and the second ground electrode 4, as well as a plurality of through-substrate vias 22. Although not shown, the waveguide element 102 may include a bonding portion, which will be described later. Each of the plurality of through-substrate vias 22 electrically connects the first ground electrode 3 and the second ground electrode 4. The first ground electrode 3, the second ground electrode 4, and the plurality of through-substrate vias 22 constitute a substrate integrated waveguide (hereinafter, referred to as SIW) capable of propagating electromagnetic waves. This allows the SIW to be provided on the supporting substrate, and the supporting substrate can be effectively used as a waveguide.

[0039] In one embodiment, the coplanar electrode 2 further includes a third ground electrode 2d in addition to the signal electrode 2a, the first ground electrode 2b, and the second ground electrode 2c. In this embodiment, one end of the signal electrode 2a is located between the first ground electrode 2b and the second ground electrode 2c that are spaced apart from each other. The first ground electrode 2b and the second ground electrode 2c may be electrically connectable to an external element (not shown). The third ground electrode 2d is spaced apart from the other end of the signal electrode 2a by a predetermined distance. The third ground electrode 2d has a substantially C-shape when viewed from above, and surrounds the other end of the signal electrode 2a. The coplanar electrode 2 does not necessarily have to include the third ground electrode 2d.

[0040] The director element 102 may further include the above-mentioned vias 6. This strengthens the ground and suppresses stray capacitance due to surrounding lines and elements. In the illustrated example, each of the ground electrodes 2b, 2c, and 2d is electrically connected to the first ground electrode 3 by a plurality of vias 6.

[0041] Each of the plurality of through-substrate vias 22 penetrates the support substrate 20 in the thickness direction and is periodically arranged in the support substrate 20. Typically, the plurality of through-substrate vias 22 includes a first via row 22a and a second via row 22b. Each of the first via row 22a and the second via row 22b is composed of a plurality of through-substrate vias 22 arranged at intervals in a predetermined direction. The second via row 22b is located away from the first via row 22a in a direction perpendicular to the extension direction of the first via row 22a. In one embodiment, in the support substrate 20, a region surrounded by the first ground electrode 3, the second ground electrode 4, the first via row 22a, and the second via row 22b functions as a SIW. In the illustrated example, the cavity (low dielectric constant portion) 50 is aligned with the SIW in the extension direction of the first via row 22a.

[0042] 16, the through-substrate via 22 is made of a conductive material, and is typically made of the same metal (described later) as the coplanar electrode 2. The through-substrate via 22 is disposed in a substrate via hole 24. That is, the waveguide element 102 has a plurality of substrate via holes 24 corresponding to the plurality of through-substrate vias 22. In the illustrated example, the substrate via holes 24 penetrate the first ground electrode 3, the support substrate 20 and the second ground electrode 4 all at once. The through-substrate vias 22 are typically conductive films formed on the entire inner surface of the substrate via holes 24. The substrate via holes 24 may penetrate only the support substrate without penetrating the first and second ground electrodes. In this case, the through-substrate vias are arranged so as to be in contact with the first and second ground electrodes. substrate The via hole is filled with the conductive material. When the through-substrate via 22 that electrically connects the first ground electrode 3 and the second ground electrode 4 is formed of a conductive film, the inside of the through-substrate via 22 may be filled with a material such as a resin.

[0043] In the director element 102, the transmission line and the SIW formed by the signal electrode 2a may be independent of each other, or may be coupled so as to allow electromagnetic waves to propagate. In one embodiment, the transmission line (coplanar transmission line) formed by the coplanar electrode 2 and the SIW are coupled by a conductor pin 25. This makes it possible to convert the propagation mode of the electromagnetic wave between a transmission line mode and a waveguide mode. For example, an electromagnetic wave (signal) in the transmission line mode propagating through an inorganic material substrate can be converted into an electromagnetic wave in the waveguide mode propagating through a support substrate via a conductor pin. The support substrate can function as an antenna that spatially radiates the electromagnetic wave propagating in the waveguide mode in the in-plane direction of the substrate.

[0044] The conductor pin 25 passes through the inorganic material substrate 1 from the signal electrode 2a and reaches the SIW in the support substrate 20. The conductor pin 25 can be a propagation medium for electromagnetic waves. The conductor pin 25 is made of a conductive material, and is typically made of the same metal (described later) as the coplanar electrode 2. In the illustrated example, the conductor pin 25 extends in the thickness direction of the inorganic material substrate 1. The conductor pin 25 may be a columnar shape such as a cylindrical shape, or may be a cylindrical shape (hollow shape) such as a cylindrical shape. The base end of the conductor pin 25 is connected to the end of the signal electrode 2a. The free end of the conductor pin 25 is inserted into an insertion hole 26 formed in the support substrate 20 (see FIG. 17). The insertion hole 26 is located between the first via row 22a and the second via row 22b, and is aligned with the recess 21. The portion of the conductor pin 25 between the base end and the free end is inserted into an opening 31 of the first ground electrode 3. The conductor pin 25 is preferably insulated from the first ground electrode 3. In one embodiment, as shown in FIG. 17, the opening 31 forms an air layer around the conductor pin 25. The opening 31 is larger than the outer shape of the conductor pin 25, and the entire periphery of the opening 31 is separated from the conductor pin 25. This makes it possible to insulate the conductor pin from the first ground electrode, and in turn to stably insulate the signal electrode from the first ground electrode. In addition, it is possible to further suppress substrate resonance caused by leakage of the electric field to the support substrate. Furthermore, it is possible to suppress the effect of dielectric loss compared to a structure in which the air layer is filled with resin.

[0045] 18, the conductor pin 25 may be covered with an insulating material 15. This also makes it possible to insulate the conductor pin from the first ground electrode. Examples of insulating materials include resin and SiO2.

[0046] A-4. Overall configuration of director element 103 Fig. 19 is a schematic perspective view of a waveguide element according to still another embodiment of the present invention, in which the ground electrode and vias are omitted for convenience. The director element 103 includes a plurality of signal electrodes spaced apart from each other. Therefore, the director element 103 includes a plurality of transmission lines corresponding to the signal electrodes. More specifically, the director element 103 includes a coplanar electrode 2 including a first signal electrode 2a and a second signal electrode 2e, and a first conductor pin and a second conductor pin (not shown). The director element 103 also includes a first cavity (first low dielectric constant portion) 50 and a second cavity (second low dielectric constant portion) 51. The first cavity 50 is disposed in the thickness direction of the inorganic material substrate 1 so as to overlap at least a portion of the first signal electrode 2a. The second cavity 51 is disposed in the thickness direction of the inorganic material substrate 1 so as to overlap at least a portion of the second signal electrode 2e. The first signal electrode 2a constitutes a first transmission line together with a ground electrode (not shown), and the second signal electrode 2e constitutes a second transmission line together with a ground electrode (not shown). The first conductor pin couples the first transmission line to an SIW consisting of the first ground electrode 3, the second ground electrode 4, and the multiple through-substrate vias 22. The second conductor pin couples the second transmission line to an SIW consisting of the first ground electrode 3, the second ground electrode 4, and the multiple through-substrate vias 22. As a result, in one embodiment, an electromagnetic wave (signal) in a transmission line mode propagating through the inorganic material substrate can be converted to a SIW mode via the first conductor pin, then propagated through the support substrate in the SIW mode, and then converted again to a transmission line mode propagating through the inorganic material substrate via the second conductor pin. In this embodiment, the electromagnetic wave propagated through the inorganic material substrate can be emitted from an antenna element provided on the inorganic material substrate.

[0047] Each of the above-mentioned waveguide elements includes one support substrate 20, but the number of support substrates 20 is not particularly limited. Although not shown, in the waveguide element, a plurality of support substrates may be arranged at intervals from each other in the thickness direction of the inorganic material substrate, and a substrate integrated waveguide (SIW) may be provided on each of the plurality of support substrates. With this configuration, the antenna portion that radiates electromagnetic waves in SIW mode can be arrayed in the thickness direction. Therefore, such a waveguide element can be used as a phased array antenna in wireless communication. In addition, when the waveguide element includes a plurality of support substrates, adjacent support substrates among the plurality of support substrates may be board A second ground electrode may be disposed between the first and second ground electrodes. Thus, the SIW provided on each support substrate is composed of metal layers (i.e., a first ground electrode and a second ground electrode, or two second ground electrodes) disposed on both sides of the support substrate, and a plurality of through-substrate vias penetrating the support substrate.

[0048] In addition, the waveguide element may include a plurality of waveguide units including SIW arranged at intervals in a thickness direction of the inorganic material substrate, each of the plurality of waveguide units including a first ground electrode, a support substrate, a second ground electrode, and a plurality of through-substrate vias. A spacer substrate may be provided between adjacent ones of the plurality of support substrates. The spacer substrate may be disposed between adjacent waveguide units. By providing the spacer substrate, the spacing between the antenna portions of the plurality of support substrates can be adjusted. In particular, by adjusting the spacing between the plurality of antenna portions to λ / 2, the radiation angle of the electromagnetic wave can be sufficiently scanned. Representative materials for the spacer substrate include inorganic material substrates, as well as inorganic material substrates. inorganic Materials (described below) are included. Moreover, a waveguide element having multiple SIWs preferably has the same number of signal electrodes and conductor pins as the number of SIWs. Each conductor pin couples a transmission path formed by each signal electrode to a corresponding SIW. With such a configuration, it is relatively easy to manufacture and can easily transmit a signal (electromagnetic wave) from an external signal source installed on the inorganic material substrate to the SIW of each supporting substrate.

[0049] In this specification, the term "waveguide element" encompasses both a wafer on which at least one waveguide element is formed (waveguide element wafer) and a chip obtained by cutting the waveguide element wafer.

[0050] B. Inorganic material substrate The inorganic material substrate 1 has an upper surface on which a coplanar electrode 2 is provided, and a lower surface located within the composite substrate. The inorganic material substrate 1 is made of an inorganic material. Any suitable material may be used as the inorganic material as long as the effect of the embodiment of the present invention can be obtained. Representative examples of such materials include single crystal quartz (relative dielectric constant 4.5, dielectric dissipation factor 0.0013), amorphous quartz (quartz glass, relative dielectric constant 3.8, dielectric dissipation factor 0.0010), spinel (relative dielectric constant 8.3, dielectric dissipation factor 0.0020), AlN (relative dielectric constant 8.5, dielectric dissipation factor 0.0015), sapphire (relative dielectric constant 9.4, dielectric dissipation factor 0.0030), SiC (relative dielectric constant 9.8, dielectric dissipation factor 0.0022), magnesium oxide (relative dielectric constant 10.0, dielectric dissipation factor 0.0012), and silicon (relative dielectric constant 11.7, dielectric dissipation factor 0.0016) (the relative dielectric constant and dielectric dissipation factor in parentheses indicate values ​​at a frequency of 300 GHz). The inorganic material substrate 1 is preferably a quartz glass substrate made of amorphous quartz. If the inorganic material substrate 1 is a quartz glass substrate, it is possible to stably suppress an increase in propagation loss even when guiding the above-mentioned high-frequency electromagnetic waves. Furthermore, since the dielectric constant is larger than that of resin-based substrates, the substrate size can be made smaller, and since the dielectric constant is relatively small among inorganic materials, it is advantageous in terms of reducing delay. In addition, silica glass has a small dielectric loss (tan δ) and, unlike resin-based substrates, can be formed with a conductor layer (metal layer) for forming lines without roughening or surface treatment, which further reduces propagation loss.

[0051] C. Coplanar Electrodes and Ground Electrodes The coplanar electrode 2 is typically provided on the upper surface of the inorganic material substrate 1 and is in direct contact with the inorganic material substrate 1. The coplanar electrode 2 is typically made of a metal. Examples of metals include chromium (Cr), nickel (Ni), copper (Cu), and gold (Au). The metals can be used alone or in combination. The coplanar electrode 2 may be a single layer, or may be formed by laminating two or more layers. The coplanar electrode 2 is formed on the inorganic material substrate 1 by a known film formation method such as sputtering (other methods include deposition and printing). The thickness of the coplanar electrode 2 is, for example, 1 μm or more, preferably 4 μm or more, and is, for example, 20 μm or less, preferably 10 μm or less. The first ground electrode 3 is provided on the upper surface of the support substrate 20. The first ground electrode 3 can be made of the same metal as the coplanar electrode 2. The metal of the first ground electrode 3 may be the same as the metal of the coplanar electrode 2. Coplanar type electrodes The metal of the first ground electrode 3 may be different from that of the coplanar electrode 2. The thickness range of the first ground electrode 3 is similar to the thickness range of the coplanar electrode 2. The first ground electrode 3 is formed on the surface of the support substrate 20 by, for example, sputtering or plating. The second ground electrode 4 is formed on the surface of the support substrate 20 opposite to the first ground electrode 3, for example, by sputtering or plating. The second ground electrode 4 can be made of the same metal as the coplanar electrode 2. The metal of the second ground electrode 4 may be the same as the metal of the coplanar electrode 2, or may be different from the metal of the coplanar electrode 2. The thickness range of the second ground electrode 4 is the same as the thickness range of the coplanar electrode 2. The second ground electrode 4 does not necessarily have to be formed on the entire surface of the support substrate 20 opposite to the first ground electrode.

[0052] D. Support substrate The support substrate 20 has an upper surface located inside the composite substrate and a lower surface exposed to the outside. The above-mentioned recess 21 may be formed on the upper surface of the support substrate 20. The support substrate 20 is provided to increase the strength of the composite substrate, and thereby the thickness of the inorganic material substrate can be reduced as described above. Any appropriate configuration may be adopted for the support substrate 20. Specific examples of materials constituting the support substrate 20 include indium phosphide (InP), silicon (Si), glass, sialon (Si3N4-Al2O3), mullite (3Al2O3·2SiO2, 2Al2O3·3SiO2), aluminum nitride (AlN), magnesium oxide (MgO), aluminum oxide (Al2O3), spinel (MgAl2O4), sapphire, quartz, quartz, gallium nitride (GaN), silicon carbide (SiC), silicon nitride (Si3N4), and gallium oxide (Ga2O3). The support substrate 20 is preferably made of at least one selected from the group consisting of indium phosphide, silicon, aluminum nitride, silicon carbide, and silicon nitride, and more preferably made of silicon. When active elements such as an oscillator or a receiver are mounted on the waveguide element 100, the inorganic material substrate may heat up, deteriorating the characteristics of other active elements and mounted components. To prevent this, a material with high thermal conductivity may be used for the support substrate. In this case, the thermal conductivity is preferably 150 W / Km or more, and from this viewpoint, examples of the support substrate 20 include silicon (Si), aluminum nitride (AlN), gallium nitride (GaN), silicon carbide (SiC), and silicon nitride (Si3N4).

[0053] Furthermore, when an SIW is formed on the support substrate 20, a material with a small dielectric loss tan δ is preferred in order to reduce the loss of the electromagnetic wave propagating through the SIW. In this case, the material of the support substrate is preferably selected from single crystal quartz, amorphous quartz, spinel, AlN, sapphire, aluminum oxide, SiC, magnesium oxide, or silicon. Of such materials for the support substrate, silicon is more preferable.

[0054] The thickness of the support substrate 20 is determined by setting the relative dielectric constant of the support substrate 20 to ε b If the wavelength of the electromagnetic wave guided by the waveguide element is λ, then, for example, λ / 4√ε b More preferably, λ / 2√ε b or more, for example, 2λ / √ε b Below 3λ / 2√ε, preferably b More preferably, λ / √ε b If the thickness of the support substrate is equal to or greater than the lower limit, the mechanical strength of the waveguide element can be stably improved. If the thickness of the support substrate is equal to or less than the upper limit, slab mode propagation can be suppressed, the waveguide element can be made thinner (maintaining the mechanical strength of the waveguide element), and substrate resonance can be suppressed. When a plurality of support substrates are arranged at intervals in the thickness direction of the inorganic material substrate, if the substrate is used as a phased array antenna, the interval between adjacent support substrates is desirably about λ / 2, which is suitable for the antenna pitch. If the thickness of the support substrate is less than the above interval, a spacer substrate can be provided between the adjacent support substrates to ensure an appropriate antenna pitch.

[0055] The linear expansion coefficient of the material constituting the support substrate 20 is preferably as close as possible to the linear expansion coefficient of the material constituting the inorganic material substrate 1. With such a configuration, thermal deformation (typically, warpage) of the composite substrate can be suppressed. Preferably, the linear expansion coefficient of the material constituting the support substrate 20 is within a range of 50% to 150% of the linear expansion coefficient of the material constituting the inorganic material substrate 1.

[0056] The support substrate 20 typically supports the waveguide member 10 by being directly bonded to the waveguide member 10. In one embodiment, the inorganic material substrate 1 and the support substrate 20 are directly bonded to each other. In this specification, "direct bonding" means that two layers or substrates are bonded to each other without the intermediation of an adhesive (e.g., an organic adhesive such as a resin). The form of direct bonding can be appropriately set according to the configuration of the layers or substrates to be bonded to each other. Furthermore, the interface bonded by direct bonding is typically amorphous. Therefore, the thermal resistance of the bonding interface can be dramatically reduced compared to resin bonding (resin bonding) using an organic adhesive. As a result, when an active element (e.g., an oscillator, a receiver, etc.) is mounted on the waveguide element, even if heat generated from the active element is transmitted to the inorganic material substrate, such heat can be smoothly released from the inorganic material substrate to the package via the support substrate. As a result, the inorganic material substrate can be prevented from being heated, and deterioration of the characteristics of other members (e.g., other active elements, mounted components) connected to the inorganic material substrate can be suppressed. The form of direct bonding can also include bonding between the support substrate and the inorganic material substrate via the above-mentioned ground electrode 3 and / or a bonding portion 60 described below. Furthermore, by integrating them by direct bonding, peeling in the waveguide element can be effectively suppressed, and as a result, damage (e.g., cracks) to the inorganic material substrate caused by such peeling can be effectively suppressed.

[0057] 20 , the waveguide element 100 may further include a bonding portion 60 provided between the waveguide member 11 and the support substrate 20 to bond the waveguide member 11 to the support substrate 20. When the support substrate 20 has a recess 21, the bonding portion 60 is typically provided between the waveguide member 11 and a portion of the support substrate 20 other than the recess 21. In this embodiment, only the bonding portion 60 is provided between the inorganic material substrate 1 and the support substrate 20. As a result, the inorganic material substrate 1 and the support substrate 20 are directly bonded to each other only via the bonding portion 60.

[0058] In the waveguide element 100 shown in FIG. 1 and FIG. 2, the joint 60 is located between the inorganic material substrate 1 and the ground electrode 3 located in a portion other than the recess 21 of the support substrate 20, and they may be integrated. As shown in FIG. 21, the ground electrode 3 is formed on the surface of the support substrate 20 on the inorganic material substrate side, and is in direct contact with the support substrate 20. In this embodiment, the joint 60 is located between the inorganic material substrate 1 and the ground electrode 3, and bonds the inorganic material substrate 1 and the ground electrode 3. In the illustrated example, the ground electrode 3 and the joint 60 are provided between the inorganic material substrate 1 and the support substrate 20. As a result, the inorganic material substrate 1 and the support substrate 20 are directly bonded via the ground electrode 3 and the joint 60.

[0059] 2, the ground electrode 3 may be in direct contact with the inorganic material substrate 1 and the supporting substrate 20 other than the recess 21, and may function as a bonding portion bonding the inorganic material substrate 1 and the supporting substrate 20. In this embodiment, only the ground electrode 3 is provided between the inorganic material substrate 1 and the supporting substrate 20. As a result, the inorganic material substrate 1 and the supporting substrate 20 are directly bonded via the ground electrode 3. When the ground electrode 3 functions as a bonding portion, metal layers may be formed on both the inorganic material substrate 1 and the supporting substrate 20, and the metal layers may be directly bonded to form the ground electrode 3. In this case, the bonding interface is formed inside the ground electrode.

[0060] In addition, in the waveguide element 100 shown in Figures 4 and 5, the junction may be located between the low dielectric constant portion 51 and the inorganic material substrate 1, or between the low dielectric constant portion 51 and the ground electrode 3, or they may be integrated together.

[0061] As described above, it is preferable that no organic material such as an adhesive for bonding is interposed between the coplanar electrode 2 and the support substrate 20. This can reduce the thermal resistance at the interface between the inorganic material substrate 1 and the support substrate 20, and suppress the deterioration of the characteristics of the active elements and mounted components. However, when the low dielectric constant portion is made of an organic material such as a low dielectric constant polymer, an organic material as the low dielectric constant portion may be disposed between the coplanar electrode 2 and the support substrate 20. A structure in which no organic material (such as an adhesive) other than the low dielectric constant portion is interposed can be obtained by directly bonding the inorganic material substrate 1 and the support substrate 20 (either or both of the inorganic material substrate 1 and the support substrate 20 may or may not have a ground electrode formed thereon).

[0062] The joint may be a single layer, or may be a laminate of two or more layers. The joint is typically made of an inorganic material. Examples of the joint layer that forms the joint include SiO2, amorphous silicon, and tantalum oxide. The joint may be a metal film selected from gold (Au), titanium (Ti), platinum (Pt), chromium (Cr), copper (Cu), tin (Sn), or a combination (alloy) thereof. When the joint is a metal film, the adhesion with the ground electrode made of metal can be stably ensured, and migration can be suppressed. Among these joints, an amorphous silicon layer is preferable. The thickness of the joint is, for example, 0.001 μm or more and 10 μm or less, and preferably 0.1 μm or more and 3 μm or less. The bonding layer is preferably formed only on the bonding portion, but may be formed on the recessed portion since the effect on the propagation of electromagnetic waves is small within the above-mentioned thickness range.

[0063] Direct bonding can be achieved, for example, by the following procedure: In a high vacuum chamber (for example, 1×10 -6A neutralizing beam is irradiated to each of the bonding surfaces of the components (layers or substrates) to be bonded at a pressure of about 100 Pa. This activates each bonding surface. Next, the activated bonding surfaces are brought into contact with each other in a vacuum atmosphere and bonded at room temperature. The load during this bonding can be, for example, 100 N to 20,000 N. In one embodiment, when performing surface activation using the neutralizing beam, an inert gas is introduced into the chamber, and a high voltage is applied from a DC power source to an electrode placed in the chamber. With this configuration, electrons are moved by an electric field generated between the electrode (positive electrode) and the chamber (negative electrode), and a beam of atoms and ions is generated by the inert gas. Of the beams that reach the grid, the ion beam is neutralized by the grid, and a beam of neutral atoms is emitted from the high-speed atom beam source. The atomic species that constitute the beam is preferably an inert gas element (for example, argon (Ar), nitrogen (N)). The voltage during activation by beam irradiation is, for example, 0.5 kV to 2.0 kV, and the current is, for example, 50 mA to 200 mA. The direct bonding method is not limited to this, and surface activation methods using FAB (Fast Atom Beam) or an ion gun, atomic diffusion methods, plasma bonding methods, etc. can also be used. EXAMPLES

[0064] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples.

[0065] <Examples 1 and 2> 1-1. Fabrication of a waveguide element (coplanar line with ground) The waveguide element shown in Figures 1 and 2 was fabricated.

[0066] A silicon wafer (support substrate) with a thickness of 525 μm was prepared. A resist film was patterned on the upper surface of the silicon wafer so as to expose an area corresponding to the width of the signal electrode + the gap g × 20 of the void portion directly below the signal electrode of the coplanar electrode described later. Thereafter, the portion of the silicon wafer exposed from the resist film was dry etched by reactive ion etching to form a recess (hollow structure). The etching depth of the recess was set to the value (thickness of the low dielectric constant portion) shown in Table 1. In this way, a silicon wafer (support substrate) having a recess was prepared.

[0067] Then, a Cr film with a thickness of 50 nm and a Ni film with a thickness of 100 nm were formed by sputtering on the silicon wafer with the recesses to form a base electrode. electrolytic A copper film was formed by plating to form a ground electrode. Next, a 0.2 μm amorphous silicon film was formed on the ground electrode by sputtering. After film formation, the amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of a 10 μm square area (a 10 μm square area; the same applies below) on the surface of the amorphous silicon film was measured using an atomic force microscope, and was found to be 0.2 nm.

[0068] In addition, a quartz glass wafer (quartz glass substrate, inorganic material substrate) with a thickness of 0.5 mm was prepared, and an amorphous silicon film with a thickness of 0.2 μm was formed on the quartz glass wafer by sputtering. After the film formation, a resist was applied to the surface of the amorphous silicon film, and the portions corresponding to the recesses (non-bonded portions) of the silicon wafer were exposed by photolithography, and developed (etched) to form a resist mask. The amorphous silicon was then removed by dry etching. Next, the amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of the surface of the amorphous silicon film over 10 μm was measured using an atomic force microscope, and found to be 0.2 nm.

[0069] The amorphous silicon surface on the quartz glass wafer and the amorphous silicon surface on the ground electrode were bonded as follows. First, the quartz glass wafer and the silicon wafer were placed in a vacuum chamber and heated for 10 -6 In a vacuum of the Pa range, both bonding surfaces (the amorphous silicon surface of the quartz glass wafer and the amorphous silicon surface on the ground electrode) were irradiated with a high-speed Ar neutral atomic beam (accelerating voltage 1 kV, Ar flow rate 60 sccm) for 70 seconds. After irradiation, the quartz glass wafer and the silicon wafer were left to cool for 10 minutes, and then the bonding surfaces of the quartz glass wafer and the silicon wafer (the surface beam irradiated surfaces of the quartz glass wafer and the silicon wafer) were brought into contact and pressed at 4.90 kN for 2 minutes to bond the quartz glass wafer and the silicon wafer. That is, the quartz glass wafer and the silicon wafer were directly bonded via the amorphous silicon layer (bonding portion). After bonding, the quartz glass wafer was polished until its thickness reached the value shown in Table 1 to form a composite wafer. No defects such as peeling were observed at the bonding interface in the obtained quartz glass / ground electrode / silicon composite substrate.

[0070] Next, a resist was applied to the surface (polished surface) of the quartz glass wafer opposite the silicon wafer, and photolithography was used to pattern the area where the coplanar electrode pattern was to be formed. After that, a 50 nm thick Cr film and a 100 nm thick Ni film were formed by sputtering on the upper surface of the quartz glass wafer exposed from the resist to form a base electrode. electrolytic A copper film was formed by plating to form a coplanar electrode pattern. The length of the signal electrode in the waveguiding direction was 10 mm. The gap g between the signal electrode and the ground electrode was 13 μm. Finally, the amorphous silicon layer in the recesses (hollow structures) of the silicon wafer was removed by wet etching using buffered hydrofluoric acid (BHF). In this manner, a waveguide element was obtained that included a waveguide member including a coplanar electrode, an inorganic material substrate, and a ground electrode, and a supporting substrate having a recess.

[0071] 1-2. Calculating propagation loss In order to measure the propagation loss of the director elements, three director elements with signal electrodes having lengths of 30 mm, 40 mm, and 50 mm were fabricated in the same manner as above. Next, an RF signal generator was coupled to the input side of the waveguide member by a probe, and a probe was placed on the output side of the waveguide member to couple electromagnetic waves to an RF signal receiver. Next, a voltage was applied to the RF signal generator, causing it to transmit electromagnetic waves at the frequencies shown in Table 1. This caused the electromagnetic waves to propagate through the coplanar line (waveguide member). The RF signal receiver measured the RF power of the electromagnetic waves output from the coplanar line. From the measurement results of three waveguide elements with different signal electrode lengths, the propagation loss (dB / cm) was calculated and evaluated according to the following criteria. The results are shown in Table 1. ◎ (Excellent): Less than 0.5 dB / cm ○ (Good): 0.5 dB / cm or more and less than 1 dB / cm △ (Acceptable): 1dB / cm or more and less than 2dB / cm × (not allowed): 2dB / cm or more

[0072] <Examples 3 and 4> 2-1. Fabrication of waveguide elements (coplanar lines) The waveguide element shown in FIG. 3 was fabricated.

[0073] A silicon wafer (support substrate) having a recess was prepared in the same manner as in Example 1. However, no ground electrode was formed on the silicon wafer on which the recess was formed. The arithmetic mean roughness of the surface of the silicon wafer, 10 μm square, was measured using an atomic force microscope and found to be 0.2 nm.

[0074] In addition, a quartz glass wafer (quartz glass substrate, inorganic material substrate) having a thickness of 0.5 mm was prepared, and an amorphous silicon film patterned on the quartz glass wafer was formed in the same manner as in Example 1. After formation, the amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of the surface of the amorphous silicon film over 10 μm square was measured using an atomic force microscope, and was found to be 0.2 nm.

[0075] Thereafter, the amorphous silicon surface on the quartz glass wafer and the silicon wafer were directly bonded. The direct bonding was performed in the same manner as in Example 1. In the obtained quartz glass / silicon composite substrate, no defects such as peeling were observed at the bonding interface. The quartz glass wafer was then polished to the thicknesses shown in Table 1.

[0076] Next, a coplanar electrode pattern was formed on the surface (polished surface) of the quartz glass wafer opposite to the silicon wafer in the same manner as in Example 1. The length of the signal electrode in the waveguiding direction was 10 mm. The gap g between the signal electrode and the ground electrode was 13 μm. In this manner, a waveguide element was obtained that included a waveguide member having a coplanar electrode and an inorganic material substrate, and a supporting substrate having a recess.

[0077] 2-2. Calculating propagation loss In addition, in order to measure the propagation loss of the director element, three director elements with signal electrode lengths of 30 mm, 40 mm, and 50 mm were fabricated in the same manner as described above. Next, as in Example 1, an RF signal generator was coupled to the input side of the waveguide member by a probe, and a probe was installed on the output side of the waveguide member to couple the electromagnetic wave to an RF signal receiver, and the RF power of the electromagnetic wave output from the coplanar waveguide was measured by the RF signal receiver. The propagation loss of the director elements of Examples 3 and 4 was evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0078] <Example 5> A 525 μm thick silicon wafer (support substrate) and a 0.5 mm thick quartz glass wafer (quartz glass substrate, inorganic material substrate) were prepared, and a waveguide element was obtained comprising a coplanar electrode, a waveguide member comprising an inorganic material substrate, a polymer layer, a ground electrode, and a support substrate having a recess. First, a silicon wafer (support substrate) having a recess and a ground electrode was prepared in the same manner as in Example 1.

[0079] Next, a Teflon (registered trademark) polymer resin with a relative dielectric constant of 2.3 was spin-coated and cured to form a polymer layer in the recesses of the support substrate. Then, CMP polishing was performed to remove the polymer outside the recesses and to flatten the polymer layer on the support substrate. After CMP polishing, an amorphous silicon film was formed by sputtering. After the film formation, a resist was applied to the amorphous silicon film surface, and the parts corresponding to the recesses were exposed by photolithography, and developed (etched) to form a resist mask. Then, the amorphous silicon was removed by dry etching. Next, the amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of 10 μm on the surface of the amorphous silicon film was measured using an atomic force microscope, and it was 0.2 nm.

[0080] In addition, for a quartz glass wafer, an amorphous silicon film of 0.2 μm was formed on the wafer by sputtering. After the film formation, a resist was applied to the amorphous silicon film surface, and the portions corresponding to the recesses (non-bonded portions) of the silicon wafer were exposed and etched by photolithography to form a resist mask. After that, the amorphous silicon was removed by dry etching.

[0081] Thereafter, the amorphous silicon surface on the quartz glass wafer and the silicon wafer were directly bonded. The direct bonding was performed in the same manner as in Example 1. In the obtained quartz glass / silicon composite substrate, no defects such as peeling were observed at the bonding interface. The quartz glass wafer was then polished to the thicknesses shown in Table 1.

[0082] Next, a coplanar electrode pattern was formed on the surface (polished surface) of the quartz glass wafer opposite to the silicon wafer in the same manner as in Example 1. The length of the signal electrode in the waveguiding direction was 10 mm. The gap g between the signal electrode and the ground electrode was 13 μm. In this manner, a waveguide element was obtained that included a waveguide member including a coplanar electrode and an inorganic material substrate, a polymer layer, a ground electrode, and a support substrate having a recess. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0083] <Example 6> A waveguide element was fabricated in the same manner as in Example 1, except that the etching depth of the recess was changed to change the thickness of the cavity to the value shown in Table 1. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0084] <Example 7> A waveguide element was fabricated in the same manner as in Example 1, except that the quartz glass wafer used as the inorganic material substrate was changed to a single crystal silicon wafer, and that the etching depth of the recess was changed to change the thickness of the cavity to the value shown in Table 1.

[0085] <Example 8> A waveguide element was fabricated in the same manner as in Example 1, except that the quartz glass wafer used as the inorganic material substrate was changed to a sapphire wafer, and that the etching depth of the recess was changed to change the thickness of the cavity to the value shown in Table 1. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0086] <Example 9> A waveguide element was fabricated in the same manner as in Example 1, except that the quartz glass wafer used as the inorganic material substrate was changed to a polycrystalline AlN wafer, and that the etching depth of the recess was changed to change the thickness of the cavity to the value shown in Table 1. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0087] <Example 10> The waveguide element shown in Figures 4 and 5 was fabricated. A 525 μm thick silicon wafer (support substrate) and a 0.5 mm thick quartz glass wafer (quartz glass substrate, inorganic material substrate) were prepared, and a waveguide element was obtained comprising a coplanar electrode, a waveguide member comprising an inorganic material substrate, a polymer layer, a ground electrode, and a support substrate having no recess.

[0088] First, a silicon wafer (support substrate) with a thickness of 525 μm was prepared. Then, a Cr film with a thickness of 50 nm and a Ni film with a thickness of 100 nm were formed on the silicon wafer by sputtering to form a base electrode. electrolytic A copper film was formed by plating to form a ground electrode.

[0089] Next, a thermosetting Teflon (registered trademark) film with a relative dielectric constant of 2.3 was adhered and cured to form a polymer layer with a thickness of 100 μm on the ground electrode. Furthermore, an amorphous silicon film was formed by sputtering. After the film formation, a resist was applied to the amorphous silicon film surface, and an area equivalent to the width of the signal electrode directly below the coplanar electrode + the gap g × 20 was exposed by photolithography, and developed (etched) to form a resist mask. Then, the amorphous silicon was removed by dry etching. Next, the amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of □10 μm on the surface of the amorphous silicon film was measured using an atomic force microscope, and it was 0.2 nm.

[0090] In addition, for a quartz glass wafer, a 0.2 μm amorphous silicon film was formed on the wafer by sputtering. After the film was formed, a resist was applied to the amorphous silicon film surface, and a resist mask was formed by exposing and etching an area equivalent to the width of the signal electrode directly below the coplanar electrode + the gap g × 20 by photolithography. The amorphous silicon was then removed by dry etching. The amorphous silicon film was polished and flattened. Here, the arithmetic mean roughness of the surface of the amorphous silicon film over a 10 μm square was measured using an atomic force microscope, and was found to be 0.2 nm.

[0091] Thereafter, the amorphous silicon surface on the quartz glass wafer and the amorphous silicon surface on the polymer layer were directly bonded to each other. The direct bonding was performed in the same manner as in Example 1. In the obtained quartz glass / silicon composite substrate, no defects such as peeling were observed at the bonding interface. The quartz glass wafer was then polished to the thicknesses shown in Table 1.

[0092] Next, a coplanar electrode pattern was formed on the surface (polished surface) of the quartz glass wafer opposite to the silicon wafer in the same manner as in Example 1. The length of the signal electrode in the waveguiding direction was 10 mm. The gap g between the signal electrode and the ground electrode was 13 μm. In this manner, a waveguide element was obtained that included a coplanar electrode, a waveguide member including an inorganic material substrate, a polymer layer, a ground electrode, and a support substrate that does not have a recess. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0093] <Example 11> Except for changing the thickness of the polished quartz glass wafer (quartz glass substrate, inorganic material substrate) to 10 μm, a waveguide element was obtained in the same manner as in Example 1. The propagation loss of the obtained waveguide element was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0094] <Comparative Examples 1 and 2> A waveguide element was fabricated in the same manner as in Example 1, except that no recesses were formed in the silicon wafer (support substrate) and that the thickness of the polished quartz glass wafer was changed to the value shown in Table 1. For the obtained waveguide element, the propagation loss was calculated and evaluated in the same manner as in Example 1. The results are shown in Table 1.

[0095] [Table 1]

[0096] As is clear from Table 1, by providing a low dielectric constant portion (particularly a cavity) having a dielectric constant smaller than that of the inorganic material substrate at the bottom of the inorganic material substrate, it is possible to ensure low propagation loss over a wide frequency range in the high frequency region exceeding 30 GHz, thereby ensuring excellent low propagation loss performance. [Industrial Applicability]

[0097] The waveguide element according to the embodiment of the present invention can be used in a wide range of fields such as a waveguide, next-generation high-speed communication, a sensor, laser processing, and solar power generation, and can be particularly suitably used as a waveguide for millimeter waves to terahertz waves. Such a waveguide element can be used, for example, in an antenna, a bandpass filter, a coupler, a delay line (phase shifter), or an isolator. [Explanation of symbols]

[0098] 1 Inorganic material substrate 2 Coplanar electrode 3 Ground electrode 10 Waveguide member 100 Waveguide element

Claims

1. A waveguide member including an inorganic material substrate and a coplanar electrode provided on an upper portion of the inorganic material substrate, the waveguide member being capable of guiding an electromagnetic wave having a frequency of 30 GHz or more and 20 THz or less; a support substrate provided under the inorganic material substrate and supporting the waveguide member; A waveguide element comprising: a low dielectric constant portion provided in a lower portion of the inorganic material substrate, the low dielectric constant portion having a dielectric constant smaller than that of the inorganic material substrate.

2. The waveguide element according to claim 1 , wherein the thickness t of the inorganic material substrate satisfies the following formula (1): [0010] (In the formula, t represents the thickness of the inorganic material substrate, λ represents the wavelength of the electromagnetic wave guided by the waveguide member, ε represents the relative dielectric constant of the inorganic material substrate, and a represents the value 2.)

3. the support substrate has a recess; a cavity is defined by a lower surface of the inorganic material substrate and a recess of the support substrate; The waveguide element according to claim 1 , wherein the cavity functions as the low dielectric constant portion.

4. the coplanar electrode includes a signal electrode extending in a predetermined direction and a ground electrode positioned at a distance from the signal electrode in a direction intersecting the predetermined direction; 4. The waveguide element according to claim 3, wherein, when a dimension of a gap between the signal electrode and the ground electrode in a direction intersecting the predetermined direction is g, a dimension of the cavity in a thickness direction of the inorganic material substrate is g or more.

5. 3. The waveguide element of claim 1, further comprising a ground electrode located between the inorganic material substrate and the supporting substrate.

6. 3. The waveguide element according to claim 1, wherein the relative dielectric constant ε and the dielectric loss tangent tan δ of the inorganic material substrate at 300 GHz are 3.5 to 12 and 0.003 or less, respectively.

7. 7. The waveguide element of claim 6, wherein the inorganic material substrate is a quartz glass substrate.

Citation Information

Patent Citations

  • Multilayer substrate

    JP2000277661A

  • Microwave transmission line

    JP2004023192A

  • Mode converter and manufacturing method of mode converter

    JP2018023030A

  • Impedance-matched conductive structures for highly efficient RF circuits.

    JP2021509767A