Adhesion improver and coating composition
Patent Information
- Application Number
- JP2020176063
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-20
- Publication Date
- 2024-09-27
- Estimated Expiration
- 2040-10-20
AI Technical Summary
【0009】 本発明のコーティング組成物用密着性向上剤は、基材に対するコーティング膜の密着性を大幅に向上できる。
Smart Images

Figure 0007557198000002 
Figure 0007557198000001
Abstract
Description
[Technical field]
[0001] The present invention relates to an adhesion improver for a coating composition and a coating composition containing the same. [Background technology]
[0002] As an adhesion imparting agent, a solution of a high molecular weight block polymer (containing 20 to 30% by weight of polyamide) is known (Non-Patent Documents 1 and 2). [Prior art documents] [Non-patent literature]
[0003] [Non-Patent Document 1] Safety Data Sheet for BYK-4500 (Updated July 9, 2018, BYK Japan Co., Ltd., available for download at https: / / www.byk.com / ja / products / additives-by-name / byk-4500) [Non-Patent Document 2] BYK-4500 Technical Data Sheet (issued December 2017, BYK Japan Co., Ltd., available for download at https: / / www.byk.com / ja / products / additives-by-name / byk-4500) Summary of the Invention [Problem to be solved by the invention]
[0004] Conventional adhesion improvers have a problem in that the adhesion of the coating film to the substrate is insufficient. An object of the present invention is to provide an adhesion improver for a coating composition that can improve the adhesion of the coating film to the substrate.
[0005] The characteristic of the adhesion improver for a coating composition of the present invention is that it is an additive for improving the adhesion of a coating film to a substrate, The gist of the present invention is that it contains a polyoxyalkylene compound (Y) represented by formula (1).
[0006] RN{-(AO) n H}2(1)
[0007] where R is an alkyl or alkenyl group, AO is an oxyalkylene group having 2 to 4 carbon atoms, and oxypropylene and It includes a mixture with oxyethylene, the content ratio (mol %) of oxyethylene is 60 to 90 based on the total number of moles of oxyalkylene, oxyethylene is bonded to the terminal part away from the nitrogen atom N, the bonding form includes a block shape, N is a nitrogen atom, H is a hydrogen atom, and n is an integer of 16 to 100.
[0008] The coating composition of the present invention is characterized in that it comprises a coating agent and the above-mentioned adhesion improver, and the content of this adhesion improver is 0.2 to 2 wt % based on the weight of the coating agent. Effect of the Invention
[0009] The adhesion improver for a coating composition of the present invention can significantly improve the adhesion of a coating film to a substrate.
[0010] Since the coating composition of the present invention contains the above-mentioned adhesion improver, it can easily form a coating film having excellent adhesion to a substrate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Of the alkyl group, alkenyl group or aryl group (R), the alkyl group includes an alkyl group having 4 to 18 carbon atoms, such as n-butyl, cyclobutyl, n-pentyl, cyclopentyl, n-hexyl, cyclohexyl, n-heptyl, methylcyclohexyl, n-octyl, 2-ethylhexyl, n-nonyl, trimethylcyclohexyl, n-decyl, n-undecyl, n-dodecyl, n-tridecyl, isotridecyl, n-tetradecyl, n-pentadecyl, nonylcyclohexyl, n-hexadecyl, n-heptadecyl, n-octadecyl and isooctadecyl.
[0012] Furthermore, the alkenyl group includes alkenyl groups having 4 to 18 carbon atoms, such as n-butenyl, n-pentenyl, n-hexenyl, n-heptenyl, n-octenyl, 2-ethylhexenyl, n-nonenyl, n-decenyl, n-undecenyl, n-dodecenyl, n-tridecenyl, isotridecenyl, n-tetradecenyl, n-pentadecenyl, n-hexadecenyl, n-heptadecenyl, n-octadecenyl, and isooctadecenyl.
[0013] The aryl group includes aryl groups having 6 to 15 carbon atoms, such as phenyl, tolyl, benzyl, xylyl, nonylphenyl, and naphthyl.
[0014] Among these R groups, an alkyl group is preferred.
[0015] Examples of the oxyalkylene group (AO) having 2 to 4 carbon atoms include oxyethylene, oxypropylene, oxybutylene, and mixtures thereof. Among these, from the viewpoint of adhesion, when R is an alkyl group having 12 to 18 carbon atoms, oxyethylene alone is preferred, and when R is an alkyl group, alkenyl group, or aryl group having 4 to 11 carbon atoms, a mixture of oxyethylene with oxypropylene and / or oxybutylene is preferred.
[0016] When a mixture of oxypropylene and / or oxybutylene with oxyethylene is contained, the content ratio (mol%) of oxyethylene is preferably 50 to 90, more preferably 60 to 90, and particularly preferably 60 to 80, based on the total number of moles of oxyalkylene. In this case, it is preferable that oxypropylene and / or oxybutylene is located at the nitrogen atom N. That is, it is preferable that oxyethylene is bonded to the terminal part remote from the nitrogen atom N. When a plurality of types of oxyalkylene groups are contained, the bonding form may be any of block, random, and a mixture thereof, but it is preferable that at least block is included.
[0017] n is preferably an integer of 16 to 100, more preferably an integer of 18 to 90, particularly preferably an integer of 20 to 70, next preferably an integer of 22 to 60, and most preferably an integer of 25 to 50. Within this range, the adhesion will be further improved.
[0018] The polyoxyalkylene compound (Y) represented by formula (1) can be produced by a chemical reaction between an amine (primary amine) having any one of an alkyl group, an alkenyl group, a cycloalkyl group, and an aryl group and an alkylene oxide having 2 to 4 carbon atoms.
[0019] In addition to the polyoxyalkylene compound (Y), the adhesion improver of the present invention may contain other additives (such as a viscosity modifier, an antifoaming agent, a wetting agent, and a dispersing agent) if necessary.
[0020] Examples of the viscosity modifier include SN Thickener 601 and 612 (manufactured by San Nopco Ltd.), etc., examples of the defoamer include SN Deformer 180, 184, and 320 (manufactured by San Nopco Ltd.), etc., examples of the wetting agent include SN Wet 125 and 126 (manufactured by San Nopco Ltd.), etc., and examples of the dispersant include Nopco Pers 6100 and 6150, SN Dispersant 2060 and 5041 (manufactured by San Nopco Ltd.). When additives are contained, the content of these is preferably 0.1 to 100% by weight based on the weight of the polyoxyalkylene compound (Y).
[0021] The adhesion improver of the present invention can be applied to aqueous and non-aqueous coating compositions as an additive for improving the adhesion of a coating film to a substrate, and is particularly suitable as an adhesion improver for baked-on paints.
[0022] The adhesion improver of the present invention may be added to any of the paint production processes, or may be added to the finished paint (i.e., coating agent). In either case, it can exhibit excellent adhesion.
[0023] The content (wt %) of the adhesion improver of the present invention is preferably 0.2 to 2, more preferably 0.5 to 1.7, and particularly preferably 0.7 to 1, based on the weight of the coating agent.
[0024] The coating composition containing the adhesion improver of the present invention can be applied (coated) to a substrate by a conventional method, and coating methods such as brush coating, roller coating, bell coating, air spray coating, airless coating, roll coater coating, and flow coater coating can be applied. The drying method may be ambient drying or baking drying, but baking drying is effective. Baking drying can be performed by using an electric hot air dryer, an indirect hot air oven, a direct hot air oven, a far-infrared oven, or the like, and maintaining the temperature at about 120 to 260°C for several tens of seconds to 30 minutes. EXAMPLES
[0025] <Examples 1 to 4> The following polyoxyalkylene compounds (Y1) to (Y4) were prepared by a normal polyalkylene oxide synthesis method, and used as adhesion improvers for coating compositions of the present invention (Examples 1 to 4, respectively). In addition, / indicates a random pattern, and · indicates a block pattern.
[0026] (Y1) n-Butylamine 20 moles of ethylene oxide / 16 moles of propylene oxide / 20 moles of ethylene oxide adduct (Y2) n-Octadecylamine 20 moles of ethylene oxide / 10 moles of propylene oxide / 20 moles of ethylene oxide adduct (Y3) n-Decylamine propylene oxide (40 moles)-ethylene oxide (60 moles) adduct (Y4) n-Heptadecylamine ethylene oxide 39 moles / propylene oxide 12 moles / ethylene oxide 9 moles adduct
[0027] <Comparative Example> BYK-4500 (BYK Japan KK) described in Non-Patent Documents 1 and 2 was used as an adhesion improver (H) for comparison.
[0028] <Adhesion evaluation> 1. Preparation of emulsion-based paint The raw material composition (grinding process, let-down process) shown in Table 1 was ground using a benchtop sand mill equipped with a disc-shaped blade (Kanpe Sand Mill, Kanpe Home Paint Co., Ltd.), and then let-down was performed using a mixer equipped with an anchor-shaped blade (Tokyo Rikakikai Co., Ltd., MAZELLA ZZ-1100) to prepare an emulsion-based paint.
[0029] [Table 1] Note 1: Dispersant (San Nopco Ltd., "Nopcol" is a registered trademark of the company.) Note 2: Thickener (San Nopco Ltd.) Note 3: Calcium carbonate (Taiyo Kagaku Co., Ltd., "Callite" is a registered trademark of Shiraishi Kogyo Co., Ltd.) Note 4: Titanium dioxide (Ishihara Sangyo Kaisha, Ltd., "Tipaque" is a registered trademark of the company.) Note 5: Defoamer (San Nopco Ltd.) Note 6: Acrylic emulsion (Japan Coating Resin Co., Ltd.)
[0030] 2. Preparation of emulsion paint for evaluation 99 parts of the emulsion base paint and 1 part of either the adhesion improver (Y1) to (Y4) or the comparative adhesion improver (H) were mixed and stirred at 25°C, 3000 rpm for 5 minutes in an Excel Auto Homogenizer (Nihon Seiki Co., Ltd., Model ED) equipped with a Colles-type blade to obtain emulsion paints (Y1) to (Y4) and (H) for evaluation. Also, an emulsion paint for evaluation (blank) was obtained in the same manner as above, except that no adhesion promoter was added.
[0031] 3. Preparation of Painted Specimens for Evaluation The emulsion paint for evaluation was applied to a 300 mm x 100 mm x 0.8 mm stainless steel plate (SUS304) using an air spray paint machine so that the coating would be 5 mm wet over an area of 100 mm x 100 mm, and then the coating was allowed to level for 15 seconds, and then dried at 140°C for 30 minutes, and then dried at 25°C for one day to prepare coating pieces for evaluation (Y1) to (Y4), (H), and (blank).
[0032] 4. Adhesion 1 The appearance of the coated evaluation pieces was visually observed and adhesion 1 was evaluated according to the following criteria. ○: No peeling or swelling was observed ×: No peeling was observed, but swelling was observed. ××: Peeling and swelling were observed.
[0033] 5. Adhesion 2 A cross-cut test was conducted in three locations on the evaluation painted specimen where no peeling or blistering was observed, in accordance with JIS K5600-5-6:1999 "General test methods for paints - Part 5: Mechanical properties of coatings - Section 6: Adhesion (cross-cut method)" {Cross-cut test compliant cutter NT cutter eL500 (NT Corporation), mtv cross-cut plate (1mm intervals, 100 squares test, All-Good Corporation), cross-cut test / cross-cut test compliant cellophane tape (width 24mm, adhesive strength 4.01N / 10mm, Nichiban Corporation, "Cellophane Tape" is a registered trademark of the company)}. The average value of the three classifications was calculated, and this was regarded as adhesion 2.
[0034] [Table 2]
[0035] The adhesion improver for a coating composition of the present invention was superior in adhesion of the coating film to the substrate as compared with the comparative adhesion improver.
Claims
1. An additive for improving adhesion of a coating film to a substrate, 1. An adhesion improver for a coating composition, comprising a polyoxyalkylene compound (Y) represented by formula (1): R-N{-(AO) n H} 2 (1) In the formula, R is an alkyl or alkenyl group, AO is an oxyalkylene group having 2 to 4 carbon atoms, including a mixture of oxypropylene and oxyethylene, the oxyethylene content (mol %) is 60 to 90 based on the total number of moles of oxyalkylene, oxyethylene is bonded to an end portion away from the nitrogen atom N, the bonding form includes a block form, N is a nitrogen atom, H is a hydrogen atom, and n is an integer of 16 to 100.
2. A coating composition comprising a coating agent and the adhesion improver according to claim 1, wherein the content of the adhesion improver is 0.2 to 2% by weight based on the weight of the coating agent.
Citation Information
Patent Citations
Aqueous polyolefin resin composition
JP1994256592A
Water-based polyolefin composition and production thereof
JP1995109359A
Dispersing resin composition, and paint composition, ink composition, adhesive composition, and primer composition containing same
WO2010018863A1