Adhesive tape, endless belt, and method for manufacturing adhesive tape
The adhesive tape with a PTFE base layer and PFA surface layer addresses the wear and adhesion issues of conventional tapes by providing enhanced abrasion resistance and mold releasability, ensuring effective lamination processes.
Patent Information
- Application Number
- JP2020055423
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-03-26
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2040-03-26
AI Technical Summary
Conventional release adhesive tapes with a PTFE resin layer suffer from surface wear and poor mold releasability due to orientation along the stretching direction, leading to adhesion of molten resin and surface fluffing during lamination.
An adhesive tape with a base layer of polytetrafluoroethylene (PTFE) and a surface layer of perfluoroalkoxyalkane (PFA) is developed, which provides excellent abrasion resistance and mold releasability by eliminating orientation and enhancing tear strength.
The adhesive tape exhibits superior mold releasability and abrasion resistance, preventing adhesion and fluffing of molten resin, thereby extending the lifespan of the adhesive tape and endless belt applications.
Smart Images

Figure 0007560091000001 
Figure 0007560091000002 
Figure 0007560091000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an adhesive tape, an endless belt, and a method for producing an adhesive tape. [Background technology]
[0002] In a lamination process in which paper or a plastic film is to be laminated, there is a problem that molten resin such as polyethylene or polypropylene adheres to the lamination roll. Conventionally, a release adhesive tape has been used to prevent the molten resin from adhering to the lamination roll. The release adhesive tape is, for example, directly attached to the lamination roll or processed into an endless belt and then hung on the lamination roll.
[0003] As a release adhesive tape, for example, a rolled polytetrafluoroethylene (PTFE) base tape having a rolled PTFE resin layer and an adhesive layer is used. The adhesive tape with the surface of the PTFE resin layer exposed has a problem that the surface is worn away by repeated use for release purposes. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2004-083706 A Summary of the Invention [Problem to be solved by the invention]
[0005] An object of the present invention is to provide an adhesive tape having excellent releasability and abrasion resistance, an endless belt provided with the adhesive tape, and a method for producing the adhesive tape. [Means for solving the problem]
[0006] According to a first aspect of the present invention, there is provided a substrate layer including polytetrafluoroethylene and a perfluoroalkoxyalkane-based film formed on at least a portion of a main surface of the substrate layer. Consists of An adhesive tape is provided that includes a surface layer and an adhesive layer formed on the surface opposite to the main surface of a base layer.
[0007] According to a second aspect of the present invention, there is provided an endless belt comprising the adhesive tape according to the first aspect.
[0008] According to a third aspect of the present invention, a method for producing a PTFE sheet having a coating film is provided by preparing an unsintered PTFE sheet, applying a dispersion containing PFA particles to at least one surface of the PTFE sheet, sintering the PTFE sheet having the coating film to obtain a PTFE film, and stretching the PTFE film after sintering to obtain a base layer containing PTFE and a PTFE film formed on a main surface of the base layer, Consists of perfluoroalkoxyalkane and forming an adhesive layer on a surface opposite to the main surface of the base layer. Effect of the Invention
[0009] According to the present invention, it is possible to provide an adhesive tape having excellent releasability and abrasion resistance, an endless belt provided with this adhesive tape, and a method for producing the adhesive tape. [Brief description of the drawings]
[0010] [Figure 1] 1 is a cross-sectional view illustrating an example of a pressure-sensitive adhesive tape according to an embodiment. [Diagram 2] FIG. 1 is a cross-sectional view illustrating an example of an endless belt according to an embodiment. [Diagram 3] FIG. 4 is a cross-sectional view illustrating another example of an endless belt according to an embodiment of the present invention. [Figure 4] FIG. 2 is a side view illustrating a schematic view of a part of the laminating device. [Diagram 5] FIG. 2 is a top view illustrating a schematic view of a portion of the lamination apparatus. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Conventionally, PTFE substrates are manufactured, for example, by the following method. First, fine powder containing PTFE resin is prepared and mixed with an auxiliary to obtain a mixture. The mixture is filled into a mold and pressure molded to obtain a preform. This is extruded into a rod shape, rolled, and then the auxiliary is removed to obtain an unsintered PTFE sheet. The unsintered PTFE sheet is sintered and then stretched to obtain a rolled PTFE substrate.
[0012] The rolled PTFE substrate has orientation along the stretching direction due to, for example, squeezing when extruding a preform or rolling, and therefore has a problem in that the rolled PTFE substrate is easily torn along the stretching direction.
[0013] When a release tape with an exposed surface of a PTFE rolled substrate is used for lamination release, the molten resin that protrudes from the paper or the like to be laminated adheres to the surface of the PTFE rolled substrate during lamination. When the laminated object is then sent out by the rotation of the lamination roll, a part of the surface of the PTFE rolled substrate may be torn off along the stretching direction when the laminated object is peeled off from the release tape, causing the surface to fluff. This is because the release tape (PTFE rolled substrate) has an orientation along the stretching direction as described above. As a result, this fluff may be mixed between the laminated object that flows next and the molten resin, which is undesirable.
[0014] In contrast, the adhesive tape according to the embodiment has a surface layer containing perfluoroalkoxyalkane (PFA) on the main surface of a base layer containing polytetrafluoroethylene (PTFE). The adhesive tape has a base layer containing PTFE, and therefore has sufficient tear strength. In addition, PFA is a fluororesin with melt flowability. Therefore, the surface layer containing PFA does not have the orientation that the PTFE base material has. Therefore, the surface of the surface layer containing PFA has excellent abrasion resistance. In other words, since the surface layer containing PFA does not have an orientation in a specific direction, when used for release purposes, even if the surface layer and the laminated object are adhered and peeled off, fluff derived from the surface layer is unlikely to occur. Furthermore, the surface of the surface layer containing PFA has excellent releasability compared to the surface of the PTFE base layer.
[0015] Therefore, the pressure-sensitive adhesive tape according to the embodiment has excellent releasability and abrasion resistance, and when used as an endless belt, can achieve excellent life characteristics.
[0016] <Adhesive tape> Hereinafter, a pressure-sensitive adhesive tape according to an embodiment will be described with reference to the drawings. FIG. 1 is a cross-sectional view that illustrates an example of a pressure-sensitive adhesive tape.
[0017] The adhesive tape 1 includes a base layer 2, a surface layer 3 formed on the main surface of the base layer 2, and an adhesive layer 4 formed on the surface opposite to the main surface of the base layer 2. Ceramic particles such as silicon dioxide may be present at the interface between the base layer 2 and the surface layer 3 and / or the interface between the base layer 2 and the adhesive layer 4.
[0018] The base layer 2 is, for example, a film containing polytetrafluoroethylene. The base layer may contain a core material (woven fabric) such as glass cloth. However, if the base layer contains a core material, this is not preferable because the core material may become exposed when the surface layer and base layer become worn, and the molten resin may adhere to the core material during lamination. Alternatively, when the adhesive tape is attached to a laminating roll, the tracking ability may deteriorate and the tape may easily peel off. In order to avoid these problems, it is preferable that the base layer 2 does not contain a core material. The base layer may be made of polytetrafluoroethylene. In other words, the base layer may be a PTFE film. . basis The material layer may have an orientation along the stretch direction. When the base material layer has an orientation along the stretch direction, the tensile strength in the direction parallel to the orientation is high.
[0019] The thickness of the base layer is, for example, in the range of 10 μm to 500 μm, and preferably in the range of 20 μm to 200 μm. If the base layer is too thick, the rigidity of the adhesive tape becomes too high, and the flexibility of the adhesive tape is lost, which is not preferable. In this case, for example, when used as an endless belt as described later, the belt may not be curved along the shape of the lamination roll. Alternatively, when the end of the object to be laminated (paper, film, etc.) passes over the adhesive tape, there are parts where the object to be laminated passes over the adhesive tape and parts where it does not pass over, so there is a disadvantage that a step mark due to the thickness of the base layer is formed on the film after lamination. If the base layer is too thin, the tensile strength is insufficient and the adhesive tape is easily broken, which is not preferable. When the adhesive tape is directly attached to the lamination roll, the base layer may be relatively thin. However, it is relatively difficult to manufacture an adhesive tape having a surface layer containing PFA on an excessively thin base layer.
[0020] The pressure-sensitive adhesive tape has a tensile strength in a direction parallel to the main surface of the base layer, for example, in the range of 30 MPa to 250 MPa, and preferably in the range of 50 MPa to 250 MPa. The direction parallel to the main surface of the base layer refers to, for example, the direction in which the base layer is uniaxially stretched (stretching direction). If the tensile strength is within this range, the pressure-sensitive adhesive tape can withstand long-term use when used as an endless belt. The tensile strength of the pressure-sensitive adhesive tape is largely dependent on, for example, the tensile strength of the base layer.
[0021] The tensile strength of the adhesive tape can be measured in accordance with JIS K 7161:1994.
[0022] The surface layer is provided on at least a part of the main surface of the base layer. The surface layer contains PFA. The melting point of PFA is 310°C, and it does not melt even at temperatures during lamination, for example, in a temperature environment of up to 300°C. The surface of the surface layer containing PFA is excellent in release properties in addition to wear resistance. Therefore, when this surface layer is used as a release surface for release applications such as lamination, the adhesive tape can achieve excellent release properties and wear resistance. The surface layer can contain other melt-flowable resins.
[0023] The method of forming the surface layer will be described later, but it is not preferable to use a PTFE resin that does not have melt flowability as the surface layer. In other words, it is preferable that the surface layer does not contain PTFE. If a surface layer containing PTFE is formed, such a surface layer is formed from a material containing, for example, fine powder of PTFE. The surface layer thus formed may have an orientation along the stretching direction as described above. Therefore, when an adhesive tape having this surface layer is used for lamination release, it has poor abrasion resistance.
[0024] The thickness of the surface layer is, for example, in the range of 0.1 μm to 50 μm, and preferably in the range of 1 μm to 10 μm.
[0025] The ratio of the thickness of the base layer to the total thickness of the base layer and the surface layer is, for example, within a range of 85% to 99%. The ratio of the thickness of the surface layer to the total thickness of the base layer and the surface layer is, for example, within a range of 15% to 1%. By setting the ratio of the base layer and the surface layer within the above range, an adhesive tape having sufficient tear strength due to the base layer and excellent abrasion resistance due to the surface layer can be obtained.
[0026] The adhesive layer 4 is a layer having adhesiveness. The adhesive layer contains, for example, an adhesive and a curing agent. The adhesive layer is formed on at least a part of the surface opposite to the main surface of the base layer.
[0027] The adhesive may be, for example, at least one selected from a natural rubber adhesive, a silicone adhesive, and an acrylic adhesive. Among these, from the viewpoint of heat resistance, it is preferable that the adhesive contains a silicone adhesive and / or an acrylic adhesive.
[0028] Examples of silicone-based adhesives include peroxide-curing adhesives and addition-curing adhesives. When a peroxide-curing adhesive is used as the adhesive, at least one selected from the group consisting of benzoyl peroxide, dicumyl peroxide, p-chlorobenzoyl peroxide, 2,4-dichlorobenzoyl peroxide, and di-t-butyl peroxide can be used as the curing agent. When an addition-curing adhesive is used as the adhesive, platinum can be used as the curing agent.
[0029] The thickness of the adhesive layer is, for example, in the range of 10 μm to 100 μm, and preferably in the range of 20 μm to 60 μm.
[0030] The thickness of the adhesive tape is, for example, in the range of 20 μm to 500 μm, and preferably in the range of 30 μm to 150 μm. If the adhesive tape is too thick, the film after lamination tends to have a step mark due to the thickness of the adhesive tape. Also, if the adhesive tape is too thin, the tensile strength tends to decrease.
[0031] The adhesive tape may have a release paper on the adhesive layer.
[0032] The thickness of each layer can be measured, for example, by observing the cross section of the adhesive tape with a scanning electron microscope (SEM). When measuring, the thickness is measured at five random points in the SEM image, and the average value is calculated.
[0033] <Endless belt> The endless belt according to the embodiment includes the adhesive tape according to the embodiment. 2 is a cross-sectional view showing an example of an endless belt according to an embodiment. The endless belt is formed, for example, by preparing two sheets of the adhesive tape according to the embodiment, bonding the two sheets together so that their adhesive layers are adhered to each other, and overlapping the adhesive layer present at one end on the surface layer present at the other end.
[0034] The endless belt 10 includes an adhesive tape 1A and an adhesive tape 1B laminated thereon. The adhesive tape 1A and the adhesive tape 1B each have the same configuration as the adhesive tape 1 described with reference to FIG. 1. That is, the adhesive tape 1A includes a base layer 2A, a surface layer 3A formed on the main surface of the base layer 2A, and an adhesive layer 4A formed on the surface opposite to the main surface of the base layer 2A. The adhesive tape 1B includes a base layer 2B, a surface layer 3B formed on the main surface of the base layer 2B, and an adhesive layer 4B formed on the surface opposite to the main surface of the base layer 2B. Here, the adhesive layer 4A of the adhesive tape 1A and the adhesive layer 4B of the adhesive tape 1B are placed face to face with each other and bonded together so that they are in contact with each other, and one end of each tape is joined to the other end (not shown), thereby forming the endless belt 10.
[0035] FIG. 3 shows an endless belt formed by bonding together an adhesive tape 1A according to the embodiment and an adhesive tape 1C without a surface layer so that their adhesive layers are in contact with each other. As shown in FIG. 3, in an endless belt formed by bonding together two adhesive tapes, one of the adhesive tapes may not have a surface layer. The adhesive tape 1C includes a base layer 2C and an adhesive layer 4C laminated thereon, and does not have a surface layer. When this endless belt 10 is used for lamination release, the endless belt 10 can exhibit excellent releasability and abrasion resistance by using the surface layer 3A as a release surface.
[0036] <Method of manufacturing adhesive tape> An example of a method for producing the pressure-sensitive adhesive tape according to the embodiment will be described. First, fine powder containing PTFE resin is prepared and mixed with auxiliary agents to obtain a mixture. The mixture is filled into a mold and pressure molded to obtain a preform. This is extruded into a sheet, which is then rolled, and the auxiliary agents are then removed to obtain an unsintered PTFE sheet.
[0037] Although molding powder may be used instead of fine powder, when tensile strength is required for the adhesive tape, it is preferable to use fine powder as a raw material. In molding using fine powder, since processes for strengthening the orientation in the stretching direction, such as an extrusion process and a rolling process, are involved, a structure with strong orientation in the stretching direction is obtained, and high tensile strength can be achieved.
[0038] The average particle size of the fine powder is, for example, in the range of 100 μm to 1000 μm.
[0039] Next, an aqueous dispersion in which PFA particles are dispersed is prepared. A dispersant such as a surfactant and other additives may be added to the aqueous dispersion as appropriate. The solvent of the dispersion does not need to be water, and an appropriate organic solvent may be used. This dispersion is applied to at least one side of the previously prepared unsintered PTFE sheet to form a coating film, thereby obtaining a PTFE sheet having a coating film. Next, this PTFE sheet is sintered to obtain a PTFE film. The sintering is performed, for example, at a temperature of 327°C to 420°C for 5 seconds to 600 seconds.
[0040] The PTFE film after baking is stretched uniaxially to obtain a laminate in which a surface layer containing PFA is formed on the main surface of the PTFE film as the base layer. In this way, the tensile strength in the stretching direction is improved by stretching the sheet after baking uniaxially. When high tensile strength is not required for the adhesive tape, this stretching process can be omitted. In addition, as described later, when high tensile strength is not required for the adhesive tape, it is the case that the adhesive tape is directly attached to the lamination roll without being processed into an endless belt. When the stretching process is omitted, there is an advantage that stress is less likely to remain in the base layer and the surface layer.
[0041] Instead of forming a surface layer using a dispersion of PFA particles, a laminate may be obtained by overlapping a PFA film on an unsintered PTFE sheet and integrating them by pressing with a hot roll or the like.
[0042] In the substrate layer contained in the obtained laminate, an adhesive layer is formed on the side where the surface layer is not provided. Alternatively, when the surface layer is formed on both sides of the substrate layer, an adhesive layer is formed on either one of the two sides. The adhesive layer can be formed by a known method. Here, the surface of the substrate layer or the surface of the surface layer may be optionally subjected to a surface modification treatment. For example, the surface modification treatment can be performed by applying a dispersion liquid containing fluororesin particles and silicon dioxide particles onto the substrate layer and drying it. The surface modification treatment is not limited to a chemical treatment, and may be a physical treatment.
[0043] The adhesive tape can be produced in the manner described above. Since the adhesive layer is provided on only one side of the adhesive tape, the adhesive tape can be wound into a roll after the adhesive layer is formed, for example.
[0044] <Use of adhesive tapes and endless belts> Next, an example of a case where the endless belt or adhesive tape according to the embodiment is used in a laminating process will be described. Fig. 4 is a side view that shows a schematic view of a part of a laminating device. Fig. 5 is a top view that shows a schematic view of a part of the laminating device.
[0045] 4 shows a laminating unit 20 provided in a single laminating device (not shown). The laminating unit 20 includes laminating rolls 21 and 22, a cooling roll 23, and a roll 25. The laminating unit 20 further includes a die 24. The die 24 can supply molten resin 31 between the cooling roll 23 and the laminating roll 22. The endless belt 10 according to the embodiment is hung across the laminating rolls 21 and 22.
[0046] In order to drive the endless belt around two laminating rolls, it is necessary to apply a certain tension to the endless belt, for example, by increasing the distance between the two laminating rolls. If the tension is insufficient, the endless belt may meander or wrinkle due to the driving of the rolls. This tension is applied along the stretching direction when the PTFE base layer is produced, and the endless belt according to the embodiment has excellent tensile strength in the stretching direction because it contains the PTFE base layer. Therefore, when the endless belt is driven across two rolls, sufficient tension can be applied to it. In other words, the endless belt can withstand a relatively high tension. As a result, the endless belt can rotate appropriately with the driving of the rolls.
[0047] On the other hand, if an endless belt is made of an adhesive tape having only a surface layer containing PFA, the tensile strength of the belt may be insufficient, and sufficient tension may not be applied to the belt. Alternatively, if the endless belt is rotated under high tension, the belt may stretch, causing the belt to meander or wrinkle.
[0048] The object 30 to be laminated supplied to the lamination section 20 passes between the lamination roll 22 and the cooling roll 23, the outer surface of the cooling roll 23, and between the cooling roll 23 and the roll 25 in this order along the conveying direction T. The object 30 to be laminated is, for example, a sheet-like object such as paper or a plastic film. When the object 30 to be laminated passes between the lamination roll 22 and the cooling roll 23, molten resin 31 is supplied from the die 24 between the object 30 to be laminated and the cooling roll 23. The molten resin 31 is cooled by the cooling roll 23 and solidifies so as to cover the object 30 to be laminated. At this time, the excess molten resin 31 protrudes from the object 30 to be laminated in a direction perpendicular to the conveying direction T of the object 30 to be laminated.
[0049] 5 shows a state where a part of the supplied molten resin 31 protrudes from the lamination target 30. The protruding molten resin 31 adheres to the endless belt 10 and solidifies. Since the endless belt 10 according to the embodiment has excellent releasability and abrasion resistance, even if the resin 31 adhered to the endless belt 10 is repeatedly peeled off from the endless belt 10 as the lamination target 30 is transported, the surface layer is not easily worn. As a result, unnecessary resin is unlikely to remain on the endless belt 10, and the endless belt 10 can withstand long-term use.
[0050] 4 and 5, the adhesive tape according to the embodiment is processed into an endless belt for use, but the adhesive tape may be directly attached to the laminating roll 22. In this case, the adhesive tape is not required to have high tensile strength compared to the case where the adhesive tape is processed into an endless belt for use.
[0051] The use of the pressure-sensitive adhesive tape according to the embodiment is not limited to release applications during lamination, and it can also be used, for example, for release applications to prevent direct contact between an object to be sealed and a heating part of a heat-sealing device when performing heat sealing. [Example] Examples will be described below, but the embodiments are not limited to the examples described below.
[0052] Example 1 <Preparation of Base Layer and Surface Layer> 100 parts by mass of PTFE fine powder was uniformly mixed with 30 parts by mass of hydrocarbon oil. This mixture was paste-extruded and preformed into a rod shape. This preform was passed between a pair of metal rolling rolls to obtain a rectangular unsintered tape. Next, an impregnation tank was prepared, filled with an aqueous dispersion containing PFA particles at a solids concentration of 40% by weight. This dispersion did not contain other resin particles such as PTFE particles. The previously prepared unsintered tape was passed through this dispersion, and then the dispersion on one side was scraped off with a blade to obtain an unsintered tape with a coating film formed on one side.
[0053] Thereafter, this unsintered tape was sintered for 60 seconds at a temperature of 360° C. Furthermore, this tape was stretched three times in the longitudinal direction of the tape using a roll stretching machine to produce a laminate in which a surface layer was formed on the main surface of the base layer.
[0054] <Preparation of adhesive layer> The other surface of the base layer was etched using metallic sodium to modify the surface. Next, a peroxide-curing silicone-based adhesive was prepared as the adhesive, and benzoyl peroxide was prepared as the curing agent. These adhesives and curing agents were dissolved in xylene as a solvent to prepare an adhesive-containing solution. This solution contained 50% by weight of the adhesive and 1% by weight of the curing agent relative to the weight of the solution.
[0055] The solution was applied onto the surface of the surface-modified substrate layer to form a coating film. The laminate with the coating film formed thereon was placed in an electric oven and subjected to a heat treatment in batches. The heat treatment was performed at a temperature of 200° C. for 280 seconds.
[0056] Thus, an adhesive tape according to Example 1 was produced. The adhesive tape according to Example 1 had a thickness of 100 μm, a thickness of the base layer of 60 μm, a thickness of the surface layer of 10 μm, and a thickness of the adhesive layer of 30 μm.
[0057] Furthermore, the tensile strength of the pressure-sensitive adhesive tape according to Example 1 was evaluated according to JIS K 7161:1994 and was found to be 90 MPa.
[0058] The prepared adhesive tape was processed into an endless belt as shown in Figures 4 and 5 and used. As a result, little molten resin remained on the endless belt, and it was able to withstand long-term use. That is, the adhesive tape according to Example 1 was excellent in abrasion resistance as well as releasability.
[0059] Comparative Example 1 An adhesive tape was produced in the same manner as in Example 1, except that the formation of the surface layer was omitted.
[0060] The prepared adhesive tape was processed into an endless belt and used as shown in Figures 4 and 5. As a result, fuzzing occurred on the surface of the PTFE base layer even after a short period of use. That is, the adhesive tape according to Comparative Example 1 was inferior in releasability and abrasion resistance to the adhesive tape according to Example 1 having a surface layer.
[0061] The present invention is not limited to the above-mentioned embodiment, and can be modified in various ways in the implementation stage without departing from the gist of the invention. In addition, each embodiment may be implemented in combination as appropriate as possible, and in that case, the combined effect can be obtained. Furthermore, the above-mentioned embodiment includes inventions at various stages, and various inventions can be extracted by appropriate combinations of the disclosed multiple constituent elements. For example, even if some constituent elements are deleted from all the constituent elements shown in the embodiment, if the problem described in the "Problem to be Solved by the Invention" column can be solved and the effect described in the "Effect of the Invention" column can be obtained, the configuration from which the constituent elements are deleted can be extracted as the invention. The invention as claimed in the original application of this application is set forth below. [1] A substrate layer comprising polytetrafluoroethylene; a surface layer formed on at least a portion of a main surface of the base layer and containing a perfluoroalkoxyalkane; and an adhesive layer formed on a surface of the base layer opposite to the main surface. [2] The pressure-sensitive adhesive tape according to [1], wherein the surface layer is made of a perfluoroalkoxyalkane. [3] The pressure-sensitive adhesive tape according to [1] or [2], wherein the thickness of the surface layer is within the range of 0.1 μm to 50 μm. [4] The pressure-sensitive adhesive tape according to any one of [1] to [3], wherein the thickness of the base layer is in the range of 10 μm to 500 μm. [5] The pressure-sensitive adhesive tape according to any one of [1] to [4], wherein the tensile strength in a direction parallel to the main surface is within a range of 30 MPa to 250 MPa. [6] The pressure-sensitive adhesive tape according to any one of [1] to [5], wherein the base layer is a polytetrafluoroethylene film. [7] An endless belt having the adhesive tape according to any one of [1] to [6]. [8] Providing an unsintered polytetrafluoroethylene sheet; applying a dispersion containing perfluoroalkoxyalkane particles to at least one surface of the polytetrafluoroethylene sheet to form a coating film, thereby obtaining the polytetrafluoroethylene sheet having the coating film; calcining the polytetrafluoroethylene sheet having the coating to obtain a polytetrafluoroethylene film; stretching the baked polytetrafluoroethylene film to obtain a laminate including a base layer containing polytetrafluoroethylene and a surface layer formed on a main surface of the base layer and containing a perfluoroalkoxyalkane; forming an adhesive layer on a surface of the base layer opposite to the main surface; A method for producing an adhesive tape comprising the steps of: [Explanation of symbols]
[0062] 1...adhesive tape, 2...base material layer, 3...surface layer, 4...adhesive layer, 10...endless belt, 20...laminating portion, 21, 22...laminating roll, 23...cooling roll, 24...die, 25...roll, 30...object to be laminated, 31...molten resin.
Claims
1. A base layer containing polytetrafluoroethylene; a surface layer formed on at least a portion of a main surface of the base layer and made of a perfluoroalkoxyalkane; and an adhesive layer formed on a surface of the base layer opposite to the main surface.
2. 2. The adhesive tape according to claim 1, wherein the surface layer has a thickness in the range of 0.1 μm to 50 μm.
3. The adhesive tape according to claim 1 or 2, wherein the thickness of the base layer is in the range of 10 μm to 500 μm.
4. The pressure-sensitive adhesive tape according to any one of claims 1 to 3, wherein the tensile strength in a direction parallel to the main surface is in the range of 30 MPa to 250 MPa.
5. The pressure-sensitive adhesive tape according to any one of claims 1 to 4, wherein the base layer is made of polytetrafluoroethylene.
6. An endless belt comprising the adhesive tape according to any one of claims 1 to 5.
7. Providing an unsintered polytetrafluoroethylene sheet; applying a dispersion containing perfluoroalkoxyalkane particles to at least one surface of the polytetrafluoroethylene sheet to form a coating film, thereby obtaining the polytetrafluoroethylene sheet having the coating film; calcining the polytetrafluoroethylene sheet having the coating to obtain a polytetrafluoroethylene film; stretching the baked polytetrafluoroethylene film to obtain a laminate including a base layer containing polytetrafluoroethylene and a surface layer formed on a main surface of the base layer and made of a perfluoroalkoxyalkane; forming an adhesive layer on a surface of the base layer opposite to the main surface; A method for producing an adhesive tape comprising the steps of:
Citation Information
Patent Citations
Process for making tubing
JP1977144073A
Releasable sheet
JP1993053941U
Self-adhesive tape
JP1994025617A
Tubular article
JP1994298952A
Molded article of polytetrafluoroethylene, and manufacture and use thereof
JP1998315400A