Coil component and method for manufacturing the coil component

The coil component's innovative electrode layer structure with varying filler and resin ratios and metallic bonding enhances adhesion strength between layers, addressing structural defects and ensuring robust electrical connections.

JP7561003B2Active Publication Date: 2024-10-03TAIYO YUDEN KK
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020184044
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-02-29
Filing Date
2020-11-04
Publication Date
2024-10-03
Estimated Expiration
2040-11-04

AI Technical Summary

Technical Problem

Conventional coil components face issues with decreased adhesion strength between the electrode layer and the plating layer due to increased resin content, leading to structural defects in the plating layer.

Method used

The coil component design includes a first electrode layer with a higher resin volume ratio and a second electrode layer with a larger filler volume ratio, where the fillers in the second electrode layer are metallically bonded to the plating layer, enhancing adhesion strength.

Benefits of technology

This design improves the adhesion strength between the electrode layer and the plating layer while maintaining strong bonding with the base material, reducing structural defects and ensuring reliable electrical connections.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007561003000001
    Figure 0007561003000001
  • Figure 0007561003000002
    Figure 0007561003000002
  • Figure 0007561003000003
    Figure 0007561003000003
Patent Text Reader

Abstract

To provide a coil component capable of improving the adhesion strength between an electrode layer contained in an external electrode and a plating layer.SOLUTION: A coil component 1 includes a substrate 10, external electrodes 21 and 22 provided on the surface of the substrate 10, and a conductor 25 that is electrically connected to the external electrodes 21 and 22, and is wound around a coil shaft Ax, and the external electrodes 21 and 22 have a first electrode layer 24A, a second electrode layer 24B covering the first electrode layer 24A, and a plating layer 26 covering the second electrode layer 24B. Each of the electrode layer 24A and the second electrode layer 24B includes a plurality of fillers F and a resin R, and the volume ratio of a filler FB in the second electrode layer 24B is larger than the volume ratio of the filler FB in the first electrode layer 24A.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a coil component and a method for manufacturing a coil component. [Background technology]

[0002] A conventional coil component such as an inductor typically includes a magnetic base made of a magnetic material, a conductor provided within the magnetic base and wound around a coil axis, and an external electrode connected to an end of the conductor. This coil component is mounted by electrically connecting the external electrode to a substrate using, for example, solder, and is used as a component of various electronic devices. A conventional coil component is disclosed, for example, in Patent Document 1. The external electrode of the coil component in Patent Document 1 includes an electrode layer formed by heat-treating a conductive paste containing a metal filler and a resin. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-120809 A Summary of the Invention [Problem to be solved by the invention]

[0004] When an electrode layer is formed using a conductive paste containing a metal filler and a resin, a plating layer is generally provided on the electrode layer. In order to improve the adhesion between the electrode layer and the substrate, it is desirable to increase the ratio of resin contained in the electrode layer. However, if the ratio of resin in the electrode layer is increased, structural defects are likely to be formed in the plating layer when the plating layer is grown on the electrode layer. As a result, there is a risk of a decrease in the adhesion strength between the electrode layer and the plating layer.

[0005] The present invention relates to a coil component having an external electrode and a plating layer, and more particularly to a coil having an external electrode and a plating layer. [Means for solving the problem]

[0006] A coil component according to one embodiment of the present invention comprises a base, an external electrode provided on a surface of the base, and a conductor electrically connected to the external electrode and wound around a coil axis, wherein the external electrode has a first electrode layer, a second electrode layer covering the first electrode layer, and a plating layer covering the second electrode layer, each of the first electrode layer and the second electrode layer including a plurality of fillers and a resin, and the volumetric proportion of the filler in the second electrode layer is greater than the volumetric proportion of the filler in the first electrode layer.

[0007] In one embodiment of the present invention, the volume fraction of the resin in the first electrode layer may be greater than the volume fraction of the resin in the second electrode layer.

[0008] In one embodiment of the present invention, the adhesion strength between the first electrode layer and the substrate may be higher than the adhesion strength between the second electrode layer and the substrate.

[0009] In one embodiment of the present invention, the proportion of resin in the first electrode layer may be 65 vol % or less.

[0010] In one embodiment of the present invention, the plurality of fillers may be made of a metallic material.

[0011] In one embodiment of the present invention, the multiple fillers may include a first filler having a spherical shape and a second filler having a flat shape, and the aspect ratio of the first filler may be 2 or less, and the aspect ratio of the second filler may be 3 or more.

[0012] In one embodiment of the present invention, among the multiple fillers in the second electrode layer, the proportion of the first filler may be 40 vol% or more and 70 vol% or less, and the proportion of the second filler may be 30 vol% or more and 60 vol% or less.

[0013] In one embodiment of the present invention, at least a portion of the plurality of fillers contained in the second electrode layer may be metallically bonded to the plating layer.

[0014] In one embodiment of the present invention, the plating layer may include a first plating layer in contact with the second electrode layer and comprised of Ni.

[0015] In one embodiment of the present invention, the first plating layer may cover the entire outer surface of the second electrode layer.

[0016] In one embodiment of the present invention, the resin may be a thermosetting resin.

[0017] An embodiment of the present invention relates to a circuit board including any one of the above electronic components. Also, an embodiment of the present invention relates to an electronic device including the above circuit board. Effect of the Invention

[0018] According to the present invention, there is provided a coil component capable of improving the adhesive strength between the electrode layer and the plating layer included in the external electrode. [Brief description of the drawings]

[0019] [Figure 1] FIG. 1 is a perspective view showing a coil component according to an embodiment of the present invention. [Diagram 2] 2 is an enlarged cross-sectional view that shows a schematic enlargement of a cross section of a magnetic base of the coil component of FIG. 1. [Diagram 3] 2 is an enlarged cross-sectional view showing a cross section of the periphery of a joint portion between one end of a conductor of the coil component of FIG. 1 and an external electrode. [Figure 4] 2 is a cross-sectional view showing an external electrode and a conductor of the coil component of FIG. 1. [Diagram 5] 2 is a schematic view of an electron microscope image of a cross section of an external electrode of the coil component of FIG. 1. [Figure 6] 2 is an enlarged cross-sectional view that illustrates a cross section of a joint portion between a base and an external electrode of the coil component in FIG. 1. [Figure 7A] 11 is a cross-sectional view showing a schematic diagram of another embodiment of an external electrode of a coil component according to the present invention. FIG. [Figure 7B] 11 is a cross-sectional view showing a schematic diagram of another embodiment of an external electrode of a coil component according to the present invention. FIG. [Figure 8] FIG. 11 is a perspective view illustrating a coil component according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] Hereinafter, various embodiments of the present invention will be described with reference to the drawings as appropriate. Note that components common to multiple drawings are given the same reference numerals throughout the multiple drawings. Please note that the drawings are not necessarily drawn to scale for the sake of convenience of explanation.

[0021] An overview of a coil component 1 according to one embodiment of the present invention will be described with reference to Fig. 1. Fig. 1 is a perspective view that typically illustrates the coil component 1. As shown in Fig. 1, the coil component 1 includes a base 10, a coil conductor (conductor) 25 provided inside the base 10, an external electrode 21 provided on the surface of the base 10, and an external electrode 22 provided on the surface of the base 10 at a position spaced apart from the external electrode 21.

[0022] In this specification, unless otherwise understood in the context, the "length" direction, "width" direction, and "height" direction of the coil device 1 are the "L-axis" direction, the "W-axis" direction, and the "T-axis" direction in Figure 1, respectively.

[0023] The coil component 1 is mounted on a circuit board (not shown). This circuit board is provided with two land portions. The coil component 1 can be mounted on the circuit board by joining the external electrodes 21, 22 to the land portions corresponding to the external electrodes 21, 22, respectively. Electronic devices in which this circuit board can be mounted include smartphones, tablets, game consoles, and various other electronic devices. This circuit board may be mounted on an electrical component of an automobile, which is a type of electronic device.

[0024] The coil component 1 can be applied to inductors, transformers, filters, reactors, and various other coil components having external electrodes 21, 22 on the surface of the base 10. The coil component 1 can also be applied to coupled inductors, choke coils, and various other magnetically coupled coil components. Applications of the coil component 1 are not limited to those explicitly stated in this specification.

[0025] The base 10 is made of an insulating material. In one embodiment, the base 10 is mainly made of a magnetic material and is formed in a rectangular parallelepiped shape. The base 10 of the coil component 1 according to one embodiment of the present invention is formed so as to have a length dimension (dimension in the L-axis direction) of 1.0 mm to 4.5 mm, a width dimension (dimension in the W-axis direction) of 0.5 mm to 3.2 mm, and a height dimension (dimension in the T-axis direction) of 0.5 mm to 5.0 mm. The dimensions of the base 10 are not limited to the dimensions specifically described in this specification. In this specification, the terms "rectangular parallelepiped" or "rectangular parallelepiped shape" do not only mean "rectangular parallelepiped" in the strict mathematical sense.

[0026] The base 10 has a first main surface 10a, a second main surface 10b, a first end surface 10c, a second end surface 10d, a first side surface 10e, and a second side surface 10f. The outer surface of the base 10 is defined by these six surfaces. The first main surface 10a and the second main surface 10b form both end surfaces in the height direction, the first end surface 10c and the second end surface 10d form both end surfaces in the length direction, and the first side surface 10e and the second side surface 10f form both end surfaces in the width direction.

[0027] As shown in Fig. 1, the first main surface 10a is located on the upper side of the base 10, and therefore the first main surface 10a may be referred to as the "upper surface". Similarly, the second main surface 10b may be referred to as the "lower surface". The coil component 1 is disposed so that the first main surface 10a faces the circuit board, and therefore the first main surface 10a may be referred to as the "mounting surface". When referring to the up-down direction of the coil component 1, the up-down direction in Fig. 1 is used as the reference.

[0028] Next, the magnetic substrate 10 will be further described with reference to FIG. 2. FIG. 2 is an enlarged cross-sectional view that typically shows an enlarged cross section of the substrate 10. As shown in the figure, the substrate 10 includes a plurality of first metal magnetic particles 11, a plurality of second metal magnetic particles 12, and a binder 13. The binder 13 binds the plurality of first metal magnetic particles 11 and the plurality of second metal magnetic particles 12 to each other. In other words, the substrate 10 is composed of the binder 13 and the plurality of first metal magnetic particles 11 and the plurality of second metal magnetic particles 12 that are bound by the binder 13. The substrate 10 may include a magnetic material, a non-magnetic material, or a dielectric material as the non-magnetic material.

[0029] The first metal magnetic particles 11 have a larger average particle size than the second metal magnetic particles 12. That is, the average particle size of the first metal magnetic particles 11 (hereinafter referred to as the first average particle size) is different from the average particle size of the second metal magnetic particles 12 (hereinafter referred to as the second average particle size). The first average particle size is, for example, 30 μm, and the second average particle size is, for example, 2 μm, but they may be different average particle sizes. In one embodiment of the present invention, the base 10 may further include a third metal magnetic particle (not shown) having an average particle size different from the first average particle size and the second average particle size (hereinafter, the average particle size of the third metal magnetic particles is referred to as the third average particle size). The third average particle size may be smaller than the first average particle size and larger than the second average particle size, or smaller than the second average particle size. In the following description, in this specification, when there is no need to distinguish between the first metal magnetic particles 11, the second metal magnetic particles 12 and the third metal magnetic particles, the first metal magnetic particles 11, the second metal magnetic particles 12 and the third metal magnetic particles contained in the magnetic base 10 may be collectively referred to as "metal magnetic particles."

[0030] The first metal magnetic particles 11 and the second metal magnetic particles 12 are made of various soft magnetic materials. The first metal magnetic particles 11 are mainly composed of Fe, for example. Specifically, the first metal magnetic particles 11 are (1) metal particles such as Fe, Ni, etc., (2) crystalline alloy particles such as alloys containing Fe, Si, and Cr, alloys containing Fe, Si, Al, and alloys containing Fe and Ni, (3) amorphous alloy particles such as alloys containing Fe, Si, Cr, B, and C, and alloys containing Fe, Si, Cr, and B, or (4) mixed particles of these. The composition of the metal magnetic particles contained in the magnetic base 10 is not limited to the above. The first metal magnetic particles 11 contain, for example, 85 wt% or more of Fe. This makes it possible to obtain a magnetic base 10 with excellent magnetic permeability. The composition of the second metal magnetic particles 12 may be the same as or different from the composition of the first metal magnetic particles 11. When the magnetic substrate 10 contains a plurality of third metal magnetic particles (not shown), the composition of the third metal magnetic particles may be the same as or different from the composition of the first metal magnetic particles 11, similar to the composition of the second metal magnetic particles 12.

[0031] The surface of the metal magnetic particles may be covered with an insulating film (not shown). For example, the insulating film is made of glass, resin, or other materials having excellent insulating properties. The insulating film is formed on the surface of the first metal magnetic particles 11 by, for example, mixing the first metal magnetic particles 11 and powder of a glass material in a friction mixer (not shown). The insulating film made of the glass material is fixed to the surface of the first metal magnetic particles 11 by a compressive friction action in the friction mixer. The glass material may include ZnO and P2O5. The insulating film may be formed from various glass materials. The insulating film 14 may be formed from alumina powder, zirconia powder, or other oxide powder having excellent insulating properties instead of or in addition to glass powder. The thickness of the insulating film is, for example, 100 nm or less.

[0032] The second metal magnetic particles 12 may be coated with an insulating film different from the insulating film of the first metal magnetic particles 11. This insulating film may be an oxide film formed by oxidizing the second metal magnetic particles 12. The thickness of this insulating film is, for example, 20 nm or less. This insulating film may be an oxide film formed on the surface of the second metal magnetic particles 12 by heat treating the second metal magnetic particles 12 in an air atmosphere. This insulating film may be an oxide film containing oxides of Fe and other elements contained in the second metal magnetic particles 12. This insulating film may be an iron phosphate film formed on the surface of the second metal magnetic particles 12 by putting the second metal magnetic particles 12 into phosphoric acid and stirring. The insulating film of the first metal magnetic particles 11 may be an oxide film formed by oxidizing the first metal magnetic particles 11, and the insulating film of the second metal magnetic particles 12 may be a coating film provided separately, regardless of the oxidation of the second metal magnetic particles 12.

[0033] The binder 13 is, for example, a thermosetting resin with excellent insulating properties. For example, epoxy resin, polyimide resin, polystyrene (PS) resin, high density polyethylene (HDPE) resin, polyoxymethylene (POM) resin, polycarbonate (PC) resin, polyvinylidene fluoride (PVDF) resin, phenolic resin, polytetrafluoroethylene (PTFE) resin, or polybenzoxazole (PBO) resin may be used as the binder 13. In addition, glass or the like may be used as the binder 13, and the binder 13 may contain an insulating filler or the like.

[0034] The conductor 25 is formed to have a predetermined pattern. In the illustrated embodiment, the conductor 25 is wound around the coil axis Ax (see FIG. 1). The conductor 25 has, for example, an elliptical shape, a meandering shape, a linear shape, or a shape that is a combination of these in a plan view. The conductor 25 may have any shape, for example, a spiral shape.

[0035] The conductor 25 is made of Cu, Ag, or another conductive material. The entire surface of the conductor 25, except for the end faces 25a2 and 25b2, may be covered with an insulating film. When the conductor 25 is wound around the coil axis Ax for a plurality of turns as shown in the figure, each turn of the conductor 25 may be separated from the adjacent turns. In this case, the base 10 is interposed between the adjacent turns.

[0036] Conductor 25 has lead conductor 25a1 at one end and lead conductor 25b1 at the other end. End face 25a2 is formed at the end of lead conductor 25a1, and end face 25b2 is formed at the end of lead conductor 25b1. Lead conductor 25a1, which is one end of conductor 25, is electrically connected to external electrode 21, and lead conductor 25b1, which is the other end of conductor 25, is electrically connected to external electrode 22.

[0037] In one embodiment of the present invention, the external electrode 21 is provided on the first main surface 10a, the second main surface 10b, the first end surface 10d, the first side surface 10e, and a part of the second side surface 10f of the base 10. The external electrode 22 is provided on the first main surface 10a, the second main surface 10b, the second end surface 10c, the first side surface 10e, and a part of the second side surface 10f of the base 10. The external electrode 21 and the external electrode 22 are arranged apart from each other. The shapes and arrangements of the external electrodes 21 and 22 are not limited to the illustrated example. The lead conductor 25a1 and the lead conductor 25b1 are each led out to the first main surface (i.e., the mounting surface) 10a of the base 10, and the end surface 25a2 of the lead conductor 25a1 and the end surface 25b2 of the lead conductor 25b1 are exposed from the base 10 on the first main surface 10a. That is, the end face 25a2 of the lead conductor 25a1 and the end face 25b2 of the lead conductor 25b1 are exposed from the base 10 at the same surface. The end face 25a2 of the lead conductor 25a1 and the end face 25b2 of the lead conductor 25b1 may be exposed from the base 10 at different surfaces.

[0038] Next, the external electrode of the coil component 1 according to one embodiment of the present invention will be described in detail with reference to Figs. 3, 4, and 5. Fig. 3 is an enlarged cross-sectional view showing a cross section of the periphery of a joint portion between one end of the conductor 25 of the coil component 1 of Fig. 1 and the external electrode 21. Fig. 4 is a cross-sectional view showing the external electrode 21 and the conductor 25 of the coil component 1. Fig. 5 is a schematic diagram of an electron microscope image of a cross section of the external electrode of the coil component of Fig. 1. In the following description, the external electrode 21 will be described, but the description of the external electrode 21 will also be applied to the external electrode 22 unless there are special circumstances. In addition, Figs. 3 to 5 are diagrams for explaining the external electrode 21, but will also be applied to the external electrode 22. As shown in Figs. 3 to 5, the external electrode 21 has a metal film 23, an electrode layer 24, and a plating layer 26. The metal film 23, the electrode layer 24, and the plating layer 26 are laminated in this order on the first main surface 10a of the base 10 on which one end (i.e., end face 25a2) of the conductor 25 is exposed. The lamination direction extends in a direction perpendicular to the surface of the base 10 on which one end (i.e., end face 25a2) of the conductor 25 is exposed (in the illustrated example, the first main surface 10a). All of Figures 3 to 5 show a cross section of the coil device 1 cut along this lamination direction.

[0039] The metal film 23 is provided so as to contact the first main surface 10a and one end of the conductor 25. The metal film 23 is, for example, a sputtered film, and at least a part of the metal film 23 and one end of the conductor 25 (i.e., the end face 25a2) are connected by metallic bonding. Here, "at least a part" means any region of the end face 25a2. For example, the metal film 23 and the end 25a1 may be connected by metallic bonding at the peripheral edge PP (see FIG. 3) of the end face 25a2. FIG. 3 shows an example in which the metal film 23 and the end 25a1 of the conductor 25 are connected by metallic bonding over the entire surface of the end face 25a2. In the example of FIG. 3, the metal film 23 and the end 25a1 are also metallically bonded at the peripheral edge PP of the end face 25a2.

[0040] The material of the metal film 23 is, for example, a metal such as Ag, Au, Pd, Pt, Cu, Ni, Ti, or Ta, or an alloy thereof. The metal used for the metal film 23 is preferably a metal that is difficult to oxidize, or a metal that can be easily reduced even if oxidized. In addition, it is preferable that a material with a low volume resistivity is used for the metal film 23. The thickness of the metal film 23 is not particularly limited, but can be, for example, 0.5 μm or more and 5 μm or less. It is preferable that the ionization tendency of the main component of the metal contained in the metal film 23 is smaller than the ionization tendency of the metal constituting the conductor 25. Here, the "main component of the metal contained in the metal film 23" refers to a metal component that occupies the majority of the metal species in terms of weight percent among the metals constituting the metal film 23. If the type of metal contained in the metal film 23 is one type, the main component refers to the component of that metal. As an example, if the material constituting the conductor 25 is Cu, the metal contained in the metal film 23 can be Ag.

[0041] The average aspect ratio of the metal particles contained in the metal film 23 is 0.8 or more and 1.5 or less. Here, the aspect ratio of the metal particles refers to the value of b / a, where a is the dimension of one metal particle contained in the metal film 23 in a direction horizontal to the boundary surface BI and b is the dimension of the one metal particle in a direction perpendicular to the boundary surface BI. The average aspect ratio of the metal particles can be, for example, the average value of the aspect ratios of a plurality of metal particles, such as 5 or 10. The metal particles contained in the metal film 23 are metallically bonded to each other.

[0042] The electrode layer 24 is provided on the metal film 23 and is electrically connected to one end of the conductor 25. The electrode layer 24 has a plurality of layers stacked in the stacking direction. In the illustrated embodiment, the electrode layer 24 has a first electrode layer 24A and a second electrode layer 24B covering the first electrode layer 24A. The second electrode layer 24B is provided on the opposite side of the first electrode layer 24A to the metal film 23 in the stacking direction. In the illustrated embodiment, the first electrode layer 24A is formed so as to cover the metal film 23 and a part of the main surface 10a of the base 10. The first electrode layer 24A may be formed so as to cover at least a part of the metal film 23. In this case, the first electrode layer 24A may be formed so as to cover a part of the main surface 10a of the base 10, or may be formed so as not to cover the main surface 10a of the base 10. The second electrode layer 24B is formed so as to cover the entire outer surface of the first electrode layer 24A (i.e., the surface not in contact with the metal film 23 and the base 10), as well as parts of the second main surface 10b, the first end surface 10d, the first side surface 10e, and the second side surface 10f of the base 10. The second electrode layer 24B included in the external electrode 22 is formed so as to cover the entire outer surface of the first electrode layer 24A (i.e., the surface not in contact with the metal film 23 and the base 10), as well as parts of the second main surface 10b, the second end surface 10c, the first side surface 10e, and the second side surface 10f of the base 10. The thickness of the first electrode layer 24A is, for example, about 10 μm to 20 μm, and the thickness of the second electrode layer 24B is, for example, about 20 μm to 30 μm. The interface between the first electrode layer 24A and the second electrode layer 24B can be the boundary between the resin R contained in the first electrode layer 24A and the resin R contained in the second electrode layer 24B. The boundary between the resin R contained in the first electrode layer 24A and the resin R contained in the second electrode layer 24B can be confirmed by observation using, for example, an optical microscope.

[0043] The electrode layer 24 (i.e., the first electrode layer 24A and the second electrode layer 24B) contains a plurality of fillers F and resins R. In the following description, the filler contained in the first electrode layer 24A is referred to as filler FA, the filler contained in the second electrode layer 24B is referred to as filler FB, the resin contained in the first electrode layer 24A is referred to as RA, and the resin contained in the second electrode layer 24B is referred to as RB. The volume ratio of the filler FB in the second electrode layer 24B is greater than the volume ratio of the filler FA in the first electrode layer 24A. In one or more embodiments of the present invention, the size of the volume of the filler FB in the first electrode layer 24A and the volume of the filler FB in the second electrode layer 24B can be determined by comparing the ratio of the area of ​​the filler FA to the area of ​​the first electrode layer 24A and the ratio of the area of ​​the filler FB to the area of ​​the second electrode layer 24B in a cut surface obtained by cutting the external electrode 21 in a plane extending along the stacking direction (i.e., a plane extending parallel to the stacking direction). That is, when the ratio of the area of ​​the filler FB to the area of ​​the second electrode layer 24B is greater than the ratio of the area of ​​the filler FA to the area of ​​the first electrode layer 24A, the ratio of the volume of the filler FB in the second electrode layer 24B is greater than the ratio of the volume of the filler FA in the first electrode layer 24A. The area of ​​the first electrode layer 24A means the sum of the area of ​​the filler FA and the area of ​​the resin RA contained in the first electrode layer 24A. The area of ​​the second electrode layer 24B means the sum of the area of ​​the filler FB and the area of ​​the resin RB contained in the second electrode layer 24B. The areas of the first electrode layer 24A, the second electrode layer 24B, the filler FA, the filler FB, the resin RA, and the resin RB in a cut surface obtained by cutting the external electrode 21 in a plane extending along the stacking direction (i.e., a plane extending parallel to the stacking direction) can be measured by performing image processing on an SEM photograph obtained by imaging the cut surface with a scanning electron microscope (SEM). The filler FA included in the first electrode layer 24A includes a plurality of first fillers FA1 and a plurality of second fillers FA2. Similarly, the filler FB included in the second electrode layer 24B includes a plurality of first fillers FB1 and a plurality of second fillers FB2. Each of the plurality of first fillers FA1 and FB1 has a spherical shape and an aspect ratio of 2 or less.Each of the second fillers FA2 and FB2 has a flat shape, and the aspect ratio is 3 or more. In this specification, the aspect ratio refers to the ratio of the dimension in the minor axis direction to the dimension in the major axis direction of the filler F in the cross section in the thickness direction of the electrode layer 24 (i.e., the value obtained by dividing the maximum particle size by the minimum particle size). In the cross section in the thickness direction of the electrode layer 24, the average of the maximum particle size of the second fillers FA2 and FB2 is larger than the average of the maximum particle size of the first fillers FA1 and FB1. The average of the maximum particle size of the first fillers FFA1 and FB1 is, for example, 1 μm to 10 μm, and the average of the maximum particle size of the second fillers FA2 and FB2 is, for example, 0.1 μm to 10 μm. Of the multiple fillers FA in the first electrode layer 24A, the ratio of the first filler FA1 is 30 vol% or more and 70 vol% or less, and the ratio of the second filler FA2 is 30 vol% or more and 70 vol% or less. Of the multiple fillers FB in the second electrode layer 24B, the proportion of the first filler FB1 is 40 vol % or more and 70 vol % or less, and the proportion of the second filler FB2 is 30 vol % or more and 60 vol % or less.

[0044] The first filler FA1, FB1 and the second filler FA2, FB2 are made of a metal material having excellent electrical conductivity, such as Ag, Cu, Au, Pd, or Ni. Alternatively, an alloy such as AgPd, brass, or bronze can be used as the material of the first filler FA1, FB1 and the second filler FA2, FB2. The first filler FA1, FB1 and the second filler FA2, FB2 may be a metal filler coated with a film of a low resistance metal such as Ag. In addition, the first filler FA1, FB1 and the second filler FA2, FB2 contain metals of the same composition. In the illustrated embodiment, the first filler FA1, FB1 and the second filler FA2, FB2 are both made of Ag. The first filler FA1, FB1 and the second filler FA2, FB2 may contain metals different from each other, or may be made of only metals different from each other. In addition, the first filler FA1 contained in the first electrode layer 24A and the first filler FB1 contained in the second electrode layer 24B may contain different metals, or may be composed only of different metals. The second filler FA2 contained in the first electrode layer 24A and the second filler FB2 contained in the second electrode layer 24B may contain different metals, or may be composed only of different metals. Even when the first filler FA1, FB1 and the second filler FA2, FB2 contain different metals, the first filler FA1, FB1 and the second filler FA2, FB2 are metallically bonded, and the bonded portion between the first filler FA1, FB1 and the second filler FA2, FB2 is alloyed. In this case, it is preferable to select a combination of the metal contained in the first filler FA1, FB1 and the metal contained in the second filler FA2, FB2 that has a stronger bond strength than the metallic bond between the same kind of metals. The bonding strength of alloys formed by combining different metals can be clarified from publicly known literature.

[0045] The first fillers FA1, FB1 and the second fillers FA2, FB2 of the first electrode layer 24A and the second electrode layer 24B are heat-treated in the manufacturing process of the coil component 1. As a result, the first fillers FA1, FB1 and the second fillers FA2, FB2 are metallically bonded to each other. The first electrode layer 24A and the second electrode layer 24B may include a portion where the second fillers FA2, FB2 are metallically bonded to each other in a state where the long axes of the second fillers FA2, FB2 are parallel to each other. The first electrode layer 24A and the second electrode layer 24B may include a portion where the first fillers FA1, FB1 are metallically bonded to each other. At the interface between the first electrode layer 24A and the metal film 23, the second filler FA2 is metallically bonded to the metal film 23. As a result, the first electrode layer 24A and the metal film 23 are electrically connected. In addition, at the interface between the second electrode layer 24B and the plating layer 26, the second filler FB2 is metallically bonded to the plating layer 26. The long axis direction of the second filler FB2 is approximately parallel to a direction perpendicular to the thickness direction of the electrode layer 24. This electrically connects the second electrode layer 24B and the plating layer 26. Similarly, the first filler FA1 of the first electrode layer 24A may be metallically bonded to the metal film 23. The first filler FB1 of the second electrode layer 24B may be metallically bonded to the plating layer 26.

[0046] The resins RA and RB contained in the first electrode layer 24A and the second electrode layer 24B are, for example, thermosetting resins. As the thermosetting resin, a thermosetting resin generally used for adhesive applications can be used, and examples thereof include epoxy resin, acrylic resin, phenol resin, cyanate resin, amino resin, oxetane resin, silicone-modified organic resin, polyimide resin, maleimide resin, and BT (bismaleimide triazine) resin. The resin contained in the first electrode layer 24A and the resin contained in the second electrode layer 24B may contain two or more types of thermosetting resins. The resin RA contained in the first electrode layer 24A and the resin RB contained in the second electrode layer 24B may be the same type as each other, or may be different from each other. In one or more embodiments of the present invention, the volume ratio of the resin RA in the first electrode layer 24A is greater than the volume ratio of the resin RB in the second electrode layer 24B. The size of the volume of the resin RA in the first electrode layer 24A and the volume of the resin RB in the second electrode layer 24B can be determined by comparing the ratio of the area of ​​the resin RA to the area of ​​the first electrode layer 24A and the ratio of the area of ​​the resin RB to the area of ​​the second electrode layer 24B in a cut surface obtained by cutting the external electrode 21 along a plane extending along the lamination direction. That is, when the ratio of the area of ​​the resin RA to the area of ​​the first electrode layer 24A is larger than the ratio of the area of ​​the resin RB to the area of ​​the second electrode layer 24B, the ratio of the volume of the resin RA in the first electrode layer 24A is larger than the ratio of the volume of the resin RB in the second electrode layer 24B. As a result, the adhesion strength between the first electrode layer 24A and the base 10 is higher than the adhesion strength between the second electrode layer 24B and the base 10. The ratio of the resin RA in the first electrode layer 24A is 65 vol% or less. The ratio of the resin RA in the first electrode layer 24A is preferably 30 vol% to 65 vol%. Furthermore, the ratio of the resin RA in the first electrode layer 24A is more preferably less than 65 vol%. The ratio of the resin RB in the second electrode layer 24B is 60 vol% or less. The ratio of the resin RB in the second electrode layer 24B is preferably 25 vol% to 60 vol%. Furthermore, the ratio of the resin RB in the second electrode layer 24B is more preferably less than 55 vol%.

[0047] The first electrode layer 24A is formed from a first conductive paste including first metal particles that become the first filler FA1, second metal particles that become the second filler FA2, and uncured resin. The second electrode layer 24B is formed from a second conductive paste including first metal particles that become the first filler FB1, second metal particles that become the second filler FB2, and uncured resin. The first conductive paste and the second conductive paste have different contents of the first metal particles and the second metal particles. The first metal particles and the second metal particles are the first fillers FA1, FB1 and the second fillers FA2, FB2, respectively, before being metal-bonded by heat treatment in the manufacturing process of the coil component 1. Each of the second metal particles has a flat shape, and the curvature of the outer shape of the second metal particle is minimum at both ends E in the long axis direction of the second metal particle. The average of the minimum radius of curvature of the second metal particles (i.e., the curvature of the end of the second metal particle in the long axis direction) is 0.5 μm or less of the first metal particles. As an example, the minimum radius of curvature of the second metal particles is 0.1 μm or less. In FIG. 5, the end of the second filler FA2, FB2 metallurgically bonded by heat treatment is shown as the end E of the second metal particle. In FIG. 5, the boundary of the end of the second filler FA2, FB2 metallurgically bonded is shown typically. The boundary of the end of the second filler FA2, FB2 can be confirmed, for example, by observing the cross section of the electrode layer 24 including the second filler FA2, FB2 at 50,000 times magnification using an electron microscope. In actual observation, the boundary of the end of the second filler FA2, FB2 may not be clearly observed. For example, when the end of the second filler FA2, FB2 is bonded to another first filler FA1, FB1 or second filler FA2, FB2, the boundary may not be clearly observed. In this case, the boundary of the crystal grains inside the second filler FA2, FB2 observed with an electron microscope may be the boundary of the second filler FA2, FB2. When the boundary of the crystal grains inside the second filler FA2, FB2 cannot be clearly observed, a curve estimated by any known estimation method from the shape of the part other than the end of the second filler FA2, FB2 that cannot be clearly observed may be the boundary of the end of the second filler FA2, FB2.

[0048] The plating layer 26 is provided on the second electrode layer 24B. The plating layer 26 covers the entire outer surface of the second electrode layer 24B (i.e., the surface not in contact with the first electrode layer 24A and the base 10). In the illustrated embodiment, the plating layer 26 has a multi-layer structure, and includes a first plating layer 26A in contact with the second electrode layer 24B and a second plating layer 26B provided on the first plating layer 26A. The thickness of the first plating layer 26A is, for example, 5 μm to 7 μm, and the thickness of the second plating layer 26B is, for example, 5 μm to 10 μm. The first plating layer 26A is made of, for example, Ni, and the second plating layer 26B is made of, for example, Sn. The first plating layer 26A may be made of a metal or alloy that serves as a barrier layer that exhibits corrosion resistance against heat treatment during soldering, other than Ni. The second plating layer 26B may be made of a metal or alloy having good solder wettability other than Sn. The plating layer 26 may be a single plating layer made of Ni or Sn.

[0049] 6 is an enlarged cross-sectional view of the joint portion between the base 10 and the external electrode 21 of the coil component 1. As shown in FIG. 6, the surface of the base 10 has a plurality of irregularities caused by shedding of the first metal magnetic particles 11 and / or the second metal particles 12. As a result, the interface between the base 10 and the first electrode layer 24A has a plurality of irregularities, and the base 10 and the first electrode layer 24A are bonded together by the anchor effect. Similarly, the interface between the first electrode layer 24A and the second electrode layer 24B, the interface between the second electrode layer 24B and the first plating layer 26A, and the interface between the first plating layer 26A and the second plating layer 26B each have a plurality of irregularities, and the first electrode layer 24A and the second electrode layer 24B, the second electrode layer 24B and the first plating layer 26A, and the first plating layer 26A and the second plating layer 26B are bonded together by the anchor effect. This improves the overall strength of the external electrodes 21, 22.

[0050] Next, a method for manufacturing the coil component 1 according to an embodiment of the present invention will be described. First, a conductor 25 formed into a coil shape using a metal material or the like, and a mixed resin composition prepared by kneading a particle group including the first metal magnetic particles 11 and the second metal magnetic particles 12 with a binder 13 made of a resin or the like are placed in a molding die, and compression molded so that an end face 25a2 of the lead conductor 25a1 and an end face 25b2 of the lead conductor 25b1 of the conductor 25 are exposed on the surface. The conductor 25 formed into a coil shape is, for example, a conductor formed by winding a conductor wire in a spiral shape, but other than a winding, a planar coil may also be used, and the coil shape is not particularly limited. The conductor 25 may have an insulating coating. By curing the resin in the molded body, a base 10 in which the conductor 25 is embedded is obtained.

[0051] Next, the surface of the magnetic base 10 where the end face 25a2 of the lead conductor 25a1 and the end face 25b2 of the lead conductor 25b1 of the conductor 25 are exposed is smoothed to remove oxides. Here, the surface is polished using an abrasive, and then plasma etching is performed. It is preferable to use an abrasive having a particle size smaller than that of the first metal magnetic particles 11. For example, if the average particle size of the first metal particles 11 is 30 μm, a particle size of 25 μm is selected. The etching may be performed by any method capable of removing oxides on the surface of the magnetic base, such as plasma etching.

[0052] Next, the metal film 23 is formed. For example, the method of forming the metal film 23 includes a sputtering deposition method, particularly a high-density sputtering deposition method. The high-density sputtering deposition method is a method of obtaining a dense film while preventing the sputtered film from becoming too hot by applying a large electric power for a short period of time. By cooling the sample during sputtering, it is possible to apply a larger electric power and obtain a denser sputtered film. If the above metals are used in this method, the sputtering yield is high and the metal film 23 can be efficiently formed. In this specification, the metal film formed by the sputtering deposition method is called a sputtered film. As for the method of forming the metal film 23, the metal film 23 may be formed by a method other than the sputtering deposition method as long as the end face 25a2 of the conductor 25 and the metal film 23 can be metallically bonded.

[0053] Next, the electrode layer 24 is formed on the metal film 23. To form the electrode layer 24, first, the first electrode layer 24A is formed. To form the first electrode layer 24A, first, a first conductive paste containing first metal particles to be the first fillers FA1 and second metal particles to be the second fillers FA2 is prepared. Next, a layer of the first conductive paste is formed by a printing method or the like. Next, the first metal particles and the second metal particles contained in the layer of the first conductive paste are metallically bonded by a heat treatment or the like. As an example, the heat treatment is performed under conditions of 170°C to 250°C and 30 minutes to 60 minutes. Also, depending on the materials of the first fillers FA1 and the second fillers FA2, the heat treatment is performed in a low-oxygen or reducing atmosphere. Next, the second electrode layer 24B is formed on the first electrode layer 24A. To form the second electrode layer 24B, a layer of a second conductive paste containing first metal particles that will become the first filler FB1 and second metal particles that will become the second filler FB2 is formed by a printing method or the like. Next, the first metal particles and the second metal particles contained in the second conductive paste layer are metallically bonded by a heat treatment or the like. The heat treatment for the second conductive paste is performed, for example, under the same conditions as the heat treatment for the first conductive paste. This process forms an electrode layer 24 that is electrically connected to the end of the conductor 25 via the metal film 23.

[0054] Finally, the first plating layer 26A and the second plating layer 26B are formed by a plating method. Through the above steps, the external electrodes 21, 22 are formed, and the coil component 1 is manufactured. The manufactured coil component 1 is mounted on a circuit board by soldering the external electrodes 21, 22 to the lands of the circuit board, respectively.

[0055] As described above, the external electrodes 21, 22 of the coil component 1 have the first electrode layer 24A, the second electrode layer 24B covering the first electrode layer 24A, and the plating layer 26 covering the second electrode layer 24B, and the volume ratio of the filler FB in the second electrode layer 24B is greater than the volume ratio of the filler FA in the first electrode layer 24A. In general, from the viewpoint of increasing the adhesion between the electrode layer 24 and the base material 10, it is desirable to increase the ratio of the resin R contained in the electrode layer 24. However, if the ratio of the resin R in the electrode layer 24 is increased, structural defects are likely to be formed in the plating layer 26 when the plating layer 26 is grown on the electrode layer 24, and there is a risk that the adhesion strength between the electrode layer 24 and the plating layer 26 is reduced. In the coil component 1 according to one embodiment of the present invention, the volume ratio of the filler FA in the first electrode layer 24A in contact with the base body 10 is relatively small (i.e., the volume ratio of the resin RA is relatively large), thereby ensuring the adhesion strength with the base body 10. On the other hand, by making the volume ratio of the filler FB in the second electrode layer 24B in contact with the plating layer 26 relatively large (i.e., making the volume ratio of the resin RB relatively small), it is possible to suppress the formation of structural defects when the plating layer 26 is grown on the second electrode layer 24B. Therefore, it is possible to improve the adhesion strength between the electrode layer 24 and the plating layer 26 while ensuring the adhesion strength between the electrode layer 24 and the base 10.

[0056] The plurality of fillers FA, FB of the electrode layer 24 include spherical first fillers FA1, FB1 and flat second fillers FA2, Fb2, and the aspect ratio of the first fillers FA1, FB1 may be 2 or less, and the aspect ratio of the second fillers FA2, FB2 may be 3 or more. Since the second fillers FA2, FB2 are flat, the curvature of the second fillers FA2, FB2 at both ends E in the long axis direction is small, and the curvature of the second fillers FA2, FB2 at the center in the long axis direction is large. Therefore, the energy required for metallic bonding by performing heat treatment is small at both ends E in the long axis direction of the second filler, and the energy required for metallic bonding by performing heat treatment is large at the center in the long axis direction of the second filler. Therefore, metallic bonding is easily promoted at both ends E in the long axis direction of the second filler, and metallic bonding is not easily promoted at the center in the long axis direction of the second filler. Therefore, while electrical connection is ensured by both ends E of the second fillers FA2, FB2 in the long axis direction, aggregation of the first fillers FA1, FB1 and the second fillers FA2, FB2 due to metallic bonding caused by heat treatment can be suppressed. As a result, uneven distribution of the first fillers FA1, FB1 and the second fillers FA2, FB2 in the electrode layer 24 is suppressed, and a decrease in the strength of the external electrodes 21, 22 can be suppressed.

[0057] Among the multiple fillers FB in the second electrode layer 24B, the ratio of the first filler FB1 may be 40 vol% or more and 70 vol% or less, and the ratio of the second filler FB2 may be 30 vol% or more and 60 vol% or less. In this way, in a dispersed state of the filler FB and the resin RB in the second electrode layer 24B, the resin RB can fill the gaps between the aggregates of the filler FB consisting of the first filler FB1 and the second filler FB2, while suppressing segregation of the resin RB. In particular, segregation of the resin RB can be suppressed near the bonding interface between the plating layer 26 and the second electrode layer 24B.

[0058] At least a portion of the plurality of fillers F contained in the second electrode layer 24B may be metallically bonded to the plating layer 26. This can reduce the electrical resistance between the plating layer 26 and the second electrode layer 24B.

[0059] Next, with reference to Figs. 7A and 7B, another embodiment of the external electrodes 21, 22 of the coil component 1 will be described. Figs. 7A and 7B are cross-sectional views that typically show another embodiment of the external electrodes of the coil component 1. As shown in Fig. 7A, an external electrode 121 according to another embodiment may be provided only on a part of the first main surface 10a of the base 10. In this case, only the outer surface of the second electrode layer 24B of the external electrode 121 is covered. Also, as shown in Fig. 7B, an external electrode 221 according to another embodiment may be provided only on a part of the first main surface 10a and the first end surface 10d of the base 10. In this case, the external electrode 221 is formed so as to cover the outer surface of the second electrode layer 24B of the external electrode 221 and a part of the first end surface 10d.

[0060] Next, a coil component 100 according to another embodiment of the present invention will be described with reference to Fig. 8. Fig. 8 is a perspective view that typically shows the coil component 100. As shown in the figure, the coil component 100, like the coil component 1, includes a coil conductor 25 within the base 10, an external electrode 21 provided on the surface of the base 10, and an external electrode 22 provided on the surface of the base 10 at a position spaced apart from the external electrode 21. The coil component 100 differs from the coil component 1 in that it includes an insulating plate 50 provided within the base 10, and the conductor 25 is provided on the upper and lower surfaces of the insulating plate 50.

[0061] Similarly to the coil component 1, the external electrodes 21, 22 of the coil component 100 also have a first electrode layer 24A, a second electrode layer 24B covering the first electrode layer 24A, and a plating layer 26 covering the second electrode layer 24B, and the volume ratio of the filler F in the second electrode layer 24B is greater than the volume ratio of the filler F in the first electrode layer 24A. Therefore, for the same reason as in the coil component 1, the adhesion strength between the electrode layer 24 and the base 10 can be ensured, while the adhesion strength between the electrode layer 24 and the plating layer 26 can be improved.

[0062] The dimensions, materials, and arrangements of each component described in the various embodiments above are not limited to those explicitly described in each embodiment, and each component can be modified to have any dimensions, materials, and arrangements that can be included in the scope of the present invention. Also, components not explicitly described in this specification can be added to each of the above-mentioned embodiments, and some of the components described in each embodiment can be omitted.

[0063] For example, the external electrodes 21, 22 of the coil component 1 and the coil component 100 may not have the metal film 23. In this case, the electrode layer 24 and the end of the conductor 25 may be directly connected to each other. [Explanation of symbols]

[0064] 1,100...coil component, 10...magnetic base, 21...external electrode, 22...external electrode, 23...metal film, 24...electrode layer, 24A...first electrode layer, 24B...second electrode layer, FA1, FB1...first filler, FA2, FB2...second filler, RA, RB...resin, 25...conductor, 26...plating layer, 26A...first plating layer, 26B...second plating layer.

Claims

1. A substrate including a plurality of metal magnetic particles and a resin binder; an external electrode provided on a surface of the base body so as to be in contact with a first surface of the surface; a conductor electrically connected to the external electrode, wound around a coil axis inside the base, and having one end and the other end exposed from the first surface of the base, the external electrode has a first electrode layer in contact with the base on the first surface, a second electrode layer covering the first electrode layer, and a plating layer covering the second electrode layer, each of the first electrode layer and the second electrode layer includes a plurality of fillers and a resin; A coil component, wherein a volume ratio of the filler in the second electrode layer is greater than a volume ratio of the filler in the first electrode layer.

2. The coil component according to claim 1 , wherein a volume ratio of the resin in the first electrode layer is greater than a volume ratio of the resin in the second electrode layer.

3. The coil component according to claim 1 , wherein an adhesive strength between the first electrode layer and the base is higher than an adhesive strength between the second electrode layer and the base.

4. The coil component according to claim 1 , wherein the ratio of the resin in the first electrode layer is 65 vol % or less.

5. The coil component according to claim 1 , wherein the plurality of fillers are made of a metal material.

6. The plurality of fillers include a first filler having a spherical shape and a second filler having a flat shape, The coil component according to any one of claims 1 to 5, wherein an aspect ratio of the first filler is 2 or less, and an aspect ratio of the second filler is 3 or more.

7. 7. The coil component according to claim 6, wherein, among the plurality of fillers in the second electrode layer, a ratio of the first filler is 40 vol% or more and 70 vol% or less, and a ratio of the second filler is 30 vol% or more and 60 vol% or less.

8. The coil component according to claim 1 , wherein at least a portion of the plurality of fillers contained in the second electrode layer is metallically bonded to the plating layer.

9. The coil component according to claim 1 , wherein the plating layer includes a first plating layer in contact with the second electrode layer and made of Ni.

10. The coil component according to claim 9 , wherein the first plating layer covers an entire outer surface of the second electrode layer.

11. The coil component according to any one of claims 1 to 10, wherein the resin is a thermosetting resin.

12. A substrate including a plurality of metal magnetic particles and a resin binder; an external electrode provided on a surface of the base body so as to be in contact with a first surface of the surface; a conductor electrically connected to the external electrode, wound around a coil axis inside the base, and having one end and the other end exposed from the first surface of the base, the external electrode includes a first electrode layer including a plurality of first fillers and a first resin, and the first surface is in contact with the base; a second electrode layer covering the first electrode layer and including a plurality of second fillers and a second resin; and a plating layer covering the second electrode layer; the first electrode layer, the second electrode layer, and the plating layer are stacked in a stacking direction, A coil component, in which, in a cross-sectional view cut along a plane extending parallel to the stacking direction, a ratio of an area of ​​the second filler to an area of ​​the second electrode layer is greater than a ratio of an area of ​​the first filler to an area of ​​the first electrode layer.

13. 13. The coil component according to claim 12, wherein in a cross-sectional view cut along a plane extending parallel to the stacking direction, a ratio of an area of ​​the first resin to an area of ​​the first electrode layer is greater than a ratio of an area of ​​the second resin to an area of ​​the second electrode layer.

14. A circuit board comprising the coil component according to any one of claims 1 to 13.

15. An electronic device comprising the circuit board according to claim 14.

Citation Information

Patent Citations

  • Surface-mounting electronic component and manufacturing method thereof

    JP2008085280A

  • Ceramic electronic component

    JP2008263013A

  • Conductive paste composition for external electrode and multilayer ceramic electronic component including the same

    JP2015023268A

  • Ceramic electronic component and method for manufacturing the same

    JP2015053495A

  • Surface-mounted inductor

    JP2017120809A