Magneto-optical memory interface
The magneto-optical memory interface addresses the integration limit of conventional interfaces by using electrically controlled magnetization changes in multiple magnetic recording cells, enabling high-density, non-volatile storage and reading of optical signals.
Patent Information
- Application Number
- JP2022553319
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-30
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2040-09-30
AI Technical Summary
Conventional magneto-optical memory interfaces are limited by the size of the memory cell to the wavelength or subwavelength of light, restricting the degree of memory integration and limiting their applications.
A magneto-optical memory interface with a structure that includes a plurality of magnetic recording cells, selected individually or in arbitrary numbers, using electric signals to control magnetization changes in response to light, and employing methods such as voltage effect, spin injection torque, thermal reduction of magnetic anisotropy, and optical writing to increase integration.
Enables high-density, non-volatile storage and reading of optical signals by controlling magnetization states, allowing for high integration and simplification of the memory interface structure.
Smart Images

Figure 0007563682000001 
Figure 0007563682000002 
Figure 0007563682000003
Abstract
Description
[Technical Field]
[0001] The present invention relates to a magneto-optical memory interface. [Background technology]
[0002] Technologies are being developed to record and read optical signals. For example, a research team at Oxford University has improved a phase-change optical memory cell and demonstrated a prototype optical memory that can record 32 states, equivalent to 5 bits, as described in Non-Patent Document 1. This type of optical memory is currently considered to have the highest recording density in the world. Optical signals are also used in electrical information processing circuits, so an interface that can convert optical signals into electrical signals at high speed and with high capacity is also required. If such an interface is available within an information processing chip, electronic circuits can directly receive optical signals, enabling high-capacity, high-speed, and low-power signal processing. In this case, it is important to develop a memory-type interface that can convert optical signals into electrical signals and temporarily store them.
[0003] As an example of a memory-type interface that converts optical signals into electrical signals and temporarily stores them, there is a known technology used in inter-chip optical interconnects, which achieves high-speed information transmission between chips using an externally prepared laser, as described in the following non-patent document 2. [Prior art documents] [Non-patent literature]
[0004] [Non-Patent Document 1] Li et al., Fast and reliable storage using a 5 bit, nonvolatile photonic memory cell, Optica, 6,1 (2019) [Non-patent document 2] H.Becker et al. Out-of-Plane Focusing Grating Couplers for Silicon Photonics Integration With Optical MRAM Technology, IEEE J. Selected topic in Quan. elec., 26, 8300408 (2020) Summary of the Invention [Problem to be solved by the invention]
[0005] The magneto-optical memory interface described in Non-Patent Document 2 has the function of directly transferring an optical signal propagating through an optical waveguide to the magnetization state of a magnetic tunnel junction and storing it non-volatilely, without using a photoelectric conversion element such as a photodiode. However, in conventional magneto-optical memory interfaces, the size of the memory cells is limited to the wavelength or subwavelength of light, making it theoretically impossible to increase the memory integration density, which limits the applications.
[0006] The present invention aims to provide a magneto-optical memory interface having a structure in which the size of a memory cell is not limited by the wavelength or subwavelength of light, and which makes it possible to increase the degree of integration of the memory. [Means for solving the problem]
[0007] (1) The magneto-optical memory interface of the present invention comprises a memory cell structure in which a plurality of magnetic recording cells are arranged, a selection means for selecting one or any number of the magnetic recording cells arranged in the memory cell structure individually and applying an electrical signal to the selected number of magnetic recording cells, and an optical signal irradiation unit for irradiating an optical signal to the any number of the magnetic recording cells arranged in the memory cell structure, wherein the magnetic recording cells are magnetic recording cells whose sensitivity to changes in their own magnetization state increases in response to the light irradiated from the optical signal irradiation unit, and the magnetic recording cells are magnetic recording cells whose magnetization state changes in response to the applied electrical signal caused by the light irradiated from the optical signal irradiating unit and selected by the selection means.
[0008] (2) In the magneto-optical memory interface of the present invention, it is preferable that the method of selecting the magnetic recording cell by applying the electrical signal is any one of a voltage effect reduction of magnetic anisotropy using a voltage signal, a spin injection torque using a current, a spin orbit torque, and a thermal reduction of magnetic anisotropy using a current.
[0009] (3) In the magneto-optical memory interface of the present invention, the change in the magnetization state is characterized by being one or more of the following: simultaneous rotation of magnetization in the magnetic layer provided in the magnetic recording cell, movement of magnetic domains, and movement of domain walls. (4) In the magneto-optical memory interface of the present invention, it is preferable to have a bias magnetic field applying means for improving the error rate with respect to changes in the magnetization state of the magnetic recording cells. (5) In the magneto-optical memory interface of the present invention, it is preferable that a plurality of the magnetic recording cells are arranged in a matrix in the memory cell structure.
[0010] (6) In the magneto-optical memory interface of the present invention, it is preferable that, among the plurality of magnetic recording cells arranged in a matrix, a reference-side selection signal line is connected to one side of the magnetic recording cells in each row arranged horizontally, and an opposite-side selection signal line is connected to the other side of the magnetic recording cells in each column arranged vertically, and that current can be freely applied to any of the magnetic recording cells of the memory cell structure by controlling the current flow to the reference-side selection signal line and the opposite-side selection signal line. (7) In the magneto-optical memory interface of the present invention, it is preferable that, of the reference side selection signal line and the opposing side selection signal line, the selection signal line closer to the optical signal irradiation unit is made of a transparent electrode line.
[0011] (8) In the magneto-optical memory interface of the present invention, it is preferable to have a read means having a magnetoresistive element with a transistor or a sensor for detecting a leakage magnetic field of a magnetic body provided in the magnetic recording cell.
[0012] (9) In the magneto-optical memory interface of the present invention, it is preferable to have one of the following: means for writing a signal corresponding to the size of a specific magnetic domain area into the magnetic layer of the selected magnetic recording cell; means for writing a signal corresponding to the size of a specific magnetic domain area corresponding to a plurality of pinning sites into the magnetic layer of the selected magnetic recording cell; and means for writing a signal corresponding to the size of a multi-value memory into the magnetic layer of the selected magnetic recording cell. [Effects of the Invention]
[0013] This embodiment can provide a magneto-optical memory interface that can transfer and store optical signals into a magnetized state with high density and non-volatility. The magnetization state is controlled by using either the voltage effect, the current effect including spin injection torque and spin orbit torque, or the thermal effect as an assisting technique for selecting the magnetic recording cell, and a signal can be written as information using a polarization-dependent optical writing technique, and the written information can be read. To read the written information, a method can be adopted in which the magnetoresistive effect or leakage magnetic field is detected by a magnetic sensor. In this embodiment, the size of the magnetic recording cell is not limited by the wavelength or subwavelength of light, allowing for high integration, and therefore has the advantage of being able to simplify the structure as a magneto-optical memory interface. [Brief explanation of the drawings]
[0014] [Figure 1A] 1 is a schematic diagram of a main configuration showing a first embodiment of a magneto-optical memory interface according to the present invention. [Figure 1B] 1B is a diagram showing an example of wiring incorporating the configuration shown in FIG. 1A. FIG. [Figure 2A] FIG. 1C is a diagram showing an example of the same wiring as in FIG. 1B. [Figure 2B] FIG. 2 is an explanatory diagram showing an example of the configuration of a magnetic recording cell in the magneto-optical memory interface according to the first embodiment. [Figure 3]These figures are for explaining an example of how the magnetization direction changes in the same magnetic recording cell due to the voltage effect and light irradiation. (a) is an explanatory diagram showing the initial magnetization direction in a free magnetic layer provided in a part of the magnetic recording cell. (b) is an explanatory diagram showing an example of the magnetization direction of the free magnetic layer when a voltage or current is applied. (c) is an explanatory diagram showing an example of the result when the perpendicular component of the magnetization of the free magnetic layer is driven by a circularly polarized signal. (d) is an explanatory diagram showing the magnetization direction of the free magnetic layer when the applied voltage or current is turned off. [Figure 4A] FIG. 10 is an explanatory diagram showing an example of a laminated structure suitable for a configuration in which the magnetization direction of a magnetic material is driven by irradiation with a circularly polarized light pulse in the magnetic recording cell. [Figure 4B] 4B is a graph showing the relationship between the polar Kerr rotation angle (°) and time (picoseconds) obtained in the stacked structure shown in FIG. 4A under the conditions of an in-plane magnetic field of 1 tesla, an optical single pulse energy density (approximately 1 mJ / cm), and a pulse width (approximately 120 fs). [Figure 5] FIG. 10 is an explanatory diagram showing an example of a stacked structure in which cell selection is possible by changing the magnetic anisotropy of the magnetic material due to the voltage effect using a voltage signal in the magnetic recording cell. [Figure 6] FIG. 10 is an explanatory diagram showing an example of a stacked structure in which cell selection is possible by changing the magnetization direction of a magnetic material due to spin injection torque using a current in the magnetic recording cell. [Figure 7] FIG. 10 is an explanatory diagram showing an example of a stacked structure in which cell selection is possible by changing the magnetization direction of a magnetic material due to spin orbit torque using a current in the magnetic recording cell. [Figure 8A] FIG. 10 is an explanatory diagram showing the direction of magnetization of the magnetic layer at the temperature in the standby state in an example of a stacked structure in the magnetic recording cell that allows cell selection by reducing magnetic anisotropy due to Joule heating using a current. [Figure 8B] FIG. 10 is an explanatory diagram showing the direction of magnetization in the example of the same laminated structure in a state where perpendicular magnetic anisotropy is reduced upon heating. [Figure 9A]This is an explanatory diagram showing a first example of a structure in the same magnetic recording cell that allows data to be written analogically in addition to cell selection, and shows the state in which the magnetic layer is divided into two magnetic domains, left and right, by a domain wall. [Figure 9B] FIG. 2 is an explanatory diagram showing a state in which a current is passed through the magnetic layer. [Figure 9C] FIG. 10 is an explanatory diagram showing the state in which the magnetic layer is irradiated with right-handed circularly polarized light. [Figure 9D] FIG. 10 is an explanatory diagram showing a state in which the magnetic domain wall in the magnetic layer has moved and the magnetic domain on the left side has expanded. [Figure 10A] FIG. 10 is an explanatory diagram showing a state in which a left-handed circularly polarized laser pulse is incident on the magnetic recording cell in a specific example of a stacked structure that allows analog data writing in addition to cell selection. [Figure 10B] FIG. 2 is an explanatory diagram showing a state in which a right-handed circularly polarized laser pulse is incident on the specific example of the same laminate structure. [Figure 11] FIG. 10 is an explanatory diagram showing a second example of a stacked structure in which data can be written in an analog manner in addition to cell selection in the magnetic recording cell. [Figure 12] FIG. 10 is an explanatory diagram showing an ICH pulse and RH measurement positions when an RH (Hall resistance)-ICH (channel current) loop is obtained in the second example. [Figure 13] FIG. 10 is an explanatory diagram showing an example of an RH-ICH loop obtained in the second example. [Figure 14] FIG. 10 is an explanatory diagram showing a circuit diagram when recording data applied to the magnetic recording cell is read using the magnetoresistive effect and when current assist or voltage assist is used. [Figure 15A] 2 is an explanatory diagram showing an example of an optical reservoir computer incorporating the first embodiment of the magneto-optical memory interface shown in FIG. 1; [Figure 15B] FIG. 15B is an explanatory diagram showing an example of a magneto-optical memory interface applied to the optical reservoir computer shown in FIG. 15A. [Figure 16] FIG. 2 is an explanatory diagram showing an example of a sensor for detecting a leakage magnetic field of a magnetic layer provided in a magnetic recording cell. [Figure 17] FIG. 10 is an explanatory diagram showing another example of a sensor for detecting a leakage magnetic field of a magnetic layer provided in a magnetic recording cell. DETAILED DESCRIPTION OF THE INVENTION
[0015] Hereinafter, an example of an embodiment of the present invention will be described in detail with reference to the accompanying drawings. Note that the drawings used in the following description may show characteristic portions enlarged for convenience in order to make the characteristics easier to understand. 1 and 2 show an example of a magneto-optical memory interface according to a first embodiment of the present invention, and the magneto-optical memory interface A in this example comprises an optical signal irradiating unit 1 and a memory cell structure 2 arranged to face the optical signal irradiating unit 1. Fig. 1A shows an example in which the memory cell structure 2 is arranged below the light emitting surface on the lower surface side of the rectangular plate-shaped optical signal irradiating unit 1. The optical signal irradiator 1 receives pulsed light transmitted from the optical transmission path 3, and emits, for example, spot-shaped irradiation light to a required region of the memory cell structure 2 provided opposite the optical signal irradiator 1. The optical signal irradiator 1 is known as a type of out-of-plane diffraction grating coupler, and can use an element that can convert the optical path of input light and generate circularly polarized light at the same time.
[0016] When right-handed circularly polarized irradiation light and left-handed circularly polarized irradiation light are transmitted from the optical transmission path 3, for example, the case where the right-handed polarized irradiation light causes the free magnetic layer described below to enter a specific magnetization state can be defined as "1," and the case where the left-handed polarized irradiation light causes the free magnetic layer described below to enter another specific magnetization state can be defined as "0." Here, information can be stored in the irradiation light irradiated from the optical transmission path 3 to the memory cell structure 2 via the optical signal irradiation unit 1. According to the above definition, information corresponding to the optical signals of "1" and "0" can be continuously or intermittently input from the optical signal irradiation unit 1 to the free magnetic layer of any of the magnetic recording cells described later in the memory cell structure 2, and the magnetic information of each free magnetic layer can be stored as electrical signal information.
[0017] 1B, in order to simplify the structure, the memory cell structure 2 has a plurality of reference-side selection signal lines 5 (five in FIG. 1) arranged to form each row aligned in the horizontal direction, and a plurality of counter-side selection signal lines 6 (five in FIG. 1) arranged to form each column aligned in the vertical direction. Therefore, the memory cell structure 2 shown in FIG. 1 has a structure in which five reference-side selection signal lines 5 and five counter-side selection signal lines 6 are arranged in a matrix form in a plan view. In the example of Figure 1B, five reference side selection signal lines 5 and five opposing side selection signal lines 6 are arranged, but in the case of an integrated circuit such as a microchip, a structure can be adopted in which the required number of fine width wirings, such as several thousand to several hundred thousand, are arranged in a matrix depending on the integration level of the circuit.
[0018] Both the reference side selection signal line 5 and the opposing side selection signal line 6 are connected to a signal line selector such as a decoder, which is omitted in the drawing, and are configured so that electricity can be freely applied to the reference side selection signal line 5 and the opposing side selection signal line 6 selected by the signal line selector as needed from a power source, not shown. 1, the reference-side selection signal line 5 is made of metal wiring, and the counter-side selection signal line 6 is made of transparent electrode wiring. Therefore, the irradiated light emitted from the optical signal irradiating unit 1 to the memory cell structure 2 passes through the counter-side selection signal line 6 and can reach the magnetic recording cells 8 (described later) arranged between the counter-side selection signal line 6 and the reference-side selection signal line 5. In this embodiment, the optical signal irradiation unit 1 is formed so as to be able to irradiate light in a spot form onto all of the intersections between the reference-side selection signal line 5 and the counter-side selection signal line 6, as exemplified in FIGS. 1B and 2A. Note that the range over which the optical signal irradiation unit 1 can irradiate light is not limited to this, and it may be configured so that light can be irradiated onto more intersections depending on the degree of integration of the signal lines, the optical signal irradiation unit, etc. Also, it is possible to provide multiple optical signal irradiation units 1 in accordance with the arrangement spacing and number of signal lines so that light can be irradiated. In other words, the optical signal irradiation unit 1 can be configured so as to be able to irradiate optical signals onto any number of magnetic recording cells 8.
[0019] In the magneto-optical memory interface A shown in FIG. 1A, magnetic recording cells 8 having a stacked structure, for example, as shown in FIG. 2B, are formed at the intersections of the reference-side selection signal lines 5 and the counter-side selection signal lines 6. The configuration in FIG. 1B shows an example in which five reference-side selection signal lines 5 and five counter-side selection signal lines 6 are provided, so there are 25 intersections of these signal lines, and magnetic recording cells 8 are provided at all of the intersections. For this reason, multiple magnetic recording cells 8 (25 cells) are arranged in the magneto-optical memory interface A of this embodiment. It is not necessary to provide a magnetic recording cell 8 at all of the intersections of the signal lines, and the required number of magnetic recording cells 8 can be provided.
[0020] The magnetic recording cell 8 has a cell selection element 9 such as a cell selection transistor or a cell selection diode, a magnetic tunnel junction 10, and an optical spin conversion layer 11 stacked on a reference-side selection signal line 5, and an opposing-side selection signal line 6 formed on the optical spin conversion layer 11. Therefore, the reference-side selection signal line 5 is connected to one side of the magnetic recording cell 8, and the opposing-side selection signal line 6 is connected to the other side of the magnetic recording cell 8. With the above structure, by passing current through a specific reference-side selection signal line 5 and a specific opposing-side selection signal line 6, it is possible to apply a voltage to a specific magnetic recording cell 8 located at the intersection of a specific reference-side selection signal line 5 and a specific opposing-side selection signal line 6, among the multiple magnetic recording cells 8 arranged in a matrix.
[0021] 1B, one side of each magnetic recording cell 8 in each row arranged in the horizontal direction is connected to one reference-side selection signal line 5. Also, one counter-side selection signal line 6 is connected to the other side of each magnetic recording cell 8 in each column arranged in the vertical direction. Therefore, by controlling the energization of each reference-side selection signal line 5 and each counter-side selection signal line 6, any number of magnetic recording cells 8 provided at each intersection can be selected and energized.
[0022] Note that a necessary number of insulating layers (not shown) are laminated between the reference-side selection signal line 5 and the counter-side selection signal line 6 and around each magnetic recording cell 8, thereby insulating the reference-side selection signal line 5 from the counter-side selection signal line 6 individually and also insulating adjacent magnetic recording cells 8 from each other. Note that when the cell selection element 9 is a cell selection transistor, control wiring is required to connect to the base of each cell selection transistor, but the corresponding control wiring is not shown in Figure 2. The control wiring is connected to a separately provided control wiring selector and is configured to be able to control the switching of any selected cell selection transistor as needed.
[0023] The magnetic tunnel junction 10 can have a structure in which an intermediate layer 15 acting as a tunnel barrier is interposed between the pinned magnetic layer 12 and the free magnetic layer 13. This structure allows the magnetic recording cell 8 to be selected by a voltage method, as shown in Figures 3(a) to 3(d), for example. As shown in FIG. 3(a), in the initial state with no voltage applied, the axis of easy magnetization of the free magnetic layer 13 is oriented perpendicular to the film surface of the free magnetic layer 13. Here, the direction of perpendicular magnetization is, for example, perpendicular and upward to the film surface of the free magnetic layer 13. If necessary, a weak magnetic field (bias magnetic field) may be applied in a direction parallel to the film surface of the free magnetic layer 13. The bias magnetic field can be generated by a bias magnetic field generating layer (not shown) disposed near the free magnetic layer 13. This bias magnetic field generating layer serves as a bias magnetic field applying means.
[0024] When a voltage is applied to the magnetic tunnel junction 10 using the reference-side selection signal line 5 and the counter-side selection signal line 6, the magnetic anisotropy of the free magnetic layer 13 disappears due to the voltage effect, and the magnetization direction of the free magnetic layer 13 rotates, for example, to a direction parallel to the film surface of the free magnetic layer 13, as shown in Figure 3(b). For example, it becomes the same direction as the bias magnetic field shown in Figure 3(b). Depending on the structure of the magnetic tunnel junction 10, the magnetic anisotropy can also be eliminated by the heating effect caused by applying a current.
[0025] Next, as shown in Figure 3(c), when the optical signal irradiator 1 irradiates the optical spin conversion layer 11 with light having a circularly polarized component (circularly polarized signal), the direction of magnetization can be rotated downward at a predetermined angle with respect to the film surface direction of the free magnetic layer 13 due to the influence of the circularly polarized signal. In other words, the perpendicular component of the magnetization can be driven. From this state, turning off (removing) the voltage applied by the reference-side selection signal line 5 and the counter-side selection signal line 6, or turning off (removing) the applied current, can result in a perpendicular magnetization state that is 180° different from the perpendicular magnetization direction in the initial state shown in Figure 3(a), as shown in Figure 3(d). In other words, the magnetization direction of the free magnetic layer 13 of the magnetic recording cell 8 itself changes when the applied electric signal is applied or removed.
[0026] 3(a) to 3(d), the magnetization direction of the free magnetic layer 13 can be changed to a plurality of directions, and therefore, before and after the change, the magnetic tunnel junction 10 can obtain different resistance states and different resistance values depending on the magnetization direction of the free magnetic layer 13 relative to the magnetization of the fixed magnetic layer 12. Therefore, by reading the resistance value according to the magnetization direction of the free magnetic layer 13, it is possible to record information in which high and low resistances are recorded as information "0" or "1." Once magnetic information is input, it is retained as is unless a voltage or current is applied, and is therefore non-volatile information.
[0027] In the magneto-optical memory interface A shown in Figures 1 and 2, right-handed or left-handed circularly polarized light is irradiated onto the memory cell structure 2, and an electrical signal is applied to the magnetic recording cells 8 to be written. As a result, the sensitivity of the magnetization state of the magnetic recording cells 8 is improved due to the previous circularly polarized light irradiation, so it is possible to change the magnetization state of the free magnetic layer 13 of only the selected specific magnetic recording cells 8. In other words, in response to the light irradiated from the light irradiating unit 1, the sensitivity of the free magnetic layer 13 of the magnetic recording cells 8 themselves that are hit by the irradiated light to changes in the magnetization state increases. The change in the magnetization state can be a simultaneous rotation of the entire magnetization of the free magnetic layer 13, as well as various magnetic domain and domain wall movements, which will be described later. The magnetic domain state is not limited to being represented by two types, "1" and "0," indicating whether or not the entire magnetization of the free magnetic layer 13 has rotated simultaneously, but can also be adopted as a magnetic domain state having multiple stable states, as will be described later.
[0028] When a voltage or current is applied to the magnetic recording cell 8 to read out the magnetic domain state of the free magnetic layer 13, a bias magnetic field may be applied as shown in FIG. 3 in order to improve the error rate. Furthermore, when reading out the magnetization state of the free magnetic layer 13 of the magnetic recording cell 8, it may be read out using an array (reading means) using a magnetoresistive element with a transistor. Alternatively, it may be read out using a magnetic sensor that detects a leakage magnetic field from the free magnetic layer 13 at a cross point without a transistor cell.
[0029] 4A is an explanatory diagram showing an example of a laminated structure in which the polar Kerr rotation angle changes when irradiated with a circularly polarized light pulse. For example, a non-magnetic metal layer (barrier layer) 18 made of MgO, a 2-nm-thick free magnetic layer (ferromagnetic layer) 19 made of an FeCo layer, and an optical spin conversion layer 20 made of Pt are laminated on a Si(100) / SiO2 substrate 17. As an example, the thickness of the non-magnetic metal layer 18 can be selected to be 2 nm, the thickness of the free magnetic layer 19 to be 1 nm, and the thickness of the optical spin conversion layer 20 to be 5 nm.
[0030] In the laminated structure shown in Figure 4A, when pulsed light is irradiated with left-handed or right-handed circularly polarized light, the polar Kerr rotation angle (the perpendicular component of magnetization) changes with time (picoseconds), as shown in the graph in Figure 4B. The conditions under which the change in the graph shown in Figure 4B can be obtained are, for example, an in-plane magnetic field of 1 tesla and an optical pulse energy density of approximately 1 mJ / cm. 2 , pulse width: about 120 fs. In the state where no voltage is applied, the polar Kerr rotation angle changes in the double layer of the free magnetic layer 19 made of a ferromagnetic layer and the non-magnetic metal layer 18.
[0031] As shown in the schematic diagram at the top of the graph in Figure 4B, irradiation with right-handed circularly polarized light sets the magnetization in an initial state with a component that is obliquely upward relative to the film surface of the free magnetic layer 19, from which the magnetization precesses over time. In contrast, as shown in the schematic diagram at the bottom of the graph in Figure 4B, irradiation with left-handed circularly polarized light sets the magnetization in an initial state with a component that is obliquely downward relative to the film surface of the free magnetic layer 19, from which the magnetization precesses over time.
[0032] FIG. 4B shows a typical magnetization precession excited by irradiating a bilayer of a free magnetic layer 19 and a non-magnetic metal layer 18 with circularly polarized pulses having different helicities for a predetermined period of time. By applying the stacked structure shown in FIG. 4(a) to the magnetic tunnel junction 10 shown in FIG. 2, it becomes possible to drive the perpendicular component of magnetization by irradiating left-handed or right-handed circularly polarized light as shown in FIG. 3(c).
[0033] In the example described based on Figures 1 to 4, a selection element 9 such as a cell selection transistor or a cell selection diode is used as a means for selecting the magnetic recording cell 8, but a selection element utilizing various phenomena described below may also be used as the selection element 9. The configuration shown in FIG. 5 shows an element having a structure in which a 3-nm-thick MgO layer (not shown), a 30-nm-thick chromium layer 25, a 0.8-nm-thick Fe layer 26, a 2.3-nm-thick MgO layer 27, and a 10-nm-thick Fe layer (ultra-thin Fe layer) 28 are stacked on an MgO (001) substrate (not shown). This device, known as an MgO-based tunnel junction (MTJ) device with an ultrathin Fe layer, is known to exhibit a large voltage-induced change in perpendicular anisotropy. Therefore, by using an element having the laminated structure shown in FIG. 5, a voltage-induced change that reduces magnetic anisotropy by a voltage signal can be used as a method for selecting the magnetic recording cell 8.
[0034] 6 is known as an example of a switching device that uses a magnetic tunnel junction (MTJ). In this structure, a barrier layer 30 is sandwiched between a pinned magnetic layer 31 and a free magnetic layer 32. A bit line 33 is connected to the free magnetic layer 32 side, and a source line 36 is connected to the pinned magnetic layer 31 side via a select transistor 35. A word line 37 is connected to the base of the select transistor 35. An example of a laminated structure is a laminated structure of SiO2 substrate / Ta(5) / Ru(10) / Ta(5) / CoFeB(1.0) / MgO(0.85) / CoFeB(1.7) / Ta(5) / Ru(5) / Cr / Au (numbers are film thicknesses in nm).
[0035] In the initial state, the magnetization direction of the free magnetic layer 32 is aligned in the film plane direction due to the influence of the magnetization direction of the pinned magnetic layer 31. However, by passing a current, STT (spin transfer torque) can be applied to the magnetization of the free magnetic layer 32, and when a threshold value is exceeded, the magnetization direction of the free magnetic layer 32 can be changed. By utilizing this phenomenon, the magnetization direction can be slightly changed when irradiated with right-handed circularly polarized light or left-handed circularly polarized light, making it easy to reverse the magnetization by circular polarization. Therefore, by using an element having the structure shown in FIG. 6, spin transfer torque using a current can be used as a method for selecting the magnetic recording cell 8.
[0036] The configuration shown in FIG. 7 is known as a spin-orbit torque induced switching device, which utilizes a current applied to a Ta channel 40 to generate a spin-orbit torque (SOT) acting on the free magnetic layer in the adjacent stack 41, thereby switching the magnetization. An example of a Ta channel and stacked structure is a stacked structure of Ta(10) / CoFeB(1.46) / MgO(1.8) / CoFeB(1.5) / Co(0.8) / Ru(0.92) / Co(2.7) / Ru(5) (numbers indicate film thickness in nm).
[0037] 7, the direction of the easy axis of magnetization can be selected from either the X-direction or Y-direction along the film surface of the stack, or the Z-direction as the thickness direction of the film surface. For example, in a structure in which the easy axis of magnetization is oriented in the Z-direction, a current is passed through the Ta channel 40 to generate a spin-orbit torque (SOT), which can change the magnetization direction of the free magnetic layer provided in the stack 41.
[0038] A circuit can be constructed by placing select transistors Tr1 and Tr2 at both ends of the Ta channel 40, connecting the bases of both transistors to the word line WL, connecting the top of the stack 41 to the read-side bit line RBL, and connecting the other terminals of both transistors to the write bit line WBL, thereby forming a switching device. Therefore, by using an element having the structure shown in Figure 7, the magnetization direction can be slightly changed when right-handed or left-handed circularly polarized light is irradiated, and magnetization reversal by circular polarization can be easily achieved, so that the spin-orbit torque caused by current can be used as a method for selecting the magnetic recording cell 8.
[0039] 8A and 8B show an example of the configuration of a switching device using a perpendicular magnetic tunnel junction and thermally induced reduction of magnetic anisotropy by current. In Figure 8A, the magnetic tunnel junction (MTJ) structure can be a seed layer / SAF layer / MgO barrier layer / free magnetic layer / cap layer structure. The SAF layer can be, for example, Ta(3) / Pt(5) / [Co(0.5) / Pt(0.4)]. x5 / Co(0.5) / Ru(0.9) / [Co(0.5) / Pt(0.4)] x3 / Co 60 Fe 20 B 20 The laminated structure of (1.5) (the numerical values indicate the film thickness in nm) can be adopted. 60 Fe 20 B 20 (1.2) / [Pd(1.2) / Co(0.3)] x38, a simplified model of an SAF layer (antiferromagnetic junction layer) 42, an MgO barrier layer 43, and a free magnetic layer 44 is shown.
[0040] As shown in Figure 8A, the material exhibits a large PMA (perpendicular magnetic anisotropy) at standby temperatures, but when current flows and heating occurs, the PMA decreases due to the influence of TIAR (thermally induced anisotropy reorientation), as shown in Figure 8B, and the magnetization of the free magnetic layer 44 becomes in-plane. In this state, by irradiating the material with right-handed or left-handed circularly polarized light, magnetization reversal by circular polarization can be achieved in a process similar to that of voltage application. Therefore, the element having the structure shown in FIGS. 8A and 8B can be used as a method for selecting the magnetic recording cell 8.
[0041] 9 and 10 are explanatory diagrams showing an example in which the magnetization state is changed not by the simultaneous rotation of magnetization in the free magnetic layer 13 as described above, but by the movement of domain walls by a current method. Figures 9 and 10 show a structure in which a magnetic domain wall 45A can move when a current is applied in a free magnetic layer 45 of a magnetic wire in which magnetic layers and other materials are stacked in a wire-like shape.The free magnetic layer 45 of the magnetic wire has two magnetic domains 46 and 47 on the left and right as shown in Figure 9A. As an example of a magnetic wire configuration, a magnetic wire having a laminated structure (numbers indicate film thickness) with six layers of Ta (3 nm) / Pt (5 nm) / Co (0.3 nm) / Ni (0.6 nm) / Co (0.3 nm) / Pt (2 nm) formed on a glass substrate can be applied.
[0042] Current is passed through the free magnetic layer 45 of the magnetic wire in the length direction (left and right direction in FIG. 9A) as shown in FIG. 9B, and the free magnetic layer 45 of the magnetic wire is heated by current. This current heating can lower the energy barrier that prevents the movement of the domain wall in the free magnetic layer 45 of the magnetic wire. However, the domain wall does not move simply by passing a current through the free magnetic layer 45 of the magnetic wire. The free magnetic layer 45 of the magnetic wire has, for example, a coercive force (Hc) of 35 Oe and a magnetic field of 770 emu / cm 3 The saturation magnetization (Ms) of
[0043] Here, while continuing current heating, if a right-handed circularly polarized laser pulse is irradiated onto the Pt surface layer on the surface of the magnetic wire as shown in Figure 9C, domain wall motion occurs due to thermal spin current drag, expanding magnetic domain 46 on the left and contracting magnetic domain 47 on the right. Next, if the current is turned off as shown in Figure 9D, the motion of domain wall 45A stops, resulting in a state in which magnetic domain 46 on the left expands and magnetic domain 47 on the right contracts as shown in Figure 9D. If the surface of the magnetic wire is irradiated with left-handed circularly polarized laser pulse light under similar conditions, the magnetic wall movement due to thermal spin current drag occurs in the opposite direction to that shown in Figure 9, resulting in a state in which magnetic domain 46 on the left side shrinks and magnetic domain 47 on the right side expands, as opposed to the case shown in Figure 9D. In this way, by selectively using right-handed circularly polarized light and left-handed circularly polarized light, the movement of magnetic domain wall 45A can be adjusted to either the right or left side.
[0044] Figure 10A shows a laminate 48 with a six-layer structure of Ta / Pt / Co / Ni / Co / Pt. It also shows a schematic diagram of the domain wall movement when the top surface of the laminate 48 is irradiated with a left-handed circularly polarized laser pulse. Figure 10B shows the domain wall movement when irradiated with a right-handed circularly polarized laser pulse. By selecting the appropriate laser pulse and applied current, the domain wall can be moved. This domain wall motion can be used to change the magnetization state of the free magnetic layer, as in the previous embodiment. According to the structure shown in Figures 9 and 10, the amount of domain wall motion can be controlled by adjusting the conditions for irradiating circularly polarized light and applying current. This means that not only can magnetic recording cells 8 be selected, but also analog information can be written.
[0045] 11 is an explanatory diagram showing an outline of a laminated structure in which a free magnetic layer 51 is laminated on an antiferromagnetic layer 50, thereby introducing multiple pinning sites into the free magnetic layer 51. In FIG. 11, the free magnetic layer 51 is divided into two specific magnetic domains 52 and 53, and a domain wall 51A is formed at the boundary between them. An example of a detailed stacked structure is Ta(3) / Pt(4) / PtMn(t PtMn ) / [Co(0.3) / Ni(0.6)]2 / Co(0.3) / MgO(1.2) / Ta(2) (the numerical values indicate the film thickness (unit: nm)). In this structure, the antiferromagnetic layer 50 is made of PtMn and the free magnetic layer 51 is made of MgO.
[0046] 11, the domain wall is pinned and does not move even when irradiated with right-handed circularly polarized light, as in the case shown in FIG. 9(c). When a current is applied, such as a SOT (spin-orbit torque) assist current or a STT (spin-transfer torque) assist current, the domain wall 51A moves only in the free magnetic layer 51 corresponding to the magnetic recording cell 8. As the domain wall 51A moves, the areas of the specific magnetic domains 52 and 53 expand or contract.
[0047] Figure 13 shows an example of the characteristics obtained by the above-mentioned laminated structure. As shown in Figure 12, the magnitude of I INT An initial pulse of I was applied to the stack, and after 0.5 seconds, the duration and magnitude of I CH A sequence of pulses is applied and the RH is measured after each pulse. In this case, the perpendicular magnetization is reversed only by the current-induced torque and the circularly polarized laser irradiation, and the RH at the midpoint of the loop is determined by I MAX It changes gradually with The fact that this result is obtained means that the structure of FIG. 11 not only allows selection of the magnetic recording cells 8 but also allows analog information to be written as a multi-valued memory. Furthermore, when the structure shown in FIG. 11 is adopted, optical signals can be recorded in a multi-value manner, which makes it possible to apply it to, for example, a brain-type information processing interface.
[0048] In the examples described so far, magnetic recording cells of the same structure are provided at all of the intersections between the multiple reference-side selection signal lines 5 and the multiple counter-side selection signal lines 6. However, magnetic recording cells of multiple different configurations may be applied to the intersections between the multiple reference-side selection signal lines 5 and the multiple counter-side selection signal lines 6. For example, two or more of the magnetic recording cell 8 employing the configuration shown in Figures 2 and 3, the magnetic recording cell employing the configuration shown in Figure 4A, the magnetic recording cell employing the stacked structure shown in Figure 5, the magnetic recording cell employing the stacked structure shown in Figure 6, the magnetic recording cell employing the stacked structure shown in Figure 7, the magnetic recording cell employing the stacked structure shown in Figure 8, the magnetic recording cell employing the stacked structure shown in Figure 9, the magnetic recording cell employing the stacked structure shown in Figure 10, and the magnetic recording cell employing the stacked structure shown in Figure 11 may be selected and applied to the intersection portion. When applying two or more types of magnetic recording cells, multiple light irradiation units 1 may be provided and a specific magnetic recording cell may be provided for each area to which each irradiation unit 1 irradiates an optical signal, or two or more types of magnetic recording cells may be applied to an area to which one light irradiation unit 1 irradiates an optical signal.
[0049] FIG. 14 is a circuit diagram showing the main part of a memory applicable to the magneto-optical memory interface of this embodiment. In the circuit diagram of Fig. 14, a plurality of memory cells 153, each of which is composed of a magnetic tunnel junction and a selection transistor Tr, denoted by reference numeral 111, are arranged in a matrix, for example. The magnetic tunnel junction 111 incorporated in the circuit shown in Fig. 14 is the magnetic tunnel junction shown in the previous embodiment, in which the sensitivity to the change in magnetization state is increased by a circularly polarized signal. 14, one terminal of the memory cells 153 belonging to the same column is connected to the same bit line 132, and the other terminal is connected to the same bit line 142. The gate electrodes (word lines) 139 of the select transistors Tr of the memory cells 153 belonging to the same row are connected to each other and further to the row decoder 151.
[0050] The bit line 132 is connected to a current source / sink circuit 155 via a switch circuit 154 such as a transistor. The bit line 142 is connected to a current source / sink circuit 157 via a switch circuit 156 such as a transistor. The current source / sink circuits 155 and 157 can supply a write current to the connected bit lines 132 and 142 or draw a write current from the connected bit lines 132 and 142.
[0051] The bit line 142 is also connected to a read circuit 152. The read circuit 152 may be connected to the bit line 132. The read circuit 152 includes a read current circuit, a sense amplifier, and the like. During a write, the switch circuits 154, 156 and the select transistor Tr connected to the memory cell to be written are turned on, forming a current path through the memory cell. Then, one of the current source / sink circuits 155, 157 functions as a current source and the other functions as a current sink depending on the information to be written. As a result, a write current flows in a direction corresponding to the information to be written.
[0052] In terms of writing speed, cell selection can be achieved by spin injection using a current with a pulse width of several nanoseconds to several microseconds synchronized with the circularly polarized signal, enabling current-assisted circularly polarized signal writing. In this case, magnetic anisotropy reduction due to current Joule heating or the spin-orbit torque effect can be used instead of spin injection. Furthermore, magnetic anisotropy reduction due to the voltage effect of a voltage signal source and sink can also be used instead of a current source and sink. During reading, a small read current that does not cause magnetization reversal is supplied to a designated MR element (magnetoresistive element) by a read current circuit, in the same manner as during writing. Then, the read circuit 152 determines the resistance state of the MR element (magnetoresistive element) by comparing the current value or voltage value resulting from the resistance value according to the magnetization state of the MR element (magnetoresistive element) with a reference value.
[0053] By applying a memory having the circuit shown in Figure 14, it is possible to provide a magnetic memory interface that can quickly transfer and store a signal corresponding to the helicity of the irradiated circularly polarized light into the magnetic state of a cell selected by current or voltage, and can also read it out.
[0054] Figure 15A shows an example of an optical reservoir computing system C to which the magneto-optical memory interface A configured as shown in Figures 1 and 2 can be applied. This optical reservoir computing system C is a device that mimics some of the functions of a biological brain. For example, research is being conducted into technology for object recognition through deep learning using deep neural networks with multi-layered structures. In neural networks, each node (corresponding to a nerve cell) weights the signal input to that node, outputs it through an appropriate nonlinear function, and propagates it to the next node. Changing this weighting to a signal appropriate for the input signal corresponds to learning.
[0055] The reservoir computing system learns by changing the weights only in the output layer, without changing the weights in the intermediate layer. The optical reservoir computing system C shown in Figure 15A performs this reservoir computing using optical circuits, enabling high-speed and low-power processing that exceeds that of electronic circuits.
[0056] The optical reservoir computing system C comprises an optical signal input means 60 , an optical modulator 61 , an optical input layer 62 , a reservoir layer 63 , a receiver 64 and an output layer 65 . Modulated light from optical signal input means 60 is multiplexed onto the light input to the optical path provided in optical modulator 61, and ultra-high speed, low power consumption processing that is difficult to achieve with electronic circuits is achieved in input layer 62, which has an optical filter function. Next, a wide variety of signals are generated in reservoir layer 63 using a simple optical loop circuit incorporating a nonlinear element. The resulting optical signal is input as an electrical signal from receiver 64 to electrical circuit 65, where it is recorded, allowing information to be recorded and stored.
[0057] In the optical reservoir computing system C, the optical signal received by the receiver 64 is converted into an electrical signal and sent to the output layer 65, which is an electrical circuit, for weighted learning. The magneto-optical memory interface A shown in Figure 15B, which has a configuration equivalent to that shown in Figures 1 and 2, can be applied to the receiver 64 and output layer 65. By applying the magneto-optical memory interface A to the optical reservoir computing system C, it is possible to significantly speed up the performance of the effect of being able to store part of the learning of brain functions and the results thereof. Therefore, it can be applied to a high-speed brain information processing interface.
[0058] FIG. 16 is an explanatory diagram showing an example of a sensor for detecting a leakage magnetic field of a magnetic material (free magnetic layer) provided in any of the magnetic recording cells described above. The magnetic sensor 70 shown in Fig. 16 is a thin-film stacked TMR (tunneling magnetoresistance) magnetic sensor in which a free magnetic layer (ferromagnetic thin film) 71, a tunnel layer (insulating thin film) 72, and a fixed magnetic layer (ferromagnetic layer) 73 are stacked. The tunnel layer 72 is an extremely thin insulating thin film with a thickness of about several nanometers that allows electrons to tunnel. The tunnel layer 72 is made of an MgO thin film or the like, and a stacked structure in which CoFeB layers are arranged on both sides of the tunnel layer can be used.
[0059] The direction of fixed magnetization in the pinned magnetic layer 73 is fixed in one direction within the film plane, as indicated by the reference numeral 74, and the direction of magnetization in the free magnetic layer 71 is affected by this and constrained to the direction indicated by the solid arrow in Figure 16. In contrast, when a signal magnetic field (leakage magnetic field) is applied, the direction of magnetization in the free magnetic layer 71 is affected by the direction of the signal magnetic field and rotates by a predetermined angle, as indicated by the dashed arrow. When a current is passed from the pinned magnetic layer 73 to the free magnetic layer 71, the electrical resistance value changes depending on the relative angular difference in the magnetization directions, and therefore this can be used as a magnetic sensor. To apply the magnetic sensor 70 to the magneto-optical memory interface A having the multiple magnetic recording cells described above, for example, multiple magnetic sensors 70 can be arranged on a substrate so that there is a one-to-one correspondence with the magnetic recording cores arranged in a matrix, and the magnetic information of each magnetic recording core can be read out using each magnetic sensor 70.
[0060] FIG. 17 is an explanatory diagram showing another example of a sensor for detecting a leakage magnetic field of a magnetic material (free magnetic layer) provided in any of the magnetic recording cells described above. 17 has a structure in which a soft magnetic yoke thin film 76, a nanogranular TMR thin film 77, and a soft magnetic yoke thin film 78 are sequentially arranged along the direction of current flow. The nanogranular TMR thin film 77 is disposed in the central gap between the rectangular soft magnetic yoke thin films 76 and 78. The nanogranular TMR thin film 77 is, for example, a multi-layer thin film made of a magnetic metal and an insulator such as an oxide or fluoride, and has a structure in which magnetic metal particles with a diameter of several nanometers are dispersed in isolation within the insulator. For example, in a (Co·Fe)-MgF system, a large magnetoresistance ratio can be obtained when the metal content of (Co·Fe) is in the range of 25 to 45 at %.
[0061] The soft magnetic yoke thin film 76 has been given uniaxial magnetic anisotropy perpendicular to the current flow direction by heat treatment in a magnetic field. When a signal magnetic field is applied from the outside parallel to the current flow direction, the magnetization of the soft magnetic yoke thin film 76 rotates in the direction of the magnetic field, generating magnetic flux. This magnetic flux is guided to the gap, and a magnetic field is applied to the nanogranular TMR thin film 77, changing the electrical resistance of the gap. By reading this change in electrical resistance, the film can function as a sensor. To apply the magnetic sensor 75 to the magneto-optical memory interface A having the multiple magnetic recording cells described above, for example, multiple magnetic sensors 75 can be arranged on a substrate so that there is a one-to-one correspondence with the magnetic recording cores arranged in a matrix, and the magnetic information of each magnetic recording core can be read out using each magnetic sensor 75. It should be noted that the sensor for reading the leakage magnetic field that can be applied to the magneto-optical memory interface A of this embodiment is not limited to the structures shown in FIGS. 16 and 17, and any known sensor capable of detecting a leakage magnetic field may of course be applied. 。 [Explanation of symbols]
[0062] A... magneto-optical memory interface, 1... light irradiation unit, 2... memory cell structure, 3...optical transmission path, 5...reference side selection signal line, 6...opposite side selection signal line, 8...magnetic recording cell, 9...cell selection element, 10...magnetic tunnel junction, 11...optical spin conversion layer, 12... fixed magnetic layer, 13... free magnetic layer, 15... intermediate layer, 17... substrate, 18...non-magnetic metal layer, 19...free magnetic layer, 20...optical spin conversion layer, 30...barrier layer, 31...fixed magnetic layer, 32...free magnetic layer 42...SAF layer (antiferromagnetic junction layer), 43...barrier layer, 44...free magnetic layer, 45...free magnetic layer, 45A...domain wall, 46, 47...magnetic domain, 50...antiferromagnetic layer, 51...free magnetic layer, 52, 53...specific magnetic domain, C...optical reservoir computing system, 60...optical signal input means, 61...optical modulator, 62...optical input layer, 63...reservoir layer, 64...receiver, 65...output layer, 70, 75...magnetic sensor, 111...magnetic tunnel junction, Tr...transistor.
Claims
1. 1. A magneto-optical memory interface comprising: a memory cell structure in which a plurality of magnetic recording cells are arranged; a selection means for selecting one or any number of the magnetic recording cells arranged in the memory cell structure and applying an electrical signal to the selected number of the magnetic recording cells; and a light irradiation unit for irradiating an optical signal to any number of the magnetic recording cells arranged in the memory cell structure, wherein the magnetic recording cells are magnetic recording cells whose sensitivity to changes in their magnetization state increases in response to light irradiated from the light irradiation unit, and the magnetic recording cells are magnetic recording cells whose magnetization state changes in response to an applied electrical signal resulting from the light irradiated from the light irradiation unit and selection by the selection means.
2. The magneto-optical memory interface of claim 1, characterized in that the method of selecting the magnetic recording cell by applying the electrical signal is any one of a reduction in magnetic anisotropy due to a voltage effect using a voltage signal, a spin injection torque using a current, a spin orbit torque, and a reduction in thermal magnetic anisotropy using a current.
3. 3. The magneto-optical memory interface according to claim 1, wherein the change in magnetization state is one or more of the following: simultaneous rotation of magnetization in a magnetic layer provided in the magnetic recording cell, movement of a magnetic domain, and movement of a magnetic wall.
4. 4. A magneto-optical memory interface according to claim 2, further comprising a bias magnetic field applying means for improving an error rate with respect to a change in the magnetization state of said magnetic recording cells.
5. 5. The magneto-optical memory interface according to claim 1, wherein a plurality of the magnetic recording cells are arranged in a matrix in the memory cell structure.
6. The magneto-optical memory interface of any one of claims 1 to 4, characterized in that, among the multiple magnetic recording cells arranged in a matrix, a reference side selection signal line is connected to one side of the magnetic recording cells of each row arranged in the horizontal direction, and an opposing side selection signal line is connected to the other side of the magnetic recording cells of each column arranged in the vertical direction, and current can be freely passed to any of the magnetic recording cells of the memory cell structure by controlling the current flow to the reference side selection signal line and the current flow to the opposing side selection signal line.
7. 7. The magneto-optical memory interface according to claim 6, wherein the selection signal line closer to the light irradiation unit out of the reference side selection signal line and the opposing side selection signal line is made of a transparent electrode line.
8. A magneto-optical memory interface as described in any one of claims 1 to 7, characterized in that it is provided with a reading means having a magnetoresistance element with a transistor or a sensor for detecting a leakage magnetic field of a magnetic material provided in the magnetic recording cell.
9. A magneto-optical memory interface as described in any one of claims 1 to 8, characterized in that it comprises either a means for writing a signal corresponding to the size of a specific magnetic domain area to the magnetic layer of a selected magnetic recording cell, a means for writing a signal corresponding to the size of a specific magnetic domain area corresponding to a plurality of pinning sites to the magnetic layer of a selected magnetic recording cell, or a means for writing a signal corresponding to the size of a multi-value memory to the magnetic layer of a selected magnetic recording cell.
Citation Information
Patent Citations
Optical assist type magnetic recorder
JP2009060057A
Nonvolatile optical memory, optical storage device, and network router
JP2012209382A
Spin polarization transistor element
WO2014027555A1