Method and device for controlling switching orbit in spin-orbit torque device

The MTJ device with an asymmetric shape and spin-orbit torque mechanism addresses thermal fluctuation-induced switching issues, enabling fast and reliable operation for non-volatile memory and logic circuits.

JP7563851B2Active Publication Date: 2024-10-08INTERNATIONAL BUSINESS MACHINE CORPORATION
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021574817
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-06-20
Filing Date
2020-06-05
Publication Date
2024-10-08
Estimated Expiration
2040-06-05

AI Technical Summary

Technical Problem

Existing three-terminal spintronic devices face challenges in achieving fast and reliable switching times due to thermal fluctuations and write error rates, and there is a need for non-volatile memory and logic circuits that can be placed in close proximity to the logical core in modern computing systems.

Method used

A magnetic tunnel junction (MTJ) device with a spin-orbit torque (SOT) generating layer and asymmetrically shaped magnetic layers, where the magnetization of the second magnetic layer has an in-plane component perpendicular to the current direction, enabling deterministic switching without thermal fluctuations.

Benefits of technology

The device achieves high-speed switching with reduced write error rates and allows for the construction of non-volatile logic circuits, such as inverters, NAND, and NOR gates, by leveraging spin-orbit torque without requiring external magnetic fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007563851000005
    Figure 0007563851000005
  • Figure 0007563851000006
    Figure 0007563851000006
  • Figure 0007563851000007
    Figure 0007563851000007
Patent Text Reader

Abstract

A method for controlling switching trajectories in a spin-orbit torque device, the device being a three-terminal device including a magnetic tunnel junction (MTJ) and a spin-orbit torque (SOT) generating layer. The MTJ has a first magnetic layer, a tunnel barrier layer below the first magnetic layer, and a second magnetic layer below the tunnel barrier, with the SOT generating layer directly below the second magnetic layer. The second magnetic layer has an asymmetric shape such that the average magnetization of the remanent state associated with the second magnetic layer has an in-plane component perpendicular to the direction of current flow in the SOT generating layer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to the field of memory and logic devices, and more particularly to non-volatile spintronic memory and logic devices and circuits that use the spin-orbit torque phenomenon to switch the magnetization of adjacent magnetic layers. [Background technology]

[0002] There is currently much interest in three-terminal spintronic devices as potential non-volatile alternatives to charge-based semiconductor devices in high-speed cache memories (such as static random access memories (SRAMs)). The write mechanism is based on the controlled manipulation of the magnetic moment using spin transfer torque (STT) generated via spin-orbit interaction. One approach to three-terminal magnetic memory devices is the one-domain wall racetrack memory element, based on current-induced motion of the domain walls of a nanoscopic wire. A second approach is to use SOT to switch the magnetization of adjacent magnetic nanoelements. One mechanism for reading the magnetic state in either type of device uses magnetic tunnel junctions (MTJs) based on the tunneling magnetoresistance (TMR) effect. Other read mechanisms include the anomalous Hall effect.

[0003] Although they have a larger overall footprint than conventional two-terminal spin transfer torque magnetic random access memory (STT-MRAM) MTJ devices, these three-terminal devices may be advantageous for high-speed memory applications. Separating the read and write paths in three-terminal devices makes optimization of materials and individual read and write schemes much more tractable. In addition, one of the degradation mechanisms in conventional STT-MRAM MTJ devices is the dielectric breakdown of the tunnel barrier, which occurs when the large voltages required for high-speed operation are applied across the tunnel barrier during the write process. This degradation mechanism is absent in three-terminal devices because the read and write paths are separated.

[0004] These three-terminal devices are primarily based on switching of magnetic nanoelements using spin-polarized currents generated in a nearby non-magnetic metal layer by the spin Hall effect. The spin Hall effect converts the longitudinal charge flow into a transverse spin current. For high-speed cache memory applications, alternative devices with both reliable operation and fast switching times are needed. In a conventional three-terminal device configuration, the current-induced spin polarization and the magnetic easy axis are coplanar and collinear with each other. Although deterministic switching can be achieved in this configuration, fast and reliable operation on short time scales is difficult to achieve because thermal fluctuations are required to initiate the switching process. This phenomenon is well known in conventional two-terminal STT-MRAM devices, leading to a so-called "write error rate" with switching times of less than 10 ns.

[0005] In modern computing systems utilizing complementary metal-oxide semiconductor (CMOS) technology, the devices used to perform computational tasks near the logic core, including register files, cache memories, and main memory, are all volatile. Therefore, the digital information held in these devices must be transferred to peripheral nonvolatile memory circuits. This data transfer process causes a significant amount of propagation delay. Furthermore, the access speed of these nonvolatile devices is significantly slower than the access speed of memory located near the logic core. Thus, there is a need for high-speed nonvolatile memory and logic circuits that can be placed in close proximity.

[0006] SUMMARY OF THE PRESENT EMBODIMENTS Embodiments of the present invention seek to improve upon the systems and methods of the prior art. Summary of the Invention

[0007] In one aspect, the invention provides a three-terminal device including: (a) a magnetic tunnel junction (MTJ), the MTJ including: (i) a first magnetic layer, (ii) a tunnel barrier layer underlying the first magnetic layer, and (iii) a second magnetic layer underlying the tunnel barrier; and (b) a spin-orbit torque (SOT) generating layer, the SOT generating layer immediately underlying the second magnetic layer, wherein the second magnetic layer has an asymmetric shape and an average magnetization of the remanent state associated with the second magnetic layer has an in-plane component orthogonal to the current direction in the SOT generating layer.

[0008] In another aspect, the present invention provides a device including: (a) a first magnetic tunnel junction (MTJ), the first MTJ including: (i) a first magnetic layer, (ii) a first tunnel barrier layer below the first magnetic layer, and (iii) a second magnetic layer below the tunnel barrier; (b) a second magnetic tunnel junction (MTJ), the second MTJ including: (i) a third magnetic layer, (ii) a second tunnel barrier layer below the first magnetic layer, and (iii) a fourth magnetic layer below the tunnel barrier; and (c) a common spin-orbit torque (SOT) generating layer, the common SOT generating layer being directly below both the second magnetic layer of the first MTJ and the fourth magnetic layer of the second MTJ, wherein the SOT generated in the common SOT generating layer sets a first magnetic state in the second magnetic layer and a second magnetic state in the fourth magnetic layer, the first magnetic state being opposite to the second magnetic state.

[0009] In yet another aspect, the invention provides a method comprising: (a) providing a three-terminal device including, in order, a spin-orbit torque (SOT) generating layer, an in-plane magnetized free layer whose magnetic moment can be switched by a spin transfer torque generated by the SOT generating layer, a tunnel barrier, and a reference magnetic layer whose orientation remains fixed during operation of the device, wherein a write plus terminal and a write minus terminal are in electrical contact with opposite ends of the SOT generating layer, a read terminal is in electrical contact with the reference magnetic layer, and the magnetic free layer has an asymmetric shape such that the average magnetization of the remanent state of the free layer has an in-plane component orthogonal to the current direction; and (b) passing a current between its terminals along the SOT generating layer, thereby switching the magnetic state of the magnetic free layer in the absence of an applied magnetic field when the direction of the passed current is oriented along the easy axis of the magnetic free layer.

[0010] The present disclosure will be described in detail with reference to the following figures, according to one or more various examples. The drawings are provided for illustrative purposes only and merely illustrate examples of the present disclosure. These drawings are provided to facilitate the reader's understanding of the present disclosure and should not be considered as limiting the breadth, scope, or applicability of the present disclosure. Please note that for clarity and ease of illustration, these drawings are not necessarily drawn to scale. [Brief description of the drawings]

[0011] [Figure 1A] Schematic of a three-terminal SOT device in Dxx configuration, where the easy axis of the magnetic nanoelement is along the x-direction and the current Ix is collinear with the easy axis direction. [Figure 1B] Schematic of a three-terminal SOT device in a Dxy configuration, where the easy axis of the magnetic nanoelement is along the x-direction and the current Iy is perpendicular to the easy axis direction. [Figure 1C] FIG. 2 is a schematic diagram of a preferred embodiment of the present invention in which magnetic nano-elements have an asymmetric shape. [Figure 2A] FIG. 13 shows time-resolved magnetization maps from micromagnetic simulations showing the absence of switching in the Dxx configuration when a 500 ps long positive current pulse is applied to the W(O) layer. [Figure 2B] FIG. 1 shows current pulses used in a micromagnetic simulation. [Figure 3A] Figure 14 shows time-resolved magnetization maps from micromagnetic simulations showing current-induced switching in a right-angle trapezoidal pattern element with a negatively slanted left leg (Dxx-), where current-induced switching from the +x state occurs for positive and negative currents, respectively, after application of a 500 ps current pulse. [Figure 3B] Figure 14 shows time-resolved magnetization maps from micromagnetic simulations showing current-induced switching in a right-angle trapezoid pattern element with a negative slanted left leg (Dxx-), where current-induced switching from the -x state occurs for positive and negative currents, respectively, after application of a 500 ps current pulse. [Figure 4] (A) and (B) are diagrams showing the remanent state magnetization configurations of a defect-free rectangular Dxx device for +x and -x magnetization directions, respectively; (C) and (D) are diagrams showing the final state magnetization maps after application of a 500 ps current pulse for positive and negative polarity current pulses, respectively; (E) is the average magnetization map under positive and negative current pulses. <mx>is the change over time. [Diagram 5] (A) and (B) are diagrams showing the remanent state magnetization configurations of a rectangular Dxx device with a defect at the bottom left edge for +x and -x magnetization directions, respectively; (C) and (D) are diagrams of the final state magnetization maps after application of a 500 ps current pulse for positive and negative polarity current pulses, respectively; (E) is the average magnetization map under positive and negative current pulses. <mx>is the change over time. [Figure 6] (A) and (B) are diagrams showing the remanent state magnetization configurations of a rectangular Dxx device with a defect at the top left edge for +x and -x magnetization directions, respectively; (C) and (D) are diagrams showing the magnetization maps of the final state after applying a 500 ps current pulse for positive and negative polarity current pulses, respectively; (E) is the average magnetization map under positive and negative current pulses. <mx>is the change over time. [Figure 7] (A) and (B) are the magnetization configurations of the remanent state of a rectangular Dxx device with symmetric defects for +x and -x magnetization directions, respectively, showing the stabilization of the C-state; (C) and (D) are magnetization maps of the final state after application of a 500 ps current pulse for positive and negative polarity current pulses, respectively; (E) is the average magnetization under positive and negative current pulses. <mx>FIG. [Figure 8A] Dxx-devices for various current pulses <mx>FIG. [Figure 8B] FIG. 1 shows current pulses and magnetization versus time for a 200 ps case, outlining the four-stage magnetization reversal process. [Figure 9] (A) is a diagram of the initial magnetization configuration of a right-angle trapezoidal device Dxx type calculated by micromagnetic simulation, (B) is a magnetization map showing the time evolution of magnetization for a non-switching event with a current pulse width of 100 ps, ​​and (C) is a magnetization map showing the time evolution of magnetization for a switching event with a current pulse width of 200 ps. [Figure 10A] Dxy device for various current pulses <mx>FIG. [Figure 10B] This figure shows a magnetization map showing the time variation of magnetization for a switching event with a current pulse of 600 ps. [Figure 11A] 13 is an SEM image of Dxx-devices patterned in the form of right-angled trapezoids. [Figure 11B] 13 is an SEM image of a Dxx+ device patterned in the form of a right-angled trapezoid. [Figure 11C] FIG. 14 shows the remanent state magnetization calculated from micromagnetic simulations for Dxx-devices. [Figure 11D] FIG. 14 shows the remanent state magnetization calculated from micromagnetic simulations for a Dxx+ device. [Figure 12A] FIG. 1 shows RH loops measured for a Dxx− device, with the insets indicating the orientation of the magnetization of the reference and free layers. [Figure 12B] FIG. 1 shows RH loops measured for a Dxx+ device, with the insets indicating the orientation of the magnetization of the reference and free layers. [Figure 12C] FIG. 1 shows RI loops measured for a Dxx− device, with the infix symbols indicating the orientation of the magnetization of the reference and free layers. [Figure 12D] FIG. 1 shows RI loops measured for a Dxx+ device, with the infix symbols indicating the orientation of the magnetization of the reference and free layers. [Figure 13A] Dxx- A truth table summarizing the conditions for switching and non-switching for devices. [Figure 13B] 1 is a truth table summarizing the conditions for switching and non-switching for Dxx+ devices. [Figure 14] FIG. 13 is a schematic diagram of a nonvolatile inverter (NOT gate) circuit realized with mirror image Dxx− and Dxx+ devices connected in series and sharing a common W(O) layer. [Figure 15A] FIG. 1 is an equivalent circuit diagram of a non-volatile (NOT gate) inverter circuit in a write mode. [Figure 15B] FIG. 1 is an equivalent circuit diagram of a non-volatile (NOT gate) inverter circuit in a read mode. [Figure 15C] FIG. 2 illustrates a non-limiting implementation of a NAND gate in write mode. [Figure 15D] FIG. 2 illustrates a non-limiting implementation of a NAND gate in read mode. [Figure 15E] FIG. 2 illustrates a non-limiting implementation of a NOR gate in write mode. [Figure 15F] FIG. 2 illustrates a non-limiting implementation of a NOR gate in read mode. [Figure 16] 2 is a truth table illustrating the operation of a nonvolatile inverter. [Figure 17] Experimental demonstration of inverter operation based on series connection of Dxx- and Dxx+ devices. The input voltage, the resistance of both devices, and the output voltage are plotted as a function of the iteration number. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Although the present invention has been shown and described in a preferred embodiment, the present invention can be produced in many different configurations. Although preferred embodiments of the present invention are shown in the drawings and described in detail herein, it should be understood that the present disclosure should be considered as an illustration of the principles of the present invention and the functional specifications associated with its configuration, and is not intended to limit the present invention to the illustrated embodiment. Those skilled in the art will envision many other possible variations within the scope of the present invention.

[0013] It should be noted that references herein to "one embodiment" or "an embodiment" mean that the referenced feature is included in at least one embodiment of the invention. Moreover, separate references herein to "one embodiment" do not necessarily refer to the same embodiment, but such embodiments are not mutually exclusive unless so stated or readily apparent to one of ordinary skill in the art. Thus, the present invention can include any various combinations and / or integrations of the embodiments described herein.

[0014] FIG. 1A shows a schematic three-terminal device configuration for switching magnetic nano-elements by spin-orbit torque. This three-terminal configuration is a type D xx where the first subscript indicates the easy axis of the magnetic nanoelement and the second subscript indicates the direction of the current flow. The magnetic nanoelement to be switched forms part of the MTJ structure, and the magnetic nanoelement is in direct contact with the layer that produces the SOT upon application of current. This layer is referred to throughout as the spin-orbit layer.

[0015] The three-terminal device 100 includes (a) a magnetic tunnel junction (MTJ) 102 including (i) a first magnetic layer 104, (ii) a tunnel barrier layer 106 below the first magnetic layer 104, and (iii) a second magnetic layer 108 below the tunnel barrier 106, and (b) a spin-orbit torque (SOT) generating layer 110 directly below the second magnetic layer 108. In FIG. 1A, the magnetization direction of the MTJ and the current-induced spin polarization direction of the SOT generating layer are orthogonal to each other. Also, in FIG. 1A, a first contact and a second contact are disposed on both ends of the SOT generating layer 110, and a third contact is disposed on the first magnetic layer 104.

[0016] Examples of materials for use in the first magnetic layer include synthetic antiferromagnetic layers composed of, for example, a CoFe-based alloy separated by a Ru layer, and an exchange bias layer in which a thin ferromagnetic layer of a CoFe-based alloy is placed adjacent to an antiferromagnet such as IrMn or PtMn. The tunnel barrier is typically composed of MgO, and the second magnetic layer is also composed of a CoFe-based alloy. Non-limiting examples of materials for use in the magnetic layers include CoFe alloys (e.g., CoFeB) and NiFe alloys (e.g., NiFeB). 80 Fe 20 ) are included.

[0017] The spin-orbital layer has two ends electrically connected, and when a voltage source is applied, a current (I x ) travels in a direction parallel to the easy axis of the adjacent magnetic free layer, generating a spin-orbit torque (SOT) in the magnetic layer. This conductive channel is the write path. The mechanism behind SOT generation in the device is due to the spin-Hall effect, which occurs in heavy metals such as Pt, W, and Ta and their alloys. In a non-limiting example, the SOT generation layer is an oxygen-doped tungsten layer W(O) formed by reactively sputtering a thin tungsten film in the presence of oxygen. This material has been experimentally demonstrated to result in a spin-Hall angle of -50%. A third terminal of the device is connected to the top of the MTJ, allowing the resistance state of the MTJ to be identified by magnetoresistance readout from the tunneling magnetoresistance effect. Readout can be achieved by passing a current through either of the write terminals and through the terminal connected to the top of the MTJ. In a preferred embodiment, a current pulse of sufficient current density and nanosecond timescale is applied to the write channel, and depending on the direction of the current, the magnetic state of the MTJ can be set along with the subsequent resistance state.

[0018] For comparison, FIG. 1B shows a prior art method for switching a magnetic nanoelement in a three-terminal configuration. This three-terminal configuration is referred to as Type D. xy It is written as follows.

[0019] D xx In type I devices, when the SOT is first applied, the magnetization and the current-induced spin polarization are orthogonal to each other. xy In the device (Fig. 1B), the initial magnetization and spin polarization are collinear with each other. xx In our device, switching is not expected to occur because the SOT only rotates the magnetization toward the in-plane hard axis (±y direction). xx When the current through the W(O) layer of the device is removed, the magnetization rotates back towards its initial orientation.

[0020] 1C shows a schematic diagram of a preferred embodiment of the invention in which the magnetic nano-elements have an asymmetric shape such that the average magnetization of the remanent state has an in-plane component perpendicular to the current direction. In a preferred embodiment, the current direction and the easy axis of the magnetic nano-element are collinear.

[0021] FIG. 2A shows this in relation to the D under a 500 ps long positive current pulse shown in FIG. 2B. xx We demonstrate this by time-resolved micromagnetic simulation of SOT switching in a 200 nm × 100 nm device in a 300 nm × 300 nm configuration. In this simulation, the SOT is modeled as a damping-like torque originating from the spin Hall effect. As expected, the micromagnetic simulation shows that the magnetization is aligned along the in-plane hard axis (±I x The current flows in the y-direction (±y direction, respectively) (upper right panel of Fig. 2A). The damping-like contribution of the SOT (

number

number

number

number

[0022] Although these simulations are performed in the zero-temperature limit, it is possible that thermal fluctuations at finite temperatures could drive magnetization reversal because the energy barrier that rotates the magnetization toward the ±x directions is suppressed when the magnetization is in the hard-axis direction. However, such a reversal mechanism is stochastic and not useful for technological applications. Therefore, D xy and D. xx The role of thermal fluctuations in the device switching process is complementary. xy In our device, thermal fluctuations are responsible for the initiation of the switching dynamics, but as the magnetization precession cone angle increases for reversal, the magnitude of the SOT increases, driving the reversal process. D xx In the device, the SOT initiates the switching process, while thermal fluctuations set the initial bias point for magnetization reversal that occurs after applying a current through the W(O) layer.

[0023] Based on this understanding, when the magnetization is in the intermediate hard axis state due to SOT, if there is an internal magnetic field that triggers the reversal process, D xx Deterministic switching can occur in the configuration, and therefore fast switching can be achieved without the need for thermal fluctuations either at the beginning or midpoint of the switching trajectory.

[0024] Figures 3A-B show micromagnetic simulations of a magnetic nanoelement with a shape of a right-angled trapezoid, with the same current pulse applied as in Figure 2B. The micromagnetic simulations show that the magnetization rotation under SOT towards the in-plane hard axis direction is larger in the wider part of the trapezoid, while the magnetization in the narrower part of the trapezoid tries to orient tangentially to the boundary of the nanoelement (500 ps time frame in Figures 3A-B). This occurs because the shape anisotropy energy density is larger in the narrower part of the trapezoid. Depending on the polarity of the current pulse, the magnetization at the tip of the trapezoid has a component either along or opposite to the initial magnetization direction (Figures 3A-B show ±I x (The magnetization at 500 ps is compared for 100 ps.) The preferred moment orientation is determined by the internal effective magnetic field of the nanoelement, which originates primarily from magnetostatic and exchange interactions.

[0025] This can also be observed in the remanent state of the nanoelement, where the magnetization of the slanted edge of the trapezoid correlates with the magnetization state of the rectangular region. Reversal of the magnetization can occur due to the growth of the domain starting from the top left corner upon removal of the current pulse. If the magnetization has a component along the same direction as the initial state of the trapezoid tip, no switching occurs. A similar argument applies when the magnetization starts from a -x orientation, where reversal occurs only with negative currents (Figure 3B). Moreover, for a right-angle trapezoid with a positive slope on the left leg, the current required to switch to the ±x configuration is ±I x The magnitude of the switching current is equivalent to switching to the ±x state in this mechanism. Therefore, by designing the geometry of the sample such that an internal magnetic field can initiate the reversal process, we can achieve deterministic switching with controlled switching current polarity without an external magnetic field. xx This can be achieved in a device.

[0026] In fact, even the presence of small everyday lithography defects caused by line edge roughness can cause D xx This has a significant enough effect on the microscopic magnetic state in the configuration to affect its switching dynamics. To illustrate this, a 200 nm × 100 nm D xx We consider three different magnetic nanoelements of configuration. In the first case (Figures 4(A)-4(E)), the nanoelement is a perfect rectangle, whereas in the other two cases, a defect is introduced in the form of a missing voxel of size 6 nm x 6 nm in either the bottom left (Figures 5(A)-5(E)) or top left (Figures 6(A)-6(E)) corner of the nanoelement. Each figure (Figures 4(A)-4(B), Figures 5(A)-5(B), Figures 6(A)-6(B)) shows the relaxed state of the magnetization of each structure. In the following description, these devices will be referred to as Devices #1, #2, and #3.

[0027] In the relaxed state of device #1, the moment curls towards the edge due to the effect of the demagnetizing field, but the net magnetization along the y axis remains constant. <m y > is zero. When a current pulse is applied to the W(O) layer, a damping-like torque from the SOT rotates the magnetization temporarily toward a direction perpendicular to the easy axis. When the current pulse is removed, the positive (+I x ) and negative (-I x As shown in the final state of the magnetization upon application of a current pulse of 1000 s (Figures 4(C) and 4(D), respectively), the magnetization relaxes toward the easy axis with the same orientation as in the initial state of the nanoelement. This dynamic process is <m x > (Figure 4(E)). When the SOT orthogonalizes the magnetization to the easy axis, there is no switching because there is no additional torque causing the magnetization to rotate.

[0028] For device #2 (Figure 5(A)-(B)), a defect has been introduced in the bottom left corner, and the relaxed magnetization state has a finite m in the form of an edge domain of the nanoelement. y The relaxation state shown here is called the S state. y The components are m x Note that the S-state is correlated with the component states (i.e., the S-state has two different orientations). This S-state is stabilized by a defect arrangement that induces an internal static magnetic field and breaks the symmetry along the y-axis. Upon application of a current pulse, the magnetization rotates towards the spin accumulation direction. However, the demagnetizing fields induced from the edge geometric defects provide an additional torque to drive the reversal. Thus, switching is observed upon removal of the current pulse (Fig. 5(C)). In the case of the opposite current pulse polarity (Fig. 5(D)), the internal magnetic field acts in the +x direction and no switching is observed. The time evolution of the magnetization during this switching process is summarized in Fig. 5(E). Here, the “quasi-ballistic” nature of the switching process is also clearly visible.

[0029] For device #3, the defects are located at the opposite edge, so the orientation of the internal static magnetic field is opposite. Note that the orientation of the S state in the remanent state of magnetization is opposite to that in the second case (Figures 6(A) and 6(B)). As a result of the location of the defects, not only are the remanent states different, but the switching behavior with respect to current polarity is reversed (Figures 6(C)-6(E)). Thus, the location of these small lithographic defects is important in influencing both the remanent state and the polarity of the switching current, as well as its overall switching trajectory.

[0030] D xx A notable feature of the switching process is that the switching process occurs in a 100-nm direction (as is evident from the magnetization time plots (Figures 5(E) and 6(E))). <m x >, but is characterized by a coherent rotation of the moment throughout the free layer. In contrast, D xy The device is <m x > exhibits a non-monotonic variation in time, as well as non-coherent inversions involving many metastable states. As a result, the switching time is xx Compared to D xy It is possible that it will be much longer.

[0031] Note also that no switching occurs if the defects are symmetrically placed with respect to the device geometry and share a common edge. Furthermore, note that no switching occurs if the trapezoid is perfectly symmetric with respect to the x-axis, since the magnetizations at the two edges of the nanoelement rotate in opposite directions. In this case, the magnetization in the remanent state corresponds to the C-state (Figures 7(A)-7(B)). Thus, the edge domains point in opposite directions both in the remanent state and upon application of a current pulse. When a current pulse is applied to the spin-orbital layer, the demagnetizing fields induced by the defects exert opposite torques on the edges of the nanoelement. Thus, the net m generated at the end of the current pulse is x There is no component and no switching occurs (FIGS. 7(C) to 7(E)).

[0032] The micromagnetic simulation also shows the magnetization of nano-elements versus time. <m x Based on this mechanism, the D xx The switching process is xy The switching process may be faster than that of the right-angle trapezoidal devices (especially the D xx- To understand the switching dynamics on fast time scales of the MOSFETs (device type), we performed micromagnetic simulations. For current flowing in the +x direction, we calculated the spatial average of the normalized magnetization component in the x direction for various current pulses with current pulse widths ranging from 100 ps to 400 ps. <m x > as a function of time is plotted in Fig. 8A. The initial state of magnetization in each simulation is primarily oriented in the x direction, as shown in the snapshot from the micromagnetic simulation in Fig. 9(A).

[0033] The switching process occurs through four steps that can be identified from the time traces and are delimited for the case of a 200 ps current pulse (Fig. 8B). 1) The magnetization first rotates from +x-direction towards +y-direction through the SOT. 2) After 200 ps, ​​when the current is removed, the magnetization acquires a small component in the opposite direction, as explained in the text, due to the shape anisotropy induced by the right-angled trapezoid. 3) The reversal of the magnetization occurs by the growth of the domain wall. 4) The magnetization relaxes to its final equilibrium state through precession about its equilibrium state. Using this mechanism, fast switching with pulse widths as short as 150 ps (see solid black line in Fig. 8A) can be achieved. Furthermore, it is noted that the switching is “quasi-ballistic” and the switching is achieved within almost one precession cycle. However, the relaxation of the magnetization in step 4) is deterministic, although it involves some precession. Unlike other fast time scale switching schemes that use non-collinear moments, this scheme is insensitive to the width of the current pulses used once the current pulses exceed a critical pulse width.

[0034] Figures 9(B) and 9(C) compare the switching dynamics for non-switching and switching events. For a current pulse width of 100 ps where no switching occurs, the magnetization rotates towards the +y direction due to SOT, but does not have enough time to reorient completely perpendicular to the current direction. As a result, the magnetization does not develop a component along the reversal direction at the end of the current pulse. The return of the magnetization to its initial direction starts from the domain formed at the top right corner of the nanoelement. This edge is favorable considering the low shape anisotropy density. In contrast, for the 200 ps case, at the end of the current pulse, the magnetization rotates perpendicular to the current direction and develops a component along the reversal direction, which forms the nucleation point for the reversal domain that later migrates from the top left corner of the nanoelement. The magnetization switches within one precession cycle and does not involve any vortex state.

[0035] In contrast, at the same current density, D xy Switching of the device requires several precession cycles during the reversal process, involving many metastable vortex states. D xy We performed micromagnetic simulations on the device to investigate its switching dynamics. xx The simulation was performed for the D device discussed in Figs. 4(A) to 4(E). xx The current pulse duration was measured in the range of 200 to 1200 ps on a rectangular device with the same dimensions as the device shown in Fig. 1. <m x The change in > (Figure 10A) is non-monotonic. Furthermore, D xy The device takes many precession cycles to switch, but D xx The device switches within one precession cycle.

[0036] Time-resolved magnetization maps from the simulations are shown in Fig. 1. xy We show that the magnetization reversal process under the 600 ps current pulse of D is complex and incoherent, involving an inhomogeneous magnetization state with the nucleation of many vortices (Fig. 10B). In contrast, xx The magnetization map in the device, as shown in Figure 9B, is more coherent without the excitation of higher-order spin-wave modes. In fact, it is the excitation of these modes that leads to a non-monotonic reversal process and requires longer current pulses to complete a reliable switching event. Moreover, <m x From the plot of the time evolution of >, it can be observed that the precession frequency is not a single value, indicating that different regions of the magnetic nano-element precess at different frequencies.

[0037] Switching based on the above-mentioned scheme was experimentally investigated by examining devices in which the MTJ was patterned into a right-angle trapezoid shape. Figures 11A and 11B show scanning electron microscope (SEM) micrographs of two such devices fabricated, where the MTJ has two base lengths of 150 nm and 100 nm, and a width of 75 nm. The MTJ stack is D xy Using the same fabrication procedure used to fabricate the GaN-GaN devices, the W(O) layer is patterned into a trapezoidal shape. In these devices, the devices with the negative tilted left leg are D xx- A device with a positively tilted left leg is called a D xx+ and the final subscript represents the slope of the left leg of the trapezoid.

[0038] 11C and 11D show the remanent states of magnetization of these two devices, respectively, calculated by micromagnetic simulation. x D xx- and D. xx+ The RH loops of the devices are shown in Figures 12A and 12B, respectively. Both devices have nominally identical RH loops, meaning that the magnetization of the reference layers of both devices is oriented in the same direction. The magnetization directions of the free and reference layers are shown in Figures 12A and 12B. D measurements performed using 1 ms current pulses xx- and D. xx+ The current-induced switching of the device is shown in the RI loops in Figures 12C and 12D, respectively. For the current-induced switching measurements, a magnetic field applied along the x-direction was also applied to compensate for the dipole magnetic field from the reference layer.

[0039] D xx- In the device, positive (negative) current drives AP→P (P→AP) switching, respectively, while D xx+ The opposite occurs for the RH and RI loops. The switched magnetization direction under a given current can be determined by comparing the RH and RI loops for a device of a given geometry, and is shown in the insets of Figures 12C and 12D for both devices. Since the orientation of the magnetization of the reference layer is fixed under the current pulse, the magnetization of the free layer is switched to a fixed orientation under the current pulse, i.e., xx+ Device and D xx- The device switches in different directions with the same current polarity. The switching observed experimentally in Figures 12C-12D is indeed consistent with that predicted by the micromagnetic simulations (Figures 3A and 3D). The truth tables (Figures 13A-13B) show that D xx- and D. xx+ This summarizes the basic switching behavior of the device.

[0040] Such deterministic switching, as determined by the geometry of the device, could potentially be useful in building nonvolatile nanomagnetic logic circuits, where several nanomagnets need to be switched in a complementary manner. xx+ and D. xx- The operation of a non-volatile inverter (NOT gate circuit) that can be built using the device is shown in Figure 14. If the reference layers of both devices are oriented in the same direction, D xx+ and D. xx- switches to the opposite resistance state under application of a current of the same polarity. Following the convention that the magnetization of the reference layer points in the -x direction, D xx+ The device operates as a D xx- Similarly, when a reverse current polarity pulse is applied, the D xx- The device is D xx+ It has a high resistance compared to the device.

[0041] Figures 15A and 15B show the equivalent circuit models of the non-volatile inverter devices. The circuit model of the NOT gate is D xx+ and D. xx- In the write mode (Figure 15A), the voltage input (V in1 ) is D xx+ and D. xx- During read mode, V is applied to both write+ terminals of the device and the write- terminals of both devices are grounded. DD D xx+ is applied to the read terminal of D xx+ and D. xx- Write-in terminal is V out Connected to D xx- The read terminal of is grounded. In practical device applications, the tunnel junction resistance is much larger than the resistance of the spin Hall layer, and therefore, the spin Hall layer is biased against V during the write mode. IN During the application of xx+ Power supply voltage V DD and D xx- The ground ON signal can remain connected during the entire operation of the device.

[0042] D xx+ and D. xx- The device can be considered as a type of complementary device similar to a transistor in CMOS technology. xx+ and D. xx- The series connection of both devices acts as a non-volatile inverter, since the logic output is maintained when the devices switch to their respective states. The truth table in Figure 16 summarizes the operation of the inverter. The operation of such an inverter circuit for up to 20 cycles has been demonstrated (Figure 17). In this demonstration, pulses of 2.5 V and 1 ms length are used. Thus, the generalization of this type of logic to build AND and OR gates is straightforward, borrowing the concept from CMOS logic. The advantage of this circuit compared to CMOS is that it is non-volatile and has no static power losses. This scheme can also be used to control the state of nanomagnetic elements in nanomagnetic logic schemes that require magnetic nanoelements to be coupled and in close proximity by their dipole fields. Furthermore, the improved TMR and spin-torque efficiency of spin-orbit materials improve the performance characteristics of the logic devices presented here.

[0043] An embodiment of the present invention uses magnetic nanoelements patterned in asymmetric shapes to enable switching of the magnetic nanoelements by spin-orbit torque, where the magnetization and write current are collinear, in the absence of an external magnetic field. In a preferred embodiment, the magnetic nanoelements are in-plane magnetized and form part of an MTJ. The state of the nanomagnet is identified from reading the magnetoresistance across the MTJ.

[0044] One aspect of the present invention is that the switching trajectory and final magnetic state of the magnetic free layer can be controllably manipulated by lithographically patterning the device geometry to alter its micromagnetic state. A second aspect of the present invention is that the spin polarization direction of the spin-polarized current generated by spin-orbit interaction is non-collinear with the magnetization direction, so that no thermal fluctuations are required to initiate switching. This could potentially reduce the write error rate typically observed in the short pulse length operation of conventional two-terminal STT-MRAM devices.

[0045] Another aspect of the present invention is that by forming mirror image patterning devices, two magnetic nanoelements can be switched to complementary states under the same write current direction. Moreover, such complementary switching of the magnetic nanoelement devices can form a non-volatile logic circuit. The present invention discloses a non-volatile inverter circuit formed from such magnetic nanoelements.

[0046] In another embodiment, the present invention provides a magnetic tunnel junction (MTJ) comprising: (a) a first magnetic tunnel junction (MTJ), the first magnetic layer comprising: (i) a first magnetic layer; (ii) a first tunnel barrier layer below the first magnetic layer; and (iii) a second magnetic layer below the tunnel barrier; and (b) a second magnetic tunnel junction (MTJ), the second magnetic layer comprising: (i) a third magnetic layer; (ii) a second tunnel barrier layer below the first magnetic layer; and (iii) a fourth magnetic layer below the tunnel barrier. and (c) a common spin-orbit torque (SOT) generating layer beneath both the second magnetic layer of the first MTJ and the fourth magnetic layer of the second MTJ, where the SOT generated in the common SOT generating layer sets a first magnetic state in the second magnetic layer and a second magnetic state in the fourth magnetic layer, the first magnetic state being opposite to the second magnetic state. FIG. 14 shows such a non-limiting example illustrating this embodiment, where two MTJs 1402 and 1406 share a common SOT generating layer 1406.

[0047] In Figure 14, the circuit is formed from a non-volatile inverter (NOT gate) via a series connection of two MTJs. Figure 14 shows a mirror image D-gate with two MTJs connected in series and sharing a common W(O) layer. xx- and D. xx+ FIG. 15A shows a circuit-level schematic of the nonvolatile inverter (NOT gate) implemented in the device. FIG. 15A shows a circuit-level schematic of the nonvolatile inverter in the write mode of the circuit, with the write voltage V in is applied to both devices. In the read mode (Figure 15B), V DD There are two MTJs connected in series between the write terminal and ground. Here, the write terminal is disconnected from the power supply.

[0048] In another embodiment, a circuit is formed from non-volatile NAND and NOR gates through series and parallel connections of MTJs. Figures 15C-15D show non-limiting implementations of a NAND gate in write and read modes. Figures 15E-15F show non-limiting implementations of a NOR gate in write and read modes. For both the NAND and NOR gates, the write mode circuitry is identical, with two D xx+ Device and two D xx- Use the device. xx+ and D. xx- The device's write positive terminal is V in1 and the other pair is connected to V in2 For reading, the NAND gate is connected to D xx- The devices are connected in series and xx+ are connected in parallel. For reading, in NOR, D xx- The devices are connected in parallel and xx+ are connected in series.

[0049] The above-described embodiments show effective implementations of control of switching trajectories in spin-orbit torque devices by micromagnetic configurations. While various preferred embodiments have been shown and described, it will be understood that no limitation of the invention is intended by such disclosure, but rather, all modifications falling within the scope of the invention as defined by the appended claims are intended to be covered.< / mx> < / mx> < / mx> < / mx> < / mx> < / mx>

Claims

1. It is a three-terminal device, (a) a magnetic tunnel junction (MTJ), the MTJ including: (i) a first magnetic layer, (ii) a tunnel barrier layer underlying the first magnetic layer, and (iii) a second magnetic layer underlying the tunnel barrier layer; (b) a spin-orbit torque (SOT) generating layer immediately below the second magnetic layer; the second magnetic layer has an asymmetric shape such that the average magnetization of the remanent state associated with the second magnetic layer has an in-plane component perpendicular to the current direction in the SOT generation layer, and has a geometry that creates defects on some of the edges of the second magnetic layer such that an internal magnetic field can initiate a reversal process. Three terminal device.

2. 10. The device of claim 1 , which is part of a non-volatile inverter circuit formed from a series connection of the MTJ of (a) with another MTJ.

3. 2. The device of claim 1 , which is part of either a non-volatile NAND gate or a NOR gate, the NAND gate or the NOR gate being formed using a combination of series and parallel connections of the MTJ of (a) and three other MTJs.

4. 2. The device of claim 1, wherein the three terminal device forms part of a non-volatile cache memory device.

5. The device of claim 1 , wherein the three terminal device forms part of a cryogenic memory device.

6. 6. The device of claim 1, wherein the SOT generating layer is made from a material that exhibits the spin Hall effect.

7. The device of claim 6 , wherein the material is selected from the group consisting of W, Pt, Ta, and combinations thereof.

8. The device of claim 6 , wherein the SOT generating layer is made of oxygen-doped tungsten.

9. A device, (a) a first magnetic tunnel junction (MTJ), the first MTJ including: (i) a first magnetic layer, (ii) a first tunnel barrier layer underlying the first magnetic layer, and (iii) a second magnetic layer underlying the first tunnel barrier layer; (b) a second magnetic tunnel junction (MTJ), the second MTJ including: (i) a third magnetic layer; (ii) a second tunnel barrier layer underlying the first magnetic layer; and (iii) a fourth magnetic layer underlying the second tunnel barrier layer; (c) a common spin-orbit torque (SOT) generating layer, the common SOT generating layer underlying both the second magnetic layer of the first MTJ and the fourth magnetic layer of the second MTJ; a first magnetic state is set in the second magnetic layer and a second magnetic state is set in the fourth magnetic layer, the first magnetic state being opposite to the second magnetic state; each of the second magnetic layer and the fourth magnetic layer has an asymmetric shape such that the average magnetization of the remanent state associated with the second magnetic layer or the fourth magnetic layer has an in-plane component perpendicular to the current direction of the SOT generation layer, and has a geometry that forms defects on a portion of an edge of the second magnetic layer or the fourth magnetic layer such that an internal magnetic field can initiate a reversal process; device.

10. 10. The device of claim 9, wherein the first and / or third magnetic layers include any or combination of a synthetic antiferromagnetic (SAF) layer, an exchange bias layer, and a layer having a higher coercivity than the second magnetic layer.

11. 10. The device of claim 9, wherein the second and / or fourth magnetic layers comprise a CoFeB alloy and / or a NiFe alloy.

12. 10. A device according to claim 9 forming part of a non-volatile cache memory device.

13. 10. The device of claim 9 forming part of a cryogenic memory device.

14. The device of claim 9 , wherein the common SOT generation layer is made of oxygen-doped tungsten.

15. The device of claim 9 , wherein the common SOT generating layer is made from a material that exhibits the spin Hall effect.

16. The device of claim 15 , wherein the material is selected from the group consisting of W, Pt, Ta, and combinations thereof.

17. It is a method, (a) providing a three-terminal device comprising, in order, a spin-orbit torque (SOT) generating layer, an in-plane magnetic free layer whose magnetic moment can be switched by a spin transfer torque generated by said SOT generating layer, a tunnel barrier, and a reference magnetic layer whose orientation remains fixed during operation of the device; a write positive terminal and a write negative terminal electrically contact both ends of the SOT generating layer; a read terminal in electrical contact with the reference magnetic layer; the in-plane magnetic free layer has an asymmetric shape such that the average magnetization of the remanent state of the in-plane magnetic free layer has an in-plane component perpendicular to the current direction, and has a geometric shape in which defects are formed on some of the edges of the in-plane magnetic free layer so that an internal magnetic field can initiate a reversal process; The providing; (b) passing a current between terminals along the SOT generation layer, thereby switching a magnetic state of the in-plane magnetic free layer in the absence of an applied magnetic field when the direction of the passed current is oriented along an easy axis of the in-plane magnetic free layer; A method comprising:

18. The method of claim 17 , wherein the in-plane magnetic free layer does not include any remnant domain walls.

19. The method of claim 17 , wherein the anisotropy of the in-plane magnetic free layer arises primarily from magnetostatic interactions between magnetic moments in the in-plane magnetic free layer.

20. The method of claim 17 , wherein the in-plane magnetic free layer comprises a CoFeB alloy or a NiFe alloy or both.

21. 20. The method of claim 17, wherein the three terminal device forms part of a non-volatile cache memory device.

22. 20. The method of claim 17, wherein the three terminal device forms part of a cryogenic memory device.

23. 20. The method of claim 17, wherein the SOT generating layer is made of oxygen-doped tungsten.

24. 20. The method of claim 17, wherein the SOT generating layer is made from one or more materials that exhibit the spin Hall effect.

Citation Information

Patent Citations

  • Expansion magnetic tunnel junction, spinning majority gate device and logic circuit

    CN107732005A

  • Gate-level reconfigurable magnetic logic

    JP2012500446A

  • Bottom pinned sot-MRAM bit structure and method of fabrication

    JP2017112358A

  • Spin current magnetization reversal element and magnetic memory

    JP2019046976A

  • Magnetic memory

    JP2019054154A