Light receiving element
The novel insulating layer configuration enhances moisture resistance in semiconductor light-receiving elements, ensuring reliability and cost-effectiveness by isolating the pad region from the element region, thus simplifying the optical transceiver structure.
Patent Information
- Application Number
- JP2023506606
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-17
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2041-03-17
AI Technical Summary
Semiconductor light-receiving elements face challenges in maintaining moisture resistance, which is crucial for reliability and cost reduction, as conventional hermetic sealing processes are complex and hinder cost efficiency.
A novel configuration with a first and second insulating layer covering the element, separated by a second insulating section perpendicular to the substrate surface, isolating the pad region from the element region, using materials like polymeric and inorganic insulating films to enhance moisture resistance.
Improves the reliability of light receiving elements by maintaining moisture resistance even with damage, simplifying the structure, and reducing the cost of optical transceivers.
Smart Images

Figure 0007564488000001 
Figure 0007564488000002 
Figure 0007564488000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a light receiving element, and more particularly to a structure of a semiconductor light receiving element. [Background technology]
[0002] Photodetectors have the role of converting incident light into electrical information. In optical communications, photodetectors are widely used at the receiving end of a transmission line to convert an optical signal propagated through an optical fiber into an electrical signal.
[0003] For semiconductor photodetectors made of semiconductors intended for application to optical communications, attention has focused on photosensitivity and operating bandwidth as important parameters among the requirements. If a semiconductor photodetector has higher photosensitivity, it can demodulate optical signals that have propagated over longer optical fibers, which contributes to reducing relay equipment. Furthermore, if the semiconductor photodetector has a wider bandwidth, it can demodulate optical signals with higher modulation speeds. The key factors for increasing the speed and reducing the cost of optical communications were to increase the sensitivity and operate at higher speeds in semiconductor photodetectors.
[0004] Among semiconductor photodetectors, avalanche photodiodes (APDs) have an internal gain and therefore can achieve higher sensitivity than general photodiodes. For this reason, APDs have been applied to optical networks that require long, fixed-distance transmission without repeaters, such as metro and access networks and large data centers.
[0005] While the transmission distances are becoming longer as mentioned above, optical communications are also being used for short-distance communications such as communications between servers that have previously been performed using electrical wiring. Optical transceivers for optical communications using APDs are being required to be significantly cheaper than before.
[0006] Not only APDs, but semiconductor light receiving elements in general, are difficult to ensure reliability against humidity in actual operating environments. This is because moisture on the surface of the element accelerates the deterioration of the semiconductor surface, leading to element failure. Conventionally, moisture resistance has been ensured for the entire optical transceiver by hermetically sealing the semiconductor light receiving element inside the package that constitutes the receiver. However, to achieve moisture resistance, the package material itself must first be made of a material that is resistant to humidity, such as metal. Furthermore, the hermetic sealing process itself requires complex steps, which has hindered efforts to reduce the cost of optical transceivers. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Patent Publication No. 2020-174079 Summary of the Invention [Problem to be solved by the invention]
[0008] The present invention proposes a novel structure for improving the moisture resistance of a semiconductor light receiving element. [Means for solving the problem]
[0009] One embodiment of the present invention is a photodetector having an element portion in which at least a first contact layer, a light absorption layer, and a second contact layer are stacked in order on a substrate, the photodetector being characterized by comprising a first insulating portion covering the substrate and the element portion, a pad region including a first pad connected to the first contact layer via an electrode wiring or a second pad connected to the second contact layer via an electrode wiring, and a separation portion between the element region including the element portion and configured perpendicular to the substrate surface by a second insulating portion made of a material different from the first insulating portion. Effect of the Invention
[0010] The reliability of the light receiving element is improved, and the cost of the optical transceiver is reduced. [Brief description of the drawings]
[0011] [Figure 1] 1 is a diagram showing a configuration of a light receiving element according to a first embodiment. [Diagram 2] FIG. 11 is a diagram showing a configuration of a light receiving element according to a second embodiment. [Diagram 3] FIG. 11 is a diagram showing a configuration of a light receiving element according to a third embodiment. [Figure 4] FIG. 13 is a diagram showing the configuration of a light receiving element according to a fourth embodiment. [Diagram 5] FIG. 13 is a diagram showing the configuration of a light receiving element according to a fifth embodiment. [Figure 6] 11A and 11B are diagrams illustrating the effect of mechanical stress on a pad on the moisture resistance of a light receiving element. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The light receiving element of the present disclosure has an element portion in which at least a first contact layer, a light absorbing layer, and a second contact layer are laminated in this order on a substrate. The substrate and the element portion are covered by a first insulating portion made of, for example, a polymer material. Looking at the substrate surface, a separation portion made of a second insulating portion is provided between an element region including an element portion of the light receiving element and a pad region including a pad for electrical and mechanical connection with the outside of the element, and is configured perpendicular to the substrate surface. The separation portion of the light receiving element may be a wall-like portion filled with the material of the second insulating portion. Even if damage occurs due to an external force to the pad in the pad region or its vicinity, the deterioration of moisture resistance due to this damage is limited to within the pad region due to the moisture resistance performance of the second insulating portion, which may be, for example, an inorganic insulating film. The element region including the element portion is not affected by damage to the pad or its vicinity, and the moisture resistance is maintained by the second insulating portion. The configuration of the passive element including the separation portion can be variously varied.
[0013] Hereinafter, the basic configuration and specific configuration of the light receiving element of the present disclosure will be described in detail with reference to the drawings. [Embodiment 1] FIG. 1 is a diagram showing the configuration of a light receiving element of the first embodiment. FIG. 1(b) shows a top view of the substrate surface, and FIG. 1(a) shows a cross-sectional view of the substrate surface cut vertically along line Ia-Ia in the top view. Referring to FIG. 1(a), the light receiving element 100 has an element part having a layer structure in which an n-type InP contact layer 11, an undoped InGaAs light absorption layer 12, and a p-type InP contact layer 13 are laminated in this order on an InP substrate 10. A reflective mirror film 17b is formed on the upper part of the p-type contact layer 13 by using Au, and this reflective mirror film 17b also serves as an electrode for the p-type contact layer 13. The element part is generally cylindrical, and the n-type contact layer 11 is formed to be slightly larger than the light absorption layer 12 and the p-type contact layer 13. A ring-shaped electrode metal 16c made of Au is formed on the periphery of the upper surface of the cylinder formed by the n-type contact layer 11.
[0014] The electrode 16c on the n-type contact layer 11 is connected to a first electrode pad 16a for extracting an electrical signal to the outside via an electrical wiring 16b arranged perpendicular to the substrate surface, and the electrode 17b is connected to a second electrode pad 17a for extracting an electrical signal to the outside via an electrical wiring.
[0015] The photoelectric conversion operation of the photodetector 100 of this embodiment is the same as that of the conventional technology. Electrons generated by photoexcitation in the photoabsorption layer 12 reach the n-type contact layer 11 and then move to the electrode 16c. On the other hand, holes reach the p-type contact layer 13 and then move to the electrode 17b. In this way, the photodetector 100 operates as a semiconductor photodetector that generates a current when light is incident on the photoabsorption layer 13. Light enters from the lower surface side of the substrate 10, reaches the photoabsorption layer 12, and is reflected by the reflective mirror film 17b, which also serves as an electrode, to the photoabsorption layer 12, efficiently converting the incident light into an electrical signal.
[0016] The light receiving element of the present disclosure improves the moisture resistance of the semiconductor light receiving element itself by a characteristic element protection structure described in detail below, and realizes a cost reduction of the optical transceiver. The element portion including the n-type contact layer 11, the light absorption layer 12, and the p-type contact layer 13 and the substrate 10 are entirely covered with the first insulating portions 14a, 14b, and 14c formed of a first material. For example, a polymer can be used as the first material, and the first insulating portion functions as an insulating film for protecting the element. Furthermore, the entire first insulating portions 14a, 14b, and 14c are entirely covered with the second insulating portion 15 made of a second material. For example, SiN can be used as the second material, and the second insulating portion 15 functions as an insulating film for protecting the first insulating portion and the element portion. The two pads 16a and 17a on the outermost surface are both formed on the second insulating portion 15.
[0017] In the light receiving element of the present disclosure, when the substrate surface is viewed, a pad region 31 including a first pad 16a and an element region 30 including an element portion are separated by a part of the second insulating portion. Specifically, referring to the cross-sectional view of FIG. 1(a), the pad regions 31, 32 and the element region 30 are separated by wall-like second insulating portions 15a, 15b formed perpendicularly to the substrate 10. Referring also to the top view of FIG. 1(b), the wall-like second insulating portion 15a separates the first insulating portion into two portions 14a, 14b indicated by dotted lines, and the first insulating portion 14a of the pad region 31 and the first insulating portion 14b of the element region 30 are not directly connected to each other.
[0018] Similarly, the pad region 32 including the second pad 17a and the element region 30 including the element portion are separated by a wall-like second insulating portion 15b formed perpendicular to the substrate 10. The first insulating portion 14c of the pad region 32 and the first insulating portion 14b of the element region 30 are separated by the second insulating portion 15b and are not directly connected to each other.
[0019] In order to use the light receiving element without hermetically sealing it, the light receiving element itself needs to be moisture resistant. As the second insulating part 15 covering the top of the light receiving element in this embodiment, an inorganic insulating film, such as SiN, whose film itself is dense against water molecules, is used. However, such an inorganic insulating film does not have sufficient strength against mechanical stress.
[0020] FIG. 6 is a diagram for explaining the effect of mechanical stress on the pad on the moisture resistance of the element. The light receiving element 600 in FIG. 6 has an element part with the same structure as the light receiving element 100 in the first embodiment. The pad region including the pads 16a and 17a has a substantially same structure as the light receiving element 100 in the first embodiment, except that the base is not an insulating part but has the same laminated structure as the element part. The difference in structure from the light receiving element in the first embodiment is that the element region 25 and the pad regions 24 and 26 are separated only by the insulating part 14. When the light receiving element is actually used, it is necessary to take out an electric signal from the pad to the outside by contacting a test probe on the pads 16a and 17a or bonding a metal wire. When forming an electric path (wiring) to the outside, the insulating part 15 around the pad may be mechanically destroyed by the stress 22. In particular, when a microcrack 23, which is a minute damage, occurs in the insulating part (insulating film) around the pad, moisture will penetrate from the damaged part even if it is minute, and the moisture resistance will be broken.
[0021] Polymer materials, which are also used as interlayer insulating films for metal wiring, are generally moisture permeable, so in the element configuration of Fig. 6, moisture that has entered through microcracks 23 reaches the element section through insulating section 14 made of the polymer material, damaging the reliability of the light receiving element.
[0022] In the light receiving element 100 of this embodiment, the first insulating part made of a polymer material covering the substrate 10 and the element part is spatially separated into a part 14b of the element region 30 and parts 14a, 14c of the pad regions 31, 32. In the light receiving element 100, the first insulating part is separated by separation parts 15a, 15b formed in a wall shape perpendicular to the substrate surface, which are part of the second insulating part made of SiN covering the top part. According to the element protection structure of the first embodiment of FIG. 1, even if the moisture resistance is broken due to slight damage to the pad region, moisture is blocked by the separation parts between the element region 30 and the pad regions 31, 32, and the moisture resistance of the element part is not broken. Even if damage occurs due to stress applied to the pad region, the moisture resistance of the element part can be secured and the reliability of the light receiving element itself can be improved. As a result, the moisture-resistant structure of the optical transceiver can be further simplified and the cost can be reduced.
[0023] Therefore, the light-receiving element of the present disclosure can be implemented as a light-receiving element 100 having an element portion in which at least a first contact layer 11, a light absorption layer 12, and a second contact layer 13 are stacked in order on a substrate 10, the light-receiving element 100 being provided with a first insulating portion covering the substrate and the element portion, pad regions 31, 32 including a first pad 16a connected to the first contact layer via an electrode wiring or a second pad 17a connected to the second contact layer via an electrode wiring, and separation portions 15a, 15b formed perpendicular to the substrate surface by a second insulating portion made of a material different from the first insulating portion between the element region 30 including the element portion.
[0024] The above-mentioned separating portions 15a, 15b can be embodied as having a wall-like shape filled with the material of the second insulating portion.
[0025] The process for realizing the light receiving element of this embodiment is as follows. First, an n-type InP contact layer, an undoped InGaAs light absorbing layer, and a p-type InP contact layer are epitaxially grown in this order on a semi-insulating InP substrate 10 using metal-organic chemical vapor deposition (MOCVD). After the three layers are crystal-grown, photolithography and etching are performed in sequence. This forms a mesa-shaped element portion consisting of an n-type contact layer 11, a light absorbing layer 12, and a p-type contact layer 13.
[0026] Next, electrode metals 17b and 16c are formed on the p-type contact layer 13 and the n-type contact layer 11, respectively, by photolithography, vapor deposition, and lift-off. After that, photosensitive polyimide is used to form through-holes of polyimide (first material) for later forming the n-type contact electrode 16b, the p-type contact electrode, and the separation part by coating, photolithography, and curing the polyimide. Here, the through-hole is not limited to a cylindrical one, but also includes a groove-like one having a width. Furthermore, SiN (second material) is formed over the entire surface to form the protective film 15 of SiN including the separation parts 15a and 15b, which are part of the second insulating part. After that, through-holes are formed in SiN for the n-type contact electrode 16b and the p-type contact electrode 17b by dry etching. Finally, metal wiring and pads 16a and 17a may be formed by photolithography, vapor deposition, and lift-off.
[0027] In the configuration of the light receiving element shown in Fig. 1, an example is shown in which there are pad regions on both sides of the element region, and three regions are arranged in a straight line, but the configuration of the light receiving element is not limited to this. For example, two pads may be on the same side of the element region, and the two pads may be configured within a common first insulating part. In this configuration, only one is required for the two isolation parts 15a and 15b in Fig. 1. Also, the three regions, the element region and the two pad regions, may be arranged in an L shape.
[0028] With a light receiving element having the element protection structure of this embodiment, even if deterioration of moisture resistance occurs due to damage to the periphery of the pad, this deterioration can be limited to the pad area, and the moisture resistance of the element area is maintained. Furthermore, the moisture resistance of the optical transceiver is improved, and the structure of the optical transceiver is simplified and the cost is reduced. The configuration of the separation part separating the element area and the pad area can be variously changed in addition to that shown in FIG. 1. [Embodiment 2] FIG. 2 is a diagram showing the configuration of a light receiving element according to the second embodiment. FIG. 2(b) shows a top view of the substrate surface, and FIG. 2(a) shows a cross-sectional view of the substrate surface cut vertically along line IIa-IIa in the top view. The light receiving element 200 of this embodiment differs from the light receiving element 100 of the first embodiment shown in FIG. 1 only in the configuration of the separation part, and only this difference will be described below. In the light receiving element 100 of the first embodiment, the separation part separating the element region and the pad region was configured as a wall-like part perpendicular to the substrate surface as a part of the second insulating part covering the top surface of the element. This separation part was formed by a process of forming a through hole in a groove shape in the first insulating part and filling the groove with the material of the second insulating part. By this process, in the light receiving element of the first embodiment, the entire surface of the element was covered with the second insulating part, except for the part where the pad was formed. However, it is not necessary that most of the chip is covered with the second insulating part.
[0029] In the light receiving element 200 of this embodiment, the element region and the pad region have second insulating parts 15a, 15b, 15c, 15d, and 15e covering the upper surface and the side surface perpendicular to the substrate surface of each of the first insulating parts. The second insulating part 15e covering the side surface of the first insulating part of the element region 30 and the second insulating part 15d covering the side surface of the first insulating part of the pad region 31 including the pad 16a face each other and are separated by a space. The same configuration is also provided between the pad region 32 including the pad 17 and the element region 30. As is clear from (a) and (b) of FIG. 2, the separation parts 33 and 34 are each composed of two second insulating parts facing each other perpendicular to the substrate surface and a space between them. As will be described last, the entire element can be covered with a third insulating part after all the elements and wiring electrodes are formed, and only the pad part is exposed, thereby providing the light receiving element with even higher environmental resistance. In this case, the space between the two opposing second insulating parts in the separation parts 33 and 34 in FIG. 2 is filled not with space (air) but with the insulating material of the third insulating part.
[0030] Therefore, the light receiving element of this embodiment can also be embodied such that the isolation portion 33 has a film-like second insulating portion 15d covering the side surface of the pad region 31 and a film-like second insulating portion 15e covering the side surface of the element region 30.
[0031] The process for realizing the light receiving element of this embodiment is as follows. First, an n-type InP contact layer, an undoped InGaAs light absorbing layer, and a p-type InP contact layer are epitaxially grown in this order on a semi-insulating InP substrate 10 using MOCVD. After the three layers are crystal-grown, photolithography and etching are performed in sequence. This forms a mesa-shaped light receiving element consisting of an n-type contact layer 11, a light absorbing layer 12, and a p-type contact layer 13.
[0032] Next, electrode metals 17b and 16c are formed on the p-type contact layer 13 and the n-type contact layer 11, respectively, by photolithography, vapor deposition, and lift-off. After that, photosensitive polyimide is used to form through-holes on the polyimide 14b in the element region 30 by coating the polyimide, photolithography, and curing, in order to later form the n-type contact electrode 16b and the p-type contact electrode. At the same time, each region of the first insulating part is formed so that the polyimide 14b in the element region 30 and the polyimides 14a and 14c in the pad regions 31 and 32 are separated into islands. Furthermore, a second insulating part, i.e., SiN, is formed over the entire surface, and protective films 15a, 15b, and 15c of SiN are formed, including the separating parts 15d and 15e, which are parts of the second insulating part. After that, through-holes are formed in the SiN for the n-type contact electrode 16b and the p-type contact electrode 17b of the element by dry etching. At the same time, a SiN pattern is formed so that the element region 30 and the pad regions 31 and 32 are separated into islands. Finally, metal wiring and pads 16a and 17a having a predetermined thickness are formed by photolithography and evaporation lift-off.
[0033] In the photodetector 200 having the element protection structure of this embodiment, deterioration in moisture resistance caused by damage to the periphery of the pad can be limited to the pad area, and the moisture resistance of the element portion is maintained. This improves the moisture resistance of the optical transceiver, and simplifies the structure of the optical transceiver and reduces its cost. [Embodiment 3] In this embodiment, a configuration is presented that further improves the moisture resistance and reliability of the element protection structure for a light-receiving element shown in the above-mentioned second embodiment.
[0034] FIG. 3 is a diagram showing the configuration of a light receiving element of the third embodiment. FIG. 3(b) shows a top view of the substrate surface, and FIG. 3(a) shows a cross-sectional view of the substrate surface cut vertically along line IIIa-IIIa in the top view. The light receiving element 300 of this embodiment differs from the light receiving element 200 of the second embodiment shown in FIG. 2 only in the top surface patterns of the first insulating part and the second insulating part, and the following description focuses on the differences from the second embodiment. The configuration in the cross-sectional view of FIG. 3(a) is exactly the same as that of FIG. 2(a). The light receiving element 300 of FIG. 3 is such that the pattern shape of the top surface of the first insulating part or the second insulating part when viewed from the substrate surface is such that the interior angle formed by two sides is greater than 90 degrees at any point.
[0035] In (a) of Fig. 3, which is a cross-sectional view taken along line IIIa-IIIa along the wiring electrode, the configuration of the isolation portions 33 and 34 separating the element region 30 from the pad regions 31 and 32 is the same as that in (a) of Fig. 2. Referring to the top view in (b) of Fig. 3, the top surface pattern of the second insulating portion covering the element region 30 and the pad regions 31 and 32 is not rectangular as in the second embodiment, but has short oblique sides 20a, 20b, and 20c at its corners.
[0036] In any of the light receiving elements disclosed herein, the first insulating part or the second insulating part is separated between the element region and the pad region, thereby improving the moisture resistance of the element region. The effect of improving the moisture resistance is premised on the first insulating part and the second insulating part being firmly attached to the substrate and the semiconductor layer. However, in reality, in both the polymer insulating film and the inorganic insulating film such as SiN, the contact part with the InP-based semiconductor layer may float and cause a gap. This problem may occur due to the manufacturing process, the heat cycle during use in the actual optical transceiver, and mechanical shock due to washing with water in the manufacturing process. Such floating of the insulating film often occurs at the end of the film where the stress of the insulating film is concentrated. Therefore, the sharper the angle formed by the end of the insulating film pattern, the more likely it is that the stress will concentrate and the floating will occur.
[0037] In the light receiving element 300 of this embodiment, as shown in FIG. 3(b), the pattern shape of the first insulating part or the second insulating part when viewed from the substrate surface is such that the interior angle formed by any two adjacent sides is greater than 90 degrees. Specifically, in the manufacturing process of the light receiving element of the above-mentioned embodiment 2, in each of the element region 30 and the pad regions 31 and 32, the four corners of the island pattern of the first insulating part on the surface (upper surface) parallel to the substrate surface may be cut to form an octagon. In this case, the interior angle of the pattern shape of each region is 135 degrees. The shape of the SiN of the second insulating part is also similarly octagonal. In order to prevent stress concentration, it is preferable to make the pattern shape such that the interior angle formed by any two adjacent sides is greater than 90 degrees for both the first insulating part and the second insulating part, but it is also possible to make only one of the insulating parts.
[0038] In the light receiving element 300 of this embodiment, the deterioration of moisture resistance caused by damage around the pad can be limited to the pad area, and the moisture resistance of the element part is maintained. By making the structure of the insulating part more robust against stress, the reliability of the light receiving element itself can be further improved. Furthermore, the moisture resistance of the optical transceiver is improved, and the structure of the optical transceiver can be simplified and the cost of the optical transceiver can be reduced. [Embodiment 4] In the light-receiving element of this embodiment, an example is presented in which, in the element protection structure for the light-receiving element shown in the above-mentioned embodiment 3, the ends of the patterns on the surfaces (top surfaces) parallel to the substrate surface of the first insulating part and the second insulating part are made circular.
[0039] FIG. 4 is a diagram showing the configuration of a light receiving element according to a fourth embodiment. FIG. 4(b) shows a top view of the substrate surface, and FIG. 4(a) shows a cross-sectional view of the substrate surface cut vertically along line IVa-IVa in the top view. The light receiving element 400 according to this embodiment is the light receiving element 300 according to the third embodiment shown in FIG. 3, in which the corner shapes of the patterns of the first insulating part or the second insulating part when viewed from the substrate surface are curved from the oblique side. As shown in FIG. 4(b), in a plane parallel to the substrate surface of the pad regions 31 and 32, the four corners of the patterns of the second insulating parts 15a and 15c are curved surfaces 21a and 21b.
[0040] In addition, in a plane parallel to the substrate surface, the patterns of the first insulating part and the second insulating part in the element region 30 are circular so as to enclose the cylindrical mesa of the element region, and the sizes of the first insulating part and the second insulating part are limited to fit the shape and size of the element region. Since the element region 30 in FIG. 4 has a cylindrical shape without an apex, the concentration of stress on the element region can be further reduced compared to the element region 30 in FIGS. 1 to 3 based on the rectangular parallelepiped shape of the first to third embodiments. The light receiving element 400 of this embodiment can be realized by a process similar to that of the third embodiment, simply by changing the upper surface patterns of the first insulating part and the second insulating part.
[0041] In the light receiving element 400 of this embodiment, the deterioration of moisture resistance caused by damage to the periphery of the pad can be limited to the pad area, and the moisture resistance of the element portion is maintained. As in the third embodiment, the reliability of the light receiving element can be further improved by making the structure of the insulating portion more robust against stress. Furthermore, the moisture resistance of the optical transceiver can be improved, and the structure of the optical transceiver can be simplified and the cost of the optical transceiver can be reduced. [Embodiment 5] The light-receiving element of the fifth embodiment differs from the light-receiving elements of the second to fourth embodiments in the positional relationship between the pads on the surface of the element and the second insulating part covering the outermost surface of the element. In the element protection structures of the light-receiving elements shown in the second to fourth embodiments, the element region and the pad region are formed in separate island shapes by providing an isolating part or restricting the shape of the element region. In the region between the element region and the pad region, the first insulating part and the second insulating part are removed, so that the substrate 10 is exposed. In the light-receiving element of the present embodiment, the second insulating part is formed between the wiring and the substrate at every location of the element and the wiring formed.
[0042] Fig. 5 is a diagram showing the configuration of a light receiving element of embodiment 5. Fig. 5(b) shows a top view of the substrate surface, and Fig. 5(a) shows a cross-sectional view of the substrate surface cut vertically along line Va-Va in the top view. The light receiving element 500 of this embodiment is different from the light receiving element 200 of embodiment 2 shown in Fig. 2 in the positional relationship between the second insulating portion and the wiring.
[0043] In the light-receiving elements of the second to fourth embodiments, the first insulating portion and the second insulating portion are spatially separated between the element region 30 and the pad regions 31, 32. Therefore, a part of the wiring between the element region and the pads 16a, 17 is formed on the substrate 10.
[0044] In general, in a substrate, a surface state may be formed on the semiconductor surface by various wet / dry etching and lithography processes, and charges may accumulate. When wiring is formed on a substrate in such a state, a leakage current may occur on the substrate. The leakage current may lead to deterioration of the performance and reliability of the light receiving element. Therefore, in the light receiving element 500 of the embodiment, a second insulating part is formed between the wiring formed in the final process and the substrate 10. Comparing the cross-sectional views of FIG. 2(a) and FIG. 5(a), in the separation parts 33 and 34 of the second embodiment, the wiring to the pads 16a and 17a is formed directly on the substrate 10. In contrast, in the light receiving element of the present embodiment, the second insulating part 15 is formed integrally without a break on the entire surface through the pad region 31, the element region 30, and the pad region 32. In the separation parts 33 and 34, the wiring to the pads 16a and 17a is formed on the second insulating part 15. With this configuration, there is no effect of the surface state due to the metal electrodes on the substrate 10. The second insulating portion formed between the substrate and the wiring can reduce leakage current caused by the wiring portion.
[0045] The process for realizing the light receiving element of this embodiment is as follows. First, an n-type InP contact layer, an undoped InGaAs light absorbing layer, and a p-type InP contact layer are epitaxially grown in this order on a semi-insulating InP substrate using MOCVD. After the three layers are crystal-grown, photolithography and etching are performed in sequence. This forms a mesa-shaped light receiving element consisting of an n-type contact layer 11, a light absorbing layer 12, and a p-type contact layer 13.
[0046] Next, electrode metals 17b and 16c are formed on the p-type contact layer 13 and the n-type contact layer 11, respectively, by photolithography, vapor deposition, and lift-off. After that, photosensitive polyimide is used to form through-holes on the polyimide 14b in the element region 30 by coating the polyimide, photolithography, and curing, in order to later form the n-type contact electrode 16b and the p-type contact electrode. At the same time, each region of the first insulating part is formed so that the polyimide 14b in the element region 30 and the polyimides 14a and 14c in the pad regions 31 and 32 are separated into islands. Furthermore, after forming the second insulating part, i.e., SiN, entirely, the n-type contact electrode 16c and the SiN through-holes for the p-type contact electrode are formed by dry etching. By this process, the first insulating part is separated between the pad regions 31 and 32 and the element region 30, and the effect of damage to the pad region on the moisture resistance of the element is avoided. Furthermore, the second insulating part 15 is formed on the entire surface of the substrate 10.
[0047] Finally, metal wiring and pads 16a and 17a are formed by photolithography, evaporation and lift-off.
[0048] In the above-mentioned light receiving elements of the first to fifth embodiments, the material of the first insulating part is polyimide and the material of the second insulating part is SiN, but the element protection structure of the light receiving element of the present disclosure is not limited to these materials. For example, the first insulating part may be benzocyclobutene (BCB). The second insulating part may be SiO2, WSiN, or a multilayer film of these.
[0049] In addition, after all the elements and wiring have been formed, the entire element can be covered with a third insulating part (insulating film) in addition to the first insulating part and the second insulating part, and only the pad part can be exposed, thereby giving the element even higher environmental resistance.
[0050] In addition, in the above-mentioned embodiments, PIN photodiodes having circular element portions are used as examples, but avalanche photodiodes having higher sensitivity may be used instead. The shape of the element portion may be elliptical or polygonal depending on the shape of the beam incident on the light receiving element and the circumstances of the element fabrication.
[0051] In the above-described embodiments, the light is vertically incident from below the substrate. However, considering that all of the light receiving elements are optical waveguide type light receiving elements, the structure of the element portion may be rectangular or other shapes so that the light can be easily incident from the optical waveguide along the substrate surface. The light receiving element of the present disclosure is based on a characteristic configuration of a plurality of insulating portions for the element region and the pad region, and does not depend on the type or structure of the element portion as the light receiving element.
[0052] The light receiving element of the present disclosure can achieve high reliability for the light receiving element alone, and can reduce the cost of the optical transceiver by eliminating the need for a hermetically sealed structure.
Claims
1. A light receiving element having an element portion in which at least a first contact layer, a light absorbing layer, and a second contact layer are laminated in this order on a substrate, a first insulating portion made of a polymer material covering the substrate and the element portion; a second insulating portion made of an inorganic insulating material that further covers the first insulating portion, the second insulating portion having one or more wall-like portions that are perpendicular to the substrate surface between the element portion and a first pad connected to the first contact layer via an electrode wiring or a second pad connected to the second contact layer via an electrode wiring; Equipped with A light-receiving element, characterized in that the first insulating portion covering the element portion and the first insulating portion below the first pad are separated by the wall-like portion, and the first insulating portion covering the element portion and the first insulating portion below the second pad are separated by the wall-like portion.
2. A light-receiving element as described in claim 1, characterized in that the first pad and the second pad are formed on the second insulating portion which covers the first insulating portion.
3. The element portion has a cylindrical mesa structure, 3. The light-receiving element according to claim 1, which is a semiconductor light-receiving element having a reflective electrode connected to the second pad and formed on the second contact layer.
4. The inorganic insulating material of the second insulating part is SiN, SiO 2 4. The light-receiving element according to claim 1, comprising either one of a SiN film and a WSiN film or a multilayer film thereof.
Citation Information
Patent Citations
Semiconductor light-receiving element
JP2014011347A
Semiconductor photodetector
JP2018098399A
Semiconductor photodetector
JP2020174079A
Optical semiconductor element
WO2019193892A1