Semiconductor Device
The described method for forming semiconductor devices through precise plasma treatment and etching techniques addresses the challenges of achieving small channel lengths and high frequency performance in transistors, resulting in improved electrical characteristics and reliability.
Patent Information
- Application Number
- JP2023100498
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2014-09-19
- Filing Date
- 2023-06-20
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2035-09-17
AI Technical Summary
Existing semiconductor technologies face challenges in achieving transistors with small channel lengths, low leakage current, small subthreshold swing values, reduced short channel effects, normally-off electrical characteristics, and high frequency performance.
A method involving the formation of a semiconductor device over a substrate, with specific conductors and insulators, using plasma treatment and etching techniques to create precise masks and shapes, allowing for the formation of transistors with controlled dimensions and improved electrical characteristics.
The method enables the production of transistors with small channel lengths, low leakage current, and high frequency characteristics, along with improved reliability and electrical performance.
Smart Images

Figure 0007565409000001 
Figure 0007565409000002 
Figure 0007565409000003
Abstract
Description
[Technical field]
[0001] The present invention relates to, for example, a semiconductor, a conductor, an insulator, a transistor, and a semiconductor device. Alternatively, the present invention relates to, for example, a semiconductor, a conductor, an insulator, a transistor, and a semiconductor device. The present invention also relates to a manufacturing method thereof, for example, a semiconductor, a conductor, an insulator, a display device, a light emitting device, and the like. Related to optical devices, lighting devices, power storage devices, memory devices, processors, electronic devices, and semiconductor devices. , conductor, insulator, display device, liquid crystal display device, light-emitting device, storage device, and method for manufacturing electronic device Or, a semiconductor device, a display device, a liquid crystal display device, a light-emitting device, a memory device, an electronic The present invention relates to a method for driving an apparatus.
[0002] Note that one embodiment of the present invention is not limited to the above technical field. The technical field of one aspect relates to an article, a method, or a manufacturing method. One aspect of the present invention is a process, machine, manufacture, or composition. It is about the nature of matter.
[0003] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. Display devices, light-emitting devices, lighting devices, electro-optical devices, semiconductor circuits, and electronic devices may include a semiconductor device. [Background technology]
[0004] Technology that uses semiconductors on substrates with insulating surfaces to construct transistors has been attracting attention. Such transistors are widely used in semiconductor devices such as integrated circuits and display devices. Silicon is known as a semiconductor that can be used for transistors.
[0005] Silicon used as a semiconductor in transistors is classified into amorphous silicon and polycrystalline silicon depending on the application. For example, it is used in transistors that make up large display devices. In this case, it is preferable to use amorphous silicon, for which a film formation technique for a large-area substrate has been established. On the other hand, a high-performance display device in which the driving circuit and the pixel circuit are formed on the same substrate is constructed. When applied to transistors that use ZnO, it is possible to create transistors with high field-effect mobility. It is preferable to use polycrystalline silicon, which has a high thermal conductivity compared to amorphous silicon. A method for forming the insulating film by heat treatment at room temperature or laser light treatment is known.
[0006] In recent years, the development of transistors using oxide semiconductors (typically In-Ga-Zn oxide) has become Development is intensifying.
[0007] The history of oxide semiconductors is long. In 1988, crystalline In-Ga-Zn oxide was used in semiconductor devices. In 1995, the use of oxide A transistor using a semiconductor has been invented, and its electrical characteristics have been disclosed (Patent Document See reference 2. ).
[0008] The transistor using an oxide semiconductor includes a transistor using amorphous silicon and a It has different characteristics from transistors using crystalline silicon. For example, It is known that a display device using such a transistor has low power consumption. Conductors can be formed into films using methods such as sputtering, so they can be used to make transistors that form large display devices. In addition, a transistor using an oxide semiconductor can be used as a high-field transistor. Because of its high effective mobility, it is possible to form a high-performance device in which the driver circuit and pixel circuit are formed on the same substrate. In addition, some of the production facilities for amorphous silicon transistors can be used Since it is possible to improve and reuse it, it also has the advantage of reducing capital investment. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Patent Publication No. 63-239117 [Patent Document 2] Special table Hei 11-505377 Summary of the Invention [Problem to be solved by the invention]
[0010] One of the objectives is to provide a fine shape. Another object of the present invention is to provide a transistor having a small subthreshold swing value. Another object of the present invention is to provide a transistor having a small short channel effect. Another object of the present invention is to provide a transistor having normally-off electrical characteristics. Another object of the present invention is to provide a transistor having a small leakage current when it is off. Another object of the present invention is to provide a transistor having excellent electrical characteristics. Another object of the present invention is to provide a highly reliable transistor. Another object is to provide a transistor having high frequency characteristics.
[0011] Another object of the present invention is to provide a semiconductor device including the transistor. Another object of the present invention is to provide a module having the semiconductor device. Another object of the present invention is to provide a device having such a module, or an electronic device having such a module. It is an object of the present invention to provide a novel semiconductor device. Another object of the present invention is to provide a novel electronic device.
[0012] The description of these problems does not preclude the existence of other problems. It is not necessary for the embodiment to solve all of these problems. The above will become apparent from the description in the specification, drawings, claims, etc. It is possible to extract other issues from the descriptions in the patent, claims, etc. [Means for solving the problem]
[0013] One embodiment of the present invention is a method for forming a semiconductor on a substrate, forming a first conductor on the semiconductor, and forming a first A first insulator is formed on the conductor, a resist is formed on the first insulator, and the resist is exposed. By exposing to light and developing, the second and third regions of the resist are left to form the first insulating film. A portion of the substrate is exposed, a bias is applied in a direction perpendicular to the upper surface of the substrate, and carbon and halo are deposited. Plasma is generated by a gas containing fluorine, and organic matter is deposited by the plasma. In both cases, after etching the organic material, the organic material, the second region, and the third region are used as a mask. and etching the first insulator to form a second insulator and a third insulator, The first conductor is exposed, and the first conductor is then masked with the second insulator and the third insulator. The semiconductor is then etched to form the second and third conductors and to expose the semiconductor. removing the organic material, the second region and the third region; and forming a fourth insulating layer on the exposed portion of the semiconductor. forming a fourth conductor on the fourth insulator; and forming the organic material on the exposed portion of the first insulator. The etching rate exceeds the deposition rate at the side of the first region, and the deposition rate This is a method for manufacturing a semiconductor device that exceeds the etching rate.
[0014] In one embodiment of the present invention, in the above-described structure, the distance between the second conductor and the third conductor is The distance between the second region and the third region is 80% or less. Effect of the Invention
[0015] It is possible to provide a fine shape. It is possible to provide a transistor with a short channel length. Alternatively, it is possible to provide a transistor with a small subthreshold swing value. Alternatively, a transistor with a small short channel effect can be provided. In this way, a transistor having normally-off electrical characteristics can be provided. It is possible to provide a transistor with a small leakage current when conducting. It is possible to provide excellent transistors. Or, it is possible to provide highly reliable transistors. Alternatively, a transistor having high frequency characteristics can be provided. do.
[0016] Alternatively, a semiconductor device including the transistor can be provided. Alternatively, a module having the semiconductor device or the module may be provided. It is possible to provide an electronic device having a novel semiconductor device. Alternatively, a new module may be provided. Alternatively, a new electronic Equipment can be provided.
[0017] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have all of these effects. Effects other than these may be included in the description, This is self-evident from the description in the drawings, claims, etc. It is possible to extract other effects from any of the descriptions. [Brief description of the drawings]
[0018] [Figure 1] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Diagram 2] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Diagram 3] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 4] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Diagram 5] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 6] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 7] 1A to 1C are cross-sectional views illustrating a method for manufacturing a semiconductor device according to one embodiment of the present invention. [Figure 8] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 9] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 10] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 11] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 12] 1A to 1C are cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 13] 1A and 1B are a cross-sectional view and a band diagram illustrating a transistor according to one embodiment of the present invention. [Figure 14] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 15] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 16] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 17] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 18] 1A and 1B are top views and cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 19] 1A to 1C are cross-sectional views illustrating a method for manufacturing a transistor according to one embodiment of the present invention. [Figure 20] FIG. 1 is a circuit diagram illustrating a semiconductor device according to one embodiment of the present invention. [Figure 21] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 22] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 23] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 24] FIG. 1 is a circuit diagram illustrating a memory device according to one embodiment of the present invention. [Diagram 25] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 26] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 27] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 28] FIG. 1 is a top view illustrating a semiconductor device according to one embodiment of the present invention. [Figure 29] FIG. 1 is a block diagram illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 30] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 31] FIG. 1 is a cross-sectional view illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 32] 1A and 1B are a perspective view and a cross-sectional view illustrating a semiconductor device of one embodiment of the present invention. [Diagram 33] FIG. 1 is a block diagram illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 34] FIG. 1 is a circuit diagram illustrating a semiconductor device according to one embodiment of the present invention. [Diagram 35] 1A to 1C are a circuit diagram, a top view, and a cross-sectional view illustrating a semiconductor device of one embodiment of the present invention. [Diagram 36] 1A and 1B are a circuit diagram and a cross-sectional view illustrating a semiconductor device of one embodiment of the present invention. [Figure 37] FIG. 1 is a perspective view illustrating an electronic device according to one embodiment of the present invention. [Figure 38] Cs-corrected high-resolution TEM image of a cross section of CAAC-OS, and a schematic cross-sectional diagram of CAAC-OS. [Figure 39] Cs-corrected high-resolution TEM image of the CAAC-OS in the plane. [Diagram 40] 13A to 13C show structural analyses of a CAAC-OS and a single-crystal oxide semiconductor by XRD. [Diagram 41] Electron diffraction pattern of CAAC-OS. [Diagram 42] FIG. 1 shows the change in the crystal part of an In-Ga-Zn oxide due to electron irradiation. [Diagram 43] Schematic diagram explaining the film formation model of CAAC-OS and nc-OS. [Diagram 44] A diagram explaining InGaZnO4 crystals and pellets. [Diagram 45] Schematic diagram explaining a film formation model of CAAC-OS. [Figure 46] Cross-sectional STEM image. [Figure 47] Cross-sectional STEM image. [Figure 48] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 49] Transistor Id-Vg characteristics. [Figure 50] Transistor Id-Vg characteristics. [Figure 51] FIG. 1 is a cross-sectional view illustrating a transistor according to one embodiment of the present invention. [Figure 52] FIG. 1 is a cross-sectional view illustrating a transistor according to one embodiment of the present invention. [Figure 53] FIG. 1 is a cross-sectional view illustrating a transistor according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] The present invention will be described in detail with reference to the drawings. The present invention is not limited to the above, and various modifications in form and detail can be easily made by those skilled in the art. It is understood that the present invention should not be construed as being limited to the description of the following embodiments. In explaining the configuration of the invention using the drawings, the same reference numerals are used in different The hatch pattern is used in common among drawings. In some cases, no particular symbol is attached.
[0020] In the figures, the size, thickness of the film (layer), or area is exaggerated for clarity. There may be cases where
[0021] In this specification, the terms "film" and "layer" are interchangeable. It is possible.
[0022] Also, a voltage is a voltage between a certain potential and a reference potential (such as ground potential (GND) or source potential). Therefore, it is possible to say "voltage" as "potential". In general, potential (voltage) is relative, and the magnitude is measured relative to a reference potential. Therefore, even if it is described as "ground potential", The potential is not necessarily 0V. For example, the lowest potential in a circuit may be the "ground potential." Or, the intermediate potential in the circuit may be the "ground potential." With respect to the potential, a positive potential and a negative potential are defined for .
[0023] The ordinal numbers such as 1st and 2nd are used for convenience and do not indicate the order of steps or stacking. Therefore, for example, "the first" should not be changed to "the second" or "the third" In addition, the ordinal numbers described in this specification and the like can be replaced with the ordinal numbers. and the ordinal numbers used to identify an aspect of the invention may not match.
[0024] Even if a material is described as a "semiconductor," if its electrical conductivity is sufficiently low, it may be considered an "insulator." In addition, the boundary between "semiconductor" and "insulator" is unclear, and Therefore, the term "semiconductor" as used herein may not be distinguishable from "insulator." Similarly, the term "insulator" used in this specification may be interpreted as "semiconductor." " This can sometimes be rephrased as ".
[0025] In addition, even if a material is written as a "semiconductor," if the material has a sufficiently high electrical conductivity, it should be written as a "conductor." In addition, the boundary between "semiconductor" and "conductor" is unclear, and Therefore, the term "semiconductor" as used herein may not be distinguished from "conductor." Similarly, the term "conductor" used in this specification may be used interchangeably with "semiconductor." " This can sometimes be rephrased as ".
[0026] The impurities in a semiconductor are, for example, those other than the main components that make up the semiconductor. For example, Elements with a concentration of less than 0.1 atomic percent are considered impurities. The formation of DOS (Density of State) in the body and carrier mobility In some cases, the semiconductor may become an oxide semiconductor, or the crystallinity may decrease. In the case of a semiconductor, impurities that change the properties of the semiconductor include, for example, Group 1 elements, Group 2 elements, Elements, Group 14 elements, Group 15 elements, transition metals other than the main component, etc., in particular, for example, Hydrogen (also found in water), lithium, sodium, silicon, boron, phosphorus, carbon, nitrogen In the case of oxide semiconductors, for example, oxygen vacancies are formed due to the inclusion of impurities such as hydrogen. Also, if the semiconductor is silicon, impurities that change the properties of the semiconductor may occur. Examples of the elements include oxygen, elements of Group 1 except hydrogen, elements of Group 2, elements of Group 13, elements of Group 15, Group elements, etc.
[0027] In this specification, when it is stated that A has a region of concentration B, for example, If the concentration in the entire depth direction in the region is B, then the concentration in the depth direction in the region with A is If the average concentration of A is B, then the median concentration in the depth direction in a region of A is B. In the case where the maximum concentration in the depth direction in a region where A is, is B, If the minimum value of the concentration in the depth direction is B, the convergence of the concentration in the depth direction in a region of A is If the value is B, the concentration in the area where the most likely value of A is obtained by measurement is B. Including certain cases.
[0028] In this specification, A has an area of size B, length B, thickness B, width B or distance B. For example, when describing the overall size, length, thickness, width, etc. of a certain area of A, or the size, length, thickness, width, or distance of an area of A if the distance is B If the average value of is B, then the size, length, thickness, width, or distance of a certain area of A If the median is B, then the minimum size, length, thickness, width, or distance in a region of A The minimum size, length, thickness, width, or distance in a region of A when the maximum value is B If the value is B, then the convergence value of size, length, thickness, width, or distance in a region of A If B is the size, length, and thickness of the area where the value of A itself can be obtained by measurement, This includes cases where the length, width, or distance is B.
[0029] Note that the channel length is, for example, the length of a semiconductor (or transistor) in a top view of a transistor. When the transistor is on, the gate electrode (the part of the semiconductor through which current flows) overlaps with the The source region or source potential in the region where the This refers to the distance between the drain (drain region or drain electrode) and the In a transistor, the channel length does not necessarily have the same value in all regions. The channel length of each transistor may not be determined to a single value. In the document, the channel length is defined as any one value, maximum value, or The minimum or average value.
[0030] The channel width is the width of the semiconductor (or transistor) when it is in the on state. The region where the current flows and the gate electrode overlap, or the region where the channel is formed. This refers to the length of the part where the source and drain face each other in the region. In a transistor, the channel width does not necessarily have the same value in all regions. The channel width of each transistor may not be determined to be a single value. In the document, the channel width is defined as any one value, maximum value, or The minimum or average value.
[0031] Depending on the structure of the transistor, the channel in the region where the channel is actually formed may vary. The effective channel width (hereinafter referred to as the effective channel width) shown in the top view of the transistor The channel width (hereinafter referred to as the apparent channel width) may be different. For example, In a transistor having a three-dimensional structure, the effective channel width is The effect of the channel width becomes larger than the apparent channel width shown in For example, in transistors with a fine, three-dimensional structure, In some cases, the proportion of the channel region formed may be large. In that case, The effective channel width of the channel is smaller than the apparent channel width. The larger the size, the larger the
[0032] By the way, in a transistor having a three-dimensional structure, the effective channel width is For example, it may be difficult to estimate the effective channel width from the design value. In order to obtain this, it is necessary to assume that the shape of the semiconductor is known. Unless k is precisely known, it is difficult to accurately measure the effective channel width.
[0033] In this specification, therefore, in a top view of a transistor, a semiconductor and a gate electrode are not mutually connected. The apparent length of the overlapping area between the source and drain The channel width of the In this specification, it is sometimes referred to as the "channel width". In some cases, this may refer to the enclosed channel width or apparent channel width; or In this specification, when simply referring to a channel width, it may refer to an effective channel width. In addition, the channel length, channel width, effective channel width, apparent channel width, and enclosure The width of the inclusion channel can be determined by acquiring a cross-sectional TEM image and analyzing the image. Thus, the value can be determined.
[0034] In addition, the field effect mobility of the transistor and the current value per channel width are calculated. In some cases, the effective channel width is calculated using the enclosed channel width. The value may differ from that calculated using the channel width.
[0035] In this specification, when it is stated that A has a shape protruding from B, it is to be understood that the shape is not limited to a top view. or in a cross-sectional view, at least one end of A is outside at least one end of B. Therefore, it may be described as having a shape in which A protrudes more than B. For example, in the top view, one end of A is outside one end of B. It can be read as having.
[0036] In this specification, "parallel" means that two straight lines are arranged at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Line" refers to the state in which two straight lines are arranged at an angle between -30° and 30°. "Perpendicular" means that two straight lines are arranged at an angle of 80° or more and 100° or less. Therefore, the angle may be between 85° and 95°. This refers to a state in which two straight lines are arranged at an angle of 60° or more and 120° or less.
[0037] In addition, in this specification, when the crystal is a trigonal or rhombohedral crystal, it is represented as a hexagonal crystal system. .
[0038] <Processing method 1> A method for processing a conductor, an insulator, or a semiconductor according to one embodiment of the present invention will be described below. do.
[0039] First, a layer 116 and a layer 110 on the layer 116 are prepared (see FIG. 1(A)). The layer 6 may be made of a conductor, an insulator, or a semiconductor. A conductive material, an insulator, or a semiconductor may be used.
[0040] Examples of conductors include boron, nitrogen, oxygen, fluorine, silicon, phosphorus, and aluminum. , titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium, yttrium , zirconium, molybdenum, ruthenium, silver, indium, tin, tantalum and tantalum A conductor containing one or more types of tin may be used in a single layer or a multilayer structure. For example, an alloy or The conductor may be a compound, and may be an aluminum-containing conductor, a copper and titanium-containing conductor, a copper and Conductors containing indium, tin and oxygen; conductors containing titanium and nitrogen A conductor containing elements may also be used.
[0041] Examples of the insulator include boron, carbon, nitrogen, oxygen, fluorine, magnesium, and aluminum. Umium, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zinc Insulators containing lanthanum, neodymium, hafnium or tantalum are used in a single layer or in For example, aluminum oxide, magnesium oxide, Silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, gallium oxide , germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, neodymium oxide In particular, silicon-containing oxides such as hafnium oxide and tantalum oxide may be used. It is preferable to use:
[0042] Semiconductors include group 14 semiconductors such as silicon and germanium, silicon carbide, and silicide. Germanium, gallium arsenide, indium phosphide, zinc selenide, cadmium sulfide, oxide Compound semiconductors such as oxide semiconductors and organic semiconductors can be used. will be discussed later.
[0043] Next, the anti-reflective layer (BARC: Bottom Anti Reflective Coa Next, a resist is formed. Next, the resist is processed. The processing of the resist is first performed by exposing the resist to light using a photomask or the like. The effect of this is to suppress halation. The resist 122 is formed by removing or leaving the resist using a liquid. For example, KrF excimer laser light, ArF excimer laser light, EUV (Extreme Ultraviolet) A liquid (e.g. a traviolet) may be used between the substrate and the projection lens. A liquid immersion technique may be used, in which the substrate is filled with water and exposed to light. A child beam or an ion beam may be used. When an electron beam or an ion beam is used, In this case, no photomask is required.
[0044] Next, the anti-reflection layer is etched using the resist 122 as a mask, and the anti-reflection layer 12 0 is formed (see FIG. 1(B)). However, instead of the anti-reflection layer 120, In some cases, non-functional organic or inorganic materials may be used. There are cases where it is not necessary to have 0.
[0045] The distance between the resists 122 is L0. The minimum dimension of L0 (also called the minimum processing dimension) .) is determined by the exposure machine, resist, etc.
[0046] Next, plasma treatment is performed. The plasma treatment is a parallel plate reactive ion etching (RI E: Reactive Ion Etching and inductively coupled plasma (ICP: This is done by the Inductively Coupled Plasma (ICP) etching method. It is possible to do so.
[0047] The plasma is generated using a gas containing carbon and a halogen. The carbon and hydrogen contained in the resist 122 react with the surface to be treated (e.g., the resist 12 2, the side of the anti-reflective layer 120, and the exposed portion of the layer 110) The deposition of the organic material occurs isotropically. Here, the deposition of the organic material occurs isotropically. When a bias perpendicular to the top surface is applied, organic matter is deposited and etched. The etching rate of organic matter is higher in the direction in which the bias is applied. This occurs anisotropically because the
[0048] Examples of gases containing carbon and halogen include methane trifluoride gas and methane tetrafluoride gas. Hexafluoroethane gas, hexafluoropropane gas, octafluoropropane gas and octafluoropropane gas Gases containing carbon and fluorine, such as cyclobutane fluoride gas, and carbon tetrachloride Gases containing carbon and chlorine may be used. Also, gases such as helium or argon may be used. A rare gas, hydrogen, etc. may be mixed and used.
[0049] The deposition rate and etching rate of organic matter are determined by a combination of various conditions. For example, a high carbon content in the gas used to generate the plasma results in a high deposition rate, A higher ratio of fluorine increases the etch rate. The etching rate is lowered by increasing the bias, and the etching rate is increased by increasing the bias. The condition where the etching rate is higher than the deposition rate in the direction of the bias is used. Therefore, organics are not likely to deposit on the top surface of resist 122 and exposed portions of layer 110. At approximately the same time that the exposed portions of layer 110 are etched, the exposed portions of layer 110 are also etched. However, depending on the conditions of the plasma treatment, it may be possible to avoid etching the exposed portion of layer 110. In addition, the plasma processing conditions can be changed in multiple steps, such as two or three steps. do.
[0050] On the other hand, the etching rate of the organic matter on the side surface of the resist 122 and the side surface of the anti-reflection layer 120 is Therefore, organic matter 124 accumulates in the region (FIG. 1( See C). ).
[0051] Next, the organic 124, resist 122 and anti-reflective layer 120 are used as a mask to form a layer 110 and layer 116 are etched to remove layers 110a and 110b, as well as layer 116. Layers 110 and 116a and 116b are formed (see FIG. 1(D)). The etching can be performed by dry etching or / and wet etching. At this time, the organic material 124 may be removed. The layers 116a and 116b may be connected in the depth direction. It doesn't matter if they're connected.
[0052] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0053] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see Figure 1(E)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A coating method and / or a wet etching method can be used.
[0054] At this time, the layer 110a has a first region, a second region, and a third region. The region is located between the first region and the third region. The first region is a flat region. The second region and the third region are regions having a slope. The second region is tilted more than the third region. The slope in the second region is gentler than that in the first region. For example, the slope may be smaller near the first region than near the second region. The layer 110a may have a shape in which the slope is gentler in the vicinity of the third region. However, by having such a shape, the step of the layer formed above the layer 110a is prevented. The covering property can be improved. Therefore, defects in shape and the like are less likely to occur. The same applies to b. The inclination refers to the change in thickness, and the angle is a right angle. In some cases, it is expressed as having a slope.
[0055] <Processing method 2> In addition, as shown in FIG. 2, by changing the conditions of the plasma treatment, a different state from that shown in FIG. 1(E) can be obtained. It is also possible to obtain a shape.
[0056] Figures 2(A) and 2(B) are the same as Figures 1(A) and 1(B), respectively. , explanation will be omitted.
[0057] Next, plasma treatment is performed, which causes deposition and etching of organic matter. The exposed portions of layer 110 are also etched. Here, the sides and While depositing organic material 124 on the sides of anti-reflective layer 120, layer 1 is removed until layer 116 is exposed. 10 is etched to form layers 110a and 110b (see FIG. 2(C)). (The layers 110a and 110b may be connected in the depth direction.)
[0058] Next, the organic 124, resist 122 and anti-reflective layer 120 are used as a mask to form a layer The layer 116 is etched to form the layers 116a and 116b (see FIG. 2(D)). The layer 116 is etched by a dry etching method or / and a wet etching method. At this time, the organic matter 124 may be removed. and layer 116b may be connected in the depth direction.
[0059] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0060] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see Figure 2(E)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A coating method and / or a wet etching method can be used.
[0061] At this time, the layer 110a has a first region and a second region. The first region is flat. The first region is a region having a slope. The second region is a region having a varying degree of slope. For example, the gradient may be steeper near the first region and steeper away from the first region. In some cases, the layer 110a has a shape in which the slope becomes gentler as the layer 110a approaches the surface. By having the layer 110a, the step coverage of layers formed above the layer 110a can be improved. This makes it possible to prevent defects in shape and the like. The same applies to the layer 110b. do.
[0062] <Processing method 3> In addition, as shown in FIG. 3, by changing the conditions of the plasma treatment, Shapes different from that shown in FIG. 2(E) can also be obtained.
[0063] Figures 3(A) and 3(B) are the same as Figures 1(A) and 1(B), respectively. , explanation will be omitted.
[0064] Next, plasma treatment is performed, which causes deposition and etching of organic matter. The exposed portions of layer 110 are also etched. Here, the sides and The layers 110 and 116 are etched while the organic material 124 is deposited on the sides of the anti-reflective layer 120. By etching, layers 110a and 110b, as well as layers 116a and 116b are formed. b is formed (see FIG. 3(C)). Note that the layer 110a and the layer 110b are connected in the depth direction. In addition, the layers 116a and 116b may be connected in the depth direction. That's fine.
[0065] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0066] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see FIG. 3(D)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A coating method and / or a wet etching method can be used.
[0067] At this time, the layer 110a has a first region and a second region. The first region is flat. The first region is a region having a slope. The second region is a region having a varying degree of slope. For example, the gradient may be steeper near the first region and steeper away from the first region. The layer 116a may have a shape in which the slope becomes gentler as the layer 116a approaches the third region. and a fourth region. The third region is a flat region. The fourth region has a slope. The fourth area may have a varying degree of inclination. For example, the third area The slope is steep near the third region, and the slope becomes gentler as it moves away from the third region. When the layer 110a and the layer 116a have such a shape, It is possible to improve the step coverage of layers formed above the layer 110a and the layer 116a. As a result, defects in shape and the like are less likely to occur. The same is true for
[0068] <Processing method 4> In addition, as shown in FIG. 4, by adding an etching process, the same process as in FIG. 1(E) and FIG. It is also possible to obtain shapes different from those in FIG. 3(E) and FIG. 3(D).
[0069] Figures 4(A) and 4(B) are the same as Figures 1(A) and 1(B), respectively. , explanation will be omitted.
[0070] Next, using the resist 122 and the anti-reflective layer 120 as a mask, layer 116 is exposed. The layer 110 is etched so as to form layers 110a and 110b (see FIG. 4(C). Etching of layer 110 may be accomplished by dry etching or / and wet etching. The layer 110a and the layer 110b are formed in a depth direction. It does not matter if they are connected in the opposite direction.
[0071] Next, plasma treatment is performed, which causes deposition and etching of organic matter. The exposed portions of layer 116 are also etched. However, depending on the plasma treatment conditions, It is possible that the exposed portions of layer 116 are not etched.
[0072] On the other hand, the side of the resist 122, the side of the anti-reflection layer 120, the side of the layer 110a, and the side of the layer 11 On the side of 0b, the etching rate of the organic material is slower than the deposition rate. Organic matter 124 accumulates in the area.
[0073] Next, the organic 124, resist 122 and anti-reflective layer 120 are used as a mask to form a layer The layer 116 is etched to form the layers 116a and 116b (see FIG. 4(D)). The layer 116 is etched by a dry etching method or / and a wet etching method. At this time, the organic matter 124 may be removed. and layer 116b may be connected in the depth direction.
[0074] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0075] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see FIG. 4(E)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A coating method and / or a wet etching method can be used.
[0076] At this time, the layer 116a has a first region, a second region, and a third region. The region is located between the first region and the third region. The first region is a flat region. The second region and the third region are regions having a slope. The second region is tilted more than the third region. The slope in the second region is gentler than that in the first region. For example, the slope may be smaller near the first region than near the second region. The layer 116a may have a shape in which the slope is gentler in the vicinity of the third region. However, by having such a shape, the step of the layer formed above the layer 116a is prevented. The covering property can be improved. Therefore, defects in shape and the like are less likely to occur. The same is true for b.
[0077] <Processing method 5> In addition, as shown in FIG. 5, an etching process was added and the plasma processing conditions were changed. As a result, a shape different from that shown in FIG. 1(E), FIG. 2(E), FIG. 3(D) and FIG. 4(E) is obtained. It is also possible.
[0078] Figures 5(A) and 5(B) are the same as Figures 1(A) and 1(B), respectively. 5C is the same as FIG. 4C, so its description will be omitted. .
[0079] Next, plasma treatment is performed, which causes deposition and etching of organic matter. In addition, the exposed portion of layer 116 is etched to form layers 116a and 116b. It should be noted that the layers 116a and 116b may be connected in the depth direction.
[0080] On the other hand, the side of the resist 122, the side of the anti-reflection layer 120, the side of the layer 110a, and the side of the layer 11 On the side of 0b, the etching rate of the organic material is slower than the deposition rate. In the area, organic matter 124 accumulates (see FIG. 5(D)).
[0081] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0082] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see FIG. 5(E)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A coating method and / or a wet etching method can be used.
[0083] At this time, the layer 116a has a first region and a second region. The first region is flat. The first region is a region having a slope. The second region is a region having a varying degree of slope. For example, the gradient may be steeper near the first region and steeper away from the first region. In some cases, the layer 116a has a shape in which the slope becomes gentler as the layer 116a approaches the surface. By having the layer 116a, the step coverage of layers formed above the layer 116a can be improved. Therefore, defects in shape and the like are less likely to occur. The same is true for layer 116b. do.
[0084] <Processing method 6> Also, as shown in FIG. 6, by not having the layer 110, the structure shown in FIG. It is also possible to obtain shapes different from those in Figs. 3(D), 4(E) and 5(E).
[0085] First, the layer 116 is prepared (see FIG. 6(A)).
[0086] Next, an anti-reflection layer is formed. Next, a resist is formed. Next, the resist is processed to remove the reflection. Forms gyst 122.
[0087] Next, the anti-reflection layer is etched using the resist 122 as a mask, and the anti-reflection layer 12 0 is formed (see FIG. 6(B)). However, in some cases, the anti-reflection layer 120 is not required. There is.
[0088] The distance between the resists 122 is defined as L0.
[0089] Next, plasma treatment is performed, which causes deposition and etching of organic matter. The exposed portions of layer 110 are also etched. However, depending on the plasma treatment conditions, It is possible that the exposed portions of layer 110 are not etched.
[0090] On the other hand, the etching rate of the organic matter on the side surface of the resist 122 and the side surface of the anti-reflection layer 120 is Therefore, organic matter 124 accumulates in the region (FIG. 6( See C). ).
[0091] Next, the organic 124, resist 122 and anti-reflective layer 120 are used as a mask to form a layer The layer 116 is etched to form the layers 116a and 116b (see FIG. 6(D)). The layer 116 is etched by a dry etching method or / and a wet etching method. At this time, the organic matter 124 may be removed. and layer 116b may be connected in the depth direction.
[0092] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0093] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see FIG. 6(E)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A wet etching method and / or a wet etching method can be used. After obtaining the shape, the layers 110a and 110b may be removed to obtain a structure similar to that shown in FIG. shape can be obtained.
[0094] At this time, the layer 116a has a first region, a second region, and a third region. The region is located between the first region and the third region. The first region is a flat region. The second region and the third region are regions having a slope. The second region is tilted more than the third region. The slope in the second region is gentler than that in the first region. For example, the slope may be smaller near the first region than near the second region. The layer 116a may have a shape in which the slope is gentler in the vicinity of the third region. However, by having such a shape, the step of the layer formed above the layer 116a is prevented. The covering property can be improved. Therefore, defects in shape and the like are less likely to occur. The same is true for b.
[0095] <Processing method 7> In addition, as shown in FIG. 7, by changing the conditions of the plasma treatment, A shape different from that shown in Figs. 2(E), 3(D), 4(E), 5(E) and 6(E) was obtained. It is also possible.
[0096] Figures 7(A) and 7(B) are the same as Figures 6(A) and 6(B), respectively. , explanation will be omitted.
[0097] Next, plasma treatment is performed, which causes deposition and etching of organic matter. The exposed portion of layer 116 is also etched to form layers 116a and 116b. It should be noted that the layers 116a and 116b may be connected in the depth direction.
[0098] On the other hand, the etching rate of the organic matter on the side surface of the resist 122 and the side surface of the anti-reflection layer 120 is Therefore, organic matter 124 accumulates in the region (FIG. 7( See C). ).
[0099] The distance between the layer 116a and the layer 116b is L1. L1 is divided by the organic matter 124. That is, it is smaller than the minimum dimension determined by the exposure machine, resist, etc. A good shape can be obtained.
[0100] Next, the organic material 124, the resist 122 and the anti-reflective layer 120 are removed to minimize processing. It is possible to form holes smaller than the dimensions (see FIG. 7(D)). The removal of the barrier layer 122 and the anti-reflection layer 120 is performed by dry etching such as plasma ashing. A wet etching method and / or a wet etching method can be used. After obtaining the shape, the layers 110a and 110b may be removed to obtain a structure similar to that shown in FIG. shape can be obtained.
[0101] At this time, the layer 116a has a first region and a second region. The first region is flat. The first region is a region having a slope. The second region is a region having a varying degree of slope. For example, the gradient may be steeper near the first region and steeper away from the first region. In some cases, the layer 116a has a shape in which the slope becomes gentler as the layer 116a approaches the surface. By having the layer 116a, the step coverage of layers formed above the layer 116a can be improved. Therefore, defects in shape and the like are less likely to occur. The same is true for layer 116b. do.
[0102] As described above, by the processing method according to one aspect of the present invention, the shape of a layer can be adjusted to the minimum processing size. It is possible to process the layers in smaller dimensions than the conventional method. can be formed.
[0103] <Transistor 1> A transistor according to one embodiment of the present invention will be described below.
[0104] FIG. 8(A), FIG. 9(A), FIG. 10(A), and FIG. 11(A) show a method for manufacturing a transistor. Each of the top views illustrates the dashed lines A1-A2 and A3-A4. The corresponding cross-sectional views are shown in Figs. 8(B), 9(B), 10(B) and 11. As shown in (B).
[0105] First, a substrate 400 is prepared.
[0106] The substrate 400 may be, for example, an insulating substrate, a semiconductor substrate, or a conductive substrate. Examples of the insulating substrate include a glass substrate, a quartz substrate, a sapphire substrate, and a stabilized zirconia substrate. There are also semiconductor substrates, such as zirconia substrates stabilized with yttria, and resin substrates. The substrate may be, for example, a single semiconductor substrate such as silicon or germanium, or a silicon carbide substrate. Silicon, silicon germanium, gallium arsenide, indium phosphide, zinc oxide, gallium oxide Furthermore, there are compound semiconductor substrates such as silicon substrates, etc. A semiconductor substrate having such a structure, for example, a SOI (Silicon On Insulator) substrate, Conductive substrates include graphite substrates, metal substrates, alloy substrates, conductive resin substrates, etc. Alternatively, there are substrates having metal nitrides, substrates having metal oxides, etc. The substrate includes an insulating substrate having a conductor or semiconductor provided thereon, a semiconductor substrate having a conductor or insulator provided thereon, Examples of such substrates include a substrate provided with an edge, and a substrate in which a semiconductor or an insulator is provided on a conductive substrate. Alternatively, a substrate having elements provided thereon may be used. Examples of the elements include a capacitance element, a resistance element, a switch element, a light-emitting element, and a memory element.
[0107] A flexible substrate may be used as the substrate 400. The method of providing the transistor is to fabricate the transistor on a non-flexible substrate and then Alternatively, the resistor may be peeled off and transferred to the flexible substrate 400. A peeling layer may be provided between the non-flexible substrate and the transistor. Alternatively, a sheet, film, or foil having woven fibers may be used. The substrate 400 may be stretchable. Also, the substrate 400 may be designed to retain its original shape when the bending or pulling is stopped. The substrate 4 may have a property of returning to its original shape. Alternatively, the substrate 4 may have a property of not returning to its original shape. The thickness of 00 is, for example, 5 μm or more and 700 μm or less, preferably 10 μm or more and 500 μm or less. More preferably, the thickness is set to 15 μm or more and 300 μm or less. The weight of the semiconductor device can be reduced. In addition, by making the substrate 400 thin, the weight of the semiconductor device can be reduced. When using a material with a stretchy surface, it may be possible for the material to return to its original shape when bending or pulling is stopped. Therefore, the semiconductor device on the substrate 400 may be damaged if it is dropped or the like. In other words, a robust semiconductor device can be provided. do.
[0108] The substrate 400, which is a flexible substrate, may be made of, for example, a metal, an alloy, a resin, or a glass. The substrate 400, which is a flexible substrate, has a linear expansion coefficient of 1.0. The lower the coefficient of thermal expansion, the more preferable it is because deformation due to the environment is suppressed. For example, the linear expansion coefficient is 1×10 -3 / K or less, 5×10 -5 / K or less, or 1×1 0 -5 The resin may be, for example, polyester or polystyrene. Olefin, polyamide (nylon, aramid, etc.), polyimide, polycarbonate, Acrylic, etc. In particular, aramid has a low linear expansion coefficient, so it is suitable for flexible substrates. 400 is preferable.
[0109] Next, a conductive film is formed. The conductive film is formed by a method such as sputtering or chemical vapor deposition (CVD). Chemical Vapor Deposition, Molecular Beam Epitaxy (MB E: Molecular Beam Epitaxy (MBE) or Pulsed Laser Deposition (PL D: Pulsed Laser Deposition) method, atomic layer deposition (ALD: At This can be done using a omic layer deposition method or the like.
[0110] The CVD method is a method that uses plasma CVD (PECVD: Plasma ECVD). enhanced CVD method, and thermal CVD (TCVD: Thermal CVD) method D) method, photo CVD method, etc. Depending on the source gas, metal CVD (MCVD) method, metal organic CVD ( MOCVD (Metal Organic CVD) method.
[0111] The PECVD method can obtain high-quality films at relatively low temperatures. This is a film formation method that can reduce plasma damage to the workpiece because it does not use plasma. For example, wiring, electrodes, elements (transistors, capacitors, etc.) included in a semiconductor device may become charged up by receiving electric charge from the plasma. The accumulated electric charge may destroy the wiring, electrodes, elements, etc. contained in the semiconductor device. On the other hand, in the case of the TCVD method, which does not use plasma, such plasma damage does not occur. Therefore, the yield of semiconductor devices can be increased. Since no plasma damage occurs, a film with few defects can be obtained.
[0112] In addition, the ALD method is also a film formation method that can reduce plasma damage to the workpiece. In addition, the ALD method does not cause plasma damage during film formation, so films with fewer defects can be produced. Obtained.
[0113] The CVD and ALD methods are deposition methods in which particles emitted from a target are deposited. Unlike the conventional method, this is a film formation method in which a film is formed by a reaction on the surface of the object to be treated. This is a film forming method that is less susceptible to the shape of the workpiece and has good step coverage. The ALD method has excellent step coverage and thickness uniformity, making it suitable for the production of films with high aspect ratios. However, the ALD method has a relatively low deposition rate. Because the deposition rate is slow, it can be used in combination with other deposition methods such as CVD, which has a high deposition rate. In some cases this is preferable.
[0114] In the CVD and ALD methods, the composition of the resulting film can be controlled by the flow rate ratio of the source gases. For example, in the CVD and ALD methods, the desired flow rate can be obtained by adjusting the flow rate ratio of the source gases. In addition, for example, in the CVD method and the ALD method, the film formed can be By changing the flow rate ratio of the source gas while maintaining the temperature, a film with a continuously changing composition can be formed. When forming a film while changing the flow rate ratio of the source gas, multiple film forming chambers can be used. Compared to deposition by a vacuum, the time required for deposition is shortened by the time required for transportation and pressure adjustment. Therefore, the productivity of the semiconductor device can be increased in some cases.
[0115] Next, a resist or the like is formed on the conductor, and the conductor 413 is formed by processing using the resist. In addition, when simply forming a resist, it is assumed that an anti-reflection layer is formed under the resist. This also includes cases where
[0116] The resist is removed after the object is processed by etching or other methods. In this case, plasma treatment and / or wet etching are used. Plasma ashing is suitable for this purpose. If removal of resist, etc. is insufficient, Hydrofluoric acid and / or ozone at a concentration of 1% to 1% by volume Any remaining resist may be removed using water or the like.
[0117] When processing a conductor to form the conductor 413, the processing method shown in any one of FIGS. may also be used.
[0118] The conductor 413 may be, for example, boron, nitrogen, oxygen, fluorine, silicon, Phosphorus, aluminum, titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium tungsten, yttrium, zirconium, molybdenum, ruthenium, silver, indium, tin, Conductors containing one or more of tantalum and tungsten may be used in a single layer or a multilayer structure. For example, the conductor may be an alloy or compound, and may include aluminum, copper and titanium. Conductors containing copper and manganese, Conductors containing indium, tin and oxygen Conductors containing titanium and nitrogen, etc. may also be used.
[0119] Next, the insulator 402 is formed. The insulator 402 can be formed by a sputtering method, a CVD method, or the like. This can be carried out by using the MBE method, the PLD method, the ALD method, or the like.
[0120] The insulator 402 may be, for example, boron, carbon, nitrogen, oxygen, fluorine, magnesium, or aluminium. Aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium , zirconium, lanthanum, neodymium, hafnium or tantalum, For example, the insulator 402 may be made of aluminum oxide, oxide magnesium oxide, silicon oxide nitride, silicon nitride oxide, silicon nitride, Gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide , neodymium oxide, hafnium oxide or tantalum oxide may be used.
[0121] The insulator 402 may have a function of preventing diffusion of impurities from the substrate 400 .
[0122] Next, a semiconductor film is formed. The semiconductor film is formed by sputtering, CVD, MBE or This can be carried out by using a PLD method, an ALD method, or the like.
[0123] Next, it is preferable to perform heat treatment. By performing heat treatment, the hydrogen concentration in the semiconductor is reduced. In some cases, it may be possible to reduce oxygen vacancies in semiconductors. There are cases.
[0124] Next, a resist or the like is formed on the semiconductor, and the semiconductor 406 is formed by processing using the resist. (See FIG. 8(A) and FIG. 8(B)). At this time, the insulating layer 406 that does not overlap the semiconductor 406 is A part of the insulator 402 may be etched. By doing so, a protrusion is formed on the insulator 402. By forming a protrusion on the insulator 402, an s-channel structure, which will be described later, is formed. This makes it easier to achieve this.
[0125] When processing a semiconductor to form a semiconductor 406, the processing method shown in any one of FIGS. may also be used.
[0126] Next, a conductor 416 is formed. The conductor 416 can be formed by a sputtering method, a CVD method, or the like. This can be carried out by using the MBE method, the PLD method, the ALD method, or the like.
[0127] The conductor 416 may be, for example, boron, nitrogen, oxygen, fluorine, silicon, phosphorus, or aluminum. nium, titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium, yttrium Lithium, Zirconium, Molybdenum, Ruthenium, Silver, Indium, Tin, Tantalum and A conductor containing one or more of tungsten and silicon may be used in a single layer or a multilayer structure. For example, Conductors that may be alloys or compounds include aluminum-containing conductors, copper- and titanium-containing conductors, etc. , conductors containing copper and manganese, conductors containing indium, tin and oxygen, conductors containing titanium and Conductors containing nitrogen may also be used.
[0128] Next, the insulator 410 is formed (see FIG. 9(A) and FIG. 9(B)). The film is formed by sputtering, CVD, MBE, PLD, ALD, etc. It can be done.
[0129] The insulator 410 may be, for example, boron, carbon, nitrogen, oxygen, fluorine, magnesium, or aluminium. Aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium , zirconium, lanthanum, neodymium, hafnium or tantalum, For example, the insulator 410 may be made of aluminum oxide, oxide film, or a laminate. magnesium oxide, silicon oxide nitride, silicon nitride oxide, silicon nitride, Gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, lanthanum oxide , neodymium oxide, hafnium oxide or tantalum oxide may be used.
[0130] Next, a resist or the like is formed on the insulator 410, and the resist is used for processing to form the insulator 41 410a and insulator 410b, and conductor 416a and conductor 416b are formed ( See Figures 10(A) and 10(B).
[0131] In this case, the processing method shown in any one of Figs. 1 to 7 may be used. For example, 7, layer 116 is replaced with conductor 416 and layer 110 is replaced with insulator 410. Here, the insulator 410 and the conductor 416 are processed by the same method as that shown in FIG. The figure shows the case where the above is processed.
[0132] For example, the conductor 413 is a gate electrode, the insulator 402 is a gate insulator, and the conductor 416a is a semiconductor. If the bottom electrode is the source electrode and the conductor 416b is the drain electrode, the process is completed up to FIG. The transistor may have a gate structure.
[0133] Next, an insulator is formed. The insulator is formed by a method such as sputtering, CVD, MBE or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0134] Next, a conductive film is formed. The conductive film may be formed by a sputtering method, a CVD method, an MBE method, or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0135] Next, a resist or the like is formed on the conductor, and the conductor 404 is formed by processing using the resist. In addition, the resist or conductor 404 is used to process an insulator, and an insulator 412 is formed. (See FIG. 11(A) and FIG. 11(B)). Note that, in this embodiment, the insulator 412 and the conductor The conductive member 404 is processed so that it has the same shape when viewed from above, but this shape is not limited to this. For example, the insulator 412 and the conductor 404 may be formed using different resists. For example, after forming the insulator 412, a conductor that will become the conductor 404 may be formed. Alternatively, a resist may be formed on the insulator that will become the insulator 412 after the conductor 404 is formed. A hole or the like may be formed.
[0136] In this case, the processing method shown in any one of Figs. 1 to 7 may be used. For example, 7, layer 116 is replaced with an insulator, which becomes insulator 412, and layer 110 is replaced with a conductor, which becomes conductor 404. Just replace it with an electric device.
[0137] Examples of the insulator that can be the insulator 412 include boron, carbon, nitrogen, oxygen, fluorine, and magnesium. Nesium, aluminum, silicon, phosphorus, chlorine, argon, gallium, germanium, Insulators containing yttrium, zirconium, lanthanum, neodymium, hafnium or tantalum The insulator may be a single layer or a multilayer. For example, the insulator 412 may be are aluminum oxide, magnesium oxide, silicon oxide, silicon oxynitride, and silicon oxynitride. Silicon, silicon nitride, gallium oxide, germanium oxide, yttrium oxide, dioxide The material may be zinc oxide, lanthanum oxide, neodymium oxide, hafnium oxide or tantalum oxide. That's good.
[0138] The conductor that becomes the conductor 404 may be, for example, boron, nitrogen, oxygen, fluorine, silicon, Phosphorus, aluminum, titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium tungsten, yttrium, zirconium, molybdenum, ruthenium, silver, indium, tin, Conductors containing one or more of tantalum and tungsten may be used in a single layer or a multilayer structure. For example, the conductor may be an alloy or compound, and may include aluminum, copper and titanium. Conductors containing copper and manganese, Conductors containing indium, tin and oxygen Conductors containing titanium and nitrogen, etc. may also be used.
[0139] Next, an insulator film may be formed. The insulator film may be formed by a sputtering method, a CVD method, or an MBE method. The method can be carried out by using a PLD method, an ALD method, or the like.
[0140] Examples of the insulator include boron, carbon, nitrogen, oxygen, fluorine, magnesium, and aluminum. Umium, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zinc Insulators containing lanthanum, neodymium, hafnium or tantalum are used in a single layer or in The insulator is preferably aluminum oxide, silicon nitride oxide, Silicon nitride, gallium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, acid Insulators containing neodymium oxide, hafnium oxide or tantalum oxide are used in single or multilayered configurations. Just use it.
[0141] The insulator preferably functions as a barrier layer. and / or has a function of blocking hydrogen. Alternatively, the insulator may be, for example, insulator 402 Alternatively, it is preferable that the insulating material 412 has a higher ability to block oxygen and / or hydrogen than the insulating material 412. I wish.
[0142] Through the above steps, a transistor according to one embodiment of the present invention can be manufactured.
[0143] The transistor shown in FIG. 11B has an insulator 4 between the conductor 416a and the conductor 404. 10a, and has an insulator 410b between the conductor 416b and the conductor 404. That is, The parasitic capacitance caused by the conductor 416a and the conductor 416b is small. A semiconductor device using the transistor shown in FIG. 1(B) has high frequency characteristics.
[0144] As shown in FIG. 11B, the side surface of the semiconductor 406 is covered with the conductor 416a and the conductor 416 b. Also, the electric field of the conductor 404 electrically surrounds the semiconductor 406. (The electric field generated by the conductor electrically surrounds the semiconductor, creating a transistor structure.) This structure is called a surrounded channel (s-channel) structure. Therefore, a channel is formed on the entire surface (top, bottom and side surfaces) of the semiconductor 406. The channel structure allows a large current to flow between the source and drain of the transistor. Therefore, the current during conduction (on-state current) can be increased.
[0145] In addition, when the transistor has an s-channel structure, the transistor is also provided on the side surface of the semiconductor 406. Thus, the thicker the semiconductor 406, the larger the channel region. That is, the thicker the semiconductor 406 is, the higher the on-state current of the transistor can be. The thicker the semiconductor 406, the greater the proportion of regions with high carrier controllability, and therefore the sub-layer The threshold swing value can be reduced. For example, it can be set to 10 nm or more, preferably 2 0 nm or more, more preferably 40 nm or more, more preferably 60 nm or more, and even more preferably The semiconductor 406 may have a thickness of 100 nm or more. For example, the thickness is set to 300 nm or less, preferably 200 nm or less, because this may reduce the productivity of the device. More preferably, the semiconductor 406 has a region with a thickness of 150 nm or less. In addition, as the channel formation region shrinks, the thinner the semiconductor 406, the smaller the transistor. In some cases, the electrical characteristics may be improved. Therefore, even if the thickness of the semiconductor 406 is less than 10 nm, good.
[0146] Because of the high on-current, the s-channel structure is suitable for miniaturized transistors. Since the transistor can be miniaturized, a semiconductor having the transistor can be The device can be a highly integrated, high-density semiconductor device. The transistor has a channel length of preferably 40 nm or less, more preferably 30 nm or less. More preferably, the region is 20 nm or less, and the transistor preferably has a channel width of Preferably, the thickness is 40 nm or less, more preferably 30 nm or less, and even more preferably 20 nm or less. has.
[0147] Note that the conductor 413 is not necessarily formed (see FIG. 12A). The insulator may be formed so as to protrude from the conductor 404 (see FIG. 12B). There is no need to process the insulator 412 (see FIG. 12(C)).
[0148] As a representative example, in FIG. 11B, a conductor 416a and a conductor 416b having the same shape as in FIG. 16b, and insulators 410a and 410b are shown, but one embodiment of the present invention is For example, as shown in FIG. 51(A), a similar structure to that shown in FIG. 2(E) may be used. Also, as shown in FIG. 51(B), the shape may be the same as that shown in FIG. 3(D). Also, as shown in FIG. 51(C), it may have a shape similar to that of FIG. 4(D). As shown in Fig. 52(A), the shape may be the same as that shown in Fig. 5(E). As shown in FIG. 52(C), the shape may be the same as that shown in FIG. 6(E). 7(D). Also, as shown in FIG. 53(A), the insulator 41 Alternatively, the insulator 410a and the insulator 410b may have a shape that gradually becomes steeper toward the end. As shown in FIG. 53B, the ends of the insulators 410a and 410b are In addition, as shown in FIG. 53(C), the inclination angle may be changed stepwise. In addition, the conductor 416a and the conductor 416b may have a stacked structure. Alternatively, the lower layer may protrude from the upper layer. Also, these shapes may be partially combined. This type of shape can be created by changing the plasma processing conditions and etching process. This can be achieved by adding steps.
[0149] <Semiconductors> By arranging semiconductors above and below the semiconductor 406, the electrical characteristics of the transistor can be improved. In the following, the semiconductor 406 and the semiconductors arranged above and below it will be described. This will be described in detail with reference to FIG.
[0150] FIG. 13A shows the semiconductor of the transistor shown in FIG. 11B in the channel length direction. FIG. 13B is an enlarged cross-sectional view of the vicinity of 406. 4 is an enlarged cross-sectional view of the transistor in the channel width direction near a semiconductor 406.
[0151] In the transistor structures shown in FIG. 13(A) and FIG. 13(B), an insulator 402 and a semiconductor A semiconductor 406a is disposed between the conductor 416a and the conductor 416b. A semiconductor 406 c is disposed between the insulator 412 and the semiconductor 406 .
[0152] Alternatively, the transistor may have the structure shown in FIG. 13(C) and FIG. 13(D). .
[0153] FIG. 13C shows the semiconductor of the transistor shown in FIG. 11B in the channel length direction. FIG. 13(D) is an enlarged cross-sectional view of the vicinity of 406. 4 is an enlarged cross-sectional view of the transistor in the channel width direction near a semiconductor 406.
[0154] In the transistor structures shown in FIG. 13C and FIG. 13D, an insulator 402 and a semiconductor A semiconductor 406a is disposed between the insulator 402, the conductor 416a, and the semiconductor 406b. A semiconductor is provided between the conductor 416b, the semiconductor 406a, and the insulator 412. 406c is placed.
[0155] The semiconductor 406 is, for example, an oxide semiconductor containing indium. For example, when indium is contained, the carrier mobility (electron mobility) increases. 6 preferably contains the element M. The element M is preferably aluminum, gallium, yttrium, Thorium or tin. Other elements that can be used for M include boron, Silicon, titanium, iron, nickel, germanium, zirconium, molybdenum, lanthanum , cerium, neodymium, hafnium, tantalum, tungsten, etc. However, the elements In some cases, M may be a combination of the above elements. The element M may be, for example, an acid. For example, the bond energy with oxygen is Alternatively, the element M may be, for example, an element having an energy gap In addition, the semiconductor 406 preferably contains zinc. When an oxide semiconductor contains zinc, it may be easily crystallized.
[0156] However, the semiconductor 406 is not limited to an oxide semiconductor containing indium. For example, zinc-containing oxides that do not contain indium, such as zinc tin oxide and gallium tin oxide, are used. an oxide semiconductor containing gallium, an oxide semiconductor containing tin, etc. That's fine.
[0157] The semiconductor 406 is, for example, an oxide having a large energy gap. The energy gap is, for example, 2.5 eV or more and 4.2 eV or less, preferably 2.8 eV. The voltage is set to 3.8 eV or less, and more preferably 3 eV or more and 3.5 eV or less.
[0158] For example, the semiconductor 406a and the semiconductor 406c are made of elements other than oxygen that constitute the semiconductor 406. The semiconductor 406 is an oxide semiconductor composed of one or more elements. The semiconductor 406a and the semiconductor 406c are made of one or more elements other than oxygen. Therefore, the interface between the semiconductor 406a and the semiconductor 406 and the interface between the semiconductor 406 and the semiconductor At the interface with 406c, defect levels are unlikely to be formed.
[0159] The semiconductor 406a, the semiconductor 406, and the semiconductor 406c contain at least indium. It is preferable that the sum of In and M is 1 when the semiconductor 406a is an In-M-Zn oxide. When the atomic percentage of In is 0.00, it is preferable that In is less than 50 atomic percent and M is less than 50 atomic percent. %, and more preferably In is less than 25 atomic % and M is 75 atomic % or more. In addition, when the semiconductor 406 is an In-M-Zn oxide, In and When the sum of In and M is 100 atomic %, In is preferably 25 atomic % or more. and M is less than 75 atomic %, and more preferably In is more than 34 atomic %. The semiconductor 406c is an In-M-Zn oxide. When the sum of In and M is 100 atomic %, In is preferably 50 atomic %, M is higher than 50 atomic %, and more preferably In is 25 atomic %. The semiconductor 406c is a semiconductor The same oxide as that of the conductor 406a may be used. However, the oxide of the semiconductor 406a and / or In some cases, semiconductor 406c does not need to contain indium. The semiconductor 406a and / or the semiconductor 406c may be gallium oxide. 06a, the number of atoms of each element contained in the semiconductor 406 and the semiconductor 406c is a simple integer ratio It doesn't matter if it doesn't become like that.
[0160] The semiconductor 406 is an oxide having a higher electron affinity than the semiconductor 406a and the semiconductor 406c. For example, the semiconductor 406 is a semiconductor having a higher current density than the semiconductor 406a and the semiconductor 406c. The electron affinity is 0.07 eV or more and 1.3 eV or less, preferably 0.1 eV or more and 0.7 eV or less More preferably, an oxide having a larger electron energy than the electron transport energy is used, the larger energy being 0.15 eV or more and 0.4 eV or less. The affinity is the energy difference between the vacuum level and the bottom of the conduction band.
[0161] Indium gallium oxide has a small electron affinity and a high oxygen blocking property. Therefore, it is preferable that the semiconductor 406c contains indium gallium oxide. The atomic ratio [Ga / (In+Ga)] is, for example, 70% or more, preferably 80% or more, and Preferably, the ratio is 90% or more.
[0162] At this time, when a gate voltage is applied, the semiconductor 406a, the semiconductor 406, and the semiconductor 406c Of these, a channel is formed in the semiconductor 406 having a large electron affinity.
[0163] Here, between the semiconductor 406a and the semiconductor 406, In addition, a semiconductor 406 may be provided between the semiconductor 406 and the semiconductor 406c. The mixed region may have a defect state density of 406 and a semiconductor 406c. Therefore, the stack of the semiconductor 406a, the semiconductor 406, and the semiconductor 406c is In the vicinity of each interface, the energy changes continuously (also called a continuous junction). The semiconductor 406a, the semiconductor 406, and the semiconductor In the conductor 406c, the interface between them may not be clearly distinguishable.
[0164] At this time, the electrons are not in the semiconductor 406a and the semiconductor 406c but in the semiconductor 406. As described above, the semiconductor 406a and the semiconductor 406 mainly move at the interface. The defect state density at the interface between the semiconductor 406 and the semiconductor 406c is reduced. By reducing the thickness, the movement of electrons in the semiconductor 406 is less hindered, and the transistor This allows the on-state current of the transistor to be increased.
[0165] The on-current of a transistor can be increased by reducing the factors that inhibit the movement of electrons. For example, if there are no factors that impede the movement of electrons, it is assumed that electrons will move efficiently. The movement of electrons is also hindered, for example, when the channel formation region has large physical irregularities. will be done.
[0166] In order to increase the on-current of the transistor, for example, the upper or lower surface ( The root mean square of the surface to be formed (here, the semiconductor 406a) in an area of 1 μm×1 μm (RMS: Root Mean Square) roughness is less than 1 nm, preferably less than 0.6 nm m, more preferably less than 0.5 nm, and even more preferably less than 0.4 nm. In addition, the average surface roughness (also called Ra) in an area of 1 μm × 1 μm is preferably less than 1 nm. Preferably less than 0.6 nm, more preferably less than 0.5 nm, even more preferably less than 0.4 nm The maximum height difference (PV) in the area of 1 μm x 1 μm should be less than 1 μm. ) is less than 10 nm, preferably less than 9 nm, more preferably less than 8 nm, and even more preferably The RMS roughness, Ra and PV are measured by SII Nanotech. Measurements are performed using a scanning probe microscope system such as SPA-500 manufactured by Nology Corporation. It is possible.
[0167] In addition, in order to increase the on-state current of the transistor, the thickness of the semiconductor 406c is preferably as small as possible. For example, it is less than 10 nm, preferably 5 nm or less, and more preferably 3 nm or less. On the other hand, the semiconductor 406c may be a semiconductor having a channel region. The semiconductor 406 is then charged with elements other than oxygen (such as hydrogen, silicon, etc.) that make up the adjacent insulator. ) to prevent the intrusion of the semiconductor 406c. For example, the thickness is 0.3 nm or more, preferably 1 nm or more, and More preferably, the semiconductor 406c has a thickness of 2 nm or more. The conductor 406c is made of an oxygen-containing material to suppress outward diffusion of oxygen released from the insulator 402 and the like. It is preferable that the polyimide has a property of blocking oxygen.
[0168] In order to increase reliability, the semiconductor 406a is thick and the semiconductor 406c is thin. For example, it is preferably 10 nm or more, more preferably 20 nm or more, and even more preferably 40 nm or more. The semiconductor 406a may have a region with a thickness of 60 nm or more, more preferably 60 nm or more. By increasing the thickness of the semiconductor 406a, the semiconductor 406a can be prevented from being heated at the interface between the adjacent insulator and the semiconductor 406a. The distance from the semiconductor 406 where the channel is formed can be increased. For example, the thickness is set to 200 nm or less, preferably 120 nm or less, because this may reduce the productivity of the device. More preferably, the semiconductor 406a has a region with a thickness of 80 nm or less. .
[0169] For example, a secondary ion mass spectrometry (SIMS) method is used to measure the distance between the semiconductor 406 and the semiconductor 406a. 1×10 16 atoms / cm 3 More than 1×10 19 atoms / cm 3 Less than or equal to 1×10 16 atoms / cm 3 5×10 or more 18 atoms / cm 3 More preferably, 1 ×10 16 atoms / cm 3 More than 2×10 18 atoms / cm3 Silicon concentration below In addition, between the semiconductor 406 and the semiconductor 406c, , 1×10 16 atoms / cm 3 More than 1×10 19 atoms / cm 3 The following is preferably is 1×10 16 atoms / cm 3 5×10 or more 18 atoms / cm 3 Below are some more Preferably 1×10 16 atoms / cm 3 More than 2×10 18 atoms / cm 3 The following It has a region of recon concentration.
[0170] The semiconductor 406 has a SIMS resolution of 1×10 16 atoms / cm 3 2×1 or more 0 20 atoms / cm 3 Less than or equal to 1×10 16 atoms / cm 3 Above 5×1 0 19 atoms / cm 3 Less than or equal to 1×10 16 atoms / cm 3 1 more ×10 19 atoms / cm 3 Less than 1×10, more preferably 16 atoms / cm 3 5×10 or more 18 atoms / cm 3 The hydrogen concentration in the semiconductor is as follows: In order to reduce the hydrogen concentration of 406, the hydrogen concentration of the semiconductor 406a and the semiconductor 406c is The semiconductor 406a and the semiconductor 406c are preferably reduced by 1× 1016 atoms / cm 3 More than 2×10 20 atoms / cm 3 Below, preferably 1x 10 16 atoms / cm 3 5×10 or more 19 atoms / cm 3 More preferably, 1×10 16 atoms / cm 3 More than 1×10 19 atoms / cm 3 The following are more preferred Or 1×10 16 atoms / cm 3 5×10 or more 18 atoms / cm 3 The following hydrogen The semiconductor 406 has a concentration of 1×10 15 at oms / cm 3 5×10 or more 19 atoms / cm 3 Less than or equal to 1×10 15 at oms / cm 3 5×10 or more 18 atoms / cm 3 Less than or equal to 1×10 15 atoms / cm 3 More than 1×10 18 atoms / cm 3 Below, more preferably 1×1 0 15 atoms / cm 3 5×10 or more 17 atoms / cm 3 The area with the following nitrogen concentration In order to reduce the nitrogen concentration in the semiconductor 406, the semiconductor 406a and the semiconductor It is preferable to reduce the nitrogen concentration in the conductor 406c. , 1×10 in SIMS 15 atoms / cm 3 5×10 or more19 atoms / c m 3 Less than or equal to 1×10 15 atoms / cm 3 5×10 or more 18 atoms / c m 3 Less than or equal to 1×10 15 atoms / cm 3 More than 1×10 18 atoms / cm 3 Less than 1×10, more preferably 15 atoms / cm 3 5×10 or more 17 at oms / cm 3 The nitrogen concentration ranges as follows:
[0171] The three-layer structure described above is an example. For example, a two-layer structure without semiconductor 406a or semiconductor 406c Alternatively, the semiconductor 406a may be disposed above or below the semiconductor 406c. Above and below, the semiconductors exemplified as semiconductor 406a, semiconductor 406, and semiconductor 406c are Alternatively, a four-layer structure may be used in which the semiconductor 406a is on the upper side of the semiconductor 406b and the semiconductor 406c is on the lower side of the semiconductor 406b. At least two of the following locations are located below the conductor 406a, above the semiconductor 406c, and below the semiconductor 406c: Any one of the semiconductors exemplified as the semiconductor 406a, the semiconductor 406, and the semiconductor 406c Alternatively, it may have an n-layer structure (n is an integer of 5 or more) having the above layers.
[0172] <Structure of oxide semiconductor> The structure of an oxide semiconductor will be described below.
[0173] Oxide semiconductors are classified into single-crystal oxide semiconductors and non-single-crystal oxide semiconductors. As a non-single-crystal oxide semiconductor, CAAC-OS (C Axis Aligned Crystalline Oxide Semiconductor, polycrystalline oxide semiconductor Examples of the oxide semiconductor include a conductor, a microcrystalline oxide semiconductor, and an amorphous oxide semiconductor.
[0174] From another point of view, the oxide semiconductor is classified into an amorphous oxide semiconductor and a crystalline oxide semiconductor other than the amorphous oxide semiconductor. Crystalline oxide semiconductors are classified into single crystal oxide semiconductors, CAAC-O S, polycrystalline oxide semiconductors, and microcrystalline oxide semiconductors.
[0175] <caac-os> First, let me explain about CAAC-OS. xis aligned nanocrystals) It is also possible.
[0176] CAAC-OS is an oxide semiconductor that has multiple crystal parts (also called pellets) aligned along the c-axis. It is a conductor.
[0177] Transmission Electron Microscope (TEM) A composite analysis image (high resolution) of the bright-field image and the diffraction pattern of CAAC-OS was obtained by using a scope. When observing the high-resolution TEM image, multiple pellets can be confirmed. In the high-resolution TEM image, the boundaries between the pellets, i.e., grain boundaries, are not clearly visible. Therefore, it is not possible to clearly confirm the presence of the CAAC-OS. Therefore, it can be said that the decrease in electron mobility caused by the above phenomenon is unlikely to occur.
[0178] The CAAC-OS observed by TEM will be described below. This shows a high-resolution TEM image of a cross section of CAAC-OS observed from a direction approximately parallel to the sample surface. For high-resolution TEM imaging, spherical aberration correction (SAC) is required. The spherical aberration corrector function was used. In particular, it is called a Cs-corrected high-resolution TEM image. This was carried out using an atomic resolution analytical electron microscope, such as the JEM-ARM200F manufactured by Nippon Denki Co., Ltd. This can be done.
[0179] FIG. 38(B) shows an enlarged Cs-corrected high-resolution TEM image of region (1) in FIG. 38(A). From FIG. 38(B), it can be seen that the metal atoms are arranged in layers in the pellet. The arrangement of each metal atom layer is the same as that of the surface on which the CAAC-OS film is formed (also called the surface on which the film is formed). The surface on which the CAAC-OS is formed or the top surface of the CAAC-OS reflects the unevenness of the surface on which the CAAC-OS is formed or the top surface of the CAAC-OS.
[0180] As shown in Figure 38(B), CAAC-OS has a characteristic atomic arrangement. The characteristic atomic arrangement is shown by auxiliary lines in Figure 38(B) and Figure 38(C). Therefore, the size of each pellet is about 1 nm to 3 nm, and the size of each pellet is about 1 nm to 3 nm. It can be seen that the size of the gap caused by the inclination of the The beads can also be referred to as nanocrystals (nc).
[0181] Here, based on the Cs-corrected high-resolution TEM image, the pellet of CAAC-OS on the substrate 5120 was The layout of the 5100 is shown diagrammatically as a stack of bricks or blocks. (See FIG. 38(D)). The inclination between the pellets observed in FIG. 38(C) The location where the crack occurs corresponds to an area 5161 shown in FIG.
[0182] FIG. 39(A) shows the Cs Corrected high-resolution TEM images are shown for regions (1), (2), and (3) in FIG. 39(A). The enlarged Cs-corrected high-resolution TEM images are shown in Fig. 39(B), Fig. 39(C) and Fig. 39(D). From Fig. 39(B), Fig. 39(C) and Fig. 39(D), the pellet is It can be seen that the metal atoms are arranged in triangular, tetragonal or hexagonal shapes. However, no regularity is observed in the arrangement of metal atoms among different pellets.
[0183] Next, the CA analyzed by X-ray diffraction (XRD) We will explain AC-OS. For example, CAAC-OS with InGaZnO4 crystals When the out-of-plane method is used to analyze the structure, the results are as shown in Figure 40(A). A peak may appear at a diffraction angle (2θ) of about 31°. Since the crystal orientation of CAAC-OS is attributed to the (009) plane of nO4, the crystal orientation of CAAC-OS is considered to be c-axis oriented. It can be seen that the c-axis is oriented in a direction substantially perpendicular to the surface on which the film is formed or the upper surface.
[0184] In addition, in the out-of-plane structural analysis of CAAC-OS, 2θ is 31° In addition to the peaks around 2θ of 36°, a peak may also appear around 2θ of 36°. The peaks near the c-axis indicate that some of the CAAC-OS contains crystals that do not have the c-axis orientation. The more preferable CAAC-OS is the structure solution by the out-of-plane method. In the analysis, a peak is observed at 2θ of approximately 31°, but no peak is observed at 2θ of approximately 36°.
[0185] On the other hand, in-plan X-ray irradiation is performed on CAAC-OS in a direction perpendicular to the c-axis. When the structure is analyzed by the δ method, a peak appears at 2θ of about 56°. This peak is due to In It is assigned to the (110) plane of the GaZnO4 crystal. In the case of CAAC-OS, 2θ is set to 56 The sample was rotated around the normal vector of the sample surface as the axis (φ axis) while performing the analysis. Even if a φ scan is performed, no clear peak appears as shown in FIG. In the case of a single crystal oxide semiconductor such as InGaZnO4, the 2θ is fixed at around 56° and the φ shift is In the case of scanning, as shown in FIG. 40(C), the peaks belonging to the crystal plane equivalent to the (110) plane Therefore, from the structural analysis using XRD, CAAC-OS has the following structure: It can be seen that the orientation of the a-axis and b-axis is irregular.
[0186] Next, we will explain the CAAC-OS analyzed by electron diffraction. For CAAC-OS with nO4 crystals, a probe with a diameter of 300 nm was placed parallel to the sample surface. When an electron beam is incident, a diffraction pattern (selected area transmission electron diffraction) like that shown in Figure 41(A) is obtained. This diffraction pattern may show the InGaZnO4 This includes spots due to the (009) plane of the crystal. Therefore, even with electron diffraction, The pellets contained in the CAAC-OS have a c-axis orientation, and the c-axis is approximately aligned on the surface to be formed or the upper surface. On the other hand, the same sample was probed perpendicular to the sample surface. The diffraction pattern when an electron beam with a diameter of 300 nm is incident is shown in FIG. (B) shows a ring-shaped diffraction pattern. Therefore, by electron diffraction, It is seen that the a-axis and b-axis of the pellets contained in the CAAC-OS have no orientation. In addition, the first ring in FIG. 41(B) is the (010) plane of the InGaZnO4 crystal. This is thought to be due to the (100) plane and other factors. The second ring in Figure 41(B) This is thought to be due to the (110) plane, etc.
[0187] In addition, the CAAC-OS is an oxide semiconductor with a low density of defect states. Examples of defects include impurity-induced defects and oxygen vacancies. C-OS can also be considered an oxide semiconductor with a low impurity concentration. It can also be said that the oxide semiconductor has few oxygen vacancies.
[0188] Impurities contained in an oxide semiconductor can act as carrier traps or carrier generation sources. In addition, oxygen vacancies in an oxide semiconductor may become carrier traps or may cause hydrogen By capturing atoms, they can become a carrier generation source.
[0189] The impurities are elements other than the main components of the oxide semiconductor, such as hydrogen, carbon, silicon, and transition metals. For example, oxygen is more abundant than metal elements such as silicon that constitute oxide semiconductors. Elements with strong bonding strength with the oxide semiconductor remove oxygen from the oxide semiconductor, thereby changing the atomic arrangement of the oxide semiconductor. In addition, heavy metals such as iron and nickel, argon, and nitrogen Carbon oxide and other elements have a large atomic radius (or molecular radius), so they can easily arrange the atoms of oxide semiconductors. This causes the crystallinity to decrease.
[0190] In addition, an oxide semiconductor with a low density of defect states (few oxygen vacancies) can reduce the carrier density. Such an oxide semiconductor can be obtained by using a high-purity intrinsic or substantially high-purity intrinsic oxide. CAAC-OS has a low impurity concentration and a low density of defect states. It is easy to obtain a high-purity intrinsic or substantially high-purity intrinsic oxide semiconductor. A transistor using C-OS has electrical characteristics in which the threshold voltage is negative (normal In addition, the acid is highly pure or substantially pure. The oxide semiconductor has fewer carrier traps. The charge takes a long time to be discharged and behaves like a fixed charge. Therefore, transistors using oxide semiconductors with high impurity concentrations and high defect state densities are On the other hand, transistors using CAAC-OS may have unstable electrical characteristics. The resulting transistor has small fluctuations in electrical characteristics and is highly reliable.
[0191] In addition, because the density of defect states in CAAC-OS is low, the capacitive coupling generated by light irradiation can be suppressed. Therefore, the transistor using CAAC-OS is less likely to be captured by the defect level. The electrical characteristics of a transistor vary little when exposed to visible or ultraviolet light.
[0192] <Microcrystalline oxide semiconductor> Next, a microcrystalline oxide semiconductor will be described.
[0193] Microcrystalline oxide semiconductors are regions where crystals can be confirmed in high-resolution TEM images. A region in which no clear crystal part can be confirmed is also included. The crystal part contained in the crystal is 1 nm to 100 nm or 1 nm to 10 nm in size. In particular, microcrystals with a size of 1 nm to 10 nm or 1 nm to 3 nm are often found. The oxide semiconductor having nanocrystals is called nc-OS (nanocrystalline- The nc-OS is called the "High Resolution Oxide Semiconductor." In some cases, the grain boundaries cannot be clearly seen in the TEM images. Therefore, in the following, we will refer to the pellets in nc-OS as the pellets of the same origin. The crystalline part of S is sometimes called a pellet.
[0194] The nc-OS is a nano-sized area (e.g., an area of 1 nm to 10 nm, especially 1 nm to 3 nm). The nc-OS has periodic atomic arrangement in the sub-nm region. There is no regularity in the crystal orientation between the dots. Therefore, no orientation is observed throughout the film. Therefore, depending on the analysis method, nc-OS may be indistinguishable from amorphous oxide semiconductors. For example, there is an XRD apparatus that uses X-rays with a diameter larger than that of the pellet for nc-OS. When structural analysis is performed using the out-of-plane method, No peaks were detected. Also, for nc-OS, the probe diameter (e.g. When electron diffraction (also called selected area electron diffraction) is performed using an electron beam with a diameter of 50 nm or more, On the other hand, for nc-OS, a halo-like diffraction pattern is observed. Nanobeam electron diffraction using an electron beam with a probe diameter close to the pellet size or smaller than the pellet size. When the electron diffraction pattern is applied to the nc-OS, a spot is observed. In some cases, a bright area that appears circular (ring-shaped) may be observed. Multiple spots may be observed within a patchy region.
[0195] In this way, the crystal orientation between the pellets (nanocrystals) is not regular, so nc- OS with RANC (Random Aligned nanocrystals) oxide semiconductors, or NANCs (Non-Aligned Nanocrystals) ) can also be referred to as an oxide semiconductor.
[0196] The nc-OS is an oxide semiconductor with higher order than an amorphous oxide semiconductor. The nc-OS has a lower density of defect states than the amorphous oxide semiconductor. There is no regularity in the crystal orientation between different pellets. Therefore, nc-OS is The defect level density is higher than that of AC-OS.
[0197] <Amorphous oxide semiconductor> Next, the amorphous oxide semiconductor will be described.
[0198] Amorphous oxide semiconductors are oxides in which the atomic arrangement in the film is irregular and there are no crystal parts. An example is an oxide semiconductor that has an amorphous state, such as quartz.
[0199] In the case of an amorphous oxide semiconductor, no crystalline parts can be confirmed in a high-resolution TEM image.
[0200] When the structure of amorphous oxide semiconductors is analyzed using an XRD device, out-of-plane In the analysis by the ane method, no peaks indicating crystal planes were detected. When electron diffraction is performed on the amorphous oxide semiconductor, a halo pattern is observed. However, when nanobeam electron diffraction is performed, no spots are observed, and only a halo pattern is observed. It is measured.
[0201] There are various views on amorphous structures. For example, A structure that does not have a completely amorphous structure is called a completely amorphous structure. In addition, the distance between the nearest neighbors or the second nearest neighbors is called the A structure that has order but no long-range order is sometimes called an amorphous structure. According to the strictest definition, an oxide semiconductor that has even a slight degree of order in its atomic arrangement is called an amorphous semiconductor. In addition, oxides with at least long-range order cannot be called solid oxide semiconductors. The semiconductor cannot be called an amorphous oxide semiconductor. For example, the CAAC-OS and nc-OS are It cannot be called a compound semiconductor.
[0202] <Amorphous-like oxide semiconductor> Note that an oxide semiconductor may have a structure between an nc-OS and an amorphous oxide semiconductor. An oxide semiconductor having such a structure is particularly called an amorphous-like oxide semiconductor (a-li ke OS:amorphous-like Oxide Semiconductor ) is called
[0203] In a-like OS, voids are observed in high-resolution TEM images. In addition, there are cases where crystals can be clearly seen in high-resolution TEM images. and regions where no crystalline portion can be identified.
[0204] Because of the porosity, the a-like OS is an unstable structure. To demonstrate that the OS has a less stable structure compared with CAAC-OS and nc-OS. , shows the change in structure due to electron irradiation.
[0205] The samples to be irradiated with electrons were a-like OS (referred to as sample A), nc-OS ( Sample B) and CAAC-OS (sample C) are prepared. The sample in is also an In-Ga-Zn oxide.
[0206] First, high-resolution cross-sectional TEM images of each sample are obtained. It can be seen that each of the samples has a crystalline portion.
[0207] The determination of which part is regarded as one crystal part can be made as follows. For example, The unit cell of the InGaZnO4 crystal has three In-O layers and one Ga-Zn-O layer. It is known that the structure has a total of nine layers, including six layers, stacked in layers in the c-axis direction. The spacing between adjacent layers is approximately the same as the lattice spacing (also called the d value) of the (009) plane. The value is calculated to be 0.29 nm from crystal structure analysis. The area where the spacing is 0.28 nm or more and 0.30 nm or less is considered to be the crystal part of InGaZnO4. The lattice fringes correspond to the ab plane of the InGaZnO4 crystal.
[0208] Figure 42 shows an example of the average size of the crystal parts (22 to 45 places) of each sample. However, the length of the lattice fringes mentioned above is the size of the crystal part. It can be seen that the crystal part of eOS becomes larger according to the cumulative dose of electron irradiation. As shown by (1) in Figure 42, the initial TEM observation showed a size of about 1.2 nm. The crystal part (also called the initial nucleus) was 4.2×10 in size, but the cumulative irradiation dose was 4.2×10 8 e - / nm 2 On the other hand, in the nc-OS, the size of the nanoparticles grows to about 2.6 nm. For CAAC-OS, the cumulative electron dose from the start of electron irradiation was 4.2 × 10 8 e - / nm 2 It can be seen that there is no change in the size of the crystals within the range of As shown in (2) and (3) in 42, the nc-OS and The sizes of the crystal parts of the CAAC-OS and CAAC-OS are about 1.4 nm and 2.1 nm, respectively. I realize something.
[0209] Thus, in a-like OS, the growth of crystals can be observed by electron irradiation. On the other hand, the growth of the crystals in the nc-OS and CAAC-OS was hardly observed by electron irradiation. In other words, a-like OS is not seen in nc-OS and CAAC-OS. It can be seen that compared with S, it has a less stable structure.
[0210] In addition, because of the porosity, a-like OS is more resistant to vascular endothelial cell proliferation than nc-OS and CAAC-OS. Specifically, the density of the a-like OS is lower than that of a single crystal of the same composition. The density of nc-OS is 78.6% or more and less than 92.3% of that of CAAC. The density of the -OS is 92.3% or more and less than 100% of the density of a single crystal of the same composition. It is difficult to form an oxide semiconductor film having a density of less than 78% of that of the oxide semiconductor film.
[0211] For example, in an oxide semiconductor with an atomic ratio of In:Ga:Zn=1:1:1, The density of single crystal InGaZnO4 with a hexagonal crystal structure is 6.357 g / cm 3 It becomes. For example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, , the density of a-like OS is 5.0g / cm 3 More than 5.9g / cm 3 It is less than. For example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, The density of nc-OS and that of CAAC-OS are 5.9 g / cm 3 More than 6.3g / cm 3 It will be less than.
[0212] In some cases, single crystals with the same composition do not exist. In such cases, it is necessary to prepare single crystals with different compositions in the desired ratio. By combining single crystals, we estimate the density equivalent to a single crystal of the desired composition. The density corresponding to a single crystal of a desired composition can be determined by combining single crystals of different compositions. The weighted average of the proportion of It is preferable to estimate by combining different types of single crystals.
[0213] As described above, oxide semiconductors have various structures, each of which has various characteristics. The oxide semiconductor may be, for example, an amorphous oxide semiconductor, an a-like OS, or a microcrystalline oxide semiconductor. The layer may be a laminated film having two or more of a semiconductor and a CAAC-OS.
[0214] <Film formation model> An example of a film formation model for CAAC-OS and nc-OS will be described below.
[0215] FIG. 43A shows how a CAAC-OS film is formed by a sputtering method. FIG.
[0216] The target 5130 is attached to a backing plate. A plurality of magnets are disposed at positions facing the target 5130. The magnetic field is generated by the magnet. The magnetic field of the magnet is used to increase the deposition speed. The sputtering method is called magnetron sputtering.
[0217] The substrate 5120 is disposed so as to face the target 5130, and the distance therebetween is d ( The target-substrate distance (TS distance) is preferably 0.01 m or more and 1 m or less. The thickness of the deposition chamber is set to 0.02m or more and 0.5m or less. Most of the deposition gas (e.g., oxygen) is The chamber is filled with a gas mixture containing 5% or more by volume of nitrogen, argon, or oxygen. The pressure is controlled to be 0.1 Pa or more and 100 Pa or less, preferably 0.1 Pa or more and 10 Pa or less. By applying a certain voltage to the target 5130, discharge begins and plasma is generated. It is noted that a high-density plasma region is formed near the target 5130 by the magnetic field. In the high density plasma region, the deposition gas is ionized, and ions 5101 are generated. The ions 5101 are, for example, positive oxygen ions (O + ) and argon cations (A r + ) etc.
[0218] Here, the target 5130 has a polycrystalline structure having a plurality of crystal grains, and any of the grains The crystal grains include cleavage planes. FIG. 44(A) shows an example of a cleavage plane included in a target 5130. The crystal structure of InGaZnO4 is shown in Fig. 44(A). This is the structure of an InGaZnO4 crystal. In the Ga-Zn-O layer, the oxygen atoms in each layer are arranged close to each other. And because the oxygen atom has a negative charge, the two adjacent G Repulsion occurs between the a-Zn-O layers. As a result, the InGaZnO4 crystals are close to each other. The cleavage plane is between the two Ga-Zn-O layers.
[0219] Ions 5101 generated in the high-density plasma region are applied to the target 5130 side by the electric field. The cleavage plane is accelerated and eventually collides with the target 5130. At this time, flat or pellet-like particles are generated from the cleavage plane. Pellet 5100a and pellet 5100b, which are pellet-shaped sputtered particles, are peeled off and struck. The pellets 5100a and 5100b are the same as the pellets 5101. The impact of a collision can cause distortion of the structure.
[0220] The pellet 5100a is a flat or pellet-shaped pellet having a triangular, for example equilateral, plane. The pellet 5100b has a hexagonal, for example, regular hexagonal, planar surface. The sputtered particles are in the form of a plate or pellet. Pellet 5100b and other flat or pellet-shaped sputter particles are collectively referred to as pellet 5 The planar shape of the pellet 5100 is not limited to a triangle or a hexagon. For example, a triangle (e.g., an equilateral triangle) may have a shape that is made up of multiple triangles. In some cases, the shape may be two squares (for example, a diamond).
[0221] The thickness of the pellet 5100 is determined according to the type of deposition gas. The reason for this will be described later. It is preferable that the thickness of the pellet 5100 is uniform. Thin pellets are preferred over thick cubes. The thickness of the 5100 is 0.4 nm or more and 1 nm or less, preferably 0.6 nm or more and 0.8 nm or less. For example, the pellet 5100 has a width of 1 nm or more and 3 nm or less, preferably The pellet 5100 is (1) in FIG. For example, the target 51 having In-Ga-Zn oxide corresponds to the initial nucleus described in . When ions 5101 are bombarded onto the surface of the semiconductor substrate 30, the Ga-Zn-O layer, A pellet 5100 having three layers, an In-O layer and a Ga-Zn-O layer, is exfoliated. (C) shows the structure of the exfoliated pellet 5100 observed from a direction parallel to the c-axis. The plate 5100 is a nanotube having two Ga-Zn-O layers (panels) and an In-O layer (tool). It can also be called a no-size sandwich structure.
[0222] The pellet 5100 may become negatively or positively charged on its sides as it passes through the plasma. The pellet 5100 may, for example, be negatively charged due to the oxygen atoms located on its sides. The sides of the particles have the same polarity of charge, causing repulsion between the charges, forming a flat or pellet-like shape. It is possible to maintain the shape of the In-Ga-Zn In the case of oxides, the oxygen atoms bonded to the indium atoms may be negatively charged. Or, an oxygen atom bonded to an indium atom, a gallium atom, or a zinc atom is negatively charged. In addition, when the pellet 5100 passes through the plasma, it may be possible that the pellet 5100 may be oxidized by the impurities in the plasma. When it grows by combining with other atoms such as tungsten, gallium, zinc, and oxygen, The difference in size between (2) and (1) in Figure 42 above corresponds to the growth in the plasma. Here, when the substrate 5120 is at room temperature, the pellets on the substrate 5120 Since the growth of 5100 is difficult to occur, it becomes nc-OS (see Figure 43(B)). Since the film can be formed in a short time, it is possible to form a film of nc-OS even on a large substrate (5120). In order to grow the pellet 5100 in plasma, the sputtering method is used. It is effective to increase the film formation power in the pellet 51. The structure of 00 can be stabilized.
[0223] As shown in FIG. 43(A) and FIG. 43(B), for example, a pellet 5100 is It flies like a kite through the air and flutters up to the top of the substrate 5120. Pellet 51 Since the 00 is electrically charged, it approaches an area where other pellets 5100 are already deposited. Here, on the upper surface of the substrate 5120, a repulsive force is generated in a direction parallel to the upper surface of the substrate 5120. In addition, the substrate 5120 and the target 51 Since a potential difference is applied between the substrate 5120 and the target 5130, Therefore, the pellet 5100 is disposed on the upper surface of the substrate 5120 in a magnetic The force (Lorentz force) is exerted by the action of the electric field and the electric current. This is explained by Fleming's This can be understood using the left-hand rule.
[0224] The pellet 5100 has a large mass compared to a single atom. In order to move the object, it is important to apply some kind of force from the outside. It is possible that the force is generated by the action of a magnetic field and a current. In order to provide sufficient force to move the top surface of the substrate 5120, The magnetic field parallel to the upper surface of the plate 5120 is 10 G or more, preferably 20 G or more, and more preferably It is preferable to provide an area where the resistance is 30 G or more, and more preferably 50 G or more. On the upper surface of the substrate 5120, a magnetic field parallel to the upper surface of the substrate 5120 is applied to the upper surface of the substrate 5120. At least 1.5 times, preferably at least 2 times, more preferably at least 3 times the magnetic field perpendicular to the surface More preferably, a region in which the difference is 5 times or more is provided.
[0225] At this time, the magnet and the substrate 5120 move or rotate relatively to each other. Thus, the orientation of the horizontal magnetic field on the top surface of the substrate 5120 continues to change. On the upper surface of 5120, the pellet 5100 is subjected to forces from various directions and is moved in various directions. Can be moved.
[0226] Also, when the substrate 5120 is heated as shown in FIG. The resistance due to friction between the substrate 5120 and the substrate 5120 is small. The pellet 5100 glides over the upper surface of the substrate 5120. The movement occurs with the flat surface facing the substrate 5120. When the pellet 5100 reaches the side of the pellet, the sides of the pellet 5100 are joined together. The oxygen atom on the side of 0 is removed. The removed oxygen atom causes the acid in CAAC-OS to be Since the electron vacancies may be filled, the CAAC-OS has a low defect level density. The temperature of the upper surface of 5120 is, for example, 100°C or more and less than 500°C, 150°C or more and less than 450°C. 170° C. or more and less than 400° C. Therefore, Even in this case, it is possible to form a CAAC-OS film.
[0227] In addition, the pellet 5100 is heated on the substrate 5120, whereby the atoms are rearranged, The structural distortion caused by the collision of the ions 5101 is relieved. The pellet 51 with the distortion relieved is shown in FIG. 00 is almost a single crystal. Pellet 5100 is almost a single crystal, Even if the pellets 5100 are heated after being bonded to each other, the pellets 5100 themselves do not expand or contract. Therefore, the gaps between the pellets 5100 widen, causing the grains to It does not form defects such as boundaries or crevasse formation.
[0228] In addition, the CAAC-OS is not made of a single crystal oxide semiconductor. The aggregates of Pellet 5100 (nano crystals) are arranged like piles of bricks or blocks. In addition, there are no grain boundaries between the pellets 5100. The CAAC-OS was deformed, such as shrinking, due to heating during film formation, heating after film formation, or bending. Even in cases where the material is not fully deformed, it is possible to relieve local stress or release strain. This structure is suitable for use in flexible semiconductor devices. The resulting arrangement resembles randomly stacked nanocrystals.
[0229] When the target 5130 is sputtered by ions 5101, not only the pellet 5100 but also However, zinc oxide may peel off. Zinc oxide is lighter than pellet 5100, so Therefore, it will reach the upper surface of the substrate 5120 first. A zinc oxide layer 5102 having a thickness of 0.5 nm to 2 nm is formed. A schematic cross-sectional view is shown in Figure 45.
[0230] As shown in FIG. 45(A), a pellet 5105a and a pellet Here, the pellets 5105a and 5105b are piled up. The pellets 5105c are arranged so that their sides are in contact with each other. After being deposited on pellet 5105b, it slides on pellet 5105b. In another aspect of 5a, a plurality of particles 5103 detached from the target along with zinc oxide. However, due to heating from the substrate 5120, it is crystallized to form a region 5105a1. The particles 5103 may include oxygen, zinc, indium, and gallium, among others.
[0231] As shown in FIG. 45(B), the region 5105a1 is integrated with the pellet 5105a. The pellet 5105c is formed by cutting the pellet 5105a2. It is arranged so as to be in contact with another side surface of 105b.
[0232] Next, as shown in FIG. 45(C), a pellet 5105d is further formed on the pellet 5105a2. and pellet 5105b, and then pellet 5105a2 and pellet 51 It slides on the pellet 5105b. It also slides towards the other side of the pellet 5105c. The pellet 5105 e slides on the zinc oxide layer 5102 .
[0233] As shown in FIG. 45(D), the pellet 5105d has a side surface similar to that of the pellet 510. The pellet 5105e is arranged so that its side surface is in contact with the pellet 5105a. Also, the other side of the pellet 5105d is arranged so as to contact the other side of the pellet 5105c. In the process, a plurality of particles 5103 peeled off from the target 5130 together with zinc oxide are deposited on the substrate. Heat from 5120 causes crystallization, forming region 5105d1.
[0234] As described above, the piled up pellets are arranged so that they come into contact with each other, and the pellets are formed on the side surfaces. As a result of this growth, a CAAC-OS is formed on the substrate 5120. The pellets of C-OS are larger than those of nc-OS. The difference in size between (1) and (2) corresponds to the growth that occurred after deposition.
[0235] In addition, the gaps between the pellets become extremely small, so that one large pellet is formed. One large pellet may have a single crystal structure. For example, The thickness is 10 nm or more and 200 nm or less, or 15 nm or more and 100 nm or less, as viewed from the top surface; or In some cases, the thickness may be between 20 nm and 50 nm. In some cases, the channel formation region of a nitride semiconductor fits into a single large pellet. In other words, the region having a single crystal structure can be used as a channel forming region. As the size of the gate increases, the region having a single crystal structure becomes the channel formation region of the transistor, In some cases, they can be used as source and drain regions.
[0236] In this way, the channel formation region of the transistor and the like are formed in a region having a single crystal structure. By doing so, it may be possible to improve the frequency characteristics of the transistor.
[0237] Based on the above model, it is considered that the pellet 5100 accumulates on the substrate 5120. It is possible to form a CAAC-OS film even if the surface on which the film is to be formed does not have a crystalline structure. This indicates that the growth mechanism is different from epitaxial growth. C-OS does not require laser crystallization and can be formed into a uniform film even on large glass substrates. For example, if the structure of the upper surface (formation surface) of the substrate 5120 is an amorphous structure (e.g., non-crystalline structure), It is possible to form a CAAC-OS film even on a substrate made of amorphous silicon oxide.
[0238] In addition, the CAAC-OS can be used even if the upper surface of the substrate 5120 on which the formation is to be performed is uneven. For example, the pellets 5100 are arranged along the shape of the upper surface of the substrate 5120. If the surface is atomically flat, the pellet 5100 will face down on a flat surface that is parallel to the ab plane. If the pellet 5100 has a uniform thickness, it is flat and has a uniform thickness. A layer with high crystallinity is formed. Then, the layer is stacked n levels (n is a natural number). By this, CAAC-OS can be obtained.
[0239] On the other hand, even if the upper surface of the substrate 5120 has unevenness, the CAAC-OS can be easily formed by the pellet 510. The structure is made up of n layers (n is a natural number) of layers with 0s arranged along the unevenness. Since the surface of the CAAC-OS is uneven, gaps may easily occur between the pellets. However, even in this case, intermolecular forces act between the pellets 5100, and unevenness may occur. The pellets are arranged so that the gaps between them are as small as possible. It is possible to obtain a CAAC-OS having high crystallinity.
[0240] Since the CAAC-OS film is formed by such a model, the sputtered particles have a thin film thickness. It is preferable that the sputtered particles are in the form of pellets. However, the surface facing the substrate 5120 may not be uniform, and the thickness and crystal orientation may not be uniform. be.
[0241] The film formation model shown above shows that a highly crystalline film can be formed even on a substrate surface with an amorphous structure. It is possible to obtain a CAAC-OS having the formula:
[0242] <Transistor 2> Next, a method for manufacturing a transistor having a partially different shape will be described. 5(A), 16(A), 17(A) and 18(A) show a method for fabricating a transistor. Each of the top views illustrates the dashed line F1-F2 and the dashed line F3-F4. The corresponding cross-sectional views are shown in Figs. 14(B), 15(B), 16(B), and 17. (B) and FIG. 18(B).
[0243] First, prepare the substrate 500. For the substrate 500, refer to the description of the substrate 400.
[0244] Next, an insulator is formed. The insulator is formed by a method such as sputtering, CVD, MBE or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0245] Next, a resist or the like is formed on the insulator, and the resist is used for processing to form the insulator 503. Complete.
[0246] When processing the insulator to form the insulator 503, the processing method shown in any one of FIGS. may also be used.
[0247] Next, a conductive film is formed. The conductive film may be formed by a sputtering method, a CVD method, an MBE method, or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0248] Next, an edge is formed from the upper surface of the conductor toward the lower surface thereof so as to be parallel to the lower surface of the substrate 500. By performing the chipping, the conductor 513 can be formed (embedded) in the groove of the insulator 503. (See FIG. 14(A) and FIG. 14(B).) In this manner, the conductor 513 is formed. By forming the conductive body 513 and the insulator 503, the height of the upper surface of the conductive body 513 and the height of the upper surface of the insulator 503 are approximately the same. Therefore, it is possible to suppress shape defects in the subsequent steps.
[0249] The insulator 503 is the same as the insulator 402. The conductor 513 is the same as the conductor 41. Please refer to the description for 3.
[0250] Next, the insulator 502 is formed. The insulator 502 can be formed by a sputtering method, a CVD method, or the like. This can be done by using the MBE method, the PLD method, the ALD method, or the like. Please refer to the description of edge 402.
[0251] Next, a semiconductor film 536 is formed. The semiconductor film 536 can be formed by a sputtering method, a CVD method, or the like. The semiconductor 536 can be formed by using an MBE method, a PLD method, an ALD method, or the like. See the description of conductor 406.
[0252] Next, a heat treatment is preferably carried out.
[0253] Next, a conductor 546 is formed. The conductor 546 can be formed by a sputtering method, a CVD method, or the like. The deposition can be performed by using an MBE method, a PLD method, an ALD method, or the like. See the description of the element 416.
[0254] Next, an insulator 540 is formed (see FIG. 15(A) and FIG. 15(B)). The deposition of 0 is performed using the sputtering method, CVD method, MBE method, PLD method, ALD method, etc. For the insulator 540, refer to the description of the insulator 510.
[0255] Next, a resist or the like is formed on the insulator 540, and the resist is used for processing to form the insulator 51. 0, a conductor 516 and a semiconductor 506 are formed (see FIG. 16(A) and FIG. 16(B)). At this time, the conductor 516 and / or the semiconductor 506 are removed from the resist. Processing may be performed using an insulator 510. In this case, the insulator 510 that does not overlap with the semiconductor 506 may be used. 2 may be etched. By doing so, a protrusion is formed on the insulator 502. do.
[0256] In this case, the processing method shown in any one of Figs. 1 to 7 may be used. For example, 7, layer 116 is replaced by conductor 516 and layer 110 is replaced by insulator 510.
[0257] Next, a resist or the like is formed on the insulator 510, and the resist is used for processing to form the insulator 51 510a and insulator 510b, and conductor 516a and conductor 516b are formed ( See Figures 17(A) and 17(B). Here, the same processing method as shown in Figure 4 is used. The figure shows a case where an insulator 510 and a conductor 516 are processed by the method. 51, 52, 53, and the like, the conductor 516a and the conductor 51 6b, as well as insulators 510a and 510b may be processed.
[0258] Next, an insulator is formed. The insulator is formed by a method such as sputtering, CVD, MBE or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0259] Next, a conductive film is formed. The conductive film may be formed by a sputtering method, a CVD method, an MBE method, or the like. This can be carried out by using a PLD method, an ALD method, or the like.
[0260] Next, a resist or the like is formed on the conductor, and the conductor 504 is formed by processing using the resist. In addition, the resist or conductor 504 is used to process an insulator, and an insulator 512 is formed. (See FIG. 18(A) and FIG. 18(B)). Note that, here, the insulator 512 and the conductor The conductive member 504 is processed so that it has the same shape when viewed from above, but this shape is not limited to this. For example, the insulator 512 and the conductor 504 may be formed using different resists. For example, after forming the insulator 512, a conductor that will become the conductor 504 may be formed. Alternatively, a resist may be formed on the insulator that will become the insulator 512 after the conductor 504 is formed. A hole or the like may be formed.
[0261] In this case, the processing method shown in any one of Figs. 1 to 7 may be used. For example, 7, layer 116 is replaced with an insulator to become insulator 512, and layer 110 is replaced with a conductor to become conductor 504. Just replace it with an electric device.
[0262] The insulator 512 is the same as the insulator 412. The conductor 504 is the same as the conductor 40. Please refer to the description for 4.
[0263] Next, an insulator film may be formed. The insulator film may be formed by a sputtering method, a CVD method, or an MBE method. The method can be carried out by using a PLD method, an ALD method, or the like.
[0264] Examples of the insulator include boron, carbon, nitrogen, oxygen, fluorine, magnesium, and aluminum. Umium, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zinc Insulators containing lanthanum, neodymium, hafnium or tantalum are used in a single layer or in The insulator is preferably aluminum oxide, silicon nitride oxide, Silicon nitride, gallium oxide, yttrium oxide, zirconium oxide, lanthanum oxide, acid Insulators containing neodymium oxide, hafnium oxide or tantalum oxide are used in single or multilayered configurations. Just use it.
[0265] The insulator preferably functions as a barrier layer. and / or has a function of blocking hydrogen. Alternatively, the insulator may be, for example, insulator 502 Alternatively, it is preferable that the insulating material 512 has a higher ability to block oxygen and / or hydrogen than the insulating material 512. I wish.
[0266] Through the above steps, a transistor according to one embodiment of the present invention can be manufactured.
[0267] The transistor shown in FIG. 18B has an insulator 5 between the conductor 516a and the conductor 504. 10a, and has an insulator 510b between the conductor 516b and the conductor 504. That is, The parasitic capacitance caused by the conductor 516a and the conductor 516b is small. A semiconductor device using the transistor shown in FIG. 8(B) has high frequency characteristics. The length of the conductor 516a protruding from the insulator 510a is set to 70% or more of the thickness of the insulator 512. 130% or less, preferably 80% or more and 120% or less, more preferably 90% or more and 110% or less. % or less, the parasitic capacitance can be reduced and the on-resistance can be reduced. The same is true for field 516b.
[0268] As shown in FIG. 18B, the transistor has an s-channel structure. The electric field from the conductor 504 penetrates the conductor 516a and the conductor 516b on the side of the semiconductor 506. The structure is not easily inhibited by 6b etc.
[0269] Note that the conductor 513 is not necessarily formed (see FIG. 19A). The insulator 504 may be formed in a shape protruding from the conductor 504 (see FIG. 19(B)). There is no need to process the insulator 512 (see FIG. 19(C)).
[0270] <Circuit> An example of a circuit of a semiconductor device using a transistor according to one embodiment of the present invention will be described below. We will explain about this.
[0271] <CMOSインバータ> The circuit diagram shown in FIG. 20A includes a p-channel transistor 2200 and an n-channel transistor 2201. Transistor 2100 is connected in series and each gate is connected. 4 shows the configuration of an S inverter.
[0272] <Semiconductor device structure 1> 21 is a cross-sectional view of the semiconductor device corresponding to FIG. 20(A). The transistor 2200 includes a transistor 2100. The transistor 2100 is disposed above the transistor 2200. 18 is used as an example, a semiconductor device according to one embodiment of the present invention may be used as the semiconductor device. The body device is not limited to this. For example, FIG. 11, FIG. 12, FIG. 19, FIG. 51, The transistor shown in FIG. 52 or FIG. 53 may be used as the transistor 2100. Therefore, the transistor 2100 may be any of the transistors described above. Please refer to the above information.
[0273] A transistor 2200 shown in FIG. 21 is a transistor using a semiconductor substrate 450 . The transistor 2200 includes a region 472 a in the semiconductor substrate 450 and a It has a region 472b, an insulator 462, and a conductor 454.
[0274] In transistor 2200, regions 472a and 472b are source and The insulator 462 functions as a gate insulator. The conductor 454 also functions as a gate electrode. The resistance of the channel forming region can be controlled by applying a potential to the body 454. That is, the electric potential applied to the conductor 454 causes a conduction line between the region 472a and the region 472b. The non-conduction can be controlled.
[0275] The semiconductor substrate 450 may be, for example, a single semiconductor substrate such as silicon or germanium. or silicon carbide, silicon germanium, gallium arsenide, indium phosphide, zinc oxide For example, a compound semiconductor substrate such as a gallium oxide substrate may be used. A single crystal silicon substrate is used as 50 .
[0276] The semiconductor substrate 450 is a semiconductor substrate having impurities that impart n-type conductivity. The semiconductor substrate 450 is a semiconductor substrate having an impurity that imparts p-type conductivity. In that case, the region that will become the transistor 2200 is given n-type conductivity. Alternatively, even if the semiconductor substrate 450 is an i-type, That's fine.
[0277] The upper surface of the semiconductor substrate 450 preferably has a (110) surface. The on-characteristics of the transistor 2200 can be improved.
[0278] Regions 472a and 472b are regions having impurities that impart p-type conductivity. In this manner, transistor 2200 constitutes a p-channel transistor.
[0279] Note that transistor 2200 is isolated from adjacent transistors by regions 460, etc. The region 460 is an insulating region.
[0280] The semiconductor device shown in FIG. 21 includes an insulator 464, an insulator 466, an insulator 468, and a conductor. 480a, conductor 480b, conductor 480c, conductor 478a, and conductor 478b. , conductor 478c, conductor 476a, conductor 476b, conductor 474a, and conductor Conductor 474b, conductor 474c, conductor 496a, conductor 496b, and conductor 496 c, conductor 496d, conductor 498a, conductor 498b, conductor 498c, and insulator It has an edge 490 , an insulator 492 , and an insulator 494 .
[0281] The insulator 464 is disposed on the transistor 2200. The insulator 466 is disposed on the insulator 4 64. Insulator 468 is disposed on insulator 466. Insulator 4 90 is disposed on the insulator 468. Also, the transistor 2100 is disposed on the insulator 490. Also, an insulator 492 is disposed on the transistor 2100. Also, an insulator 4 94 is disposed on the insulator 492 .
[0282] The insulator 464 has an opening reaching the region 472a, an opening reaching the region 472b, and a conductive The openings each include a conductor 480a, a conductor 480b, and an opening that reaches the conductor 454. The conductive body 480b or the conductive body 480c is embedded therein.
[0283] In addition, the insulator 466 has an opening that reaches the conductor 480a and an opening that reaches the conductor 480b. The openings each have a conductor 480c. 478a, conductor 478b or conductor 478c is embedded therein.
[0284] In addition, the insulator 468 has an opening that reaches the conductor 478b and an opening that reaches the conductor 478c. The openings are filled with a conductor 476a or a conductor 476b. It's embedded.
[0285] The insulator 490 has an opening overlapping the channel formation region of the transistor 2100 and a conductive The opening reaches the conductor 476a and the opening reaches the conductor 476b. The mouths are embedded with conductors 474a, 474b, and 474c, respectively. is.
[0286] The conductor 474a may function as a gate electrode of the transistor 2100. Alternatively, for example, a constant potential may be applied to the conductor 474a to turn on the transistor 210. Alternatively, the electrical properties of the conductor 474 may be controlled, such as the threshold voltage of 0. a and the conductor 404 serving as the gate electrode of the transistor 2100 are electrically This can increase the on-state current of the transistor 2100. In addition, since the punch-through phenomenon can be suppressed, the transistor 210 The electrical characteristics in the saturation region of 0 can be stabilized.
[0287] Also, the insulator 492 is connected to one of the source and drain electrodes of the transistor 2100. An opening through one conductor 416b to conductor 474b and a transistor 2100 An opening reaching the conductor 416a, which is the other of the source electrode or drain electrode of the transistor, An opening reaching the conductor 404, which is the gate electrode of the transistor 2100, and an opening reaching the conductor 474c The openings are provided with a conductor 496a and a conductor 496b. , a conductor 496c or a conductor 496d is embedded in each opening. may further pass through any of the components such as transistor 2100.
[0288] The insulator 494 has an opening that reaches the conductor 496a, and a conductor 496b and a The opening reaches the conductor 496d, and the opening reaches the conductor 496c. The conductive body 498a, the conductive body 498b, and the conductive body 498c are embedded in the conductive body 498a, the conductive body 498b, and the conductive body 498c, respectively. do.
[0289] Insulator 464, insulator 466, insulator 468, insulator 490, insulator 492 and insulator Examples of 494 include boron, carbon, nitrogen, oxygen, fluorine, magnesium, and aluminum. Umium, silicon, phosphorus, chlorine, argon, gallium, germanium, yttrium, zinc Insulators containing lanthanum, neodymium, hafnium or tantalum are used in a single layer or in For example, the insulator 401 may be aluminum oxide, magnesium oxide, or the like. Nesium, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, gas oxide Sodium oxide, Germanium oxide, Yttrium oxide, Zirconium oxide, Lanthanum oxide, Neodymium oxide, hafnium oxide or tantalum oxide may be used.
[0290] Insulator 464, insulator 466, insulator 468, insulator 490, insulator 492 or insulator At least one of 494 has an insulator that has the function of blocking impurities such as hydrogen and oxygen. It is preferable to add impurities such as hydrogen and oxygen to the vicinity of the transistor 2100. By disposing an insulator having a locking function, the electrical characteristics of the transistor 2100 are It can stabilize the sex.
[0291] Examples of insulators that have the function of blocking impurities such as hydrogen and oxygen include boron. Element, carbon, nitrogen, oxygen, fluorine, magnesium, aluminum, silicon, phosphorus, chlorine, Argon, Gallium, Germanium, Yttrium, Zirconium, Lanthanum, Neodymium Insulators containing hafnium or tantalum may be used in a single layer or in a multilayer.
[0292] Conductor 480a, conductor 480b, conductor 480c, conductor 478a, conductor 478b, Conductor 478c, conductor 476a, conductor 476b, conductor 474a, conductor 474b, Conductor 474c, conductor 496a, conductor 496b, conductor 496c, conductor 496d, The conductor 498a, the conductor 498b, and the conductor 498c may be, for example, boron, nitrogen, or the like. , oxygen, fluorine, silicon, phosphorus, aluminum, titanium, chromium, manganese, cobalt , nickel, copper, zinc, gallium, yttrium, zirconium, molybdenum, ruthenium A conductor containing one or more of aluminum, silver, indium, tin, tantalum and tungsten is formed in a single layer. For example, the material may be an alloy or a compound, and aluminum may be used. Conductor containing copper and titanium Conductor containing copper and manganese Conductor containing indium Alternatively, a conductor containing tin and oxygen, or a conductor containing titanium and nitrogen may be used.
[0293] The semiconductor device shown in FIG. 22 is the same as the transistor 2200 of the semiconductor device shown in FIG. Only the structure is different. Therefore, the semiconductor device shown in FIG. Please refer to the description of the semiconductor device. Specifically, the semiconductor device shown in FIG. The transistor 2200 is a Fin type. As a result, the effective channel width is increased, improving the on-characteristics of the transistor 2200. In addition, the contribution of the electric field of the gate electrode can be increased, The off characteristics of the transistor 2200 can be improved.
[0294] 23 is a semiconductor device in which the transistor 2200 of the semiconductor device shown in FIG. Only the structure is different. Therefore, the semiconductor device shown in FIG. Please refer to the description of the semiconductor device. Specifically, the semiconductor device shown in FIG. FIG. 23 shows the case where the semiconductor device 200 is provided on an SOI substrate. The region 456 is separated from the semiconductor substrate 450. Therefore, the punch-through phenomenon can be suppressed, and the transistor 2200 is turned off. The insulator 452 insulates a part of the semiconductor substrate 450. For example, the insulator 452 can be formed by densifying the insulating material. Recons can be used.
[0295] The semiconductor device shown in FIG. 21 to FIG. 23 is a p-channel transistor formed on a semiconductor substrate. By fabricating a MOSFET and fabricating an n-channel transistor above it, the area occupied by the device is reduced. In other words, the integration density of the semiconductor device can be increased. A p-channel transistor and a p-channel transistor were fabricated using the same semiconductor substrate. Since the process can be simplified compared to the conventional method, the productivity of the semiconductor device can be increased. In addition, the yield of the semiconductor device can be increased. The transistor is in the LDD (Lightly Doped Drain) region, shallow trench In some cases, complex processes such as ch-structure and distortion design can be omitted. Compared to manufacturing transistors using a semiconductor substrate, the productivity and yield are improved. It may be possible to reduce the
[0296] <CMOSアナログスイッチ> The circuit diagram shown in FIG. 20B is that of a transistor 2100 and a transistor 2200. The source and drain of each transistor are connected. It can function as a so-called CMOS analog switch.
[0297] <Storage device 1> A transistor according to one embodiment of the present invention is used to retain stored contents even when power is not supplied FIG. 24 shows an example of a semiconductor device (memory device) that can hold data and has no limit on the number of times it can be written. As shown in.
[0298] The semiconductor device shown in FIG. 24A includes a transistor 3200 using a first semiconductor and a The semiconductor device includes a transistor 3300 and a capacitor 3400. The transistor 3300 can be any of the transistors described above.
[0299] The transistor 3300 is preferably a transistor having a low off-state current. For example, a transistor including an oxide semiconductor can be used as the transistor 00. The low off-state current of the capacitor 3300 allows for long-term recording at a specific node of the semiconductor device. The contents of the memory can be retained, i.e., no refresh operation is required, or This allows the frequency of refresh operations to be reduced significantly, resulting in a semiconductor with low power consumption. It becomes a body device.
[0300] In FIG. 24A, a first wiring 3001 is electrically connected to the source of a transistor 3200. The second wiring 3002 is electrically connected to the drain of the transistor 3200. The third wiring 3003 is electrically connected to one of the source and drain of the transistor 3300. The fourth wiring 3004 is electrically connected to the gate of the transistor 3300. The gate of the transistor 3200 and the source of the transistor 3300 are connected to each other. The other of the drains is electrically connected to one of the electrodes of the capacitor 3400 and is connected to the fifth wiring 30 05 is electrically connected to the other electrode of the capacitor 3400 .
[0301] The semiconductor device shown in FIG. 24A can hold a gate potential of the transistor 3200. This property makes it possible to write, hold, and read information, as shown below. do.
[0302] The writing and holding of information will be described. First, the potential of the fourth wiring 3004 is changed by a transistor. The transistor 3300 is set to a potential at which the transistor 3300 is turned on. As a result, the potential of the third wiring 3003 is applied to the gate of the transistor 3200 and the The signal is applied to a node FG that is electrically connected to one of the electrodes of the capacitance element 3400. A predetermined charge is applied to the gate of the transistor 3200 (write). Charges that give two potential levels (hereinafter referred to as low-level charge and high-level charge) Then, the potential of the fourth wiring 3004 is applied to the transistor. By setting the potential at which the transistor 3300 is in a non-conducting state, the transistor 3300 is in a non-conducting state. As a result, charge is held at the node FG (retention).
[0303] Since the off-state current of the transistor 3300 is small, the charge of the node FG is retained for a long period of time. It will be held.
[0304] Next, reading of information will be described. A predetermined potential (constant potential) is applied to the first wiring 3001. When an appropriate potential (read potential) is applied to the fifth wiring 3005 in this state, 3002 takes a potential according to the amount of charge held in the node FG. This is the transistor If 3200 is an n-channel type, a high-level charge is applied to the gate of transistor 3200. The apparent threshold voltage V th_H is the transistor 3200 The apparent threshold voltage V when a low-level charge is applied to the gate th_L Yo Here, the apparent threshold voltage is the voltage at which the transistor 3200 is This refers to the potential of the fifth wiring 3005 required to make it in a "conductive state." Then, the potential of the fifth wiring 3005 is V th_H and V th_L By setting the potential between For example, in a write, the charge applied to node FG can be determined. When a high-level charge is applied to the fifth wiring 3005, the potential of the fifth wiring 3005 becomes V0 (> V th_H ), the transistor 3200 is in a "conducting state." On the other hand, the node FG When a low-level charge is applied to the fifth wiring 3005, the potential of the fifth wiring 3005 becomes V0 ( <V th_L ), transistor 3200 remains in a "non-conducting state." By determining the potential of the second wiring 3002, the data stored in the node FG is read. It can be put out.
[0305] When memory cells are arranged in an array, the information of a desired memory cell is read. In order not to read information from other memory cells, A potential at which transistor 3200 is in a "non-conducting state" regardless of the charge applied to FG. , that is, V th_H A lower potential may be applied to the fifth wiring 3005. A potential at which transistor 3200 is "on" regardless of the charge applied to the FG. , that is, V th_L A higher potential may be applied to the fifth wiring 3005 .
[0306] <Structure of semiconductor device 2> 25 is a cross-sectional view of the semiconductor device corresponding to FIG. 24(A). The semiconductor memory device includes a transistor 3200, a transistor 3300, and a capacitor 3400. The transistor 3300 and the capacitor 3400 are disposed above the transistor 3200. The transistor 3300 is arranged in the same manner as the transistor 2100 described above. In addition, the transistor 3200 may be the transistor shown in FIG. Please refer to the description of transistor 2200 in FIG. The case where the transistor 3200 is an n-channel transistor has been described. A transistor of a channel type may also be used.
[0307] A transistor 3200 shown in FIG. 25 is a transistor using a semiconductor substrate 450. The transistor 3200 includes a region 472 a in the semiconductor substrate 450 and a It has a region 472b, an insulator 462, and a conductor 454.
[0308] The semiconductor device shown in FIG. 25 includes an insulator 464, an insulator 466, an insulator 468, and a conductor. 480a, conductor 480b, conductor 480c, conductor 478a, and conductor 478b. , conductor 478c, conductor 476a, conductor 476b, conductor 474a, and conductor Conductor 474b, conductor 474c, conductor 496a, conductor 496b, and conductor 496 c, conductor 496d, conductor 498a, conductor 498b, conductor 498c, and conductor It has an insulator 498d, an insulator 490, an insulator 492, and an insulator 494.
[0309] An insulator 464 is disposed on the transistor 3200. Also, an insulator 466 is disposed on the insulator 4 64. Insulator 468 is disposed on insulator 466. Insulator 4 90 is disposed on the insulator 468. Also, the transistor 3300 is disposed on the insulator 490. Also, an insulator 492 is disposed on the transistor 3300. Also, an insulator 4 94 is disposed on the insulator 492 .
[0310] The insulator 464 has an opening reaching the region 472a, an opening reaching the region 472b, and a conductive The openings each include a conductor 480a, a conductor 480b, and an opening that reaches the conductor 454. The conductive body 480b or the conductive body 480c is embedded therein.
[0311] In addition, the insulator 466 has an opening that reaches the conductor 480a and an opening that reaches the conductor 480b. The openings each have a conductor 480c. 478a, conductor 478b or conductor 478c is embedded therein.
[0312] In addition, the insulator 468 has an opening that reaches the conductor 478b and an opening that reaches the conductor 478c. The openings are filled with a conductor 476a or a conductor 476b. It's embedded.
[0313] The insulator 490 has an opening overlapping the channel formation region of the transistor 3300 and a conductive The opening reaches the conductor 476a and the opening reaches the conductor 476b. The mouths are embedded with conductors 474a, 474b, and 474c, respectively. is.
[0314] The conductor 474a may function as a bottom gate electrode of the transistor 3300. Alternatively, for example, applying a constant potential to the conductor 474a may cause the transistor It is also possible to control electrical properties such as the threshold voltage of 3300. 474a is electrically connected to the conductor 404 which is the top gate electrode of the transistor 3300. This can increase the on-current of the transistor 3300. In addition, the punch-through phenomenon can be suppressed, so the transistor 3300 The electrical characteristics in the saturation region can be stabilized.
[0315] Also, the insulator 492 is connected to one of the source and drain electrodes of the transistor 3300. An opening through one conductor 416b to conductor 474b and a transistor 3300 An opening reaching the conductor 414 which is the other of the source electrode or drain electrode of the transistor An opening reaching the conductor 404 which is the gate electrode of the transistor 3300, and The other of the source electrode or drain electrode, conductor 416a, is passed through conductor 474c. The openings are provided with conductors 496a and 49 6b, conductor 496c or conductor 496d are embedded. The port may further go through any of the components such as transistor 3300.
[0316] Further, the insulator 494 has an opening that reaches the conductor 496a and an opening that reaches the conductor 496b. 496c, and an opening reaching conductor 496d. In addition, the openings are provided with a conductor 498a, a conductor 498b, a conductor 498c, or Electrical body 498d is embedded.
[0317] Insulator 464, insulator 466, insulator 468, insulator 490, insulator 492 or insulator At least one of 494 has an insulator that has the function of blocking impurities such as hydrogen and oxygen. It is preferable to add impurities such as hydrogen and oxygen to the vicinity of the transistor 3300. By disposing an insulator having a locking function, the electrical characteristics of the transistor 3300 are It can stabilize the sex.
[0318] The conductor 498d may be, for example, boron, nitrogen, oxygen, fluorine, silicon, phosphorus, or aluminum. Aluminum, titanium, chromium, manganese, cobalt, nickel, copper, zinc, gallium, Thorium, zirconium, molybdenum, ruthenium, silver, indium, tin, tantalum and A conductor containing one or more of copper and tungsten may be used in a single layer or a multilayer. For example, Conductors including aluminum, copper and titanium may be alloys or compounds. Conductors containing copper and manganese, conductors containing indium, tin and oxygen, titanium and conductors containing nitrogen may also be used.
[0319] The source or drain of transistor 3200 is connected to conductor 480b and conductor 478b. , the conductor 476a, the conductor 474b, and the conductor 496c. The conductor 416b is electrically connected to one of the source and drain electrodes of MOSFET 00. The conductor 454, which is the gate electrode of the transistor 3200, is connected to the conductor 480c. The conductor 478c, the conductor 476b, the conductor 474c, and the conductor 496d are connected to the The conductor 416a, which is the other of the source electrode or drain electrode of the transistor 3300, is electrically connected to Connect to the target.
[0320] The capacitor 3400 is connected to the other of the source electrode and the drain electrode of the transistor 3300. The electrode is electrically connected to the conductor 414, and the insulator 411. Since the gate insulator 1 can be formed in the same process as the gate insulator of the transistor 3300, the productivity can be improved. The conductor 414 may be a gate electrode of the transistor 3300. When layers formed through the same process are used, productivity can be increased.
[0321] For other structures, please refer to the descriptions in Figure 21 etc. as appropriate.
[0322] The semiconductor device shown in FIG. 26 is the same as the transistor 3200 of the semiconductor device shown in FIG. Only the structure is different. Therefore, the semiconductor device shown in FIG. Please refer to the description of the semiconductor device. Specifically, the semiconductor device shown in FIG. The figure shows a case where the transistor 200 is a fin type. For details, refer to the description of the transistor 2200 shown in FIG. The transistor 2200 is a p-channel transistor. The transistor 3200 may be an n-channel transistor.
[0323] 27 is a semiconductor device in which the transistor 3200 of the semiconductor device shown in FIG. Only the structure is different. Therefore, the semiconductor device shown in FIG. Please refer to the description of the semiconductor device. Specifically, the semiconductor device shown in FIG. 200 is provided on a semiconductor substrate 450 which is an SOI substrate. The transistor 3200 provided on the semiconductor substrate 450 is shown in FIG. Please refer to the description of the transistor 2200. Note that in FIG. The case where the transistor 3200 is an n-channel transistor has been described. A transistor of a channel type may also be used.
[0324] <Storage device 2> The semiconductor device shown in FIG. 24B differs from the semiconductor device shown in FIG. 24A in that it does not include the transistor 3200. In this case, the operation is the same as that of the semiconductor device shown in FIG. This makes it possible to write and retain information more easily.
[0325] The reading of data in the semiconductor device shown in FIG. When the capacitor 3300 is turned on, the third wiring 3003 and the capacitor element 3400, which are in a floating state, The third wiring 3003 and the capacitor 3400 are electrically connected to each other, and electric charges are redistributed between the third wiring 3003 and the capacitor 3400. As a result, the potential of the third wiring 3003 changes. The amount of change in the potential of the third wiring 3003 is expressed by the capacitance The potential of one of the electrodes of the element 3400 (or the charge stored in the capacitor element 3400) , take different values.
[0326] For example, the potential of one electrode of the capacitor 3400 is V, the capacitance of the capacitor 3400 is C, The capacitance component of the third wiring 3003 before the charge is redistributed is CB. If the potential is VB0, the potential of the third wiring 3003 after the charge is redistributed is (CB× VB0+C×V) / (CB+C). Therefore, the state of the memory cell is If the potential of one of the electrodes of the element 3400 takes two states, V1 and V0 (V1>V0), , the potential of the third wiring 3003 when the potential V1 is held (=(CB×VB0+C×V 1) / (CB+C)) is the potential of the third wiring 3003 when the potential V0 is held (= It can be seen that it is higher than (CB×VB0+C×V0) / (CB+C)).
[0327] Then, the potential of the third wiring 3003 is compared with a predetermined potential, thereby reading out information. can be done.
[0328] In this case, the transistor in which the first semiconductor is applied to a driving circuit for driving the memory cell. A transistor in which a second semiconductor is applied is used as the transistor 3300. The structure may be such that the electrodes are stacked on the driving circuit.
[0329] The above-described semiconductor device uses a transistor including an oxide semiconductor and has low off-state current. By doing so, it is possible to retain the memory contents for a long period of time. This eliminates the need for refresh operations or makes it possible to reduce the frequency of refresh operations significantly. Therefore, a semiconductor device with low power consumption can be realized. Even if the potential is fixed, it is possible to store the potential for a long period of time. It is possible to maintain the capacity.
[0330] In addition, the semiconductor device does not require a high voltage to write information, so that deterioration of the elements does not occur. For example, unlike conventional non-volatile memory, injection of electrons into the floating gate Since electrons are not introduced or removed from the floating gate, there is no risk of degradation of the insulator. That is, the semiconductor device according to one embodiment of the present invention does not have the problem of a conventional nonvolatile memory. A semiconductor device with dramatically improved reliability, without the problematic limit on the number of times it can be rewritten Furthermore, information is written depending on whether the transistor is conductive or non-conductive. This enables high-speed operation.
[0331] <Imaging device> An imaging device according to an aspect of the present invention will be described below.
[0332] FIG. 28A is a plan view illustrating an example of an imaging device 200 according to one embodiment of the present invention. The device 200 includes a pixel section 210, a peripheral circuit 260 for driving the pixel section 210, and a peripheral circuit The pixel section 210 has p rows and q columns. (p and q are integers of 2 or more) have a plurality of pixels 211 arranged in a matrix. The peripheral circuits 260, 270, 280, and 290 each include a plurality of The pixel 211 is connected to the pixel 211 and has a function of supplying a signal for driving the pixel 211. In this specification, the peripheral circuits 260, 270, 280, and and peripheral circuit 290 may be referred to as a "peripheral circuit" or a "drive circuit." For example, peripheral circuit 260 may be considered a part of the peripheral circuit.
[0333] The imaging device 200 preferably also includes a light source 291. The light source 291 emits detection light P It can emit 1.
[0334] The peripheral circuits include at least a logic circuit, a switch, a buffer, an amplifier, or a converter. The peripheral circuits may be formed on the same substrate as the pixel portion 210. Also, a semiconductor device such as an IC chip may be used for part or all of the peripheral circuits. The peripheral circuits are a peripheral circuit 260, a peripheral circuit 270, a peripheral circuit 280, and a peripheral circuit 290. Any one or more of these may be omitted.
[0335] As shown in FIG. 28B, in the pixel section 210 of the imaging device 200, By arranging the pixels 211 at an angle, the pixel size in the row direction and the pixel size in the pixel area can be increased. The pixel interval (pitch) in the column direction can be shortened. This can further improve the quality of the captured images.
[0336] <Pixel configuration example 1> The imaging device 200 has a pixel 211 that is composed of a plurality of sub-pixels 212. The pixel 212 is combined with a filter (color filter) that transmits light of a specific wavelength band. By this, it is possible to obtain information for realizing a color image display.
[0337] FIG. 29A is a plan view showing an example of a pixel 211 for acquiring a color image. The pixel 211 shown in FIG. 29(A) is provided with a color filter that transmits the red (R) wavelength band. The subpixel 212 (hereinafter also referred to as "subpixel 212R") transmits light in the green (G) wavelength band. A subpixel 212 (hereinafter also referred to as "subpixel 212G") provided with a color filter A subpixel 212 (hereinafter, referred to as a “subpixel”) is provided with a color filter that transmits light in the blue (B) wavelength band. The sub-pixel 212 can function as a photosensor. This can be done.
[0338] The subpixels 212 (subpixels 212R, 212G, and 212B) are connected to the wiring 23 1, electrically connected to wiring 247, wiring 248, wiring 249, and wiring 250. The pixel 212R, the sub-pixel 212G, and the sub-pixel 212B are each connected to an independent wiring 25 3. In this specification, for example, The wiring 248 and the wiring 249 are respectively represented as wiring 248[n] and wiring 249[n]. For example, the wiring 253 connected to the pixel 211 in the mth column is designated as wiring 253[m]. In FIG. 29A, the sub-pixel 212R of the pixel 211 in the m-th column is written as The wiring 253 connected to the subpixel 212G is disposed as wiring 253[m]R. The wiring 253 connected to the line 253[m]G and the subpixel 212B is referred to as a wiring 253[m]B. The subpixel 212 is electrically connected to the peripheral circuitry via the wiring.
[0339] In addition, the imaging device 200 has color filters that transmit the same wavelength band for adjacent pixels 211. The sub-pixels 212 in which the transistors are provided are electrically connected to each other via switches. 29(B), arranged in n rows (n is an integer between 1 and p) and m columns (m is an integer between 1 and q). A sub-pixel 212 of the pixel 211 and a sub-pixel 213 arranged in the n+1th row and the mth column adjacent to the pixel 211 29B shows an example of a connection of the sub-pixels 212 of the pixel 211. The sub-pixel 212R arranged in the n+1th row and the mth column is switched In addition, the sub-pixel 212G arranged in the nth row and the mth column is connected via the n+1 The sub-pixels 212G arranged in rows and columns m are connected via the switches 202. The sub-pixel 212B arranged in row m and column m and the sub-pixel 212B arranged in row (n+1) and column m are switched. The two are connected via a switch 203.
[0340] The color filters used for the subpixels 212 are not limited to red (R), green (G), and blue (B). The color filters transmit cyan (C), yellow (Y) and magenta (M) light respectively. A single pixel 211 may have three sub-pixels for detecting light of different wavelength bands. By providing 212, a full color image can be obtained.
[0341] Alternatively, color filters that transmit red (R), green (G) and blue (B) light are provided. In addition to the sub-pixel 212, a sub-pixel having a color filter that transmits yellow (Y) light is provided. Alternatively, pixel 211 may be used with pixel 212, or with cyan (C), yellow (Y In addition to the subpixel 212 provided with a color filter that transmits light of red (A) and magenta (M), The pixel 21 has a sub-pixel 212 provided with a color filter that transmits blue (B) light. A single pixel 211 may include sub-pixels 211 for detecting light of four different wavelength bands. By providing the second filter 12, the color reproducibility of the captured image can be further improved.
[0342] Also, for example, in FIG. 29A, a sub-pixel 212 detects the red wavelength band, The ratio of the number of sub-pixels 212 that detect the blue wavelength band and the number of sub-pixels 212 that detect the blue wavelength band ( or light receiving area ratio) does not have to be 1:1:1. For example, The Bayer array may be used with red:green:blue=1:2:1. The light area ratio may be red:green:blue=1:6:1.
[0343] The number of sub-pixels 212 provided in the pixel 211 may be one, but it is preferable that the number is two or more. By providing two or more sub-pixels 212 that detect the same wavelength band, redundancy is increased, and the imaging device This can improve the reliability of the device 200.
[0344] In addition, IR (IR: Infrared) filters absorb or reflect visible light and transmit infrared light. By using a filter, it is possible to realize an imaging device 200 that detects infrared light.
[0345] In addition, ND (Neutral Density) filters are used. This prevents output saturation that occurs when a large amount of light is incident on the photoelectric conversion element (light receiving element). By combining ND filters with different light reduction levels, This allows the dynamic range of the device to be increased.
[0346] In addition to the above-mentioned filter, a lens may be provided in the pixel 211. An example of the arrangement of the pixel 211, the filter 254, and the lens 255 will be described with reference to a cross-sectional view. By providing the lens 255, the photoelectric conversion element can efficiently receive incident light. Specifically, as shown in FIG. 30A, a lens 255 and a filter 25 are formed in a pixel 211. 4 (filter 254R, filter 254G and filter 254B), and pixel circuit 2 30 or the like, light 256 can be made incident on the photoelectric conversion element 220.
[0347] However, as shown in the area surrounded by the dashed line, a part of the light 256 indicated by the arrow is Therefore, as shown in Figure 30(B), A lens 255 and a filter 254 are disposed on the conversion element 220 side. It is preferable that the light 256 is received efficiently from the photoelectric conversion element 220 side. By making the light incident on the photoelectric conversion element 220, the imaging device 200 with high detection sensitivity is provided. can be done.
[0348] As the photoelectric conversion element 220 shown in FIG. 30, a pn-type junction or a pin-type junction is formed. A photoelectric conversion element may also be used.
[0349] In addition, the photoelectric conversion element 220 is made of a material having a function of absorbing radiation and generating electric charges. The material having the function of absorbing radiation and generating electric charges may be a sintered material. Iron, lead iodide, mercury iodide, gallium arsenide, cadmium telluride, cadmium zinc alloy etc.
[0350] For example, if selenium is used for the photoelectric conversion element 220, in addition to visible light, ultraviolet light, and infrared light, Photoelectric conversion element 2 that has a light absorption coefficient over a wide wavelength range, including X-rays and gamma rays 20 can be achieved.
[0351] Here, one pixel 211 included in the imaging device 200 has a sub-pixel 212 shown in FIG. 2, may include a subpixel 212 having a first filter.
[0352] <Pixel configuration example 2> In the following, a transistor using silicon and a transistor using an oxide semiconductor will be described. An example of forming a pixel using the above will be described.
[0353] 31(A) and 31(B) are cross-sectional views of elements constituting an imaging device. The imaging device shown in FIG. 1 includes a silicon transistor 35 provided on a silicon substrate 300. 1. Transistor 35 using an oxide semiconductor stacked over transistor 351 2 and a transistor 353, and a photodiode provided on the silicon substrate 300. Each transistor and photodiode 360 is connected to a different plug 370. and is electrically connected to the wiring 371. 61 has an electrical connection to plug 370 through low resistance region 363 .
[0354] The imaging device includes a transistor 351 and a photodiode 352 disposed on a silicon substrate 300. A layer 310 having an electrode 360 and a layer 371 provided in contact with the layer 310. 20 and in contact with layer 320, and includes transistors 352 and 353. A layer 330 is provided in contact with the layer 330 and has wiring 372 and wiring 373. It has 40.
[0355] In the example of the cross-sectional view of FIG. 31(A), the transistor 35 is disposed on the silicon substrate 300. The light receiving surface of the photodiode 360 is located on the surface opposite to the surface on which the photodiode 1 is formed. This configuration ensures an optical path without being affected by various transistors and wiring. This makes it possible to form pixels with a high aperture ratio. The light receiving surface of 360 may be the same as the surface on which the transistor 351 is formed.
[0356] In the case where a pixel is formed using a transistor including an oxide semiconductor, the layer 310 Alternatively, the layer 310 may be omitted. Alternatively, a pixel may be formed using only a transistor including an oxide semiconductor.
[0357] When a pixel is constructed using a silicon transistor, the layer 330 is omitted. An example of a cross-sectional view in which the layer 330 is omitted is shown in FIG. In this case, the wiring 372 of the layer 340 may also be omitted.
[0358] The silicon substrate 300 may be an SOI substrate. Instead, germanium, silicon germanium, silicon carbide, gallium arsenide, and aluminum arsenide The substrate has a gallium nitride, indium phosphide, gallium nitride or organic semiconductor. You can also be there.
[0359] Here, a layer 310 having a transistor 351 and a photodiode 360, An insulator 380 is provided between the layer 330 having the resistor 352 and the transistor 353. However, the position of the insulator 380 is not limited.
[0360] The hydrogen in the insulator provided near the channel forming region of the transistor 351 is converted into silicon diaphragm. This has the effect of terminating the ring bond and improving the reliability of the transistor 351. , hydrogen in an insulator provided near the transistor 352 and the transistor 353, etc. This is one of the factors that generate carriers in the oxide semiconductor. This may cause a decrease in reliability of the transistor 52 and the transistor 353. Therefore, a transistor using an oxide semiconductor is placed on top of a transistor using a silicon semiconductor. When the capacitors are stacked, an insulator 380 having a function of blocking hydrogen is provided between them. It is preferable to provide the insulator 380. By confining hydrogen below the insulator 380, the transistor The reliability of the insulator 351 can be improved. Since hydrogen diffusion to layers above 380 can be suppressed, the transistors 352 and This can improve the reliability of the transistor 353 and the like.
[0361] As the insulator 380, for example, an insulator having a function of blocking oxygen or hydrogen is used. There are.
[0362] In the cross-sectional view of FIG. 31(A), a photodiode 360 provided in the layer 310 and a The transistor 330 can be formed so as to overlap with the transistor 330. In other words, the resolution of the imaging device can be increased.
[0363] As shown in FIG. 32(A1) and FIG. 32(B1), a part or the whole of the imaging device may be 32(A1) shows the imaging device in the direction of the dashed line X1-X2 in the figure. FIG. 32(A2) shows the curved state. FIG. 32(A3) is a cross-sectional view of the portion indicated by the dashed line Y1-2 in FIG. This is a cross-sectional view of the portion indicated by Y2.
[0364] FIG. 32(B1) shows a case where the imaging device is bent in the direction of the dashed line X3-X4 in the same figure, and FIG. 32(B2) shows a state where the wire is bent in the direction of the dashed line Y3-Y4 in the figure. FIG. 32(B3) is a cross-sectional view of a portion indicated by a dashed line X3-X4 in FIG. 32(B1) is a cross-sectional view of a portion indicated by dashed dotted line Y3-Y4 in FIG.
[0365] By curving the imaging device, it is possible to reduce the field curvature and astigmatism. This makes it easier to design the lenses and other components used in combination with the imaging device. For example, The number of lenses required for aberration correction can be reduced, which contributes to the miniaturization of electronic devices that use imaging devices. It is possible to realize a lighter weight and a smaller camera. It is also possible to improve the quality of the captured image. .
[0366] <cpu> In the following, a CPU including the above-mentioned transistor and the above-mentioned semiconductor device such as the memory device will be described. I will explain this in more detail.
[0367] FIG. 33 is a block diagram showing the configuration of an example of a CPU that uses the above-mentioned transistor in part. be.
[0368] The CPU shown in FIG. 33 includes an ALU 1191 (ALU: Arithmetic logic unit) on a board 1190. ic logic unit, arithmetic circuit), ALU controller 1192, instruction A timing decoder 1193, an interrupt controller 1194, and a timing controller 1195, register 1196, register controller 1197, bus interface 1 198, rewritable ROM 1199, and ROM interface 1189 The substrate 1190 may be a semiconductor substrate, an SOI substrate, a glass substrate, or the like. 199 and the ROM interface 1189 may be provided on a separate chip. The CPU shown in FIG. 33 is merely an example showing a simplified configuration. There are many different configurations depending on the application. For example, the CPU or arithmetic circuit shown in FIG. A configuration including the above is considered as one core, and multiple such cores are included, and each core operates in parallel. The number of bits that the CPU can handle in the internal arithmetic circuit and data bus is as follows: For example, it can be 8-bit, 16-bit, 32-bit, 64-bit, etc.
[0369] The instructions input to the CPU via the bus interface 1198 are The signal is input to the decoder 1193, decoded, and then passed to the ALU controller 1192, the interface Rupture Controller 1194, Register Controller 1197, Timing Controller Entered into 1195.
[0370] ALU controller 1192, interrupt controller 1194, register controller The controller 1197 and the timing controller 1195 control various Specifically, the ALU controller 1192 controls the operation of the ALU 1191. The interrupt controller 1194 also generates signals for the CPU program. During system execution, interrupt requests from external I / O devices and peripheral circuits are handled according to their priority and mask. The register controller 1197 determines the address of the register 1196 and processes it. It generates addresses and reads and writes to register 1196 depending on the state of the CPU.
[0371] The timing controller 1195 also includes the ALU 1191 and the ALU controller 119 2, an instruction decoder 1193, an interrupt controller 1194, and It generates a signal to control the operation timing of the register controller 1197. The timing controller 1195 generates an internal clock signal based on the reference clock signal. The internal clock generating unit supplies an internal clock signal to the various circuits described above.
[0372] In the CPU shown in FIG. 33, a register 1196 is provided with a memory cell. The above-mentioned transistors and memory devices can be used as the memory cells of 1196. do.
[0373] In the CPU shown in FIG. 33, the register controller 1197 receives the According to the instruction, the holding operation is selected in the register 1196. In the memory cell of the Select whether to hold data by flip-flops. If the power supply voltage is set to 0, the power supply voltage is supplied to the memory cells in the register 1196. If data retention is selected for the capacitive element, data is rewritten to the capacitive element. This allows the supply of power supply voltage to the memory cells in the register 1196 to be stopped.
[0374] FIG. 34 is a circuit diagram of an example of a storage element 1200 that can be used as the register 1196. The memory element 1200 includes a circuit 1201 in which stored data is volatilized when the power is cut off, and a A circuit 1202 that prevents stored data from volatilizing when the circuit is turned off, a switch 1203, and a switch 1204. 1206, a capacitor 1207, and a circuit 1220 having a selection function. The circuit 1202 includes a capacitor 1208, a transistor 1209, and a transistor 10. The memory element 1200 may include a diode, a resistor, It may further include other elements such as an inductor.
[0375] Here, the above-mentioned memory device can be used for the circuit 1202. When the supply of power supply voltage to the ND (0V) or a potential at which the transistor 1209 is turned off is continuously input. For example, the gate of the transistor 1209 is grounded via a load such as a resistor. .
[0376] The switch 1203 uses a transistor 1213 of one conductivity type (for example, an n-channel type). The switch 1204 is configured as a transistor of the opposite conductivity type (for example, a p-channel type). An example using a transistor 1214 is shown. Here, the first terminal of the switch 1203 The input corresponds to one of the source and drain of the transistor 1213, and the second input of the switch 1203. The terminal of corresponds to the other of the source and drain of the transistor 1213, and the switch 1203 A control signal RD input to the gate of the transistor 1213 switches the first terminal and the second terminal Conduction or non-conduction between the terminals (i.e., the conductive or non-conductive state of the transistor 1213) The first terminal of the switch 1204 is connected to the source and drain of a transistor 1214. The second terminal of the switch 1204 corresponds to one of the drains of the The switch 1204 is connected to the gate of the transistor 1214. A control signal RD is input to the first terminal and the second terminal to establish or break continuity (i.e., The conductive or non-conductive state of transistor 1214 is selected.
[0377] One of the source and drain of the transistor 1209 is connected to a pair of electrodes of the capacitor 1208. The connection part is electrically connected to one of the gate electrodes of the transistor 1210 and the gate of the transistor 1210. The node M2 is connected to the source or drain of the transistor 1210. The other is electrically connected to a wiring (for example, a GND line) that can supply 1203 (one of the source and drain of the transistor 1213). The second terminal of the switch 1203 (the source and drain of the transistor 1213) is connected to the The other terminal of the switch 1204 (one of the source and drain terminals of the transistor 1214) The second terminal of the switch 1204 (the source terminal of the transistor 1214) is electrically connected to the The other of the source and drain terminals is electrically connected to a wiring that can supply the power supply potential VDD. The second terminal of the switch 1203 (the other of the source and drain of the transistor 1213) ) and a first terminal of the switch 1204 (one of the source and drain of the transistor 1214 ), an input terminal of a logic element 1206, and one of a pair of electrodes of a capacitor 1207; are electrically connected. Here, the connection point is referred to as node M1. The other of the electrodes may be configured to have a constant potential input thereto. It can be configured so that a power supply potential (GND, etc.) or a high power supply potential (VDD, etc.) is input. The other of the pair of electrodes of the capacitor 1207 is connected to a line that can supply a low power supply potential. The other of the pair of electrodes of the capacitor 1208 is electrically connected to a line (for example, a GND line). For example, a low power supply potential (GND, etc.) can be input. ) or a high power supply potential (such as VDD) can be input to the capacitance element 120. The other of the pair of electrodes 8 is connected to a wiring capable of supplying a low power supply potential (for example, GND The power supply is electrically connected to the power supply line.
[0378] The capacitors 1207 and 1208 are used to reduce parasitic capacitance of transistors and wirings. It is possible to omit it by making active use of it.
[0379] A control signal WE is input to the gate of the transistor 1209. and the switch 1204 is connected between the first terminal and the second terminal by a control signal RD that is different from the control signal WE. A conductive state or a non-conductive state between the first and second terminals of one switch is selected. When the terminals of the switch are in a conductive state, the first and second terminals of the other switch are in a non-conductive state. It becomes.
[0380] The other of the source and drain of the transistor 1209 is connected to a data register 1204. In FIG. 34, the signal output from the circuit 1201 corresponds to the The example shown is input to the other of the source and drain of the switch 1203. The signal output from the second terminal (the other of the source and drain of the transistor 1213) is The logic value is inverted by the logic element 1206 to become an inverted signal, and the inverted signal is output via the circuit 1220. and input to the circuit 1201.
[0381] In FIG. 34, the second terminal of the switch 1203 (the source and drain of the transistor 1213) The signal output from the other of the two trains is routed through logic element 1206 and circuit 1220. The second terminal of the switch 1203 is connected to the first terminal of the switch 1203. The signal output from the other of the source and drain of the transistor 1213 is inverted. For example, the following may be included in the circuit 1201: When there is a node that holds a signal with the inverted logical value of the signal input from the input terminal The second terminal of the switch 1203 (the other of the source and drain of the transistor 1213) A signal output from the input terminal can be input to the node.
[0382] In addition, in FIG. 34, among the transistors used in the memory element 1200, The transistors other than the transistor 1209 are made of a film or a substrate 119 made of a semiconductor other than an oxide semiconductor. For example, a transistor having a channel formed at 0 can be used. The transistor may have a channel formed in a silicon substrate. All the transistors used in 1200 are transistors whose channels are formed of oxide semiconductors. Alternatively, the memory element 1200 may include other elements besides the transistor 1209. The other transistors may include a transistor in which the channel is formed of an oxide semiconductor. The transistor has a channel formed in a film or substrate 1190 made of a semiconductor other than an oxide semiconductor. Alternatively, the transistor may be a transistor having a capacitance of 100 .mu.m.
[0383] For example, a flip-flop circuit can be used for the circuit 1201 in FIG. The logic element 1206 may be, for example, an inverter or a clocked inverter. It is possible.
[0384] In the semiconductor device according to one embodiment of the present invention, while a power supply voltage is not supplied to the memory element 1200, The data stored in the circuit 1201 is transferred to the capacitor 1208 in the circuit 1202. It can be held by
[0385] In addition, a transistor in which a channel is formed in an oxide semiconductor has an extremely small off-state current. For example, the off-state current of a transistor in which a channel is formed in an oxide semiconductor The off-current is significantly lower than that of transistors with a channel formed in silicon. By using this transistor as the transistor 1209, the memory element 120 The signal held in the capacitance element 1208 is maintained for a long period of time even while the power supply voltage is not supplied to the In this way, the memory element 1200 can retain its stored contents (data) even when the supply of power supply voltage is stopped. ) can be held.
[0386] In addition, by providing the switches 1203 and 1204, the precharge operation Since the circuit 1201 is a memory element that performs the above-mentioned operation after the power supply voltage is restarted, This shortens the time it takes to restore the original data.
[0387] In the circuit 1202, the signal held by the capacitor 1208 is The power supply voltage to the memory element 1200 is then restarted. After that, the signal held by the capacitance element 1208 is converted into the state of the transistor 1210 ( The state can be converted to a conductive state or a non-conductive state and read out from the circuit 1202. Therefore, even if the potential corresponding to the signal held in the capacitance element 1208 fluctuates slightly, the original signal It is possible to read out the number accurately.
[0388] Such a memory element 1200 may be a register or a cache memory of a processor. By using it in a storage device, it is possible to prevent data loss in the storage device due to a power supply interruption. In addition, after the supply of power voltage is resumed, the state before the power supply was stopped can be restored in a short time. Therefore, the entire processor, or one or more components of the processor, Since the power supply can be stopped for a short period of time in multiple logic circuits, power consumption can be reduced. It can be suppressed.
[0389] Although the memory element 1200 has been described as being used as a CPU, the memory element 1200 can also be used as a DSP ( Digital Signal Processor), Custom LSI, PLD (Pr LSIs such as grammable logic devices, RF (Radio Frequency It can also be applied to low-requency devices.
[0390] <Display device> A display device according to one embodiment of the present invention will be described below with reference to FIGS. 35 and 36. do.
[0391] Display elements used in display devices include liquid crystal elements (also called liquid crystal display elements), light-emitting elements, etc. The light-emitting element can be a light-emitting display element. Therefore, the category includes elements whose luminance can be controlled, specifically inorganic EL (Electroluminescent) The following is an example of a display device. Display devices using EL elements (EL display devices) and display devices using liquid crystal elements (liquid crystal display devices) This section explains the display device.
[0392] The display device described below is a panel in which a display element is sealed, and a control circuit is attached to the panel. This includes modules in which ICs including controllers are mounted.
[0393] The display device described below refers to an image display device or a light source (including a lighting device). Also, connectors, such as FPC, modules with TCP attached, and TCP with printers A module or display element with a printed wiring board has an IC (integrated circuit) mounted on it by the COG method. The display device also includes all modules mounted on the display device.
[0394] 35A and 35B are diagrams illustrating an example of an EL display device according to one embodiment of the present invention. 35(B) is a top view showing the entire EL display device.
[0395] FIG. 35A is an example of a circuit diagram of a pixel used in an EL display device.
[0396] In this specification, the terms "active elements" and "passive elements" are used interchangeably. For all terminals of devices (capacitive elements, resistive elements, etc.), the connection destination is not specified. However, a person skilled in the art may be able to configure one aspect of the invention. Even if the destination is not specified, one aspect of the invention is clear. When the contents are described in this specification, etc., one aspect of the invention that does not specify a connection destination is the same as the embodiment of the present specification. In particular, if the terminal is connected to multiple When multiple locations are anticipated, it is not necessary to limit the connection destination of the terminal to a specific location. Therefore, active elements (transistors, diodes, etc.) and passive elements (capacitive elements, resistive elements) By specifying the connection destinations of only some of the terminals on It may be possible to configure a clear embodiment.
[0397] In this specification and the like, if at least the connection destination of a certain circuit is specified, it is understood by those skilled in the art that If you are a person who has experience in the field of electronics, you may be able to identify the invention. In some cases, a person skilled in the art can identify an invention by at least specifying the function. In other words, if the function is specified, one aspect of the invention is clear. It may be possible to determine that one aspect of the invention is described in the present specification. Therefore, even if the function of a circuit is not specified, if the connection destination is specified, it can be considered as an embodiment of the invention. and can constitute one embodiment of the invention. For a certain circuit, even if the connection destination is not specified, if the function is specified, it can be considered as one aspect of the invention. What is disclosed can constitute an embodiment of the invention.
[0398] The EL display device shown in FIG. 35(A) includes a switch element 743, a transistor 741, and a capacitor. The light emitting element 719 includes a capacitance element 742 and a light emitting element 719 .
[0399] Note that FIG. 35(A) is an example of a circuit configuration, and therefore, if a transistor is added, Conversely, at each node in FIG. 35(A), a transistor, a switch, It is also possible to avoid adding passive elements.
[0400] The gate of the transistor 741 is connected to one end of the switch element 743 and one end of the capacitance element 742. The source of the transistor 741 is electrically connected to the other electrode of the capacitor 742. and is electrically connected to one electrode of the light-emitting element 719. The drain of the switch element 741 is supplied with a power supply potential VDD. The other end of the switch element 743 is connected to the signal line 7 The other electrode of the light-emitting element 719 is electrically connected to the light-emitting element 44. A constant potential is applied to the other electrode of the light-emitting element 719. The constant potential is the ground potential GND or a potential lower than that.
[0401] It is preferable to use a transistor as the switch element 743. This allows the pixel area to be reduced, resulting in an EL display device with high resolution. The switch element 743 is a transistor manufactured through the same process as the transistor 741. By using the transistor 74, the productivity of the EL display device can be improved. As the switch element 743, for example, the above-mentioned transistor is applied. It is possible.
[0402] FIG. 35(B) is a top view of the EL display device. The EL display device is made up of a substrate 700 and a substrate 7 50, a sealant 734, a driving circuit 735, a driving circuit 736, a pixel 737, and an FP The sealing material 734 includes the pixel 737, the driving circuit 735, and the driving circuit The driving circuit 735 is disposed between the substrate 700 and the substrate 750 so as to surround the driving circuit 736. Alternatively / and the driving circuit 736 may be disposed outside the sealing material 734 .
[0403] FIG. 35(C) is a cross-sectional view of an EL display device corresponding to a part of the dashed line MN in FIG. 35(B). It is.
[0404] In FIG. 35C, a conductor 704 a on a substrate 700 and a conductor An insulator 712a on the body 704a, an insulator 712b on the insulator 712a, and an insulator 712 A semiconductor 706 that is on the semiconductor 704a and overlaps with the conductor 704a, and a conductor 716 that is in contact with the semiconductor 706. a and conductor 716b, an insulator 710a on the conductor 716a, and an insulator 710b on the conductor 716b. The insulator 710b, the semiconductor 706, the conductor 716a, the conductor 716b, and the insulator 71 Insulator 718a on insulator 710a and on insulator 710b, and insulator 718b on insulator 718a. , an insulator 718c on the insulator 718b, and an insulator 718c on the insulator 718c overlapping the semiconductor 706. Note that the structure of the transistor 741 is just an example. Therefore, the structure may be different from the structure shown in FIG.
[0405] Therefore, in the transistor 741 shown in FIG. The insulators 712a and 712b function as gate insulators. The conductor 716a functions as a source electrode, and the conductor 716b functions as a drain electrode. The insulators 718a, 718b, and 718c function as gate electrodes. The conductor 714a functions as a gate insulator, and the conductor 714b functions as a gate electrode. The electrical characteristics of the semiconductor 706 may change when exposed to light. At least one of the conductor 704a, the conductor 716a, the conductor 716b, and the conductor 714a is shielded. It is preferable that the photosensitive material has a photoresist property.
[0406] The interface between the insulator 718a and the insulator 718b is shown by a dashed line. For example, insulators 718a and 718b may not be clearly defined. Therefore, when the same type of insulator is used, it may be difficult to distinguish between the two depending on the observation method.
[0407] In FIG. 35C, a conductor 704b on a substrate and a conductor 704b are used as the capacitor 742. an insulator 712a on the insulator 712a, an insulator 712b on the insulator 712a, and an insulator 712b on the insulator 712b. A conductor 716a overlapping the conductor 704b, an insulator 718a on the conductor 716a, and an insulating An insulator 718b on the insulator 718a, an insulator 718c on the insulator 718b, and an insulator 718 and a conductor 714b that is on the conductor 714c and overlaps the conductor 716a. In the overlapping region of the insulator 714b, a part of the insulator 718a and the insulator 718b are removed. The structure shown is as follows:
[0408] In the capacitor 742, the conductor 704b and the conductor 714b function as one electrode. The conductor 716a serves as the other electrode.
[0409] Therefore, the capacitor 742 can be formed using a film common to the transistor 741. In addition, it is preferable that the conductor 704a and the conductor 704b are made of the same type of conductor. In this case, the conductor 704a and the conductor 704b can be formed through the same process. In addition, the conductor 714a and the conductor 714b are preferably made of the same type of conductor. In this case, the conductor 714a and the conductor 714b can be formed through the same process. .
[0410] A capacitor 742 shown in FIG. 35C has a large capacitance per occupied area. Therefore, the EL display device shown in FIG. 35(C) has high display quality. The illustrated capacitive element 742 is formed by thinning the overlapping area of the conductor 716a and the conductor 714b. Therefore, the insulator 718a and the insulator 718b are partially removed. The capacitive element according to one embodiment is not limited to this. For example, the conductors 716a and A structure in which a part of the insulator 718c is removed to thin the overlapping area of the conductor 714b. It is okay to have one.
[0411] An insulator 720 is provided over the transistor 741 and the capacitor 742. The insulator 720 extends to a conductor 716a which serves as the source electrode of the transistor 741. The insulator 720 may have an opening. A conductor 781 is disposed on the insulator 720. The conductor 78 1 may be electrically connected to transistor 741 through an opening in insulator 720.
[0412] A partition 784 having an opening reaching the conductor 781 is disposed over the conductor 781. A light-emitting layer 782 is disposed on the wall 784 so as to be in contact with the conductor 781 at the opening of the partition wall 784. A conductor 783 is disposed over the light-emitting layer 782. The overlapping region of the conductor 783 becomes the light-emitting element 719 .
[0413] So far, an example of an EL display device has been described. Next, an example of a liquid crystal display device will be described. do.
[0414] FIG. 36(A) is a circuit diagram showing an example of the configuration of a pixel of a liquid crystal display device. The pixel shown in FIG. A transistor 751, a capacitor element 752, and an element in which liquid crystal is filled between a pair of electrodes (liquid crystal The liquid crystal element 753 is also included.
[0415] In the transistor 751, one of the source and the drain is electrically connected to a signal line 755. The gate is electrically connected to a scan line 754 .
[0416] In the capacitor 752, one electrode is electrically connected to the other of the source and drain of the transistor 751. The other electrode is electrically connected to a wiring that supplies a common potential.
[0417] In the liquid crystal element 753, one electrode is electrically connected to the other of the source and drain of the transistor 751. The other electrode is electrically connected to a wiring that supplies a common potential. A common potential applied to a wiring to which the other electrode of the capacitor 752 is electrically connected, The common potential applied to the other electrode of the liquid crystal element 753 may be different from the common potential applied to the other electrode of the liquid crystal element 753 .
[0418] The liquid crystal display device will be described assuming that the top view is the same as that of the EL display device. A cross-sectional view of the liquid crystal display device corresponding to the dotted-chain line MN is shown in FIG. In this case, the FPC 732 is connected to the wiring 733a via the terminal 731. 3a is a conductor or a semiconductor of the same type as the conductor or semiconductor that constitutes the transistor 751. Alternatively, a semiconductor may be used.
[0419] For the transistor 751, refer to the description of the transistor 741. For 752, refer to the description of the capacitor 742. Although the structure of the capacitor 752 corresponding to the capacitor 742 in (C) is shown, the present invention is not limited to this. stomach.
[0420] Note that when an oxide semiconductor is used as the semiconductor of the transistor 751, the off-state current is extremely small. Therefore, the charge held in the capacitor 752 can be Therefore, the voltage applied to the liquid crystal element 753 can be maintained for a long period of time. Therefore, when displaying a moving image or a still image with little movement, the transistor 751 is turned off. This eliminates the need for power to operate the transistor 751, and the liquid crystal display has low power consumption. In addition, the area occupied by the capacitor 752 can be reduced; It is possible to provide a liquid crystal display device with a high aperture ratio or a high-definition liquid crystal display device.
[0421] An insulator 721 is provided over the transistor 751 and the capacitor 752. The insulator 721 has an opening that reaches the transistor 751. The conductor 791 is disposed on the insulator 721. The conductor 791 is connected to the transistor Electrically connect to 751.
[0422] An insulator 792 functioning as an alignment film is provided over the conductor 791. A liquid crystal layer 793 is disposed on the liquid crystal layer 793. An insulator 794 that functions as an alignment film is disposed on the liquid crystal layer 793. 94 is disposed on the insulator 794. A spacer 795 is disposed on the insulator 794. A conductor 796 is disposed on the insulator 794. The substrate 79 7 is placed.
[0423] By using the above-mentioned structure, it is possible to provide a display device having a capacitance element with a small occupancy area. Alternatively, a display device with high display quality can be provided. It is possible to provide a display device.
[0424] For example, in this specification and the like, the term "display element," "display device having a display element," "light-emitting element," A light-emitting device, which is a device having a light-emitting element and a light-emitting element, can be used in various forms or in various The display element, the display device, the light-emitting element, or the light-emitting device may include, for example, For example, EL elements (EL elements containing organic and inorganic materials, organic EL elements, inorganic EL elements), white Light emitting diodes (LEDs) of various colors, such as red, green, or blue. g Diode), transistor (transistor that emits light according to electric current), electron emitter , liquid crystal elements, electronic ink, electrophoretic elements, grating light valves (GLVs), plastics Zuma Display (PDP), MEMS (Micro-Electro-Mechanical System) ), digital micromirror device (DMD), DMS (digital Micro Shutter), IMOD (Interference Modulation) element, Shutter-type MEMS display element, optical interference-type MEMS display element, electrowet display elements using piezoelectric ceramic displays and carbon nanotubes At least one of the following is possible: contrast, brightness, and reflection are controlled by electrical or magnetic effects. It may have a display medium whose reflectance, transmittance, etc. change.
[0425] An example of a display device using an EL element is an EL display. An example of a display device using this method is a field emission display (FED). is a flat panel display using the SED method (SED: Surface-conduction E LCD displays are used in the following applications: An example of the device is a liquid crystal display (transmissive liquid crystal display, semi-transmissive liquid crystal display, etc.). play, reflective LCD, direct-view LCD, projection LCD) An example of a display device using electronic ink or electrophoretic elements is an electronic page. In addition, there are also other LCDs that can realize semi-transmissive and reflective LCD displays. In this case, a part or the whole of the pixel electrode may be made to function as a reflective electrode. For example, a part or the whole of the pixel electrode may be made of aluminum, silver, etc. In this case, a memory circuit such as an SRAM may be provided under the reflective electrode. This makes it possible to further reduce power consumption.
[0426] When using an LED, graphene or graphene is placed under the LED electrode or nitride semiconductor. Graphene and graphite can be arranged in layers to form a multilayer film. In this way, by providing graphene or graphite, it is possible to form a nitride on the graphene or graphite. Semiconductors, such as n-type GaN semiconductors having crystals, can be easily formed into films. Furthermore, a p-type GaN semiconductor having crystals can be placed on top of it to form an LED. It is possible to fabricate a crystalline n-type GaN semiconductor using graphene or graphite. An AlN layer may be provided. The GaN semiconductor in the LED is formed by MOCVD. However, by providing graphene, the GaN semiconductor of the LED can be It is also possible to form the film by a tar deposition method.
[0427] <Electronic equipment> A semiconductor device according to one aspect of the present invention includes a display device, a personal computer, and a recording medium. Image playback devices with advanced functions (typically DVD: Digital Versatile Disc (Devices having a display capable of playing back recording media such as 3D models and displaying the images) In addition, an electronic device in which the semiconductor device according to one embodiment of the present invention can be used Mobile phones, handheld game consoles, portable data terminals, e-book terminals, video cameras , cameras such as digital still cameras, goggle-type displays (head-mounted displays) Ray), navigation systems, audio playback devices (car audio, digital audio players, copiers, fax machines, printers, printer-combiners, automated teller machines Examples of such electronic devices include ATMs and vending machines. vinegar.
[0428] FIG. 37A shows a portable game machine, which includes a housing 901, a housing 902, a display unit 903, and a display unit 904. 904, microphone 905, speaker 906, operation key 907, stylus 908 The portable game machine shown in FIG. 37A has two display units 903 and a display However, the number of display units that the portable game machine has is not limited to this. .
[0429] FIG. 37B shows a portable data terminal, which includes a first housing 911, a second housing 912, and a first display unit 9 13, a second display unit 914, a connection unit 915, an operation key 916, etc. The first display unit 911 is provided in the first housing 911, and the second display unit 914 is provided in the second housing 912. The first housing 911 and the second housing 912 are connected by a connection part 915. The angle between the first housing 911 and the second housing 912 can be changed by the connection part 915. The image on the first display unit 913 is transmitted between the first housing 911 and the second housing 912 at the connection unit 915. 12. Also, the first display unit 913 may be configured to switch according to the angle between the first display unit 913 and the second display unit 913. and a display having a function as a position input device added to at least one of the first and second display units 914. The function of the position input device may be achieved by touching the display device. The function as a position input device can be added by providing a touch panel. It can also be added by providing a photoelectric conversion element, also called a photosensor, in the pixel portion of the display device. It is possible.
[0430] FIG. 37C shows a notebook personal computer, which includes a housing 921, a display unit 922, and a keyboard. The display device 922 includes a keyboard 923, a pointing device 924, and the like.
[0431] FIG. 37(D) shows an electric refrigerator-freezer, which includes a housing 931, a refrigerator compartment door 932, and a freezer compartment door 93. Holds 3rd place.
[0432] FIG. 37E shows a video camera, which includes a first housing 941, a second housing 942, a display unit 943, The operation key 944, the lens 945, the connection part 946, etc. 945 is provided in the first housing 941, and the display unit 943 is provided in the second housing 942. The first housing 941 and the second housing 942 are connected by a connection portion 946. The angle between the first housing 941 and the second housing 942 can be changed by the connection part 946. The image on the display unit 943 is transmitted between the first housing 941 and the second housing 94 at the connection unit 946. 2.
[0433] FIG. 37(F) shows an automobile, which includes a body 951, wheels 952, a dashboard 953, and lights. 954 etc. EXAMPLES
[0434] In this example, an example of using a processing method according to one embodiment of the present invention will be described.
[0435] First, a 126.6 mm square silicon substrate is prepared. Then, a thickness of 400 mm is reduced by thermal oxidation. Next, a 40-nm-thick In- A Ga-Zn oxide film is then formed. Next, a tungsten film with a thickness of 50 nm is formed by sputtering. A tenn film is formed.
[0436] Next, a 170 nm thick anti-reflection layer is deposited. Next, a resist is deposited. Next, The resist is exposed using a photomask. The resist is then developed to create a 300 nm groove. do.
[0437] Next, 50 sccm of trifluoromethane gas and 100 sccm of helium gas were added. The plasma was generated using a pressure of 5.5 Pa and the substrate temperature was 1000 MPa. The temperature was 70°C, the ICP power was 475 W, the bias power was 300 W, and the treatment time was 80 seconds. At this time, organic matter adheres to the sides of the resist and the anti-reflection layer as shown in FIG. 6(C). do.
[0438] Next, 45 sccm of chlorine gas, 55 sccm of carbon tetrafluoride gas, and 55 sccm The plasma is generated using oxygen gas of 10000 vol., and the tungsten film is etched by the plasma treatment. The pressure was 0.67 Pa, the ICP power was 3000 W, and the bias power was 11 The etching time was set to 15 seconds (referred to as tungsten etching condition A). The tungsten film is then etched as shown in FIG. 6(D).
[0439] Next, the organics, resist and anti-reflection materials are removed by plasma ashing and wet etching. By removing the antireflection layer, the shape shown in FIG. 6(E) can be obtained. 46(A) and 46(B). In FIG. 46(A), Cross-sectional scanning transmission electron microscope (STEM) Figure 46(B) shows the silicon substrate. A cross-sectional STEM image of a corner of the plate is shown.
[0440] In both Figure 46(A) and Figure 46(B), the distance between the tungsten films is 177 nm. That is, a groove having a smaller shape than the size of the resist groove is formed in the tungsten film. was created.
[0441] In addition, the same evaluation was performed when the etching conditions for the tungsten film were changed. Specifically, 60 sccm of carbon tetrafluoride gas and 40 sccm of oxygen gas were used. The plasma was generated by the plasma treatment, and the tungsten film was etched. The pressure was 2 Pa, the ICP power was 1000 W, the bias power was 25 W, and the treatment time was 35 seconds. (This is referred to as tungsten etching condition B).
[0442] Next, the organics, resist and anti-reflection materials are removed by plasma ashing and wet etching. The antireflection layer is removed. The results are shown in Figure 47(A) and Figure 47(B). Figure 47(A) shows a cross-sectional STEM image of the center of the silicon substrate, and Figure 47(B) shows the cross-sectional STEM image of the silicon substrate. A cross-sectional STEM image of a corner of the plate is shown.
[0443] In both Figure 47(A) and Figure 47(B), the distance between the tungsten films is 158 nm. Even under these conditions, grooves smaller than the size of the resist grooves were formed in the tungsten film. I was able to do it. EXAMPLES
[0444] In this embodiment, the tungsten film shown in Example 1 is used as a source electrode and a drain electrode. By using this, a transistor with a reduced channel length was manufactured.
[0445] The structure of the fabricated transistor is shown in Figure 48. Figure 48(A) is a top view of the transistor. FIG. 48(B) corresponds to the dashed line G1-G2 and the dashed line G3-G4 in FIG. 48(A). 48 is a cross-sectional view of a transistor shown in FIG. Since the structure is similar to that of the transistor, the same reference numerals are used. 13(D), a semiconductor 406a and a semiconductor 406b are provided on the top and bottom of the semiconductor 406, respectively. A structure having a conductor 406c was used.
[0446] A silicon substrate measuring 126.6 mm square was used as the substrate 400. A silicon oxide layer having a thickness of 100 nm and a silicon oxynitride layer having a thickness of 300 nm are laminated. The semiconductor 406a was used with an atomic ratio of In:Ga:Zn=1:3:4. A 20 nm thick In-Ga-Zn film was deposited using an In-Ga-Zn oxide target. The semiconductor 406 was made of In:Ga:Zn=1:1:1 [atomic ratio] A 20 nm thick In-Ga film was deposited using an In-Ga-Zn oxide target. The semiconductor 406c was made of In:Ga:Zn=1:3:4 [primary A 5 nm thick In film was formed using an In-Ga-Zn oxide target with a molecular weight ratio of 1.0 to 1.0. The conductor 416a and the conductor 416b were made of n-Ga-Zn oxide. The insulator 412 is a silicon oxynitride layer having a thickness of 10 nm. The conductor 404 is made of tantalum nitride with a thickness of 30 nm and silicon nitride with a thickness of 13 nm. 5 nm tungsten was used.
[0447] For the transistor using tungsten etching condition A, the drain voltage V The Id-Vg characteristics were measured at 25 points for each of d being 0.1 V and 1.8 V. , Id is the drain current, and Vg is the gate voltage. 49(B) shows the Id-Vg characteristics of a transistor with a gate width of 500 nm and a channel width of 500 nm. is the Id-Vg characteristic of a transistor with a channel length of 180 nm and a channel width of 800 nm. It is.
[0448] For the transistor using tungsten etching condition B, the drain voltage V The Id-Vg characteristics were measured at 25 points for each of d being 0.1 V and 1.8 V. 0(A) is the Id- of a transistor with a channel length of 180 nm and a channel width of 500 nm. Vg characteristics. Figure 50(B) shows the results for a channel length of 180 nm and a channel width of 800 nm. This is the Id-Vg characteristics of a transistor.
[0449] As shown in FIG. 49 and FIG. 50, the transistors fabricated in this embodiment have small variations and are excellent. In particular, the transistor using tungsten etching condition A has the following electrical characteristics: The variation was small. In other words, the shape was uniform within the 126.6 mm square silicon substrate surface. It can be seen that the shape is as follows. [Explanation of symbols]
[0450] 110 layers 110a layer 110b layer 116 layers 116a layer 116b layer 120 Anti-reflection layer 122 Resist 124 Organic matter 200 Imaging device 201 Switch 202 Switch 203 Switch 210 Pixel section 211 pixels 212 subpixels 212B subpixel 212G subpixel 212R subpixel 220 Photoelectric conversion element 230 Pixel Circuit 231 Wiring 247 Wiring 248 Wiring 249 Wiring 250 Wiring 253 Wiring 254 Filter 254B Filter 254G Filter 254R Filter 255 Lens 256 light 257 Wiring 260 Peripheral Circuits 270 Peripheral Circuits 280 Peripheral Circuits 290 Peripheral Circuits 291 Light source 300 Silicon substrate 310 layers 320 layers 330 layers 340 layers 351 Transistor 352 Transistor 353 Transistor 360 Photodiode 361 Anode 363 Low resistance region 370 Plug 371 Wiring 372 Wiring 373 Wiring 380 Insulator 400 Substrates 401 Insulators 402 Insulator 404 Conductors 406 Semiconductors 406a Semiconductors 406c Semiconductors 410 Insulators 410a Insulator 410b Insulator 411 Insulators 412 Insulators 413 Conductors 414 Conductors 416 Conductors 416a Conductor 416b Conductor 450 Semiconductor Substrate 452 Insulator 454 Conductors 456 areas 460 areas 462 Insulator 464 Insulator 466 Insulators 468 Insulator 472a area 472b area 474a Conductors 474b Conductors 474c Electrical conductors 476a Conductors 476b Conductors 478a Conductors 478b Conductor 478c Conductor 480a Conductor 480b Conductor 480c conductor 490 Insulator 492 Insulators 494 Insulators 496a Conductors 496b Conductors 496c Conductors 496d Conductors 498a Conductors 498b Conductor 498c Electrical conductor 498d Conductor 500 boards 502 Insulator 503 Insulators 504 Conductors 506 Semiconductors 510 Insulators 510a Insulator 510b Insulator 512 Insulators 513 Conductors 516 Conductors 516a Conductor 516b Conductor 536 Semiconductors 540 Insulator 546 Conductors 700 Substrates 704a Conductor 704b Conductor 706 Semiconductors 710a Insulator 710b Insulator 712a Insulator 712b Insulator 714a Conductor 714b Conductor 716a Conductor 716b Conductor 718a Insulator 718b Insulator 718c Insulator 719 Light emitting element 720 Insulator 721 Insulators 731 Terminal 732 FPC 733a Wiring 734 Sealing material 735 Drive Circuit 736 Drive Circuit 737 pixels 741 Transistor 742 Capacitive element 743 Switching element 744 Signal Line 750 Board 751 Transistor 752 Capacitive element 753 Liquid crystal element 754 scan lines 755 Signal Line 781 Conductors 782 Light-emitting layer 783 Conductors 784 Bulkhead 791 Conductors 792 Insulators 793 Liquid crystal layer 794 Insulators 795 Spacer 796 Conductors 797 Circuit Board 901 Case 902 Case 903 Display section 904 Display section 905 Microphone 906 Speaker 907 Operation Key 908 Stylus 911 Case 912 Case 913 Display section 914 Display section 915 Connection 916 Operation Key 921 Case 922 Display section 923 Keyboard 924 Pointing Device 931 Case 932 Refrigerator door 933 Freezer door 941 Case 942 Case 943 Display section 944 Operation Key 945 Lens 946 Connection 951 Body 952 wheels 953 Dashboard 954 Light 1189 ROM Interface 1190 Board 1191 ALU 1192 ALU Controller 1193 Instruction Decoder 1194 Interrupt Controller 1195 Timing Controller 1196 Registers 1197 Register Controller 1198 Bus Interface 1199 ROM 1200 memory elements 1201 Circuit 1202 Circuit 1203 Switch 1204 Switch 1206 Logic elements 1207 Capacitive element 1208 Capacitive element 1209 Transistor 1210 Transistor 1213 Transistor 1214 Transistor 1220 Circuit 2100 Transistor 2200 Transistor 3001 Wiring 3002 Wiring 3003 Wiring 3004 Wiring 3005 Wiring 3200 Transistors 3300 Transistors 3400 Capacitive element 5100 pellets 5100a Pellet 5100b Pellets 5101 AEON 5102 Zinc oxide layer 5103 particles 5105a Pellet 5105a1 area 5105a2 Pellet 5105b Pellet 5105c Pellet 5105d Pellet 5105d1 area 5105e Pellet 5120 PCB 5130 Target 5161 area< / cpu>
Claims
[Claim 1] An oxide semiconductor layer on an insulating layer; a source electrode provided on and in contact with the oxide semiconductor layer; a drain electrode provided on and in contact with the oxide semiconductor layer; a first insulator provided on and in contact with the source electrode; a second insulator provided on and in contact with the drain electrode; a gate insulating layer provided on the first insulator and the second insulator; a gate electrode located on the oxide semiconductor layer via the gate insulating layer, the gate insulating layer and the gate electrode are located between the source electrode and the drain electrode and between the first insulator and the second insulator; the first insulator has a first region, a second region, a third region, and a fourth region; the first region is a flat region; the third region is a region having an inclination, the second region has a slope that is gentler than a slope of the third region, the second insulator has a fifth region, a sixth region, a seventh region, and an eighth region; the fifth region is a flat region, the seventh region is a region having an inclination, the sixth region has a slope that is gentler than a slope of the seventh region, a distance between an upper end of the second region and an upper end of the sixth region via the gate insulating layer and the gate electrode is greater than a distance between a lower end of the second region and a lower end of the sixth region via the gate insulating layer and the gate electrode; a lower end of the first insulator coincides with an upper end of the source electrode in the fourth region; In the eighth region, a lower end of the second insulator coincides with an upper end of the drain electrode; the insulating layer has a ninth region in contact with the oxide semiconductor layer on an upper surface thereof and a tenth region in contact with the source electrode or the drain electrode on an upper surface thereof; a thickness of the insulating layer in the ninth region is greater than a thickness of the insulating layer in the tenth region; A semiconductor device, wherein, in a plan view, the ninth region is a region between the third region and the seventh region.
Citation Information
Patent Citations
Compound having lamellar structure of hexagonal system expressed in ingazn2o5 and its production
JP1988239117A
Semiconductor equipment
JP1999505377A
Semiconductor device and manufacturing method for the same
JP2012248829A
Semiconductor device and manufacturing method of the same
JP2014003280A
Semiconductor device and semiconductor device manufacturing method
JP2014029994A