Broadband Visible Light Reflector

The broadband visible light reflector addresses inefficiencies in multilayer films by optimizing layer thickness and composition to enhance reflectance and reduce blue leakage, achieving high photopic weighted average reflectance with a thinner design.

JP7566107B2Active Publication Date: 2024-10-113M INNOVATIVE PROPERTIES CO
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023149672
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-12-18
Filing Date
2023-09-15
Publication Date
2024-10-11
Estimated Expiration
2036-12-12

AI Technical Summary

Technical Problem

Existing multilayer optical films struggle to achieve high reflectance across a broad spectrum while minimizing blue leakage and maintaining thin film thickness, leading to inefficiencies in display and lighting applications.

Method used

Designing a broadband visible light reflector with optical repeat units comprising a first birefringent polymer layer and a second polymer layer, where each unit has an optical thickness greater than or equal to 220 nm, and optimizing the layer profile to minimize thin layers that absorb blue light, thereby enhancing reflectance and reducing blue leakage.

Benefits of technology

The solution results in a reflector with improved photopic weighted average reflectance and reduced blue leakage, achieving high reflectance across the visible spectrum with a thinner film design, comparable to or better than conventional high-performance reflectors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566107000006
    Figure 0007566107000006
  • Figure 0007566107000007
    Figure 0007566107000007
  • Figure 0007566107000008
    Figure 0007566107000008
Patent Text Reader

Abstract

To provide a broadband visible reflector that can be used for a backlight and a display.SOLUTION: A broadband visible reflector includes a plurality of optical repeat units, each including a first birefringent polymer layer and a second polymer layer and each having an f ratio of 50%. The broadband visible reflector transmits 10% or more of unpolarized light at normal incidence between 380 nm and 430 nm. The plurality of optical repeat units are arranged in a single packet so that the broadband visible reflector becomes a single packet reflector. The broadband visible reflector provides, over a visible spectrum, at least 95% photopically-weighted average Rhemi(λ) determined by using the CIE 1931 photopic response function.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Background technology]

[0001] Polymeric multilayer optical films are formed by coextrusion of tens to hundreds of molten polymer layers followed by orienting or stretching the resulting film. These microlayers have different refractive index characteristics and are thin enough that light is reflected at the interfaces between adjacent microlayers. Broadband visible light reflectors reflect all or substantially all of the visible spectrum and can be useful for display and lighting applications. Summary of the Invention

[0002] In one aspect, the present disclosure relates to a broadband visible light reflector. In particular, the broadband visible light reflector includes a plurality of optical repeat units, each optical repeat unit including a first birefringent polymer layer and a second polymer layer. Each optical repeat unit has an optical thickness, and the optical thickness of every optical repeat unit is 220 nm or more.

[0003] In another aspect, the present specification relates to a broadband visible light reflector. The broadband visible light reflector includes a plurality of optical repeat units, each of which includes a first birefringent polymer layer and a second polymer layer. The broadband visible light reflector transmits 30% or more of normally incident unpolarized light between 380 nm and 430 nm.

[0004] In yet another aspect, the present disclosure relates to a broadband visible light reflector that appears yellow in reflection and has a photopic weighted average R of at least 95% as determined using the CIE 1931 photopic response function. hemi (λ) across the visible spectrum. [Brief description of the drawings]

[0005] [Figure 1] FIG. 2 is a schematic perspective view of a reflective film. [Diagram 2] 1 is a graph showing measured versus calculated hemispherical reflectance for a multilayer polymeric reflective film. [Diagram 3] 1 is a graph showing a layer profile of a multilayer film in Comparative Example C1. [Figure 4] 1 is a graph showing the on-axis transmittance of a multilayer film in Comparative Example C1. [Diagram 5] 2 is a graph showing a layer profile of a multilayer film in Example 1. [Figure 6] 1 is a graph showing the on-axis transmittance of a multilayer film in Example 1. [Figure 7] 1 is a graph showing the relationship between photopic weighted hemispherical reflectance and layer thickness, normalized to Comparative Example C1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0006] Multilayer optical films, i.e. films that provide desired transmission and / or reflection properties at least in part through an arrangement of microlayers of different refractive index, are known. It is known to make such multilayer optical films by depositing a series of inorganic materials as optically thin layers ("microlayers") onto a substrate in a vacuum chamber. Inorganic multilayer optical films are described, for example, in texts by HA Macleod, Thin-Film Optical Filters, 2nd Edition, Macmillan Publishing Co. (1986) and A. Thelan, Design of Optical Interference Filters, McGraw-Hill Inc. (1989).

[0007] Multilayer optical films have also been demonstrated by coextrusion of alternating polymer layers. See, for example, U.S. Pat. Nos. 3,610,729 (Rogers), 4,446,305 (Rogers et al.), 4,540,623 (Im et al.), 5,448,404 (Schrenk et al.), and 5,882,774 (Jonza et al.). In these polymeric multilayer optical films, the individual layers are mostly or exclusively made of polymeric materials. These are sometimes called thermoplastic multilayer optical films. Such films are compatible with mass production processes and can be made in large sheets and roll goods. The following description and examples relate to thermoplastic multilayer optical films.

[0008] Multilayer optical films include individual microlayers with different refractive index characteristics, such that some light is reflected at the interfaces between adjacent microlayers. The microlayers are thin enough that the light reflected at the interfaces undergoes constructive or destructive interference to give the multilayer optical film the desired reflective or transmissive properties. In multilayer optical films designed to reflect ultraviolet, visible, or near infrared wavelengths of light, each microlayer typically has an optical thickness (physical thickness multiplied by refractive index) of less than about 1 μm. In general, the layers may be arranged from thinnest to thickest. In some embodiments, the alternating optical layers may vary substantially linearly as a function of the number of layers. These layer profiles may be referred to as linear layer profiles. Thicker layers may also be included, such as skin layers on the outer surfaces of the multilayer optical film, or protective boundary layers (PBLs) arranged within the multilayer optical film and separating coherent groups (referred to herein as "packets") of microlayers. In some cases, the protective boundary layers may be the same material as at least one of the alternating layers of the multilayer optical film. In other cases, the protective boundary layers may be different materials selected for their physical or rheological properties. The protective boundary layers may be on one or both sides of the optical packet. In the case of a single packet multilayer optical film, the protective boundary layers may be on one or both of the outer surfaces of the multilayer optical film.

[0009] For purposes herein, a packet generally varies monotonically in thickness of the optical repeat unit. For example, a packet may be monotonically increasing, monotonically decreasing, both increasing and unchanged, or both decreasing and unchanged, but not both increasing and decreasing. It should be understood that one or several layers that do not follow this pattern are not important to the overall definition or identification of a particular group of optical repeat layers as a packet. In some embodiments, it may be useful to define a packet as the largest individual group of consecutive non-redundant layer pairs that collectively provide a reflectance over a particular subrange of the spectrum of interest (e.g., the visible spectrum).

[0010] In some cases, the microlayers have thicknesses and refractive index values ​​that result in a quarter-wave stack (i.e., arranged as optical repeat units or unit cells each having two adjacent microlayers of equal optical thickness (f ratio = 50%), such optical repeat units being effective for constructive interference light reflections with wavelength λ approximately twice the total optical thickness of the optical repeat unit). Other layer arrangements are also known, such as multilayer optical films having two microlayer optical repeat units with f ratios different from 50%, or films in which the optical repeat unit contains three or more microlayers. The design of these optical repeat units can be configured to reduce or increase certain high order reflections. See, for example, U.S. Pat. Nos. 5,360,659 (Arends et al.) and 5,103,337 (Schrenk et al.). A thickness gradient of the optical repeat unit along the thickness axis (e.g., z-axis) of the film can be used to provide an extended reflection band, such as a reflection band that extends across the entire human visible range and into the near infrared, so that the finely layered stack continues to reflect across the entire visible spectrum, even as the band shifts toward shorter wavelengths at oblique angles of incidence. Tailored thickness gradients to sharpen the band edges, i.e., the wavelength transition between high reflection and high transmission, are described in U.S. Patent No. 6,157,490 (Wheatley et al.).

[0011] In many applications, the reflective properties of a film are measured using the "hemispherical reflectance" (R hemi Hemispherical reflectance is characterized by the reflectance ratio (λ), which means the total reflectance of a component (whether a surface, film, or group of films) when light (of a particular wavelength or range of wavelengths of interest) is incident on the component (whether it is a surface, film, or group of films) from all possible directions. Thus, the component is illuminated with incident light (and all polarization states, unless otherwise specified) from all directions within a hemisphere centered on the normal, and all light reflected within the same hemisphere is collected. The ratio of the total luminous flux of reflected light to the total luminous flux of incident light in the wavelength range of interest is called the hemispherical reflectance, R hemi (λ). Because light is likely to be incident on the interior surfaces of the cavity (whether it is a front, back, or side reflector) at all angles, a backlight recycling cavity will use a reflector with its R hemi Moreover, unlike the reflectance for normally incident light, R hemi (λ) is insensitive to and takes into account variability in reflectance with angle of incidence, which can be quite significant for some components (e.g., prismatic films) in a recycled backlight.

[0012] It is understood that in many electronic display applications that use backlighting, and in backlights for general and special lighting applications, it may be desirable for the reflector film that forms the rear surface of the backlight to have highly reflective properties. Indeed, the hemispherical reflectance spectrum R hemi (λ) shows a strong correlation with the light output efficiency of the backlight and R hemi It is further understood that the higher the value of (λ), the higher the output efficiency of the backlight. This is especially true for recycled backlights where other optical films may be configured to cover the backlight exit aperture to output collimated or polarized light from the backlight.

[0013] Further details of multilayer optical films and related designs and structures are described in U.S. Patents 5,882,774 (Jonza et al.) and 6,531,230 (Weber et al.), PCT / WO95 / 17303 (Ouderkirk et al.) and 99 / 39224 (Ouderkirk et al.), and the publication entitled "Giant Birefringent Optics in Multilayer Polymer Mirrors," Science, Vol. 287, March 2000 (Weber et al.). Multilayer optical films and related articles may include additional layers and coatings selected for their optical, mechanical, and / or chemical properties. For example, a UV-absorbing layer may be added to the incident side of the film to protect components from degradation caused by UV light. A UV-curable acrylate adhesive or other suitable material may be used to attach the multilayer optical film to the mechanically reinforced layer. Such reinforcing layers may include polymers such as PET or polycarbonate, and may also include structured surfaces that provide optical functions such as light diffusion or collimation, for example, by using beads or prisms. Additional layers and coatings may also include scratch-resistant layers, tear-resistant layers, and hardeners. See, for example, U.S. Patent No. 6,368,699 (Gilbert et al.). Methods and apparatus for making multilayer optical films are described in U.S. Patent No. 6,783,349 (Neavin et al.).

[0014] The reflective and transmissive properties of a multilayer optical film are a function of the refractive index of each microlayer and the thickness and thickness distribution of the microlayers. Each microlayer has an in-plane refractive index n x , n y and the refractive index associated with the thickness axis of the film, n zThese indices represent the refractive index of the subject material for light polarized along mutually orthogonal x-, y-, and z-axes, respectively. For ease of description in this patent application, unless otherwise specified, the x-, y-, and z-axes are axes of a local Cartesian coordinate system applicable to any point of interest on the multilayer optical film, with the microlayers extending parallel to the xy plane, the x-axis being Δn x It is assumed that the molecules are oriented in the plane of the film so as to maximize the magnitude of Δn y The magnitude of is Δn x Furthermore, the difference Δn x , Δn y , Δn z The choice of which material layer to start with when calculating Δn x In other words, the difference in refractive index between the two layers forming the interface is Δn j =n 1j -n 2j where j=x, y, or z, and the layer designations 1, 2 are n 1x ≧n 2x , i.e., Δn x It is chosen to be ≧0.

[0015] In practice, the refractive index is controlled by appropriate material selection and processing conditions. Multilayer films are made by co-extruding many layers, e.g., tens or hundreds of layers, of two alternating polymers A and B, optionally followed by passing the multilayer extrudate through one or more layer increments, casting through a film die, and then stretching or otherwise orienting the extrudate to form the final film. The resulting film is typically composed of hundreds of individual microlayers whose thicknesses and refractive indices are tailored to provide one or more reflection bands in the desired region of the spectrum, such as the visible or near infrared. To obtain high reflectance with a reasonable number of layers, adjacent microlayers typically have a refractive index difference (Δn xIn some embodiments, the materials are selected so that the refractive index difference for light polarized along the x-axis is as high as possible after orientation. If high reflectivity is desired for two orthogonal polarizations, adjacent microlayers exhibit a refractive index difference (Δn y ) can also be displayed.

[0016] The above-referenced '774 (Jonza et al.) patent, among other things, describes the refractive index difference (Δn z ) to obtain the desired reflectance characteristics for the p-polarized component of obliquely incident light. To maintain high reflectance for p-polarized light at oblique incidence angles, the z-index mismatch Δn between the fine layers is z is the largest in-plane refractive index difference Δn x By controlling the Δn z ≦0.5×Δn x or Δn z ≦0.25×Δn x A zero or near-zero magnitude z-index mismatch results in interfaces between the fine layers whose reflectivity for p-polarized light is constant or nearly constant as a function of the angle of incidence. Furthermore, the z-index mismatch Δn z is the in-plane refractive index difference Δn x , i.e., Δn z <0. This condition results in an interface whose reflectivity for p-polarized light increases with increasing angle of incidence, just as it does for s-polarized light.

[0017] Another design consideration described in '774 (Jonza et al.) concerns surface reflections at the air interfaces of the multilayer reflective polarizer. Unless the polarizer is double-laminated with a clear optical adhesive to an existing piece of glass or another existing film, such surface reflections will reduce the transmission of the desired polarization through the optical system. Therefore, in some cases it may be useful to add an anti-reflection (AR) coating to the reflective polarizer.

[0018] The polymeric multilayer optical films described herein can be highly reflective, for example, reflecting more than 95% or 99%, or even 99.5% of visible light when measured at normal incidence. Visible light can be characterized as having a wavelength between 400 nm and 700 nm, or in some cases between 420 nm and 700 nm. Additionally, the polymeric multilayer optical films described herein can be thin, in some cases thinner than 100 μm, 85 μm, or 65 μm. In embodiments where the polymeric multilayer optical film includes a third optical packet, the film can be thinner than 165 μm.

[0019] Skin layers may be added. This is often done after construction of the layers and before the melt exits the film die. The multilayer melt is then cast through a film die onto a chill roll in the conventional manner for polyester films and then quenched. The cast web is then stretched in various ways to obtain birefringence in at least one of the optical layers, often producing either a reflective polarizer or a mirror film, as described, for example, in U.S. Patent Publication No. 2007 / 047080 (A1), U.S. Patent Publication No. 2011 / 0102891 (A1), and U.S. Patent No. 7,104,776 (Merrill et al.).

[0020] Broadband visible reflectors are designed to provide a broad range of the visible spectrum and reflect both on-axis and angled light. For example, a broadband visible reflector may have a photopic weighted average R of at least 95% as determined using the CIE 1931 photopic response function. hemi(λ) across the visible spectrum. This means designing the layer profile to allow for a pair of layers with optical thicknesses of 200 nm or even less to reflect blue light on-axis. These thin layers were thought to be necessary to provide a uniform appearance and high performance of the reflector (i.e. to ensure that it remains a broadband reflector). However, for typical birefringent materials used in broadband visible light reflectors, these thin layers have the greatest absorption. Furthermore, at certain angles from the film, these thinnest layers either reflect only ultraviolet (non-visible) light or are transparent to the incident light and do not contribute any reflection to the system. Surprisingly, the benefits of eliminating or minimizing the bluest layers (by using fewer layers or by providing a sharper gradient in the layer profile) outweigh any disadvantages that would result from the transmission of some of the blue light on-axis. Layers of intermediate thickness, such as green reflecting layers, shift their reflection wavelengths at certain angles to cover the blue wavelengths. Therefore, when photopic weighting the visible wavelengths, R hemi An increase in (λ) is observed. This is particularly surprising since, upon inspection, such films will have a property described as blue leak. Blue leak refers to the transmission of blue light through the film. In transmission, the reflector will appear blue. In reflection, such films will appear yellow. Despite this appearance drawback, the examples provided herein show that such films can provide excellent reflective performance in displays, with on-axis reflectance being less important compared to angular reflection. This improvement in performance is due to the photopic averaged R across the visible spectrum. hemi(λ). In some embodiments, the optical thickness of any optical repeat unit is 220 nm or more (corresponding to a wavelength of approximately 440 nm on the reflected axis). In some embodiments, the optical thickness of any optical repeat unit is 225 nm or more. In some embodiments, the broadband visible light reflector transmits 20% or more of normally incident unpolarized light between 380 nm and 430 nm. In some embodiments, the broadband visible light reflector transmits 20% or more of normally incident unpolarized light between 380 nm and 450 nm. In some embodiments, the broadband visible light reflector transmits 30, 40, or 50% or more of normally incident unpolarized light between 380 nm and 410 nm. These technical design conditions, i.e., minimizing or eliminating the bluest layer, can also result in performance comparable to or better than other high performance multilayer reflectors, while reducing the required overall thickness of the broadband visible light reflector. EXAMPLES

[0021] R hemi Measurement and calculation of (λ) R hemi (λ) was measured using the apparatus described in U.S. Patent Application Publication No. 2013 / 0215512 (Coggio et al.). A commercially available 6-inch integrating sphere with Spectralon® reflective coating and three mutually orthogonal ports manufactured by Labsphere, Inc. (North Sutton, NH) was used to illuminate the sample and obtain a hemispherical reflectance spectrum R hemi(λ) was determined. A stabilized light source illuminated the sphere through one port. A Photo Research® PR650 spectrophotometer (available from Photo Research Inc., Chatsworth, Calif.) was used to measure the radiance of the sphere's inner wall through the second port. The sample was placed on the third port. A known reflectance standard (Spectralon® Reference Target SRT-99-050 available from Labsphere, Inc., North Sutton, New Hampshire) placed on the third port was used to calibrate the radiance of the integrating sphere's walls, and the radiance of the sphere's walls was measured with and without the calibration standard. R hemi (λ) was measured by placing a sample on the third port. That is, the hemispherical reflectance R hemi (λ) was obtained by taking the ratio of the radiance of the sphere wall with and without the sample and using a simple integrating sphere luminous intensity gain algorithm.

[0022] The equilibrium luminous intensity distribution inside the integrating sphere is expected to approximate a Lambertian distribution, which means that the probability distribution of luminous intensity versus the angle of incidence on the sample falls off as cos(θ), where θ=0 is normal to the sample.

[0023] FIG. 1 is a schematic perspective view of a reflective film. FIG. 1 shows a light ray 130 incident on a reflective film 110 at an incidence angle θ, thereby forming a plane of incidence 132. The reflective film 110 includes a first reflective axis 116 parallel to the x-axis and a second reflective axis 114 parallel to the y-axis. The plane of incidence 132 of the light ray 130 is parallel to the first reflective axis 116. The light ray 130 has a p-polarized component that is in the plane of incidence 132 and an s-polarized component that is orthogonal to the plane of incidence 132. The p-polarized light of the light ray 130 has a reflectance R pp-x (the projection of the electric field of p-polarized light ray 130 onto the plane of the reflective film 110 is parallel to the x-direction), whereas s-polarized light ray 130 is reflected by the reflective film with a reflectance R ss-y (the electric field of the s-polarized light of ray 130 is parallel to the y-direction).

[0024] 1 further shows a light ray 120 incident on the reflective film in a plane of incidence 122 that is parallel to the second reflective axis 114 of the film 110. The light ray 120 has a p-polarized component that is in the plane of incidence 122 and an s-polarized component that is orthogonal to the plane of incidence 122. The p-polarized light of the light ray 120 has a reflectance R pp-y while s-polarized light 120 is reflected by the reflective film with a reflectance R ss-x As described further herein, the amount of transmission and reflection of p-polarized and s-polarized light for a given plane of incidence depends on the properties of the reflective film.

[0025] R hemi (λ) can be calculated from knowledge of the layer thickness profiles of the microlayers and other layer elements of the optical film, and from the refractive index values ​​associated with each of the microlayers and other layers in the film. Using a software application for solving a 4×4 matrix for the optical response of a multilayer film, both the reflection and transmission spectra can be calculated from the known layer thickness profiles and refractive index properties for the x-axis and y-axis planes of incidence, and for both p-polarized and s-polarized incident light. From this, R hemi (λ) can be calculated using the formula shown below:

number

number

number

number

[0026] A multilayer polymeric reflective film was obtained that was configured with an array of higher harmonic visible reflection bands, generally as described in U.S. Pat. No. 6,531,230 (Weber et al.). hemi (λ) was measured using a Labsphere integrating sphere as described above, and the resulting spectrum 208 is shown in Figure 2. The transmission spectrum of this multilayer polymeric reflective film was measured using a PerkinElmer L1050 spectrophotometer (PerkinElmer Inc., Waltham, PA) and calculated using the equation (and the measured spectral input) shown above. hemi In this calculation, all further R hemi For the calculation of (λ), E(θ) is taken as a Lambertian luminous intensity distribution depending on cos(θ). Figure 2 shows the calculated R hemi (λ) spectrum 204 is the measured R hemi (λ) spectrum 208, demonstrating that the computational technique captures the physics relevant to the reflection from broadband visible light reflectors, including the effect of absorption losses on the detailed reflectance spectrum.

[0027] Comparative Example C1 A single packet reflector with PEN and PMMA optical repeat units was modeled using the layer profile shown in FIG. 3. The layer profile is the total physical thickness of each optical repeat unit versus the number of optical repeat units. This layer profile represents a conventional wide range across both the on-axis and angular visible range. The modeled film had a total thickness of 62.1 micrometers.

[0028] The reflectance spectra of the films were calculated using a software application for solving 4 × 4 matrices for the optical response of multilayer films. The real part of the wavelength-dependent refractive index (n x ,n y ,n z ) and the imaginary part (k x ,k y ,kz ) are shown in Table 1. In this calculation, the refractive index values ​​were taken to vary smoothly between and beyond the values ​​in Table 1. [Table 1]

[0029] The normal angle reflectance and transmission spectra were calculated for light incident on the thinner optical repeat unit side. The transmission spectrum for normally incident unpolarized light is shown in Figure 4. The hemispherical reflectance of the film was also calculated. The photopic weighted average R was determined using the CIE 1931 photopic response function. hemi (λ) is calculated to be 99.55%, with a loss of 0.45% (100%-R hemi ) became.

[0030] Example 1 A single packet reflector was designed and modeled using the values ​​in Table 1 for Comparative Example C1, except that all optical repeat units were made 10% thicker. A layer profile showing the total physical thickness of the optical repeat units versus the number of optical repeat units is shown in Figure 5. The modeled film had a total thickness of 67.8 micrometers.

[0031] The normal angle reflectance and transmission spectra were calculated for light incident on the thinner optical repeat unit side. The transmission spectrum for normally incident unpolarized light is shown in Figure 6. The hemispherical reflectance of the film was also calculated. The photopic weighted average R was determined using the CIE 1931 photopic response function. hemi (λ) was calculated to be 99.61%, with a loss of 0.39% (100%-R hemi ) became.

[0032] Additional films were designed and modeled in the same manner as Example 1, except with different adjustments to the thickness of the optical repeat unit. The photopic weighted average R determined using the CIE 1931 photopic response function hemi(λ) was calculated for each film. FIG. 7 shows the photopic averaged hemispherical reflectance normalized to the baseline layer profile of Comparative Example 1, and the R at 100% thickness (99.55% of Comparative Example C1). hemi ), 105% thickness (99.59% R hemi ), 110% thickness (99.61% R of Example 1 hemi ), 115% thickness (99.59% R hemi ), and 120% thickness (99.48% R hemi ) became.

[0033] Below are exemplary embodiments according to the present disclosure.

[0034] Item 1 includes a plurality of optical repeat units, each having a first birefringent polymer layer and a second polymer layer; each of the optical repeat units has an optical thickness; The optical thickness of all optical repeat units is 220 nm or more; Broadband visible light reflector.

[0035] Item 2 includes a plurality of optical repeat units, each having a first birefringent polymer layer and a second polymer layer; The broadband visible light reflector transmits 10% or more of normally incident unpolarized light having a wavelength of 380 nm to 430 nm. Broadband visible light reflector.

[0036] Item 3. The broadband visible reflector according to item 2, which transmits 20% or more of normally incident unpolarized light of 380 nm to 430 nm.

[0037] Item 4. The broadband visible light reflector according to Item 2, which transmits 30% or more of normally incident unpolarized light of 380 nm to 430 nm.

[0038] Item 5. A method for fabricating a multilayer optical device comprising: said broadband visible light reflector appears yellow in reflection; The broadband visible light reflector has a photopic weighted average R of at least 95% as determined using the CIE 1931 photopic response function. hemi (λ) across the visible spectrum, Broadband visible light reflector.

[0039] Item 6. The broadband visible light reflector of item 5, which appears blue in transmission.

[0040] Item 7. Providing a broadband visible light reflector according to any one of items 1, 2, or 5; Incorporating a broadband visible light reflector into the backlight A method comprising:

[0041] Item 8. A backlight comprising the broadband visible reflector of any one of items 1, 2, or 5.

[0042] Item 9. A display comprising the broadband visible light reflector of any one of items 1, 2, or 5.

[0043] Item 10. The broadband visible light reflector of any one of items 1, 2, or 5, wherein the plurality of optical repeating units are disposed in a first packet and a second packet.

[0044] Item 11. The broadband visible light reflector of any one of items 1, 2, or 5, wherein the plurality of optical repeating units are disposed in a first packet, a second packet, and a third packet.

[0045] Item 12. The broadband visible light reflector of any one of items 1, 2, or 5, wherein a plurality of optical repeat units are arranged in a single packet.

Claims

1. 1. A broadband visible light reflector comprising: a plurality of optical repeat units each having a first birefringent polymer layer and a second polymer layer, each having an f-ratio of 50%; the broadband visible light reflector transmits at least 10% of normally incident unpolarized light having a wavelength between 380 nm and 430 nm; the plurality of optical repeat units are arranged in a single packet such that the broadband visible light reflector is a single packet reflector; The broadband visible light reflector has a photopic weighted average R of at least 95%, as determined using the CIE 1931 photopic response function. hemi (λ) across the visible spectrum, Broadband visible light reflector.

2. The optical repeat unit according to claim 1, wherein each of the optical repeat units has an optical thickness, 10. The broadband visible light reflector of claim 1, wherein the optical thickness of all optical repeat units is 220 nm or greater.

3. A broadband visible light reflector as described in claim 1, wherein the broadband visible light reflector appears yellow in reflection and blue in transmission.

Citation Information

Patent Citations

  • Multilayer laminate with harmonic generation for broad visible light / infrared coverage

    JP2016520861A

  • Multilayer stack combinations with interleaved overlapping harmonics for wide visible-infrared coverage

    US20130250405A1

  • Polymeric multilayer optical film

    WO2015048624A1