Tubular structure for cooling and agglomeration of ultrafine powder particles and method for forming ultrafine powder particles
The tubular structure and method for agglomeration cooling of ultrafine powder particles address the issue of uneven particle sizes by stabilizing and controlling the formation process, resulting in uniform and well-dispersed ultrafine powder particles.
Patent Information
- Application Number
- JP2023507584
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-01-25
- Filing Date
- 2021-08-27
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-08-27
AI Technical Summary
Conventional methods for preparing ultrafine powder particles using evaporation condensation vapor phase molding result in uneven particle sizes and distributions, leading to the generation of ultrasmall and ultralarge particles, which affect the subsequent use of the powder.
A tubular structure for agglomeration cooling of ultrafine powder particles, incorporating an exhaust and reflux structure, waste collection structure, and particle shaping control structure, along with a method that includes a heating system, carrier gas, and precise temperature and velocity control, to stabilize and control the particle formation process.
The method achieves uniform particle size and stable morphology, ensuring good dispersion of ultrafine powder particles by precisely controlling the formation process through temperature and velocity field management.
Smart Images

Figure 0007566375000001
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of ultrafine powder particle preparation technology, and particularly to a tubular structure for agglomeration and cooling of ultrafine powder particles and a method for forming ultrafine powder particles. [Background technology]
[0002] When using the evaporation condensation gas-phase molding and cooling technology to prepare ultrafine powder particles, the material to be prepared is first heated and vaporized at high temperature, and then hardened and molded through the gaseous state to liquid state, so the ultrafine powder particles to be prepared are fine materials, mainly nanometer, submicron or micron powders, the molded particle size is small, the molding speed is very fast, and the temperature is very high, and the technical principle is simple, but it is very difficult to put into practical use. It is even more difficult to produce uniform, stable and well-dispersed powder particles that can be used in large quantities.
[0003] Common methods include a flare structure that slows down the steam flow and then controls particle formation, or a blowing cooling structure that rapidly cools the steam. However, either method results in uneven temperatures between the inner and outer layers of the airflow, or uneven internal flow patterns due to blowing onto the inner layer, resulting in the generation of a large number of extremely small or oversized particles, which affects the subsequent use of the powder. Summary of the Invention [Problem to be solved by the invention]
[0004] The object of the present invention is to provide a tubular structure for agglomeration and cooling of ultrafine powder particles and a method for molding ultrafine powder particles, which solves the problem that a large amount of ultrafine particles and ultra-large particles are generated in the conventional technology, which affects the subsequent use. [Means for solving the problem]
[0005] A tubular structure for cooling and agglomerating ultrafine powder particles in an ultrafine powder particle preparation system, comprising an exhaust and return structure, a waste return structure or waste collection structure, and a particle formation control structure, which are connected in series; The front end of the exhaust and return structure is connected to a front high-temperature evaporator, and the rear end of the particle shaping control structure is connected to a rear collection or cooling structure; The ultrafine powder particle preparation system further includes a heating system installed in the high-temperature evaporator to provide a heat source, a raw material supply system to supply raw material to the high-temperature evaporator, a circulating cooling system to perform cooling, a gas source or circulating gas system to supply carrier gas and cooling gas, a pressure balance system to perform pressure balance control, a first jet cooling structure, and a curved pipe variable direction delivery structure.
[0006] Optionally, the front end of the exhaust and return structure is connected to the exhaust port of the high temperature evaporator; The exhaust and return structure includes at least a first flow path for receiving high-temperature steam, and a heat retaining or heating device is provided outside the first flow path.
[0007] Optionally, the waste return structure or waste collection structure includes at least a second flow path inside, the front end of the second flow path is connected to the first flow path, the rear end of the second flow path is connected to the inner cavity of the particle forming control structure, and a heat retention or heating device is provided outside the second flow path.
[0008] Optionally, the lumen front end of the particle forming control structure is connected to a second flow path, the lumen rear end of the particle forming control structure is connected to a collection or cooling structure, and an ultrafine powder particle forming region is provided inside the particle forming control structure; A heat-retaining, heating or cooling structure is provided inside the particle forming control structure, and the temperature of the ultrafine powder particle forming region is indirectly controlled by heat conduction or heat radiation; The velocity of the carrier gas and the cross-sectional dimensions of the ultrafine powder particle forming region control the rate at which the particles move with the carrier gas through the ultrafine powder particle forming region.
[0009] Optionally, the rear end of the particle formation control structure further includes the first jet cooling structure and the curved tube variable direction delivery structure; The first jet cooling structure includes at least a third flow passage therein, the front end of the third flow passage is connected to the ultrafine powder particle molding area, and the rear end of the third flow passage is connected to the curved pipe variable direction delivery structure; A porous inner plate is provided outside the third flow passage, and a cooling gas is uniformly blown into the third flow passage from the periphery.
[0010] Optionally, the bent variable direction delivery structure includes a variable direction chamber; An intake duct and an exhaust duct are connected to the variable direction chamber, the intake duct is connected to a third flow path and the exhaust duct is connected to the collection or cooling structure; The angle between the axis of the intake duct and the axis of the exhaust duct is 30° to 150°.
[0011] Optionally, the cooling structure connected to the exhaust duct is a second jet cooling structure; the second jet cooling structure includes at least an inner fourth flow passage; A front end of the fourth flow passage is connected to an exhaust duct of the curved pipe variable direction delivery structure, and a rear end of the fourth flow passage is connected to a collection cooling structure; The fourth flow path is provided with 1 to 12 jet holes of 5 to 50 mm for jet cooling to a central region of the fourth flow path, Alternatively, a porous jet tube is provided on the axis of the fourth flow passage.
[0012] A method for forming ultrafine powder particles using a tubular structure for cooling and agglomerating ultrafine powder particles, comprising: Step S1: put the material for preparing ultrafine powder particles into a high-temperature evaporator, mix the heated and evaporated material vapor and carrier gas into a mixed gas, and then feed the mixed gas into the exhaust and reflux structure through the exhaust port of the high-temperature evaporator, and control the internal temperature of the exhaust and reflux structure to be higher than the melting point of the required preparation material by keeping warm or heating; After passing through the exhaust and return structure and the waste return structure or waste collection structure, the mixed gas enters the particle forming control structure, and passes through a heat retention structure, a heating structure or a cooling structure in the ultrafine powder particle forming region of the particle forming control structure, and indirectly controls the temperature of each part of the ultrafine powder particle forming region by heat conduction or heat radiation, and controls the speed at which the particles pass through each internal region with the carrier gas according to the speed of the carrier gas and the cross-sectional dimensions of the duct, thereby providing a stable and controllable condition for forming the particles, and changing the preparation material from a gas state to a liquid state. and (S2) changing the liquid state to a solid state, the gaseous state contacting each other and condensing to become small droplets, the small droplets contacting each other and becoming large droplets, or the gaseous state and the small droplets contacting each other to become large droplets, the large droplets continue to contact each other and grow or solidify to become solid particles, the small droplets and the solid particles combine to become large solid particles or form a nucleus shell structure, the gaseous state combines with the solid particles to become large solid particles or form a nucleus shell structure, and the solid particles are continuously cooled to prepare particles with a desired particle size and shape. Step S3: the particles having the desired particle size and shape prepared in step S2 enter the first jet cooling structure with the carrier gas, and the cooling gas is uniformly blown into the internal flow path from the periphery by the porous inner layer plate, and mixed with the high-temperature gas and the formed particles to cool them; Step S4: the cooled particles are carried by the carrier gas into the curved tube variable direction delivery structure, and defective particles and good particles are separated from each other, and the good particles are carried by the carrier gas to the next process, and the defective particles are collected in the waste return structure or waste collection structure; The non-defective particles enter the collecting structure along with the carrier gas, and the formed ultrafine particles are separated from the carrier gas, among which the ultrafine particles are collected as products, and the carrier gas is discharged or recycled.
[0013] Optionally, step S4 includes: The method further includes a step S41 in which non-defective particles enter the second jet cooling structure along with the carrier gas, and are jet-cooled toward the central region of the flow path inside the second jet cooling structure via a cooling gas outlet provided inside the second jet cooling structure or a jet pipe provided on the axial line of the second jet cooling structure. Effect of the Invention
[0014] The present disclosure precisely controls each stage of the ultrafine powder particle molding process through specific structures, such as temperature field control, velocity field control, and control of the connection between structures, and utilizes its internal circulation to ensure that steam passes through the controlled parts uniformly, providing stable and controllable conditions for ultrafine powder particle molding, resulting in uniform particle size, stable morphology, and good dispersion of the molded particles. [Brief description of the drawings]
[0015] [Figure 1] FIG. 2 is a structural diagram of a tubular structure for cooling the aggregation of ultrafine powder particles according to the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] The present invention will be described in detail below with reference to examples. The following examples are merely illustrative and can only be used to interpret and explain the present invention, and cannot be interpreted as limitations of the present invention. In the description of the present invention, the terms "center", "upper", "lower", "left", "right", "front", "rear", "vertical", "horizontal", "inner", "outer", and other designated orientations or positional relationships are based on the orientations or positional relationships shown in the drawings, and are merely used to facilitate and simplify the description of the present invention, while not indicating or implying that a specified device or element must have a specific orientation, be configured in a specific orientation, and be operated in a specific orientation, and therefore cannot be understood as limitations on the present invention. In addition, the terms "first", "second", and "third" are used for explanatory purposes only, and cannot be understood as indicating or implying relative importance. In the description of the present invention, unless otherwise clearly specified and limited, the terms "attached", "connected" and "coupled" should be understood in a broad sense, for example, they may be fixedly connected, detachably connected, or integrally connected, mechanically connected, electrically connected, directly connected, indirectly connected via an intermediate medium, or connected inside two elements. Those skilled in the art can understand the specific meaning of the above terms in the present invention according to the circumstances.
[0017] The present structure is used for preparing ultrafine powder particles, including preparing ultrafine metal powder particles. In the following examples, the preparation of ultrafine metal powder particles is taken as an example for explanation, but the present structure is not limited to being used only for preparing ultrafine metal powder particles.
[0018] The particle condensation cooling tubular structure and particle forming method are used when preparing nano-scale, submicron-scale, and micron-scale fine particle powders by evaporation condensation gas phase method. The particle condensation cooling tubular structure is a flow path with interfaces designed to connect various parts, and precisely controls various stages of the particle forming process, such as temperature field control, velocity field control, and control of the connection between various structures, and utilizes the internal flow of steam through the control parts to provide stable and controlled conditions for particle forming, and to prepare conditions for forming fine particles. The material to be prepared goes from gas state to liquid state, liquid state to solid state, the gas state collides and condenses into smaller droplets, the small droplets collide and become larger droplets, or the gas state collides with the small droplets and becomes larger droplets, the large droplets continue to collide and grow or solidify into solid particles, the small droplets combine with the solid particles to become large solid particles or nucleus shell structures, the gas state combines with the solid particles to become large solid particles or nucleus shell structures, and the solid particles continue to be cooled, thereby making particles of the desired size and shape. The formed particles are uniform in size, stable in shape and well dispersed.
[0019] As shown in FIG. 1, the tubular structure for cooling and agglomerating ultrafine powder particles provided in the present disclosure is installed in an ultrafine powder particle preparation system. The ultrafine powder particle preparation system of the present disclosure includes a heating system installed in a high-temperature evaporator to provide a heat source, a raw material supply system to supply raw material to the high-temperature evaporator, a circulating cooling system to perform cooling, a gas source or circulating gas system to supply carrier gas and cooling gas, and a pressure balance system to perform pressure balance control. All of these components mentioned above are conventional technologies, and their connection relationships and structures are not improved in the present invention. Therefore, they will not be described in detail in the present application, and all of them can be understood through the prior patent documents.
[0020] At the same time, the present disclosure further provides each functional part inside the tubular structure for cooling the aggregate of ultrafine powder particles. As long as the connection of each functional part can be designed according to the need, the cross-sectional shape, aperture size, etc. of each functional part can be set to be the same, similar, deformed, or variable diameter, etc. according to the need. At the same time, the length of each functional part can be selected according to the need without affecting the implementation of the technical solution of the present disclosure. In addition, each functional part may be a plurality of sections or individual parts of the whole structure, and can be adjusted according to the actual needs (e.g., space, production volume, etc.), and does not limit or improve the technical solution of the present invention.
[0021] The design point of the present invention is a condensation cooling tubular structure set between a high-temperature evaporator and a reflux structure, which includes an exhaust and reflux structure 1, a waste reflux structure or waste collection structure 2, a particle formation control structure 3, a first jet cooling structure 4, a curved tube variable direction delivery structure 5, and a second jet cooling structure, which are connected in series.
[0022] Here, the front end of the exhaust and return structure 1 is connected to the exhaust port of the front high-temperature evaporator bore 7 , and the second jet cooling structure 6 is connected to a collection structure 8 .
[0023] The exhaust and return structure 1 includes at least a first flow path through which high-temperature steam enters, and a case for the exhaust and return structure 1 is provided outside the first flow path. A heat-insulating structure is provided between the first flow path and the case for the exhaust and return structure 1, and a reinforcing structure or a heating device is provided outside the first flow path. Here, the case for the exhaust and return structure 1 is a jacket structure, and a circulating cooling liquid is passed through the inside of the jacket structure. Here, the first flow path is made of a material that does not react physically or / and chemically with the material to be prepared. By heat insulation or heating, the temperature inside the exhaust and return structure 1 is maintained above the melting point of the ultrafine powder particle material to be prepared.
[0024] The waste recycling structure or waste collecting structure 2 includes at least a second flow path. The front end of the second flow path is connected to the first flow path, and the rear end of the second flow path is connected to the inner cavity of the particle forming control structure 3. While ensuring the passage of gas, the waste in the upper duct or flow path is melted and liquefied and then refluxed, or the waste in the upper duct or flow path is collected in a waste holding storage drum, thereby not impeding the passage of gas in the flow path. A heat retaining device or a heating device is installed on the outside of the second flow path. The heat retaining device or the heating device controls the temperature in the waste recycling structure to be maintained above the melting point of the material to be prepared, or the temperature in the gas flow path of the waste collecting structure to be maintained above the melting point of the material to be prepared, and the temperature in the waste holding storage drum to be maintained below the melting point of the material to be prepared.
[0025] The tip of the cavity of the particle forming control structure 3 is connected to the second flow path, and the rear end of the cavity of the particle forming control structure 3 is connected to a collection or cooling structure, and an ultrafine powder particle forming area is installed inside the particle forming control structure 3. The ultrafine powder particle forming area is a flow path structure and is the main place for particle forming control. A heat preservation or heating or cooling structure is installed inside the particle forming control structure 3, and the temperature of the ultrafine powder particle forming area is indirectly controlled by heat conduction or heat radiation, and the speed at which the particles pass through the ultrafine powder particle forming area with the carrier gas is controlled by the speed of the carrier gas and the cross-sectional dimension of the ultrafine powder particle forming area, thereby providing a stable and controlled condition for particle forming.
[0026] The particle molding control structure 3 is composed of an outer shell structure, an intermediate heat-insulating layer, and an inner heat-transfer layer. The outer shell structure is a jacket structure having a jacket structure for circulating a coolant. The intermediate heat-insulating layer has a single layer or multi-layer structure. The inner heat-transfer layer is molded with a heat-insulated flow path, i.e., an ultrafine powder particle molding region, which is used to indirectly control the temperature of the material flowing through the flow path by heat conduction or heat radiation.
[0027] Through the particle forming control structure, the material to be prepared goes from a gaseous state to a liquid state, from a liquid state to a solid state, the gaseous states contact each other and condense into small droplets, the small droplets contact each other and become larger droplets, or the gaseous states collide with the small droplets and become larger droplets, the larger droplets continue to collide with each other and grow or solidify into solid particles, the small droplets combine with the solid particles to become larger solid particles or nucleus shell structures, the gas combines with the solid particles to become larger solid particles or nucleus shell structures, the solid particles continue to cool, and particles with the desired particle size and shape are generated.
[0028] The first jet cooling structure 4 includes at least an internal third flow passage, the front end of the third flow passage is connected to the ultrafine powder particle molding area, the rear end of the third flow passage is connected to the curved pipe variable direction delivery structure, and a porous inner layer plate is provided outside the third flow passage, and cooling gas is uniformly blown into the third flow passage from the periphery to prevent the formed particles from softening or hardening due to high temperature.
[0029] The curved pipe variable direction delivery structure 5 includes a variable direction chamber, an intake duct and an exhaust duct are connected to the variable direction chamber, the intake duct is connected to the third flow path, and the exhaust duct is connected to the collection or cooling structure. The angle between the axis of the intake duct and the axis of the exhaust duct is 30° to 150°.
[0030] The cooling structure connected to the exhaust duct is a second jet cooling structure 6, and the second jet cooling structure 6 includes at least an internal fourth flow passage, the front end of the fourth flow passage is connected to the exhaust duct of the curved pipe variable direction delivery structure 5, and the rear end of the fourth flow passage is connected to the collection cooling structure 8. In the fourth flow passage, 1 to 12 jet holes of 5 to 50 mm for jet cooling to the central region of the fourth flow passage are provided. Alternatively, a porous jet tube is provided on the axis of the fourth flow passage.
[0031] The method for molding ultrafine powder particles using any one of the above tubular structures for agglomerating and cooling ultrafine powder particles includes steps S1, S2, S3, S4, S41, and S5. Step S1: The preparation material of the ultrafine powder particles to be prepared is put into a high-temperature evaporator, and the heated and evaporated material vapor and carrier gas are mixed into a mixed gas, which is then fed into the exhaust and reflux structure through the exhaust port of the high-temperature evaporator, and the internal temperature of the exhaust and reflux structure is controlled to be higher than the melting point of the required preparation material by heat retention or heating. Step S2: After the mixed gas passes through the exhaust and return structure and the waste return structure or waste collection structure, it enters the particle forming control structure, passes through a heat retention structure or a heating structure or a cooling structure in the ultrafine powder particle forming region in the particle forming control structure, and indirectly controls the temperature of each part of the ultrafine powder particle forming region by heat conduction or heat radiation, and controls the speed at which the particles pass through each internal region with the carrier gas according to the speed of the carrier gas and the cross-sectional dimensions of the duct, thereby providing a stable and controllable condition for forming the particles, and converts the preparation material from a gaseous state into a gaseous state. The liquid state is changed to a solid state, the gaseous state contacts each other and condenses into small droplets, the small droplets contact each other and become larger droplets, or the gaseous state and the small droplets contact each other and become larger droplets, the larger droplets continue to contact each other and grow or solidify into solid particles, the small droplets and the solid particles combine to become larger solid particles or form a nucleus shell structure, the gaseous state combines with the solid particles to become larger solid particles or form a nucleus shell structure, and the solid particles are continuously cooled to prepare particles of the desired particle size and morphology. Step S3: The particles of the desired particle size and shape prepared in step S2 enter the first jet cooling structure along with the carrier gas, and the porous inner layer plate uniformly blows cooling gas into the internal flow path from the periphery, mixing with the entering high-temperature gas and formed particles to cool them. Step S4: The cooled particles enter the curved pipe variable direction delivery structure along with the carrier gas, and defective particles (particles that do not meet the standards and cannot become products) and good particles (particles that meet the standards and can become products) are separated from each other. The good particles are transported to the next process along with the carrier gas, and the defective particles are collected in the waste circulation structure or waste collection structure. Step S41: The non-defective particles enter the second jet cooling structure along with the carrier gas, and are jet-cooled toward the central region of the flow path inside the second jet cooling structure via a cooling gas outlet provided inside the second jet cooling structure or a jet pipe provided on the axial line of the second jet cooling structure. Step S5: The non-defective particles enter the collecting structure along with the carrier gas, and the formed ultrafine powder particles are separated from the carrier gas, among which the ultrafine powder particles are collected as products, and the carrier gas is discharged or recycled.
[0032] The aggregated, cooled and shaped particles are collected as a product, and the carrier gas is discharged or recycled.
[0033] Through the above structure, together with the high-temperature evaporator at the front, the collecting and cooling structure at the rear, the heating system for supplying a heat source to the high-temperature evaporator, the supply system for supplying raw material to the front of the high-temperature evaporator, the circulating cooling system for cooling, the gas source or circulating gas system for carrier gas and cooling, and the pressure balance system for controlling the pressure balance, a continuous cycle production process of particle aggregation, cooling and molding is completed, and nano-scale, sub-micron-scale or micron-scale powder with uniform particle size, stable morphology and good dispersibility can be produced.
[0034] While embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions, and variations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is best defined by the appended claims. [Explanation of symbols]
[0035] 1: Exhaust and return structure 2: Waste return structure or waste collection structure 3: Particle forming control structure 4: First jet cooling structure 41: Jet in the first jet cooling structure 5: Curved pipe variable direction delivery structure 6: Second jet cooling structure 61: Jet in the second jet cooling structure 7: High temperature evaporator bore 8: Collection Structure 81: Jet in the Collector
Claims
1. A tubular structure for cooling and agglomerating ultrafine powder particles, which is provided in an ultrafine powder particle preparation system including a high-temperature evaporator, a carrier gas supply system and a collection structure, comprising: a tubular structure for cooling the ultrafine powder particles is located between the high temperature evaporator and the collection structure; The present invention includes an exhaust and return structure, a waste return structure or waste collection structure, a particle shaping control structure, a first jet cooling structure, a curved tube variable direction delivery structure, and a second jet cooling structure, which are connected in series; The front end of the exhaust and return structure is connected to a front high-temperature evaporator; a rear end of the second jet cooling structure connected to the collection structure; The exhaust and return structure, the waste return structure or waste collection structure, the particle formation control structure, the first jet cooling structure, the curved pipe variable direction delivery structure and the second jet cooling structure are provided with flow paths that are sequentially connected to each other; The carrier gas supply system supplies carrier gas from the high temperature evaporator through the exhaust and return structure, the waste return structure or waste collection structure, the particle formation control structure, the first jet cooling structure, and the curved tube variable direction delivery structure to the second jet cooling structure; The high-temperature evaporator evaporates the ultrafine powder particles to form a vaporized material, and the vaporized material is supplied to a tubular structure for cooling the ultrafine powder particles through a carrier gas; said collection structure collecting the shaped ultrafine powder particles; the bent pipe variable directional delivery structure includes a first portion connected to the first jet cooling structure and a second portion connected to the second jet cooling structure and bent from the first portion; the first portion of the exhaust and return structure, the waste return structure or waste collection structure, the particle forming control structure, the first jet cooling structure and the curved tube variable direction delivery structure are provided in a sloping manner from bottom to top in sequence; the second portion of the curved pipe variable direction delivery structure and the second jet cooling structure are provided in a sequential manner inclined from top to bottom, The curved tube variable direction delivery structure separates the defective particles from the good particles, which are ultrafine powder particles, and passes the good particles through the first part by the carrier gas and into the second part, and collects the defective particles in the waste return structure or waste collection structure by the partial inclination of the tubular structure for agglomerating and cooling the ultrafine powder particles. A tubular structure for cooling the aggregation of ultrafine powder particles, characterized in that
2. The front end of the exhaust and return structure is connected to the exhaust port of the high-temperature evaporator; The tubular structure for cooling the agglomeration of ultrafine powder particles as described in claim 1, characterized in that the inside of the exhaust and return structure includes at least a first flow path into which high-temperature steam enters, and a heat-retaining or heating device is provided on the outside of the first flow path.
3. The waste return structure or waste collection structure includes at least a second flow path therein; The front end of the second flow path is connected to the first flow path, The rear end of the second flow path is connected to the inner cavity of the particle formation control structure, 3. The tubular structure for agglomerating and cooling ultrafine powder particles according to claim 2, further comprising a heat retaining or heating device provided on the outside of the second flow path.
4. The first jet cooling structure includes at least an internal third flow passage, a front end of the third flow passage is connected to an inner cavity as a flow passage of the particle forming control structure, and a rear end of the third flow passage is connected to a flow passage of the first part of the curved tube variable direction delivery structure, The tubular structure for cooling the aggregation of ultrafine powder particles as described in claim 3, characterized in that a porous inner layer plate is provided outside the third flow path, and cooling gas is uniformly blown into the third flow path from the periphery.
5. The first portion and the second portion each include an intake flow path and an exhaust flow path, the intake passage is connected to the third passage, and the exhaust passage is connected to a passage of the second jet cooling structure; 5. The tubular structure for cooling the agglomeration of ultrafine powder particles as claimed in claim 4, wherein an angle between the axis of the intake passage and the axis of the exhaust passage is 30° to 150°.
6. The second jet cooling structure includes at least an internal fourth flow passage, The tubular structure for cooling and agglomerating ultrafine powder particles as claimed in claim 5, wherein the front end of the fourth flow passage is connected to the exhaust flow passage of the curved tube variable direction delivery structure, and the rear end of the fourth flow passage is connected to a collection structure.
Citation Information
Patent Citations
Method for internal-reverse-flow type rubbish removal
CN103537703A
Surface treatment method for superfine metal nickel powder
CN109648093A
Direction-changing tank type material distributing structure for preparing superfine powder material
CN112762263A
Superfine powder particle aggregation cooling pipe type structure and superfine powder particle forming method
CN112891967A
Ultra-fine powder particle gathering and cooling tank type structure and ultra-fine powder particle forming method
CN112915919A